Photovoltaic cell series and photovoltaic module manufacturing method
By designing trapezoidal projection and groove structure on the packaging layer of the photovoltaic module, the extrusion pressure problem between the cells during the lamination process is solved, the risk of hidden cracking is reduced, and high-power, small-size photovoltaic modules are realized Stable manufacturing.
Patent Information
- Application Number
- CN202010834480.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-08-19
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2040-08-19
AI Technical Summary
During the lamination process, existing photovoltaic modules cannot eliminate the squeeze pressure between adjacent cells after the welding tape is flattened, resulting in small cracks on the edge of the cell cutting surface, increasing the risk of hidden cracks.
The trapezoidal protrusion and groove structure are designed on the packaging layer of the battery cell, and corresponding grooves are provided on the welding belt, and the protrusions protrude into the groove. The formed packaging layer offsets the adhesive sheet from the battery during the lamination process. The extrusion pressure of the sheet reduces the shear force.
It effectively reduces the risk of hidden cracks in the cell, meets the manufacturing needs of high-power, small-size photovoltaic modules, and reduces the occurrence of cracks after cell lamination.
Smart Images

Figure CN114078980B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a photovoltaic cell series and a photovoltaic component manufacturing method, belonging to the technical field of photovoltaic component lamination. Background Art
[0002] With the continuous development of the photovoltaic industry, high power and small size have become the mainstream of the new generation. The current photovoltaic industry uses small-pitch 156 half-cells as mainstream products, but small-pitch components have the following defects: due to the reduction in the distance between cells, the solder strips need to be flattened, and even after the solder strips are flattened, the squeezing force between two adjacent cells cannot be eliminated. Therefore, the compression of the rubber sheet on the component during the lamination process will cause fine cracks on the edge of the cut surface of the cell, increasing the risk of hidden cracks after the cell is laminarized.
[0003] In view of this, it is indeed necessary to improve the existing photovoltaic modules to solve the above problems. Summary of the invention
[0004] The object of the present invention is to provide a photovoltaic cell series and a photovoltaic module manufacturing method to reduce the pressing force of the adhesive sheet on the cut surface of the cell sheet during lamination.
[0005] To achieve the above-mentioned purpose, the present invention provides a photovoltaic cell series, including a plurality of cells arranged in an extension direction thereof, a welding strip connecting two adjacent cells in series, and an encapsulation layer encapsulating and fixing the cell cells and the welding strip, wherein the encapsulation layer includes an encapsulation body and a convex portion protruding outward from a side surface in a thickness direction of the encapsulation body, a groove is concavely provided on the welding strip, and the convex portion protrudes into the groove, and in the extension direction of the encapsulation body, the convex portion is located beside the center line of the encapsulation body; the cell includes a first cell and a second cell arranged adjacently, the encapsulation layer includes a second encapsulation layer located above the first cell and a first encapsulation layer located below the second cell, a first convex portion is formed on the first encapsulation layer, a second convex portion is formed on the second encapsulation layer, grooves are respectively concavely provided on the upper wall surface and the lower wall surface of the welding strip, and the first convex portion and the second convex portion respectively protrude into the corresponding grooves.
[0006] As a further improvement of the present invention, the protrusion is arranged in a trapezoidal shape, and the width of the long side of the trapezoid is 1 to 2 mm, and the height is 0.3 to 0.5 mm.
[0007] As a further improvement of the present invention, the groove is close to the gap between the first battery cell and the second battery cell, the first protrusion and the second protrusion are respectively located on both sides of the gap, and the width of the groove is greater than the maximum width of the corresponding first protrusion or the second protrusion.
[0008] As a further improvement of the present invention, the groove recessed in the lower wall of the welding strip is defined as a first groove, and the groove recessed in the upper wall of the welding strip is defined as a second groove. The first groove and the second groove overlap at the gap between the first battery cell and the second battery cell, and in the series connection direction of the first battery cell and the second battery cell, the sum of the widths of the first groove and the second groove is 4 to 5 mm.
[0009] To achieve the above object, the present invention also provides a method for manufacturing a photovoltaic module, comprising:
[0010] Providing a first encapsulation layer, wherein a first protrusion is formed on one side surface of the first encapsulation layer in a thickness direction;
[0011] Placing a battery string on the first packaging layer, and making the gap between two adjacent battery cells in the battery string close to the first protrusion;
[0012] Providing a second encapsulation layer, wherein a second protrusion is formed on one side surface of the second encapsulation layer in the thickness direction, and laying the second encapsulation layer on the surface of the battery string so that the second protrusion and the first protrusion are respectively located on both sides of the gap;
[0013] A pressure perpendicular to the thickness direction of the first packaging layer and the second packaging layer is provided to package the battery string between the first packaging layer and the second packaging layer.
[0014] As a further improvement of the present invention, the height of the first protrusion and the height of the second protrusion are both greater than the thickness of the battery cell.
[0015] As a further improvement of the present invention, both the first encapsulation layer and the second encapsulation layer are EVA adhesive layers; or both the first encapsulation layer and the second encapsulation layer are POE adhesive layers.
[0016] The beneficial effect of the present invention is as follows: the present invention forms a first protrusion on one side surface of the first packaging layer in the thickness direction, and simultaneously forms a second protrusion on one side surface of the second packaging layer in the thickness direction, so that during the lamination process, the first protrusion and the second protrusion can be used to offset the squeezing force of the rubber plate on the battery cell, reduce the shear force between the welding strip and the cut surface of the battery cell, and reduce the risk of hidden cracks in the battery cell. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a flow chart of the photovoltaic module manufacturing method of the present invention.
[0018] Figure 2 It corresponds to Figure 1 Schematic diagram of the structure of step S1 in FIG.
[0019] Figure 3 It corresponds to Figure 1Schematic diagram of the structure of step S2 in FIG.
[0020] Figure 4 It corresponds to Figure 1 Schematic diagram of the structure of step S3 in FIG.
[0021] Figure 5 It is a schematic diagram of a photovoltaic module manufactured by the photovoltaic module manufacturing method of the present invention. DETAILED DESCRIPTION
[0022] In order to make the purpose, technical solutions and advantages of the present invention more clear, the present invention is described in detail below with reference to the accompanying drawings and specific embodiments.
[0023] like Figure 1 and Figure 4 As shown, the present invention discloses a method for manufacturing a photovoltaic module, which mainly includes the following steps:
[0024] S1, providing a first encapsulation layer 10, wherein a first protrusion 11 is formed on one side surface of the first encapsulation layer 10 in a thickness direction;
[0025] S2, placing a battery string 20 on the first packaging layer 10, and making the gap 24 between two adjacent battery cells in the battery string 20 close to the first protrusion 11;
[0026] S3, providing a second encapsulation layer 30, wherein a second protrusion 31 is formed on one side surface of the second encapsulation layer 30 in the thickness direction, and laying the second encapsulation layer 30 on the surface of the battery string 20, so that the second protrusion 31 and the first protrusion 11 are respectively located on both sides of the gap 24;
[0027] S4. Providing pressure perpendicular to the thickness direction of the first encapsulation layer 10 and the second encapsulation layer 30 to encapsulate the battery string 20 between the first encapsulation layer 10 and the second encapsulation layer 30 .
[0028] Combination Figures 2 to 4 As shown, the first encapsulation layer 10 includes a first encapsulation body 12 and a first protrusion 11 formed by protruding outward from a side surface in the thickness direction of the first encapsulation body 12; in the extension direction of the first encapsulation body 12, the first protrusion 11 is located beside the center line of the first encapsulation body 12. The second encapsulation layer 30 includes a second encapsulation body 32 and a second protrusion 31 formed by protruding outward from a side surface in the thickness direction of the second encapsulation body 32; in the extension direction of the second encapsulation body 32, the second protrusion 31 is located beside the center line of the second encapsulation body 32.
[0029] In other words, the first encapsulation layer 10 and the second encapsulation layer 30 are arranged correspondingly, and the structure and size of the first encapsulation layer 10 are respectively the same as the structure and size of the second encapsulation layer 30. In this way, when manufacturing the first encapsulation layer 10 and the second encapsulation layer 30, only one encapsulation layer needs to be manufactured separately to meet the requirements, which reduces the number of molds to be manufactured, and saves manufacturing time and manufacturing costs. When in use, the first encapsulation layer 10 can be directly rotated 180° to be used as the second encapsulation layer 30.
[0030] The first encapsulation layer 10 and the second encapsulation layer 30 are both EVA adhesive layers or POE adhesive layers; of course, they can also be other adhesive layers as long as they can achieve the encapsulation of the photovoltaic cell series.
[0031] In this embodiment, the first protrusion 11 and the second protrusion 31 are both arranged in a trapezoidal shape, and the width of the long side of the trapezoid is 1 to 2 mm, and the height is 0.3 to 0.5 mm. Of course, in other embodiments, the shape of the first protrusion 11 and the second protrusion 31 can also be cylindrical, semicircular or triangular, as long as they have the function of absorbing pressure. The number of the first protrusion 11 and the second protrusion 31 can be designed according to actual needs, and is not limited here.
[0032] The photovoltaic cell series includes a plurality of cells arranged in the extension direction thereof, a welding strip connecting two adjacent cells in series, and the aforementioned packaging layer that seals and fixes the cells and the welding strip. For example, a cell string 20 includes a first cell 21 and a second cell 22 arranged adjacent to each other, and a welding strip 23 connecting the first cell 21 and the second cell 22 in series. Figure 3 As shown, the cells are arranged horizontally with spacing therebetween and vertically with staggered spacing therebetween, so as to leave a gap 24 of about 0.7 mm between the first cell sheet 21 and the second cell sheet 22 to facilitate serial connection of the solder strips 23 .
[0033] The second encapsulation layer 30 is located above the first battery cell 21, and the first encapsulation layer 10 is located below the second battery cell 22. The welding strip 23 includes a first portion 231 connected to the lower surface of the first battery cell 21, a second portion 232 connected to the upper surface of the second battery cell 22, and a connecting portion 233 passing through the gap 24 and connecting the first portion 231 and the second portion 232. Grooves (not numbered) are respectively formed on the upper wall and the lower wall of the welding strip 23, and the first protrusion 11 and the second protrusion 31 protrude into the corresponding grooves.
[0034] The groove concavely arranged on the lower wall of the welding strip 23 is defined as the first groove 234, and the groove concavely arranged on the upper wall of the welding strip 23 is defined as the second groove 235, and the first groove 234 and the second groove 235 overlap at the gap 24 between the first battery cell 21 and the second battery cell 22. In other words, the first groove 234 is formed by being concave upward from the lower surface of the first portion 231 and the connecting portion 233 of the welding strip 23, and the second groove 235 is formed by being concave downward from the upper surface of the second portion 232 and the connecting portion 233 of the welding strip 23, so that the connecting portion 233 and the left and right parts of the connecting portion 233 of the welding strip 23 are flat (i.e., the thickness of the connecting portion 233 and the left and right parts of the connecting portion 233 are reduced), and the vertical distance between the first battery cell 21 and the second battery cell 22 (i.e., the distance in the vertical direction) is shortened.
[0035] The first groove 234 and the second groove 235 are close to the gap 24 and are disposed on both sides of the gap 24. Figure 4 In the horizontal direction shown, the widths of the first groove 234 and the second groove 235 are greater than the maximum widths of the corresponding first protrusion 11 and the second protrusion 31; Figure 4 In the vertical direction shown, the heights of the first protrusion 11 and the second protrusion 31 are both greater than the thicknesses of the first battery cell 21 and the second battery cell 22. This arrangement enables the first protrusion 11 and the second protrusion 31 to play a certain supporting role before lamination, and gradually melt and solidify during the lamination process to absorb the squeezing force of the rubber sheet on the battery cell during lamination, reduce the shear force between the welding ribbon 23 and the cut surface of the battery cell, and reduce the risk of hidden cracks in the battery cell.
[0036] In the series connection direction of the first battery cell 21 and the second battery cell 22 (i.e. Figure 3 In the horizontal direction shown in the figure, the sum of the widths of the first groove 234 and the second groove 235 is 4 to 5 mm, so that better manufacturing accuracy can be achieved.
[0037] In the present invention, the first raised portion 11 and the second raised portion 31 are regularly arranged and correspond to the flattened portion of the welding strip 23, and have better laying accuracy; of course, due to the continuous change in the size of the battery cell, the positions of the first raised portion 11 and the second raised portion 31 also change accordingly, as long as they are close to the gap 24 of the battery cell, they can also achieve the effect of absorbing the extrusion force and reducing the risk of hidden cracks in the battery cell.
[0038] like Figure 5 As shown, the photovoltaic module manufactured by the photovoltaic module manufacturing method of the present invention rarely or even never has the phenomenon of hidden cracks in the cell, thus meeting the mainstream requirements of high power and small size.
[0039] To sum up, the present invention forms a first protrusion 11 on one side surface of the first packaging layer 10 in the thickness direction, and simultaneously forms a second protrusion 31 on one side surface of the second packaging layer 30 in the thickness direction, so that before lamination, the first protrusion 11 and the second protrusion 31 can play a certain supporting role, and during the lamination process, the first protrusion 11 and the second protrusion 31 gradually melt and solidify and harden, which can offset the squeezing force of the rubber plate on the battery cell, reduce the shear force between the welding strip 23 and the cut surface of the battery cell, and reduce the risk of hidden cracks in the battery cell.
[0040] The above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention may be modified or replaced by equivalents without departing from the spirit and scope of the technical solution of the present invention.
Claims
1. A photovoltaic cell series, comprising a plurality of cells arranged in the extension direction thereof, a welding strip connecting two adjacent cells in series, and a packaging layer for packaging and fixing the cells and the welding strip, characterized in that: The packaging layer includes a packaging body and a protrusion formed by protruding outward from one side surface of the packaging body in the thickness direction, a groove is concavely provided on the welding strip, the protrusion protrudes into the groove, and in the extension direction of the packaging body, the protrusion is located beside the center line of the packaging body; the battery cell includes a first battery cell and a second battery cell arranged adjacent to each other, the packaging layer includes a second packaging layer located above the first battery cell and a first packaging layer located below the second battery cell, a first protrusion is formed on the first packaging layer, and a second protrusion is formed on the second packaging layer, grooves are respectively concavely provided on the upper wall surface and the lower wall surface of the welding strip, the grooves are close to the gap between the first battery cell and the second battery cell and are arranged on both sides of the gap, the grooves overlap at the gap, the first protrusion and the second protrusion are respectively located on both sides of the gap, and respectively protrude into the corresponding grooves.
2. The photovoltaic cell series according to claim 1, characterized in that: The protrusion is arranged in a trapezoidal shape, and the width of the long side of the trapezoid is 1 to 2 mm, and the height is 0.3 to 0.5 mm.
3. The photovoltaic cell series according to claim 1, characterized in that: The width of the groove is greater than the maximum width of the corresponding first protrusion or the second protrusion.
4. The photovoltaic cell series according to claim 3, characterized in that: The groove recessed in the lower wall of the welding strip is defined as the first groove, and the groove recessed in the upper wall of the welding strip is defined as the second groove. The first groove and the second groove overlap at the gap between the first battery cell and the second battery cell, and in the series connection direction of the first battery cell and the second battery cell, the sum of the widths of the first groove and the second groove is 4 to 5 mm.
5. A method for manufacturing a photovoltaic module, characterized in that: include: Providing a first encapsulation layer, wherein a first protrusion is formed on one side surface of the first encapsulation layer in a thickness direction; A battery string is placed on the first packaging layer, and a gap between two adjacent battery cells in the battery string is close to the first protrusion, the battery string includes a welding strip connecting the two battery cells in series, and grooves are respectively formed on the upper wall and the lower wall of the welding strip, the grooves are close to the gap and are arranged on both sides of the gap, the grooves overlap at the gap, and the first protrusion protrudes into the corresponding grooves; Providing a second encapsulation layer, wherein a second protrusion is formed on one side surface of the second encapsulation layer in the thickness direction, laying the second encapsulation layer on the surface of the battery string, and making the second protrusion and the first protrusion respectively located on both sides of the gap, and the second protrusion protruding into the corresponding groove; A pressure perpendicular to the thickness direction of the first packaging layer and the second packaging layer is provided to package the battery string between the first packaging layer and the second packaging layer.
6. The method for manufacturing a photovoltaic module according to claim 5, characterized in that: The height of the first protrusion and the height of the second protrusion are both greater than the thickness of the battery cell.
7. The method for manufacturing a photovoltaic module according to claim 5, characterized in that: The first encapsulation layer and the second encapsulation layer are both EVA adhesive layers; or, the first encapsulation layer and the second encapsulation layer are both POE adhesive layers.
Citation Information
Patent Citations
Photovoltaic module and preparation method
CN107887462A
Photovoltaic module and manufacturing method thereof
CN110176513A
Solar cell module and preparation method
CN111293190A
Double-sided double-glass photovoltaic module
CN208970536U
Packaging adhesive film and device for producing packaging adhesive film
CN210379073U