Forming dies for the manufacture of iron or nickel-based toroidal cores

By designing a shaped mold for iron-based or nickel-based annular magnetic core, the combined structure of the outer frame and inner frame molds reserves the loss width, the problem of dimensional control of the core during soaking and baking is solved, and high-precision The finished magnetic core product meets the client's requirements for accuracy.

CN112117117BActive Publication Date: 2024-11-22XIANTAO XINHENRUI NEW MATERIAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011085983.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-10-12
Publication Date
2024-11-22
Estimated Expiration
2040-10-12

AI Technical Summary

Technical Problem

In the prior art, the iron-based nanocrystal open-close ring magnetic core has a large error after cutting, which cannot meet the client's requirements for accuracy, and it is difficult to control the size during soaking and baking, resulting in a high loss value of the cutting gap.

Method used

A fixed mold for iron-based or nickel-based annular magnetic core is designed. Through the combined structure of the outer frame mold and the inner frame mold, the loss width is reserved to ensure that the size of the magnetic core can be accurately controlled during soaking and baking. , including the positioning beam and connecting beam of the outer frame mold, as well as the positioning plate and snap groove of the inner frame mold, fix the magnetic core body to prevent deformation.

Benefits of technology

By reserved loss width and precise fixing structure, the core can be prevented from deforming during soaking and baking, the finished product accuracy of the magnetic core can be improved, the size requirements of the downstream process can be met, and the cutting error can be reduced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112117117B_ABST
    Figure CN112117117B_ABST
Patent Text Reader

Abstract

The present invention discloses a shaping mold for manufacturing an iron-based or nickel-based annular magnetic core, comprising: an outer frame mold, the outer frame mold comprising two positioning beams and at least two connecting beams; an inner frame mold, the inner frame mold comprising a first positioning plate and a second positioning plate arranged crosswise, the two ends of the upper portion of the first positioning plate are provided with positioning parts, the two ends of the upper portion of the first positioning plate are respectively clamped in two positioning grooves by the positioning parts, the lower portion of the first positioning plate is arranged between the two positioning beams, and the second positioning plate is arranged between the two connecting beams; the width of the positioning groove is a, the spacing between the two connecting beams is (a+b), and the length of the second positioning plate is (a+c), wherein a is the loss width of the iron-based or nickel-based annular magnetic core cutting, b is the outer end width of the iron-based or nickel-based annular magnetic core after cutting, and c is the inner end width of the iron-based or nickel-based annular magnetic core after cutting. The present invention is applied to the technical field of annular magnetic cores.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of annular magnetic cores, and in particular to a shaping die used for manufacturing iron-based or nickel-based annular magnetic cores. Background Art

[0002] The iron-based nanocrystalline split toroidal core is used for split induction electromagnetic devices. Due to its excellent magnetic permeability, high Bs value, high precision and other characteristics, in recent years, the iron-based nanocrystalline split toroidal core has been widely used in transmission lines in the fields of power transmission and distribution in the fields of high-voltage overhead transmission lines, cables, ring network cabinets, etc. Because the working voltage of the cable transmission line is as high as 10kV-1150kV, the current ranges from tens of amperes to thousands of amperes. Using the iron-based nanocrystalline split toroidal core to draw electricity has a high safety factor for operators, is convenient and quick to install and use, and is also easy to disassemble, maintain and install again.

[0003] The iron-based nanocrystalline split-type toroidal magnetic core is cut in half using a green carbon silicon grinding wheel. Figure 1 to Figure 2 As shown in the figure, the thickness of the cutting grinding wheel is 0.8mm, which causes the iron-based nanocrystalline open-and-closed toroidal core to have a cutting gap loss of more than 0.8mm after cutting. In addition, the cutting surface grinding, deburring, and polishing of the iron-based nanocrystalline open-and-closed toroidal core have resulted in a cutting gap loss of 1.0mm. In actual use, the molds of the supporting parts of the client's products have tolerance accuracy requirements. Some clients require that the error of the iron-based nanocrystalline open-and-closed toroidal core after cutting is within ±0.3mm, which makes the iron-based nanocrystalline open-and-closed toroidal core in the prior art unable to meet the requirements.

[0004] In the prior art, it is difficult to control the size of the iron-based nanocrystalline split-and-closed toroidal magnetic core during soaking and baking, which also causes a large error in the cut iron-based nanocrystalline split-and-closed toroidal magnetic core. Summary of the invention

[0005] 1. Technical issues to be resolved

[0006] A shaping mold for manufacturing an iron-based or nickel-based annular magnetic core reserves a loss width when fixing an outer frame mold and an inner frame mold. During soaking and baking, the size of the annular magnetic core body can be accurately controlled to meet downstream process requirements.

[0007] (II) Technical solution

[0008] In order to solve the above technical problems, the present invention provides a shaping die for manufacturing an iron-based or nickel-based annular magnetic core, comprising:

[0009] An outer frame mold, the outer frame mold comprising two positioning beams and at least two connecting beams, the two ends of the two positioning beams are detachably connected by the connecting beams to form a frame structure, the tops of the two positioning beams are respectively provided with positioning grooves, and the positioning grooves on the two positioning beams are opposite and located on the same straight line;

[0010] An inner frame mold, the inner frame mold comprising a first positioning plate and a second positioning plate arranged crosswise, positioning parts are arranged at both ends of the upper portion of the first positioning plate, the two ends of the upper portion of the first positioning plate are respectively clamped in two positioning grooves through the positioning parts, the lower portion of the first positioning plate is arranged between the two positioning beams, and the second positioning plate is arranged between the two connecting beams;

[0011] The width of the positioning groove is a, the spacing between the two connecting beams is (a+b), and the length of the second positioning plate is (a+c), wherein a is the loss width of the iron-based or nickel-based annular magnetic core after cutting, b is the outer end width of the iron-based or nickel-based annular magnetic core after cutting, and c is the inner end width of the iron-based or nickel-based annular magnetic core after cutting.

[0012] As a further improvement, the number of the connecting beams is two, and the two positioning beams and the two connecting beams are detachably connected to form a square frame structure.

[0013] As a further improvement, the two positioning beams are of equal length, and the positioning groove is located at the center of the positioning beam.

[0014] As a further improvement, the lower portion of the first positioning plate and the lower portion of the second positioning plate are respectively provided with snap grooves, and the lower portion of the first positioning plate and the lower portion of the second positioning plate are cross-arranged through the two snap grooves.

[0015] As a further improvement, the two snap grooves are respectively located at the center of the lower part of the first positioning plate and the lower part of the second positioning plate.

[0016] As a further improvement, the depth of the buckle groove is 3 mm to 5 mm.

[0017] As a further improvement, the positioning beam, the connecting beam, the first positioning plate and the second positioning plate are all made of metal.

[0018] As a further improvement, the connecting beam and the positioning beam are detachably connected via a back-head screw.

[0019] Further improved, the a is 0.8mm to 1.3mm.

[0020] As a further improvement, the depth of the positioning groove is 3 mm to 5 mm, the height of the positioning portion is equal to the depth of the positioning groove, and the height of the lower portion of the first positioning plate is equal to the height of the second positioning plate.

[0021] (III) Beneficial effects

[0022] In the shaping mold for manufacturing iron-based or nickel-based annular magnetic cores of the present invention, at least one connecting beam is removed from the frame structure composed of positioning beams and connecting beams, so that the annular magnetic core body can be placed into the frame structure from the disassembled opening. After the annular magnetic core body is placed, the second positioning plate is placed at the inner end of the annular magnetic core body, and the second positioning plate is arranged along the width direction of the annular magnetic core body. The lower part of the first positioning plate is pressed against the other direction of the inner end of the annular magnetic core body, and the positioning parts at both ends of the upper part of the first positioning plate are stuck in the two positioning grooves, so that the first positioning plate and the second positioning plate can be fixed. By fixing the inner end of the annular magnetic core body by the lower part of the first positioning plate and the second positioning plate, the inner end of the annular magnetic core body can be prevented from being deformed during the soaking and baking of glue, which causes a large error in subsequent cutting. Finally, the disassembled connecting beams are connected at the corresponding positions to close the frame structure, so that the outer frame mold can fix the outer end of the annular magnetic core body, which prevents the outer end of the annular magnetic core body from being deformed during the soaking and baking of glue, which causes a large error in subsequent cutting.

[0023] On the other hand, since the outer frame mold and the inner frame mold reserve a loss width when fixing the annular magnetic core body to be cut, after the annular magnetic core body of the present invention is cut, the inner end width and the outer end width of the annular magnetic core body can just meet the target size requirements, and the error is within the ideal range, so the finished annular magnetic core has a high precision.

[0024] The present invention uses an inner frame mold to fix the inside of the annular magnetic core body and an outer frame mold to fix the outside of the annular magnetic core body, so that the annular magnetic core body can be fixed to prevent it from deforming during soaking and baking. And through the reserved loss width, the size of the annular magnetic core body can be accurately controlled to meet the downstream process requirements. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 A schematic diagram of the loss width of an iron-based nanocrystalline split-type annular magnetic core after cutting in the prior art;

[0026] Figure 2 A dimension diagram of the loss width of an iron-based nanocrystalline split-type annular magnetic core after cutting in the prior art;

[0027] Figure 3 Three views of an outer frame mold in one embodiment of the present invention;

[0028] Figure 4 Two views of a first positioning plate in one embodiment of the present invention;

[0029] Figure 5 Two views of the second positioning plate in one embodiment of the present invention;

[0030] Figure 6 It is a schematic structural diagram of an outer frame mold and an inner frame mold fixing an annular magnetic core according to an embodiment of the present invention. DETAILED DESCRIPTION

[0031] The specific implementation of the present invention is further described in detail below in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention.

[0032] In the description of the present invention, it is necessary to understand that the terms "center", "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.

[0033] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0034] Please refer to Figures 3 to 6 , a shaping die for manufacturing an iron-based or nickel-based toroidal magnetic core, comprising:

[0035] An outer frame mold, the outer frame mold comprising two positioning beams 1 and at least two connecting beams 2, the two ends of the two positioning beams 1 are detachably connected by the connecting beams 2 to form a frame structure, the tops of the two positioning beams 1 are respectively provided with positioning grooves 3, and the positioning grooves 3 on the two positioning beams 1 are opposite and located on the same straight line;

[0036] The inner frame mold includes a first positioning plate 4 and a second positioning plate 5 which are cross-arranged, and positioning portions 41 are provided at both ends of the upper portion of the first positioning plate 4. The two ends of the upper portion of the first positioning plate 4 are respectively clamped in the two positioning grooves 3 through the positioning portions 41. The lower portion of the first positioning plate 4 is arranged between the two positioning beams 1, and the second positioning plate 5 is arranged between the two connecting beams 2.

[0037] The width of the positioning groove 3 is a, the spacing between the two connecting beams 2 is (a+b), and the length of the second positioning plate 5 is (a+c), wherein a is the loss width of the iron-based or nickel-based annular magnetic core after cutting, b is the outer end width of the iron-based or nickel-based annular magnetic core after cutting, and c is the inner end width of the iron-based or nickel-based annular magnetic core after cutting.

[0038] In this embodiment, the shaping mold for manufacturing an iron-based or nickel-based annular magnetic core is used to fix the annular magnetic core body 8 to be cut. In this embodiment, the normal direction of the surface to be cut of the annular magnetic core body 8 is customized as the width direction of the annular magnetic core body 8. The specific fixing method is:

[0039] At least one connecting beam 2 is removed from the frame structure composed of the positioning beam 1 and the connecting beam 2, so that the annular core body 8 can be placed into the frame structure from the disassembled opening. After the annular core body 8 is placed, the second positioning plate 5 is placed at the inner end of the annular core body 8, and the second positioning plate 5 is arranged along the width direction of the annular core body 8. The lower part of the first positioning plate 4 is pressed against the other direction of the inner end of the annular core body 8, and the positioning parts 41 at both ends of the upper part of the first positioning plate 4 are stuck in the two positioning grooves 3, so that the first positioning plate 4 and the second positioning plate 5 can be fixed. By fixing the inner end of the annular core body 8 by the lower part of the first positioning plate 4 and the second positioning plate 5, the inner end of the annular core body 8 can be prevented from deforming during the glue soaking and baking, which causes a large error in subsequent cutting. Finally, the disassembled connecting beam 2 is connected to the corresponding position to close the frame structure, so that the outer frame mold can fix the outer end of the annular core body 8, so as to prevent the outer end of the annular core body 8 from deforming during the glue soaking and baking, which causes a large error in subsequent cutting.

[0040] On the other hand, since the outer frame mold and the inner frame mold reserve a loss width when fixing the annular magnetic core body 8 to be cut, after the annular magnetic core body 8 of this embodiment is cut, the inner end width and the outer end width of the annular magnetic core body 8 just meet the target size requirements, and the error is within the ideal range, so the finished annular magnetic core has a high precision.

[0041] In this embodiment, the inner frame mold is used to fix the inner part of the annular core body, and the outer frame mold is used to fix the outer part of the annular core body, so that the annular core body 8 can be fixed to prevent it from deforming during soaking and baking. And through the reserved loss width, the size of the annular core body 8 can be accurately controlled to meet the downstream process requirements.

[0042] The annular magnetic core body 8 of this embodiment includes an iron-based nanocrystalline annular magnetic core, an iron-based amorphous annular magnetic core and a nickel-based annular magnetic core. The nickel-based is a nickel-iron alloy, the main component of the nickel-based is nickel, and the main component of the iron-based is iron. Among them, the annular shape includes a circular ring, a square ring and an elliptical ring, etc. Further, in one embodiment, the number of the connecting beams 2 is two, the two positioning beams 1 and the two connecting beams 2 are detachably connected to form a square frame structure, and the finished product of the annular magnetic core manufactured at last is a circular ring or an elliptical shape.

[0043] Further, in one embodiment, when the manufactured annular magnetic core body 8 is in the shape of a circular ring, the lengths of the two positioning beams 1 are equal, and the positioning groove 3 is located at the center of the positioning beam 1. Specifically, the spacing between the two positioning beams 1 is b, and the length of the lower portion of the first positioning plate 4 is c. In this way, after cutting, the finished product of the annular magnetic core is in the shape of a circular ring, with a high roundness, ensuring accuracy. Further preferably, the two snap grooves 6 are located at the center of the lower portion of the first positioning plate 4 and the lower portion of the second positioning plate 5, respectively.

[0044] Further, in one embodiment, the depth of the snap groove 6 is 3 mm to 5 mm, specifically, the depth of the snap groove 6 is 4 mm, wherein a is 0.8 mm to 1.3 mm, preferably, a is 1 mm, b is 25 mm, and c is 35 mm.

[0045] Furthermore, in one embodiment, the lower portion of the first positioning plate 4 and the lower portion of the second positioning plate 5 are respectively provided with snap grooves 6, and the lower portion of the first positioning plate 4 and the lower portion of the second positioning plate 5 are cross-arranged through the two snap grooves 6, so that the first positioning plate 4 and the second positioning plate 5 are connected, which is convenient for disassembly and assembly.

[0046] Furthermore, in one embodiment, the positioning beam 1, the connecting beam 2, the first positioning plate 4 and the second positioning plate 5 are all made of metal. During baking, the positioning beam 1, the connecting beam 2, the first positioning plate 4 and the second positioning plate 5 can withstand high temperatures and are not easily deformed, so as to ensure the finished product accuracy of the annular magnetic core.

[0047] Furthermore, in one embodiment, the connecting beam 2 and the positioning beam 1 are detachably connected via a back-head screw 7, which has low cost, convenient assembly and disassembly, and a firm connection.

[0048] Furthermore, in one embodiment, the depth of the positioning groove 3 is 3 mm to 5 mm, the height of the positioning portion 41 is equal to the depth of the positioning groove 3, and the height of the lower portion of the first positioning plate 4 is equal to the height of the second positioning plate 5. In the actual production process, the height of the lower portion of the first positioning plate 4 and the height of the second positioning plate 5 may not be equal, but if they are not equal, it may be inconvenient to store and process. If they are equal, it can be convenient to store and process.

[0049] In a specific embodiment, based on the above-mentioned shaping mold, a method for manufacturing an iron-based or nickel-based annular magnetic core includes the following steps:

[0050] S1, preparing an annular magnetic core body to be cut, wherein the annular magnetic core body has a loss width reserved for cutting;

[0051] S2, using an inner frame mold to fix the inside of the annular magnetic core body, and using an outer frame mold to fix the outside of the annular magnetic core body;

[0052] S3, subjecting the fixed annular magnetic core body to heat treatment, glue soaking, baking, cutting and polishing in sequence to manufacture a finished annular magnetic core.

[0053] The manufacturing method of the iron-based or nickel-based annular magnetic core of this embodiment reserves a loss width for the annular magnetic core body to be cut, so that after the annular magnetic core body 8 is cut, the inner end width and the outer end width of the annular magnetic core body 8 just meet the target size requirements, and the error is within the ideal range, so that the finished product precision of the annular magnetic core is high. By using an inner frame mold to fix the inside of the annular magnetic core body 8 and using an outer frame mold to fix the outside of the annular magnetic core body 8, the annular magnetic core body 8 can be fixed to prevent it from deforming during soaking and baking. The size of the annular magnetic core body 8 can be accurately controlled to meet the downstream process requirements.

[0054] Preferably, a release agent is applied between the annular magnetic core body 8 and the outer frame mold and the inner frame mold, respectively. When the annular magnetic core body and the inner frame mold and the outer frame mold are separated, the release agent can facilitate the demoulding of the annular magnetic core body 8.

[0055] Further, in one embodiment, in step S3, the annular magnetic core body is heat treated at a temperature of 540°C to 570°C to improve the magnetic properties of the annular magnetic core body, and the heat treatment time is 3h to 5h, where h is the abbreviation of the hour unit. Preferably, the annular magnetic core body is heat treated at a temperature of 560°C for 5h. The magnetic properties of the annular magnetic core body can be improved by heat treatment.

[0056] Further, in one embodiment, in step S3, the annular magnetic core body is soaked in glue using epoxy resin glue in a vacuum container of -0.1MPa, and the soaking time is 25min to 45min, where min is the abbreviation of minute unit. Preferably, the soaking time is 30min. The annular magnetic core body 8 can be hardened by soaking in glue, and the annular magnetic core body soaked in glue can be hardened by baking, which is convenient for cutting.

[0057] Further, in one embodiment, in step S3, after the glue is soaked, the annular magnetic core body 8 is baked at a temperature of 150° C. to 170° C. for 3 to 6 hours. Preferably, after the glue is soaked, the annular magnetic core body 8 is baked at a temperature of 160° C. for 5 hours. Baking can further improve the hardness of the annular magnetic core body 8, which is conducive to cutting.

[0058] Furthermore, in one embodiment, in step S3, after drying, the annular magnetic core body is cut in the direction of the reserved loss width, and the cut loss width just matches the reserved loss width. After cutting, the finished annular magnetic core has extremely high precision and can meet customer requirements.

[0059] Of course, the shaping mold used for manufacturing the iron-based or nickel-based annular magnetic core in this embodiment can also be used to fix the non-annular magnetic core. The specific method is to only fix the outer frame mold to the outside of the non-annular magnetic core body and reserve the loss width at the same time. However, in the actual production process, the size control of the annular magnetic core is much more difficult to control than the size of the non-annular magnetic core. Therefore, the shaping mold used for manufacturing the iron-based or nickel-based annular magnetic core in this embodiment is of great significance in the manufacturing application of the annular magnetic core.

[0060] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. A shaping die for manufacturing an iron-based or nickel-based toroidal magnetic core, characterized in that: include: An outer frame mold, the outer frame mold comprising two positioning beams and at least two connecting beams, the two ends of the two positioning beams are detachably connected by the connecting beams to form a frame structure, the tops of the two positioning beams are respectively provided with positioning grooves, and the positioning grooves on the two positioning beams are opposite and located on the same straight line; An inner frame mold, the inner frame mold comprising a first positioning plate and a second positioning plate arranged crosswise, positioning parts are arranged at both ends of the upper portion of the first positioning plate, the two ends of the upper portion of the first positioning plate are respectively clamped in two positioning grooves through the positioning parts, the lower portion of the first positioning plate is arranged between the two positioning beams, and the second positioning plate is arranged between the two connecting beams; The width of the positioning groove is a, the spacing between the two connecting beams is (a+b), and the length of the second positioning plate is (a+c), wherein a is the loss width of the iron-based or nickel-based annular magnetic core after cutting, b is the outer end width of the iron-based or nickel-based annular magnetic core after cutting, and c is the inner end width of the iron-based or nickel-based annular magnetic core after cutting; There are two connecting beams, and the two positioning beams and the two connecting beams are detachably connected to form a square frame structure; The two positioning beams have the same length, and the positioning groove is located at the center of the positioning beam; The lower part of the first positioning plate and the lower part of the second positioning plate are respectively provided with buckle grooves, and the lower part of the first positioning plate and the lower part of the second positioning plate are cross-arranged through the two buckle grooves; The depth of the buckle groove is 3 mm to 5 mm; The a is 0.8 mm to 1.3 mm; The depth of the positioning groove is 3 mm to 5 mm, the height of the positioning portion is equal to the depth of the positioning groove, and the height of the lower portion of the first positioning plate is equal to the height of the second positioning plate.

2. The molding die for manufacturing an iron-based or nickel-based annular magnetic core according to claim 1, characterized in that: The two buckle grooves are respectively located at the center of the lower part of the first positioning plate and the lower part of the second positioning plate.

3. The shaping die for manufacturing an iron-based or nickel-based annular magnetic core according to any one of claims 1 to 2, characterized in that: The positioning beam, the connecting beam, the first positioning plate and the second positioning plate are all made of metal.

4. The shaping die for manufacturing an iron-based or nickel-based annular magnetic core according to any one of claims 1 to 2, characterized in that: The connecting beam and the positioning beam are detachably connected via a back-head screw.