A method for condition inspection of heating surface of boiler in thermal power plant

By establishing a prediction model for the thickness, lifespan and oxide scale generation of water-cooled wall tubes, real-time monitoring of the status of water-cooled walls and high-temperature heating surfaces of boilers in thermal power plants has solved the problems of high-temperature corrosion and over-temperature tube explosions in boilers, and improved the safety of the unit. performance and efficiency of use.

CN113379072BActive Publication Date: 2024-10-29SUZHOU XIRE ENERGY SAVING ENVIRONMENTAL PROTECTION TECH CO LTD +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202110499251.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-05-08
Publication Date
2024-10-29
Estimated Expiration
2041-05-08
Patent Text Reader

Abstract

The present invention relates to a state inspection method for the heating surface of a boiler in a thermal power plant, which comprises the following steps: S1, collecting coal quality parameters, water-cooled wall tube wall temperature, high-temperature heating surface tube wall temperature, high-temperature heating surface inlet and outlet steam temperature and pressure, and water-cooled wall reducing atmosphere composition and concentration data during the operation of the unit; S2, based on the collected data, establishing a water-cooled wall tube wall thickness data prediction model, a high-temperature heating surface life prediction model, and a high-temperature heating surface oxide scale generation prediction model; S3, based on the acquired water-cooled wall wall thickness change data, high-temperature heating surface life change data, and high-temperature heating surface oxide scale generation data, the water-cooled wall and the high-temperature heating surface are monitored in real time, and the conditions of the water-cooled wall and the high-temperature heating surface are analyzed. The state inspection method provided by the present invention can monitor the thickness of the water-cooled wall and the high-temperature heating surface and the oxide scale production in real time, and analyze them, so as to timely inspect and repair the unit and improve the unit operation safety.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of boiler maintenance, and in particular relates to a state maintenance method for a heating surface of a boiler in a thermal power plant. Background Art

[0002] For a long time, the inspection and maintenance of thermal power generating units are mainly based on regular inspection and maintenance. It is an equipment inspection system based on time cycles. The more common practice is to conduct C-level inspection once a year, B-level inspection once every three years, and A-level inspection once every six years. However, the disadvantages of this equipment inspection system based on time cycles are becoming more and more prominent. The most important one is "treating even if there is no disease". Just because it is time for regular inspection and maintenance, even if the unit is in good condition, it has to stop for inspection and maintenance, which affects the unit's utilization efficiency and causes "over-repair" of the equipment. Therefore, the concept of condition-based maintenance was proposed, emphasizing that by strengthening equipment status detection, it is possible to judge the existing defects and hidden dangers of the unit as a whole, or major defects in the system locally, and continuing to operate will bring greater safety risks.

[0003] In the operation of thermal power plant boilers, high-temperature corrosion occurs in the water-cooled wall of the boiler, resulting in continuous thinning of the water-cooled wall tube wall, and the effective bearing capacity of the water-cooled wall tube wall continues to decline. In severe cases, the water-cooled wall tube will burst, causing the unit to shut down, seriously affecting the safe operation of the unit. With the improvement of boiler technology, steam parameters have also increased, and the probability of over-temperature and tube burst accidents on the high-temperature heating surface is greater. Once the heating surface of the boiler leaks due to excessive temperature somewhere, shutdown and furnace shutdown are inevitable, which not only directly affects the economic benefits of the power plant, threatens personal safety, but also affects the safe and stable operation of the power grid. In the long-term use of most boilers, a lot of oxide scale will be produced on the inner wall of the boiler. When the oxide scale slag is too large, it will block the furnace tube, resulting in over-temperature tube burst, affecting the normal operation of the boiler.

[0004] Especially after the ultra-clean emission transformation of the unit, the problem of high-temperature corrosion in the unit furnace has become increasingly prominent. How to accurately understand the status of the water-cooled wall of the furnace tube and the high-temperature heating surface of the furnace tube, and understand the thickness of the water-cooled wall of the furnace tube and the high-temperature heating surface of the furnace tube and the formation of oxide scale are extremely important for whether to carry out unit status maintenance. Summary of the invention

[0005] The object of the present invention is to provide a method for condition inspection of heating surfaces of boilers in thermal power plants.

[0006] In order to achieve the above object, the technical solution adopted by the present invention is:

[0007] The present invention provides a method for condition inspection of a heating surface of a boiler in a thermal power plant, which comprises the following steps:

[0008] S1. Collect coal quality parameters, water-cooled wall tube temperature, high-temperature heating surface tube temperature, high-temperature heating surface inlet and outlet steam temperature and pressure, and water-cooled wall reducing atmosphere composition and concentration data during unit operation;

[0009] S2, based on the collected data in step S1, establish a water-cooled wall tube wall thickness data prediction model, a high-temperature heating surface life prediction model, and a high-temperature heating surface oxide scale generation prediction model,

[0010] Obtain water wall thickness variation data based on water wall tube thickness data prediction model;

[0011] Obtaining high-temperature heating surface life change data based on the high-temperature heating surface life prediction model;

[0012] Acquire the generation data of the oxide scale of the high-temperature heating surface based on the prediction model of the oxide scale generation of the high-temperature heating surface;

[0013] S3. Based on the water-cooled wall thickness change data, high-temperature heating surface life change data, and high-temperature heating surface oxide scale generation data obtained in step S2, real-time monitoring of the water-cooled wall and the high-temperature heating surface is achieved, and the conditions of the water-cooled wall and the high-temperature heating surface are analyzed.

[0014] Furthermore, in step S3, analyzing the condition of the water-cooled wall includes:

[0015] The water-cooled wall thickness change data includes the wall thickness data of the water-cooled wall after a time Ti. If the obtained water-cooled wall thickness data is less than the preset wall thickness threshold, the water-cooled wall needs to be repaired. If the obtained water-cooled wall thickness data is not less than the preset wall thickness threshold, no repair is required.

[0016] Furthermore, in step S3, analyzing the condition of the high-temperature heating surface includes:

[0017] The high-temperature heating surface life change data includes the life data of the high-temperature heating surface after a time Ti. If the acquired high-temperature heating surface life data is less than a preset life threshold, the high-temperature heating surface needs to be repaired. If the acquired high-temperature heating surface life data is not less than the preset life threshold, no repair is required.

[0018] Furthermore, in step S3, analyzing the condition of the high-temperature heating surface includes:

[0019] The generation data of the high-temperature heating surface oxide scale includes the high-temperature heating surface oxide scale thickness data after a time Ti. If the obtained high-temperature heating surface oxide scale thickness data is greater than a preset thickness threshold, the high-temperature heating surface needs to be inspected and repaired. If the obtained high-temperature heating surface oxide scale thickness data is not greater than the preset thickness threshold, no inspection and repair is required.

[0020] Furthermore, the water-cooled wall tube thickness data prediction model is as follows:

[0021] WT t =WT0-WT0×f(C, St, T, t)=WT0×K w ×O2 a ×CO b ×H2S c ×St d ×T e ×t f

[0022] Among them, WT t is the wall thickness of the water-cooled wall after time Ti, WT0 is the wall thickness at the beginning of calculation, C is the reducing atmosphere concentration, O2 is the concentration of O2, CO is the concentration of CO, H2S is the concentration of H2S; St is the sulfur content of the coal; T is the water-cooled wall temperature, t is the effective operation time of the power plant unit, Kw, a, b, c, d, e, f are all weight coefficients.

[0023] Furthermore, in the water-cooled wall tube thickness data prediction model, the Kw range is set to 3-8, the a range is -2-0, the b range is 1-3, the c range is 2-5, the d range is 1-4, the e range is 0.5-3, and the f range is 0.5-3.

[0024] Furthermore, the high temperature heating surface life prediction model is as follows:

[0025] L t =L0×f(Tso, Tsi, Pso, Psi, Tw, t)=L0·K L ·Tso g ·Tsi h ·Pso i ·Psi j ·Tw k ·t l

[0026] Among them, L t is the life of the heating surface after time Ti, L0 is the pipe life at the beginning of calculation, Tso is the steam temperature at the inlet of the high-temperature heating surface, Tsi is the steam temperature at the outlet of the high-temperature heating surface, Pso is the steam pressure at the inlet of the high-temperature heating surface, Psi is the steam pressure at the outlet of the high-temperature heating surface, Tw is the wall temperature of the heating surface, t is the effective operation time of the power plant unit, K L , g, h, i, j, k, and l are all weight coefficients.

[0027] Furthermore, in the high-temperature heating surface life prediction model, K is set LThe range is 0.3-1.2, the range of g is -0.02-0, the range of h is -0.02-0, the range of i is -0.03-0, the range of j is -0.03-0, the range of k is -0.07-0, and the range of l is -0.007-0.

[0028] Furthermore, the high temperature heated surface oxide scale generation prediction model is as follows:

[0029] T t =f(Tso, Tsi, Pso, Psi, Tw, t)=K T ·Tso m ·Tsi n ·Pso o ·Psi p ·Tw q ·t r

[0030] Among them, T t is the oxide scale thickness of the high-temperature heating surface after time Ti, Tso is the steam temperature at the inlet of the high-temperature heating surface, Tsi is the steam temperature at the inlet of the high-temperature heating surface, Pso is the steam pressure at the outlet of the high-temperature heating surface, Psi is the steam pressure at the outlet of the high-temperature heating surface, Tw is the wall temperature of the high-temperature heating surface, t is the effective operation time of the power plant unit, K T , m, n, o, p, q, and r are all weight coefficients.

[0031] Furthermore, in the high-temperature heated surface oxide scale generation prediction model, K is set T The range is 0.5-1.2, the range of m is 0-0.1, the range of n is 0-0.1, the range of o is 0-0.1, the range of p is 0-0.1, the range of q is 0-0.1, and the range of r is 0-0.002.

[0032] Due to the application of the above technical scheme, the present invention has the following advantages compared with the prior art: the condition inspection and maintenance method of the heating surface of the boiler of a thermal power plant provided by the present invention can monitor the changes in the wall thickness of the water-cooled wall and the high-temperature heating surface and the generation of oxide scale on the high-temperature heating surface in real time by establishing a water-cooled wall tube wall thickness data prediction model, a high-temperature heating surface life prediction model, and a high-temperature heating surface oxide scale generation prediction model, and analyze the conditions of the water-cooled wall and the high-temperature heating surface, accurately understand the conditions of the water-cooled wall and the high-temperature heating surface in the furnace, and accurately understand the thickness of the water-cooled wall and the high-temperature heating surface and the generation of oxide scale, so as to judge whether there are defects and hidden dangers in the unit as a whole, or whether there are major defects in the local system, so as to timely inspect and repair the unit when problems occur, without having to inspect and repair it only during regular inspections, without affecting the use efficiency of the unit, and without causing "over-repair" of the equipment, thereby improving the safety of unit operation. DETAILED DESCRIPTION

[0033] The present invention is further described below in conjunction with the illustrated embodiments.

[0034] The present invention provides a method for condition inspection of heating surfaces of boilers in thermal power plants, which comprises the following steps:

[0035] S1. Collect coal quality parameters, water-cooled wall tube wall temperature, high-temperature heating surface (platen-type superheater, high-temperature superheater and high-temperature reheater, etc.) tube wall temperature, high-temperature heating surface (platen-type superheater, high-temperature superheater and high-temperature reheater, etc.) inlet and outlet steam temperature and pressure, water-cooled wall reducing atmosphere composition and concentration data, reducing atmosphere O2, CO, H2S during unit operation.

[0036] S2. Based on the collected data in step S1, a water-cooled wall tube wall thickness data prediction model, a high-temperature heating surface life prediction model, and a high-temperature heating surface oxide scale generation prediction model are established, wherein:

[0037] Obtain water wall thickness variation data based on water wall tube thickness data prediction model;

[0038] Obtaining high-temperature heating surface life change data based on the high-temperature heating surface life prediction model;

[0039] The generation data of the oxide scale on the high-temperature heating surface is obtained based on the prediction model of the oxide scale generation on the high-temperature heating surface.

[0040] S3. Based on the water-cooled wall thickness change data, high-temperature heating surface life change data, and high-temperature heating surface oxide scale generation data obtained in step S2, real-time monitoring of the water-cooled wall and the high-temperature heating surface is achieved, and the conditions of the water-cooled wall and the high-temperature heating surface are analyzed.

[0041] In step S3, analyzing the condition of the water-cooled wall includes:

[0042] The water-cooled wall thickness change data includes the wall thickness data of the water-cooled wall after a time Ti. If the calculated water-cooled wall thickness data is less than a preset wall thickness threshold, the water-cooled wall needs to be repaired. If the calculated water-cooled wall thickness data is not less than the preset wall thickness threshold, no repair is required. The preset wall thickness threshold is 50%-60% of the initial wall thickness of the water-cooled wall, preferably 60%.

[0043] In step S3, analyzing the condition of the high-temperature heating surface includes:

[0044] The high-temperature heating surface life change data includes the life data of the high-temperature heating surface after a time Ti. If the calculated high-temperature heating surface life data is less than a preset life threshold, the high-temperature heating surface needs to be repaired. If the calculated high-temperature heating surface life data is not less than the preset life threshold, no repair is required. The preset life threshold is 50%-60% of the initial life of the high-temperature heating surface, preferably 60%.

[0045] In step S3, analyzing the condition of the high-temperature heating surface includes:

[0046] The generation data of the oxide scale of the high temperature heating surface includes the oxide scale thickness data of the high temperature heating surface after the time Ti has passed. If the calculated oxide scale thickness data of the high temperature heating surface is greater than the preset thickness threshold, the high temperature heating surface needs to be repaired. If the calculated oxide scale thickness data of the high temperature heating surface is not greater than the preset thickness threshold, no repair is required. The preset thickness threshold is 50%-60% of the initial thickness of the high temperature heating surface, preferably 60%.

[0047] The water-cooled wall tube thickness data prediction model is as follows:

[0048] WT t =WT0-WT0×f(C, St, T, t)=WT0×K w ×O2 a ×CO b ×H2S c ×St d ×T e ×t f

[0049] Among them, WT t is the wall thickness of the water-cooled wall after time Ti, WT0 is the wall thickness at the beginning of calculation, C is the reducing atmosphere concentration, O2 is the concentration of O2, CO is the concentration of CO, H2S is the concentration of H2S; St is the sulfur content of the coal; T is the water-cooled wall temperature, t is the effective operation time of the power plant unit, Kw, a, b, c, d, e, f are all weight coefficients.

[0050] In the water-cooled wall tube thickness data prediction model, the Kw range is set to 3-8, the a range is -2-0, the b range is 1-3, the c range is 2-5, the d range is 1-4, the e range is 0.5-3, and the f range is 0.5-3.

[0051] The embodiment shows that the initial thickness of the water-cooled wall tube wall in a furnace is WT0, which is 7 mm. After the unit has been running for one year, the actual thickness of the water-cooled wall tube wall WT is calculated by the water-cooled wall tube wall thickness data prediction model. tThe specific calculation process is: the operating oxygen content O2 is 0.1% (volume percentage), CO emission concentration is 10% (volume percentage), H2S concentration is 0.1% (volume percentage), sulfur content St is 0.6% (volume percentage), the average water-cooled wall temperature T is 623.15K, the effective operation time t of the power plant unit is 16200000s, Kw is 4.972, a is -1, b is 1.5, c is 3, d is 2, e is 1, f is 1, WT t =7*4.972*0.001^ -1 *0.1^ 1.5 *0.001^ 3 *0.006^ 2 *623.15*16200000=4mm.

[0052] If the preset wall thickness threshold is 60% of the initial wall thickness of the water-cooled wall, the preset wall thickness threshold is 4.2 mm. The actual thickness WT t If it is less than 4.2mm, it indicates that the thickness of the water-cooled wall tube changes rapidly, reminding maintenance personnel that maintenance is needed.

[0053] The actual wall thickness of the water-cooled wall tube after time Ti is calculated by the water-cooled wall tube thickness data prediction model, so that the water-cooled wall can be monitored in real time, and the change of the water-cooled wall tube thickness can be promptly and quickly known under the condition of normal operation of the unit. When the obtained water-cooled wall thickness data is less than the preset wall thickness threshold, the water-cooled wall is promptly repaired and repaired in time when problems occur. There is no need to repair it during regular maintenance, which does not affect the unit's utilization efficiency and does not cause "over-repair" of the equipment.

[0054] The high temperature heating surface life prediction model is as follows:

[0055] L t =L0×f(Tso, Tsi, Pso, Psi, Tw, t)=L0·K L ·Tso g ·Tsi h ·Pso i ·Psi j ·Tw k ·t l

[0056] Among them, L t is the life of the heating surface after time Ti, L0 is the pipe life at the beginning of calculation, and the pipe life is obtained by detection during cold shutdown; Tso is the steam temperature at the inlet of the high-temperature heating surface, Tsi is the steam temperature at the outlet of the high-temperature heating surface, Pso is the steam pressure at the inlet of the high-temperature heating surface, Psi is the steam pressure at the outlet of the high-temperature heating surface, Tw is the wall temperature of the heating surface, t is the effective operation time of the power plant unit, K L, g, h, i, j, k, and l are all weight coefficients.

[0057] In the high temperature heating surface life prediction model, K is set L The range is 0.3-1.2, the range of g is -0.02-0, the range of h is -0.02-0, the range of i is -0.03-0, the range of j is -0.03-0, the range of k is -0.07-0, and the range of l is -0.007-0.

[0058] The embodiment shows that in the initial stage, the pipe life L0 is 50,000 hours. After one year of operation, the high-temperature heating surface life prediction model is used to calculate the high-temperature heating surface life data. The specific calculation process is: Tso is 873.15K, Tsi is 813.15K, Pso is 31.0MPa, Psi is 32.5MPa, Tw is 843.15K, t is 16200000s, K L is 0.8556, g is -0.01, h is -0.01, i is -0.02, j is -0.02, k is -0.06, l is -0.005,

[0059] L t =50000*0.8556*873.15^ -0.01 *813.15^ -0.01 *31.0^ -0.02 *32.5^ -0.02 *843.15^ -0.06 *16200000^ -0.005 =20000 hours.

[0060] If the preset life threshold is 60% of the initial stage of the pipe life, the preset life threshold is 30,000 hours, the actual life L t If it is less than 30,000 hours, it indicates that the life of the high-temperature heating surface changes rapidly, reminding maintenance personnel to inspect or replace the pipes.

[0061] The life data of the high-temperature heating surface after the time Ti is calculated by the high-temperature heating surface life prediction model, and the high-temperature heating surface can be monitored in real time. The change of the high-temperature heating surface life can be promptly and quickly known under the condition of normal operation of the unit. When the life data of the high-temperature heating surface is less than the preset life threshold, the high-temperature heating surface can be repaired in time. When problems occur, it is not necessary to repair it during regular maintenance, which does not affect the use efficiency of the unit and will not cause "over-repair" of the equipment.

[0062] The prediction model for the formation of oxide scale on high-temperature heated surfaces is as follows:

[0063] T t =f(Tso, Tsi, Pso, Psi, Tw, t)=K T·Tso m ·Tsi n ·Pso o ·Psi p ·Tw q ·t r

[0064] Among them, T t is the oxide scale thickness of the high-temperature heating surface after time Ti, Tso is the steam temperature at the inlet of the high-temperature heating surface, Tsi is the steam temperature at the inlet of the high-temperature heating surface, Pso is the steam pressure at the outlet of the high-temperature heating surface, Psi is the steam pressure at the outlet of the high-temperature heating surface, Tw is the wall temperature of the high-temperature heating surface, t is the effective operation time of the power plant unit, K T , m, n, o, p, q, and r are all weight coefficients.

[0065] In the prediction model of oxide scale formation on high temperature heating surface, K is set T The range is 0.5-1.2, the range of m is 0-0.1, the range of n is 0-0.1, the range of o is 0-0.1, the range of p is 0-0.1, the range of q is 0-0.1, and the range of r is 0-0.002.

[0066] The embodiment shows that in the initial stage, it is considered that the inside of the tube is relatively clean and no oxide scale is generated. After one year of operation, the oxide scale thickness Tt of the high-temperature heating surface after time Ti is calculated by the high-temperature heating surface oxide scale generation prediction model. The actual oxide scale thickness is calculated as follows: Tso is 873.15K, Tsi is 813.15K, Pso is 31.0MPa, Psi is 32.5MPa, Tw is 843.15K, t is 16200000s, K T is 0.9993, m is 0.01, n is 0.01, o is 0.02, p is 0.02, q is 0.06, r is 0.001,

[0067] T t =0.9993*873.15^ 0.01 *813.15^ 0.01 *31.0^ 0.02 *32.5^ 0.02 *843.15^0.06*16200000^ 0.001 =2mm.

[0068] A 2mm oxide scale is generated. If the preset thickness threshold is 1.5mm, the actual thickness of the oxide scale is T t If it is greater than 1.5mm, it indicates that the oxide scale is growing rapidly, reminding the maintenance personnel to inspect the pipe according to the change in thickness to remove the oxide scale.

[0069] The oxide scale thickness data of the high-temperature heating surface after the time Ti is calculated by the high-temperature heating surface oxide scale generation prediction model, and the oxide scale generation of the high-temperature heating surface can be monitored in real time. The generation of the oxide scale of the high-temperature heating surface can be promptly and quickly known under the condition of normal operation of the unit. When the oxide scale thickness data of the high-temperature heating surface is greater than the preset thickness threshold, the high-temperature heating surface can be promptly repaired to remove the oxide scale. When problems occur, timely maintenance is carried out without the need for regular maintenance, which does not affect the unit's utilization efficiency and does not cause "over-repair" of the equipment.

[0070] In the above three models, time Ti is different from the effective operation time t of the power plant units. Due to unit maintenance, adjustment, etc., the effective operation time t of the power plant units in one day (Ti is 24 hours) is generally less than Ti.

[0071] The condition inspection method for the heating surface of the boiler of a thermal power plant provided by the present invention can monitor the changes in the wall thickness of the water-cooled wall and the high-temperature heating surface and the generation of oxide scale on the high-temperature heating surface in real time by establishing a water-cooled wall tube wall thickness data prediction model, a high-temperature heating surface life prediction model, and a high-temperature heating surface oxide scale generation prediction model, and analyze the conditions of the water-cooled wall and the high-temperature heating surface, accurately understand the conditions of the water-cooled wall and the high-temperature heating surface in the furnace, and accurately understand the thickness of the water-cooled wall and the high-temperature heating surface and the generation of oxide scale, so as to judge whether there are defects and hidden dangers in the unit as a whole, or whether there are major defects in the system locally, so as to timely inspect the unit when problems occur, without having to inspect it only during regular inspections, without affecting the use efficiency of the unit, and without causing "over-repair" of the equipment, thereby improving the safety of unit operation.

[0072] The above embodiments are only for illustrating the technical concept and features of the present invention, and their purpose is to enable people familiar with the technology to understand the content of the present invention and implement it accordingly, and they cannot be used to limit the protection scope of the present invention. Any equivalent changes or modifications made according to the spirit of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for condition inspection of heating surfaces of boilers in thermal power plants, characterized in that: The steps include: S1. Collect coal quality parameters, water-cooled wall tube temperature, high-temperature heating surface tube temperature, high-temperature heating surface inlet and outlet steam temperature and pressure, and water-cooled wall reducing atmosphere composition and concentration data during unit operation; S2, based on the collected data in step S1, establish a water-cooled wall tube wall thickness data prediction model, a high-temperature heating surface life prediction model, and a high-temperature heating surface oxide scale generation prediction model, Obtain water wall thickness variation data based on water wall tube thickness data prediction model; Obtaining high-temperature heating surface life change data based on the high-temperature heating surface life prediction model; Acquire the generation data of the oxide scale of the high-temperature heating surface based on the prediction model of the oxide scale generation of the high-temperature heating surface; S3, based on the water-cooled wall thickness change data, high-temperature heating surface life change data, and high-temperature heating surface oxide scale generation data obtained in step S2, the water-cooled wall and the high-temperature heating surface are monitored in real time, and the conditions of the water-cooled wall and the high-temperature heating surface are analyzed; In step S3, analyzing the condition of the water-cooled wall includes: The water-cooled wall thickness change data includes the wall thickness data of the water-cooled wall after a time Ti. If the obtained water-cooled wall thickness data is less than a preset wall thickness threshold, the water-cooled wall needs to be repaired. If the obtained water-cooled wall thickness data is not less than the preset wall thickness threshold, no repair is required, wherein the preset wall thickness threshold is 50%-60% of the initial wall thickness of the water-cooled wall. In step S3, analyzing the condition of the high-temperature heating surface includes: The high-temperature heating surface life change data includes the life data of the high-temperature heating surface after a time Ti. If the obtained high-temperature heating surface life data is less than a preset life threshold, the high-temperature heating surface needs to be repaired. If the obtained high-temperature heating surface life data is not less than the preset life threshold, no repair is required. In step S3, analyzing the condition of the high-temperature heating surface includes: The generation data of the oxide scale of the high-temperature heating surface includes the oxide scale thickness data of the high-temperature heating surface after a time Ti. If the obtained oxide scale thickness data of the high-temperature heating surface is greater than a preset thickness threshold, the high-temperature heating surface needs to be repaired. If the obtained oxide scale thickness data of the high-temperature heating surface is not greater than the preset thickness threshold, no repair is required, wherein the preset thickness threshold is 50%-60% of the initial thickness of the high-temperature heating surface; The water-cooled wall tube thickness data prediction model is as follows: WT t =WT0-WT0×f(C、St、T、t)=WT0×K w ×O2 a ×CO b ×H2S c ×St d ×T e ×t f Among them, WT t is the wall thickness of the water-cooled wall after time Ti, WT0 is the wall thickness at the beginning of calculation, C is the concentration of reducing atmosphere, O2 is the concentration of O2, CO is the concentration of CO, H2S is the concentration of H2S; St is the sulfur content of coal; T is the wall temperature of the water-cooled wall, t is the effective operation time of the power plant unit, K w , a, b, c, d, e, and f are all weight coefficients; In the water-cooled wall tube thickness data prediction model, K is set w The range is 3-8, the range of a is -2-0, the range of b is 1-3, the range of c is 2-5, the range of d is 1-4, the range of e is 0.5-3, and the range of f is 0.5-3; The high temperature heating surface life prediction model is as follows: L t =L0×f(Tso、Tsi、Pso、Psi、Tw、t)=L0·K L ·Tso g ·Tsi h ·Pso i ·Psi j ·Tw k ·t l Among them, L t is the life of the heating surface after time Ti, L0 is the pipe life at the beginning of calculation, Tso is the steam temperature at the inlet of the high-temperature heating surface, Tsi is the steam temperature at the outlet of the high-temperature heating surface, Pso is the steam pressure at the inlet of the high-temperature heating surface, Psi is the steam pressure at the outlet of the high-temperature heating surface, Tw is the wall temperature of the heating surface, t is the effective operation time of the power plant unit, K L , g, h, i, j, k, and l are all weight coefficients; In the high temperature heating surface life prediction model, K is set L The range is 0.3-1.2, the range of g is -0.02-0, the range of h is -0.02-0, the range of i is -0.03-0, the range of j is -0.03-0, the range of k is -0.07-0, and the range of l is -0.007-0; The prediction model for the generation of oxide scale on the high temperature heated surface is as follows: T t =f(Tso、Tsi、Pso、Psi、Tw、t)=K T ·Tso m ·Tsi n ·Pso o ·Psi p ·Tw q ·t r Among them, T t is the oxide scale thickness of the high-temperature heating surface after time Ti, Tso is the steam temperature at the inlet of the high-temperature heating surface, Tsi is the steam temperature at the inlet of the high-temperature heating surface, Pso is the steam pressure at the outlet of the high-temperature heating surface, Psi is the steam pressure at the outlet of the high-temperature heating surface, Tw is the wall temperature of the high-temperature heating surface, t is the effective operation time of the power plant unit, K T , m, n, o, p, q, r are all weight coefficients; In the high temperature heating surface oxide scale generation prediction model, K is set T The range is 0.5-1.2, the range of m is 0-0.1, the range of n is 0-0.1, the range of o is 0-0.1, the range of p is 0-0.1, the range of q is 0-0.1, and the range of r is 0-0.002.

Citation Information

Patent Citations

  • Method and device for predicting thickness of tube wall of water cooling wall in furnace and readable storage medium

    CN112765872A