Coil components

By providing groove-like voids and convex ribs in the laminated coil components, the problem of inconsistency in electrical characteristics caused by stress between the insulating portion and the coil is solved, and a low DC resistance and miniaturized coil component is realized.

CN113314313BActive Publication Date: 2024-11-12MURATA MFG CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110200403.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-02-27
Filing Date
2021-02-23
Publication Date
2024-11-12
Estimated Expiration
2041-02-23

AI Technical Summary

Technical Problem

In the laminated coil component, due to the stress between the insulating portion and the coil, the DC resistance increases when the stress relief space is arranged by the lower surface of the coil conductor.

Method used

A laminated coil component is designed, with groove-like gaps and convex edges along the length direction of the coil between the coil and the insulator. The gap width is less than 80% of the coil width, and the convex edge width is more than 10μm and less than 100μm to alleviate Stress and reduce DC resistance.

Benefits of technology

Effectively alleviate internal stress, reduce DC resistance, and achieve low and miniaturization of coils.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113314313B_ABST
    Figure CN113314313B_ABST
Patent Text Reader

Abstract

The present invention provides a coil component with reduced stress inside the coil component and low DC resistance. The laminated coil component includes: a body including an insulator portion and a coil buried in the insulator portion; and an external electrode provided on the surface of the insulator portion and electrically connected to the end of the coil, wherein the laminated coil component has a groove-shaped gap portion along the length direction of the coil at a boundary between the coil and the insulator portion, and the coil has a ridge portion along the length direction of the coil in the gap portion.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to coil components. Background Art

[0002] In coil components, especially laminated coil components, stress is generated between the insulating portion of the body and the coil, and the influence of this stress may cause inconsistency in the electrical characteristics of the laminated coil component. Therefore, it is desired to alleviate this stress.

[0003] In Patent Document 1, in order to relax the above-mentioned stress, a stress relaxation space including powder is arranged to be in contact with the lower surface of the coil conductor.

[0004] Patent Document 1: Japanese Patent Application Publication No. 2017-59749

[0005] The coil component of Patent Document 1 has a stress relaxation space that exists throughout the lower surface of the coil conductor, so that the cross-sectional area of ​​the coil conductor is reduced, resulting in an increase in direct current resistance. Summary of the invention

[0006] An object of the present invention is to provide a coil component in which stress inside the coil component is relaxed and DC resistance is low.

[0007] The present disclosure includes the following aspects.

[0008] [1] A laminated coil component comprising:

[0009] a body including an insulator portion and a coil embedded in the insulator portion; and

[0010] an external electrode disposed on a surface of the insulator portion and electrically connected to an end of the coil,

[0011] In the above-mentioned laminated coil component,

[0012] A groove-shaped gap portion is provided at a boundary between the coil and the insulator portion along the length direction of the coil.

[0013] The coil has a ridge portion along a longitudinal direction of the coil in the gap portion.

[0014] [2] In the laminated coil component according to [1] above, the width of the gap is not more than 80% of the width of the coil conductor.

[0015] [3] In the laminated coil component described in [1] or [2] above, the width of the ridge portion is not less than 10 μm and not more than 100 μm.

[0016] According to the present disclosure, it is possible to provide a coil component in which stress of the coil component is relaxed and DC resistance is low. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a perspective view schematically showing a laminated coil component 1 according to the present disclosure.

[0018] Figure 2 Yes means Figure 1 The illustrated laminated coil component 1 is a cross-sectional view taken along a cutting plane xx.

[0019] Figure 3 Yes means Figure 1 The illustrated laminated coil component 1 is a cross-sectional view taken along a cutting plane yy.

[0020] Figure 4 yes Figure 1 2 is a cross-sectional view of the coil 7 of the laminated coil component 1 shown.

[0021] Figure 5 (a) and (b) are used to Figure 1 The drawings are for explaining a method of manufacturing the laminated coil component 1, and are respectively a cross-sectional view including a coil portion and a plan view viewed from the upper surface.

[0022] Figure 6 (a) and (b) are used to Figure 1 The drawings are for explaining a method of manufacturing the laminated coil component 1, and are respectively a cross-sectional view including a coil portion and a plan view viewed from the upper surface.

[0023] Figure 7 (a) and (b) are used to Figure 1 The drawings are for explaining a method of manufacturing the laminated coil component 1, and are respectively a cross-sectional view including a coil portion and a plan view viewed from the upper surface.

[0024] Figure 8 (a) and (b) are used to Figure 1 The drawings are for explaining a method of manufacturing the laminated coil component 1, and are respectively a cross-sectional view including a coil portion and a plan view viewed from the upper surface.

[0025] Description of Reference Numerals

[0026] 1… stacked coil component; 2… main body; 4, 5… external electrodes; 6… insulator portion; 7… coil; 8… ridge portion; 11… gap portion; 12… wall portion; 22… ferrite paste layer; 23a, 23b… resin paste layer; 25… conductive paste layer; 26… ferrite paste layer; 27… ferrite paste layer. DETAILED DESCRIPTION

[0027] Hereinafter, a laminated coil component 1 according to an embodiment of the present disclosure will be described in detail with reference to the drawings. However, the shapes and arrangements of the laminated coil component and each component of the present embodiment are not limited to the examples shown in the drawings.

[0028] Figure 1 A perspective view showing a laminated coil component 1 according to this embodiment is shown. Figure 2 Shown is a sectional view of xx, Figure 3 The yy cross-sectional view is shown. However, the shapes and arrangements of the laminated coil component and the components of the following embodiments are not limited to the examples shown in the drawings.

[0029] like Figure 1 , Figure 2 and Figure 3 As shown in FIG. 1 , the laminated coil component 1 of the present embodiment is a laminated coil component having a substantially rectangular parallelepiped shape. Figure 1 The surface perpendicular to the L axis is called the "end surface", the surface perpendicular to the W axis is called the "side surface", and the surface perpendicular to the T axis is called the "upper and lower surface". The laminated coil component 1 generally includes a main body 2 and external electrodes 4 and 5 provided on both end surfaces of the main body 2. The main body 2 includes: an insulator portion 6 and a coil 7 buried in the insulator portion 6. The coil 7 is electrically connected to the above-mentioned external electrodes 4 and 5 at the lead portions extending from the two ends of the winding portion. On one main surface ( Figure 2 A slot-shaped gap portion 11 along the length direction of the coil is provided at the boundary between the lower main surface of the coil 7 and the insulator portion 6. The gap portion 11 can suppress the generation of stress between the coil 7 and the insulator portion 6. In addition, the coil 7 has a ridge portion 8 protruding toward the inside of the slot as the gap portion, and has a wall portion 12 on both sides of the slot. Therefore, the cross-sectional area of ​​the coil is increased by the amount of the ridge portion and the wall portion, and the DC resistance is reduced.

[0030] As described above, in the laminated coil component 1 of the present embodiment, the main body 2 is composed of the insulator portion 6 and the coil 7 .

[0031] The insulator portion 6 is preferably a magnetic body, and more preferably is made of sintered ferrite. The sintered ferrite contains at least Fe, Ni, and Zn as main components. The sintered ferrite may further contain Cu.

[0032] In one embodiment, the sintered ferrite contains at least Fe, Ni, Zn, and Cu as main components.

[0033] In the above-mentioned sintered ferrite, the Fe content is preferably 40.0 mol% to 49.5 mol% (based on the total of main components, the same applies hereinafter), and more preferably 45.0 mol% to 49.5 mol% in terms of Fe2O3.

[0034] In the sintered ferrite, the Zn content is preferably 5.0 mol% to 35.0 mol% (based on the total of main components, the same applies hereinafter), and more preferably 10.0 mol% to 30.0 mol% in terms of ZnO.

[0035] In the sintered ferrite, the Cu content is preferably 4.0 mol% to 12.0 mol% (based on the total of main components, the same applies hereinafter), and more preferably 7.0 mol% to 10.0 mol% in terms of CuO.

[0036] In the above-mentioned sintered ferrite, the Ni content is not particularly limited, and may be the remainder of the above-mentioned other main components, namely, Fe, Zn, and Cu.

[0037] In one embodiment, for the above-mentioned sintered ferrite, Fe is converted into Fe2O3 of 40.0 mol% or more and 49.5 mol% or less, Zn is converted into ZnO of 5.0 mol% or more and 35.0 mol% or less, Cu is converted into CuO of 4.0 mol% or more and 12.0 mol% or less, and NiO is the remainder.

[0038] In the present disclosure, the above-mentioned sintered ferrite may also include additives. As additives of sintered ferrite, for example, Mn, Co, Sn, Bi, Si, etc. can be cited, but are not limited to this. The content (addition amount) of Mn, Co, Sn, Bi and Si is preferably 0.1 parts by weight or more and 1 part by weight or less, respectively, converted into Mn3O4, Co3O4, SnO2, Bi2O3 and SiO2, relative to a total of 100 parts by weight of the main components (Fe (converted to Fe2O3), Zn (converted to ZnO), Cu (converted to CuO) and Ni (converted to NiO)). In addition, the above-mentioned sintered ferrite may also include impurities that are inevitable in manufacturing.

[0039] The above-mentioned sintered ferrite may also include Mn, Co, Sn, Bi, Si, etc. as additive components. As additive components of sintered ferrite, for example, Mn, Co, Sn, Bi, Si, etc. can be cited, but it is not limited to this. The content (addition amount) of Mn, Co, Sn, Bi and Si is preferably 0.1 weight part or more and 1 weight part or less, respectively, converted into Mn3O4, Co3O4, SnO2, Bi2O3 and SiO2, relative to a total of 100 weight parts of the main components (Fe (converted to Fe2O3), Zn (converted to ZnO), Cu (converted to CuO) and Ni (converted to NiO)). In addition, the above-mentioned sintered ferrite may also include impurities that are inevitable in manufacturing.

[0040] The coil 7 is formed by electrically connecting the coil patterns to each other. The coil pattern is a conductive layer containing a conductive material. Preferably, the coil pattern is a conductive layer substantially composed of a conductive material. Such a conductive material is not particularly limited, but examples thereof include Au, Ag, Cu, Pd, Ni, etc. The conductive material is preferably Ag or Cu, and more preferably Ag. The conductive material may be only one kind or may be two or more kinds.

[0041] The coil 7 includes a ridge portion 8 protruding toward the inside of the slot-shaped gap portion 11 and a wall portion 12 covering the gap portion 11. The ridge portion 8 is formed in the center of the slot to be substantially parallel to the slot. The wall portion 12 is formed to surround the gap portion 11. For example, in a cross section perpendicular to the length direction of the coil (e.g. Figure 2 ), the ridge portion 8 is arranged to protrude downward from the coil conductor at a substantially central portion in the width direction of the coil conductor, and the wall portion 12 is arranged to sandwich the gap portion 11 at both ends of the coil conductor. The shape of the ridge portion is not particularly limited, and may have a rectangular, trapezoidal, circular arc, or other shape in a cross section perpendicular to the length direction of the coil.

[0042] The thickness of the conductor of the coil 7 is preferably 30 μm or more and 80 μm or less, more preferably 40 μm or more and 70 μm or less. In addition, the thickness of the conductor of the coil refers to the thickness of the portion where there is no gap, typically the thickness at the position of the wall portion 12. By making the thickness of the coil conductor 30 μm or more, the DC resistance can be reduced. By making the thickness of the coil conductor 80 μm or less, it is easy to make the coil component low and small.

[0043] The width of the ridge portion 8 is preferably 10 μm or more and 100 μm or less, more preferably 30 μm or more and 60 μm or less. By making the width of the ridge portion 8 within the above range, the internal stress can be effectively relieved and the DC resistance can be reduced. Here, the width of the ridge portion refers to the width at a position of 1 / 2 of the height of the ridge portion in a cross section perpendicular to the length direction of the coil.

[0044] The width of the ridge portion 8 is preferably 50% or more of the width of the gap portion 11, more preferably 70% or more of the width of the gap portion 11, and further preferably 80% or more of the width of the gap portion 11. By increasing the width of the ridge portion 8, the DC resistance of the coil can be further reduced. In addition, the width of the ridge portion 8 is preferably 90% or less of the width of the gap portion 11, and more preferably 85% or less of the width of the gap portion 11.

[0045] The thickness of the ridge 8 may be appropriately adjusted according to the thickness of the cavity 11, but is preferably 0.9 μm to 29 μm. By setting the thickness of the ridge to 0.9 μm to 29 μm, internal stress can be effectively relaxed and DC resistance can be reduced.

[0046] The thickness of the ridge portion 8 is preferably 50% or more of the thickness of the gap portion 11, more preferably 70% or more of the thickness of the gap portion 11, and further preferably 90% or more of the thickness of the gap portion 11. By increasing the thickness of the ridge portion 8, the DC resistance of the coil can be further reduced. In addition, the thickness of the ridge portion 8 is preferably 99% or less of the thickness of the gap portion 11, and more preferably 95% or less of the thickness of the gap portion 11.

[0047] The thickness of the wall portion 12 can be appropriately adjusted according to the thickness of the cavity 11, and is preferably 0.9 μm to 29 μm. By setting the thickness of the wall portion to 0.9 μm to 29 μm, internal stress can be effectively relaxed and DC resistance can be reduced.

[0048] A gap portion 11 exists at the boundary between the coil 7 and the insulator portion 6. The gap portion 11 functions as a so-called stress relaxation space.

[0049] The above-mentioned gap portion 11 is provided in a groove shape along the length direction of the coil 7. By forming the gap portion along the length direction of the coil, the cross-sectional area of ​​the coil 7 is increased by the amount of the ridge portion 8 and the wall portion 12 of the coil 7, and the DC resistance can be reduced. That is, by forming the gap portion along the direction of current flow, the increase in DC resistance caused by the formation of the gap portion can be suppressed.

[0050] The width of the above-mentioned gap ( Figure 4 W2) is preferably the width of the coil pattern ( Figure 4 The width of the gap is less than 95% of the width of the coil pattern, and more preferably less than 90% of the width of the coil pattern. By making the width of the gap less than 95% of the width of the coil pattern, the width of the outer wall portion 12 is increased, and the DC resistance can be further reduced. In addition, by increasing the width of the outer wall portion 12, the delamination between the coil 7 and the insulator portion 6 can be suppressed. In addition, Figure 4 The cross section of the coil conductor has corners, but the coil conductor of the present disclosure does not necessarily need to have corners and may also have rounded corners.

[0051] The width W2 of the gap is preferably 40% or more of the width W1 of the coil pattern, more preferably 50% or more of the width W1 of the coil pattern, and further preferably 60% or more of the width W1 of the coil pattern. By making the width of the gap 40% or more of the width of the coil pattern, internal stress can be more effectively relieved.

[0052] The thickness of the above-mentioned gap portion is preferably 1 μm or more and 30 μm or less, and more preferably 5 μm or more and 15 μm or less. By making the thickness of the above-mentioned gap portion 1 μm or more, the internal stress can be more effectively relieved. By making the thickness of the above-mentioned gap portion 30 μm or less, it is beneficial to low profile and the DC resistance of the coil can be further reduced. In addition, the thickness of the gap portion refers to the thickness of the portion where the ridge portion 8 does not exist.

[0053] The sizes of the gap and the coil can be measured as follows.

[0054] The chip was polished with the LT surface of the chip facing the polishing paper, and the polishing was stopped at the approximate center of the body. Thereafter, ion etching was performed and the body was observed under a microscope.

[0055] In the laminated coil component 1 of the present disclosure, the external electrodes 4 and 5 are provided to cover both end surfaces of the body 2. The external electrodes are made of a conductive material, preferably one or more metal materials selected from Au, Ag, Pd, Ni, Sn and Cu.

[0056] The external electrode may be a single layer or a multi-layer. In one embodiment, the external electrode is a multi-layer, preferably 2 or more layers and 4 or less layers, for example 3 layers.

[0057] In one embodiment, the external electrode is multilayered and may include a layer containing Ag or Pd, a layer containing Ni or a layer containing Sn. In a preferred embodiment, the external electrode is composed of a layer containing Ag or Pd, a layer containing Ni and a layer containing Sn. Preferably, the layers are arranged in the order of a layer containing Ag or Pd, preferably a layer containing Ag, a layer containing Ni and a layer containing Sn from the coil conductor side. Preferably, the layer containing Ag or Pd is a layer fired with Ag paste or Pd paste, and the layer containing Ni and the layer containing Sn may be a plated layer.

[0058] The laminated coil component 1 of the present embodiment described above is manufactured, for example, as follows. In the present embodiment, a mode in which the insulator portion 6 is formed of a ferrite material will be described.

[0059] (1) Preparation of ferrite paste

[0060] First, a ferrite material is prepared. The ferrite material contains Fe, Zn and Ni as main components, and further contains Cu as desired. Generally, the main components of the ferrite material are substantially composed of oxides of Fe, Zn, Ni and Cu (ideally, Fe2O3, ZnO, NiO and CuO).

[0061] As a ferrite material, Fe2O3, ZnO, CuO, NiO and additional components as required are weighed to a prescribed composition, mixed and crushed. The crushed ferrite material is dried, for example, pre-fired at a temperature of 700 to 800°C to obtain a pre-fired powder. A prescribed amount of solvent (ketone solvent, etc.), resin (polyvinyl acetal, etc.) and plasticizer (alkyd plasticizer, etc.) are added to the pre-fired powder, kneaded with a planetary mixer, etc., and further dispersed with a three-roll mill, etc., so that a ferrite paste can be prepared.

[0062] In addition, it can also be considered that the Fe content (converted to Fe2O3), Mn content (converted to Mn2O3), Cu content (converted to CuO), Zn content (converted to ZnO) and Ni content (converted to NiO) of the sintered ferrite are essentially no different from the Fe content (converted to Fe2O3), Mn content (converted to Mn2O3), Cu content (converted to CuO), Zn content (converted to ZnO) and Ni content (converted to NiO) of the ferrite material before firing.

[0063] (2) Preparation of conductive paste for coil conductor

[0064] First, a conductive material is prepared. As the conductive material, for example, Au, Ag, Cu, Pd, Ni, etc. can be cited, preferably Ag or Cu, more preferably Ag. A predetermined amount of powder of the conductive material is weighed, and kneaded with a predetermined amount of solvent (eugenol, etc.), resin (ethyl cellulose, etc.) and dispersant using a planetary mixer, etc., and then dispersed using a three-roll mill, etc., so that a conductive paste for a coil conductor can be prepared.

[0065] (3) Preparation of resin paste

[0066] A resin paste is prepared for forming the gap 11 of the laminated coil component 1. Such a resin paste can be prepared by adding a resin (acrylic resin, etc.) that disappears during firing to a solvent (isophorone, etc.).

[0067] (4) Fabrication of laminated coil components

[0068] (4-1) Production of the main body

[0069] First, a substrate (not shown) is prepared in which a heat-release sheet and a PET (polyethylene terephthalate) film are laminated on a metal plate. The ferrite paste is printed on the substrate a predetermined number of times to form a ferrite paste layer 22 ( Figure 5 (a) and (b)).

[0070] Next, the resin paste is printed on the portion where the gap 11 is to be formed, thereby forming resin paste layers 23a and 23b ( Figure 5(a) and (b)).

[0071] Next, the conductive paste is printed on the entire portion where the coil conductor is to be formed, forming a conductive paste layer 25 ( Figure 6 (a) and (b)).

[0072] Next, in the area where the conductive paste layer 25 is not formed, the ferrite paste is printed to the same height as the conductive paste layer to form a ferrite paste layer 26 ( Figure 7 (a) and (b)).

[0073] Next, the ferrite paste is printed on the entire surface to form a ferrite paste layer 27 ( Figure 8 (a) and (b)).

[0074] Next, the resin paste layer 23 ( Figure 5 )、Conductive paste layer 25( Figure 6 )、Ferrite paste layer 26( Figure 7 ) and ferrite paste layer 27 ( Figure 8 ) are repeated a predetermined number of times. Finally, the ferrite paste is printed a predetermined number of times to form a ferrite paste layer for the outer layer, and a laminated body block as an assembly of elements is obtained on the substrate.

[0075] Next, after the layers are pressed together while the laminate block is mounted on the substrate, the laminate block is cooled. After cooling, the metal plate and the PET film are peeled off from the laminate block. The laminate block is cut by a cutter or the like to separate into components.

[0076] The corners of the element are ground by barrel grinding to form rounded corners. The barrel grinding can be performed on an unfired laminate or a fired laminate. In addition, the barrel grinding can be either dry or wet. The barrel grinding can be a method of rubbing the elements together or a method of barrel grinding with a medium.

[0077] After the barrel grinding process, the element is fired at a temperature of, for example, 910°C to 930°C to obtain the main body 2 of the laminated coil component 1. During the firing, the resin paste layer 23 disappears, and a void portion is generated in the portion where the resin paste layer 23 existed. The existence of such a void portion can reduce the generation of stress caused by the contraction of the fired ferrite paste layer and the conductive paste layer. At this time, due to the contraction of the above-mentioned ferrite paste layer and the conductive paste layer, the portion of the coil existing between the resin paste layers 23a and 23b is peeled off from the insulating body portion 6 to form a ridge portion 8. By peeling off the coil portion existing between the resin paste layers 23a and 23b from the magnetic body portion, the generation of stress can be further reduced.

[0078] (4-2) Formation of External Electrodes

[0079] Next, an Ag paste containing Ag and glass for forming an external electrode is applied to the end surface of the body 2 and fired to form a base electrode. Next, a Ni film and a Sn film are sequentially formed on the base electrode by electroplating to form an external electrode. Figure 1 The laminated coil component 1 is as shown.

[0080] As mentioned above, although one embodiment of the present invention has been described, this embodiment can be modified in various ways.

[0081] For example, in the above-mentioned embodiment, the number of the resin paste layers is two, but the number may be three or more, for example, three, four or five.

[0082] In addition, in the above-mentioned embodiment, the void portion is formed almost entirely except for the portion connected by the via hole, but it can also be formed only locally. For example, the void portion may exist in more than 30% of the length of the coil pattern of each layer, preferably more than 50%, more preferably more than 70%, and further preferably more than 80%. By forming the void portion in more than 30% of the length of the coil pattern of each layer, the generation of stress can be further reduced. Here, the "length of the coil pattern of each layer" refers to the distance from the via hole (or external electrode) used to connect to the coil pattern of other layers to the via hole used to connect to the other layers.

[0083] In the above description, the magnetic body portion is formed by printing the ferrite paste, but the ferrite paste layers 22 and 27 may be formed using ferrite sheets instead of the paste layers.

[0084] Example

[0085] The coil conductor after firing has a width of 150 μm and a thickness of 40 μm. The laminated coil components of the embodiment and the comparative example are obtained by forming two rows (embodiment) of resin paste layers and one row (comparative example) of resin paste layers and forming a gap. As for the dimensions of the samples, the length (L) of the embodiment and the comparative example samples is 1.0 mm, the width (W) is 0.5 mm, and the height (T) is 0.5 mm.

[0086] For the samples of the examples and comparative examples, a heat cycle of -55°C to +125°C was performed for 2000 cycles, and the change rate of the inductance of the samples before and after the test was calculated, and the stress relaxation effect was evaluated. In addition, the DC resistance of the samples of the examples and comparative examples was measured. As a result, the stress relaxation effect was the same in the samples of the examples and comparative examples. In addition, for the DC resistance, the values ​​of 5% lower were obtained for the samples of the examples than for the comparative examples.

[0087] Industrial Applicability

[0088] The laminated coil component disclosed herein can be used in a wide variety of applications such as an inductor.

Claims

1. A laminated coil component, comprising: A body, comprising an insulator portion and a coil embedded in the insulator portion; and an external electrode disposed on a surface of the insulator portion and electrically connected to an end of the coil, The laminated coil component is characterized in that: A groove-shaped gap portion is provided at a boundary between the coil and the insulator portion along the length direction of the coil. The coil has a ridge portion in the gap portion along the length direction of the coil, The rib portion does not contact the insulator portion at the gap portion.

2. The laminated coil component according to claim 1, wherein: The width of the gap is equal to or less than 80% of the width of the coil conductor.

3. The laminated coil component according to claim 1 or 2, characterized in that: The ridge portion has a width of 10 μm or more and 100 μm or less.