Porous region structure and method for manufacturing the same

By using hard masks covering transverse holes in the porous regional structure and selective etching technology, the problems of uneven shape and corrosion of holes in the hard mask boundary area are solved, and high accuracy and stability of the porous regional structure are achieved.

CN112119512BActive Publication Date: 2024-11-26MURATA MFG CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201980031729.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-05-11
Filing Date
2019-05-09
Publication Date
2024-11-26
Estimated Expiration
2039-05-09

AI Technical Summary

Technical Problem

In the prior art, uneven pore shapes and corrosion problems in the hard mask boundary area make it difficult to accurately control and improve the electrical value of the porous area structure, and easily lead to halogen corrosion.

Method used

By depositing anodized hard mask on the first metal layer and depositing a hard mask with openings on top of it to cover the transverse pores of the porous region, ensuring that the layered structure is embedded only in the defined region, combined with selective etching to remove Anodize hard masks to improve surface and robustness and use materials that are resistant to halogen corrosion.

Benefits of technology

High precision control of pore ratio and pore shape of the pore structure in the porous region is achieved, reducing the risk of halogen corrosion, and improving the accuracy of electrical values ​​and structural stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112119512B_ABST
    Figure CN112119512B_ABST
Patent Text Reader

Abstract

A porous region structure and a method for making the same are disclosed. The porous region structure is characterized by sealing a hard mask boundary region having non-uniform pores, thereby excluding functionality from the structure. The sealing of the hard mask boundary region is accomplished by using a hard mask deposited on top of an anodized hard mask used to define the porous region of the structure. By excluding the hard mask boundary region, the porosity ratio and equivalent specific surface of the porous region structure can be controlled or quantified with greater precision. By sealing the hard mask boundary region, corrosion caused by exposure of the underlying metal layer of the structure can also be significantly reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of integration, and more particularly, to electronic products, related semiconductor products and methods of manufacturing the same. Background Art

[0002] Today, silicon passive integration technology is available for industrial design. For example, PICS technology developed by Murata Integrated Passive Solutions allows high-density capacitive components to be integrated into a silicon substrate. With this technology, dozens or even hundreds of passive components can be efficiently integrated into a silicon die.

[0003] In the work of P. Banerjee et al. entitled "Nanotubular metal-insulator-metal capacitor arrays for energy storage" (published in Natural technology in May 2009), metal-insulator-metal (MIM) structures formed in porous anode materials such as, for example, porous anodic alumina (PAA) are described. Successive layers of metal, insulator and then metal follow the contours of the porous material so that the MIM structure is embedded inside the pores of the porous material. However, due to the thickness of PAA that can be deposited by atomic layer deposition (ALD), Banerjee's PAA embedded structure suffers from high equivalent series resistance (ESR) and limited capacitance density.

[0004] The structure of F. Voiron et al. that improves Banerjee's ESR and capacitance is described in International Application Publication WO2015 / 063420A1. Voiron's structure results in a highly integrated capacitor that can be used in a variety of applications. In this structure, the bottom of the hole is opened, and the lower metal layer of the MIM structure contacts the conductive layer located under the porous area, providing electrical contact and reducing ESR.

[0005] Typically, the PAA embedded structure described above is obtained by embedding a structure (e.g., a MIM capacitive stack) inside a porous region above a substrate, such as a silicon wafer. Typically, the porous region is obtained by anodizing a thin layer of a metal, such as aluminum, deposited above the substrate. Anodization converts the aluminum layer into porous anodized aluminum. Typically, the porous region is formed in any shape (viewed from the top) and extends across the aluminum oxide layer in a direction perpendicular to the wafer surface.

[0006] Figure 1 is a cross-sectional view of an example structure 100 for manufacturing a product having a porous region. For example, the example structure 100 may be an intermediate product in the process of manufacturing an integrated capacitor structure as described in WO 2015 / 063420 A1. The example structure 100 is provided for the purpose of illustrating the formation of a porous region, and the example structure 100 is not limiting with respect to the type of product that may be generated.

[0007] like Figure 1 As shown in FIG. 1 , structure 100 includes silicon layer 102, aluminum layer 104, barrier layer 106, aluminum layer 108, and hard mask layer 110. In an example product, aluminum layer 104 may provide an electrode for an integrated capacitor structure. Barrier layer 106 may provide protection to aluminum layer 104, for example, by preventing the progression of anodization from reaching aluminum layer 104 and / or provide protection to aluminum layer 104 during a subsequent PAA etching step in the manufacturing process.

[0008] When forming the porous region, for some applications it may be desirable to have the resulting porous region embedded within the original aluminum layer. For example, it may be desirable to control the size of the resulting porous region in order to control the size and electrical values ​​(e.g., capacitance, resistance, etc.) of the structure to be embedded therein. Typically, this is accomplished by applying a hard mask layer 110 on top of the aluminum layer 108 to mask the areas of the aluminum layer 108 that are not to be anodized. The mask shields this area from contact with the anodizing electrolyte, and thus, the porous region is formed in the areas of the aluminum layer 108 where the hard mask layer 110 is open.

[0009] Figure 2 is a scanning electron microscope (SEM) image showing a top view of the boundary between the hard mask (HM1) and the porous area (PAA) formed using the above-mentioned anodizing process. As shown, the hard mask HM1 is formed in such a way as to define the perimeter and position of the porous area PAA within the original embedded metal (e.g., aluminum) layer.

[0010] Typically, a silicon dioxide mask layer is used for the hard mask HM1. This choice is driven by several factors, including: the availability of silicon dioxide deposition processes at medium / low temperatures that are compatible with deposition over aluminum-based stacks, the availability of silicon dioxide patterning techniques with good selectivity over underlying aluminum layers, silicon dioxide's resistance to anodization steps, and relatively low stress caused by the oxide layer.

[0011] However, while this choice is beneficial for the reasons above, it has an undesirable effect on pore formation in the region of the aluminum layer close to the hard mask (hereinafter the "hard mask boundary region"). In essence, the use of silicon dioxide for the hard mask layer weakens the anodization electric field through the underlying aluminum layer near the hard mask boundary. This weakening of the anodization electric field results in pores in the hard mask boundary region that are not fully opened and / or are misshapen.

[0012] Figure 3 is a cross-sectional SEM image showing the hard mask boundary region of an example porous region formed using a silicon dioxide hard mask over an aluminum layer. Figure 3 As shown in , the holes in the hard mask boundary region (hereinafter "lateral holes") are highly non-uniform, having non-uniform diameters and / or depths. In addition, the lateral holes tend to bend away from the substrate to penetrate into the sides of the embedded aluminum layer, rather than extending vertically or substantially vertically toward the substrate.

[0013] The degree of non-uniformity in the depth of the lateral holes depends on the density of the aluminum grain boundaries (and other microstructural parameters), but mainly on the distribution of the anodizing electric field. Close to the edge of the hard mask, the anodizing electric field is weakest and the lateral holes remain in the residual aluminum flange. By controlling the anodizing process, the width of the aluminum flange in a direction parallel to the substrate surface can be reduced, but this control is limited by the risk of oxidation of the anodized barrier layer under the aluminum layer. Away from the edge of the hard mask, the anodizing electric field is stronger, the aluminum flange gradually disappears and is replaced by aluminum oxide. The lateral holes in this area can extend all the way through the aluminum layer. In one implementation, the holes can be opened to a bottom metal layer placed below the aluminum layer to enable electrical contact with the structure embedded in the porous area. However, despite being fully opened, the lateral holes in this area may still be deformed with a high probability.

[0014] In practice, as the inventors of the present invention have been able to determine, the width of the hard mask boundary region is related to the thickness of the aluminum layer being anodized (the thicker the aluminum layer, the wider the hard mask boundary region). For example, for a porous region produced by a typical 60V anodization process, the hard mask boundary region may include a deformed region that is approximately 10 microns wide for a 5 micron deep PAA structure and approximately 20 microns wide for a 10 micron deep PAA structure. Although controllable by the anodization process, the width of the residual aluminum ridge near the edge of the hard mask is typically regulated between 5 microns and 20 microns. Therefore, the hard mask boundary region may be significant in size, especially for smaller sized porous regions.

[0015] Because the hard mask boundary region may be uncontrollable in terms of pore shape (i.e., depth, diameter, orthogonality to the substrate), the contribution of the hard mask boundary region to the porosity ratio of the porous region (i.e., the component of air / vacuum in the porous region), and accordingly, the contribution of the hard mask boundary region to the electrical values ​​of the structures embedded in the porous region (e.g., capacitance, resistance, etc.) may be difficult to quantify with high accuracy. This may be problematic in cases where a precise specific area is required (where specific area is defined as the ratio of 3D to 2D exposed surface, where the 3D exposed surface includes the surface area of ​​the pores and the 2D exposed surface is the top surface of the porous region). For example, in the case where a capacitive structure is embedded in a porous region, a variation tolerance of less than 1% of the rated capacitance may be required. For capacitive structures embedded in small porous regions (e.g., <0.5mm 2 ), the hard mask boundary region may contribute approximately 4% of the volume of the porous region. Therefore, geometric fluctuations within the hard mask boundary region may cause errors in the actual structure capacitance that exceed the variation tolerance. For certain applications, where good control of the pore shape (depth, diameter, orthogonality to the substrate) of the porous region structure is required, the uncontrollability of the lateral pores may also be problematic.

[0016] Lateral holes may also tend to cause corrosion of the resulting product. In one implementation, the hole formation process is followed by a hole enlargement process in which the PAA walls between the holes ("hole walls") are wet etched (e.g., using phosphoric acid) to expand the hole diameter and, correspondingly, the surface area embedded in the hole. Through this step, most of the hole walls can be etched away, and the layers below the bottom of the hole can be exposed. For non-lateral holes (i.e., holes outside the hard mask boundary region and these holes extend vertically or substantially vertically toward the substrate), the underlying barrier layer made of a metal such as tungsten (W) or titanium (Ti) can be exposed. As discussed above, the lateral holes may extend into the sides of the embedded aluminum, causing the aluminum to be exposed.

[0017] Exposure of aluminum during barrier etching (phosphoric acid etching is not selective for Al) or in subsequent process steps may result in corrosion. For example, where a capacitive MIM structure is deposited into a porous region, the electrodes of the MIM structure may be formed from titanium nitride (TiN), which is typically deposited by an atomic layer deposition (ALD) process with a gaseous halogen-based (e.g., chlorine) precursor. Exposure of aluminum to this precursor results in its corrosion and the growth of AlClO compounds, which may result in catastrophic failure or short-term reliability issues. Figure 4A and Figure 4BAn image of an SEM cross section and a surface tilt view of an example porous region showing corrosion due to aluminum exposure are provided in FIG. 1 , respectively. Note that the barrier layer (e.g., made of W or Ti) beneath the non-lateral pores of the porous region is less prone to halogen corrosion than aluminum. In the resulting product, exposing this layer to a halogen-based precursor does not pose a risk of catastrophic corrosion.

[0018] In view of the above problems, the present invention is proposed. Summary of the invention

[0019] The present invention provides a method for manufacturing a porous region structure, comprising:

[0020] depositing a first metal layer over the substrate;

[0021] depositing an anodized hard mask on top of the first metal layer, the anodized hard mask having openings over anodized regions of the first metal layer;

[0022] anodizing the first metal layer to form a porous region in the first metal layer, the porous region being below the anodized region of the first metal layer;

[0023] depositing a hard mask on top of the porous region, the hard mask having an opening over a defined area of ​​the porous region, the defined area being smaller than the anodized region and included within the anodized region; and

[0024] A layered structure is deposited on top of the hard mask and the porous region to embed the layered structure into the porous region above a defined area of ​​the porous region.

[0025] In an embodiment, the porous region formed by anodization of the first metal layer includes an anodic oxide having a plurality of holes extending from the top surface of the porous region toward the substrate. However, in the region where the first metal layer is adjacent to the anodized hard mask ("hard mask boundary region"), the holes may be very non-uniform. Specifically, the holes in this region ("lateral holes") may have non-uniform diameters and / or depths. In addition, the lateral holes tend to bend away from the substrate to penetrate into the side of the first metal layer embedded in the porous region, rather than extending vertically or substantially vertically toward the substrate. Therefore, when depositing a layered structure, the electrical contribution (e.g., capacitance, resistance, etc.) of these lateral holes may be difficult to accurately quantify. In addition, when subsequent process steps use halogen-based precursors, the lateral holes may tend to cause halogen corrosion in the resulting product.

[0026] Depositing a hard mask having smaller openings above the porous region than the anodized hard mask on top of the anodized hard mask ensures that the lateral pores of the porous region are sealed by the hard mask when the layered structure is deposited. Because the lateral pores are eliminated from the resulting porous region embedded structure, the accuracy of the electrical values ​​of the structure (e.g., capacitance, resistance, etc.) can be improved. In addition, the porosity ratio (i.e., the air / vacuum component in the porous region) and the pore shape (i.e., depth, diameter, orthogonality to the substrate) of the structure can be better controlled. Sealing the lateral pores also significantly reduces the risk of halogen corrosion in the first metal layer due to subsequent process steps using halogen-based precursors.

[0027] In another embodiment, the manufacturing method may further include: selectively etching the anodized hard mask before depositing the hard mask. Partially or completely removing the anodized hard mask before depositing the hard mask can have several benefits. For example, during anodization, the anodized hard mask may break at the edges of the porous region due to expansion of the PAA. Removing the anodized hard mask allows any broken areas of the anodized hard mask to be removed, which is conducive to better deposition of the hard mask. The resulting structure is improved from both a surface and robustness perspective (in the case of complete removal of the anodized hard mask, the possibility of anodized hard mask breakage is reduced or eliminated). By removing the anodized hard mask, subsequent process steps (e.g., metallization or photoresist spin coating) are also simplified.

[0028] In the porous region structure formed according to the above method, the lateral pores fall within the anodized region, but outside the defined region of the porous region. In an embodiment, the distance between the edge of the anodized region and the corresponding edge of the defined region is made proportional to the thickness of the first metal layer anodized to form the porous region. This configuration is based on the inventor's recognition that the width of the hard mask boundary region increases as the thickness of the first metal layer is anodized.

[0029] In an embodiment, the hard mask is made of a material that is substantially resistant to halogen corrosion. This further protects the resulting structure from corrosion that may be caused by the use of halogen-based precursors in subsequent process steps. In another embodiment, the hard mask is also substantially resistant to wet (e.g., phosphoric acid) or dry chemical components used during the etching of the barrier layer at the bottom of the hole and during the hole enlargement process described above.

[0030] In an embodiment, the method of manufacturing a porous region structure may further include depositing a second metal layer above the substrate such that the second metal layer is below the first metal layer. The second metal layer may be used to provide electrical contact with the conductive layer of the layered structure. In this way, the non-lateral pores of the porous region may be configured to extend through the porous region to open onto the second metal layer. The second metal layer may be made of a metal that is resistant to halogen corrosion and is therefore compatible with subsequent process steps using halogen-based precursors.

[0031] The present invention also provides a porous domain structure that can be formed using the steps of the method described above. In an embodiment, the porous domain structure comprises:

[0032] substrate;

[0033] a first metal layer over the substrate;

[0034] a porous region comprised of an anodized portion of the first metal layer, the porous region comprising an anodic oxide having a plurality of pores extending from a top surface of the porous region toward the substrate; and

[0035] A hard mask is provided over the first metal layer and the porous region, the hard mask having openings over defined areas of the porous region, configured such that the hard mask covers lateral holes in the plurality of holes in the porous region.

[0036] By sealing the lateral pores for subsequent process steps, the porosity and pore shape of the structure can be better controlled. Furthermore, the accuracy of the electrical values ​​of a device using the formed structure can be improved. Additionally, the likelihood of corrosion in the device due to the use of halogen-based precursors during the process steps is reduced.

[0037] In an embodiment, the porous region structure further comprises an anodized hard mask on top of the first metal layer, the anodized hard mask having an opening above the anodized region of the porous region, wherein the distance between the edge of the anodized region of the porous region and the corresponding edge of the defined region is proportional to the thickness of the portion of the first metal layer that is anodized to form the porous region. This construction is based on the inventor's recognition that the width of the hard mask boundary region increases as the thickness of the first metal layer is anodized. In an embodiment, the distance between the edge of the anodized region and the corresponding edge of the defined region ranges from 100 nanometers to 50 microns. In an embodiment, the lateral pores fall within the anodized region but outside the defined region of the porous region.

[0038] In an embodiment, the hard mask is made of a material that is substantially resistant to halogen corrosion. This further protects the structure from corrosion that may be caused by the use of halogen-based precursors in the process steps.

[0039] In an embodiment, the porous region structure may further include a layered structure deposited on top of the hard mask, the layered structure being embedded in the plurality of holes of the porous region, excluding lateral holes. The layered structure may include a metal-insulator-metal (MIM) stack such that the porous region structure provides a capacitive component.

[0040] In an embodiment, the porous region structure may further include a second metal layer below the first metal layer, wherein the non-lateral holes in the plurality of holes extend through the porous region to open onto the second metal layer. The second metal layer may be used to provide electrical contact with the structure deposited in the non-lateral holes of the porous region. For example, where the layered structure is deposited in the non-lateral holes, the conductive layer of the layered structure may be in electrical contact with the second metal through the non-lateral holes. The second metal layer may be made of a metal that is resistant to halogen corrosion and is therefore compatible with process steps using halogen-based precursors.

[0041] As noted above, in an embodiment, the anodized hard mask may be partially or completely removed (e.g., using selective etching) before the hard mask is deposited. Removing the anodized hard mask may have several benefits. For example, during anodization, the anodized hard mask may break at the edges of the porous region due to the expansion of the PAA. Removing the anodized hard mask allows any broken areas of the anodized hard mask to be removed, which is beneficial for better deposition of the hard mask. The resulting structure is improved from both a surface and robustness perspective (in the case of complete removal of the anodized hard mask, the possibility of anodized hard mask breakage is reduced or eliminated). By removing the anodized hard mask, subsequent process steps (e.g., metallization or photoresist spin coating) are also simplified. In fact, during anodization, the edges of the anodized hard mask are pushed upward by the expanded PAA. This creates a vertical topology that can reach several microns compared to a flat reference surface. Typically, the vertical topology also has a flange toward the PAA side. This complicates subsequent process steps, including deposition of hardmasks, whenever they need to cover the ridges to maintain, for example, continuity of layers deposited across the ridges. Removal of the anodized hardmask eliminates this vertical topology and ridges, reducing limitations in step coverage and the risk of having discontinuous layers.

[0042] In an embodiment, the porous region structure may further include an electronic component formed on the substrate and electrically connected to the second metal layer. Therefore, the device formed in the porous region may be connected to another electronic component on the substrate to obtain a functional module.

[0043] In embodiments, the substrate may be made of silicon, glass, or a polymer.The substrate may be a raw substrate (ie, unprocessed) or processed by forming other electronic components thereon. BRIEF DESCRIPTION OF THE DRAWINGS

[0044] Other characteristics and advantages of the invention will become apparent from the following description of certain embodiments of the invention, given by way of illustration only and not limitation, with reference to the accompanying drawings, in which:

[0045] Figure 1 is a cross-sectional view of an example structure for making a product having a porous region;

[0046] Figure 2 is a scanning electron microscope (SEM) image showing a boundary between a hard mask and a porous region in a porous region structure;

[0047] Figure 3 is a cross-sectional SEM image showing the hard mask boundary region of an example porous region;

[0048] Figure 4A and Figure 4B is a SEM image showing corrosion in an example porous region structure.

[0049] FIG. 5A to FIG. 5C shows stages in an example method of manufacturing a porous region structure according to an embodiment; and

[0050] Figure 6 is a top view of an example porous region structure according to an embodiment. DETAILED DESCRIPTION

[0051] Embodiments of the present invention solve existing deficiencies of the prior art by using a hard mask to seal the hard mask boundary region of the porous region. The sealing of the hard mask boundary region means that the porosity ratio (i.e., the air / vacuum component in the porous region) and the equivalent specific surface (i.e., the surface area provided by the unsealed pores in the porous region) of the available portion of the porous region can be quantified more accurately. Therefore, when a structure is embedded in the porous region, the electrical value of the structure (e.g., capacitance, resistance, etc.) can be defined with high accuracy.

[0052] Sealing of the hard mask boundary regions also makes the porous region with its embedded structure less prone to corrosion in the metal layer below it. In an embodiment, the structure is made more compatible with subsequent processes using halogen-based precursors or processes that may cause corrosion to exposed areas of the underlying metal layer.

[0053] According to these characteristics, FIG. 5A to FIG. 5C A method of manufacturing a porous region structure according to an embodiment of the present invention is described. In an embodiment, the porous region structure may include a high density integrated capacitor structure.

[0054] like Figure 5AAs shown in , the manufacturing method may include: depositing a first metal layer 506 above a substrate 500; depositing an anodized hard mask 508 on top of the first metal layer 506, wherein the anodized hard mask 508 has an opening above an anodized region 518 of the first metal layer 506; and anodizing the first metal layer 506 to form a porous region 510 within the first metal layer 506 below the anodized region 518 of the first metal layer 506.

[0055] The substrate 500 may be made of, without limitation, silicon, glass, or a polymer, and may be a raw (ie, unprocessed) substrate or processed by forming other electronic components thereon.

[0056] For example, the first metal layer 506 can be made of a metal such as aluminum. The first metal layer 506 can be formed directly on top of the substrate 500. In another embodiment, the porous region structure can include structures in the porous region that require bottom electrical contact. Figure 5A As shown in , the first metal layer 506 can be formed above the electrode layer 502. The electrode layer 502 can include one or more metal layers including aluminum, copper (Cu), silver (Ag), or aluminum copper (AlCu) in combination with a barrier metal such as titanium (Ti), titanium nitride (TiN), tantalum (Ta), and tantalum nitride (TaN) or without a barrier metal. In one embodiment, the electrode layer 502 is formed by an AlCu layer sandwiched between two TiN or TiTiN layers.

[0057] In an embodiment, in order to protect the electrode layer 502 during the formation of the porous region 510, a second metal layer 504 may be disposed between the first metal layer 506 and the electrode layer 502. The second metal layer 504 may be selected to act as an anodization prevention layer for preventing the progress of anodization from reaching the electrode layer 502. In an embodiment, during anodization, the second metal layer 504 may be oxidized to form oxide plugs 512 at the bottom of the holes that reach the second metal layer 504. The oxide plugs 512 may be etched away during subsequent process steps to allow electrical contact between the structures deposited in the holes and the electrode layer 502.

[0058] In another embodiment, the second metal layer 504 can also be selected to act as a barrier layer for shielding the electrode layer 502 from exposure to halogen-based precursors that may be used in subsequent process steps. Thus, for example, the second metal layer 504 can be made of a halogen-resistant metal such as W or Ti.

[0059] The porous region 510 includes an anodic oxide having a plurality of pores extending from the top surface of the porous region 510 toward the substrate 500. As used herein, the term "anodic oxide" is a general term that refers to a material including an anodic oxide or hydroxide and carbon and hydrogen byproducts that may be generated from anodic oxidation. Figure 5A , the central ("non-lateral") hole extends perpendicular or substantially perpendicular to the substrate 500. In an embodiment, the non-lateral holes extend through the porous region 510 to open onto the second metal layer 504. However, lateral holes, i.e., those lateral holes that fall within the hard mask boundary region including the region of the first metal layer 506 adjacent to the anodized hard mask 508, tend to bend further away from the substrate as they approach the edge of the anodized hard mask 508. In addition, the lateral holes may have a non-uniform depth and / or diameter.

[0060] As discussed above, because the hard mask boundary region may be uncontrollable in terms of pore shape (i.e., depth, diameter, orthogonality to the substrate), the contribution of the hard mask boundary region to the porosity ratio of the porous region (i.e., the component of air / vacuum in the porous region), and accordingly, the contribution to the electrical values ​​(e.g., capacitance, resistance, etc.) of the structures embedded in the porous region, may be difficult to define with high precision. This may be problematic where precise specific area is required. The lateral pores in the hard mask boundary region may also tend to induce corrosion into the resulting product if exposed to halogen-based precursors used to deposit the structures into the porous region.

[0061] To overcome these problems, in embodiments of the present invention, the hard mask boundary region is excluded from the portion of the porous region that accommodates the embedded structure in its pores. In embodiments, the hard mask boundary region is sealed before the structure is deposited into the porous region. In one implementation, as Figure 5B As shown in , this is achieved by depositing a hard mask 514 on top of the anodized hard mask 508 and the porous region 510, wherein the hard mask 514 has an opening above a defined region 520 of the porous region 510, the defined region 520 being smaller than the anodized region 518 and included within the anodized region 518. In an embodiment, the defined region 520 is designed so that the hard mask 514 covers the hard mask boundary region of the porous region 510.

[0062] exist Figure 6A top view illustration showing an anodized region 518 (denoted as a first region) and a defined region 520 (denoted as a second region) relative to a porous region 510 according to an example embodiment is provided. This example is provided for illustrative purposes only and is not limited to embodiments. Based on the teachings herein, as will be appreciated by those skilled in the art, the perimeters of the anodized region 518 and the defined region 520 are not limited to rectangles, but may have any shape (e.g., circular, elliptical, etc.).

[0063] The inventors of the present invention have recognized that the width of the hard mask boundary region is proportional to the thickness of the anodized first metal layer 506 (the thicker the first metal layer 506, the wider the hard mask boundary region). For example, for a porous region produced by a typical 60V anodization process, the hard mask boundary region may include a region with misshapen holes that is approximately 10 microns wide for a 5 micron deep PAA structure, or approximately 20 microns wide for a 10 micron deep PAA structure. In addition, the hard mask boundary region generally surrounds an area where a residual flange of the first metal layer 506 is present. As discussed above, although it can be controlled by the anodization process, the flange is generally adjusted between 5 microns and 20 microns. In an implementation, the two regions may or may not overlap.

[0064] Based on this recognition, in an embodiment, the distance "d" between the edge of the anodized region 518 and the corresponding edge of the defined region 520 (see Figure 6 ) is configured to be proportional to the thickness of a portion of the first metal layer 506 that is anodized to form the porous region 510. In an example embodiment, the distance "d" may range from 100 nanometers to 50 micrometers.

[0065] In another embodiment, the anodized hard mask 508 is partially or completely removed (e.g., using selective etching) before depositing the hard mask 514. Removing the anodized hard mask 508 can have several benefits. For example, during anodization, the anodized hard mask 508 may break at the edge of the porous region 510 due to the expansion of the PAA. Removing the anodized hard mask 508 allows any broken areas of the anodized hard mask 508 to be removed, which is conducive to better deposition of the hard mask 514. The resulting structure is improved from both a surface and robustness perspective (in the case of complete removal of the anodized hard mask, the possibility of anodized hard mask breakage is reduced or eliminated). By removing the anodized hard mask 508, subsequent process steps (e.g., metallization or photoresist spin coating) are also simplified. In fact, during anodization, the edge of the anodized hard mask 508 is pushed upward by the expanded PAA. This creates a vertical topology that can reach several microns compared to a flat reference surface. Typically, the vertical topology also has a flange toward the PAA side. This complicates subsequent process steps, including deposition of hardmasks, whenever they need to cover the ridges to maintain, for example, continuity of layers deposited across the ridges. Removal of the anodized hardmask 508 eliminates this vertical topology and ridges, reducing limitations in step coverage and the risk of having discontinuous layers.

[0066] After sealing the hard mask boundary region with hard mask 514, the method may subsequently include depositing structure 516 on top of hard mask 514 and porous region 510. Because porous region 510 is only exposed in defined region 520, structure 516 is embedded in porous region 510 only on defined region 520.

[0067] The accuracy of the electrical values ​​(e.g., capacitance, resistance, etc.) of the structure 516 is improved because the lateral pores do not contribute to the resulting structure 516. In addition, the porosity (i.e., the fraction of air / vacuum in the porous region) and pore shape (i.e., depth, diameter, orthogonality to the substrate) of the structure 516 can be better controlled.

[0068] In an embodiment, structure 516 may be a layered structure including multiple layers. The layered structure may include a conductive layer that is in electrical contact with second metal layer 504 through non-lateral holes. In one embodiment, the layered structure is a metal-insulator-metal (MIM) stack or a double MIM stack, resulting in a capacitive component in a porous region structure.

[0069] In one implementation, a conductive layer may be deposited using an atomic layer deposition (ALD) process using a gaseous halogen-based (e.g., chlorine) precursor, which may provide an electrode for a layered structure. For example, the conductive layer may be made of titanium nitride (TiN). As discussed above, exposure of the first metal layer 506, which may be made of aluminum, to a halogen-based precursor may cause it to corrode, causing catastrophic failures or short-term reliability issues. Since the lateral holes in the porous region are most prone to this type of corrosion, the use of a hard mask 514 to seal the hard mask boundary region significantly reduces the risk of halogen corrosion in the resulting porous region structure. In an embodiment, the hard mask 514 is also made of a material that is substantially resistant to halogen corrosion to provide further protection against this type of corrosion.

[0070] According to the features discussed above, the present invention also provides a porous domain structure. The porous domain structure can be manufactured using the steps of the method described above, and the porous domain structure may include Figure 5B and Figure 5C In an embodiment, the porous region structure comprises:

[0071] substrate;

[0072] a first metal layer over the substrate;

[0073] a porous region comprised of an anodized portion of the first metal layer, the porous region comprising an anodic oxide having a plurality of pores extending from a top surface of the porous region toward the substrate; and

[0074] A hard mask is provided over the first metal layer and the porous region, the hard mask having openings over defined areas of the porous region and configured such that the hard mask covers lateral holes in the plurality of holes in the porous region.

[0075] In an embodiment, an anodized hard mask is used to form a porous region. Specifically, the anodized hard mask is deposited on top of the first metal layer and has an opening above the anodized region of the first metal layer, the anodized region corresponding to the portion to be anodized. In an embodiment, the hard mask is designed to have an opening above a defined area of ​​the porous region, the opening being smaller than the anodized region formed by the anodized hard mask. In this way, the hard mask covers a portion or all of the hard mask boundary region of the porous region. This excludes lateral holes whose shapes are difficult to control (i.e., diameter, depth, orthogonality to the substrate) from being used to accommodate embedded electrical structures. Therefore, as an embedded structure, the remaining functionally active portion of the porous region structure has an equivalent specific surface (i.e., the surface area provided by the pores of the porous region) that can be more accurately quantified. Therefore, for the electrical values ​​(e.g., capacitance, resistance, etc.) of the electrical structures (e.g., capacitive, resistive, etc.) formed inside the porous region structure, higher accuracy can be achieved.

[0076] In an embodiment, the distance between the edge of the anodized region of the porous region and the corresponding edge of the defined region is proportional to the thickness of the portion of the first metal layer that is anodized to form the porous region. This configuration is based on the inventor's recognition that the width of the hard mask boundary region increases as the thickness of the first metal layer is anodized. This configuration ensures that the lateral holes are substantially or completely covered by the hard mask. In an embodiment, the distance between the edge of the anodized region and the corresponding edge of the defined region ranges from 100 nanometers to 50 micrometers.

[0077] In an embodiment, the porous region structure may also include a layered structure deposited on top of the hard mask, the layered structure being embedded in the plurality of holes of the porous region, excluding lateral holes. The layered structure may include a metal-insulator-metal (MIM) stack, resulting in a porous region structure providing a capacitive component.

[0078] In one implementation, a conductive layer of the layered structure may be deposited using an atomic layer deposition (ALD) process using a gaseous halogen-based (e.g., chlorine) precursor, and the conductive layer of the layered structure may provide an electrode for the layered structure. For example, the conductive layer may be made of titanium nitride (TiN). As discussed above, when exposed to this type of precursor, the first metal layer, which may be made of aluminum, may tend to corrode, and the exposure is most likely caused by the lateral holes in the porous region.

[0079] By having the hard mask boundary regions sealed by the hard mask, the porous region structure of the present invention is made compatible with subsequent processes involving the use of halogen-based precursors or processes that may result in corrosion of the exposed regions of the first metal layer. In an embodiment, the hard mask is also made of a material that is substantially resistant to halogen corrosion to provide further protection against this type of corrosion.

[0080] In an embodiment, the porous region structure may further include a second metal layer below the first metal layer, wherein the non-transverse pores of the porous region extend through the porous region to open onto the second metal layer. The second metal layer may be used to provide electrical contact with the structure deposited in the non-transverse pores of the porous region. For example, where the layered structure is deposited in the non-transverse pores, the conductive layer of the layered structure may be in electrical contact with the second metal through the non-transverse pores. The second metal layer may also be made of a metal that is resistant to halogen corrosion, thereby increasing the compatibility of the porous region structure with subsequent processes involving the use of halogen-based precursors.

[0081] In an embodiment, the porous region structure may further include an electronic component formed on the substrate and electrically connected to the second metal layer. Therefore, the device formed in the porous region may be connected to another electronic component on the substrate to obtain a functional module.

[0082] In embodiments, the substrate may be made of silicon, glass, or a polymer.The substrate may be a raw substrate (ie, unprocessed) or processed by forming other electronic components thereon.

[0083] In an embodiment, the anodized hard mask may be partially or completely removed (e.g., using selective etching) before the hard mask is deposited. This may have several benefits. For example, during anodization, the anodized hard mask may break at the edges of the porous region due to the expansion of the PAA. Removing the anodized hard mask allows any broken areas of the anodized hard mask to be removed, which is conducive to better deposition of the hard mask. The resulting structure is improved from both a surface and robustness perspective (in the case of complete removal of the anodized hard mask, the possibility of anodized hard mask breakage is reduced or eliminated). By removing the anodized hard mask, subsequent process steps (e.g., metallization or photoresist spin coating) are also simplified. In fact, during anodization, the edge of the anodized hard mask is pushed upward by the expanded PAA. This creates a vertical topology that can reach several microns compared to a flat reference surface. Typically, the vertical topology also has a flange toward the PAA side. Whenever a subsequent process step needs to cover the flange to maintain the continuity of a layer deposited across the flange, for example, this complicates subsequent process steps (including the deposition of the hard mask). The removal of the anodized hard mask eliminates this vertical topology and ledges, reducing limitations in step coverage and the risk of having discontinuous layers.

[0084] Other variants

[0085] Although the invention has been described above with reference to certain specific embodiments, it will be appreciated that the invention is not limited to the characteristics of the specific embodiments. Many variations, modifications and developments are possible in the embodiments described above within the scope of the appended claims.

Claims

1. A porous region structure for electronic products, comprising: substrate; a first metal layer over the substrate; a porous region comprised of an anodized portion of the first metal layer, the porous region comprising an anodic oxide having a plurality of pores extending from a top surface of the porous region toward the substrate; as well as A hard mask is provided over the first metal layer and the porous region, the hard mask having openings over defined areas of the porous region, configured such that the hard mask covers lateral holes in the plurality of holes in the porous region.

2. The porous area structure according to claim 1, further comprising: an anodized hard mask on top of the first metal layer, the anodized hard mask having openings above the anodized regions of the porous region, The distance between the edge of the anodized region and the corresponding edge of the defined region is related to the thickness of the portion of the first metal layer that is anodized to form the porous region.

3. The porous area structure according to claim 2, wherein: The distance ranges from 100 nanometers to 50 micrometers.

4. The porous domain structure according to any one of claims 2 to 3, wherein: The transverse pores fall within the anodized region but outside the defined area of ​​the porous region.

5. The porous area structure according to any one of claims 1 to 3, further comprising: A second metal layer is below the first metal layer, wherein non-lateral holes in the plurality of holes extend through the porous region to open onto the second metal layer.

6. The porous area structure according to claim 5, wherein: The second metal layer is made of tungsten or titanium.

7. The porous area structure according to claim 5, further comprising: An electronic component, formed on the substrate, is electrically connected to the second metal layer.

8. The porous area structure according to claim 5, further comprising: A layered structure is deposited on top of the hard mask, the layered structure being embedded in the plurality of holes in the porous region excluding the lateral holes.

9. The porous area structure according to claim 8, wherein: The layered structure includes a conductive layer that is in electrical contact with the second metal layer through the non-transverse hole.

10. The porous area structure according to claim 8, wherein: The layered structure includes a metal-insulator-metal (MIM) stack.

11. The porous domain structure according to any one of claims 1 to 3, wherein: The hard mask is made of tungsten or titanium.

12. The porous domain structure according to any one of claims 1 to 3, wherein: The substrate is made of silicon, glass, or polymer.

13. The porous domain structure according to any one of claims 1 to 3, wherein: The substrate is an unprocessed substrate.

14. A capacitive component comprising a porous area structure according to any one of claims 1 to 13.

15. A method for manufacturing a porous area structure for an electronic product, comprising: depositing a first metal layer over the substrate; depositing an anodized hard mask on top of the first metal layer, the anodized hard mask having openings over anodized regions of the first metal layer; anodizing the first metal layer to form a porous region in the first metal layer, the porous region being below the anodized region of the first metal layer; depositing a hard mask on top of the porous region, the hard mask having an opening over a defined area of ​​the porous region, the defined area being smaller than and included within the anodized region; as well as A layered structure is deposited on top of the hard mask and the porous region to embed the layered structure into the porous region over the defined area of ​​the porous region.

16. The method according to claim 15, further comprising: Prior to depositing the hard mask, the anodized hard mask is selectively etched.