Semiconductor device and method for manufacturing the same

By designing the wider and narrower well regions with alternating distributions in Schottky diodes, the problem of increasing on-resistance of Schottky diodes under high current conditions is solved, and strong inrush current on-resistance and low on-resistance are achieved balance.

CN110581180BActive Publication Date: 2024-11-12WEEN SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201910865839.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-09-12
Publication Date
2024-11-12
Estimated Expiration
2039-09-12

AI Technical Summary

Technical Problem

Under high current conditions, the larger the P-type well area of ​​the existing Schottky diode, the greater the on-resistance, which affects the forward conduction capability of the device.

Method used

A semiconductor device is designed, which includes an alternately distributed wider first well region and a narrower second well region. The wider first well region is opened in advance when conducting inrush current, injects fewer holes and increases drift region The second well region increases the Schottky region through the doping unit distributed intervals to avoid affecting the reverse blocking leakage current capability.

Benefits of technology

It realizes the on-resistance while maintaining the on-resistance of strong inrush current while reducing the on-resistance, ensuring the forward rated current conduction capability and reverse blocking capability of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110581180B_ABST
    Figure CN110581180B_ABST
Patent Text Reader

Abstract

The embodiment of the present invention provides a semiconductor device and a method for manufacturing the same. The semiconductor device provided by the embodiment of the present invention includes a first electrode layer; a substrate layer, located on the first electrode layer; an epitaxial layer, located on the substrate layer and having a first surface away from the substrate layer; a well region, the well region extends from the first surface into the epitaxial layer, the well region includes a first well region and a second well region alternately distributed in a first direction, the second well region includes a plurality of doping units distributed at intervals, and the maximum width of the first well region in the first direction is greater than or equal to the maximum width of the doping unit; a second electrode layer, covering the epitaxial layer and the well region. The semiconductor device provided by the embodiment of the present invention has an excellent forward rated conduction capability and a stronger surge current conduction capability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor device and a manufacturing method thereof. Background Art

[0002] As a semiconductor device structure with a long development history and mature technology, the Schottky diode is an ultra-high-speed semiconductor device that is widely used in the field of energy conversion and is mostly used in high-frequency application environments.

[0003] The current Schottky diodes often use junction barrier Schottky diodes. Under high current conditions (when surge current comes), the PN junction is turned on and minority holes are injected into the drift region of the device, thereby improving the surge current capability of the device. Therefore, the larger the P-type well area, the stronger the surge current capability of the device. However, the larger the P-type well area, the smaller the Schottky area between the P-type well areas of the device under the same area conditions, resulting in a significant increase in the on-resistance of the device in the forward conduction mode.

[0004] Therefore, a new and improved semiconductor device is urgently needed. Summary of the invention

[0005] The embodiments of the present invention provide a semiconductor device and a method for manufacturing the same, which can have excellent forward rated conduction capability and stronger surge current conduction capability.

[0006] In a first aspect, an embodiment of the present invention provides a semiconductor device, including:

[0007] a first electrode layer;

[0008] A substrate layer, located on the first electrode layer;

[0009] an epitaxial layer, located on the substrate layer and having a first surface away from the substrate layer;

[0010] A well region, the well region is extended from the first surface into the epitaxial layer, the well region includes a first well region and a second well region alternately distributed in a first direction, the second well region includes a plurality of doping units distributed at intervals, and a maximum width of the first well region in the first direction is greater than or equal to a maximum width of the doping unit;

[0011] The second electrode layer is arranged to cover the epitaxial layer and the well region.

[0012] According to one aspect of the embodiments of the present invention, the orthographic projection of the first well region on the first surface is a strip, and the orthographic projection of the doping unit on the first surface is a circle or a polygon.

[0013] According to one aspect of an embodiment of the present invention, a plurality of doping units are regularly arranged in the second well region, and one or more columns of doping units are distributed in a second direction perpendicular to the first direction.

[0014] According to one aspect of an embodiment of the present invention, the second electrode layer includes a first metal layer and a second metal layer that are electrically connected, the first metal layer is located on a side of the well region facing away from the substrate layer, and the second metal layer covers the epitaxial layer and the first metal layer;

[0015] An ohmic contact is formed between the first metal layer and the well region, and a Schottky contact is formed between the second metal layer and the epitaxial layer.

[0016] According to one aspect of an embodiment of the present invention, the first metal layer includes a plurality of metal blocks arranged in one-to-one correspondence with the well regions, and the orthographic projections of the metal blocks on the well regions are within the boundary range of the well regions.

[0017] According to one aspect of the embodiment of the present invention, in the first direction, the maximum width of the first well region is 3 μm to 20 μm, and the maximum width of the doping unit is 0.5 μm to 3 μm.

[0018] According to one aspect of the embodiments of the present invention, the substrate layer is of a first conductivity type with a first doping concentration, the epitaxial layer is of the first conductivity type with a second doping concentration, and the well region is of a second conductivity type;

[0019] The first doping concentration is higher than the second doping concentration, the first conductivity type is opposite to the second conductivity type, and the first conductivity type is N type.

[0020] In a second aspect, an embodiment of the present invention provides a method for manufacturing a semiconductor device, the method comprising:

[0021] providing a substrate layer;

[0022] forming an epitaxial layer on the substrate layer;

[0023] A well region is formed on a first surface of the epitaxial layer away from the substrate layer, the well region is extended from the first surface into the epitaxial layer, the well region includes a first well region and a second well region alternately distributed in a first direction, the second well region includes a plurality of doping units distributed at intervals, and a maximum width of the first well region in the first direction is greater than or equal to a maximum width of the doping unit;

[0024] forming a first electrode layer on a side of the substrate layer facing away from the epitaxial layer;

[0025] A second electrode layer is formed on the side of the epitaxial layer and the well region facing away from the substrate layer, and the second electrode layer covers the epitaxial layer and the well region.

[0026] According to one aspect of an embodiment of the present invention, a second electrode layer is formed on a side of the epitaxial layer and the well region facing away from the substrate layer, including:

[0027] Forming a first metal layer on a side of the well region facing away from the substrate layer, the first metal layer comprising a plurality of metal blocks arranged in one-to-one correspondence with the well region, and the orthographic projections of the metal blocks on the well region are within the boundary range of the well region;

[0028] A second metal layer covering the epitaxial layer and the first metal layer is formed, and the second metal layer is electrically connected to the first metal layer to obtain a second electrode layer.

[0029] According to one aspect of an embodiment of the present invention, the step of forming a well region and a first metal layer includes:

[0030] A silicon dioxide film is deposited on a first surface of the epitaxial layer away from the substrate layer, and the silicon dioxide film is patterned;

[0031] Implanting ions of a second conductive type on the patterned silicon dioxide film to obtain a well region;

[0032] forming a carbon film covering the patterned silicon dioxide film and the well region;

[0033] Performing high temperature annealing treatment and removing the carbon film;

[0034] Performing high temperature oxidation treatment to obtain a high temperature oxidized silicon dioxide film, wherein the thickness and width of the high temperature oxidized silicon dioxide film are greater than the thickness and width of the silicon dioxide film before the high temperature oxidation;

[0035] Metal plating is performed on the side of the well region facing away from the substrate layer, and alloy annealing is performed to obtain a first metal layer. The first metal layer includes a plurality of metal blocks arranged in one-to-one correspondence with the well region, and the orthographic projections of the metal blocks on the well region are within the boundary range of the well region.

[0036] According to the semiconductor device provided by the embodiment of the present invention, the first well region and the second well region are alternately distributed in the first direction, the second well region includes a plurality of doping units distributed at intervals, and the maximum width of the first well region in the first direction is greater than the maximum width of the doping unit. On the one hand, the wider first well region can enable the well region PN junction to be opened in advance when conducting surge current, inject minority holes into the high-resistance drift region, and the minority concentration injected and accumulated in the drift region will be very large. In order to maintain the neutral condition of the semiconductor, its majority concentration is also greatly increased accordingly, so that its resistivity is significantly reduced, that is, the conductivity is greatly increased, thereby forming a conductivity modulation effect and improving the surge current conduction capability of the semiconductor device; on the other hand, the second well region includes a plurality of doping units distributed at intervals, which can increase the area of ​​the non-well region (i.e., the Schottky region) relative to the first well region, avoid affecting the ability of the semiconductor device to reversely block leakage current, and ensure the forward rated current conduction capability of the semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Other features, objects and advantages of the present invention will become more apparent from the following detailed description of non-limiting embodiments with reference to the accompanying drawings, in which the same or similar reference numerals represent the same or similar features and the accompanying drawings are not drawn to scale.

[0038] Figure 1 A schematic diagram of a top view of a semiconductor device according to an embodiment of the present invention is shown;

[0039] Figure 2 A schematic diagram of a top view of a semiconductor device according to another embodiment of the present invention is shown;

[0040] Figure 3 A schematic diagram showing a cross-sectional structure of a semiconductor device according to an embodiment of the present invention is shown;

[0041] Figure 4 A schematic flow chart showing a method for manufacturing a semiconductor device according to an embodiment of the present invention;

[0042] FIG. 5A to FIG. 5O A schematic cross-sectional structure diagram showing steps of forming various components included in a semiconductor device in a method for manufacturing a semiconductor device according to an embodiment of the present invention.

[0043] Description of reference numerals:

[0044] 1- first electrode layer;

[0045] 2-substrate layer; 20-terminal structure; 21-silicon dioxide film; 211-silicon dioxide film after high temperature oxidation; 22-second conductive type ions; 23-carbon film; 24-first electrode metal; 25-second electrode metal; 26-passivation layer;

[0046] 3-epitaxial layer; 30-first surface;

[0047] 4-well region; 41-first well region; 42-second well region; 420-doping unit;

[0048] 5-second electrode layer; 51-first metal layer; 52-second metal layer; 510-metal block;

[0049] D1-first direction; D2-second direction. DETAILED DESCRIPTION

[0050] The features and exemplary embodiments of various aspects of the present invention will be described in detail below. In order to make the purpose, technical solutions and advantages of the present invention clearer, the present invention will be further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be understood that the specific embodiments described herein are only configured to explain the present invention and are not configured to limit the present invention. For those skilled in the art, the present invention can be implemented without the need for some of these specific details. The following description of the embodiments is only to provide a better understanding of the present invention by illustrating examples of the present invention.

[0051] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the statement "include..." do not exclude the presence of other identical elements in the process, method, article or device including the elements.

[0052] It should be understood that when describing the structure of a component, when a layer or a region is referred to as being "on" or "over" another layer or another region, it may mean that it is directly on the other layer or another region, or that other layers or regions are included between it and the other layer or another region. Moreover, if the component is turned over, the layer or a region will be "below" or "beneath" another layer or another region.

[0053] The silicon carbide junction barrier Schottky diode is a simple Schottky diode structure with a PN junction structure. When subjected to reverse voltage, the depletion region of the PN structure will expand and protect the Schottky metal between the PN junctions. The electric field borne by the Schottky metal is greatly reduced, thereby significantly reducing the reverse leakage current.

[0054] The turn-on voltage of the silicon carbide PN structure is generally around 2.6V. To ensure that the PN structure is turned on, the potential difference above and below the PN junction must be greater than 2.6V. The potential difference below the PN junction mainly comes from the lateral flow of current. The applicant found that the potential difference above and below the center of the PN structure will reach 2.6V the earliest. The wider the PN structure, the earlier the PN junction turns on. However, the wider the PN structure, the smaller the area of ​​the Schottky part between the PN junctions, which will cause the on-resistance of the semiconductor device to increase significantly in the forward rated conduction mode.

[0055] In order to solve the problems of the prior art, the semiconductor device provided by the present invention includes a certain number of wider PN junctions to ensure that minority carrier injection starts earlier, and also includes a large number of narrower PN junctions to ensure the area of ​​the Schottky part. The structure of the semiconductor device provided by the present invention is described in detail below.

[0056] Figure 1 The figure is a schematic top view of the structure of a semiconductor device according to an embodiment of the present invention. Figure 2 FIG. 4 is a schematic top view of a semiconductor device according to another embodiment of the present invention. Figure 3 FIG. 1 is a schematic cross-sectional view of a semiconductor device according to an embodiment of the present invention. Figures 1 to 3 The semiconductor device of the embodiment of the present invention comprises a first electrode layer 1, a substrate layer 2, an epitaxial layer 3, a well region 4 and a second electrode layer 5. It should be understood that Figure 1 and Figure 2 Only a schematic diagram of a top view of a part of the semiconductor device is shown, which can be formed by designing and drawing a photolithography mask with corresponding shape features. Figure 1 Or the layout structure of the well region 4 shown in 2. Figure 3 Only a schematic diagram of the cross-sectional structure of a partial region of the semiconductor device is shown.

[0057] The semiconductor device according to the embodiment of the present invention may be a semiconductor device such as silicon carbide, silicon, gallium nitride, gallium oxide, diamond, etc. Preferably, the semiconductor device according to the embodiment of the present invention is a silicon carbide semiconductor device. The shape of the semiconductor device may be square, rectangular, circular, irregular, etc., and the present invention is not limited thereto.

[0058] The first electrode layer 1 serves as a cathode of the semiconductor device. The first electrode layer 1 may be a metal layer, and the metal may be gold, silver, copper, etc. or a combination thereof.

[0059] The substrate layer 2 is located on the first electrode layer 1. In one embodiment, an ohmic contact is formed between the first electrode layer 1 and the substrate layer 2. The substrate layer 2 is of a first conductivity type with a first doping concentration.

[0060] The epitaxial layer 3 is located on the substrate layer 2 and has a first surface 30 away from the substrate layer 2. The epitaxial layer 3 is a first conductivity type with a second doping concentration. In some optional embodiments, the first conductivity type is N-type, and the substrate layer 2 and the epitaxial layer 3 are both N-type semiconductors. There are a large number of electrons in the N-type semiconductor, and the electrons have a higher mobility, so they have a stronger current conduction capability. In some optional embodiments, the first doping concentration is higher than the second doping concentration, for example, the substrate layer 2 is a heavily doped N-type semiconductor, and the epitaxial layer 3 is a lightly doped N-type semiconductor.

[0061] The well region 4 is extended from the first surface 30 of the epitaxial layer 3 into the epitaxial layer 3. In one embodiment, the well region 4 is formed in the epitaxial layer 3 and at least a portion of the well region 4 overlaps with the first surface 30 of the epitaxial layer 3. The epitaxial layer 3 may have a plurality of well regions 4, and the well regions 4 are of the second conductivity type. In some optional embodiments, the first conductivity type is opposite to the second conductivity type, that is, the well region 4 is of P type.

[0062] The well region 4 includes a first well region 41 and a second well region 42 alternately distributed in a first direction D1, the second well region 42 includes a plurality of doping units 420 distributed at intervals, and the maximum width of the first well region 41 in the first direction is greater than or equal to the maximum width of the doping unit 420 in the first direction. Exemplarily, the maximum width of the first well region 41 is 3 μm to 20 μm, and the maximum width of the doping unit 420 is 0.5 μm to 3 μm, and the widths of the first well region 41 and the doping unit 420 can be set according to actual needs. Exemplarily, the first direction D1 can be understood as the width direction of the first well region 41, and the second direction D2 can be understood as the length direction of the first well region 41.

[0063] The second electrode layer 5 covers the epitaxial layer 3 and the well region 4. The second electrode layer 5 serves as an anode of the semiconductor device. The first metal layer 51 can be a metal layer of gold, silver, copper, etc. or a combination thereof. The second electrode layer 5 forms an ohmic contact with the well region 4, and the second electrode layer 5 forms a Schottky contact with the epitaxial layer 3 around the well region 4.

[0064] According to the semiconductor device provided by the embodiment of the present invention, the first well region 41 and the second well region 42 are alternately distributed in the first direction D1, the second well region 42 includes a plurality of doping units 420 distributed at intervals, and the maximum width of the first well region 41 in the first direction D1 is greater than the maximum width of the doping unit 420. On the one hand, the wider first well region 41 can enable the well region PN junction to be opened in advance when conducting surge current, inject minority holes into the high-resistance drift region, and the minority concentration injected and accumulated in the drift region will be very large. In order to maintain the neutral condition of the semiconductor, its majority carrier concentration is also greatly increased accordingly, so that its resistivity is significantly reduced, that is, the conductivity is greatly increased, thereby forming a conductivity modulation effect and improving the surge current conduction capability of the semiconductor device; on the other hand, the second well region 42 includes a plurality of doping units 420 distributed at intervals, which can increase the area of ​​the non-well region (i.e., Schottky region) relative to the first well region 41, avoid affecting the reverse blocking leakage current capability of the semiconductor device, and ensure the forward rated current conduction capability of the semiconductor device.

[0065] In some optional embodiments, the orthographic projection of the first well region 41 on the first surface 30 is a strip, and the orthographic projection of the doping unit 420 on the first surface 30 is a circle or a polygon. Figure 1, the orthographic projection of the first well region 41 is a continuous long strip, and the orthographic projection of the doping unit 420 is a circle, or, please refer to Figure 2 , the orthographic projection of the first well region 41 is a continuous long strip, the orthographic projection of the doping unit 420 is a regular hexagon, and the orthographic projection of the exemplary doping unit 420 on the first surface 30 may also be a regular octagon, a regular decagon, an irregular polygon, etc. The strip-shaped first well region 41 can ensure that the wider first well region 41 enters the minority carrier injection mode at the same time, and the circular or polygonal doping units 420 are distributed at intervals to form the second well region 42, which can increase the area ratio of the non-well region (i.e., the Schottky region), avoid affecting the reverse blocking leakage current capability of the semiconductor device, and ensure the forward rated current conduction capability and reverse blocking capability of the semiconductor device.

[0066] In some optional embodiments, the plurality of doping units 420 are regularly arranged in the second well region 42, and one or more columns of doping units 420 are distributed in the second direction D2 perpendicular to the first direction D1. Figure 1 or Figure 2 , in the second direction D2, there are three columns of doping units 420. It can be understood that, in the second direction D2, the more columns of doping units 420 are distributed, or the larger the spacing between the doping units 420 is, the larger the area proportion of the Schottky region will be. The number of columns of the doping units 420 and the spacing between the doping units 420 can be set according to actual needs, and the present invention is not limited to this.

[0067] For some optional implementations, please continue to refer to Figure 3 The second electrode layer 5 includes an electrically connected first metal layer 51 and a second metal layer 52, the first metal layer 51 is located on the side of the well region 4 facing away from the substrate layer 2, and the second metal layer 52 covers the epitaxial layer 3 and the first metal layer 51; an ohmic contact is formed between the first metal layer 51 and the well region 4, and a Schottky contact is formed between the second metal layer 52 and the epitaxial layer 3. Exemplarily, the first metal layer 51 and the second metal layer 52 can be metal layers of gold, silver, copper, etc. or a combination thereof.

[0068] In some optional embodiments, the first metal layer 51 includes a plurality of metal blocks 510 arranged in one-to-one correspondence with the well region 4, and the orthographic projection of the metal block 510 on the well region 4 is within the boundary of the well region 4. The boundary of the metal block 510 is smaller than the boundary of the well region 4, ensuring that the metal block 510 forming an ohmic contact with the well region 4 is completely within the well region 4, avoiding the risk of short circuit.

[0069] It is understandable that, according to the semiconductor device of the embodiment of the present invention, the terminal structure 20 and the passivation layer 26 may also be provided at the edge of the semiconductor device. For example, see Figure 3The terminal structure 20 is located on the side of the epitaxial layer 3 facing away from the substrate layer 2 , and the passivation layer 26 is located on the side of the terminal structure 20 facing away from the epitaxial layer 3 .

[0070] Figure 4 FIG. 1 is a flow chart showing a method for manufacturing a semiconductor device according to an embodiment of the present invention. Figure 4 As shown, the semiconductor device manufacturing method provided by the embodiment of the present invention includes:

[0071] S110, providing a substrate layer 2;

[0072] S120, forming an epitaxial layer 3 on the substrate layer 2;

[0073] S130, forming a well region 4 on a first surface 30 of the epitaxial layer 3 away from the substrate layer 2, the well region 4 extending from the first surface 30 into the epitaxial layer 3, the well region 4 including a first well region 41 and a second well region 42 alternately distributed in a first direction, the second well region 42 including a plurality of doping units 420 distributed at intervals, and a maximum width of the first well region 41 in the first direction being greater than or equal to a maximum width of the doping unit 420;

[0074] S140, forming a first electrode layer 1 on a side of the substrate layer 2 facing away from the epitaxial layer 3;

[0075] S150 , forming a second electrode layer 5 on a side of the epitaxial layer 3 and the well region 4 facing away from the substrate layer 2 , wherein the second electrode layer 5 covers the epitaxial layer 3 and the well region 4 .

[0076] According to the semiconductor device provided by the embodiment of the present invention, the first well region 41 and the second well region 42 are alternately distributed in the first direction, the second well region 42 includes a plurality of doping units 420 distributed at intervals, and the maximum width of the first well region 41 in the first direction is greater than the maximum width of the doping unit 420. On the one hand, the wider first well region 41 can enable the well region PN junction to be opened in advance when conducting surge current, inject minority holes into the high-resistance drift region, and the minority concentration injected and accumulated in the drift region will be very large. In order to maintain the neutral condition of the semiconductor, its majority carrier concentration is also greatly increased accordingly, so that its resistivity is significantly reduced, that is, the conductivity is greatly increased, thereby forming a conductivity modulation effect and improving the surge current conduction capability of the semiconductor device; on the other hand, the second well region 42 includes a plurality of doping units 420 distributed at intervals, which can increase the area of ​​the non-well region (i.e., the Schottky region) relative to the first well region 41, avoid affecting the reverse blocking leakage current capability of the semiconductor device, and ensure the forward rated current conduction capability of the semiconductor device.

[0077] In some optional embodiments, the first electrode layer 1 and the second electrode layer 5 may be formed simultaneously.

[0078] In some optional embodiments, the step of forming the second electrode layer 5 includes:

[0079] A first metal layer 51 is formed on the side of the well region 4 facing away from the substrate layer 2. The first metal layer 51 includes a plurality of metal blocks 510 arranged one-to-one corresponding to the well region 4. The orthographic projections of the metal blocks 510 on the well region 4 are within the boundary range of the well region 4.

[0080] A second metal layer 52 is formed to cover the epitaxial layer 3 and the first metal layer 51 . The second metal layer 52 is electrically connected to the first metal layer 51 to obtain a second electrode layer 5 .

[0081] The orthographic projection of the metal block 510 on the well region 4 is within the boundary of the well region 4 to avoid short circuit.

[0082] In some optional implementations, the steps of forming the well region 4 and the first metal layer 51 include:

[0083] A silicon dioxide film 21 is deposited on a first surface 30 of the epitaxial layer 3 away from the substrate layer 2, and the silicon dioxide film 21 is patterned;

[0084] Implanting ions 22 of the second conductivity type on the patterned silicon dioxide film 21 to obtain a well region 4;

[0085] forming a carbon film 23 covering the patterned silicon dioxide film 21 and the well region 4;

[0086] Performing high temperature annealing treatment and removing the carbon film 23;

[0087] Performing high temperature oxidation treatment to obtain a high temperature oxidized silicon dioxide film 211, wherein the thickness and width of the high temperature oxidized silicon dioxide film 211 are greater than the thickness and width of the silicon dioxide film 21 before the high temperature oxidation;

[0088] Metal plating is performed on the side of the well region 4 facing away from the substrate layer 2, and alloy annealing is performed to obtain a first metal layer 51. The first metal layer 51 includes a plurality of metal blocks 510 arranged in a one-to-one correspondence with the well region 4. The orthographic projection of the metal block 510 on the well region 4 is within the boundary range of the well region 4.

[0089] After high-temperature oxidation, the silicon dioxide film 21 used as an ion implantation mask is used to continue to define the boundary of the ohmic contact electrode (i.e., the metal block 510). Since silicon dioxide will become wider and thicker after oxidation, the ohmic contact boundary defined by it will be smaller than the boundary of the well region 4 previously defined by it, ensuring that the metal block 510 that forms an ohmic contact with the well region 4 is completely within the well region 4, avoiding the risk of subsequent short circuits. This step can save the additional photolithography process required in the traditional process, saving production costs. At the same time, the new process flow can break through the process limit of the photolithography machine, and the ohmic contact electrode (i.e., the metal block 510) can be formed on the doping unit 420 even with a width of about 1 micron.

[0090] In a specific embodiment, the semiconductor device manufacturing method of the embodiment of the present invention comprises the steps of:

[0091] Provide as Figure 5A The initial silicon carbide semiconductor material shown has a heavily doped N-type substrate layer 2 and a lightly doped N-type epitaxial layer 3;

[0092] By patterning the mask and implanting a low dose of second conductive type ions, a Figure 5B The terminal structure 20 of the silicon carbide device is shown;

[0093] The chemical vapor deposition method forms Figure 5C The silicon dioxide film 21 is shown;

[0094] The silicon dioxide film 21 is patterned using photolithography and etching techniques to obtain Figure 5D The silicon dioxide film 21 after patterning is shown;

[0095] like Figure 5E As shown, a certain dose of the second conductive type ions 22 is injected to obtain Fig. 5F The well region 4 is shown;

[0096] like Figure 5G As shown, a carbon film 23 of a certain thickness is deposited;

[0097] Perform high temperature annealing to activate the implanted second conductive type ions 22. For example, the annealing temperature is 1500° C. to 1600° C.;

[0098] like Figure 5H As shown, the high temperature annealing protection carbon film 23 is removed by plasma ashing;

[0099] A high temperature oxidation process is performed, and the previous silicon dioxide film (21) becomes wider and thicker after oxidation, and the obtained Fig.5I The silicon dioxide film 211 after high temperature oxidation is shown;

[0100] Using a relatively short dry etching or wet etching process to remove the thin silicon dioxide film formed on the exposed silicon carbide surface;

[0101] like Figure 5J As shown, a second electrode metal 25 capable of forming an ohmic contact is deposited on the first surface 30 of the epitaxial layer 3, and a first electrode metal 24 capable of forming an ohmic contact is also deposited on the surface of the substrate layer 2 facing away from the epitaxial layer 3, thereby obtaining a first electrode layer 1 as a cathode;

[0102] The alloy is annealed at a certain temperature to remove the remaining ohmic metal that has not formed an alloy, forming a Figure 5K A plurality of metal blocks 510 are shown in ohmic contact with the well region 4 , and the plurality of metal blocks 510 constitute a first metal layer 51 ;

[0103] like Figure 5L As shown, the silicon dioxide film 211 after high temperature oxidation is removed;

[0104] like Figure 5M As shown, a pad passivation layer 26 is deposited;

[0105] like Figure 5N As shown, the passivation layer 26 is patterned by photolithography and etching techniques; and a metal pad is deposited to form a Schottky contact with the non-well region;

[0106] like Fig.5O As shown, the Schottky metal is patterned by photolithography and etching process, and the alloy is annealed to form the second metal layer 52 of Schottky contact. Thus, the first metal layer 51 and the second metal layer 52 obtained constitute the second electrode layer 5 as the anode;

[0107] Furthermore, conventional front and back metal thickening processes may be performed.

[0108] It should be noted that, in this article, the sequence of process steps is only used as an example to illustrate this embodiment. According to cost control and different manufacturing process capabilities, the sequence can be appropriately adjusted without affecting the implementation effect of the embodiment of the present invention. This is also obvious to those skilled in the art.

[0109] It should be understood that the description of the specific embodiments of the present invention is exemplary and should not be interpreted as an improper limitation on the scope of protection of the present invention. The scope of protection of the present invention is defined by its claims and covers all embodiments and obvious equivalent variations falling within its scope.

Claims

1. A method for manufacturing a semiconductor device, characterized in that: The method comprises: Providing a substrate layer (2); forming an epitaxial layer (3) on the substrate layer (2); A well region (4) is formed on a first surface (30) of the epitaxial layer (3) away from the substrate layer (2), the well region (4) extending from the first surface (30) into the epitaxial layer (3), the well region (4) comprising a first well region (41) and a second well region (42) alternately distributed in a first direction, the second well region (42) comprising a plurality of doping units (420) distributed at intervals, the maximum width of the first well region (41) in the first direction being greater than or equal to the maximum width of the doping unit (420), a plurality of doping units (420) being distributed between two adjacent first well regions (41) in the first direction, and a plurality of doping units (420) being arranged in a second direction, the first direction and the second direction intersecting; forming a first electrode layer (1) on a side of the substrate layer (2) facing away from the epitaxial layer (3); forming a second electrode layer (5) on a side of the epitaxial layer (3) and the well region (4) facing away from the substrate layer (2), wherein the second electrode layer (5) covers the epitaxial layer (3) and the well region (4); The second electrode layer (5) is formed on a side of the epitaxial layer (3) and the well region (4) facing away from the substrate layer (2), comprising: A first metal layer (51) is formed on a side of the well region (4) facing away from the substrate layer (2), the first metal layer (51) comprising a plurality of metal blocks (510) arranged in one-to-one correspondence with the well region (4), and the orthographic projections of the metal blocks (510) on the well region (4) are within the boundary range of the well region (4); forming a second metal layer (52) covering the epitaxial layer (3) and the first metal layer (51), wherein the second metal layer (52) is electrically connected to the first metal layer (51) to obtain the second electrode layer (5); The steps of forming the well region (4) and the first metal layer (51) include: A silicon dioxide film (21) is deposited on a first surface (30) of the epitaxial layer (3) away from the substrate layer (2), and the silicon dioxide film (21) is patterned; Implanting second conductive type ions (22) above the patterned silicon dioxide film (21) to obtain the well region (4); forming a carbon film (23) covering the patterned silicon dioxide film (21) and the well region (4); Performing high temperature annealing treatment and removing the carbon film (23); Performing high temperature oxidation treatment to obtain a high temperature oxidized silicon dioxide film (211), wherein the thickness and width of the high temperature oxidized silicon dioxide film (211) are greater than the thickness and width of the silicon dioxide film (21) before the high temperature oxidation; Metal plating is performed on a side of the well region (4) facing away from the substrate layer (2), and alloy annealing is performed to obtain the first metal layer (51), wherein the first metal layer (51) comprises a plurality of metal blocks (510) arranged in one-to-one correspondence with the well region (4), and the orthographic projections of the metal blocks (510) on the well region (4) are within the boundary range of the well region (4).