Directed energy and sensing for detecting inconsistencies in laminates
By using a scanning mirror system with energy sources and imaging devices during the assembly process of composite materials, the energy dissipation of the composite surface is detected, and the problems of difficulty in detecting defects before curing and high repair costs after curing are solved, and fast and accurate defects are achieved Testing improves manufacturing efficiency.
Patent Information
- Application Number
- CN201910285286.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2018-04-10
- Filing Date
- 2019-04-10
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2039-04-10
AI Technical Summary
During the assembly process of composite materials, the accuracy of detecting defects and impurities before curing is low, resulting in the components being scrapped or expensive repairs after curing. The existing thermal imaging methods require manual or robot assistance, which is time-consuming and not suitable for large areas. examine.
Using a system combining energy source and imaging devices, the energy level of the area to be inspected is increased through the first scanning mirror, and the second scanning mirror synchronizes the imaging device to detect energy dissipation, identify inconsistencies on the surface of composite materials, and achieve long-distance rapidity. Test.
It realizes rapid and accurate detection of defects on uncured composite materials, shortens inspection time, reduces operation steps, improves detection efficiency, and avoids the cost and efficiency losses of expensive repairs after curing.
Smart Images

Figure CN110361393B_ABST
Abstract
Description
[0001] Prior application
[0002] This application claims priority to U.S. Provisional Patent Application No. 62 / 655,587, filed on April 10, 2018, the contents of which are incorporated herein by reference. Technical Field
[0003] The present application generally relates to improved methods of detecting inconsistencies or foreign objects that cause defects during the assembly process. More specifically, the present invention relates to detecting inconsistencies or foreign objects by increasing the energy level of a surface and sensing the inconsistent dissipation of the energy level. Background Art
[0004] During certain manufacturing processes, there is the possibility that impurities or other defects become trapped in the assembly, making the subsequent part unusable. For example, when constructing a composite part, a multi-layer or multi-ply composite material is sequentially placed on a mandrel or work surface to form, for example, a lightweight aerospace component. Once a predetermined number of plies have been placed, the epoxy or other resin impregnated with the fiber material of each of the layers is cured. If impurities, voids or other defects become trapped between the layers, the proper interlayer bonding when curing the composite may be defective. Such defects concentrate stress within the component and may lead to catastrophic failure of the component.
[0005] After the composite forming the component is cured, the component is usually tested to verify that the component is free of defects or at least within the necessary quality standards. Thermal testing or ultrasonic testing is performed to identify defects that will compromise the structural integrity of the component outside the required quality standards, but has always been performed only after the polymer forming the component has been cured. When these defects have been identified, the cured component is usually scrapped at great expense and loss of manufacturing efficiency. Alternatively, expensive repairs are performed at additional cost and loss of manufacturing efficiency.
[0006] To avoid these manufacturing setbacks, it is desirable to verify the composite component before curing the resin. However, accurate detection of these defects before curing has proven to be difficult to achieve. To date, verification has been performed only after curing with limited success.
[0007] An example of post-curing verification of a composite is the use of thermal imaging. Thermal imaging requires raising the temperature of an already cured composite component. If the surface of the cured component is heated, the thermal monitor attempts to detect inconsistencies in the heat dissipation. Efforts have been made to improve this method to heat the cured component more accurately and capture thermal distribution maps. However, these systems require the heat source and thermal camera to be placed very close to the surface of the cured composite. This method either requires manual positioning of the heat source and thermal camera, or requires the use of a robotic arm or gantry, especially when inspecting large areas (such as, for example, commercial aircraft wings or fuselages). Since it takes time for heat transfer to occur, the measurement process takes several seconds, which causes unacceptable delays in manufacturing.
[0008] While this method does identify defective components, it has only proven to be sufficiently accurate on fully cured components. As a result, the components must either be scrapped or undergo expensive repairs. Therefore, to avoid this dilemma, it would be useful to develop an inspection process and system that is performed before the resin is cured and the multi-layer plies are permanently adhered. Summary of the invention
[0009] A method and assembly for detecting inconsistencies in an assembly using an energy source and an imaging device are disclosed. The energy source directs energy to the surface of the assembly via a first scanning mirror for increasing the energy level of the area to be inspected. The imaging device directs the field of view of the imaging device to the area to be inspected via a second scanning mirror, and the imaging device detects the rate of change of energy at the surface of a laminated composite. Movement of the first scanning mirror is associated with movement of the second scanning mirror for directing the field of view of the imaging device to the area of the surface being inspected after the energy level of the area of the surface being inspected has been increased. The imaging device detects the energy dissipation at the area of the surface being inspected and identifies a defect in the assembly associated with the inconsistency.
[0010] Due in part to the rapid movement of the first scanning mirror and the second scanning mirror in a correlated or synchronized manner, the inspection system of the present invention is capable of inspecting, for example, an uncured composite component from a great distance. The first scanning mirror and the second scanning mirror are sequentially scanned over a large area while the energy source and the imaging device remain stationary. Because the first mirror and the second mirror are moved in rapid succession, even very precise inconsistencies in energy dissipation on an uncured layer of a ply are detected. In this manner, defects are detected quickly at a great distance, thereby shortening inspection time and freeing the operator from an extra step in the manufacturing process. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Other advantages of the present invention will be readily appreciated as they become better understood by reference to the following detailed description when considered in conjunction with the accompanying drawings, in which:
[0012] Figure 1 shows an exemplary cross-sectional view of a suitably constructed composite assembly;
[0013] Figure 2 An exemplary cross-sectional view showing an impurity trapped between two layers of a plate layer;
[0014] Figure 3 A schematic diagram showing a detection system of the present invention;
[0015] Figure 4 A top view showing a ply layer with impurities trapped beneath it; and
[0016] Figure 5 Shown is a top view of an image of one ply produced by the imaging device of the present invention. DETAILED DESCRIPTION
[0017] During manufacturing processes, such as, for example, the manufacture of laminated composites for aircraft wings and the like, serious defects are known to occur when objects become trapped between layers. Figure 1 , a cross section of a suitably constructed composite assembly is schematically shown at 10. A mandrel or assembly tool 12 is used as a substrate for accommodating a first ply layer 14. The first ply layer 14 is formed by cutting a fiber-reinforced sheet of a composite material (not shown) into a fiber-reinforced strip or portion suitable for a predetermined configuration of the object being formed. The use of "composite material" and "ply" throughout this application is merely exemplary and not limiting in any way. The invention of the present application can be used to identify inconsistencies on various surfaces, including, but not limited to, welded surfaces, coated surfaces, metals, and any other surface or substrate on which non-destructive determination of inconsistencies by evaluating energy dissipation may be useful. Composite materials are thermosetting or thermoplastic polymers impregnated with fillers (such as, for example, carbon fibers, glass fibers, etc.) to provide additional strength to the composite. After the relevant portion of the assembly tool 12 is covered with the first ply layer 14, the second ply layer 16 is covered on the first ply layer 14.
[0018] As is known to those skilled in the art, after the second ply layer 16 is applied to the first ply layer 14, additional ply layers (not shown) are applied to the second ply layer 16 to achieve the desired composite thickness. Once a sufficient number of layers have been put in place, the composite material is cured to induce inter-layer adhesion by cross-linking or other chemical interactions that prevent the layers from separating. As will become more apparent herein below, the heat dissipation or energy dissipation of a properly constructed, defect-free composite is expected to be uniform.
[0019] Figure 2A defective composite assembly is schematically shown at 20. In this example, a first ply layer 14 is overlaid on an assembly tool 12. A second ply layer 16 is overlaid on the first ply layer 14, but an impurity 18 becomes trapped between the first ply layer 14 and the second ply layer 16. While the impurity 18 is generally represented, examples of impurities include, but are not limited to, packaging, liner paper, clothing, industrial contaminants, and even bubbles or voids 19. The problems associated with embedded impurities 18 have been described above and will not be further described here.
[0020] Now refer to Figure 3 , the inspection system of the present invention is schematically shown at 30. The inspection system includes an energy source 32 that generates an energy beam 34. The energy beam 34 is optionally focused by a lens 36. The energy beam is directed toward a first scanning mirror 38 and redirected to a predetermined inspection area 40 on a surface 42 of an assembly. The first scanning mirror 38 includes a first scanning member 44 and a second scanning member 46. The first scanning member 44 and the second scanning member 46 include a servo first reflector 48 and a servo second reflector 50, respectively, which cooperatively and quickly redirect the energy beam 34 along the inspection area 40 to increase the energy level of the inspection area 40. The first scanning member 44 is driven by a first servo motor 45, and the second scanning member 46 is driven by a second servo motor 47. The energy beam 34 is generated by any one of a halogen lamp, a xenon flash lamp, or a coherent light source. When one or a combination of these energy sources 32 is selected, the temperature of the inspection area 40 is increased from ambient temperature to a temperature slightly above ambient temperature. Other energy sources 32 are within the scope of the present invention, including, but not limited to, those that excite molecules of the polymer above a ground state.
[0021] When the energy source 32 is selected to increase the temperature of the composite assembly 10, 20, the temperature increase is only about 1°C. The uniform layering of the properly constructed assembly 10 results in uniform heat (energy) absorption and dissipation. Impurities 18 (or air pockets) disposed between the first ply layer 14 and the second ply layer 16 result in non-uniform heat (energy) absorption and dissipation.
[0022] An imaging device 48 is provided that is capable of detecting non-uniform energy absorption and dissipation from the inspection region 40. The imaging device 48, in one embodiment, is a camera 50 having thermal imaging capabilities for detecting small thermal variations on a surface, such as, but not limited to, a long wave infrared camera including a cooled mercury cadmium telluride array. Alternative imaging devices 48 that are capable of detecting energy variations on the surface of a composite, including, but not limited to, detecting molecular excitations, are also within the scope of the present invention.
[0023] The imaging device 48 includes a second scanning mirror 52 for redirecting a field of view 54 of a camera 50. The field of view 54 of the camera 50 is optionally focused by a camera lens 56. The field of view 54 is redirected by the second scanning mirror 52 toward a predetermined inspection area 40 on the assembly surface 42. The second scanning mirror 52 includes a third scanning member 58 and a fourth scanning member 60. The third scanning member 58 and the fourth scanning member 60 include a servo-driven third reflector 62 and a servo-driven fourth reflector 64, respectively, which cooperatively and rapidly redirect the camera field of view 54 along the inspection area 40 to detect the energy level of the inspection area 40.
[0024] The first scanning member 44, the second scanning member 46, the third scanning member 58 and the fourth scanning member 60 are cooperatively driven by a controller 66. The controller 66 coordinates the scanning members 44, 46, 58, 60 so that the camera field of view 54 quickly follows the movement of the energy beam 34. The increase in the energy level of the inspection area 40 is slight to avoid adverse physical changes that dissipate quickly in the complex. Therefore, the camera field of view 54 closely follows the path 68 of the energy beam.
[0025] The first scanning mirror 38 and the second scanning mirror 52 constitute a galvanometer system. In this embodiment, the galvanometer assembly includes two scanning mirrors 38, 52, which cooperate to synchronize the field of view 54 of the imaging device 50 with the delivery position of the energy beam 34 from the energy source 32. However, it should be understood that a rapidly moving galvanometer assembly including a single scanning mirror can also synchronize the field of view 54 of the imaging device 50 with the delivery position of the energy beam 34 from the energy source 32. In this embodiment, the scanning mirrors will synchronously and continuously redirect one of the field of view 54 of the imaging device 50 and the energy beam 34 away from the surface being inspected while redirecting the other of the field of view 54 and the energy beam 34 toward the surface.
[0026] Different methods can be used to synchronize the path of the energy beam 34 over the surface with the path of the field of view 54 of the imaging device 50. For example, a beam splitter (not shown) will reflect the shorter higher wavelength energy beam 34 to the surface through the scanning galvanometer, but allow the longer wavelengths associated with the surface energy to pass to the camera. Additional accuracy is obtainable by rapidly activating and deactivating the energy beam 34 in synchronization with the field of view 54 of the imaging device so that the camera 50 prevents the reflected energy from the energy beam 34 from interfering with the accurate imaging of the surface 42 being viewed through the imaging device 50.
[0027] Multiple inspection areas 40 are optionally subjected to an increase in energy and then scanned by the camera 50 so that sequentially arranged images can be interleaved. In this way, a simultaneous response to the energy pulses is obtained. The combination of multiple individual image segments based on the accurate positioning of the camera field of view 54 provides a high-resolution thermal map image that enables detection of even very small defects present in the assembly 20 by identifying slight deviations in energy dissipation.
[0028] Further enhancements are achieved when the inspection system 30 is integrated with a laser projector (not shown) that is used to locate the assembly surface 42 and project a laser template that guides the operator where to place a ply. If the inspection system 30 is registered to the reference frame of the assembly surface 42 and integrated into the assembly process, the imaging sequence performed by the inspection system 30 can be limited to the nearest area of placement of a ply, further improving the efficiency of the inspection.
[0029] For example, the laser projection system disclosed in U.S. Patent No. 9,200,899, the contents of which are incorporated herein by reference, discloses a laser projection component that uses a photogrammetry component to locate a workpiece or stack for projecting a laser template. Figure 3 Thus, the photogrammetric or equivalent positioning system disclosed in the '899 patent also directs where the first scanning mirror 38 and the second scanning mirror 52 direct the energy beam 34 from the energy source 32 and the camera field of view 54, thereby providing an efficient and fast response time.
[0030] The controller 66 coordinates the movement of the laser projector disclosed in the 9,200,899 patent with the first scanning mirror 38 and the second scanning mirror 52 of the present application. In one embodiment, the first scanning mirror 38 and the second scanning mirror 52 scan the area of interest 40 before the resin impregnating the carbon fibers is cured as described above. This allows the operator to take necessary corrective actions without having to subject the laminated composite to the repair process by removing only the plies previously placed to correct the defects. Therefore, it should be understood that the temperature of the inspection area 40 of the composite assembly 10 is not raised to the curing temperature of the resin to avoid unwanted polymer reactions.
[0031] Now refer to Figure 4 and Figure 5 , impurities (such as, for example, plastic knots 70) are placed between the uncured first ply layer 14 and the second ply layer 16. Figure 4It is easy to see that the flat black opaque nature of the second ply layer 16 makes it almost impossible for an operator to detect the plastic knot 70, even though it may appear obvious. In addition, a grid of voids 71 is formed in the first ply layer 14 to represent the air pockets formed between the two layers 14,16. Figure 5 An image of the first ply 14 is shown after being subjected to the energy beam 34, thereby increasing the energy level of the composite. The camera produces an image on a monitor 72 that indicates to the operator the location of impurities 70 (18) based on the different levels of energy dissipation due to impurities 18, or even simply due to voids 71, which are caused by bubbles disposed between the first ply layer 14 and the second ply layer 16. The monitor 72 includes a template, a computer monitor, a smart device, or even goggles. The monitor field of view is optionally related to the location of the inspection area 40 and produces an expanded field of view of the inspection area in a manner similar to that disclosed in co-pending U.S. Patent Application No. 15 / 058,867, the contents of which are incorporated herein by reference, to further assist the operator in finding defects.
[0032] In one embodiment, the first scanning mirror 38 and the second scanning mirror 52 are driven by a galvanometer scanning system (such as the 62xxH series from Cambridge Technologies). Each of the reflectors 48, 50, 62, 64 includes a 350nm to 12μm broadband mirror coating. In addition, the imaging device 48 is an uncooled micro-bolometer detector array, such as a FLIR A325sc infrared camera with a 76mm focal length camera lens 56, thereby providing a 6x4.5 degree field of view through the second scanning mirror 52.
[0033] The present invention has been described herein in an illustrative manner, and it is to be understood that the terms used are intended to be words or descriptive properties, rather than limiting. It is apparent that many modifications and variations of the present invention are possible in accordance with the above teachings. The present invention may be implemented in a manner different from that specifically described within the scope of the appended claims.
Claims
1. A method for detecting inconsistencies in an assembly using an energy source and an imaging device, comprising the steps of: providing an energy source and directing energy from the energy source toward a surface of the laminated composite assembly to be inspected via a first scanning mirror, thereby increasing the energy level of the area to be inspected; providing an imaging device, and directing the field of view of the imaging device to the area to be inspected by a second scanning mirror, and the imaging device detecting the rate of change of energy at the surface of the laminated composite; synchronizing movement of the first scanning mirror with movement of the second scanning mirror to direct the field of view of the imaging device toward the area of the surface being inspected after the energy level of the area of the surface being inspected is increased; as well as Dissipated changes in energy levels at regions of the surface being inspected are detected, thereby identifying defects in the assembly associated with the inconsistency.
2. The method according to claim 1, wherein: The step of providing an energy source is further defined as providing a thermal energy source to increase the temperature of the assembly in the area to be inspected prior to directing the field of view of the imaging device toward the area to be inspected.
3. The method according to claim 2, further comprising: The step of redirecting the energy source away from the area to a second area to be inspected after providing the desired energy exposure.
4. The method according to claim 3, further comprising: After the step of increasing the energy level of the second area to be inspected, the step of directing the imaging device toward the second area to be inspected is performed.
5. The method according to claim 1, wherein: The step of providing an energy source is further defined by providing a thermal energy source.
6. The method according to claim 5, wherein: The step of providing a thermal energy source is further defined by providing one of a halogen lamp, a xenon flash lamp, and a coherent light source.
7. The method according to claim 3, wherein: The step of providing an imaging device is further defined by providing a long wave infrared camera comprising a cooled mercury cadmium telluride array.
8. The method according to claim 1, further comprising: The step of sequentially redirecting energy from said energy source to sequential areas to be inspected.
9. The method according to claim 1, further comprising: The imaging device repeatedly scans sequential areas to be inspected to construct a time-sequenced step of energy dissipation response.
10. The method according to claim 9, wherein: The step of configuring the time-sequenced energy dissipation is further defined by detecting the location of a defect associated with the inconsistency through a reduction in the inconsistency in energy conduction.
11. The method according to claim 1, further comprising: The step of limiting the area to be inspected to the designated placement area of the ply of composite material.
12. The method according to claim 11, further comprising: The step of informing the first scanning mirror of the energy source and the second scanning mirror of the imaging device with a signal of the position of the area to be inspected, the position of the area to be inspected being defined by a laser template projected by a laser projector.
13. A method of detecting inconsistencies in an assembly using an energy source and an imaging device, comprising the steps of: providing an energy source so that the energy beam is directed toward the surface to be inspected; providing an imaging device including a field of view of the surface to be inspected and capable of detecting changes in energy on the surface to be inspected; providing a galvanometer system to synchronize the delivery position of the energy beam on the surface with the field of view of the surface through the imaging device; using the energy source to increase the energy level of the surface; using the imaging device to detect inconsistencies in the assembly based on uneven energy dissipation across the surface; as well as The galvanometer system is used to synchronize the delivery of the energy beam with the position of the imaging device's field of view on the surface, thereby enabling the imaging device to detect inconsistencies at the surface of the assembly being inspected.
14. The method according to claim 13, wherein: The step of providing a galvanometer system is further defined by providing a galvanometer system comprising a first scanning mirror and comprising a second scanning mirror, wherein the first scanning mirror is used to redirect the energy beam from the energy source and the second scanning mirror is used to redirect the field of view of the imaging device in a synchronized manner on the surface being inspected.
15. The method according to claim 13, further comprising: The step of sequentially moving the position of the energy beam over the surface being inspected, followed by synchronously moving the field of view of the imaging device along the surface following an increase in energy through the energy beam.
Citation Information
Patent Citations
Laser projection system with video overlay
US20160260259A1
Directed energy and sensing for thermal detection of foreign objects
US62655587P0
Laser projection system and method
US9200899B2
Nondestructive Tester.
GB1151081A
Method and apparatus for detection of defects using thermal stimulation
US20040028113A1