Semiconductor structure and method for forming the same

By forming a silicon carbide barrier layer on both sides of the dummy gate structure, the short channel effect problem caused by doped ions diffusion in the fin field effect transistor is solved, and the performance and current stability of the semiconductor device are improved.

CN113937002BActive Publication Date: 2024-11-22SEMICON MFG INT (SHANGHAI) CORP +1
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202010676925.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-07-14
Publication Date
2024-11-22
Estimated Expiration
2040-07-14

AI Technical Summary

Technical Problem

The short-channel effect problem of existing fin field effect transistors leads to difficulty in improving performance, and the diffusion of boron and phosphorus doped ions affects channel mobility, junction capacitance and leakage performance.

Method used

A first opening is formed in the substrates on both sides of the dummy gate structure, and a barrier layer is formed on the sidewall surface of the channel. The barrier layer material is silicon carbide, with a dimension of 4 nanometers to 5 nanometers perpendicular and 3 nanometers to 7 nanometers long. Barrier the diffusion of doped ions, forming a cover layer to increase resistance.

Benefits of technology

It effectively suppresses the short channel effect, reduces the diffusion of doped ions into the channel, avoids tunneling and leakage, and improves the performance of semiconductor devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113937002B_ABST
    Figure CN113937002B_ABST
Patent Text Reader

Abstract

A method for forming a semiconductor structure includes: providing a substrate, forming a dummy gate structure on the substrate; forming first openings in the substrate on both sides of the dummy gate structure, respectively, wherein the first openings have channel sidewalls adjacent to the dummy gate structure; forming a barrier layer on the surface of the channel sidewalls so that the first opening forms a second opening; and forming a covering layer in the second opening. The barrier layer can effectively block the diffusion of source and drain doping ions into the channel region, thereby suppressing the short channel effect problem.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor manufacturing, and in particular to a semiconductor structure and a forming method thereof. Background Art

[0002] In the existing semiconductor field, the fin field effect transistor (FinFET) is an emerging multi-gate device. Compared with the planar metal-oxide semiconductor field effect transistor (MOSFET), the fin field effect transistor has stronger short channel suppression capability and stronger operating current, and is now widely used in various semiconductor devices.

[0003] With the continuous development of semiconductor technology, the gate size of fin field effect transistors is also constantly decreasing. At this time, the distribution width of boron and phosphorus doped ions becomes an important factor affecting the short channel effect (SCE) of fin field effect transistors. At the same time, the diffusion of boron and phosphorus doped ions caused by transient enhanced diffusion (TED) not only affects the short channel effect, but also affects the transistor channel mobility, junction capacitance, and leakage performance.

[0004] The performance of the semiconductor structure formed by the existing fin field effect transistor needs to be improved urgently. Summary of the invention

[0005] The technical problem solved by the present invention is to provide a semiconductor structure and a method for forming the same, which can improve the performance of the semiconductor structure.

[0006] To solve the above technical problems, the technical solution of the present invention provides a method for forming a semiconductor structure, including: providing a substrate, forming a dummy gate structure on the substrate; forming first openings in the substrate on both sides of the dummy gate structure, respectively, the first opening having a channel sidewall adjacent to the dummy gate structure; forming a blocking layer on the surface of the channel sidewall so that the first opening forms a second opening; and forming a covering layer in the second opening.

[0007] Optionally, the material of the barrier layer includes silicon carbide.

[0008] Optionally, a dimension of the barrier layer along a direction perpendicular to the substrate is 4 nanometers to 5 nanometers, and a dimension of the barrier layer along a channel length direction is 3 nanometers to 7 nanometers.

[0009] Optionally, the substrate includes: a base, and a fin located on a surface of the base.

[0010] Optionally, the dummy gate structure spans across the fin, and the dummy gate structure is located on a portion of the top surface and sidewall surface of the fin.

[0011] Optionally, the dummy gate structure includes: a dummy gate layer and a first spacer located on a sidewall surface of the dummy gate layer.

[0012] Optionally, a material of the first spacer includes silicon oxide, silicon nitride, silicon oxynitride, silicon oxycarbide, silicon carbonitride or silicon carbon oxynitride.

[0013] Optionally, the thickness of the first sidewall spacer is 3 nanometers to 7 nanometers.

[0014] Optionally, the first opening exposes the bottom of the first side wall.

[0015] Optionally, the method for forming the barrier layer includes: forming an initial barrier layer in the first opening; using the first sidewall as a mask, etching the initial barrier layer until the bottom of the first opening is exposed, thereby forming the barrier layer and the second opening.

[0016] Optionally, the initial barrier layer is formed by an epitaxial growth process.

[0017] Optionally, the process of etching the initial barrier layer includes dry etching.

[0018] Optionally, the method for forming the first opening includes: forming an initial first opening in the substrate on both sides of the pseudo gate structure; forming a first epitaxial layer on the side wall surface and the bottom surface of the initial first opening, and the first epitaxial layer has first doping ions.

[0019] Optionally, the formation process of the first epitaxial layer is an epitaxial growth process; the material of the first epitaxial layer includes silicon carbide or silicon phosphide, and the first doping ions are N-type ions; the material of the first epitaxial layer includes silicon germanium, and the first doping ions are P-type ions.

[0020] Optionally, before forming the barrier layer, the first epitaxial layer is surface treated to reduce the roughness of the surface of the first epitaxial layer.

[0021] Optionally, the surface treatment process is one or both of dry etching and wet etching.

[0022] Optionally, the process parameters of the dry etching include: the etching gas includes hydrogen bromide and chlorine, the power of the etcher is 100 W to 1000 W, the gas pressure in the etching chamber is 2 mTorr to 20 mTorr, the flow rate of hydrogen bromide is 10 to 500 standard milliliters per minute, and the flow rate of chlorine is 10 to 500 standard milliliters per minute.

[0023] Optionally, the thickness of the first epitaxial layer is less than the depth of the initial first opening.

[0024] Optionally, the first initial opening exposes a portion of the bottom of the pseudo gate structure, and the method for forming the first epitaxial layer includes: forming an initial first epitaxial layer on the side wall surface and the bottom surface of the initial first opening; using the pseudo gate structure as a mask, etching the initial first epitaxial layer to form the first epitaxial layer.

[0025] Optionally, the process of etching the initial first epitaxial layer includes one or both of dry etching and wet etching.

[0026] Optionally, the covering layer is formed by an epitaxial growth process, the covering layer contains second doping ions, the material of the covering layer includes silicon carbide or silicon phosphide, and the doping ions are N-type ions; the material of the covering layer includes silicon germanium, and the doping ions are P-type ions.

[0027] Optionally, the barrier layer includes third doping ions, the third doping ions are P-type ions or N-type ions, and the conductivity type of the third doping ions is opposite to the conductivity type of the second doping ions.

[0028] Optionally, the method further includes: before forming the covering layer, forming a second epitaxial layer in the second opening.

[0029] Optionally, the formation process of the second epitaxial layer is an epitaxial growth process, the second epitaxial layer has a fourth doping ion, the material of the second epitaxial layer includes silicon carbide or silicon phosphide, and the doping ion is an N-type ion; the material of the second epitaxial layer includes silicon germanium, and the fourth doping ion is a P-type ion.

[0030] Optionally, a depth of the first opening is 4 nanometers to 5 nanometers.

[0031] Optionally, the method for forming the first opening includes: etching the substrate using the gate structure as a mask to form the first opening.

[0032] Optionally, the process of etching the substrate to form the first opening includes one or both of dry etching and wet etching.

[0033] Correspondingly, the technical solution of the present invention also provides a semiconductor structure, including: a substrate; a pseudo gate structure located on the substrate; a first opening in the substrate located on both sides of the pseudo gate structure, respectively, the first opening including a channel sidewall adjacent to the pseudo gate structure; a blocking layer located on the surface of the channel sidewall, a second opening in the substrate on both sides of the pseudo gate structure; and a covering layer located in the second opening.

[0034] Optionally, the material of the barrier layer includes silicon carbide.

[0035] Optionally, a dimension of the barrier layer along a direction perpendicular to the substrate is 4 nanometers to 5 nanometers, and a dimension of the barrier layer along a channel length direction is 3 nanometers to 7 nanometers.

[0036] Optionally, the substrate includes: a base, and a fin located on a surface of the base.

[0037] Optionally, the dummy gate structure spans across the fin, and the dummy gate structure is located on a portion of the top surface and sidewall surface of the fin.

[0038] Optionally, the dummy gate structure includes: a dummy gate layer and a first spacer located on a sidewall surface of the dummy gate layer.

[0039] Optionally, a material of the first spacer includes silicon oxide, silicon nitride, silicon oxynitride, silicon oxycarbide, silicon carbonitride or silicon carbon oxynitride.

[0040] Optionally, the thickness of the first sidewall spacer is 3 nanometers to 7 nanometers.

[0041] Optionally, the first opening exposes the bottom of the first side wall.

[0042] Optionally, it also includes: a first epitaxial layer located in the substrate at the bottom of the first opening; and the barrier layer is located on the surface of the first epitaxial layer.

[0043] Optionally, the method further includes: the first epitaxial layer is also located between the side wall of the barrier layer and the substrate.

[0044] Optionally, the first epitaxial layer has first doping ions, the material of the first epitaxial layer includes silicon carbide or silicon phosphide, and the first doping ions are N-type ions; the material of the first epitaxial layer includes silicon germanium, and the first doping ions are P-type ions.

[0045] Optionally, the cover layer contains second doping ions, the cover layer material includes silicon carbide or silicon phosphide, and the second doping ions are N-type ions; the cover layer material includes silicon germanium, and the second doping ions are P-type ions.

[0046] Optionally, the barrier layer includes third doping ions, the third doping ions are P-type ions or N-type ions, and the conductivity type of the third doping ions is opposite to the conductivity type of the second doping ions.

[0047] Optionally, a second epitaxial layer is provided in the second opening, and the cover layer is located on the second epitaxial layer.

[0048] Optionally, the second epitaxial layer has fourth doping ions, the material of the second epitaxial layer includes silicon carbide or silicon phosphide, and the fourth doping ions are N-type ions; the material of the second epitaxial layer includes silicon germanium, and the fourth doping ions are P-type ions.

[0049] Optionally, the depth of the first opening in a direction perpendicular to the substrate is 4 nanometers to 5 nanometers.

[0050] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:

[0051] In the method for forming a semiconductor structure in the technical solution of the present invention, first openings are respectively formed in the substrate on both sides of the pseudo gate structure, and a blocking layer is formed on the surface of the side wall of the first opening channel. The blocking layer is located at the bottom of the side wall of the gate structure and at the interface between the channel and the source and drain. Since the blocking layer has a blocking effect on the diffusion of doped ions, the blocking layer can effectively block the diffusion of source and drain doped ions into the channel region, thereby suppressing the short channel effect problem.

[0052] Furthermore, the barrier layer is silicon carbide. Since carbon has a barrier effect on the diffusion of doped ions, the barrier layer can effectively block the diffusion of source and drain doped ions into the channel region, thereby suppressing the short channel effect problem.

[0053] Furthermore, the size of the barrier layer is 4 to 5 nanometers along the direction perpendicular to the substrate, and the size of the barrier layer along the channel length direction is 3 to 7 nanometers. Since the volume of the barrier layer is very small, no large stress is generated in the channel, and no higher tunnel leakage is caused, which effectively improves the performance of the semiconductor device.

[0054] Furthermore, the barrier layer contains doped ions, and the doped ions have opposite conductivity types to the doped ions of the source and drain. The doped ions increase the resistance of the interface between the channel and the source and drain, thereby increasing the difficulty of current flowing from the source through the channel to the drain, avoiding tunnel leakage, and further suppressing the short channel effect of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0055] Figure 1 It is a schematic diagram of a cross-sectional structure of a semiconductor structure;

[0056] Figures 2 to 9 It is a schematic cross-sectional structure diagram corresponding to each step in a method for forming a semiconductor structure according to an embodiment of the present invention;

[0057] Figures 10 to 14 It is a schematic cross-sectional structure diagram corresponding to each step in a semiconductor structure forming method according to another embodiment of the present invention. DETAILED DESCRIPTION

[0058] As described in the background art, the performance of the semiconductor structure formed by the existing fin field effect transistor needs to be improved. Now, a semiconductor structure is described and analyzed.

[0059] Figure 1 It is a schematic diagram of the cross-sectional structure of a semiconductor structure.

[0060] Please refer to Figure 1 , a substrate 100, the substrate comprising a base 101, and a fin 102 located on the surface of the base; a gate structure 103 located on the fin 102, and the sidewalls of the gate structure 103 have a sidewall 104; and an epitaxial layer 105 located in the fin 102 on both sides of the gate structure 103 and the sidewall 104.

[0061] In the semiconductor structure, there are doped ions in the epitaxial layer 105, and the fin between the epitaxial layer 105 below the gate structure 103 is the channel region. As the size of semiconductor devices becomes smaller and smaller, the gate size is correspondingly reduced, and the channel region below the gate structure 103 becomes shorter. As the channel region becomes shorter, the doped ions will diffuse into the channel due to their wider distribution, thereby causing a short channel effect. At the same time, the annealing step in the formation process of the epitaxial layer 105 will also cause the doped ions in the epitaxial layer 105 to diffuse into the channel due to the thermal diffusion effect, thereby generating a short channel effect, which seriously affects the performance of the semiconductor device.

[0062] In order to improve the short channel effect, a method for forming a semiconductor structure in which carbon ions are directly doped into the source and drain regions is proposed. Due to the barrier effect of carbon on the diffusion of doped ions, this method can inhibit the diffusion of doped ions into the channel. However, due to the large damage generated in the channel during the doping process, it is easy to cause device leakage.

[0063] In order to solve the above problems, the technical solution of the present invention provides a semiconductor structure and a method for forming the same, comprising: forming first openings in the substrate on both sides of the pseudo gate structure, and forming a barrier layer on the sidewall surface of the first opening channel. Due to the barrier effect of the barrier layer on the diffusion of doped ions, the barrier layer can effectively block the diffusion of doped ions in the source and drain regions to the channel region, thereby suppressing the short channel effect problem.

[0064] In order to make the above-mentioned objects, characteristics and beneficial effects of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings.

[0065] Figures 2 to 9 It is a schematic cross-sectional structure diagram corresponding to each step in a semiconductor structure forming method according to an embodiment of the present invention.

[0066] Please refer to Figure 2, providing a substrate 200, wherein the substrate 200 includes a base 201 and a fin 202 on the surface of the base.

[0067] In this embodiment, the substrate 200 also has an isolation structure (not shown) covering the fin 202, the top surface of the isolation structure is lower than the top surface of the fin 202, and covers part of the sidewall of the fin 202. In other embodiments, the substrate is a planar base. The isolation structure is used to achieve electrical insulation between different semiconductor devices.

[0068] The substrate 201 and the fin 202 are made of silicon.

[0069] Please refer to Figure 3 A dummy gate structure 203 is formed on the substrate 200 , wherein the dummy gate structure 203 spans across the fin 202 , and the dummy gate structure 203 is located on a top surface and a sidewall surface of a portion of the fin 202 .

[0070] In this embodiment, the dummy gate structure 203 includes: a dummy gate layer 204 and a first spacer 205 located on the sidewall surface of the dummy gate layer 204. The first spacer 205 is used to locate the position of the barrier layer and the capping layer in the subsequent device manufacturing process.

[0071] The material of the first spacer 205 includes silicon oxide, silicon nitride, silicon oxynitride, silicon oxycarbide, silicon carbonitride or silicon carbon oxynitride.

[0072] The thickness of the first sidewall spacer 205 is 3 nanometers to 7 nanometers.

[0073] The method for forming the first sidewall spacer 205 includes: depositing a first sidewall spacer material on the surface of the substrate 200, the surface of the dummy gate junction layer 204 and the sidewall of the dummy gate layer 204, and etching the first sidewall spacer material until the surface of the substrate 200 and the surface of the dummy gate layer 204 are exposed.

[0074] In other embodiments, the method for forming the gate structure further includes: before forming the first sidewall, forming a second sidewall on the sidewall surface of the gate layer, wherein the second sidewall is located between the inner surface of the first sidewall and the sidewall surface of the gate layer.

[0075] The material of the second spacer includes silicon oxide, silicon nitride, silicon oxynitride, silicon oxycarbide, silicon carbonitride or silicon carbon oxynitride. The second spacer serves as a dielectric layer of the device in the subsequent device manufacturing process.

[0076] In this embodiment, first openings are subsequently formed in the substrate on both sides of the dummy gate structure 203, respectively, and the first openings have channel sidewalls adjacent to the dummy gate structure 203. The method for forming the first opening includes forming an initial first opening, forming an initial first epitaxial layer on the sidewall surface and the bottom surface of the initial first opening, etching the initial first epitaxial layer to form a first epitaxial layer, and forming the first opening. The formation process of the first opening is as follows: Figures 4 to 6 shown.

[0077] Please refer to Figure 4 Initial first openings 206 are respectively formed in the substrate 200 on both sides of the dummy gate structure 203 .

[0078] In this embodiment, the initial first opening 206 exposes a portion of the bottom of the dummy gate structure 203 , but does not expose the dummy gate layer 204 .

[0079] The initial first opening 206 is formed by one or both of a dry etching process and a wet etching process.

[0080] In this embodiment, the method for forming the initial first opening 206 includes: using the pseudo gate structure 203 as a mask, adopting an anisotropic dry etching process, etching the substrate 200 along a direction perpendicular to the substrate 200, and forming a transition opening in the substrate; using an isotropic wet etching process to etch the transition opening to form the initial first opening 206, so that the initial first opening 206 exposes a portion of the bottom of the first side wall 205, and the initial first opening 206 does not expose the bottom surface of the pseudo gate layer 204.

[0081] The process parameters of the anisotropic dry etching process include: the etching gas includes hydrogen bromide and chlorine, the power of the etcher is 100 watts to 1000 watts, the gas pressure in the etching chamber is 2 mTorr to 20 mTorr, the flow rate of hydrogen bromide is 10 standard milliliters per minute to 500 standard milliliters per minute, and the flow rate of chlorine is 10 standard milliliters per minute to 500 standard milliliters per minute.

[0082] The isotropic wet etching process comprises etching with tetramethylammonium hydroxide or potassium hydroxide solution.

[0083] Please refer to Figure 5 , at the initial first opening 206 (eg Figure 4 An initial first epitaxial layer 207 is formed on the sidewall surfaces and the bottom surface of the epitaxial layer 207.

[0084] The initial first epitaxial layer 207 is formed by an epitaxial growth process.

[0085] The initial first epitaxial layer 207 has a first doping ion. In this embodiment, the material of the initial first epitaxial layer 207 includes silicon carbide or silicon phosphide, and the first doping ion is an N-type ion. In other embodiments, the material of the initial first epitaxial layer includes silicon germanium, and the doping ion is a P-type ion. The initial first epitaxial layer is used to form a subsequent first epitaxial layer, and the first epitaxial layer is used to subsequently form a source and drain of a semiconductor device.

[0086] Please refer to Figure 6 , using the gate structure 203 as a mask, etching the initial first epitaxial layer 207, and forming a thin film on the initial first opening 206 (such as Figure 4 A first epitaxial layer 208 is formed in the dummy gate structure 203, and the first epitaxial layer 208 has a first opening 209 located on both sides of the dummy gate structure. The first opening 209 has a channel sidewall adjacent to the dummy gate structure, and the first opening 209 exposes a portion of the bottom of the dummy gate structure 203.

[0087] The thickness of the first epitaxial layer 208 is smaller than the depth of the initial first opening 206 .

[0088] The first opening 209 exposes a portion of the bottom of the dummy gate structure 203, but does not expose the dummy gate layer 204. The size and position of the first opening 209 determine the position and size of the barrier layer in the subsequent device manufacturing process.

[0089] The process of etching the initial first epitaxial layer 207 is one or both of a dry etching process and a wet etching process.

[0090] In this embodiment, the method for forming the first opening 209 includes: using the first side wall as a mask, and adopting an anisotropic dry etching process to etch the surface of the initial first epitaxial layer 207 along a direction perpendicular to the surface of the substrate 200; after etching the initial first epitaxial layer 207 by the anisotropic dry etching process, etching the initial first epitaxial layer 207 by an isotropic dry etching process, and exposing the bottom of the first side wall 205, and the bottom surface of the pseudo gate layer 204 is not exposed, so as to form the first epitaxial layer 208 and the first opening 209.

[0091] In this embodiment, the initial first epitaxial layer 207 is etched until a portion of the sidewall of the initial first opening is exposed to form the first epitaxial layer. In other embodiments, after etching the initial first epitaxial layer, a portion of the material of the initial first epitaxial layer is retained on the sidewall of the initial first opening, so that the first epitaxial layer is formed on the bottom surface of the initial first opening and the sidewall surface of the initial first opening.

[0092] In this embodiment, the depth of the first opening 209 is 4 nanometers to 5 nanometers. The size of the first opening 209 can be controlled by adjusting process parameters such as etching time and etching speed of the initial first epitaxial layer 207 .

[0093] In this embodiment, the first epitaxial layer 208 is further subjected to surface treatment to reduce the surface roughness of the first epitaxial layer 208. By reducing the surface roughness of the first epitaxial layer 208, defects introduced due to interface stress between the first epitaxial layer 208 and a subsequently formed cover layer can be reduced, thereby improving the reliability of the device.

[0094] The surface treatment process is dry etching.

[0095] The dry etching is chemical dry etching, and the process parameters include: the etching gas is CF4, Br2 or Cl2, the etching gas is treated with microwaves, the microwave power is 2GHz~3GHz, the reaction gas flow rate is 300sccm~500sccm, the pressure is 300mTorr~700mTorr, and the distance between the gas source after microwave treatment and the semiconductor substrate is 25cm~50cm.

[0096] In other embodiments, the initial first epitaxial layer does not fill the first initial opening. The first epitaxial layer on the sidewall surface of the initial first opening is relatively thin, so that the bottom of the gate structure is still partially exposed, thereby forming a first opening. The initial first epitaxial layer becomes the first epitaxial layer without further processing. The formation process of the first epitaxial layer is an epitaxial growth process, and the first epitaxial layer has doped ions. The material of the first epitaxial layer includes silicon carbide or silicon phosphide, and the doped ions are N-type ions; the material of the first epitaxial layer includes silicon germanium, and the doped ions are P-type ions.

[0097] Please refer to Figure 7 , at the first opening 209 (such as Figure 6 An initial barrier layer 210 is formed in the interior of the substrate.

[0098] The material of the initial barrier layer 210 includes silicon carbide. The reasons why silicon carbide can block the diffusion of doped ions include: first, because the carbon in the silicon carbide material has the function of blocking ion diffusion, it is difficult for doped ions such as boron ions or phosphorus ions to pass through the barrier layer when migrating to the barrier layer of the silicon carbide material, thereby reducing the diffusion of doped ions into the channel region; in addition, the silicon carbide material can be grown on the inner wall surface of the first opening by a selective epitaxial growth process, so that it is not easy to form defects such as dislocations between the silicon carbide material and the substrate material.

[0099] The initial barrier layer 210 is formed by an epitaxial growth process.

[0100] Please refer to Figure 8 , using the pseudo gate structure 203 as a mask, etching the initial blocking layer 210 (such as Figure 7 until the first opening 209 is exposed (as shown in Figure 6 A blocking layer 211 is formed on the surface of the channel sidewalls, and a second opening 212 is formed in the substrate on both sides of the dummy gate structure.

[0101] Subsequently, a capping layer is formed in the first opening 209, the capping layer has second doping ions, the first epitaxial layer 208 and the capping layer together form the source and drain of the device, and the region between the source and drain and below the gate structure 203 forms the channel of the device. The blocking layer 211 is located at the bottom of the sidewall of the gate structure 203 and at the interface between the channel and the source and drain. Due to the blocking effect of the blocking layer 211 on the diffusion of doping ions, the doping ions in the source and drain are blocked from diffusing into the channel.

[0102] The size of the barrier layer 211 along the direction perpendicular to the substrate is 4 to 5 nanometers, and the size of the barrier layer along the channel length direction is 3 to 7 nanometers. Since the volume of the barrier layer 211 is very small, no large stress will be generated at the interface between the barrier layer 211 and the source and drain, and at the interface between the barrier layer 211 and the channel, and no defects such as dislocation will be caused, thereby not causing device leakage.

[0103] In other embodiments, the barrier layer contains third doping ions. The third doping ions have a conductivity type opposite to that of the source and drain doping ions. The third doping ions increase the resistance of the interface between the channel and the source and drain, thereby increasing the difficulty of current flowing from the source through the channel to the drain, avoiding tunneling leakage, and further suppressing the short channel effect of the device.

[0104] The third doping ion concentration is 1E18 to 5E19 per cubic centimeter.

[0105] Please refer to Fig. 9 , at the second opening 212 (such as Figure 8 A covering layer 213 is formed inside the substrate.

[0106] The covering layer 213 is formed by an epitaxial growth process.

[0107] The cover layer 213 has second doping ions, the second doping ions are N-type ions, and the material of the cover layer includes silicon carbide or silicon phosphide. In other embodiments, the material of the cover layer includes silicon germanium, and the second doping ions are P-type ions. The cover layer 213 and the first epitaxial layer 208 together form the source and drain of the device, and the area between the source and drain and located below the gate structure 203 forms the channel of the device.

[0108] In other embodiments, before forming the cover layer, a second epitaxial layer is further formed in the second opening. The second epitaxial layer is formed by an epitaxial growth process. The second epitaxial layer fills up the second opening.

[0109] The second epitaxial layer has a fourth doping ion, and the first epitaxial layer, the second epitaxial layer and the capping layer together form a source and drain of the device. The material of the second epitaxial layer includes silicon carbide or silicon phosphide, and the fourth doping ion is an N-type ion. In other embodiments, the material of the second epitaxial layer includes silicon germanium, and the fourth doping ion is a P-type ion.

[0110] An embodiment of the present invention further provides a semiconductor structure formed by the above-mentioned forming method, please continue to refer to Fig. 9 , comprising: a substrate 200; a dummy gate structure 203 located on the substrate 200; first openings 209 (such as Figure 6 As shown), the first opening 209 includes a channel sidewall adjacent to the dummy gate structure 203; a barrier layer 211 located on the surface of the channel sidewall, and a second opening 212 (as shown) in the substrate on both sides of the dummy gate structure Figure 8 a covering layer 213 located in the second opening 212; and

[0111] The material of the barrier layer 211 includes silicon carbide.

[0112] The dimension of the barrier layer 211 along the direction perpendicular to the substrate is 4 nanometers to 5 nanometers, and the dimension of the barrier layer 211 along the channel length direction is 3 nanometers to 7 nanometers.

[0113] The substrate 200 includes a base 201 and a fin 202 located on a surface of the base 201 .

[0114] The dummy gate structure 203 spans across the fin 202 , and the dummy gate structure 203 is located on a portion of the top surface and sidewall surface of the fin 202 .

[0115] The dummy gate structure 203 includes a dummy gate layer 204 and a first spacer 205 located on the sidewall surface of the dummy gate layer 204 .

[0116] The material of the first spacer 205 includes silicon oxide, silicon nitride, silicon oxynitride, silicon oxycarbide, silicon carbonitride or silicon carbon oxynitride.

[0117] The thickness of the first sidewall spacer 205 is 3 nanometers to 7 nanometers.

[0118] The first opening 209 exposes the bottom of the first sidewall 205 .

[0119] The first epitaxial layer 208 is located in the substrate at the bottom of the first opening 209 ; the barrier layer 211 is located on the surface of the first epitaxial layer 208 .

[0120] The first epitaxial layer 208 has first doping ions therein. The material of the first epitaxial layer 208 includes silicon carbide or silicon phosphide, and the first doping ions are N-type ions. The material of the first epitaxial layer 208 includes silicon germanium, and the first doping ions are P-type ions.

[0121] The cover layer 213 has second doping ions therein. The material of the cover layer 213 includes silicon carbide or silicon phosphide, and the second doping ions are N-type ions. The material of the cover layer 213 includes silicon germanium, and the second doping ions are P-type ions.

[0122] The barrier layer 211 includes third doping ions, the third doping ions are P-type ions or N-type ions, and the conductivity type of the third doping ions is opposite to the conductivity type of the second doping ions.

[0123] The depth of the first opening 209 in a direction perpendicular to the substrate is 4 nanometers to 5 nanometers.

[0124] Figures 10 to 14 It is a schematic cross-sectional structure diagram corresponding to each step in a semiconductor structure forming method according to another embodiment of the present invention.

[0125] Please Figure 3 Continue to refer to Fig.10 A first opening 300 is formed in the substrate 200 on both sides of the dummy gate structure 203, wherein the first opening 300 has a channel sidewall adjacent to the dummy gate structure 203.

[0126] The first opening 300 is formed by one or both of a dry etching process and a wet etching process.

[0127] In this embodiment, the method for forming the first opening 300 includes: using the pseudo gate structure 203 as a mask, adopting an anisotropic dry etching process, etching the substrate 200 along a direction perpendicular to the substrate 200, and forming a transition opening in the substrate; using an isotropic wet etching process to etch the transition opening to form the initial first opening 206, so that the initial first opening 206 exposes a portion of the bottom of the first sidewall 205, and the initial first opening 300 does not expose the bottom surface of the pseudo gate layer 204.

[0128] The process parameters of the anisotropic dry etching process include: the etching gas includes hydrogen bromide and chlorine, the power of the etcher is 100 watts to 1000 watts, the gas pressure in the etching chamber is 2 mTorr to 20 mTorr, the flow rate of hydrogen bromide is 10 standard milliliters per minute to 500 standard milliliters per minute, and the flow rate of chlorine is 10 standard milliliters per minute to 500 standard milliliters per minute.

[0129] The wet etching process includes etching with tetramethylammonium hydroxide or potassium hydroxide solution.

[0130] Please refer to Fig.11 , at the first opening 300 (such as Fig.10 An initial barrier layer 301 is formed on the sidewall surface and the bottom surface of the substrate.

[0131] The material of the initial barrier layer 301 includes silicon carbide. The reasons why silicon carbide can block the diffusion of doped ions include: first, because the carbon in the silicon carbide material has the function of blocking ion diffusion, it is difficult for doped ions such as boron ions or phosphorus ions to pass through the barrier layer when migrating to the barrier layer of the silicon carbide material, thereby reducing the diffusion of doped ions into the channel region; in addition, the silicon carbide material can be grown on the inner wall surface of the first opening by a selective epitaxial growth process, so that it is not easy to form defects such as dislocations between the silicon carbide material and the substrate material.

[0132] The initial barrier layer 301 is formed by an epitaxial growth process.

[0133] Please refer to Fig.12 , using the pseudo gate structure 203 as a mask, etching the initial blocking layer 301 (such as Fig.11 ), until the surface of the substrate 200 is exposed, in the first opening 300 (as shown Fig.10 A blocking layer 303 is formed on the surface of the channel sidewalls, and a second opening 302 is formed in the substrate on both sides of the dummy gate structure.

[0134] The process of forming the second opening 302 is a dry etching process, and dry etching can achieve selective etching.

[0135] Subsequently, a second epitaxial layer and a capping layer are formed in the second opening 302, and the second epitaxial layer and the capping layer have doped ions. The second epitaxial layer and the capping layer together form the source and drain of the device, and the region between the source and drain and below the gate structure 203 forms the channel of the device. The blocking layer 303 is located at the bottom of the sidewall of the gate structure 203 and at the interface between the channel and the source and drain. Due to the blocking effect of the blocking layer 303 on the diffusion of doped ions, the doped ions in the source and drain are blocked from diffusing into the channel.

[0136] The size of the barrier layer 303 along the direction perpendicular to the substrate is 4 to 5 nanometers, and the size of the barrier layer along the channel length direction is 3 to 7 nanometers. Since the volume of the barrier layer 303 is very small, no large stress will be generated at the interface between the barrier layer 303 and the source and drain, and at the interface between the barrier layer 303 and the channel, and no defects such as dislocation will be caused, thereby not causing device leakage.

[0137] In other embodiments, the barrier layer contains third doping ions. The third doping ions have a conductivity type opposite to that of the source and drain doping ions. The third doping ions increase the resistance of the interface between the channel and the source and drain, thereby increasing the difficulty of current flowing from the source through the channel to the drain, avoiding tunneling leakage, and further suppressing the short channel effect of the device.

[0138] The third doping ion concentration is 1E18 to 5E19 per cubic centimeter.

[0139] Please refer to Fig.13 , a second epitaxial layer 304 is formed in the second opening 302 . The second epitaxial layer 304 completely fills the second opening 302 .

[0140] The process of forming the second epitaxial layer 304 is an epitaxial growth process.

[0141] The second epitaxial layer 304 has a fourth doping ion. In this embodiment, the material of the second epitaxial layer includes silicon carbide or silicon phosphide, and the fourth doping ion is an N-type ion. In other embodiments, the material of the second epitaxial layer includes silicon germanium, the second epitaxial layer has a doping ion, and the doping ion is a P-type ion.

[0142] Please refer to Fig.14 , a capping layer 305 is formed on the surface of the second epitaxial layer 304 .

[0143] The process of forming the cover layer 305 is an epitaxial growth process.

[0144] The capping layer 305 has second doping ions. In this embodiment, the material of the second epitaxial layer includes silicon carbide or silicon phosphide, and the second doping ions are N-type ions. In other embodiments, the material of the second epitaxial layer includes silicon germanium, and the second doping ions are P-type ions. The capping layer 305 and the second epitaxial layer 304 together form the source and drain of the device, and the area between the source and drain and located below the gate structure 203 forms the channel of the device.

[0145] Correspondingly, another embodiment of the present invention further provides a semiconductor structure formed by the above-mentioned forming method, please continue to refer to Fig.14 , comprising: a substrate 200; a dummy gate structure 203 located on the substrate 200; first openings 300 (such as Fig.10 As shown), the first opening 300 includes a channel sidewall adjacent to the dummy gate structure 203; a barrier layer 303 located on the surface of the channel sidewall, and a second opening 302 (as shown) in the substrate on both sides of the dummy gate structure 203 Fig.12 A covering layer 305 located in the second opening 302 .

[0146] The material of the barrier layer 303 includes silicon carbide.

[0147] The size of the barrier layer 303 along the direction perpendicular to the substrate is 4 nanometers to 5 nanometers, and the size of the barrier layer 303 along the channel length direction is 3 nanometers to 7 nanometers.

[0148] The substrate 200 includes a base 201 and a fin 202 located on a surface of the base 201 .

[0149] The dummy gate structure 203 spans across the fin 202 , and the dummy gate structure 203 is located on a portion of the top surface and sidewall surface of the fin 202 .

[0150] The dummy gate structure 203 includes a dummy gate layer 204 and a first spacer 205 located on the sidewall surface of the dummy gate layer 204 .

[0151] The material of the first spacer 205 includes silicon oxide, silicon nitride, silicon oxynitride, silicon oxycarbide, silicon carbonitride or silicon carbon oxynitride.

[0152] The thickness of the first sidewall spacer 205 is 3 nanometers to 7 nanometers.

[0153] The first opening 300 exposes the bottom of the first sidewall 205 .

[0154] The cover layer 305 has second doping ions therein. The material of the cover layer 305 includes silicon carbide or silicon phosphide, and the second doping ions are N-type ions. The material of the cover layer 305 includes silicon germanium, and the second doping ions are P-type ions.

[0155] The blocking layer 303 includes third doping ions, the third doping ions are P-type ions or N-type ions, and the conductivity type of the third doping ions is opposite to the conductivity type of the second doping ions.

[0156] A second epitaxial layer 304 is disposed in the second opening 302 , and the capping layer 305 is located on the second epitaxial layer 304 .

[0157] The second epitaxial layer 304 has fourth doping ions therein. The material of the second epitaxial layer 304 includes silicon carbide or silicon phosphide. The fourth doping ions are N-type ions. The material of the second epitaxial layer 304 includes silicon germanium. The fourth doping ions are P-type ions.

[0158] The depth of the first opening 300 in a direction perpendicular to the substrate is 4 nanometers to 5 nanometers.

[0159] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art may make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.

Claims

1. A method for forming a semiconductor structure, characterized in that: include: providing a substrate; forming a dummy gate structure on the substrate; forming an initial first opening in the substrate on both sides of the dummy gate structure; forming an initial first epitaxial layer in the initial first opening, wherein the initial first epitaxial layer is formed by an epitaxial growth process, and the initial first epitaxial layer has first doping ions; Using the dummy gate structure as a mask, etching the initial first epitaxial layer to form a first epitaxial layer in the initial first opening, wherein the first epitaxial layer has first openings located on both sides of the dummy gate structure, the first openings have channel sidewalls adjacent to the dummy gate structure, and the first openings expose a portion of the bottom of the dummy gate structure; A barrier layer is formed on the surface of the channel sidewall so that the first opening forms a second opening, and the method for forming the barrier layer includes: forming an initial barrier layer in the first opening, wherein the initial barrier layer is formed by an epitaxial growth process; Using the dummy gate structure as a mask, etching the initial barrier layer until the bottom of the first opening is exposed to form the barrier layer and the second opening; A cover layer is formed in the second opening, and the first epitaxial layer and the cover layer are used as a source and a drain.

2. The method for forming a semiconductor structure according to claim 1, wherein: The material of the barrier layer includes silicon carbide.

3. The method for forming a semiconductor structure according to claim 1, wherein: The size of the barrier layer along the direction perpendicular to the substrate is 4 nanometers to 5 nanometers, and the size of the barrier layer along the channel length direction is 3 nanometers to 7 nanometers.

4. The method for forming a semiconductor structure according to claim 1, wherein: The substrate includes: a base and a fin located on a surface of the base.

5. The method for forming a semiconductor structure according to claim 4, wherein: The dummy gate structure crosses the fin portion, and the dummy gate structure is located on a portion of a top surface and a sidewall surface of the fin portion.

6. The method for forming a semiconductor structure according to claim 1, wherein: The dummy gate structure includes: a dummy gate layer and a first spacer located on the sidewall surface of the dummy gate layer.

7. The method for forming a semiconductor structure according to claim 6, wherein: The material of the first spacer includes silicon oxide, silicon nitride, silicon oxynitride, silicon oxycarbide, silicon carbonitride or silicon carbon oxynitride.

8. The method for forming a semiconductor structure according to claim 6, wherein: The thickness of the first sidewall spacer is 3 nanometers to 7 nanometers.

9. The method for forming a semiconductor structure according to claim 6, wherein: The first opening exposes the bottom of the first side wall.

10. The method for forming a semiconductor structure according to claim 1, wherein: The process of etching the initial barrier layer includes dry etching.

11. The method for forming a semiconductor structure according to claim 1, wherein: The formation process of the first epitaxial layer is an epitaxial growth process; the material of the first epitaxial layer includes silicon carbide or silicon phosphide, and the first doping ions are N-type ions; the material of the first epitaxial layer includes silicon germanium, and the first doping ions are P-type ions.

12. The method for forming a semiconductor structure according to claim 1, wherein: Also includes: Before forming the barrier layer, the first epitaxial layer is subjected to surface treatment to reduce the roughness of the surface of the first epitaxial layer.

13. The method for forming a semiconductor structure according to claim 12, wherein: The surface treatment process is one or both of dry etching and wet etching.

14. The method for forming a semiconductor structure according to claim 13, wherein: The process parameters of the dry etching include: the etching gas includes hydrogen bromide and chlorine, the power of the etcher is 100 watts to 1000 watts, the gas pressure in the etching chamber is 2 mTorr to 20 mTorr, the flow rate of hydrogen bromide is 10 standard milliliters per minute to 500 standard milliliters per minute, and the flow rate of chlorine is 10 standard milliliters per minute to 500 standard milliliters per minute.

15. The method for forming a semiconductor structure according to claim 1, wherein: The thickness of the first epitaxial layer is less than the depth of the initial first opening.

16. The method for forming a semiconductor structure according to claim 1, wherein: The initial first opening exposes the bottom of the pseudo gate structure portion, and the method for forming the first epitaxial layer includes: forming an initial first epitaxial layer on the side wall surface and the bottom surface of the initial first opening; using the pseudo gate structure as a mask, etching the initial first epitaxial layer to form the first epitaxial layer. 17 . The method for forming a semiconductor structure according to claim 16 , wherein the process of etching the initial first epitaxial layer comprises one or both of dry etching and wet etching.

18. The method for forming a semiconductor structure according to claim 1, wherein: The covering layer is formed by an epitaxial growth process, the covering layer contains second doping ions, the material of the covering layer includes silicon carbide or silicon phosphide, and the second doping ions are N-type ions; the material of the covering layer includes silicon germanium, and the second doping ions are P-type ions.

19. The method for forming a semiconductor structure according to claim 18, wherein: The barrier layer includes third doping ions, the third doping ions are P-type ions or N-type ions, and the conductivity type of the third doping ions is opposite to the conductivity type of the second doping ions.

20. The method for forming a semiconductor structure according to claim 1, wherein: Also includes: Before forming the capping layer, a second epitaxial layer is formed in the second opening.

21. The method for forming a semiconductor structure according to claim 20, wherein: The second epitaxial layer is formed by an epitaxial growth process, the second epitaxial layer has fourth doping ions, the second epitaxial layer material includes silicon carbide or silicon phosphide, and the fourth doping ions are N-type ions; The material of the second epitaxial layer includes silicon germanium, and the fourth doping ions are P-type ions.

22. The method for forming a semiconductor structure according to claim 1, wherein: The depth of the first opening is 4 nanometers to 5 nanometers.

23. A semiconductor structure, characterized in that: include: substrate; a dummy gate structure located on the substrate; First openings in the substrate respectively located on both sides of the dummy gate structure, the first openings including channel sidewalls adjacent to the dummy gate structure; a first epitaxial layer in the substrate at the bottom of the first opening; A barrier layer located on the surface of the channel sidewall and the surface of the first epitaxial layer, wherein the barrier layer is an epitaxial layer, and the first opening not filled by the barrier layer is a second opening; The cover layer located in the second opening uses the first epitaxial layer and the cover layer as a source and a drain.

24. The semiconductor structure according to claim 23, wherein: The material of the barrier layer includes silicon carbide.

25. The semiconductor structure according to claim 23, wherein: The size of the barrier layer along the direction perpendicular to the substrate is 4 nanometers to 5 nanometers, and the size of the barrier layer along the channel length direction is 3 nanometers to 7 nanometers.

26. The semiconductor structure according to claim 23, wherein: The substrate includes: a base and a fin located on a surface of the base.

27. The semiconductor structure according to claim 26, wherein: The dummy gate structure crosses the fin portion, and the dummy gate structure is located on a portion of a top surface and a sidewall surface of the fin portion.

28. The semiconductor structure according to claim 23, wherein: The dummy gate structure includes: a dummy gate layer and a first spacer located on the sidewall surface of the dummy gate layer.

29. The semiconductor structure according to claim 28, wherein: The material of the first spacer includes silicon oxide, silicon nitride, silicon oxynitride, silicon oxycarbide, silicon carbonitride or silicon carbon oxynitride.

30. The semiconductor structure of claim 28, wherein: The thickness of the first sidewall spacer is 3 nanometers to 7 nanometers.

31. The semiconductor structure of claim 28, wherein: The first opening exposes the bottom of the first side wall.

32. The semiconductor structure of claim 23, wherein: Also includes: The first epitaxial layer is also located between the sidewall of the barrier layer and the substrate.

33. The semiconductor structure of claim 23, wherein: The first epitaxial layer has first doping ions therein, the material of the first epitaxial layer includes silicon carbide or silicon phosphide, and the first doping ions are N-type ions; the material of the first epitaxial layer includes silicon germanium, and the first doping ions are P-type ions.

34. The semiconductor structure of claim 23, wherein: The cover layer has second doping ions in it, the cover layer material includes silicon carbide or silicon phosphide, and the second doping ions are N-type ions; the cover layer material includes silicon germanium, and the second doping ions are P-type ions.

35. The semiconductor structure of claim 34, wherein: The barrier layer includes third doping ions, the third doping ions are P-type ions or N-type ions, and the conductivity type of the third doping ions is opposite to the conductivity type of the second doping ions.

36. The semiconductor structure of claim 23, wherein: Also includes: A second epitaxial layer is disposed in the second opening, and the cover layer is located on the second epitaxial layer.

37. The semiconductor structure according to claim 36, wherein: The second epitaxial layer has fourth doping ions, the material of the second epitaxial layer includes silicon carbide or silicon phosphide, and the fourth doping ions are N-type ions; the material of the second epitaxial layer includes silicon germanium, and the fourth doping ions are P-type ions.

38. The semiconductor structure of claim 23, wherein: The depth of the first opening in a direction perpendicular to the substrate is 4 nanometers to 5 nanometers.

Citation Information

Patent Citations

  • Semiconductor structure and formation method thereof

    CN108074973A

  • Semiconductor device and manufacturing method thereof

    CN110047754A

  • Semiconductor device and method of fabricating the same

    CN110047908A

  • Semiconductor structure and forming method thereof

    CN110323137A

  • Semiconductor Devices Having Shallow Junctions

    US20120091469A1