Athermal arrayed waveguide grating
By introducing a multi-layer structure of negative temperature coefficient material into the arrayed waveguide grating, the temperature drift problem of the arrayed waveguide grating at different temperatures is solved, heatless operation and simplified design are achieved, the temperature drift coefficient is reduced, and the stability of the device is improved. sex.
Patent Information
- Application Number
- CN201910812393.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-08-30
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2039-08-30
AI Technical Summary
The temperature drift coefficient of the central wavelength of arrayed waveguide grating is large at different ambient temperatures, which requires additional temperature control devices, increases design complexity and power consumption, and is limited in use in environments with large temperature differences.
Design a heatless array waveguide grating, using a multi-layer structure of negative temperature coefficient materials such as titanium dioxide and double-layer silicon dioxide materials. The negative temperature coefficient material is used to compensate for the thermal expansion and deformation of the silicon-based substrate and reduce the temperature drift coefficient.
It achieves a heatless working mode, simplifies the structural design, reduces the temperature drift coefficient, meets process requirements, avoids additional mechanical structures and power input, and improves the stability of the device.
Smart Images

Figure CN110376677B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a planar optical waveguide device, belonging to a athermal array waveguide grating. Background Art
[0002] Arrayed waveguide grating is an angular dispersion passive device based on planar optical waveguide technology. It was first proposed by Smit in the late 1980s and has since attracted the attention of many research institutions such as Bell Research and NTT. With the development of planar optical waveguide technology, corresponding products have gradually been commercialized. Compared with other wavelength division multiplexing devices, arrayed waveguide grating has the advantages of flexible design, low insertion loss, good filtering, long-term stability, and easy fiber coupling. In addition, arrayed waveguide gratings are relatively easy to combine with active devices such as optical amplifiers and semiconductor lasers to achieve monolithic integration, which is a research hotspot today.
[0003] There is a correlation between the central wavelength of the arrayed waveguide grating and the ambient temperature. The main principles are as follows:
[0004]
[0005] The above formula is the central wavelength expression of the arrayed waveguide grating, where n eff is the effective refractive index of the waveguide, ΔL is the geometric length difference between adjacent waveguides, and m is the diffraction order, which determines the grating dispersion capability. eff Both ΔL and ΔL can be described by temperature-dependent functions. The change of the central wavelength of the device with temperature can be obtained by taking the derivative of the above formula with respect to temperature, and the final expression is as follows:
[0006]
[0007] Among them
[0008] α sub is the linear expansion coefficient of the array waveguide grating substrate material. For array waveguide gratings with silicon-based silicon dioxide structure, the thickness of the silicon dioxide waveguide is much smaller than that of the silicon-based substrate. The dimensional deformation caused by temperature change is mainly determined by the substrate material. sub ≈2.6x10 -6 ,Conventional silica waveguide, n eff =1.456, after comprehensive calculation, the center wavelength temperature drift coefficient is 0.012nm / deg.
[0009] In order to keep the center wavelength of the arrayed waveguide grating constant under different ambient temperatures and reduce the temperature drift coefficient of its center wavelength, the traditional technology is to attach a temperature control device, such as a heater or an electro-cooler to stabilize the working temperature of the AWG, which requires additional power input, and in working environments with large temperature differences, the use of active temperature control is limited. Conventional athermal technology requires the introduction of additional mechanical structures to the grating to achieve the wavelength-temperature drift compensation function, and this technology itself requires relatively complex structural design and process methods.
[0010] Therefore, in order to solve the above problems, it is necessary to provide a athermal array waveguide grating with a simple structure. Summary of the invention
[0011] In order to solve the above technical problems, the purpose of the present invention is to provide a athermal array waveguide grating with a negative temperature characteristic waveguide structure, which utilizes a specially designed negative temperature change characteristic to achieve an athermal working mode of the device.
[0012] In order to achieve the above object, the present invention provides the following technical solutions:
[0013] A athermal array waveguide grating comprises a silicon-based substrate; and disposed on the silicon-based substrate:
[0014] at least one input waveguide for inputting an optical signal;
[0015] A first free transmission region formed by a first slab waveguide, coupled to the output end of the input waveguide;
[0016] an athermal array waveguide coupled to an output end of the first free transmission region;
[0017] A second free transmission region formed by a second slab waveguide is coupled to the output end of the waveguide array;
[0018] At least one output waveguide for outputting an optical signal, coupled to an output end of the second free transmission region;
[0019] The athermal array waveguide comprises a cladding layer and a waveguide core layer, wherein the core layer is arranged in the cladding layer and has a refractive index higher than that of the cladding layer;
[0020] The waveguide core layer includes a periodically arranged multilayer structure, which includes: a double-layer silicon dioxide material and a negative temperature coefficient material arranged between the double-layer silicon dioxide material; the negative temperature coefficient material is used to compensate for the dimensional deformation of the silicon-based substrate after being heated, so as to reduce the temperature drift coefficient of the athermal array waveguide grating.
[0021] Furthermore, the negative temperature coefficient material is titanium dioxide.
[0022] Furthermore, in the multilayer structure, the thickness of the silicon dioxide material is 0.5-1 μm, and the thickness of the titanium dioxide material is 0.05-0.1 μm.
[0023] Furthermore, the effective refractive index of the multilayer structure is 1.5-1.6.
[0024] Furthermore, the effective refractive index temperature coefficient of the multilayer structure is -2e-6 to -4e-6 / K.
[0025] Furthermore, the thickness of the negative temperature coefficient material is related to the optimum effective refractive index of the waveguide core.
[0026] Further, the thickness of the negative temperature coefficient material is related to the optimum effective refractive index temperature coefficient of the waveguide core layer.
[0027] The beneficial effects of the present invention are:
[0028] The technical solution of the present invention overcomes the problem of complex design structure of the athermal array waveguide grating, does not require additional structural design and assembly process, simplifies the athermal array waveguide grating structure, introduces negative temperature coefficient material into the core layer structure, makes the grating itself have athermal characteristics, and ultimately ensures that the temperature drift coefficient of the grating meets the process requirements, thereby achieving athermal working conditions.
[0029] The above description is only an overview of the technical solution of the present invention. In order to more clearly understand the technical means of the present invention and implement it according to the contents of the specification, the following is a detailed description of the preferred embodiments of the present invention in conjunction with the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 This is a schematic diagram of the structure of the athermal array waveguide core layer of Example 1, wherein 10 is a multilayer structure, 11 is a silicon dioxide material, 12 is a negative temperature coefficient material, and 30 is a silicon dioxide cladding.
[0031] Figure 2 It is a schematic diagram of the structure of the athermal array waveguide grating of the second embodiment, wherein 101-input waveguide, 102-output waveguide, 103-first free transmission region, 104-second free transmission region, 105-athermal array waveguide, 140-silicon-based substrate. DETAILED DESCRIPTION
[0032] The specific implementation of the present invention is further described in detail below in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention.
[0033] Embodiment 1
[0034] See also Figure 1, a heatless array waveguide, comprising a silicon dioxide cladding 30 and a waveguide core layer arranged between the silicon dioxide cladding 30, the waveguide core layer comprising a periodically arranged multilayer structure 10, the multilayer structure 10 comprising: a double layer of silicon dioxide material 11 and a negative temperature coefficient material 12 arranged between the double layer of silicon dioxide material 11; the negative temperature coefficient material 12 is used to Figure 2 ) is compensated for the dimensional deformation after being heated to reduce the temperature drift coefficient of the athermal array waveguide grating.
[0035] In the above-described embodiments, the refractive index of the core layer is higher than that of the cladding layer.
[0036] In the above embodiment, the negative temperature coefficient material 12 is titanium dioxide.
[0037] In the above embodiment, in the multilayer structure, the thickness of the silicon dioxide material 11 is 0.5-1 μm, and the thickness of the titanium dioxide material 12 is 0.05-0.1 μm. The thickness of the negative temperature coefficient material 12 is related to the optimal effective refractive index and the optimal refractive index temperature coefficient of the waveguide core layer. For example, when the thickness of the silicon dioxide material 11 is 1 μm, the thickness of the titanium dioxide waveguide 12 is 0.1 μm, and the thickness of the multilayer structure 10 is 4.2 μm; the effective refractive index of the silicon dioxide material 11 is 1.476, and its effective refractive index temperature coefficient is 7.6e-6 / k; the effective refractive index of the titanium dioxide waveguide 12 is 2.614, and its effective refractive index temperature coefficient is -1.2e-4 / k; the effective refractive index of the multilayer structure 10 is 1.5795, and its effective refractive index temperature coefficient is -4e-6 / k.
[0038] In other embodiments, the effective refractive index of the multilayer structure 10 is 1.5-1.6.
[0039] In other embodiments, the optimal effective refractive index temperature coefficient of the waveguide core layer is -2e-6 to -4e-6 / K.
[0040] Figure 1 In the illustrated embodiment, two periods of multilayer structures 10 are provided, but the number and thickness of the multilayer structures 10 in the present invention are not limited thereto.
[0041] Embodiment 2
[0042] See also Figure 2 The present invention further provides a athermal arrayed waveguide grating device, comprising a silicon-based substrate 140, and:
[0043] an input waveguide 101 for inputting an optical signal;
[0044] A first free transmission region 103 formed by a first slab waveguide is coupled to the output end of the input waveguide 101;
[0045] The athermal array waveguide 105 prepared in the first embodiment of the present invention is coupled to the output end of the first free transmission region 103;
[0046] A second free transmission region 104 formed by a second slab waveguide is coupled to an output end of the waveguide array 105;
[0047] At least one output waveguide 102 for outputting an optical signal is coupled to an output end of the second free transmission region 104 .
[0048] Based on the grating device of the above waveguide structure, the calculated center wavelength temperature drift coefficient is -0.0014nm / deg, while the center wavelength temperature drift coefficient of the array waveguide grating with silicon-based silica structure is 0.012nm / deg after comprehensive calculation, which is an order of magnitude less.
[0049] The present invention improves the structural design of the waveguide so that the waveguide itself has negative temperature characteristics, thereby offsetting the influence of the thermal expansion coefficient of the silicon-based material in the grating device, greatly reducing the overall temperature drift coefficient of the array waveguide grating device, and improving the device performance.
[0050] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0051] The above-mentioned embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. A athermal arrayed waveguide grating, comprising a silicon-based substrate; and disposed on the silicon-based substrate: at least one input waveguide for inputting an optical signal; A first free transmission region formed by a first slab waveguide, coupled to the output end of the input waveguide; an athermal array waveguide coupled to an output end of the first free transmission region; A second free transmission region formed by a second slab waveguide, coupled to an output end of the waveguide array; At least one output waveguide for outputting an optical signal, coupled to an output end of the second free transmission region; The athermal array waveguide comprises a silica cladding and a waveguide core layer, wherein the core layer is arranged in the silica cladding and has a refractive index higher than that of the silica cladding; The waveguide core layer comprises a periodically arranged multilayer structure, wherein the multilayer structure comprises: A double-layer silicon dioxide material and a negative temperature coefficient material disposed between the double-layer silicon dioxide material; The negative temperature coefficient material is used to compensate for the dimensional deformation of the silicon-based substrate after being heated, so as to reduce the temperature drift coefficient of the athermal array waveguide grating.
2. The athermal arrayed waveguide grating according to claim 1, characterized in that: The negative temperature coefficient material is titanium dioxide.
3. The athermal arrayed waveguide grating according to claim 1, characterized in that: In the multilayer structure, the thickness of the silicon dioxide material is 0.5-1 μm, and the thickness of the titanium dioxide material is 0.05-0.1 μm.
4. The athermal arrayed waveguide grating according to claim 1, characterized in that: The effective refractive index of the multilayer structure is 1.5-1.
6.
5. The athermal arrayed waveguide grating according to claim 1, characterized in that: The effective refractive index temperature coefficient of the multilayer structure is -2e-6 to -4e-6 / K.
6. The athermal arrayed waveguide grating according to claim 1, characterized in that: The thickness of the negative temperature coefficient material is related to the optimum effective refractive index of the waveguide core.
7. The athermal arrayed waveguide grating according to claim 1, characterized in that: The thickness of the negative temperature coefficient material is related to the optimum effective refractive index temperature coefficient of the waveguide core layer.