Combined metal-ceramic composite integrated coal mill dynamic and static ring and preparation method

By using a combined metal-ceramic composite integrated dynamic and static ring design, the wear problem of the dynamic and static rings in medium-speed coal mills has been solved, achieving the effect of simplifying maintenance and reducing maintenance costs.

CN110773277BActive Publication Date: 2024-11-12ANHUI TONGCHUANG ELECTRIC POWER SCI & TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201911199921.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-11-29
Publication Date
2024-11-12
Estimated Expiration
2039-11-29

AI Technical Summary

Technical Problem

The dynamic and static rings of medium-speed coal mills are prone to severe wear due to wind erosion and impurity erosion during operation, which leads to increased operating costs, long maintenance periods, and high and complex maintenance costs.

Method used

The design adopts a combined metal-ceramic composite integrated dynamic and static ring design. The outer side of the dynamic ring is equipped with wear-resistant zirconia ceramic separation teeth. A wear-resistant composite layer is formed through casting and heat treatment. The segmented design of the dynamic and static rings facilitates partial replacement and avoids the need for complete replacement.

Benefits of technology

It simplifies the maintenance process of medium-speed coal mills, reduces maintenance costs and time, extends the service life of dynamic and static rings, and improves the operating efficiency of the equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110773277B_ABST
    Figure CN110773277B_ABST
Patent Text Reader

Abstract

The present invention discloses a combined metal-ceramic composite integrated coal mill dynamic and static ring and a preparation method, which relates to the technical field of coal mill devices, and mainly includes a static ring installed on a casing bracket and a dynamic ring installed on a grinding disc; the static ring includes a plurality of arc-shaped static ring segments with the same structure, and the plurality of static ring segments are connected end to end in sequence to form a circular ring; the dynamic ring includes a plurality of arc-shaped dynamic ring segments with the same structure, and the plurality of dynamic ring segments are connected end to end in sequence to form a circular ring; a plurality of dynamic ring separation teeth are evenly arranged on the outer side of the dynamic ring. The dynamic and static rings made by the combined metal-ceramic composite integrated coal mill dynamic and static ring preparation method provided by the present invention can simplify the maintenance of the dynamic and static rings of a medium-speed coal mill and reduce maintenance costs.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of coal mill devices, and in particular to a combined metal-ceramic composite integrated coal mill dynamic and static ring and a preparation method thereof. Background Art

[0002] Medium-speed coal mill refers to a coal mill with a working speed of 50 to 300 r / min. The motor drives the grinding disc to rotate through the reducer. The material falls from the feed port to the center of the grinding disc through the air lock feeder, and the hot air enters the mill from the air inlet. As the grinding disc rotates, the material moves to the edge of the grinding disc under the action of centrifugal force, and is crushed by the grinding roller when passing through the annular groove on the grinding disc. The crushed material is blown up by the primary wind that enters the surroundings of the grinding ring through the moving ring at the edge of the grinding disc. Large particles fall directly on the grinding disc and are crushed again. When the material in the air flow passes through the upper separator, the coarse powder falls from the cone bucket to the grinding disc for re-grinding under the action of the rotating rotor. The qualified fine powder is discharged from the mill with the air flow and collected by the dust collection device, which is the product.

[0003] The static ring of the medium-speed coal mill is installed on the housing bracket, and the moving ring of the grinding disc is connected to the grinding disc and rotates together. There is a certain gap between the moving and static rings of the grinding disc. The hot air used to transport coal powder and dry raw coal, namely the primary air, enters the grinding ring evenly through the moving ring, dries the coal powder mixture thrown out from the grinding ring in the circumferential direction and transports it to the separator for separation. The coarse powder is separated and returned to the grinding ring for re-grinding. The qualified grinding powder is brought to the furnace by the primary air. The impurities such as stone coal, iron blocks, etc. that are difficult to crush and heavier fall back to the primary air chamber through the moving ring and are discharged to the slag box through the scraper.

[0004] After a medium-speed coal mill has been in operation for a period of time, it is often subject to severe wear of the dynamic and static rings due to wind erosion, erosion by impurities such as stone coal and iron blocks, especially at the nozzle throat of the dynamic ring and the upper part of the static ring. Sometimes, the static ring may even be worn through, resulting in primary air leakage in the coal mill, which in turn increases the amount of stone coal in the coal mill, reduces output, increases power consumption, and increases the operating cost of the coal mill. At present, coal mills generally use integral dynamic and static rings, and the wear of the dynamic and static rings is often uneven. Integral dynamic and static rings often cause the dynamic ring or static ring to fail due to severe wear in one part. Since integral dynamic and static rings are used, the most commonly used measure after failure is replacement. This brings about the following defects: (1) When replacing, it is necessary to first remove the separator, then remove the hydraulic device, press frame, grinding roller device, grinding disc, etc. according to the coal mill maintenance process, and then replace the dynamic and static rings. Therefore, the equipment maintenance period is very long. (2) The replacement of the dynamic and static rings causes a long downtime (the coal mill needs to be shut down and cannot be produced when the rollers are repaired and replaced), which affects production. (3) The replacement of the entire dynamic ring or static ring due to local wear and failure of the dynamic and static rings results in high equipment maintenance costs, heavy workload, and complex maintenance procedures. Summary of the invention

[0005] The purpose of the present invention is to provide a combined metal-ceramic composite integrated coal mill dynamic and static ring and a preparation method to solve the problems existing in the above-mentioned prior art, simplify the maintenance of the dynamic and static rings of the medium-speed coal mill, and reduce the maintenance cost.

[0006] To achieve the above object, the present invention provides the following solutions:

[0007] The present invention provides a combined metal-ceramic composite integrated coal mill dynamic and static ring, comprising a static ring installed on a casing bracket and a dynamic ring installed on a grinding disc; the static ring comprises a plurality of arc-shaped static ring segments with the same structure, and the plurality of static ring segments are connected end to end in sequence to form a circular ring; the dynamic ring comprises a plurality of arc-shaped dynamic ring segments with the same structure, and the plurality of dynamic ring segments are connected end to end in sequence to form a circular ring; a plurality of dynamic ring separation teeth are evenly arranged on the outer side of the dynamic ring.

[0008] Optionally, the stationary ring segment includes an integrally formed transverse plate and a vertical plate, the connection between the transverse plate and the vertical plate is a smooth arc structure, an extension plate is connected to the outer side of the transverse plate, and a mounting hole is formed on the transverse plate.

[0009] Optionally, a wedge-shaped reinforcement block is connected between the horizontal plate and the vertical plate.

[0010] Optionally, the cross-section of the moving ring segment is an L-shaped structure, the moving ring separation teeth are arranged on the outer side of the long side of the moving ring segment, and a connecting hole is opened on the short side of the moving ring segment.

[0011] Optionally, the dynamic ring separation tooth includes an integrally formed structure with a water droplet-shaped cross section and a triangular structure with a cross section, and the triangular structure is located on one side of the tip of the water droplet-shaped structure.

[0012] The present invention also provides a method for preparing a combined metal-ceramic composite integrated coal mill moving and stationary rings, comprising the following steps:

[0013] Step 1: Cast the required number of stationary ring segments respectively, and machine them respectively after casting; fix the stationary ring segments to the casing bracket in sequence, forming a stationary ring;

[0014] Step 2: Mix the zirconium oxide ceramic powder and the viscose solution and granulate them to obtain zirconium oxide ceramic particles;

[0015] Step three: Place the zirconium oxide ceramic particles in a cross-shaped aluminum can for drying and forming to obtain a zirconium oxide ceramic-aluminum can molded body, the drying and forming temperature is 80 to 120°C, and the drying time is 3 to 5 hours;

[0016] Step 4: Place multiple zirconia ceramic-aluminum can molded bodies in the casting mold cavity, and install overflow protection covers around them, and cast them in one go to obtain metal-ceramic composite integrated coal mill dynamic ring segments, and fix multiple dynamic ring segments to the grinding disc in sequence to form a dynamic ring.

[0017] Compared with the prior art, the present invention has achieved the following technical effects:

[0018] The characteristics of the dynamic ring separation teeth of the present invention are small surface area and relatively thin thickness. During the casting process, the temperature drop rate of the molten steel of the grinding roller is increased by 40% compared with that in the original patent, so it is more difficult to form. Therefore, in the forming process of the metal ceramic dynamic ring separation teeth, a unique M-shaped preform is designed according to its structural characteristics, so that the ceramic particles can be quickly and evenly diffused at a moderate temperature (and the cylindrical ceramic preform is generally suitable for the preparation of large-area composite layers with a thickness of more than 25 mm). An overflow shield is installed at the edge of the separation teeth to be formed. It is more appropriate to select heat-resistant steel for the overflow shield, and the pore size is smaller than the ceramic ball particle size. In this way, during pouring, the ceramic powder is effectively prevented from flowing to other parts. After pouring, the overflow shield is fused with the separation teeth and does not affect the overall performance of the dynamic ring. According to the shape of the dynamic ring separation teeth, the overflow shield adopts a butterfly-shaped overflow shield.

[0019] During pouring, the aluminum can (melting point is about 660°C) in the zirconia ceramic-aluminum can molded body melts first, the zirconia ceramic particles burst, and the released zirconia ceramic powder is fully mixed with the molten metal to form a wear-resistant composite layer on the outer surface of the dynamic ring matrix. Among them, by adopting a multi-sprue and U-shaped runner (where the pouring cup and runner size are determined according to the size of the casting to control the flow rate of the molten metal) pouring method and controlling the pouring temperature (casting material Cr20, pouring temperature is about 1350°C), the flow rate of the molten metal is limited to 40-60mm / min, which is conducive to the formation of a uniform wear-resistant composite layer, avoiding the problem of uneven distribution of zirconia ceramic powder in the wear-resistant composite layer caused by the erosion of the molten metal, and improving the wear resistance of the dynamic ring separation teeth. The wear-resistant layer after molding of the present invention is located on the surface of the protrusion outside the dynamic ring, with a thickness of 12-15mm. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0021] Figure 1 It is a schematic diagram of the structure of the static ring segment of the present invention;

[0022] Figure 2 It is a cross-sectional view of the stationary ring section at AA of the present invention;

[0023] Figure 3 It is a cross-sectional view of the stationary ring section BB of the present invention;

[0024] Figure 4 It is a partial enlarged view of the stationary ring section C of the present invention;

[0025] Figure 5 It is a schematic diagram of the structure of the dynamic ring segment of the present invention;

[0026] Figure 6 It is a cross-sectional view of the dynamic ring segment AA of the present invention;

[0027] Figure 7 It is a cross-sectional view of the dynamic ring segment BB of the present invention;

[0028] Figure 8 It is a partially enlarged schematic diagram of the dynamic ring separation tooth structure of the dynamic ring segment of the present invention;

[0029] Among them, 1 is the static ring segment, 101 is the horizontal plate, 102 is the vertical plate, 103 is the extension plate, 104 is the mounting hole, 105 is the reinforcement block, 2 is the dynamic ring segment, 201 is the connecting hole, and 3 is the dynamic ring separation tooth. DETAILED DESCRIPTION

[0030] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0031] The purpose of the present invention is to provide a combined metal-ceramic composite integrated coal mill dynamic and static ring and a preparation method to solve the problems existing in the above-mentioned prior art, simplify the maintenance of the dynamic and static rings of the medium-speed coal mill, and reduce the maintenance cost.

[0032] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.

[0033] The present invention provides a combined metal-ceramic composite integrated coal mill dynamic and static ring, such as Figure 1-Figure 8As shown, it includes a stationary ring installed on the housing bracket and a dynamic ring installed on the grinding disc; the stationary ring includes a plurality of arc-shaped stationary ring segments 1 with the same structure, and the plurality of stationary ring segments 1 are connected end to end in sequence to form a circular ring-shaped stationary ring; the dynamic ring includes a plurality of arc-shaped dynamic ring segments 2 with the same structure, and the plurality of dynamic ring segments 2 are connected end to end in sequence to form a circular ring-shaped dynamic ring; a plurality of dynamic ring separation teeth 3 are evenly arranged on the outer side of the dynamic ring. The stationary ring segment 1 includes an integrally formed horizontal plate 101 and a vertical plate 102, and the connection between the horizontal plate 101 and the vertical plate 102 is a smooth arc structure, and an extension plate 103 is connected to the outer side of the horizontal plate 101, and a mounting hole 104 is opened on the horizontal plate 101, and a wedge-shaped reinforcement block 105 is connected between the horizontal plate 101 and the vertical plate 102.

[0034] The cross section of the moving ring segment 2 is an L-shaped structure, the moving ring separation tooth 3 is arranged outside the long side of the moving ring segment 2, and a connecting hole 201 is opened on the short side of the moving ring segment. The moving ring separation tooth 3 includes an integrally formed head and tail, the cross section of the head is a water drop-shaped structure, and the cross section of the tail is a triangular structure, and the triangular structure is located on the tip side of the water drop-shaped structure.

[0035] The present invention also provides a method for preparing a combined metal-ceramic composite integrated coal mill moving and stationary rings, comprising the following steps:

[0036] Step 1: Cast the required number of stationary ring segments respectively, and machine them respectively after casting; fix the stationary ring segments 1 to the casing bracket in sequence, forming a stationary ring;

[0037] Step 2: For the movable ring separation tooth 3 which is easy to wear, a metal-ceramic composite material is used to improve its wear resistance, and the zirconium oxide ceramic powder is mixed with the viscose liquid and granulated to obtain zirconium oxide ceramic particles;

[0038] Step three: Place the zirconium oxide ceramic particles in a cross-shaped aluminum can for drying and forming to obtain a zirconium oxide ceramic-aluminum can formed body. The drying and forming temperature is 80-120°C and the drying time is 3-5 hours. During the drying and forming process, the solvent in the viscose liquid evaporates to form spheres with a particle size of 0.2-0.3 mm.

[0039] Step 4: Place multiple zirconia ceramic-aluminum can molded bodies in the casting mold cavity, and place an overflow cover around it, cast and mold it in one go, and obtain a metal-ceramic composite integrated coal mill dynamic ring segment 2, and fix multiple dynamic ring segments 2 to the grinding disc in sequence to form a dynamic ring. After heat treatment, the matrix hardness is 57HRC, which has good wear resistance. The medium-speed coal mill dynamic ring with separation teeth cast using metal-ceramic composite materials can have a service life of more than 30,000 hours, and the service life of the dynamic ring cast with Cr20 is generally about 10,000 hours.

[0040] The present invention uses metal ceramics to prepare the easily worn parts of the dynamic ring and the dynamic ring separation teeth, which effectively prolongs the service life of the dynamic and static rings. The combined design of the dynamic and static rings only requires the replacement of the worn and failed parts during maintenance and replacement, without the need to replace the entire ring. It is also unnecessary to remove other parts of the coal mill during replacement, which is convenient for maintenance, short maintenance time and low maintenance cost. The present invention adopts one-time casting, which saves procedures compared to the secondary casting process of the grinding roller disclosed in the original patent.

[0041] Example 1: The segmented ZGM95G medium-speed coal mill static ring is cast with a material of Cr20 and is cast in 6 segments at a casting temperature of 1400°C. It is assembled and used after forced air cooling and heat treatment, and the effect is good.

[0042] Example 2: The moving ring of ZGM95G medium-speed coal mill is prepared by metal-ceramic integration. The moving ring separation tooth part is cast in one step using a metal-ceramic composite material (the metal matrix material is Cr20, and the reinforcing ceramic is zirconium oxide ceramic powder), and the other parts are cast using high-chromium cast iron Cr20. It is cast in 6 sections with a casting temperature of 1340°C. It is assembled and used after forced air cooling and heat treatment. It has good wear resistance and a service life of 30200 hours. It is easy to replace local damage.

Claims

1. A method for preparing a combined metal-ceramic composite integrated coal mill dynamic and static ring, characterized in that: The structure of the combined metal-ceramic composite integrated coal mill dynamic and static rings comprises a static ring mounted on a casing bracket and a dynamic ring mounted on a grinding disc; the static ring comprises a plurality of arc-shaped static ring segments of the same structure, and the plurality of static ring segments are connected end to end in sequence to form a circular ring; the dynamic ring comprises a plurality of arc-shaped dynamic ring segments of the same structure, and the plurality of dynamic ring segments are connected end to end in sequence to form a circular ring; a plurality of dynamic ring separation teeth are evenly arranged on the outer side of the dynamic ring; the static ring segment comprises an integrally formed horizontal plate and a vertical plate, the connection between the horizontal plate and the vertical plate is a smooth arc structure, the outer side of the horizontal plate is connected to an extension plate, and a mounting hole is provided on the horizontal plate; the cross-section of the dynamic ring segment is an L-shaped structure, the dynamic ring separation teeth are arranged on the outer side of the long side of the dynamic ring segment, and a connecting hole is provided on the short side of the dynamic ring segment; the preparation method comprises the following steps: Step 1: Cast the required number of stationary ring segments respectively, and machine them respectively after casting; fix the stationary ring segments to the casing bracket in sequence, forming a stationary ring; Step 2: Mix the zirconium oxide ceramic powder and the viscose solution and granulate them to obtain zirconium oxide ceramic particles; Step three: Place the zirconium oxide ceramic particles in a cross-shaped aluminum can for drying and forming to obtain a zirconium oxide ceramic-aluminum can molded body, the drying and forming temperature is 80~120°C, and the drying time is 3~5h; Step 4: Place multiple zirconia ceramic-aluminum can molded bodies in the casting mold cavity, and install overflow protection covers around them, and cast them in one go to obtain metal-ceramic composite integrated coal mill dynamic ring segments, and fix the multiple dynamic ring segments to the grinding disc in sequence to form a dynamic ring.

2. The method for preparing the combined metal-ceramic composite integrated coal mill moving and stationary rings according to claim 1, characterized in that: A wedge-shaped reinforcement block is connected between the transverse plate and the vertical plate.

3. The method for preparing the combined metal-ceramic composite integrated coal mill dynamic and static rings according to claim 1, characterized in that: The dynamic ring separation tooth includes an integrally formed structure with a water droplet-shaped cross section and a triangular structure with a cross section, and the triangular structure is located on one side of the tip of the water droplet-shaped structure.