A preparation method of 2,2,4,4-tetramethyl-1,3-cyclobutanediamine
By performing a hydroxyl amination reaction between 2,2,4,4-tetramethyl-1,3-cyclobutanediol and ammonia in the presence of a catalyst and hydrogen, the lack of 2,2,4 in the existing technology is solved. , the problem of the synthesis method of 4-tetramethyl-1,3-cyclobutanediamine achieves efficient and low-cost preparation and is suitable for industrial applications.
Patent Information
- Application Number
- CN202210043340.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-01-14
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2042-01-14
AI Technical Summary
The existing technology lacks a synthesis method of 2,2,4,4-tetramethyl-1,3-cyclobutanediamine, which limits its widespread use in industrial applications.
2,2,4,4-tetramethyl is prepared by selecting 2,2,4,4-tetramethyl-1,3-cyclobutanediol and ammonia for hydroxyl amination in the presence of a catalyst and hydrogen. Based on 1,3-cyclobutanediamine, supported catalysts and specific reaction conditions are used to increase yields and reduce costs.
The efficient preparation of 2,2,4,4-tetramethyl-1,3-cyclobutanediamine is achieved, with a yield of more than 99%. The process is simple, the production cost is reduced, and it is suitable for large-scale industrial production.
Smart Images

Figure BDA0003471170020000021 
Figure BDA0003471170020000031 
Figure BDA0003471170020000071
Abstract
Description
Technical Field
[0001] The invention relates to the field of chemical synthesis, and specifically to obtaining 2,2,4,4-tetramethyl-1,3-cyclobutanediamine by reacting 2,2,4,4-tetramethyl-1,3-cyclobutanediol with ammonia. Background Art
[0002] 2,2,4,4-Tetramethyl-1,3-cyclobutanediamine is an important chemical raw material with a wide range of uses in many fields. For example, it can be used as an epoxy resin curing agent in coatings; as a chelating agent in the textile industry and water treatment; or as a monomer to produce polyamide, polyurethane, etc.
[0003] There is no relevant report on the synthesis method of 2,2,4,4-tetramethyl-1,3-cyclobutanediamine.
[0004] Among them, 2,2,4,4-tetramethyl-1,3-cyclobutanediol can be prepared by a one-step hydrogenation reaction of 2,2,4,4-tetramethyl-1,3-cyclobutanedione and hydrogen. Lou Yang et al. used 2,2,4,4-tetramethyl-1,3-cyclobutanedione as raw material and Cu-ZnO-Al 2 O 3 As catalyst, at 180℃, reaction pressure 4MPa, mass space velocity of 2,2,4,4-tetramethyl-1,3-cyclobutanedione 4h -1 , the yield of 2,2,4,4-tetramethyl-1,3-cyclobutanediol reached 91.8% (Petrochemical Technology and Application, 2015, 33, 405-407). Our research group proposed to use nitric acid-modified Ru / C catalyst to catalyze the reaction of 2,2,4,4-tetramethyl-1,3-cyclobutanedione with hydrogen to prepare 2,2,4,4-tetramethyl-1,3-cyclobutanediol, and the yield of the product can reach more than 99% (Catalysis Communications, 2015, 72, 20-23).
[0005] Therefore, if a method for preparing 2,2,4,4-tetramethyl-1,3-cyclobutanediamine using 2,2,4,4-tetramethyl-1,3-cyclobutanediol can be developed, it will have important industrial application significance. Summary of the invention
[0006] In view of the problems existing in the prior art, the purpose of the present invention is to select 2,2,4,4-tetramethyl-1,3-cyclobutanediol as a raw material, and prepare 2,2,4,4-tetramethyl-1,3-cyclobutanediamine through an amination reaction in the presence of a catalyst and hydrogen, thereby providing a low-cost preparation method.
[0007] In order to achieve the above object, the technical solution adopted by the present invention is:
[0008] Under the action of a supported catalyst, the reaction substrate 2,2,4,4-tetramethyl-1,3-cyclobutanediol undergoes a hydroxylation reaction in a solvent in an atmosphere of pressurized hydrogen and pressurized ammonia to obtain the 2,2,4,4-tetramethyl-1,3-cyclobutanediamine. The reaction process is shown below:
[0009]
[0010] More specifically, the preparation method of the 2,2,4,4-tetramethyl-1,3-cyclobutanediamine according to the present invention comprises the following steps:
[0011] 1) adding the reaction substrate 2,2,4,4-tetramethyl-1,3-cyclobutanediol to the solvent in the reaction kettle until the concentration of the 2,2,4,4-tetramethyl-1,3-cyclobutanediol is 1wt% to 50wt%, and then adding a catalyst, wherein the mass ratio of the catalyst to the 2,2,4,4-tetramethyl-1,3-cyclobutanediol is 0.1 to 4;
[0012] 2) After hydrogen replaces the air in the kettle, 0.1 to 10 MPa of ammonia is charged under continuous stirring. After stirring and dissolving for 0.1 to 2 hours, hydrogen with a partial pressure 0.3 to 3 MPa higher than that of ammonia is charged. After reacting at 180-270°C for 1 to 24 hours, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine can be generated.
[0013] The solvent is selected from one or more of water, methanol, ethanol, propanol, butanol, isopropanol, tert-butanol, acetone, tetrahydrofuran, ethyl acetate, 1,4-dioxane, dichloromethane, chloroform, methyl acetate, 1,3-dioxane, and p-xylene.
[0014] The concentration of the reaction substrate 2,2,4,4-tetramethyl-1,3-cyclobutanediol is 1 wt% to 50 wt%, preferably 1 wt%, 2 wt%, 10 wt%, 15 wt%, 20 wt%, 35 wt% or 50 wt%.
[0015] The supported catalyst is selected from, but not limited to, one or more of Raney Ni, Raney Cu, Raney Co and supported catalysts, the active metal in the supported catalyst is selected from one or more of Pd, Ru, Ir, Pt, Ni, Co, Cu, Ag and Au, and the carrier in the supported catalyst is selected from Al 2 O 3 、SiO 2 、ZrO 2 , activated carbon, TiO 2 、MgO、CeO 2 and SnO 2One or more of; the supported catalyst is further preferably 30% Ni-Al 2 O 3 , 25%Ni-15%Cu-Al 2 O 3 、20%Ni-10%Co-Al 2 O 3 、30%Ni-20%ZnO-Al 2 O 3 , 25%Co-5%Fe-Al 2 O 3 、3%Ru-Al 2 O 3 ,5%Ru-C,2%Pd-1%Ru-TiO 2 、3%Rh-TiO 2 、15%Ni-15%Co-Al 2 O 3 , Raney Ni, Raney Cu, Raney Co, 2%Ru-3%Ni / Al 2 O 3 3%Ru-3%Cu / SiO 2 , 20%Ni-10%Cr / TiO 2 、10%Co-10%Cr / SiO 2 , 2%Pt-3%Ni / Al 2 O 3 , 2%Rd-3%Co / Al 2 O 3 or 2%Pt-2%Cu / Al 2 O 3 .
[0016] The preparation method of the supported catalyst includes, but is not limited to, coprecipitation, impregnation, deposition precipitation, sol-gel, microemulsion, etc. In the impregnation method, a metal salt precursor solution is impregnated on the surface of the carrier, wherein the metal salt precursor includes one or a mixture of two or more of acetylacetonate, chloride, nitrate, and ammonium salt. In the precipitation deposition method or coprecipitation method, a metal salt solution and a precipitant are fed in parallel, wherein the metal salt is one or a mixture of two or more of nitrate, chloride, nitrate, acetate, and acetylacetonate, and the precipitant is Na 2 CO 3 、NaHCO 3 、NaOH、(NH4) 2 CO 3 NH 4 HCO 3 One or a mixture of two or more.
[0017] The mass ratio of the catalyst to 2,2,4,4-tetramethyl-1,3-cyclobutanediol is 0.1 to 4, preferably 0.1 to 3; the reaction temperature is 180-270°C, preferably 200°C to 250°C; the reaction time is 1 to 24 hours, preferably 3 to 24 hours, more preferably 4 to 15 hours, and most preferably 6 hours.
[0018] Compared with the prior art, the beneficial effects of the present invention are as follows:
[0019] The preparation method of the invention adopts a one-step method to prepare 2,2,4,4-tetramethyl-1,3-cyclobutanediamine, has a simple process, adopts easily available and inexpensive 2,2,4,4-tetramethyl-1,3-cyclobutanediol as a raw material, effectively reduces the production cost, and is conducive to large-scale industrial production. DETAILED DESCRIPTION
[0020] In the preparation method of 2,2,4,4-tetramethyl-1,3-cyclobutanediamine according to the present invention, the reaction mechanism is as follows:
[0021]
[0022] In the presence of a catalyst, one of the hydroxyl groups of 2,2,4,4-tetramethyl-1,3-cyclobutanediol is dehydrogenated to a carbonyl group, which then reacts with ammonia to obtain an imine. The imine is then hydrogenated to generate 2,2,4,4-tetramethyl-3-amino-cyclobutanol under the action of a catalyst, which is then further dehydrogenated, aminated and hydrogenated to generate 2,2,4,4-tetramethyl-1,3-cyclobutanediamine. The reaction needs to be carried out in a hydrogen atmosphere. Although the total amount of hydrogen remains unchanged during the reaction, hydrogen participates in the hydrogenation reaction of the imine. If hydrogen is not added during the reaction, the hydrogenation reaction of the imine is difficult to proceed, and even cannot be completed under conditions such as lower temperatures. Therefore, the presence of hydrogen is essential.
[0023] The catalyst used in the preparation method of 2,2,4,4-tetramethyl-1,3-cyclobutanediamine of the present invention is not particularly limited, as long as it can promote the reaction of the present invention and does not cause adverse effects on the reaction yield, purification, etc. Commercially available catalyst products such as Raney Ni, Raney Cu, Raney Co, etc. can be used, and supported catalysts commonly used in the field of 2,2,4,4-tetramethyl-1,3-cyclobutanediamine synthesis can also be used. The supported catalyst can be prepared according to the method described in the prior art, such as the Co-Fe / Al described in Chemical Progress. 2 O 3 、Ni / Al 2 O 3 、Ni-Fe / Al 2 O3 The preparation method of the catalyst includes coprecipitation method, impregnation method, deposition precipitation method, sol-gel method, microemulsion method, etc. Preferably, the catalyst used in the preparation method of 2,2,4,4-tetramethyl-1,3-cyclobutanediamine according to the present invention is selected from, but not limited to, one or more of Raney Ni, Raney Cu, Raney Co and supported catalysts, the active metal in the supported catalyst is selected from one or more of Pd, Ru, Ir, Pt, Ni, Co, Cu, Ag and Fe, and the carrier in the supported catalyst is selected from Al 2 O 3 、SiO 2 、ZrO 2 , activated carbon, TiO 2 、MgO、CeO 2 and SnO 2 One or more of .
[0024] The mass ratio of the catalyst to 2,2,4,4-tetramethyl-1,3-cyclobutanediol is 0.05 to 4. If the mass ratio is less than 0.05, the reaction rate is low; if the mass ratio is greater than 4, that is, the catalyst is excessive, it is difficult to control the reaction degree and be economical.
[0025] The reaction temperature is 180-270° C. If the reaction temperature is too low, it is not conducive to the smooth progress of the reaction. If the reaction temperature is too high, due to the presence of hydrogen, the requirements for the reactor are very high, which is not conducive to safe operation.
[0026] The following examples are merely listed as examples of embodiments of the present invention and do not constitute any limitation to the present invention. Those skilled in the art will appreciate that modifications within the scope of the spirit and concept of the present invention fall within the protection scope of the present invention.
[0027] Example 1
[0028] In a 100 ml reactor, 0.6 g of the reaction substrate 2,2,4,4-tetramethyl-1,3-cyclobutanediol was added to 30 mL of tert-butyl alcohol solvent. The concentration of 2,2,4,4-tetramethyl-1,3-cyclobutanediol was about 2 wt%. 0.1 g of the supported catalyst 30% Ni / Al was added under stirring. 2 O 3 (Ni content 30wt%), stirred for about 1 hour. Then, after hydrogen replaced the air in the kettle, 0.5MPa of ammonia was filled in under continuous stirring, stirred and dissolved for 1 hour, and then 1.0MPa of hydrogen was filled in, and the reaction was carried out at 240°C for 5 hours. After the reaction was completed, the liquid product was obtained by centrifugation, and the product composition was analyzed by gas chromatography. The experimental results are shown in Table 1. The supported catalyst of this embodiment was prepared by coprecipitation method, using nickel nitrate and (NH4 ) 2 CO 3 The solution is fed in parallel with Al 2 O 3 The mixture is mixed, and then filtered, dried, calcined and reduced to obtain the product.
[0029] Example 2
[0030] The reaction temperature was raised to 250° C., and the other conditions remained unchanged. 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as in Example 1. The experimental results are shown in Table 1.
[0031] Example 3
[0032] The reaction temperature was raised to 260° C., and the other conditions remained unchanged. 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as in Example 1. The experimental results are shown in Table 1.
[0033] Example 4
[0034] The reaction temperature was raised to 270° C., and the other conditions remained unchanged. 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as in Example 1. The experimental results are shown in Table 1.
[0035] Example 5
[0036] Except that tetrahydrofuran was used to replace tert-butyl alcohol, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 1. The experimental results are shown in Table 1.
[0037] Example 6
[0038] 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 1 except that 1,4-dioxane was used to replace tert-butyl alcohol. The experimental results are shown in Table 1.
[0039] Example 7
[0040] Except that tert-butyl alcohol was replaced by ethanol, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 1. The experimental results are shown in Table 1.
[0041] Example 8
[0042] Except that acetonitrile was used to replace tert-butyl alcohol, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 1. The experimental results are shown in Table 1.
[0043] Example 9
[0044] 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 1 except that p-xylene was used to replace tert-butyl alcohol. The experimental results are shown in Table 1.
[0045] Example 10
[0046] 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as in Example 1 except that the partial pressure of ammonia was adjusted to 0.2 MPa. The experimental results are shown in Table 1.
[0047] Embodiment 11
[0048] In addition to adjusting the partial pressure of ammonia to 1.0 MPa and replacing the catalyst with 25% Ni-15% Cu-Al 2 O 3 In addition, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as in Example 1. The experimental results are shown in Table 1.
[0049] Example 12
[0050] In addition to adjusting the partial pressure of ammonia to 1.5 MPa, the partial pressure of hydrogen was changed to 2.0 MPa and the catalyst was replaced with 20% Ni-10% Co-Al 2 O 3 In addition, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as in Example 1. The experimental results are shown in Table 1.
[0051] Embodiment 13
[0052] In a 200 ml reactor, 8 g of the reaction substrate 2,2,4,4-tetramethyl-1,3-cyclobutanediol was added to 80 g of tert-butyl alcohol solvent. The concentration of 2,2,4,4-tetramethyl-1,3-cyclobutanediol was about 10 wt %. 4 g of the supported catalyst 30% Ni-20% ZnO-Al was added under stirring. 2 O 3 , stirring for about 0.5 hours. Then, after hydrogen replaced the air in the kettle, 0.6MPa of ammonia was charged under continuous stirring, and after stirring and dissolving for 1 hour, 1.5MPa of hydrogen was charged, and the reaction was carried out at 260°C for 8 hours. The product was analyzed by gas chromatography, and the conversion rate of 2,2,4,4-tetramethyl-1,3-cyclobutanediol was 79.5%, and the selectivity of the product was 85.4%. The supported catalyst of this embodiment was prepared by coprecipitation method, using nickel nitrate, zinc chloride and (NH 4 ) 2 CO 3 The solution is fed in parallel with Al 2 O 3 The mixture is mixed, and then filtered, dried, calcined and reduced to obtain the product.
[0053] Embodiment 14
[0054] In addition to changing the reaction temperature to 250 °C and replacing the catalyst with 25% Co-5% Fe-Al 2 O 3 In addition, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 13. The experimental results are shown in Table 1.
[0055] Embodiment 15
[0056] In addition to replacing tert-butyl alcohol with 1,4-dioxane solvent, the reaction temperature was changed to 270 °C and the catalyst was replaced with 3% Ru-Al 2 O 3 In addition, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 13. The experimental results are shown in Table 1.
[0057] Example 16
[0058] 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 13, except that 1,4-dioxane solvent was used to replace tert-butanol, the reaction temperature was changed to 270°C, and the catalyst was replaced with 5% Ru-C. The experimental results are shown in Table 1.
[0059] Embodiment 17
[0060] Except that tert-butyl alcohol was replaced by tetrahydrofuran and the catalyst was changed to 2% Pd-1% Ru-TiO 2 In addition, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 13. The experimental results are shown in Table 1.
[0061] Embodiment 18
[0062] In addition to replacing tert-butyl alcohol with 1,4-dioxane, the reaction temperature was changed to 280 °C and the catalyst was changed to 3% Rh-TiO 2 In addition, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 13. The experimental results are shown in Table 1.
[0063] Table 1 Catalyst evaluation results
[0064]
[0065] Embodiment 19
[0066] In a 200 ml reactor, 10 g of the reaction substrate 2,2,4,4-tetramethyl-1,3-cyclobutanediol was added to 90 g of tetrahydrofuran solvent. The concentration of 2,2,4,4-tetramethyl-1,3-cyclobutanediol was about 10 wt%. 10 g of the supported catalyst 15% Ni-15% Co / Al was added under stirring. 2 O 3 , stirring for about 1 hour. Then, after hydrogen replaced the air in the kettle, 0.8MPa of ammonia was charged under continuous stirring. After stirring and dissolving for 1 hour, 1.6MPa of hydrogen was charged and reacted at 250°C for 7 hours. The experimental results are shown in Table 2. The supported catalyst of this embodiment was prepared by coprecipitation method, using nickel nitrate, cobalt chloride and (NH 4 ) 2 CO 3 The solution is fed in parallel with Al 2 O 3 The mixture is mixed, and then filtered, dried, calcined and reduced to obtain the product.
[0067] Embodiment 20
[0068] 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 19, except that p-xylene was used to replace tetrahydrofuran. The experimental results are shown in Table 2.
[0069] Embodiment 21
[0070] Except that tetrahydrofuran was replaced by butanol, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 19. The experimental results are shown in Table 2.
[0071] Embodiment 22
[0072] 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 19, except that tetrahydrofuran was replaced by isopropanol and the hydrogen pressure was changed to 3.0 MPa. The experimental results are shown in Table 2.
[0073] Embodiment 23
[0074] 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 19, except that dichloromethane was used to replace tetrahydrofuran and the ammonia pressure was changed to 3.0 MPa. The experimental results are shown in Table 2.
[0075] Embodiment 24
[0076] 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 19, except that chloroform was used to replace tetrahydrofuran and the temperature was changed to 260° C. The experimental results are shown in Table 2.
[0077] Embodiment 25
[0078] 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 19, except that methyl acetate was used to replace tetrahydrofuran and the temperature was changed to 230° C. The experimental results are shown in Table 2.
[0079] Embodiment 26
[0080] 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 19, except that 1,3-dioxane was used to replace tetrahydrofuran, the hydrogen pressure was changed to 0.8 MPa, and the ammonia pressure was changed to 1.6 MPa. The experimental results are shown in Table 2.
[0081] Embodiment 27
[0082] 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 19, except that methyl formate was used instead of tetrahydrofuran. The experimental results are shown in Table 2.
[0083] Embodiment 28
[0084] 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 19, except that tetrahydrofuran was replaced by aqueous ammonia. The experimental results are shown in Table 2.
[0085] Embodiment 29
[0086] In a 200ml reactor, 16g of the reaction substrate 2,2,4,4-tetramethyl-1,3-cyclobutanediol was added to 84g of 1,4-dioxane, and the concentration of 2,2,4,4-tetramethyl-1,3-cyclobutanediol was about 16wt%. 48g of catalyst RaneyNi was added under stirring and stirred for about 1 hour. Then, after hydrogen replaced the air in the reactor, 1.0MPa of ammonia was filled in under continuous stirring. After stirring and dissolving for 1 hour, 1.5MPa of hydrogen was filled in, and the reaction was carried out at 240°C for 10 hours. The experimental results are shown in Table 2.
[0087] Embodiment 30
[0088] Except for replacing Raney Ni with Raney Cu, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 29. The experimental results are shown in Table 2.
[0089] Embodiment 31
[0090] Except for replacing Raney Ni with Raney Co, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 29. The experimental results are shown in Table 2.
[0091] Embodiment 32
[0092] In a 200 ml reactor, 10 g of the reaction substrate 2,2,4,4-tetramethyl-1,3-cyclobutanediol was added to 90 g of ethyl acetate. The concentration of 2,2,4,4-tetramethyl-1,3-cyclobutanediol was about 10 wt%. 40 g of supported 2% Ru-3% Ni / Al was added under stirring. 2 O 3 The catalyst was stirred for about 1 hour. Then, after hydrogen replaced the air in the kettle, 0.4MPa of ammonia was charged under continuous stirring. After stirring and dissolving for 1 hour, 2.0MPa of hydrogen was charged and reacted at 230°C for 24 hours. The experimental results are shown in Table 2. The supported catalyst of this embodiment was prepared by coprecipitation method, using nickel nitrate, ruthenium chloride and (NH 4 ) 2 CO 3 The solution is fed in parallel with Al 2 O 3 The mixture is mixed, and then filtered, dried, calcined and reduced to obtain the product.
[0093] Embodiment 33
[0094] In addition to using 3%Ru-3%Cu / SiO 2 Replacement of 2%Ru-3%Ni / Al 2 O 3 Except for the active metal as the supported catalyst, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 32. The experimental results are shown in Table 2.
[0095] Embodiment 34
[0096] In addition to using 20% Ni-10% Cr / TiO 2 Replacement of 2%Ru-3%Ni / Al 2 O 3 Except for the active metal as the supported catalyst, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 32. The experimental results are shown in Table 2.
[0097] Embodiment 35
[0098] In addition to using 10%Co-10%Cr / SiO 2 Except for replacing 2%Ru-3%Ni / Al2O3 as the active metal of the supported catalyst, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 32. The experimental results are shown in Table 2.
[0099] Embodiment 36
[0100] In addition to using 2% Pt-3% Ni / Al 2 O 3 Replacement of 2%Ru-3%Ni / Al 2 O 3 Except for the active metal as the supported catalyst, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 32. The experimental results are shown in Table 2.
[0101] Embodiment 37
[0102] In addition to using 2% Rd-3% Co / Al 2 O 3 Replacement of 2%Ru-3%Ni / Al 2 O 3 Except for the active metal as the supported catalyst, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 32. The experimental results are shown in Table 2.
[0103] Embodiment 38
[0104] In addition to using 2% Pt-2% Cu / Al 2 O 3 Replacement of 2%Ru-3%Ni / Al 2 O 3 Except for the active metal as the supported catalyst, 2,2,4,4-tetramethyl-1,3-cyclobutanediamine was prepared in the same manner as Example 32. The experimental results are shown in Table 2.
[0105] Table 2 Catalyst evaluation results
[0106]
[0107]
Claims
1. A method for preparing 2,2,4,4-tetramethyl-1,3-cyclobutanediamine, characterized in that: The steps include: Under the action of a supported catalyst, a reaction substrate 2,2,4,4-tetramethyl-1,3-cyclobutanediol is subjected to a hydroxylation reaction in a solvent in an atmosphere of pressurized hydrogen and pressurized ammonia to obtain a solution rich in 2,2,4,4-tetramethyl-1,3-cyclobutanediamine, and then a 2,2,4,4-tetramethyl-1,3-cyclobutanediamine product is obtained by further separation of the catalyst, concentration crystallization, and solid-liquid separation; The solvent is selected from one or more of ammonia, water, methanol, ethanol, propanol, butanol, isopropanol, tert-butanol, acetone, tetrahydrofuran, ethyl acetate, 1,4-dioxane, dichloromethane, chloroform, methyl acetate, 1,3-dioxane, and p-xylene; The supported catalyst is selected from 30%Ni-Al2O3, 25%Ni-15%Cu-Al2O3, 20%Ni-10%Co-Al2O3, 30%Ni-20%ZnO-Al2O3, 25% Co-5%Fe-Al2O3, 3%Ru-Al2O3, 5%Ru-C, 2%Pd-1%Ru-TiO2, 3%Rh-TiO2, 15%Ni-15%Co-Al2O3, Raney Ni, Raney Cu, Raney Co, 2%Ru-3%Ni / Al2O3, 3%Ru-3%Cu / SiO2, 20%Ni-10%Cr / TiO2, 10%Co-10%Cr / SiO2, 2%Pt-3%Ni / Al2O3, 2%Rd-3%Co / Al2O3 or 2%Pt-2%Cu / Al2O3.
2. The method for preparing 2,2,4,4-tetramethyl-1,3-cyclobutanediamine according to claim 1, characterized in that: The concentration of the reaction substrate 2,2,4,4-tetramethyl-1,3-cyclobutanediol in the reaction solution is 1 wt % to 50 wt %.
3. The method for preparing 2,2,4,4-tetramethyl-1,3-cyclobutanediamine according to claim 2, characterized in that: The concentration of the reaction substrate 2,2,4,4-tetramethyl-1,3-cyclobutanediol in the reaction solution is 1wt%, 2wt%, 10wt%, 15wt%, 20wt%, 35wt% or 50wt%.
4. The method for preparing 2,2,4,4-tetramethyl-1,3-cyclobutanediamine according to claim 1, characterized in that: The mass ratio of the supported catalyst to 2,2,4,4-tetramethyl-1,3-cyclobutanediol is 0.05-4.
5. The method for preparing 2,2,4,4-tetramethyl-1,3-cyclobutanediamine according to claim 4, characterized in that: The supported catalyst is prepared by an impregnation method, a precipitation deposition method or a co-precipitation method; In the impregnation method, a metal salt precursor solution is impregnated on the surface of the carrier, wherein the metal salt precursor is one of acetylacetonate, chloride, nitrate, and ammonium salt, or a mixture of two or more thereof; In the precipitation deposition method or co-precipitation method, the metal salt solution and the precipitant are precipitated by parallel feeding, the metal salt is one or a mixture of two or more of nitrate, chloride, nitrate, acetate, acetylacetonate, and the precipitant is one or a mixture of two or more of Na2CO3, NaHCO3, NaOH, (NH4)2CO3, NH4HCO3.
6. The method for preparing 2,2,4,4-tetramethyl-1,3-cyclobutanediamine according to claim 1, characterized in that: The reaction temperature is 180-270°C, and the reaction time is 1 to 24 hours.
7. The method for preparing 2,2,4,4-tetramethyl-1,3-cyclobutanediamine according to claim 6, characterized in that: The reaction temperature is 200° C. to 250° C., and the reaction time is 3 to 24 hours.
8. The method for preparing 2,2,4,4-tetramethyl-1,3-cyclobutanediamine according to claim 1, characterized in that: The method comprises the following steps: adding a reaction substrate 2,2,4,4-tetramethyl-1,3-cyclobutanediol into a tert-butyl alcohol solvent in a reaction kettle, adding a supported catalyst 25% Ni-15% Cu-Al2O3 with stirring, and stirring for 0.5-1.5 hours; then replacing the air in the kettle with hydrogen, and then charging 0.8-1.0 MPa of ammonia under the condition of continuous stirring; after stirring and dissolving, charging 0.8-1.0 MPa of hydrogen, and reacting at 230-260° C.; after the reaction is completed, further obtaining a 2,2,4,4-tetramethyl-1,3-cyclobutanediamine product through catalyst separation, concentrated crystallization, and solid-liquid separation.
Citation Information
Patent Citations
Preparation method of 1,2-cyclohexylenediamine
CN105237407A
Novel cyp17 inhibitors / antiandrogens
CN105339355A
2, 2, 4, 4-tetramethylcyclobutyl compounds
US3287390A