Preparation method of peel strength test sample and peel strength test sample

By preparing peel strength test samples of photovoltaic modules, the inaccuracy and safety hazards of traditional testing methods are solved by using stacking and lamination technology, low-cost and rapid peel strength testing are achieved, and production efficiency and testing safety are improved. sex.

CN114295434BActive Publication Date: 2024-11-19WUXI UTMOST LIGHT TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111406779.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-11-24
Publication Date
2024-11-19
Estimated Expiration
2041-11-24

AI Technical Summary

Technical Problem

The peel strength testing method of traditional photovoltaic modules has problems such as inaccurate testing, high cost, long cycle and safety hazards. Especially when using PVB packaging materials, the existing methods cannot effectively evaluate the adhesion between the glass and the packaging film.

Method used

A method for preparing a peel strength test sample is adopted, including stacking a glass substrate, an isolation sheet, a first PVB plate, a metal back plate and a second PVB plate in sequence, and fixing and extracting the isolation sheet to prepare a peel strength test sample. The parts avoid tensile deformation and bonding problems of traditional methods, reduce test costs and cycles, and improve safety.

Benefits of technology

It realizes rapid and low-cost peel strength testing in the photovoltaic module factory, avoiding the safety risks of ball drop experiments and shotgun experiments, improving testing accuracy and production efficiency, and reducing testing costs and cycles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114295434B_ABST
    Figure CN114295434B_ABST
Patent Text Reader

Abstract

The present application discloses a method for preparing a peel strength test sample and a peel strength test sample, wherein a glass substrate, a spacer, a first PVB board and a metal backplane are stacked in sequence; wherein the length of the spacer is less than the length of the glass substrate, and the length of the first PVB board is greater than the length of the spacer; the spacer is laminated and fixed, and the spacer is extracted to obtain the peel strength preparation sample. Thus, the second PVB board, the metal backplane, the first PVB board, the spacer and the glass substrate are packaged. On the one hand, there is no need to use finished photovoltaic modules for peel strength testing, which can reduce testing costs and testing cycles, and facilitate photovoltaic module manufacturers to adjust lamination parameters in a timely manner, improve production efficiency and production utilization rate; on the other hand, photovoltaic modules encapsulated with PVB can obtain relevant data of glass strength testing without the need for falling ball tests or shotgun tests, which can improve the experimental safety of glass strength testing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of peel strength testing of photovoltaic modules, and in particular to a method for preparing a peel strength testing sample and a peel strength testing sample. Background Art

[0002] The adhesion between the encapsulation film and glass of photovoltaic modules is an important indicator of product performance, which directly determines the safe use and long-term performance of the product. It is generally characterized by tensile testing the peel strength between the glass and the encapsulation film.

[0003] Since the encapsulation film has greater elasticity after lamination, the encapsulation film has greater extension deformation during the tensile test, which leads to inaccurate test results. Therefore, for double-glass photovoltaic modules using EVA (ethylene-vinyl acetate copolymer) or POE (polymer of ethylene and butene; or ethylene and octene) as the encapsulation film, when testing the encapsulation film and glass, a backplane that is well bonded to the glass and has a large tensile modulus is attached to the side of the encapsulation film away from the glass. The glass is fixed at one end and the encapsulation film and the backplane are pulled at the other end to obtain the peel strength between the encapsulation film and the glass.

[0004] However, when photovoltaic modules with traditional EVA or POE encapsulation films are assembled on the top of buildings as BAPV modules (photovoltaic modules installed on existing buildings), because EVA or POE are new materials, they are not favored by owners and architects. Therefore, PVB (polyvinyl butyral) material is used as the encapsulation material to process photovoltaic modules.

[0005] However, the current PVB-encapsulated photovoltaic modules can refer to the mature manufacturing methods of traditional architectural glass, using the process of laminator pre-pressing + autoclave, or the process of laminator combined with high-pressure roller. Because PVB, like EVA and POE materials, has large deformation during stretching, and PVB cannot be bonded to existing backplane materials, it is impossible to use the existing peeling method to perform peeling strength tests. Instead, the finished photovoltaic modules are used for drop ball tests or shotgun tests to determine whether the adhesion between PVB and glass is qualified based on whether the fragments are still attached to the encapsulation film after the glass is broken.

[0006] However, this type of test requires the use of a specialized testing machine, which poses certain safety risks. PV module manufacturers usually do not have the testing conditions and generally outsource the testing, which has a long testing cycle and high costs. Summary of the invention

[0007] The present invention aims to solve at least one of the technical problems existing in the prior art. To this end, one purpose of the present invention is to provide a method for preparing a peel strength test sample of a photovoltaic module, wherein the peel strength test sample prepared by the preparation method can be used to perform a peel strength test on a photovoltaic module with a short cycle and low cost.

[0008] The present application further proposes a peel strength test sample prepared by the above preparation method.

[0009] According to the first aspect of the present application, a method for preparing a peel strength test sample of a photovoltaic module includes:

[0010] A glass substrate, a spacer, a first PVB board, a metal backboard and a second PVB board are stacked in sequence; wherein the length of the spacer is shorter than the length of the glass substrate, and the length of the first PVB board is longer than the length of the spacer;

[0011] The laminate is fixed, and the isolation sheet is extracted to obtain the peel strength sample.

[0012] According to the preparation method of the glass strength test sample of the embodiment of the present application, the second PVBA board, the metal backboard, the first PVB board, the isolation sheet and the glass substrate are packaged. On the one hand, there is no need to use finished photovoltaic modules for peel strength testing, and there is no need to outsource the testing to a special testing organization, which can reduce the testing cost and testing cycle, and facilitate photovoltaic module manufacturers to adjust the lamination parameters in time, improve production efficiency and production utilization rate; on the other hand, photovoltaic modules packaged with PVB do not need to conduct falling ball tests or shotgun tests to obtain relevant data of the glass strength test, which can improve the experimental safety of the glass strength test.

[0013] According to some embodiments of the present application, the preparation method further includes: before lamination and fixing, stacking a second PVB board on top of the metal backboard.

[0014] Furthermore, the length L1 of the isolation plate and the length L2 of the glass substrate satisfy: 0.4L2≤L1≤0.6L2.

[0015] In some embodiments, the width of the isolation sheet is smaller than the width of the glass substrate, and the width of the isolation sheet is greater than the width of the first PVB board.

[0016] According to some embodiments of the present application, the width of the metal back plate is ≥ the width of the first PVB plate.

[0017] Furthermore, the length of the metal back plate is less than the length of the first PVB plate, and an end of the metal back plate away from the isolation sheet is flush with an edge of an end on the same side of the first PVB plate.

[0018] In some embodiments, the thickness of the metal back plate is 0.1 mm-1.0 mm.

[0019] Furthermore, the metal back plate is constructed as any one of a copper back plate, a tinned copper back plate, and an aluminum back plate.

[0020] In some embodiments, geometric dimensions of the second PVB board are consistent with geometric dimensions of the first PVB board.

[0021] According to the peel strength test sample of the photovoltaic module in the second embodiment of the present application, the peel strength test sample is prepared based on the preparation method described in the above embodiment.

[0022] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, in which:

[0024] Figure 1 is a three-dimensional schematic diagram of a peel strength test sample and a separator according to an embodiment of the present application;

[0025] Figure 2 is a schematic diagram of the cooperation of a peel strength test sample and a separator at an angle according to an embodiment of the present application;

[0026] Figure 3 is a schematic diagram of the cooperation between the glass strength test sample and the isolation sheet at another angle according to an embodiment of the present application;

[0027] Figure 4 4 is a flow chart of a method for preparing a glass strength test sample according to an embodiment of the present application.

[0028] Reference numerals:

[0029] Peel strength test sample 100, isolation sheet 200,

[0030] A glass substrate 10 , a first PVB board 20 , a metal back board 30 , and a second PVB board 40 . DETAILED DESCRIPTION

[0031] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.

[0032] Reference below Figure 1-Figure 4 A method for preparing a peeling strength test specimen 100 and the peeling strength test specimen 100 according to an embodiment of the present invention are described.

[0033] like Figure 1 and Figure 4 As shown, a method for preparing a peel strength test sample 100 of a photovoltaic module according to an embodiment of the first aspect of the present application includes:

[0034] Step 10: stacking a glass substrate 10, a spacer 200, a first PVB board 20, a metal backboard 30 and a second PVB board 40 in sequence; wherein the length of the spacer 200 is shorter than the length of the glass substrate 10, and the length of the first PVB board 20 is longer than the length of the spacer 200;

[0035] Step 20: After lamination and fixing, the isolation sheet 200 is extracted to obtain a peel strength sample.

[0036] Among them, step 10 is specifically: stacking the isolation film 200 on the glass substrate 10, then stacking the first PVB board 20 on the isolation film 200, and then stacking the metal backboard 30 on the first PVB board 20. Step 20 is specifically: after the stacking is completed, lamination and fixation are performed, and after lamination and fixation, the isolation film 200 is pulled out.

[0037] It should be pointed out that during the preparation process of the present application, the length of the isolation film 200 selected is smaller than the length of the glass substrate 10, and the length of the first PVB board 20 is larger than the length of the isolation film 200, so that after lamination and packaging fixation, a peel strength test opening in the form of a blind hole can be defined by the glass substrate 10, which is convenient for subsequent peel strength testing.

[0038] It is understandable that in the prior art, when conducting a peel strength test on a photovoltaic module that is encapsulated and laminated using a PVB board, it is necessary to use a whole photovoltaic module to conduct the peel strength test, which is costly. However, in the present application, a metal back plate 30 is used to fix the first PVB board 20 so that the deformation of the first PVB board 20 during the stretching process can be suppressed by the metal back plate 30, and a glass substrate 10 and a first PVB board 20 with a size smaller than the standard size can be selected to prepare a peel strength test sample 100. On the one hand, photovoltaic module processing manufacturers can conduct peel strength tests by themselves, which can reduce the cost and test cycle of glass strength tests; on the other hand, the first PVB board 20 is fixed by the metal back plate 30, and during the peel strength test, a micro material testing machine or a manual tensile instrument can be directly used for measurement, so that photovoltaic module processing manufacturers can optimize the lamination parameters in a timely manner and improve production efficiency.

[0039] It should be noted that, for photovoltaic modules encapsulated and laminated with PVB materials, when it is necessary to prepare peel strength test samples 100, a glass substrate 10 with the same structure as the photovoltaic module can be used. However, the size of the glass substrate 10 is smaller than that of the standard glass substrate 10. The size of the glass strength test sample is even smaller, and a micro material testing machine or a manual tensile instrument can be used for measurement. There is no need to use more dangerous experimental methods such as falling ball tests and shotgun tests, and the safety of peel strength tests can also be improved.

[0040] like Figure 1 , Figure 2 and Figure 3 As shown, according to some embodiments of the present application, the preparation method further includes: before lamination and fixing, stacking a second PVB board 40 on the metal backboard 30.

[0041] That is to say, a second PVB board 40 is further arranged above the metal backboard 30, and the first PVB board 20, the metal backboard 30 and the second PVB board 40 form a sandwich structure, which can further improve the structural strength of the peel strength test sample 100 and ensure that the peel strength data of the photovoltaic module can be accurately obtained.

[0042] According to the preparation method of the glass strength test sample of the embodiment of the present application, the second PVB board 40, the metal backboard 30 are packaged with the first PVB board 20, the isolation sheet 200 and the glass substrate. On the one hand, there is no need to use finished photovoltaic modules for peel strength testing, which can reduce the test cost and test cycle, and facilitate photovoltaic module manufacturers to adjust the lamination parameters in time to improve production efficiency and production utilization rate; on the other hand, photovoltaic modules encapsulated with PVB do not need to conduct falling ball tests or shotgun tests to obtain relevant data of the glass strength test, which can improve the experimental safety of the glass strength test.

[0043] It is understandable that when the existing photovoltaic modules using PVB encapsulation are subjected to conventional pulling means for peel strength testing, the encapsulation film is prone to tensile deformation, which affects the test accuracy, and the existing backplane material cannot be bonded to the first PVB board 20. The present application uses a metal backplane 30 to avoid tensile deformation of the encapsulation film during the pulling process to ensure the accuracy of the peel strength test. The size of the glass substrate 10 can be selected according to demand (for example: 10cm-20cm), and the length of the first PVB board 20 can be the same as or less than the length of the glass substrate 10.

[0044] like Figure 3 As shown, the length L1 of the spacer 200 and the length L2 of the glass substrate 10 satisfy: 0.4L2≤L1≤0.6L2. In this way, the length of the spacer 200 is more reasonable, and the accuracy of the peel strength test can be further improved.

[0045] It should be pointed out that in the process of using a micro material testing machine to perform a peel strength test, it is preferred to make L1=0.5L2. The peel strength test sample 100 can be folded over for peel strength testing. When a manual tensile instrument is used for testing, the proportional relationship of 0.4L2≤L1≤0.6L2 is satisfied, which can also improve the structural strength of the peel strength test sample 100.

[0046] like Figure 1 and Figure 2 As shown, the width of the spacer 200 is smaller than the width of the glass substrate 10, and the width of the spacer 200 is larger than the width of the first PVB board 20. In this way, the spacer 200 can be removed more simply and conveniently, and the end of the spacer 200 can be made to protrude from the end of the glass substrate 10, which can further reduce the difficulty of removing the spacer 200.

[0047] like Figure 3 As shown, the width of the metal back plate 30 is ≥ the width of the first PVB plate 20 , the length of the metal back plate 30 is < the length of the first PVB plate 20 , and the end of the metal back plate 30 away from the isolation sheet 200 is flush with the edge of the same side of the first PVB plate 20 .

[0048] In this way, a receiving groove can be defined between the first PVB board 20, the metal backboard 30 and the second PVB board 40. During the lamination process, at least part of the packaging glue can enter the receiving groove to further improve the structural strength of the peel strength test sample 100 and thereby improve the test accuracy of the peel strength test.

[0049] In some embodiments, the thickness of the metal back plate 30 is 0.1 mm-1.0 mm, and the metal back plate 30 is constructed as any one of a copper back plate, a tinned copper back plate, and an aluminum back plate. The metal back plate 30 made of the above materials can achieve stable fixation of the first PVB board 20 and the metal back plate 30.

[0050] It should be noted that the isolation sheet 200 can be made of polytetrafluoroethylene fiber material, PET (polyester resin) material, or other thin sheet materials that are not adhesive to the glass substrate 10 .

[0051] Preferably, the geometric dimensions of the second PVB board 40 are consistent with those of the first PVB board 20. This not only avoids crushing during the lamination process, but also makes the force distribution of the peel strength test specimen 100 more uniform, thereby improving the test accuracy of subsequent peel strength tests.

[0052] According to the peel strength test specimen 100 of the photovoltaic module according to the second aspect of the present application, the peel strength test specimen 100 is prepared based on the preparation method of the above embodiment, and the technical effect it has is consistent with the above preparation method, which will not be repeated here.

[0053] Next, the preparation process of the peel strength test sample 100 of the present application is described in detail by taking a peel strength test process of a specific peel strength test sample 100 .

[0054] A glass substrate 10 with a side length of 10 cm-20 cm is selected. The material of the glass substrate 10 is the same as the process, material and thickness of the glass used in photovoltaic modules. A spacer 200 made of polytetrafluoroethylene is stacked on the glass substrate 10. The length and width of the spacer 200 are both smaller than the glass substrate 10. A first PVB board 20 is stacked on the spacer 200. A metal backboard 30 (the width of the metal backboard 30 is about 10 mm-20 mm, and the metal backboard 30 is constructed as a tinned copper backboard) whose length is smaller than the first PVB board 20 is stacked on the first PVB board 20. A second PVB board 40 is stacked on the metal backboard 30.

[0055] Then, vacuum was applied for 6 minutes, lamination was performed for 6 minutes, and the lamination pressure was 1 atmosphere. Different temperatures were selected for lamination, and the peel strength at different temperatures was tested (see the table below).

[0056]

[0057] In summary, it can be seen from the above specific embodiments that by using the peel strength test sample 100 of the embodiment of the present application, the strength of the glass after lamination at different temperatures can be obtained, which is convenient for photovoltaic module manufacturers to perform peel strength tests, timely optimize lamination parameters, and improve production efficiency, yield rate and production utilization rate.

[0058] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0059] In the description of the present invention, "first feature" or "second feature" may include one or more of the features.

[0060] In the description of the present invention, "plurality" means two or more.

[0061] In the description of the present invention, a first feature being “on” or “under” a second feature may include that the first and second features are directly in contact with each other, or may include that the first and second features are not in direct contact with each other but are in contact with each other via another feature therebetween.

[0062] In the description of the present invention, “on”, “over” and “above” a first feature from a second feature includes the first feature being directly above and obliquely above the second feature, or simply means that the first feature is horizontally higher than the second feature.

[0063] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.

[0064] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.

Claims

1. A method for preparing a peel strength test sample (100) of a photovoltaic module, characterized in that: include: A glass substrate (10), a spacer (200), a first PVB plate (20), a metal back plate (30), and a second PVB plate (40) are stacked in sequence; wherein the length of the spacer (200) is less than the length of the glass substrate (10), and the length of the first PVB plate (20) is greater than the length of the spacer (200); Laminating and fixing, and extracting the isolation sheet (200) to obtain the peel strength preparation sample; The metal back plate (30) is constructed as any one of a copper back plate, a tinned copper back plate, and an aluminum back plate.

2. The method for preparing the photovoltaic module peel strength test sample (100) according to claim 1, characterized in that: The length L1 of the isolation plate (200) and the length L2 of the glass substrate (10) satisfy the following relationship: 0.4L2≤L1≤0.6L2.

3. The method for preparing the photovoltaic module peel strength test sample (100) according to claim 1, characterized in that: The width of the isolation sheet (200) is smaller than the width of the glass substrate (10), and the width of the isolation sheet (200) is larger than the width of the first PVB plate (20).

4. The method for preparing the photovoltaic module peel strength test sample (100) according to claim 1, characterized in that: The width of the metal back plate (30) is greater than or equal to the width of the first PVB plate (20).

5. The method for preparing the photovoltaic module peel strength test sample (100) according to claim 4, characterized in that: The length of the metal back plate (30) is less than the length of the first PVB plate (20), and one end of the metal back plate (30) away from the isolation plate (200) is flush with an edge of one end on the same side of the first PVB plate (20).

6. A method for preparing a photovoltaic module peel strength test sample (100) according to any one of claims 1 to 5, characterized in that: The thickness of the metal back plate (30) is 0.1 mm-1.0 mm.

7. The method for preparing a photovoltaic module peel strength test sample (100) according to any one of claims 1 to 5, characterized in that: The geometric dimensions of the second PVB board (40) are consistent with the geometric dimensions of the first PVB board (20).

8. A photovoltaic module peel strength test specimen (100), characterized in that: The peel strength test specimen (100) is prepared based on the preparation method described in any one of claims 1 to 7.