Methods for improving deformation of ultra-thin plates
By adjusting the grip position and tension direction of the thin core plate in the electroplating step, the deformation problem of multi-layer circuit board during laser drilling and electroplating is solved, the uniformity of copper thickness distribution and etching quality are improved, and the pattern collapse is reduced Blind hole risk.
Patent Information
- Application Number
- CN202110771429.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-07-08
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-07-08
AI Technical Summary
During laser drilling and electroplating of existing multi-layer circuit boards, the thin core core layer is prone to severe deformation, resulting in an increased risk of pattern collapse and blind holes, and the uneven pulling position of the electroplating wires affects the copper thickness distribution and etching quality.
By adjusting the clamping point position, tension direction and plate placement times of the thin core plate in different electroplating steps, the clamping single hole, small face times are facing up or double holes, small face times are facing up, and in each electroplating step, the clamping single holes, small face times are facing up, Specify the pulling direction to ensure complementary positions of the electroplating grips and regularize the copper thickness distribution.
It effectively reduces plate deformation, improves the uniformity and regularity of copper thickness distribution, reduces the problem of pattern collapse and blind holes, and improves the etching yield and copper thickness consistency.
Smart Images

Figure CN113630963B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of circuit boards, and in particular to a method for improving deformation of ultra-thin boards. Background Art
[0002] At present, circuit boards are divided into three major categories according to the number of layers: single-sided boards, double-sided boards, and multi-layer circuit boards. Multi-layer boards refer to printed boards with more than three layers of conductive graphic layers and insulating materials in between, and the conductive graphics in between are interconnected as required. Multi-layer circuit boards are the product of the development of electronic information technology towards high speed, multi-function, large capacity, small size, thinness, and light weight. Circuit boards are divided into flexible circuit boards (FPC), rigid circuit boards (PCB), and flexible and rigid combined circuit boards (FPCB) according to their characteristics.
[0003] However, the existing multilayer boards have the following defects:
[0004] 1. In the current high-end multi-layer board structure, the core layer in the middle is designed to be thinner and thinner (core thickness 1.6mil-2.5mil), and the number of laser drilled holes is as high as 800,000-1.5 million holes. After drilling the laser holes, the thin board needs to undergo horizontal copper flash plating LB, the first horizontal copper filling electroplating CU18-1, and the second horizontal copper filling electroplating CU18-2. After the thin core is pulled by the horizontal electroplating line for many times, the board is severely deformed at the pulling position.
[0005] 2. Board deformation increases the risk of blind hole collapse. In the early stage of testing, the blind hole welding ring was enlarged and the CFM window opening process was changed. The test results showed that the defective rate of blind hole collapse was high. Therefore, it is necessary to find a process method to improve the deformation of ultra-thin boards. Summary of the invention
[0006] In order to overcome the deficiencies of the prior art, one of the objectives of the present invention is to provide a method for improving the deformation of ultra-thin plates, which can solve the problem of severe plate deformation.
[0007] One of the purposes of the present invention is achieved by the following technical solution:
[0008] A method for improving deformation of an ultra-thin plate comprises the following steps:
[0009] Cutting preparation steps: Select the thin core board and process it into the required size;
[0010] One preparation step: adjust the clamping point position, pulling direction and board placement of the thin core board in the horizontal copper flash plating, so that the single hole and small surface of the horizontal copper flash plating are facing upwards;
[0011] Copper flash plating step: pulling the thin core board along a first direction to perform copper flash plating;
[0012] Secondary preparation steps: adjust the clamping point position, pulling direction and board placement of the thin core board in the first horizontal copper filling electroplating, so that the double holes and small surface of the thin core board are facing upwards in the first horizontal copper filling electroplating;
[0013] A horizontal copper filling electroplating step: pulling the thin core board along the first direction to perform horizontal copper flash plating;
[0014] Three preparation steps: adjust the clamping point position, pulling direction and board placement of the thin core board in the secondary horizontal copper filling electroplating, so that the single hole and small surface of the secondary horizontal copper filling electroplating are facing upward;
[0015] Secondary horizontal copper filling electroplating step: pulling the thin core board along a second direction opposite to the first direction to perform secondary horizontal copper filling electroplating.
[0016] Furthermore, in the cutting preparation step, it is checked whether the size processing is in place, if so, the next step is executed, if not, rework is performed.
[0017] Furthermore, in the cutting preparation step, the surface is cleaned after the processing is completed.
[0018] Furthermore, in the cutting preparation step, it is checked whether the surface finish and cleanliness of the thin core board meet the requirements. If so, the next step is executed; if not, rework or scrapping is performed.
[0019] Furthermore, in the material preparation step, a thin core board with a thickness of 1.6-2.5 mil is selected.
[0020] Furthermore, in the one-time preparation step, check whether the clamping part in the horizontal copper flash plating is a single hole and whether the small surface is facing upward. If so, execute the next step, if not, readjust.
[0021] Furthermore, in the secondary preparation step, check whether the clamping holes in the first horizontal copper filling electroplating are double holes and whether the small side is facing upward. If so, execute the next step, if not, readjust.
[0022] Furthermore, in the three preparation steps, check whether the clamping hole in the secondary horizontal copper filling electroplating is a single hole and whether the small side is facing upward. If so, execute the next step, if not, readjust.
[0023] Furthermore, in the copper flash plating step, the thin core board is pulled leftward for copper flash plating.
[0024] Furthermore, in the secondary horizontal copper filling electroplating step, the thin core board is pulled to the right to perform secondary horizontal copper filling electroplating.
[0025] Compared with the prior art, the present invention has the following beneficial effects:
[0026] Select a thin core board and process it in place according to the required size; adjust the clamping point position, pulling direction and board placement of the thin core board in horizontal copper flash plating, so that the single hole and small surface of the horizontal copper flash plating are facing upward; pull the thin core board along the first direction for copper flash plating; adjust the clamping point position, pulling direction and board placement of the thin core board in the first horizontal copper filling electroplating, so that the double holes and small surface of the first horizontal copper filling electroplating are facing upward; pull the thin core board along the first direction for the first horizontal copper filling electroplating; adjust the clamping point position, pulling direction and board placement of the thin core board in the second horizontal copper filling electroplating, so that the single hole and small surface of the second horizontal copper filling electroplating are facing upward; pull the thin core board along the second direction opposite to the first direction for the second horizontal copper filling electroplating. The tension at the electroplating clamping point is complementary to solve the problem of pulling and deformation of the thin core board. During electroplating, the direction and surface of the board are specified, which improves the uniformity of the copper thickness on the board surface. The copper thickness distribution is consistent and has a strong regularity, which is very helpful for capturing the DES etching parameters and effectively improves the etching yield.
[0027] The above description is only an overview of the technical solution of the present invention. In order to more clearly understand the technical means of the present invention, it can be implemented in accordance with the contents of the specification. In order to make the above and other purposes, features and advantages of the present invention more obvious and easy to understand, the following specifically cites a preferred embodiment and describes it in detail with the accompanying drawings as follows. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 A flow chart of a preferred embodiment of the method for improving deformation of ultra-thin plates of the present invention;
[0029] Figure 2 is a schematic diagram of the pinch point location;
[0030] Figure 3 This is a diagram of the stacking structure of a multilayer board. DETAILED DESCRIPTION
[0031] The present invention is further described below in conjunction with the accompanying drawings and specific implementation methods. It should be noted that, under the premise of no conflict, the various embodiments or technical features described below can be arbitrarily combined to form a new embodiment.
[0032] It should be noted that when a component is referred to as being "fixed to" another component, it may be directly on the other component or there may also be a component centered. When a component is considered to be "connected to" another component, it may be directly connected to the other component or there may also be a component centered. When a component is considered to be "set on" another component, it may be directly set on the other component or there may also be a component centered. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only.
[0033] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.
[0034] See also Figure 1 , a method for improving deformation of an ultra-thin plate, comprising the following steps:
[0035] Material preparation step: select a thin core board and process it in place according to the required size; preferably, in the material preparation step, check whether the size processing is in place, if yes, proceed to the next step, if not, rework. Clean the surface after processing. Check whether the surface finish and cleanliness of the thin core board meet the requirements, if yes, proceed to the next step, if not, rework or scrap.
[0036] Preferably, in the material preparation step, a thin core board with a thickness of 1.6-2.5 mil is selected.
[0037] A preparation step: adjust the clamping point position, pulling direction and board placement surface of the thin core board in the horizontal copper flash plating, so that the single hole is clamped in the horizontal copper flash plating and the small surface is facing upward; preferably, in the one preparation step, check whether the clamping part in the horizontal copper flash plating is a single hole and whether the small surface is facing upward. If so, execute the next step, if not, readjust.
[0038] Copper flash plating step: pulling the thin core board along a first direction to perform copper flash plating;
[0039] Secondary preparation step: adjust the clamping point position, pulling direction and board placement surface of the thin core board in the first horizontal copper filling electroplating, so that the clamping holes in the first horizontal copper filling electroplating are double holes and the small surface is facing upward; preferably, in the secondary preparation step, check whether the clamping holes in the first horizontal copper filling electroplating are double holes and whether the small surface is facing upward. If so, execute the next step, if not, readjust.
[0040] A horizontal copper filling electroplating step: pulling the thin core board along the first direction to perform a horizontal copper filling electroplating;
[0041] Three preparation steps: adjust the clamping point position, pulling direction and board placement surface of the thin core board in the secondary horizontal copper filling electroplating, so that the clamping hole in the secondary horizontal copper filling electroplating is a single hole and the small surface is facing upward; preferably, in the three preparation steps, check whether the clamping hole in the secondary horizontal copper filling electroplating is a single hole and whether the small surface is facing upward. If so, execute the next step, if not, readjust.
[0042] Secondary horizontal copper filling electroplating steps: Pull the thin core board in the second direction opposite to the first direction for secondary horizontal copper filling electroplating. Complement the pulling force at the electroplating clamping point to solve the problem of pulling and deforming the thin core board. During electroplating, the direction and surface of the board are specified, which improves the uniformity of the copper thickness on the board surface. The copper thickness distribution is consistent and has a strong regularity, which is very helpful for grasping the DES etching parameters and effectively improves the etching yield.
[0043] Specifically, during pattern transfer exposure, the thin core board is less deformed, which reduces the problem of pattern collapse and blind holes caused by board deformation.
[0044] Specifically, in the copper flash plating step, the thin core board is pulled to the left for copper flash plating, that is, the first direction is to the left. In the secondary horizontal copper filling electroplating step, the thin core board is pulled to the right for secondary horizontal copper filling electroplating, that is, the second direction is to the right. In this application, a single hole is a single L hole, and a double hole is a double L hole. Please refer to Figure 2 , is a schematic diagram of the clamping point location of this application. Please refer to Figure 3 , which is a stacking diagram of the multilayer board of this application.
[0045] The above-mentioned embodiments are only preferred embodiments of the present invention and cannot be used to limit the scope of protection of the present invention. Any non-substantial changes and substitutions made by technicians in this field on the basis of the present invention shall fall within the scope of protection required by the present invention.
Claims
1. A method for improving deformation of ultra-thin plates, characterized in that: The following steps are involved: Cutting preparation steps: Select the thin core board and process it into the required size; One preparation step: adjust the clamping point position, pulling direction and board placement of the thin core board in the horizontal copper flash plating, so that the single hole and small surface of the horizontal copper flash plating are facing upwards; Copper flash plating step: pulling the thin core board along a first direction, i.e., the direction of tension, to perform copper flash plating; Secondary preparation steps: adjust the clamping point position, pulling direction and board placement of the thin core board in the first horizontal copper filling electroplating, so that the double holes and small surface of the thin core board are facing upwards in the first horizontal copper filling electroplating; A horizontal copper filling electroplating step: pulling the thin core board along the first direction to perform horizontal copper flash plating; Three preparation steps: adjust the clamping point position, pulling direction and board placement of the thin core board in the secondary horizontal copper filling electroplating, so that the single hole and small surface of the secondary horizontal copper filling electroplating are facing upward; Secondary horizontal copper filling electroplating step: pulling the thin core board along a second direction opposite to the first direction to perform secondary horizontal copper filling electroplating.
2. The method for improving deformation of ultra-thin plates according to claim 1, characterized in that: In the cutting preparation step, check whether the size processing is in place. If so, proceed to the next step. If not, rework is performed.
3. The method for improving deformation of ultra-thin plates according to claim 1, characterized in that: In the material preparation step, the surface is cleaned after processing is completed.
4. The method for improving deformation of ultra-thin plates according to claim 1, characterized in that: In the material preparation step, check whether the surface finish and cleanliness of the thin core board meet the requirements. If so, proceed to the next step. If not, rework or scrapping is performed.
5. The method for improving deformation of ultra-thin plates according to claim 1, characterized in that: In the material preparation step, a thin core board with a thickness of 1.6-2.5 mil is selected.
6. The method for improving deformation of ultra-thin plates according to claim 1, characterized in that: In the one preparation step, check whether the clamping part in the horizontal copper flash plating is a single hole and whether the small surface is facing upward. If so, execute the next step, if not, readjust.
7. The method for improving deformation of ultra-thin plates according to claim 1, characterized in that: In the secondary preparation step, check whether the clamping hole in the first horizontal copper filling electroplating is a double hole and whether the small side is facing upward. If so, execute the next step, if not, readjust.
8. The method for improving deformation of ultra-thin plates according to claim 1, characterized in that: In the three preparation steps, check whether the clamping hole in the secondary horizontal copper filling electroplating is a single hole and whether the small side is facing upward. If so, execute the next step, if not, readjust.
9. The method for improving deformation of ultra-thin plates according to claim 1, characterized in that: In the copper flash plating step, the thin core board is pulled leftward for copper flash plating.
10. The method for improving deformation of ultra-thin plates according to claim 1, characterized in that: In the secondary horizontal copper filling electroplating step, the thin core board is pulled to the right to perform secondary horizontal copper filling electroplating.