A rewiring wafer-level packaging structure and preparation method thereof
By treating the rewiring metal layer of copper material on the surface of the passivation layer, the organic insulation layer is abolished, and the problems of high packaging costs and insufficient current bearing capacity in the prior art are solved, thereby achieving lower cost and higher current bearing crystals Circular-level packaging structure.
Patent Information
- Application Number
- CN202011133674.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-10-21
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2040-10-21
AI Technical Summary
The existing wafer-level packaging structure uses two layers of metal and two layers of organic insulation, resulting in high packaging costs and limited unsuitable range, making it difficult to meet the needs of high-density and high-current devices.
By using CMP process on the passivation layer surface, the first rewiring metal layer is directly formed, the organic insulation layer on the passivation layer surface is eliminated, and the rewiring structure is constructed using multi-layer copper material to increase the thickness of the metal interconnect layer to increase the thickness of the metal interconnect layer to increase the Current carrying capacity.
It reduces packaging costs, improves the current carrying capacity of wafer-level packaging structures, reduces power loss, avoids chip warping problems, and meets the requirements of large-current devices.
Smart Images

Figure CN112185927B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor manufacturing technology, and more particularly to a rewiring wafer-level packaging structure and a preparation method thereof. Background Art
[0002] With the development of semiconductor technology and the drive of the consumer electronics market, packaging technology is developing towards lighter, thinner, smaller, and better electrical and thermal performance. The chip packaging process has also changed from chip-by-chip packaging to wafer-level packaging. Wafer-level packaging, referred to as wafer-level chip packaging (Wafer Level Chip Scale Packaging, WLCSP), has gradually become one of the most advanced and important packaging forms because of its high density, small size, high reliability, and excellent electrical and thermal performance, and meets the development requirements of packaging technology.
[0003] In order to make the chip suitable for different packaging forms, the existing wafer-level packaging structure uses rewiring technology to change the contact position of the chip circuit. At present, the rewiring layer of the wafer-level packaging structure is mainly a 2P2M structure, such as Figure 1 As shown, the rewiring wafer-level packaging structure includes a substrate 11, a metal interconnection layer 12 located on the substrate 11, a passivation layer 13, a first organic insulating layer 14, a first rewiring metal layer 15, a second organic insulating layer 16, a second rewiring metal layer 17 and solder balls 18, wherein the metal interconnection layer 12 includes a sub-top metal interconnection layer and a top metal interconnection layer sequentially located on the substrate 11. However, since the rewiring wafer-level packaging structure uses two metal layers and two organic insulating layers for rewiring, it will affect the scope of application on the one hand, and will also lead to a higher packaging cost of the packaging structure on the other hand. Summary of the invention
[0004] In view of this, the present invention provides a rewiring wafer-level packaging structure and a preparation method thereof, so as to reduce the packaging cost of the existing rewiring wafer-level packaging structure.
[0005] To achieve the above object, the present invention provides the following technical solutions:
[0006] A rewiring wafer-level packaging structure, comprising:
[0007] A substrate, wherein a plurality of chips to be packaged are integrated in the substrate, and a plurality of lead electrodes are provided on the surface of the substrate, wherein the lead electrodes are electrically connected to the corresponding chips to be packaged;
[0008] a passivation layer located on the surface of the substrate, wherein a portion of the passivation layer covering the lead-out electrode has a first opening, wherein the first opening exposes the lead-out electrode, and the surface of the passivation layer is a surface processed by a CMP process;
[0009] a first rewiring metal layer located on a surface of the passivation layer, wherein the first rewiring metal layer is electrically connected to the lead-out electrode through the first opening;
[0010] A first organic insulating layer located on a surface of the first rewiring metal layer, the first organic insulating layer having a second opening, and the second opening exposing the first rewiring metal layer;
[0011] A second rewiring metal layer is located on a surface of the first organic insulating layer, and the second rewiring metal layer is electrically connected to the first rewiring metal layer through the second opening.
[0012] Optionally, a solder ball is further included, wherein the solder ball is fixed on the surface of the second rewiring metal layer and is electrically connected to the second rewiring metal layer.
[0013] Optionally, a portion of the passivation layer covering the lead-out electrode has a plurality of first openings, and the plurality of first openings are evenly arranged.
[0014] Optionally, the projection of the first opening on the substrate is in a square shape;
[0015] The shortest side length of the square is 2um to 3um.
[0016] Optionally, the resistivity of the material of the first rewiring metal layer is smaller than the resistivity of aluminum material.
[0017] Optionally, the material of the first rewiring metal layer is copper;
[0018] The material of the second rewiring metal layer is copper.
[0019] Optionally, the extraction electrode includes one or more top metal interconnection layers.
[0020] Optionally, the material of the second top metal interconnection layer is aluminum.
[0021] A method for preparing a rewiring wafer-level packaging structure, comprising:
[0022] Providing a substrate, wherein a plurality of chips to be packaged are integrated in the substrate, and a plurality of lead electrodes are provided on the surface of the substrate, wherein the lead electrodes are electrically connected to the corresponding chips to be packaged;
[0023] forming a passivation layer on the surface of the substrate, treating the surface of the passivation layer by a CMP process, and forming a first opening at a portion of the passivation layer covering the lead-out electrode, wherein the first opening exposes the lead-out electrode;
[0024] forming a first rewiring metal layer on the surface of the passivation layer, wherein the first rewiring metal layer is electrically connected to the lead-out electrode through the first opening;
[0025] forming a first organic insulating layer on the surface of the first rewiring metal layer, and forming a second opening on the first organic insulating layer, wherein the second opening exposes the first rewiring metal layer;
[0026] A second rewiring metal layer is formed on the surface of the first organic insulating layer, and the second rewiring metal layer is electrically connected to the first rewiring metal layer through the second opening.
[0027] Optionally, it also includes:
[0028] A solder ball is fixed on the surface of the second rewiring metal layer, and the solder ball is electrically connected to the second rewiring metal layer.
[0029] Optionally, forming a first opening at a portion of the passivation layer covering the extraction electrode comprises:
[0030] A plurality of uniformly arranged first openings are formed in a portion of the passivation layer covering the extraction electrode.
[0031] Compared with the prior art, the technical solution provided by the present invention has the following advantages:
[0032] The rewiring wafer-level packaging structure and preparation method thereof provided by the present invention, since the surface of the passivation layer is a surface treated by a CMP process, a first rewiring metal layer can be directly formed on the surface of the passivation layer, thereby eliminating the organic insulating layer on the surface of the passivation layer, thereby saving materials and reducing packaging costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying creative work.
[0034] Figure 1 A schematic diagram of a cross-sectional structure of a chip in an existing rewiring wafer-level packaging structure;
[0035] Figure 2 A schematic cross-sectional structure diagram of a chip to be packaged in a rewiring wafer-level packaging structure provided by an embodiment of the present invention;
[0036] Figure 3 A flow chart of a method for preparing a rewiring wafer-level packaging structure provided by one embodiment of the present invention;
[0037] Figures 4 to 7 A schematic diagram of the cross-sectional structure of various parts of a chip to be packaged in a rewiring wafer-level packaging structure during the preparation process provided by an embodiment of the present invention. DETAILED DESCRIPTION
[0038] The above is the core idea of the present invention. In order to make the above-mentioned purposes, features and advantages of the present invention more obvious and easy to understand, the technical solutions in the embodiments of the present invention will be clearly and completely described below in combination with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0039] The embodiment of the present invention provides a rewiring wafer-level packaging structure, such as Figure 2 As shown, including:
[0040] The substrate 21 has multiple chips to be packaged integrated therein, and the surface of the substrate 21 has multiple lead electrodes 22, which are electrically connected to the corresponding chips to be packaged and are used to achieve electrical connection between the chips to be packaged and external circuits. It should be noted that: Figure 2 In this paper, only one chip to be packaged is used as an example to illustrate, that is, Figure 2 The figure shows a schematic cross-sectional structure of a chip to be packaged. The structures of other chips to be packaged are the same or similar to this, and will not be repeated here. Optionally, the substrate 21 is a silicon wafer. The passivation layer 23 located on the surface of the substrate 21, the portion of the passivation layer 23 covering the lead-out electrode 22 has a plurality of first openings 230, and the first openings 230 expose the lead-out electrode 22. In other words, the passivation layer 23 covers the substrate 21 and the lead-out electrode 22 on the surface of the substrate 21, and the passivation layer 23 covering the lead-out electrode 22 has a plurality of first openings 230, so as to expose the lead-out electrode 22 covered by the passivation layer 23 through the first openings 230. In addition, the surface of the passivation layer 23 is a flat surface treated by a CMP (Chemical Mechanical Polishing) process.
[0041] The first rewiring metal layer 24 is located on the surface of the passivation layer 23, and the first rewiring metal layer 24 is electrically connected to the extraction electrode 22 through the first opening 230. That is, the first rewiring metal layer 24 is formed on the surface of the passivation layer 23, and the material of the first rewiring metal layer 24 fills the first opening 230 on the passivation layer 23, based on which the first rewiring metal layer 24 can be electrically connected to the extraction electrode 22 through the first opening 230.
[0042] The first organic insulating layer 25 is located on the surface of the first rewiring metal layer 24. In some embodiments, the first organic insulating layer 25 covers the surface and surrounding sides of the first rewiring metal layer 24. Of course, the present invention is not limited thereto. In other embodiments, the first organic insulating layer 25 may only cover the surface of the first rewiring metal layer 24. In addition, the first organic insulating layer 25 has a second opening 250. The second opening 250 exposes the first rewiring metal layer 24 at the bottom of the first organic insulating layer 25.
[0043] The second rewiring metal layer 26 is located on the surface of the first organic insulating layer 25, and the second rewiring metal layer 26 is electrically connected to the first rewiring metal layer 24 through the second opening 250. In some embodiments of the present invention, the second rewiring metal layer 26 is only located in the second opening 250, but the present invention is not limited thereto. In other embodiments, the second rewiring metal layer 26 is formed on the surface of the first organic insulating layer 25, and the material of the second rewiring metal layer 26 fills the second opening 250 on the first organic insulating layer 25, so that the second rewiring metal layer 26 is electrically connected to the first rewiring metal layer 24 through the second opening 250.
[0044] Optionally, the projection of the second opening 250 on the substrate 21 does not overlap with the projection of the first opening 230 on the substrate 21. Of course, the present invention is not limited to this. In other embodiments, the projection of the second opening 250 on the substrate 21 may partially overlap with the projection of the first opening 230 on the substrate 21.
[0045] and Figure 1 Compared with the structure shown in FIG. 1 , the passivation layer 23 in the embodiment of the present invention not only covers the surface of the substrate 21, but also Figure 2 As shown, the passivation layer 23 also covers the surface of the lead-out electrode 22, and the portion of the passivation layer 23 covering the lead-out electrode 22 has a first opening 230, and since the surface of the passivation layer 23 is a surface treated by a CMP process, a first rewiring metal layer 24 can be formed directly on the surface of the passivation layer 23, that is, the passivation layer 23 can replace the organic insulating layer to provide a smooth surface and realize the insulation of the first rewiring metal layer 24 and the area outside the lead-out electrode 22, so that the organic insulating layer on the surface of the passivation layer 23 can be eliminated, thereby saving materials and reducing packaging costs.
[0046] also, Figure 1 The maximum current that the wafer-level packaging structure shown can carry is 4A. If a large current of more than 4A is required, the thickness of the top metal interconnect layer in the metal interconnect layer 12 and the thickness of the first rewiring metal layer 15 need to be increased in theory. However, the inventors have found that since the material of the top metal interconnect layer is aluminum, and the resistivity of aluminum is too large, increasing the thickness of the top metal interconnect layer will cause the wafer-level packaging structure to generate more heat when carrying a large current, resulting in greater power loss and a smaller output current. In addition, Figure 1 The maximum thickness of the first rewiring metal layer 15 of the wafer-level packaging structure shown is about 9 um. If the thickness of the first rewiring metal layer 15 is further increased, the chip will be warped, affecting the performance of the wafer-level packaging structure. That is, increasing the thickness of the top metal interconnect layer and the thickness of the first rewiring metal layer 15 cannot effectively increase the current that the wafer-level packaging structure can carry.
[0047] Based on this, in some embodiments of the present invention, the lead-out electrode 22 only includes one or more layers of top-level metal interconnection layers, that is, the lead-out electrode 22 does not include the top-level metal interconnection layer located on top of the sub-top-level metal interconnection layer, that is, the top-level metal interconnection layer is cancelled in the embodiments of the present invention, and, in the embodiments of the present invention, the first rewiring metal layer 24 is used as the top-level metal interconnection layer, which can not only further save materials and reduce packaging costs, but also eliminate the heat generated by the top-level metal interconnection layer during current transmission, thereby reducing power loss, so that the wafer-level packaging structure can carry a larger current, that is, the current that the wafer-level packaging structure can carry can be increased so that it can meet the requirements of high-current devices.
[0048] It should also be noted that, compared with the prior art, the thickness of the first rewiring metal layer 24 needs to be increased in the embodiment of the present invention so that the first rewiring metal layer 24 can play a protective role for the top metal interconnect layer, and can further increase the current that the wafer-level packaging structure can carry. In addition, the thickness of the first rewiring metal layer 24 will not exceed 9um, preferably 9um, so there will be no problem of chip warping.
[0049] Optionally, in some embodiments of the present invention, the resistivity of the material of the first rewiring metal layer 24 is lower than that of aluminum material. Based on this, the first rewiring metal layer 24 generates less heat and loses less power, thereby further increasing the current that the wafer-level packaging structure can carry.
[0050] Optionally, in some embodiments of the present invention, the material of the first rewiring metal layer 24 is copper. Since the resistivity of copper is (1.75×10 -8Ω·m) is lower than the resistivity of aluminum (2.83X10 -8 Ω·m), and the thickness of the first rewiring metal layer 24 (generally 9um) is greater than the thickness of the top metal interconnect layer in the prior art (generally 3.4um), so the current carrying capacity of the wafer-level packaging structure can be increased. Further optionally, in some embodiments of the present invention, the material of the second top metal interconnect layer is aluminum, and the material of the second rewiring metal layer 26 is copper, so as to further increase the current carrying capacity of the wafer-level packaging structure.
[0051] In some embodiments of the present invention, Figure 2 As shown, the wafer-level packaging structure further includes solder balls 27, which are fixed on the surface of the second rewiring metal layer 26 and electrically connected to the second rewiring metal layer 26. Optionally, the solder balls 27 and the second openings 250 are arranged in a one-to-one correspondence.
[0052] In some embodiments of the present invention, Figure 2 As shown, the portion of the passivation layer 23 covering the extraction electrode 22 has a plurality of uniformly arranged first openings 230, that is, the first rewiring metal layer 24 can be electrically connected to the extraction electrode 22 through the plurality of first openings 230, thereby relieving the stress of the first rewiring metal layer 24 on the second top metal interconnection layer, that is, the extraction electrode 22. In some embodiments of the present invention, the projection of the first opening 230 on the substrate 21 is in the shape of a square, and the shortest side length of the square is 2um to 3um.
[0053] The embodiment of the present invention also provides a method for preparing a rewired wafer-level packaging structure, such as Figure 3 As shown, including:
[0054] S101: providing a substrate, wherein a plurality of chips to be packaged are integrated in the substrate, and a plurality of lead electrodes are provided on the surface of the substrate, wherein the lead electrodes are electrically connected to corresponding chips to be packaged;
[0055] like Figure 4 As shown, the substrate 21 can be a silicon wafer. After a series of processes are performed on the substrate 21, a plurality of chips to be packaged and lead electrodes 22 corresponding to the chips to be packaged can be formed on the substrate 21. The lead electrodes 22 are used to realize electrical connection between the chips to be packaged and external circuits.
[0056] It should be noted that the drawings of the embodiments of the present invention illustrate the cross-sectional structure of a chip to be packaged in a wafer-level packaging structure, and the structures of other chips to be packaged are the same or similar to this, which will not be described in detail here.
[0057] In some embodiments of the present invention, the lead-out electrode 22 includes only one or more layers of top metal interconnection layers, excluding the top metal interconnection layer, wherein the thickness of the sub-top metal interconnection layer is about 0.8 um. Based on this, the first rewiring metal layer 24 formed subsequently can be used as the top metal interconnection layer, thereby not only saving materials and reducing packaging costs, but also increasing the current that the wafer-level packaging structure can carry, so that it can meet the requirements of high-current devices.
[0058] S102: forming a passivation layer on the surface of the substrate, treating the surface of the passivation layer by a CMP process, and forming a first opening in a portion of the passivation layer covering the lead-out electrode, wherein the first opening exposes the lead-out electrode;
[0059] like Figure 4 As shown, a passivation layer 23 is formed on the surface of the substrate 21, and the passivation layer 23 covers the substrate 21 and the lead-out electrode 22 on the surface of the substrate 21. The surface of the passivation layer 23 is processed by a CMP process to form a flat surface, and then a first opening 230 is formed in the portion of the passivation layer 23 covering the lead-out electrode 22, and the first opening 230 exposes the lead-out electrode 22 at the bottom of the passivation layer 23.
[0060] Since the surface of the passivation layer 23 is processed by the CMP process, the first rewiring metal layer 24 can be directly formed on the surface of the passivation layer 23, thereby eliminating the organic insulating layer on the surface of the passivation layer 23, thereby further saving materials and reducing packaging costs.
[0061] In some embodiments of the present invention, forming a first opening 230 exposing the lead-out electrode 22 at a portion of the passivation layer 23 covering the lead-out electrode 22 includes:
[0062] A plurality of uniformly arranged first openings 230 are formed in the portion of the passivation layer 23 covering the extraction electrode 22 .
[0063] Since the first rewiring metal layer 24 formed subsequently can be electrically connected to the extraction electrode 22 through the plurality of first openings 230, the stress of the first rewiring metal layer 24 on the next top metal interconnect layer, i.e., the extraction electrode 22, can be relieved. In some embodiments of the present invention, the projection of the first opening 230 on the substrate 21 is in the shape of a square, and the shortest side length of the square is 2um to 3um.
[0064] S103: forming a first rewiring metal layer on the surface of the passivation layer, wherein the first rewiring metal layer is electrically connected to the lead-out electrode through the first opening;
[0065] Optionally, the first rewiring metal layer 24 includes a titanium tungsten seed layer and a copper seed layer located on the surface of the passivation layer 23, and an electroplated copper layer located on the surface of the seed layer. Figure 5As shown, a first rewiring metal layer 24 is formed on the surface of the passivation layer 23 , and the material of the first rewiring metal layer 24 fills the first opening 230 on the passivation layer 23 , so that the first rewiring metal layer 24 is electrically connected to the extraction electrode 22 through the first opening 230 .
[0066] The specific process of forming the first rewiring metal layer 24 on the surface of the passivation layer 23 is as follows: a titanium tungsten seed layer and a copper seed layer are sputtered on the surface of the passivation layer 23, each with a thickness of 0.2 um, and then a layer of photoresist is coated on the surface of the seed layer, and a pattern to be electroplated is photoetched, and then the first rewiring metal layer 24 is electroplated through an electroplating process. After the electroplating is completed, the surface photoresist is dissolved with an organic solvent, and the seed layer outside the electroplating area is removed.
[0067] S104: forming a first organic insulating layer on the surface of the first rewiring metal layer, and forming a second opening on the first organic insulating layer, wherein the second opening exposes the first rewiring metal layer;
[0068] Optionally, in some embodiments of the present invention, the first organic insulating layer 25 is a photoresist layer. Figure 6 As shown, a first organic insulating layer 25 is formed on the surface of the first rewiring metal layer 24. The specific process is: a layer of photoresist is coated on the surface of the first rewiring metal layer 24, and then a pattern of the second opening 250 is developed on the surface of the first rewiring metal layer 24 through photolithography technology. After high-temperature baking, an organic insulating anti-etching layer having the second opening 250, namely the first organic insulating layer 25, is formed, wherein the second opening 250 exposes the first rewiring metal layer 24 at the bottom of the first organic insulating layer 25.
[0069] Optionally, the projection of the second opening 250 on the substrate 21 does not overlap with the projection of the first opening 230 on the substrate 21. Of course, the present invention is not limited to this. In other embodiments, the projection of the second opening 250 on the substrate 21 may partially overlap with the projection of the first opening 230 on the substrate 21.
[0070] S105: forming a second rewiring metal layer on the surface of the first organic insulating layer, wherein the second rewiring metal layer is electrically connected to the first rewiring metal layer through the second opening.
[0071] like Figure 7As shown, a second rewiring metal layer 26 is formed on the surface of the first organic insulating layer 25. The formation process of the second rewiring metal layer 26 is the same as that of the first rewiring metal layer 24, that is, a titanium tungsten seed layer and a copper seed layer are sputtered first, and then a layer of photoresist is coated on the surface of the seed layer, and a pattern to be electroplated is photoetched, and then the second rewiring metal layer 26 is electroplated by an electroplating process. After the electroplating is completed, the surface photoresist is dissolved with an organic solvent, and the seed layer outside the electroplating area is removed.
[0072] The method for preparing the wafer-level packaging structure provided by the embodiment of the present invention further includes:
[0073] The solder ball 27 is fixed on the surface of the second rewiring metal layer 26, and the solder ball 27 is electrically connected to the second rewiring metal layer 26. Figure 2 shown.
[0074] Specifically, the soldering flux can be first applied to the surface of the substrate 21 using a screen, wherein the screen is a tool for printing the soldering flux, and the opening positions of the soldering flux screen correspond to the positions of the second openings 250. After that, the solder ball 27 is printed on the surface of the second rewiring metal layer 26 at the second opening 250 using a screen, and then reflow soldering is performed at a temperature of 220°C to 250°C to solder and fix the solder ball 27 to the second rewiring metal layer 26. The soldering flux is cleaned off and completed. Figure 2 Wafer level packaging shown.
[0075] In this specification, each embodiment is described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the embodiments can be referred to each other. For the device disclosed in the embodiment, since it corresponds to the method disclosed in the embodiment, the description is relatively simple, and the relevant parts can be referred to the method part.
[0076] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.
Claims
1. A rewiring wafer-level packaging structure, characterized in that: include: A substrate, wherein a plurality of chips to be packaged are integrated in the substrate, and a plurality of lead electrodes are provided on the surface of the substrate, wherein the lead electrodes are electrically connected to the corresponding chips to be packaged; a passivation layer located on the surface of the substrate, wherein a portion of the passivation layer covering the lead-out electrode has a first opening, wherein the first opening exposes the lead-out electrode, and the surface of the passivation layer is a surface processed by a CMP process; a first rewiring metal layer located on the surface of the passivation layer, the first rewiring metal layer being electrically connected to the lead-out electrode through the first opening, a portion of the passivation layer covering the lead-out electrode having a plurality of first openings, and the plurality of first openings being evenly arranged; A first organic insulating layer located on a surface of the first rewiring metal layer, the first organic insulating layer having a second opening, and the second opening exposing the first rewiring metal layer; a second rewiring metal layer located on a surface of the first organic insulating layer, the second rewiring metal layer being electrically connected to the first rewiring metal layer through the second opening; The invention also includes a solder ball, which is fixed on the surface of the second rewiring metal layer and is electrically connected to the second rewiring metal layer.
2. The wafer-level packaging structure according to claim 1, characterized in that: The projection of the first opening on the substrate is in a square shape; The shortest side length of the square is 2um to 3um.
3. The wafer-level packaging structure according to claim 1, characterized in that: The resistivity of the material of the first rewiring metal layer is lower than that of the aluminum material.
4. The wafer-level packaging structure according to claim 3, characterized in that: The material of the first rewiring metal layer is copper; The material of the second rewiring metal layer is copper.
5. The wafer-level packaging structure according to claim 1, characterized in that: The extraction electrode includes one or more top metal interconnection layers.
6. The wafer-level packaging structure according to claim 5, characterized in that: The material of the second top metal interconnection layer is aluminum.
7. A method for preparing a rewired wafer-level packaging structure, characterized in that: include: Providing a substrate, wherein a plurality of chips to be packaged are integrated in the substrate, and a plurality of lead electrodes are provided on the surface of the substrate, wherein the lead electrodes are electrically connected to the corresponding chips to be packaged; forming a passivation layer on the surface of the substrate, treating the surface of the passivation layer by a CMP process, and forming a first opening at a portion of the passivation layer covering the lead-out electrode, wherein the first opening exposes the lead-out electrode; forming a first rewiring metal layer on the surface of the passivation layer, wherein the first rewiring metal layer is electrically connected to the lead-out electrode through the first opening; forming a first organic insulating layer on the surface of the first rewiring metal layer, and forming a second opening on the first organic insulating layer, wherein the second opening exposes the first rewiring metal layer; forming a second rewiring metal layer on the surface of the first organic insulating layer, wherein the second rewiring metal layer is electrically connected to the first rewiring metal layer through the second opening; Fixing a solder ball on the surface of the second rewiring metal layer, and electrically connecting the solder ball to the second rewiring metal layer; Forming a first opening at a portion of the passivation layer covering the extraction electrode comprises: A plurality of uniformly arranged first openings are formed in a portion of the passivation layer covering the extraction electrode.
Citation Information
Patent Citations
Wafer level packaging structure with rewiring
CN212874486U