A carbon dioxide thickening fracturing system and process method thereof

Through the mixing of liquid carbon dioxide thickener and water and high-pressure pump injection technology, the problem that conventional liquid carbon dioxide cannot create fractures is solved, and the effective transformation of the reservoir and production increase are achieved.

CN113738333BActive Publication Date: 2024-10-01YANAN SHUANG FENG GRP
View PDF 13 Cites 0 Cited by

Patent Information

Application Number
CN202111208843.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-10-18
Publication Date
2024-10-01
Estimated Expiration
2041-10-18

AI Technical Summary

Technical Problem

Conventional liquid carbon dioxide cannot effectively create fractures in the reservoir, resulting in poor reservoir stimulation effects.

Method used

Design a carbon dioxide thickening fracturing system that mixes liquid CO2 thickener with water to form a fracturing fluid of moderate consistency, and uses liquid carbon dioxide high-pressure pump injection technology to thicken liquid carbon dioxide in the reservoir and combine it with the fracturing fluid Together, they carry proppant to achieve effective reservoir transformation.

Benefits of technology

It improves the viscosity and carrying capacity of liquid carbon dioxide, enhances the reservoir modification effect, reduces the impact of liquid on the reservoir, and increases the flowback rate and single well production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113738333B_ABST
    Figure CN113738333B_ABST
Patent Text Reader

Abstract

The present invention is applicable to the field of fracturing transformation, and provides a carbon dioxide thickening fracturing system, including an output system, a fracturing fluid processing system and a liquid CO2 processing system: the fracturing fluid processing system includes: a liquid CO2 thickener stock solution processing system and a fracturing fluid thickening system; the process method steps are as follows: 1) a telescopic short circuit 21, a safety joint 23, a low-temperature and high-pressure gas-sealed hydraulic anchor 24, a low-temperature and high-pressure gas-sealed anchored packer 25, a sandblasting nozzle 26 and a fracturing completion oil pipe 22 are lowered into the well through a well repair machinery. The present invention realizes the thickening of liquid carbon dioxide, the creation of seams by thickening liquid carbon dioxide, and the carrying of sand by thickening liquid carbon dioxide and liquid through the design of a fracturing fluid and liquid carbon dioxide pumping program, which can effectively reduce the impact of liquid on the reservoir, improve the return flow rate, maximize the reservoir transformation effect, and increase the single well production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of fracturing transformation, and in particular relates to a carbon dioxide thickening fracturing system and a process method thereof. Background Art

[0002] Fracturing technology is the most direct and effective method to improve oil recovery and single well production. The oil and gas industry has also conducted a large number of field tests and applications over the years and developed a variety of process methods to improve the effect of fracturing. CO2 fracturing technology is a transformation process that replaces water-based fracturing fluid with liquid CO2 on the basis of traditional fracturing technology. It mainly uses liquid CO2 to create fractures and carry sand to achieve the purpose of reservoir transformation.

[0003] Chinese patent CN110761764A discloses a liquid carbon dioxide fracturing method. This patent is an optimized design for the dry CO2 fracturing process, and the problem it addresses does not involve the performance of CO2 itself.

[0004] Chinese patents 2019100482187 (application number) and CN109736767A (publication number) involve a supercritical carbon dioxide fracturing production enhancement process. The invention is a CO2 pure dry fracturing process, that is, only liquid CO2 is used in the fracturing process, and no water-based fracturing fluid is involved;

[0005] Chinese patent CN108864387B provides a drag reducer for carbon dioxide dry fracturing and its application. This patent is a drag reducer developed for carbon dioxide dry fracturing, which is an optimization of liquid carbon dioxide and does not involve related process methods combining water-based and liquid carbon dioxide. Summary of the invention

[0006] The object of the present invention is to provide a carbon dioxide thickening fracturing system and a process method thereof, aiming to solve the problem that conventional liquid carbon dioxide cannot normally create fractures in a reservoir.

[0007] The present invention is implemented as follows: a carbon dioxide thickening fracturing system, including an output system, a fracturing fluid processing system and a liquid CO2 processing system:

[0008] The fracturing fluid processing system includes: a liquid CO2 thickener stock solution processing system and a fracturing fluid thickening system;

[0009] The liquid CO2 thickener stock solution processing system includes: a liquid CO2 thickener stock solution tank 18, a CO2 thickener solution preparation tank, a water storage tank, a sand mixing liquid supply vehicle, a liquid high-pressure pump vehicle and a fracturing fluid wellhead injection head; the liquid high-pressure pump vehicle is connected to the output system through a normal temperature high-pressure pipeline, the liquid high-pressure pump vehicle is connected to the sand mixing liquid supply vehicle through a medium-pressure normal temperature pipeline, the sand mixing liquid supply vehicle is connected to the CO2 thickener solution preparation tank through a low-pressure normal temperature pipeline, the CO2 thickener solution preparation tank is connected to the liquid CO2 thickener stock solution tank through a low-pressure normal temperature pipeline, the thickener solution preparation tank is connected to the water storage tank through a low-pressure normal temperature pipeline, and the water storage tank is connected to the sand mixing liquid supply vehicle through a low-pressure normal temperature pipeline;

[0010] The fracturing fluid thickening system is connected to the sand mixing and liquid supply vehicle, and the liquid CO2 processing system is connected to one end of the output system;

[0011] The output system includes: production casing, telescopic short-circuit, fracturing completion oil pipe, safety joint low-temperature high-pressure gas-sealed hydraulic anchor, low-temperature high-pressure gas-sealed anchored packer, sandblasting nozzle, reservoir fracture, injection wellhead, perforation hole; the telescopic short-circuit, safety joint, low-temperature high-pressure gas-sealed hydraulic anchor, low-temperature high-pressure gas-sealed anchored packer, sandblasting nozzle are respectively connected with the fracturing completion oil pipe, the perforation hole is arranged on the production casing, the injection wellhead is equipped with a fracturing fluid wellhead injection head, and the fracturing fluid wellhead injection head is connected with a normal temperature high-pressure pipeline;

[0012] The liquid CO2 processing system comprises: a liquid carbon dioxide storage tank, a cryogenic pipeline, a carbon dioxide booster pump, a medium-pressure cryogenic pipeline, a liquid carbon dioxide high-pressure pump truck, a cryogenic and high-pressure pipeline, and a liquid carbon dioxide wellhead injection head; the liquid carbon dioxide storage tank is connected to the carbon dioxide booster pump via a cryogenic pipeline, the carbon dioxide booster pump is connected to the liquid carbon dioxide high-pressure pump truck via a medium-pressure cryogenic pipeline, the liquid carbon dioxide high-pressure pump truck is connected to the liquid carbon dioxide wellhead injection head via a cryogenic and high-pressure pipeline, and the liquid carbon dioxide wellhead injection head is connected to the injection wellhead;

[0013] The carbon dioxide thickening fracturing process comprises the following steps:

[0014] 1) The telescopic short-circuit, safety joint, low-temperature and high-pressure gas-sealed hydraulic anchor, low-temperature and high-pressure gas-sealed anchored packer, sandblasting nozzle and fracturing completion tubing are lowered into the well through the well repair machinery. The low-temperature and high-pressure gas-sealed anchored packer is seated and started by rotating the fracturing completion tubing, and the anchoring machinery contacts and anchors the inner wall of the production casing;

[0015] 2) The concentration of the CO2 thickener stock solution in the liquid CO2 thickener stock tank is 80-90%. The CO2 thickener stock solution is transported to the CO thickener solution configuration tank through a low-pressure normal temperature pipeline. The water storage tank is transported to the CO2 thickener solution configuration tank through a low-pressure normal temperature pipeline. The CO2 thickener stock solution is mixed with water in the CO2 thickener solution configuration tank. The CO2 thickener stock solution concentration is diluted to 12-17%. The CO2 thickener solution configuration tank transports the diluted CO2 thickener solution with a concentration of 12-17% to the sand mixing liquid supply vehicle through a low-pressure normal temperature pipeline. The water storage tank transports water to the sand mixing liquid supply vehicle through a low-pressure normal temperature pipeline. The CO2 thickener solution is mixed with water in the sand mixing liquid supply vehicle, and a CO2 thickener solution with a concentration of 1-1.5% is formed at this time;

[0016] 3) The fracturing fluid thickener stock tank delivers the fracturing fluid thickener to the sand mixing liquid supply vehicle through a low-pressure normal temperature pipeline, and the fracturing fluid thickener is mixed with a CO2 thickener solution with a concentration of 1-1.5% to form a fracturing fluid with a fracturing fluid thickener concentration of 0.4-0.8% and a fracturing fluid viscosity of 40-60mPa.S;

[0017] 4) The mixed sand supply truck pressurizes the mixed solution with a CO2 thickener concentration of 1-1.5% and a fracturing fluid thickener concentration of 0.4-0.8% to 0.5-0.8MPa, and then delivers it to the liquid high-pressure pump truck through a medium-pressure normal temperature pipeline. The liquid high-pressure pump truck pressurizes the fracturing fluid with a CO2 thickener concentration of 1-1.5% and a fracturing fluid thickener concentration of 0.4-0.8% to 50-65MPa, and then delivers it to the fracturing fluid wellhead injection head through a normal temperature high-pressure pipeline;

[0018] 5) The low-temperature and low-pressure liquid CO2 with a temperature of -35--28°C in the liquid carbon dioxide storage tank is transported to the carbon dioxide booster pump through a low-temperature pipeline. The carbon dioxide booster pump pressurizes the low-temperature liquid CO2 to 2.4-3.0MPa, and the temperature of the liquid CO2 rises to -20--16°C. After the carbon dioxide booster pump pressurizes the liquid CO2, it is transported to the liquid carbon dioxide high-pressure pump truck through a medium-pressure low-temperature pipeline. The liquid CO2 with a pressure of 2.4-2.8MPa and a temperature of -20--16°C is pressurized to 50-65MPa by the liquid carbon dioxide high-pressure pump truck, and the temperature rises to above 0°C, and then it is transported to the liquid carbon dioxide wellhead injection head through a low-temperature and high-pressure pipeline;

[0019] 6) The treated fracturing fluid in step 4) is mixed with the liquid CO2 treated by the liquid carbon dioxide high-pressure pump truck 5 in step 5) at the injection wellhead 28. During the mixing process, the liquid CO2 extracts the CO2 thickener from the mixed solution, and the viscosity of the liquid CO2 increases from 0.3-0.5 mPa.S to 40-60 mPa.S. During the mixing process, the displacement of the liquid carbon dioxide from the liquid carbon dioxide wellhead injection head into the injection wellhead is 2.5-3 times the displacement of the fracturing fluid from the fracturing fluid wellhead injection head into the injection wellhead;

[0020] 7) The mixture of liquid CO2 and fracturing fluid is transported to the sandblasting nozzle 26 in the fracturing completion tubing 22, enters the production casing 20, and then enters the reservoir through the perforation holes 31, forming reservoir fractures 27;

[0021] 8) The fracturing proppant storage tank transports the fracturing proppant to the sand mixing and liquid supply truck through the proppant delivery pipeline, and mixes with the mixed liquid of liquid CO2 and fracturing fluid. The viscosity of the liquid CO2 at this time reaches 40-60mPa.S after thickening, which can effectively carry the fracturing proppant. The fracturing proppant, fracturing fluid and liquid CO2 are transported to the sandblasting nozzle through the fracturing completion tubing, enter the production casing and then enter the reservoir cracks through the perforated holes. The fracturing fluid and liquid CO2 are filtered out and enter the reservoir, and the proppant remains in the reservoir cracks to support the cracks, so that the crack morphology is kept in an open state.

[0022] A further technical solution is that the fracturing fluid thickening system includes: a fracturing proppant storage tank and a fracturing fluid thickener stock liquid storage tank; the fracturing proppant storage tank is connected to the proppant delivery pipeline, the proppant delivery pipeline is connected to the sand mixing and liquid supply vehicle, and the fracturing fluid thickener stock liquid storage tank is connected to the sand mixing and liquid supply vehicle through a low-pressure normal temperature pipeline.

[0023] According to a further technical solution, the liquid carbon dioxide wellhead injection head is installed on the injection wellhead by means of a flange, and the fracturing fluid wellhead injection head is connected to the injection wellhead by means of a flange.

[0024] According to a further technical solution, the telescopic short-circuit, the safety joint, the low-temperature and high-pressure gas-sealed hydraulic anchor, the low-temperature and high-pressure gas-sealed anchored packer and the sandblasting nozzle are respectively connected to the fracturing completion tubing by means of threads.

[0025] Compared with the prior art, the present invention has the following beneficial effects:

[0026] The present invention realizes the thickening of liquid carbon dioxide, the creation of seams by thickened liquid carbon dioxide, and the carrying of sand by thickened liquid carbon dioxide and liquid through the design of fracturing fluid and liquid carbon dioxide pumping program. During the flowback process, the liquid carbon dioxide undergoes a phase change from liquid to gaseous in the reservoir, and all the injected fracturing fluid is displaced out of the ground, effectively reducing the impact of the liquid on the reservoir, improving the flowback rate, maximizing the reservoir transformation effect, and increasing the single well production. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 The figure is a schematic diagram of the connection between various system structures in one embodiment of the present invention.

[0028] Notes on figure numbers: 1 liquid carbon dioxide storage tank, 2 cryogenic pipeline, 3 carbon dioxide booster pump, 4 medium-pressure cryogenic pipeline, 5 liquid carbon dioxide high-pressure pump truck, 6 cryogenic high-pressure pipeline, 7 liquid carbon dioxide wellhead injection head, 8 fracturing fluid wellhead injection head, 9 normal temperature high-pressure pipeline, 10 liquid high-pressure pump truck, 12 sand mixing liquid supply truck, 13 low-pressure normal temperature pipeline, 14CO2 thickener solution preparation tank, 18 liquid CO2 thickener stock tank, 19 water storage tank, 20 production casing, 21 telescopic short circuit, 22 fracturing completion oil pipe, 23 safety joint, 24 cryogenic high-pressure gas-sealed hydraulic anchor, 25 cryogenic high-pressure gas-sealed anchored packer, 26 sandblasting nozzle, 27 reservoir fracture, 28 injection wellhead, 30 fracturing fluid thickener stock storage tank, 31 perforation holes, 32 fracturing proppant storage tank, 33 proppant delivery pipeline. DETAILED DESCRIPTION

[0029] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention will be further described in detail in conjunction with the accompanying drawings and the following embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0030] The specific implementation of the present invention is described in detail below in conjunction with specific embodiments.

[0031] Embodiment 1, a carbon dioxide thickening fracturing process, comprising the following steps:

[0032] 1) The telescopic short circuit 21, the safety joint 23, the low-temperature and high-pressure gas-sealed hydraulic anchor 24, the low-temperature and high-pressure gas-sealed anchored packer 25, the sandblasting nozzle 26 and the fracturing completion tubing 22 are lowered into the well through the well repair machinery, and the low-temperature and high-pressure gas-sealed anchored packer 25 is seated and started by rotating the fracturing completion tubing 22, and the anchoring machinery contacts and anchors the inner wall of the production casing 20;

[0033] The seal is close to the inner wall of the production casing 20 to play a sealing role. The low-temperature and high-pressure gas-sealed hydraulic anchor 24 is activated when high-pressure fracturing fluid and liquid CO2 enter the oil pipe, and contacts and anchors with the inner wall of the production casing 20. When the low-temperature liquid CO2 enters the fracturing completion oil pipe 22, the fracturing completion oil pipe 22 will shrink due to the change in temperature. At this time, the telescopic short circuit 21 will open and then stretch to make up for the shrinkage distance of the fracturing completion oil pipe 22, thereby ensuring the safety of the pipe string.

[0034] 2) The concentration of the CO2 thickener stock solution in the liquid CO2 thickener stock tank is 80%, the CO2 thickener stock solution is transported to the CO2 thickener solution configuration tank 14 through the low-pressure normal temperature pipeline 13, the water storage tank 19 is transported to the CO2 thickener solution configuration tank 14 through the low-pressure normal temperature pipeline 13, the CO2 thickener stock solution is mixed with water in the CO2 thickener solution configuration tank 14, the CO2 thickener stock solution concentration is diluted to 12%, the CO2 thickener solution configuration tank 14 transports the diluted CO2 thickener solution with a concentration of 12% to the sand mixing liquid supply vehicle 12 through the low-pressure normal temperature pipeline 13, the water storage tank 19 transports water to the sand mixing liquid supply vehicle 12 through the low-pressure normal temperature pipeline 13, the CO2 thickener solution is mixed with water in the sand mixing liquid supply vehicle 12, and a CO2 thickener solution with a CO2 thickener solution concentration of 1% is formed at this time;

[0035] 3) The fracturing fluid thickener stock liquid storage tank 30 delivers the fracturing fluid thickener to the sand mixing liquid supply vehicle 12 through the low-pressure normal temperature pipeline 13, and the fracturing fluid thickener is mixed with the CO2 thickener solution with a concentration of 1% to form a fracturing fluid with a fracturing fluid thickener concentration of 0.4% and a fracturing fluid viscosity of 40mPa.S;

[0036] 4) The sand mixing and liquid supply vehicle 12 pressurizes the mixed solution with a CO2 thickener concentration of 1% and a fracturing fluid thickener concentration of 0.4% to 0.5 MPa, and then delivers it to the liquid high-pressure pump vehicle 10 through a medium-pressure normal temperature pipeline. The liquid high-pressure pump vehicle 10 pressurizes the fracturing fluid with a CO2 thickener concentration of 1% and a fracturing fluid thickener concentration of 0.4% to 50 MPa, and then delivers it to the fracturing fluid wellhead injection head 8 through a normal temperature high-pressure pipeline 9;

[0037] 5) The low-temperature and low-pressure liquid CO2 with a temperature of -35°C in the liquid carbon dioxide storage tank 1 is transported to the carbon dioxide booster pump 3 through the low-temperature pipeline 2. The carbon dioxide booster pump 3 pressurizes the low-temperature liquid CO2 to 2.4MPa, and the temperature of the liquid CO2 rises to -20°C. The carbon dioxide booster pump 3 pressurizes the liquid CO2 and then transports it to the liquid carbon dioxide high-pressure pump truck 5 through the medium-pressure low-temperature pipeline 4. The liquid CO2 with a pressure of 2.4MPa and a temperature of -20°C is pressurized to 50MPa by the liquid carbon dioxide high-pressure pump truck 5, and the temperature is raised to above 0°C, and then transported to the liquid carbon dioxide wellhead injection head 7 through the low-temperature and high-pressure pipeline 6;

[0038] 6) The treated fracturing fluid in step 4) is mixed with the liquid CO2 treated by the liquid carbon dioxide high-pressure pump truck 5 in step 5) at the injection wellhead 28. During the mixing process, the liquid CO2 extracts the CO2 thickener from the mixed solution, and the viscosity of the liquid CO2 increases from 0.3 mPa.S to 40 mPa.S. During the mixing process, the displacement of the liquid carbon dioxide from the liquid carbon dioxide wellhead injection head 7 into the injection wellhead 28 is 2.5-3 times the displacement of the fracturing fluid from the fracturing fluid wellhead injection head 8 into the injection wellhead 28;

[0039] 7) The mixture of liquid CO2 and fracturing fluid is transported to the sandblasting nozzle 26 in the fracturing completion tubing 22, enters the production casing 20, and then enters the reservoir through the perforation holes 31, forming reservoir fractures 27;

[0040] 8) The fracturing proppant storage tank 32 transports the fracturing proppant to the sand mixing and liquid supply vehicle 12 through the proppant delivery pipeline 33, and mixes with the mixed liquid of liquid CO2 and fracturing fluid. At this time, the viscosity of the liquid CO2 reaches 40mPa.S after thickening, which can effectively carry the fracturing proppant. The fracturing proppant, fracturing fluid and liquid CO2 are transported to the sandblasting nozzle 26 through the fracturing completion oil pipe 22, enter the production casing 20, and then enter the reservoir cracks 27 through the perforation holes 31. The fracturing fluid and liquid CO2 are filtered out and enter the reservoir, and the proppant remains in the reservoir cracks 27 to support the cracks, so that the crack morphology is kept in an open state.

[0041] Embodiment 2, a carbon dioxide thickening fracturing process, comprising the following steps:

[0042] 1) The telescopic short circuit 21, the safety joint 23, the low-temperature and high-pressure gas-sealed hydraulic anchor 24, the low-temperature and high-pressure gas-sealed anchored packer 25, the sandblasting nozzle 26 and the fracturing completion tubing 22 are lowered into the well through the well repair machinery, and the low-temperature and high-pressure gas-sealed anchored packer 25 is seated and started by rotating the fracturing completion tubing 22, and the anchoring machinery contacts and anchors the inner wall of the production casing 20;

[0043] The seal is close to the inner wall of the production casing 20 to play a sealing role. The low-temperature and high-pressure gas-sealed hydraulic anchor 24 is activated when high-pressure fracturing fluid and liquid CO2 enter the oil pipe, and contacts and anchors with the inner wall of the production casing 20. When the low-temperature liquid CO2 enters the fracturing completion oil pipe 22, the fracturing completion oil pipe 22 will shrink due to the change in temperature. At this time, the telescopic short circuit 21 will open and then stretch to make up for the shrinkage distance of the fracturing completion oil pipe 22, thereby ensuring the safety of the pipe string.

[0044] 2) The concentration of the CO2 thickener stock solution in the liquid CO2 thickener stock tank is 85%, the CO2 thickener stock solution is transported to the CO2 thickener solution configuration tank 14 through the low-pressure normal temperature pipeline 13, the water storage tank 19 is transported to the CO2 thickener solution configuration tank 14 through the low-pressure normal temperature pipeline 13, the CO2 thickener stock solution is mixed with water in the CO2 thickener solution configuration tank 14, the CO2 thickener stock solution concentration is diluted to 15%, the CO2 thickener solution configuration tank 14 transports the diluted CO2 thickener solution with a concentration of 15% to the sand mixing liquid supply vehicle 12 through the low-pressure normal temperature pipeline 13, the water storage tank 19 transports water to the sand mixing liquid supply vehicle 12 through the low-pressure normal temperature pipeline 13, the CO2 thickener solution is mixed with water in the sand mixing liquid supply vehicle 12, and a CO2 thickener solution with a concentration of 1-1.5% is formed at this time;

[0045] 3) The fracturing fluid thickener stock liquid storage tank 30 delivers the fracturing fluid thickener to the sand mixing liquid supply vehicle 12 through the low-pressure normal temperature pipeline 13, and the fracturing fluid thickener is mixed with a CO2 thickener solution with a concentration of 1.2% to form a fracturing fluid with a fracturing fluid thickener concentration of 0.6% and a fracturing fluid viscosity of 50 mPa.S;

[0046] 4) The sand mixing and liquid supply truck 12 pressurizes the mixed solution with a CO2 thickener concentration of 1.2% and a fracturing fluid thickener concentration of 0.6% to 0.6MPa, and then delivers it to the liquid high-pressure pump truck 10 through a medium-pressure normal temperature pipeline. The liquid high-pressure pump truck 10 pressurizes the fracturing fluid with a CO2 thickener concentration of 1.2% and a fracturing fluid thickener concentration of 0.6% to 60MPa, and then delivers it to the fracturing fluid wellhead injection head 8 through a normal temperature high-pressure pipeline 9;

[0047] 5) The low-temperature and low-pressure liquid CO2 with a temperature of -31°C in the liquid carbon dioxide storage tank 1 is transported to the carbon dioxide booster pump 3 through the low-temperature pipeline 2. The carbon dioxide booster pump 3 pressurizes the low-temperature liquid CO2 to 2.6MPa, and the temperature of the liquid CO2 rises to -18°C. After the carbon dioxide booster pump 3 pressurizes the liquid CO2, it is transported to the liquid carbon dioxide high-pressure pump truck 5 through the medium-pressure low-temperature pipeline 4. The liquid CO2 with a pressure of 2.6MPa and a temperature of -18°C is pressurized to 60MPa by the liquid carbon dioxide high-pressure pump truck 5, and the temperature is raised to above 0°C, and then transported to the liquid carbon dioxide wellhead injection head 7 through the low-temperature and high-pressure pipeline 6;

[0048] 6) The treated fracturing fluid in step 4) is mixed with the liquid CO2 treated by the liquid carbon dioxide high-pressure pump truck 5 in step 5) at the injection wellhead 28. During the mixing process, the liquid CO2 extracts the CO2 thickener from the mixed solution, and the viscosity of the liquid CO2 increases from 0.4 mPa.S to 50 mPa.S. During the mixing process, the displacement of the liquid carbon dioxide from the liquid carbon dioxide wellhead injection head 7 into the injection wellhead 28 is 2.5-3 times the displacement of the fracturing fluid from the fracturing fluid wellhead injection head 8 into the injection wellhead 28;

[0049] 7) The mixture of liquid CO2 and fracturing fluid is transported to the sandblasting nozzle 26 in the fracturing completion tubing 22, enters the production casing 20, and then enters the reservoir through the perforation holes 31, forming reservoir fractures 27;

[0050] 8) The fracturing proppant storage tank 32 transports the fracturing proppant to the sand mixing and liquid supply vehicle 12 through the proppant delivery pipeline 33, and mixes with the mixed liquid of liquid CO2 and fracturing fluid. At this time, the viscosity of the liquid CO2 reaches 50mPa.S after thickening, which can effectively carry the fracturing proppant. The fracturing proppant, fracturing fluid and liquid CO2 are transported to the sandblasting nozzle 26 through the fracturing completion oil pipe 22, enter the production casing 20, and then enter the reservoir cracks 27 through the perforation holes 31. The fracturing fluid and liquid CO2 are filtered out and enter the reservoir, and the proppant remains in the reservoir cracks 27 to support the cracks, so that the crack shape is kept in an open state.

[0051] Embodiment 3, a carbon dioxide thickening fracturing process, comprising the following steps:

[0052] 1) The telescopic short circuit 21, the safety joint 23, the low-temperature and high-pressure gas-sealed hydraulic anchor 24, the low-temperature and high-pressure gas-sealed anchored packer 25, the sandblasting nozzle 26 and the fracturing completion tubing 22 are lowered into the well through the well repair machinery, and the low-temperature and high-pressure gas-sealed anchored packer 25 is seated and started by rotating the fracturing completion tubing 22, and the anchoring machinery contacts and anchors the inner wall of the production casing 20;

[0053] The seal is close to the inner wall of the production casing 20 to play a sealing role. The low-temperature and high-pressure gas-sealed hydraulic anchor 24 is activated when high-pressure fracturing fluid and liquid CO2 enter the oil pipe, and contacts and anchors with the inner wall of the production casing 20. When the low-temperature liquid CO2 enters the fracturing completion oil pipe 22, the fracturing completion oil pipe 22 will shrink due to the change in temperature. At this time, the telescopic short circuit 21 will open and then stretch to make up for the shrinkage distance of the fracturing completion oil pipe 22, thereby ensuring the safety of the pipe string.

[0054] 2) The concentration of the CO2 thickener stock solution in the liquid CO2 thickener stock tank is 90%, the CO2 thickener stock solution is transported to the CO2 thickener solution configuration tank 14 through the low-pressure normal temperature pipeline 13, the water storage tank 19 is transported to the CO2 thickener solution configuration tank 14 through the low-pressure normal temperature pipeline 13, the CO2 thickener stock solution is mixed with water in the CO2 thickener solution configuration tank 14, the CO2 thickener stock solution concentration is diluted to 17%, the CO2 thickener solution configuration tank 14 transports the diluted CO2 thickener solution with a concentration of 17% to the sand mixing liquid supply vehicle 12 through the low-pressure normal temperature pipeline 13, the water storage tank 19 transports water to the sand mixing liquid supply vehicle 12 through the low-pressure normal temperature pipeline 13, the CO2 thickener solution is mixed with water in the sand mixing liquid supply vehicle 12, and a CO2 thickener solution with a concentration of 1.5% is formed at this time;

[0055] 3) The fracturing fluid thickener stock liquid storage tank 30 delivers the fracturing fluid thickener to the sand mixing liquid supply vehicle 12 through the low-pressure normal temperature pipeline 13, and the fracturing fluid thickener is mixed with a CO2 thickener solution with a concentration of 1.5% to form a fracturing fluid with a fracturing fluid thickener concentration of 0.8% and a fracturing fluid viscosity of 60mPa.S;

[0056] 4) The sand mixing and liquid supply truck 12 pressurizes the mixed solution with a CO2 thickener concentration of 1.5% and a fracturing fluid thickener concentration of 0.8% to 0.8MPa, and then delivers it to the liquid high-pressure pump truck 10 through a medium-pressure normal temperature pipeline. The liquid high-pressure pump truck 10 pressurizes the fracturing fluid with a CO2 thickener concentration of 1.5% and a fracturing fluid thickener concentration of 0.8% to 65MPa, and then delivers it to the fracturing fluid wellhead injection head 8 through a normal temperature high-pressure pipeline 9;

[0057] 5) The low-temperature and low-pressure liquid CO2 with a temperature of -35--28°C in the liquid carbon dioxide storage tank 1 is transported to the carbon dioxide booster pump 3 through the low-temperature pipeline 2. The carbon dioxide booster pump 3 pressurizes the low-temperature liquid CO2 to 3.0MPa, and the temperature of the liquid CO2 rises to -16°C. The carbon dioxide booster pump 3 pressurizes the liquid CO2 and then transports it to the liquid carbon dioxide high-pressure pump truck 5 through the medium-pressure low-temperature pipeline 4. The liquid CO2 with a pressure of 2.8MPa and a temperature of -16°C is pressurized to 65MPa by the liquid carbon dioxide high-pressure pump truck 5, and the temperature rises to above 0°C, and then transported to the liquid carbon dioxide wellhead injection head 7 through the low-temperature and high-pressure pipeline 6;

[0058] 6) The treated fracturing fluid in step 4) is mixed with the liquid CO2 treated by the liquid carbon dioxide high-pressure pump truck 5 in step 5) at the injection wellhead 28. During the mixing process, the liquid CO2 extracts the CO2 thickener from the mixed solution, and the viscosity of the liquid CO2 increases from 0.5 mPa.S to 60 mPa.S. During the mixing process, the displacement of the liquid carbon dioxide from the liquid carbon dioxide wellhead injection head 7 into the injection wellhead 28 is 2.5-3 times the displacement of the fracturing fluid from the fracturing fluid wellhead injection head 8 into the injection wellhead 28;

[0059] 7) The mixture of liquid CO2 and fracturing fluid is transported to the sandblasting nozzle 26 in the fracturing completion tubing 22, enters the production casing 20, and then enters the reservoir through the perforation holes 31, forming reservoir fractures 27;

[0060] 8) The fracturing proppant storage tank 32 transports the fracturing proppant to the sand mixing and liquid supply vehicle 12 through the proppant delivery pipeline 33, and mixes with the mixed liquid of liquid CO2 and fracturing fluid. At this time, the viscosity of the liquid CO2 reaches 60mPa.S after thickening, which can effectively carry the fracturing proppant. The fracturing proppant, fracturing fluid and liquid CO2 are transported to the sandblasting nozzle 26 through the fracturing completion oil pipe 22, enter the production casing 20, and then enter the reservoir cracks 27 through the perforation holes 31. The fracturing fluid and liquid CO2 are filtered out and enter the reservoir, and the proppant remains in the reservoir cracks 27 to support the cracks, so that the crack shape is kept in an open state.

[0061] Key points of the technical solution to solve the problem in the present invention:

[0062] 1. Design of liquid carbon dioxide pressure thickening fracturing process and pumping procedure: The fracturing process is divided into two pumping ends. The first is the conventional liquid pumping end, which mainly pumps the fracturing fluid and carbon dioxide thickener to the fracturing wellhead, mixes with liquid carbon dioxide and enters the reservoir through the fracturing string, and pumps the sand-carrying fluid to carry the fracturing proppant into the crack. The second is the liquid carbon dioxide pumping end, which pressurizes the liquid carbon dioxide and pumps it to the fracturing wellhead to mix with the fracturing fluid and carbon dioxide thickener. After mixing, the liquid carbon dioxide extracts the thickener from the fracturing fluid to increase its viscosity, and enters the reservoir together with the fracturing fluid to create fractures. In the proppant addition stage, the thickened liquid carbon dioxide and the fracturing fluid carry the proppant into the crack together.

[0063] 2. The design is suitable for low-temperature and gas explosion-resistant thickened liquid carbon dioxide fracturing process pipe strings, which meet the requirements of low temperature and resistance to gasified carbon dioxide erosion. At the same time, the pipe string adopts a fixed structure to prevent pipe string creep caused by phase changes of liquid carbon dioxide during pumping.

[0064] The present invention realizes the thickening of liquid carbon dioxide, the creation of seams by thickened liquid carbon dioxide, and the carrying of sand by thickened liquid carbon dioxide and liquid through the design of fracturing fluid and liquid carbon dioxide pumping program. During the flowback process, the liquid carbon dioxide undergoes a phase change from liquid to gaseous in the reservoir, and all the injected fracturing fluid is displaced out of the ground, effectively reducing the impact of the liquid on the reservoir, improving the flowback rate, maximizing the reservoir transformation effect, and increasing the single well production.

[0065] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

[0066] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.

Claims

1. A carbon dioxide thickening fracturing process method, using a carbon dioxide thickening fracturing system, the system includes an output system, a fracturing fluid processing system and a liquid CO2 processing system: The fracturing fluid processing system comprises: Liquid CO2 thickener stock solution processing system and fracturing fluid thickening system; Liquid CO2 thickener stock solution processing system It includes: a liquid CO2 thickener stock tank, a CO2 thickener solution preparation tank, a water storage tank, a sand mixing liquid supply truck, a liquid high-pressure pump truck and a fracturing fluid wellhead injection head; the liquid high-pressure pump truck is connected to the output system through a normal temperature high-pressure pipeline, the liquid high-pressure pump truck is connected to the sand mixing liquid supply truck through a medium-pressure normal temperature pipeline, the sand mixing liquid supply truck is connected to the CO2 thickener solution preparation tank through a low-pressure normal temperature pipeline, the CO2 thickener solution preparation tank is connected to the liquid CO2 thickener stock tank through a low-pressure normal temperature pipeline, the thickener solution preparation tank is connected to the water storage tank through a low-pressure normal temperature pipeline, and the water storage tank is connected to the sand mixing liquid supply truck through a low-pressure normal temperature pipeline; The fracturing fluid thickening system is connected to the sand mixing and liquid supply vehicle, and the liquid CO2 processing system is connected to one end of the output system; The output system includes: production casing, telescopic short-circuit, fracturing completion oil pipe, safety joint low-temperature high-pressure gas-sealed hydraulic anchor, low-temperature high-pressure gas-sealed anchored packer, sandblasting nozzle, reservoir fracture, injection wellhead, perforation hole; the telescopic short-circuit, safety joint, low-temperature high-pressure gas-sealed hydraulic anchor, low-temperature high-pressure gas-sealed anchored packer, sandblasting nozzle are respectively connected with the fracturing completion oil pipe, the perforation hole is arranged on the production casing, the injection wellhead is equipped with a fracturing fluid wellhead injection head, and the fracturing fluid wellhead injection head is connected with a normal temperature high-pressure pipeline; The liquid CO2 processing system comprises: a liquid carbon dioxide storage tank, a cryogenic pipeline, a carbon dioxide booster pump, a medium-pressure cryogenic pipeline, a liquid carbon dioxide high-pressure pump truck, a cryogenic and high-pressure pipeline, and a liquid carbon dioxide wellhead injection head; the liquid carbon dioxide storage tank is connected to the carbon dioxide booster pump through the cryogenic pipeline, the carbon dioxide booster pump is connected to the liquid carbon dioxide high-pressure pump truck through the medium-pressure cryogenic pipeline, the liquid carbon dioxide high-pressure pump truck is connected to the liquid carbon dioxide wellhead injection head through the cryogenic and high-pressure pipeline, and the liquid carbon dioxide wellhead injection head is connected to the injection wellhead, characterized in that the process method comprises the following steps: 1) The telescopic short-circuit, safety joint, low-temperature and high-pressure gas-sealed hydraulic anchor, low-temperature and high-pressure gas-sealed anchored packer, sandblasting nozzle and fracturing completion tubing are lowered into the well through the well repair machinery. The low-temperature and high-pressure gas-sealed anchored packer is seated and started by rotating the fracturing completion tubing, and the anchoring machinery contacts and anchors the inner wall of the production casing; 2) The concentration of the CO2 thickener stock solution in the liquid CO2 thickener stock tank is 80-90%. The CO2 thickener stock solution is transported to the CO2 thickener solution configuration tank through a low-pressure normal temperature pipeline. The water storage tank is transported to the CO2 thickener solution configuration tank through a low-pressure normal temperature pipeline. The CO2 thickener stock solution is mixed with water in the CO2 thickener solution configuration tank. The CO2 thickener stock solution concentration is diluted to 12-17%. The CO2 thickener solution configuration tank transports the diluted CO2 thickener solution with a concentration of 12-17% to the sand mixing liquid supply vehicle through a low-pressure normal temperature pipeline. The water storage tank transports water to the sand mixing liquid supply vehicle through a low-pressure normal temperature pipeline. The CO2 thickener solution is mixed with water in the sand mixing liquid supply vehicle, and a CO2 thickener solution with a concentration of 1-1.5% is formed at this time; 3) The fracturing fluid thickener stock tank delivers the fracturing fluid thickener to the sand mixing liquid supply vehicle through a low-pressure normal temperature pipeline, and the fracturing fluid thickener is mixed with a CO2 thickener solution with a concentration of 1-1.5% to form a fracturing fluid with a fracturing fluid thickener concentration of 0.4-0.8% and a fracturing fluid viscosity of 40-60mPa.S; 4) The mixed sand supply truck pressurizes the mixed solution with a CO2 thickener concentration of 1-1.5% and a fracturing fluid thickener concentration of 0.4-0.8% to 0.5-0.8MPa, and then delivers it to the liquid high-pressure pump truck through a medium-pressure normal temperature pipeline. The liquid high-pressure pump truck pressurizes the fracturing fluid with a CO2 thickener concentration of 1-1.5% and a fracturing fluid thickener concentration of 0.4-0.8% to 50-65MPa, and then delivers it to the fracturing fluid wellhead injection head through a normal temperature high-pressure pipeline; 5) The low-temperature and low-pressure liquid CO2 in the liquid carbon dioxide storage tank with a temperature of -35-28°C is transported to the carbon dioxide booster pump through a low-temperature pipeline. The carbon dioxide booster pump pressurizes the low-temperature liquid CO2 to 2.4-3.0MPa. The temperature of the liquid CO2 rises to -20-16°C. The carbon dioxide booster pump pressurizes the liquid CO2 and then transports it to the liquid carbon dioxide high-pressure pump truck through a medium-pressure low-temperature pipeline. The liquid CO2 with a pressure of 2.4-2.8MPa and a temperature of -20-16°C is pressurized to 50-65MPa by the liquid carbon dioxide high-pressure pump truck (5) and the temperature rises to above 0°C. It is then transported to the liquid carbon dioxide wellhead injection head through a low-temperature and high-pressure pipeline; 6) The treated fracturing fluid in step 4) is mixed with the liquid CO2 treated by the liquid carbon dioxide high-pressure pump truck (5) in step 5) at the injection wellhead (28). During the mixing process, the liquid CO2 extracts the CO2 thickener from the mixed solution, and the viscosity of the liquid CO2 increases from 0.3-0.5 mPa.S to 40-60 mPa.S. During the mixing process, the displacement of the liquid carbon dioxide from the liquid carbon dioxide wellhead injection head into the injection wellhead is 2.5-3 times the displacement of the fracturing fluid from the fracturing fluid wellhead injection head into the injection wellhead; 7) The mixture of liquid CO2 and fracturing fluid is transported to the sandblasting nozzle in the fracturing completion tubing, enters the production casing, and then enters the reservoir through the perforated holes to form reservoir fractures; 8) The fracturing proppant storage tank transports the fracturing proppant to the sand mixing and liquid supply truck through the proppant delivery pipeline, and mixes with the mixed liquid of liquid CO2 and fracturing fluid. The viscosity of the liquid CO2 at this time reaches 40-60mPa.S after thickening, which can effectively carry the fracturing proppant. The fracturing proppant, fracturing fluid and liquid CO2 are transported to the sandblasting nozzle through the fracturing completion tubing, enter the production casing and then enter the reservoir cracks through the perforated holes. The fracturing fluid and liquid CO2 are filtered out and enter the reservoir, and the proppant remains in the reservoir cracks to support the cracks, so that the crack morphology is kept in an open state.

2. The carbon dioxide thickening fracturing process according to claim 1, characterized in that: The fracturing fluid thickening system comprises: a fracturing proppant storage tank and a fracturing fluid thickener stock liquid storage tank; the fracturing proppant storage tank is connected to a proppant delivery pipeline, the proppant delivery pipeline is connected to a sand mixing and liquid supply vehicle, and the fracturing fluid thickener stock liquid storage tank is connected to the sand mixing and liquid supply vehicle via a low-pressure normal temperature pipeline.

3. The carbon dioxide thickening fracturing process according to claim 1, characterized in that: The liquid carbon dioxide wellhead injection head is installed on the injection wellhead by means of a flange, and the fracturing fluid wellhead injection head is connected to the injection wellhead by means of a flange.

4. The carbon dioxide thickening fracturing process according to claim 1, characterized in that: The telescopic short-circuit, the safety joint, the low-temperature and high-pressure gas-sealed hydraulic anchor, the low-temperature and high-pressure gas-sealed anchored packer and the sandblasting nozzle are respectively connected to the fracturing completion oil pipe by means of threads.

Citation Information

Patent Citations

  • A drag-reducing agent for dry carbon dioxide fracturing and its application

    CN108864387B

  • Supercritical carbon dioxide fracturing yield-increasing process

    CN109736767A

  • Liquid carbon dioxide fracturing method

    CN110761764A

  • Liquid CO2 fracturing technology for shale gas well

    CN102852508A

  • Normal-pressure sand-mixing carbon dioxide fracturing construction process