Semiconductor device and method for manufacturing trench gate structure thereof

By forming and etching the sacrificial layer to fill the recessed structure in the semiconductor device, the poor contact problems caused by the recessed structure in the trench gate structure are solved, device performance is improved and manufacturing difficulty and cost are reduced.

CN112542387BActive Publication Date: 2024-11-26BEIJING YANDONG MICROELECTRONICS TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011416328.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-12-04
Publication Date
2024-11-26
Estimated Expiration
2040-12-04

AI Technical Summary

Technical Problem

In semiconductor devices, during the manufacturing process of the trench gate structure, the recessed structure causes difficulty in effective contact between the contact plug and the gate conductor layer, affecting device performance, and the existing processes increase manufacturing difficulty and cost.

Method used

A sacrificial layer is formed on the surface of the semiconductor structure, a portion of the recessed structure is filled, and the sacrificial layer and the gate conductor layer are synchronized to planarize the surface, control the etching rate and selection ratio, and eliminate V-type Recess.

Benefits of technology

It effectively eliminates V-shaped Recess, improves the quality of the trench gate structure, reduces manufacturing difficulty and cost, ensures the performance of semiconductor devices, and has high process flexibility, and is suitable for a variety of devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112542387B_ABST
    Figure CN112542387B_ABST
Patent Text Reader

Abstract

The present application discloses a semiconductor device and a method for manufacturing a trench gate structure thereof, wherein the method for manufacturing the trench gate structure comprises: forming a sacrificial layer on the surface of a semiconductor structure, wherein the semiconductor structure comprises a semiconductor layer, a trench in the semiconductor layer, a gate conductor layer covering the semiconductor layer and filling the trench, and the surface of the gate conductor layer corresponding to the trench has a recessed structure, and the sacrificial layer at least fills a portion of the recessed structure; and synchronously etching the sacrificial layer and the gate conductor layer to flatten the surface of the gate conductor layer. The method for manufacturing the trench gate structure reduces the manufacturing difficulty and manufacturing cost of the trench gate structure while ensuring that the trench gate structure of the semiconductor device has a high quality.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor device manufacturing, and more specifically, to a semiconductor device and a method for manufacturing a trench gate structure thereof. Background Art

[0002] In semiconductor devices, especially in power devices such as vertical double-diffused metal oxide semiconductor field effect transistor (VDMOS) and insulated gate bipolar transistor (IGBT), the use of trench gate structure can improve the utilization of device planar area, so as to obtain a larger device unit channel width and current density per unit area, thereby obtaining a greater current conduction capability. Therefore, the quality of the trench gate structure plays a vital role in the performance of semiconductor devices.

[0003] At present, the manufacturing process of the trench gate structure generally includes: etching the semiconductor layer to form a trench, forming a gate dielectric layer on the inner sidewall of the trench, depositing process materials such as polysilicon in the trench and on the surface of the semiconductor layer and etching back to form a gate conductor layer. After the trench gate structure is formed, it is generally necessary to form an insulating layer (or an interlayer dielectric layer) on the surface of the semiconductor layer, open a contact hole corresponding to the trench in the insulating layer, and fill the contact hole with a conductive material such as a metal, thereby forming a contact plug that is electrically in contact with the gate conductor layer.

[0004] In the process of manufacturing the trench gate structure, a chemical vapor deposition (CVD) process is generally used to deposit process materials, such as polysilicon, on the surface of the semiconductor layer and in the trench. As the deposited process material becomes thicker, the gate conductor layer at the sidewall of the trench gradually closes toward the middle. Figure 1a and Figure 1b The effects of depositing gate conductor layers of different thicknesses are shown. Figure 1a As shown in FIG. 1 , if the thickness d of the process material deposited on the surface of the semiconductor layer 101 is less than half of the maximum width D of the trench 111, the gate conductor layer 113 at the sidewall of the trench 111 cannot be completely closed, and the trench 111 cannot be completely filled. If the deposition thickness d is greater than or equal to half of the maximum width D of the trench 111 (ignoring the thickness of the gate dielectric layer 112), although the trench 111 can be filled, a conical recessed structure 113a will be formed at the closed position of the gate conductor layer 113 in the middle of the trench 111, which is V-shaped in the cross-sectional view, and is generally referred to as a V-shaped recess in the industry, such as Figure 1bAnd generally, the wider the trench 111 is, the deeper the depth h1 of the recessed structure 113a is.

[0005] like Figure 1c As shown, if the initial morphology of the gate conductor layer 113 is not interfered, the recessed structure 113a will be transferred into the trench 111 in the subsequent etching back process, and the depth h2 of the recessed structure 113a may even be greater than the depth h1 before etching back.

[0006] like Figure 1d As shown, since the recessed structure 113a in the trench 111 is too deep, the isolation layer 102 corresponding to the trench 111 in the subsequently formed isolation layer 102 is too thick, so that the contact plug 120 cannot completely pass through the isolation layer 102, thereby affecting the effective contact between the contact plug 120 and the gate conductor layer 113, resulting in a decrease in device performance; in severe cases, the contact plug 120 is even insulated from the gate conductor layer 113, ultimately causing device failure. Figure 1e That is, a SEM photograph showing that the recessed structure is directly transferred into the groove, wherein the depth of the recessed structure 113a in the groove is about 930±150nm. Figure 1f 1 is a SEM photograph showing poor contact between the contact plug and the gate conductor layer, wherein the contact plug 120 fails to make sufficient contact with the gate conductor layer 113 in the trench, resulting in device failure.

[0007] Therefore, it is expected to improve the manufacturing process of the trench gate structure to eliminate the adverse effects caused by the V-shaped recess, thereby improving the quality of the trench gate structure and further improving the quality of semiconductor devices. Summary of the invention

[0008] In view of this, the present invention provides a semiconductor device and a method for manufacturing a trench gate structure thereof, which can reduce the manufacturing difficulty and manufacturing cost of the trench gate structure while ensuring that the trench gate structure of the semiconductor device has a high quality.

[0009] According to one aspect of an embodiment of the present invention, a method for manufacturing a trench gate structure is provided, comprising the following steps:

[0010] Forming a sacrificial layer on the surface of a semiconductor structure, wherein the semiconductor structure includes a semiconductor layer, a groove in the semiconductor layer, and a gate conductor layer covering the semiconductor layer and filling the groove, and a surface of the gate conductor layer corresponding to the groove has a recessed structure, and the sacrificial layer fills at least a portion of the recessed structure;

[0011] The sacrificial layer and the gate conductor layer are etched synchronously to planarize the surface of the gate conductor layer.

[0012] Optionally, the step of forming the sacrificial layer includes: coating a fluid material on the surface of the semiconductor structure, and allowing the fluid material to flow into the recessed structure to form the sacrificial layer.

[0013] Optionally, the fluid material is selected from at least one of the following materials: photoresist, silicate glass, spin-on glass, ethyl silicate, and an anti-reflective coating composition.

[0014] Optionally, the step of forming the sacrificial layer further includes: solidifying the fluid material.

[0015] Optionally, the thickness of the sacrificial layer located on the surface of the semiconductor layer is 80-120 nm.

[0016] Optionally, the thickness of the gate conductor layer is greater than or equal to half of the maximum width of the trench, and the difference between the thickness of the gate conductor layer and the maximum width of the trench does not exceed 100 nm.

[0017] Optionally, in the step of synchronously etching the sacrificial layer and the gate conductor layer, the etching rate of the sacrificial layer is controlled not to be greater than the etching rate of the gate conductor layer.

[0018] Optionally, an etching selection ratio between the sacrificial layer and the gate conductor layer is 0.8 to 0.9.

[0019] Optionally, the sacrificial layer only fills a portion of the recessed structure, and before the step of simultaneously etching the sacrificial layer and the gate conductor layer, the manufacturing method further comprises: etching the gate conductor layer until the remaining gate conductor layer is flush with the sacrificial layer.

[0020] According to another aspect of an embodiment of the present invention, a method for manufacturing a semiconductor device is provided, including the method for manufacturing the trench gate structure as described above.

[0021] According to the manufacturing method of the trench gate structure provided by the embodiment of the present invention, a sacrificial layer is filled at the recessed structure of the gate conductor layer to repair the surface of the gate conductor layer with the recessed structure, thereby obtaining a relatively flat surface, and then in the process of synchronously etching the gate conductor layer and the sacrificial layer, the repaired flat surface is etched at a relatively consistent rate as a whole, thereby effectively eliminating the V-shaped Recess, so that the trench gate structure of the semiconductor device has a higher quality and the performance of the semiconductor device is guaranteed. In addition, this manufacturing process is easy to implement and can reduce the manufacturing difficulty and manufacturing cost of the trench gate structure compared to using CMP.

[0022] Furthermore, by adjusting the thickness of the sacrificial layer, the etching selectivity, the thickness of the gate conductor layer and other conditions, flexible and effective control of the process is achieved, further eliminating the adverse effects of the V-shaped Recess on device performance. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings of the embodiments are briefly introduced below. Obviously, the drawings in the following description only relate to some embodiments of the present invention, but are not intended to limit the present invention.

[0024] Figure 1a to Figure 1d The invention shows cross-sectional views at some stages of a method for manufacturing a trench gate structure of a semiconductor device in the related art.

[0025] Figure 1e This is a SEM photograph of the recessed structure being directly transferred into the groove.

[0026] Figure 1f This is a SEM photo showing poor contact between the contact plug and the gate conductor layer.

[0027] Figure 1g A schematic diagram of a trench gate structure formed after the recessed structure is removed by a CMP process is shown.

[0028] Figure 2a to Figure 2d The cross-sectional views at some stages of a method for manufacturing a trench gate structure of a semiconductor device according to an embodiment of the present invention are shown.

[0029] Figure 3 This is a SEM photo after synchronous etching of the sacrificial layer and the gate conductor layer. DETAILED DESCRIPTION

[0030] The present invention will be described in more detail below with reference to the accompanying drawings. In each of the accompanying drawings, the same elements are represented by similar reference numerals. For the sake of clarity, the various parts in the accompanying drawings are not drawn to scale. In addition, some well-known parts may not be shown. For the sake of simplicity, the semiconductor structure obtained after several steps can be described in one figure.

[0031] refer to Figure 1g Combined with Figures 1a to 1f In order to reduce the adverse effects of the V-shaped recess on the device performance mentioned above, so that the contact plug 120 can completely pass through the isolation layer 102 to form an effective contact with the gate conductor layer 113, the solution commonly adopted at present is to deposit a thicker gate conductor layer 113 to fully fill the groove 111, and control the bottom of the recess structure 113a to be higher than the surface of the semiconductor layer 101, and then use a chemical mechanical polishing (CMP) process to grind the surface of the gate conductor layer 113 flat, so as to remove the recess structure 113a as much as possible, and then etch back the gate conductor layer 113, so that the morphology of the gate conductor layer 113 located in the groove 111 will be relatively smooth.

[0032] However, in addition to the CMP step, the above method also requires multiple processes such as deposition of a stop layer and post-CMP cleaning, which not only significantly increases the processing cost and time cost, but also the growth of a thicker gate conductor layer 113 will affect the production capacity and maintenance frequency of the diffusion furnace. Therefore, it is necessary to provide a new manufacturing process for a trench gate structure to effectively reduce the adverse effects of the V-type recess on device performance while reducing the manufacturing cost and difficulty.

[0033] Figure 2a to Figure 2d The cross-sectional views at some stages of a method for manufacturing a trench gate structure of a semiconductor device according to an embodiment of the present invention are shown.

[0034] like Figure 2a and Figure 2b As shown, the manufacturing process of the trench gate structure of the embodiment of the present invention includes: forming a sacrificial layer 202 on the surface of the semiconductor structure. The semiconductor structure includes: a semiconductor layer 201, a trench 211, a gate dielectric layer 212 and a gate conductor layer 213. The trench 211 is located in the semiconductor layer 201, the gate dielectric layer 212 is located on the surface of the semiconductor layer 201 and the inner surface of the trench 211, and the gate conductor layer 213 covers the gate dielectric layer 212 and fills the trench 211. Among them, the surface of the gate conductor layer 213 corresponding to the trench 211 has a recessed structure 213a.

[0035] In this embodiment, the semiconductor layer 201 can be specifically determined according to the semiconductor device to be manufactured. For example, the semiconductor layer 201 can be a single crystal or an epitaxial wafer, wherein the single crystal can be N-type doped or P-type doped, and the epitaxial wafer includes a single crystal and an epitaxial layer located on the surface of the single crystal. In addition, the semiconductor layer 201 can also have a doped region (body region), etc.

[0036] like Figure 2a As shown, the groove 211 is U-shaped, the top opening of the groove 211 is located on the surface of the semiconductor layer 201, the bottom of the groove 211 is located in the semiconductor layer 201, and the width of the groove 211 generally increases from the bottom to the top of the groove 211. The groove 211 can be obtained by anisotropic etching methods such as ion milling etching, plasma etching, reactive ion etching, laser ablation, etc., which is not particularly limited. In addition, according to different functions, grooves 211 of various shapes and sizes can be formed in the semiconductor layer 201. Generally speaking, as the width of the groove 211 increases, the corresponding recessed structure 213a is also deeper.

[0037] The material of the gate dielectric layer 212 can be, for example, an insulating material such as silicon dioxide or silicon nitride, and can be obtained by a thermal oxidation process or a chemical vapor deposition process. The material of the gate conductor layer 213 includes polysilicon, but the embodiment of the present invention is not limited thereto, and those skilled in the art can make other selections for the materials of the gate dielectric layer 212 and the gate conductor layer 213 as needed.

[0038] The sacrificial layer 202 at least fills a portion of the recessed structure 213a. Figure 2b As shown, the sacrificial layer 202 completely fills the recessed structure 213a and covers the surface of the semiconductor layer 101. That is, the surface of the sacrificial layer 202 is higher than the normal surface of the gate conductor layer 213 (the surface of the gate conductor layer 213 except the recessed structure 213a).

[0039] In the step of forming the sacrificial layer 202, a fluid material can be coated on the surface of the semiconductor structure so that the fluid material flows into the recessed structure 213a to form the sacrificial layer 202. In this embodiment, the fluid material is a material that has a certain fluidity at a certain temperature and can be removed by dry etching directly or after a simple treatment. For example, positive photoresist, negative photoresist, anti-reflective coating composition, ethyl silicate, silicate glass, spin-on glass (SOG). The silicate glass may include at least one of phosphosilicate glass (PSG), borosilicate glass (BSG) and borophosphosilicate glass (BPSG). By using the above-mentioned silicate glass, spin-on glass, and ethyl silicate as fluid materials, a sacrificial layer 202 with SiO2 as the main component can be formed; by using the anti-reflective coating composition as a fluid material, an anti-reflective coating as the sacrificial layer 202 can be obtained. Taking into account the material cost and the actual effect of filling the recessed structure 213a, a positive photoresist is generally selected.

[0040] In this step, for example, a spin coating process is used to coat the fluid material on the surface of the gate conductor layer 213, and the fluid material flows into the recessed structure 213a by utilizing its fluidity, thereby obtaining a relatively flat surface. In addition, the rotation speed, ambient temperature and other parameters during the spin coating process can be reasonably adjusted based on factors such as the viscosity of the fluid material, so as to obtain a sacrificial layer 202 with a relatively flat surface.

[0041] In some preferred embodiments, the fluid material can also be cured. For example, when the material of the sacrificial layer 202 is positive photoresist or negative photoresist, it can be cured by baking to remove small molecular compounds such as water, which is more conducive to the subsequent steps.

[0042] In this embodiment, the sacrificial layer 202 may also be slightly lower than the normal surface of the gate conductor layer 213, that is, the fluid-like material only fills a portion of the recessed structure 213a, and does not fill the recessed structure 213a; or, the surface of the sacrificial layer 202 may also be flush with the normal surface of the gate conductor layer 213, that is, the fluid-like material completely fills the recessed structure 213a and forms a relatively complete and flat surface with the gate conductor layer 213.

[0043] Reasonable control of the thickness of the sacrificial layer 202 is conducive to better reducing the adverse effects of the recessed structure 213a on device performance. In actual processes, it is found that when the surface of the sacrificial layer 202 is higher than the normal surface of the gate conductor layer 213, it is more conducive to eliminating the V-shaped Recess. And, generally speaking, the thicker the sacrificial layer 202, the better the planarization effect, but an overly thick sacrificial layer 202 will increase the etching time of subsequent steps. In the specific implementation process, the thickness of the sacrificial layer 202 is usually controlled to be 80 to 120 nm. Reference Figure 2b The thickness of the sacrificial layer 202 refers to the vertical distance L between the surface of the sacrificial layer 202 and the normal surface of the gate conductor layer 213 , or in other words, the thickness of the sacrificial layer 202 refers to the thickness of the sacrificial layer 202 located above the semiconductor layer 201 .

[0044] Furthermore, the sacrificial layer 202 and the gate conductor layer 213 are etched synchronously to planarize the surface of the gate conductor layer 213. Figure 2c shown.

[0045] In this step, if the surface of the sacrificial layer 202 formed in the previous step is flush with the surface of the gate conductor layer 213, or the surface of the sacrificial layer 202 is higher than the surface of the gate conductor layer 213, by selecting appropriate etching conditions, the etching selectivity of the sacrificial layer 202 and the gate conductor layer 213 is close to each other, so as to eliminate the recessed structure 213a as much as possible. Specifically, the corresponding etching selectivity can be achieved by adjusting the etching conditions such as the ratio of appropriate reaction gases. In some other embodiments, if the sacrificial layer 202 only fills a part of the recessed structure 213a, but does not fill the recessed structure 213a, it is necessary to etch the gate conductor layer 213 before the step of synchronously etching the sacrificial layer 202 and the gate conductor layer 213, until the remaining gate conductor layer 213 is flush or substantially flush with the sacrificial layer 202, and then the step of synchronously etching the sacrificial layer 202 and the gate conductor layer 213 is performed.

[0046] Theoretically, in the process of simultaneously etching the sacrificial layer 202 and the gate conductor layer 213, it is best to keep the etching rates of the sacrificial layer 202 and the gate conductor layer 213 close to or even the same. However, in the actual process, it is found that when the etching rate of the sacrificial layer 202 is controlled to be slightly lower than the etching rate of the gate conductor layer 213, the influence of the recessed structure 213a can be eliminated to a greater extent. It is speculated that after the large area of ​​the sacrificial layer 202 is etched away, only a small amount of the sacrificial layer 202 remains in the recessed structure 213a, and the large area of ​​the gate conductor layer 213 is exposed, which changes the etching reaction and accelerates the etching of the remaining sacrificial layer 202. Considering the deposition principle of the gate conductor layer 213, the etching rate of the gate conductor layer 213 at the opening closed position (at the recessed structure 213a) is slightly faster than that at other positions. Therefore, it is best to control the etching rate of the sacrificial layer 202 to be slightly lower than the etching rate of the gate conductor layer 213. In a specific implementation process, when the etching selectivity ratio of the sacrificial layer 202 to the gate conductor layer 213 is controlled between 0.8 and 0.9, the V-shaped Recess can be effectively eliminated, and a gate conductor layer 213 with a relatively flat surface can be obtained, thereby meeting the device process requirements.

[0047] In addition, the deposition thickness of the gate conductor layer 213 will also affect the depth of the recessed structure 213a, thereby affecting the subsequent planarization effect. Generally speaking, as long as the deposition thickness of the gate conductor layer 213 is equal to or greater than half of the maximum width of the groove 211 (excluding the gate dielectric layer 212), the groove 211 can be filled. The thicker the gate conductor layer 213, the smoother the surface obtained, that is, the shallower the recessed structure 213a, but it will increase the subsequent etching time. In the specific implementation process, the deposition thickness of the gate conductor layer 213 is generally controlled to be D max To D max +100nm, where D max is half of the maximum width of the groove 211. Of course, when there are multiple grooves 211, D max is the maximum width of the largest groove.

[0048] The step of simultaneously etching the sacrificial layer 202 and the gate conductor layer 213 may be stopped when the etching reaches the bottom of the recessed structure 213a. Then, the gate conductor layer 213 located above the semiconductor layer 201 may be further removed, and at least a portion of the gate conductor layer 213 located in the trench 211 may be retained. Figure 2d In this step, for example, the remaining gate conductor layer 213 is continuously etched under the condition of a high selectivity ratio between the gate conductor layer 213 and the gate dielectric layer 212 until the thickness of the gate conductor layer 213 in the trench 211 reaches a preset thickness. After the gate conductor layer 213 is etched back as described above, the gate dielectric layer 212 located above the semiconductor layer 201 may be etched away according to actual device requirements.

[0049] Figure 3 This is a SEM photo after the sacrificial layer and the gate conductor layer are simultaneously etched. Figure 1e and Figure 3 Under the conditions of basically the same groove morphology and basically the same recessed structure, the prior art is used to directly transfer the recessed structure 113a into the groove, so that the final depth of the recessed structure 113a is as high as 930±150nm; while using the technical solution provided in this embodiment, by adding a sacrificial layer 202, the sacrificial layer 202 and the gate conductor layer 213 are firstly etched synchronously to eliminate the recessed structure 213a as much as possible, and then the gate conductor layer 213 is etched separately, and the depth of the recessed structure 213a transferred into the groove 211 is significantly reduced to about 450±100nm, which meets the process requirements.

[0050] Therefore, the manufacturing method of the trench gate structure provided by the embodiment of the present invention can effectively reduce the depth of the recessed structure 213a in the trench 211, and solve the problem of poor contact of the contact plug caused by the V-shaped recess. And by adjusting the thickness of the sacrificial layer 202, the etching selection ratio, the thickness of the gate conductor layer 213 and other conditions, the process can be flexibly and effectively controlled to meet the process requirements of trench gate structures of various shapes and sizes. Therefore, the technical solution can be applied to the processing technology of various devices such as VDMOS and IGBT.

[0051] In addition, compared with the solution of performing CMP after manufacturing a thicker gate conductor layer, the method for manufacturing a trench gate structure provided by the embodiment of the present invention and the method for manufacturing a semiconductor device based thereon can significantly reduce the manufacturing cost and manufacturing cycle. In addition, since there is no need to configure a separate CMP device, the equipment cost is also significantly reduced.

[0052] The embodiments of the present invention are described above. However, these embodiments are only for illustrative purposes and are not intended to limit the scope of the present invention. The scope of the present invention is defined by the appended claims and their equivalents. Without departing from the scope of the present invention, those skilled in the art may make various substitutions and modifications, which should all fall within the scope of the present invention.

Claims

1. A method for manufacturing a trench gate structure, comprising the following steps: Forming a sacrificial layer on the surface of a semiconductor structure, wherein the semiconductor structure includes a semiconductor layer, a groove in the semiconductor layer, and a gate conductor layer covering the semiconductor layer and filling the groove, and a surface of the gate conductor layer corresponding to the groove has a concave structure, and the thickness of the sacrificial layer on the surface of the semiconductor layer is 80 to 120 nm; The sacrificial layer and the gate conductor layer are etched synchronously, and the etching selection ratio of the sacrificial layer to the gate conductor layer is controlled to be 0.8 to 0.9, so as to planarize the surface of the gate conductor layer.

2. The manufacturing method according to claim 1, in, The step of forming the sacrificial layer includes: coating a fluid material on the surface of the semiconductor structure, and allowing the fluid material to flow into the recessed structure to form the sacrificial layer.

3. The manufacturing method according to claim 2, in, The fluid material is selected from at least one of the following materials: Photoresist, silicate glass, spin-on glass, ethyl silicate, and antireflective coating compositions.

4. The manufacturing method according to claim 3, in, The step of forming the sacrificial layer further includes: curing the fluid material.

5. The manufacturing method according to claim 1, in, The thickness of the gate conductor layer is greater than or equal to half of the maximum width of the trench, and the difference between the thickness of the gate conductor layer and the maximum width of the trench does not exceed 100 nm.

6. The manufacturing method according to any one of claims 1 to 4, in, The sacrificial layer only fills a portion of the recessed structure. Before the step of synchronously etching the sacrificial layer and the gate conductor layer, the manufacturing method further includes: etching the gate conductor layer until the remaining gate conductor layer is flush with the sacrificial layer.

7. A method for manufacturing a semiconductor device, comprising the method for manufacturing a trench gate structure according to any one of claims 1 to 6.