Induction heating atomic and molecular furnace and its process

The induction heating atomic and molecular furnace uses eddy current heating technology to solve the efficiency reduction and safety problems of direct current heating at high temperatures, achieving efficient and safe high-temperature heating, which is suitable for cold atom and molecule research and applications.

CN113883896BActive Publication Date: 2024-10-29INNOVATION ACAD FOR PRECISION MEASUREMENT SCI & TECH CAS
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202111127744.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-09-26
Publication Date
2024-10-29
Estimated Expiration
2041-09-26

AI Technical Summary

Technical Problem

The direct current heating method requires too much current when heating to high temperatures, which causes the wire temperature to increase, the heating efficiency to decrease, and is unsafe.

Method used

An induction heating atomic and molecular furnace is used to generate eddy current heating of the metal tube through the AC magnetic field wound by the solenoid coil outside the ceramic tube to avoid direct contact between the wire and the metal tube. The DC conversion AC circuit is used to achieve alternating current heating.

Benefits of technology

It achieves high high-temperature heating efficiency, fast temperature rise and safety, and is suitable for cold atom and molecule research and application fields.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113883896B_ABST
    Figure CN113883896B_ABST
Patent Text Reader

Abstract

The invention discloses an induction heating atomic molecule furnace and a process thereof, and relates to the field of atomic molecule source devices. The structure of the invention is: a sample (1) is placed in a metal tube (2), a ceramic tube (3) is sleeved outside the metal tube (2), a solenoid coil (4) is sleeved outside the ceramic tube (3), and it does not directly contact the ceramic tube (3), and a plug (5) blocks one end of the metal tube (2); a ceramic shell (6) and a ceramic cover plate (7) are used for support, the metal tube (2) passes through two holes on the side of the ceramic shell (6), and the two ends of the solenoid coil (4) are tapped from the two holes on the ceramic cover plate (7) and connected to the output end of the DC to AC conversion circuit (8). The invention has the following advantages and positive effects: while ensuring the stability and safety of the circuit function, it can be heated to above 1000°C, has high heating efficiency, fast temperature rise, easy control, good safety, and can be widely used in cold atomic molecule research and application fields.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of atomic and molecular source devices, and in particular to an induction heating atomic and molecular furnace and a process thereof, which are suitable for cold atomic and molecular research and application fields. Background Art

[0002] Cold atomic molecular physics mainly studies the energy level structure, motion law, interaction and application of cold atomic molecules. In the research and application of cold atomic molecules, the vapor of atomic molecules is generally prepared as the sample source. This is because compared with liquid and solid states, the gaseous atomic molecules have little interaction and little effect on the internal structure and properties of atomic molecules, which is conducive to high-precision research on the internal structure of atomic molecules. For samples that are gaseous at room temperature, atomic molecular beams can be directly generated through constrained pinholes. For samples that are solid or liquid at room temperature, they need to be heated to a certain temperature to increase the vapor pressure to produce the required concentration of atomic molecular vapor. The general heating methods are photon heating and current heating. Among them, photon heating uses the photothermal effect to heat the target material through the action of laser and target material, but the interaction between light and matter is relatively complex, different samples have different requirements for laser, and the cost of laser is high, so photon heating is only suitable for samples with some special applications; current heating uses the electrothermal effect to heat the metal furnace tube by passing current through it. Its principle is simple and suitable for most samples. This method is low-cost and easy to control, so it has a wider range of applications.

[0003] At present, the commonly used current heating method is to add current to both ends of the metal tube and use the thermal effect of the metal tube resistance for direct current heating. Generally, a current of 10 to 20A can heat the metal tube to 300 to 500°C, and use the heat conduction effect to heat the sample inside the metal tube. However, when the metal tube needs to be heated to above 500°C, the heating power is limited by the current that the wire can carry, and the current needs to be continuously increased. At this time, the following problems are prone to occur: 1. As the current on the wire increases, the temperature of the wire itself increases, resulting in a decrease in the heating efficiency of the metal tube and a slow heating; 2. The wire is directly connected to the metal tube, and the temperature of the metal tube will also transfer heat to the wire, causing the outer insulation layer of the wire to melt, which is unsafe.

[0004] In order to make up for the problems caused by direct current heating, induction heating is a good solution. The basic principle of induction heating is: a metal conductor is placed in a solenoid coil with an alternating current; the solenoid coil generates an AC magnetic field around it; the AC magnetic field induces eddy currents on the metal conductor; the metal conductor is heated by the thermal effect of the eddy currents. Generally, a solenoid coil with a current of 10A can heat the metal conductor to above 1000°C. And the wire is not in direct contact with the metal conductor, so it can maintain a lower temperature and is safe. In addition, eddy current heating has a high power density, high heating efficiency, and fast heating, which is more suitable for heating samples in cold atomic and molecular research and applications.

[0005] In summary, when using traditional direct current heating to heat samples to above 500°C, the current required is too large and unsafe, and the heating efficiency decreases as the temperature rises, resulting in slow heating. In comparison, induction heating is a better solution, which is characterized by fast heating, easy control, and good safety. Summary of the invention

[0006] The purpose of the present invention is to provide an induction heating atomic molecular furnace and its process in order to solve the above problems existing in the existing direct current heating atomic molecular furnace.

[0007] The object of the present invention is achieved in that:

[0008] The device includes a sample, a metal tube, a ceramic tube, a solenoid coil, a plug, and a DC-to-AC conversion circuit. The device of the present invention solves the problem that when heating to a high temperature, direct current heating requires continuous increase of current, the heating power is limited by the current that the wire can carry, the heating efficiency is reduced, and the temperature rise is slow. At the same time, the device can heat the sample to more than 1000°C while ensuring the stability and safety of the circuit function, and can be widely used in cold atomic and molecular research and application fields.

[0009] Specifically:

[0010] The induction heating atomic and molecular furnace includes a sample, a metal tube, a ceramic tube, a solenoid coil, a plug, a ceramic shell, a ceramic cover plate and a DC to AC conversion circuit;

[0011] The sample is placed in a metal tube, a ceramic tube is sleeved outside the metal tube, a solenoid coil is sleeved outside the ceramic tube, and it does not directly contact the ceramic tube, and a plug blocks one end of the metal tube; the ceramic shell and the ceramic cover are used for support, the metal tube passes through two holes on the side of the ceramic shell, and taps at both ends of the solenoid coil are led out from the two holes on the ceramic cover and connected to the output end of the DC-to-AC conversion circuit.

[0012] Compared with the existing atomic and molecular furnace heated by direct current, the present invention has the following advantages and positive effects:

[0013] While ensuring the stable and safe function of the circuit, it is heated to above 1000°C. It has high heating efficiency, fast temperature rise, easy control, and good safety. It can be widely used in cold atomic and molecular research and application fields. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a structural exploded diagram of the present invention;

[0015] Figure 2 It is a schematic diagram of a DC to AC conversion circuit.

[0016] In the figure:

[0017] 1—sample;

[0018] 2—Metal pipe;

[0019] 3—Ceramic tube;

[0020] 4—solenoid coil;

[0021] 5—Plug head.

[0022] 6—Ceramic shell;

[0023] 7—ceramic cover plate;

[0024] 8—DC to AC conversion circuit;

[0025] DC—direct current power supply,

[0026] R1, R2, R3, R4—1st, 2nd, 3rd, 4th resistors,

[0027] D1, D2—1st and 2nd voltage zener diodes,

[0028] D3, D4—3rd and 4th fast recovery diodes,

[0029] Q1, Q2—1st and 2nd effect transistors,

[0030] C—capacitor,

[0031] L1, L2—1st and 2nd inductors. DETAILED DESCRIPTION

[0032] The following is a detailed description with reference to the accompanying drawings and embodiments:

[0033] 1. Structure of induction heating atomic and molecular furnace

[0034] 1. Overall

[0035] like Figure 1 The induction heating atomic and molecular furnace includes a sample 1, a metal tube 2, a ceramic tube 3, a solenoid coil 4, a plug 5, a ceramic shell 6, a ceramic cover 7 and a DC-to-AC conversion circuit 8;

[0036] The sample 1 is placed in the metal tube 2, the ceramic tube 3 is sleeved outside the metal tube 2, the solenoid coil 4 is sleeved outside the ceramic tube 3, and it does not directly contact the ceramic tube 3, and the plug 5 blocks one end of the metal tube 2. The ceramic shell 6 and the ceramic cover 7 are used for support, the metal tube 2 passes through the two holes on the side of the ceramic shell 6, and the taps at both ends of the solenoid coil 4 are led out from the two holes on the ceramic cover 7 and connected to the output end of the DC conversion AC circuit 8.

[0037] 2. Functional components

[0038] 1) Sample 1

[0039] It is a high purity beryllium rod.

[0040] Used to generate the required atomic and molecular vapor, heating to 800°C can produce beryllium atomic vapor of the required concentration.

[0041] 2) Metal pipe 2

[0042] Tantalum tubes are selected for loading sample 1 due to their high temperature resistance, good thermal stability, high resistivity, high magnetic permeability, and good ductility.

[0043] 3) Ceramic tube 3

[0044] Black zirconia ceramics are selected. Black zirconia ceramics are resistant to high temperatures and have good thermal stability. They can absorb the light emitted by the metal tube 2 and shield part of the heat radiation.

[0045] 4) Solenoid coil 4

[0046] For copper winding coils, copper wire is selected for even and tight spiral winding. It has good conductivity and can reduce its own resistance heating.

[0047] 5) Plug head 5

[0048] Tantalum is selected, which is resistant to high temperature and has good thermal stability, so that the atomic molecular vapor can be discharged along the metal tube 2 in one direction.

[0049] 6) Ceramic shell 6

[0050] Alumina ceramics are selected for support and can shield part of the heat radiation.

[0051] Its structure is a rectangular container, and the left and right side walls are respectively provided with small holes for the ceramic tube 3 to pass through.

[0052] 7) Ceramic cover plate 7

[0053] Alumina ceramics are selected for support and can shield part of the heat radiation.

[0054] Its structure is a rectangular plate with windows on the left and right sides for the ends of the solenoid coil 4 to pass through.

[0055] 8) DC to AC conversion circuit 8

[0056] The DC to AC conversion circuit 8 uses a zero voltage switching circuit;

[0057] Specifically, if Figure 2The DC to AC conversion circuit 8 includes a solenoid coil 4, a DC power supply DC, first, second, third, fourth resistors R1, R2, R3, R4, first, second voltage zener diodes D1, D2, third, fourth fast recovery diodes D3, D4, first, second effect transistors Q1, Q2, a capacitor C, first, second inductors L1, L2;

[0058] A parallel resonant circuit is formed, and its output end is connected to the solenoid coil 4.

[0059] After power is turned on, direct current is converted into alternating current, and the alternating current induction heats the metal tube 2 through the solenoid coil 4, causing the temperature of the sample 1 inside to rise.

[0060] The DC-to-AC circuit 8 is mature in technology, modularizable and low in cost.

[0061] The present invention can heat to above 1000° C. while ensuring stable and safe circuit functions, has high heating efficiency, fast temperature rise, easy control, and good safety, and can be widely used in cold atom and molecule research and application fields.

[0062] 2. Process of Induction Heating Atomic and Molecular Furnace

[0063] ①Heating the sample by induction heating (1):

[0064] The output end of the DC to AC conversion circuit (8) is connected to the solenoid coil (4), and an eddy current is generated on the metal tube (2) through the solenoid coil (4), and then the sample (1) is heated by the thermal effect of the eddy current to generate atomic and molecular vapor;

[0065] ② The metal tube (2) is made of a metal material having high temperature resistance, good thermal stability, high resistivity, high magnetic permeability and good ductility, and is selected from tantalum, niobium, tungsten, molybdenum or their alloys. 3. Specific embodiments

[0067] In specific implementation, if the sample 1 is a metal sample, the solenoid coil 4 directly has an induction heating effect on it; the inner diameter of the metal tube 2 can be adjusted according to the required width of the atomic molecular vapor beam; the solenoid coil 4 uses copper wire to be evenly and tightly spirally wound, and each turn does not touch each other, and the inductance is preferably 0.5-1.0μH; the copper wire diameter is preferably 1.5-2.0mm; select a suitable diameter of the solenoid coil 4 to ensure that the metal tube 2 can be induced; the number of turns of the solenoid coil 4 is preferably 10-20, ensuring that most of the length of the metal tube 2 is within the solenoid coil 4; if heating is required When the temperature reaches a higher level, it is more appropriate to wind the solenoid coil 4 with a more high-temperature resistant molybdenum wire; the plug 5 blocks one end of the metal tube 2 to allow the atomic molecular vapor to be unidirectionally discharged along the metal tube 2; if the metal tube 2 is designed with one end open and the other end closed, the plug 5 is not required; the ceramic shell 6 and the ceramic cover 7 are only used for support and can shield part of the heat radiation, and different designs can be adopted according to actual needs; the DC-to-AC circuit 8 can select a zero-voltage switching circuit module with an input voltage of 12 to 24V and a power of about 200W, or other DC-to-AC circuits can be selected according to actual needs.

[0068] Those skilled in the art to which the present invention relates may make various modifications or additions to the specific embodiments described or replace them in a similar manner, but they will not deviate from the spirit of the present invention or exceed the scope defined by the attached claims.

Claims

1. An induction heating atomic and molecular furnace, characterized in that: It includes a sample (1), a metal tube (2), a ceramic tube (3), a solenoid coil (4), a plug (5), a ceramic housing (6), a ceramic cover plate (7) and a DC to AC conversion circuit (8); Its location and connection relationship are: The sample (1) is placed in the metal tube (2), the ceramic tube (3) is sleeved outside the metal tube (2), the solenoid coil (4) is sleeved outside the ceramic tube (3) and does not directly contact the ceramic tube (3), and the plug (5) blocks one end of the metal tube (2); the ceramic shell (6) and the ceramic cover (7) are used for support, the metal tube (2) passes through two holes on the side of the ceramic shell (6), and the two ends of the solenoid coil (4) are tapped out from the two holes on the ceramic cover (7) and connected to the output end of the DC-to-AC conversion circuit (8); The DC to AC conversion circuit (8) comprises a solenoid coil (4), provided with a DC power supply (DC), first, second, third and fourth resistors (R1, R2, R3 and R4), first and second voltage regulator diodes (D1 and D2), third and fourth fast recovery diodes (D3 and D4), first and second effect transistors (Q1 and Q2), a capacitor (C), and first and second inductors (L1 and L2); A parallel resonant circuit is formed, the output end of which is connected to the solenoid coil (4); The sample (1) is a metal sample, and the solenoid coil (4) directly has an induction heating effect on it; Heating the sample using induction heating (1): The output end of the DC to AC conversion circuit (8) is connected to the solenoid coil (4), and an eddy current is generated on the metal tube (2) through the solenoid coil (4), and then the sample (1) is heated by the thermal effect of the eddy current to generate atomic and molecular vapor; The metal tube (2) is made of a metal material having high temperature resistance, good thermal stability, high resistivity, high magnetic permeability and good ductility, and is selected from tantalum, niobium, tungsten, molybdenum or alloys thereof; The ceramic tube (3) is black zirconium oxide ceramic, which is resistant to high temperatures and has good thermal stability, and can absorb the light emitted by the metal tube (2) and shield part of the heat radiation; The solenoid coil (4) is made of copper wire that is evenly and tightly spirally wound, with an inductance of 0.5 to 1.0 μH; the copper wire diameter is 1.5 to 2.0 mm; the number of turns of the solenoid coil 4 is 10 to 20; and it is ensured that most of the length of the metal tube (2) is within the solenoid coil (4).

Citation Information

Patent Citations

  • Power supply for induction heating

    CN101523713A

  • Atom generator capable of improving atomic beam density

    CN105376923A

  • ECR ion source induction furnace

    CN109916177A

  • Closed-cavity magnetic induction heating device for neutron scattering measurement, and application thereof

    CN113395796A

  • Control by temperature change low -power consumption atom stove

    CN206021107U