- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-12-28
AI Technical Summary
The debonding method in the prior art is time-consuming and difficult to clean, especially for brittle and cantilever beam ultra-thin devices and optical devices with high cleanliness requirements, resulting in a decrease in yield.
Through holes are formed in the wafer preset area of the slide structure, and the slide structure is inverted onto the support, soaked in the debonding solution to stir to dissolve the bonding glue, speed up the dissolution rate through the through holes and prevent the deposition of glue particles.
It improves the dissolution speed of bonding glue and the cleanliness of wafer surface, and is suitable for brittle and cantilever beam devices, improving yield.
Smart Images

Figure CN114455539B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of micro-nano processing technology, and in particular to a debonding method for a temporarily bonded carrier structure. Background Art
[0002] With the development of micro-nano processing technology, the integration and performance of various devices are becoming increasingly higher. Therefore, in order to meet the requirements of miniaturization of these devices, wafers and wafers or chips and wafers are usually stacked layer by layer to improve the integration of chips or corresponding electronic devices. Generally, the device needs to be thinned, but the ultra-thin wafers are flexible and fragile, prone to warping and undulation, which makes subsequent process operations inconvenient. The device wafer needs to be bonded to a thicker carrier with a temporary bonding material first. The carrier is used to support and transfer the thin wafer and prevent deformation of the thin wafer. After the back-side process of the wafer is completed, the carrier is separated from the thin wafer.
[0003] The current debonding method typically involves directly immersing the entire bonded wafer in a chemical. Due to the tight bond between the carrier and the wafer, the chemical solution has difficulty penetrating, resulting in a long debonding time. Furthermore, solid adhesive residue often remains on the wafer surface after debonding, making it difficult to clean. This chemical immersion process is not suitable for some fragile and ultra-thin cantilever-type devices. This is especially true for optical devices with high cleanliness requirements, as this step results in a significant loss of good parts, resulting in a reduced yield. Summary of the Invention
[0004] In view of the deficiencies in the prior art, the present invention provides a method for debonding a temporarily bonded slide structure, the debonding method comprising:
[0005] forming a through hole in a predetermined area of the wafer of the carrier structure;
[0006] placing the slide structure upside down on a support member, so that a contact area between the support member and the slide structure is located within the through hole, and the contact area is smaller than an area of the through hole;
[0007] The wafer carrier structure and the support member are immersed in a debonding solution, and the debonding solution is stirred to dissolve the temporary bonding glue between the wafer of the wafer carrier structure and the wafer carrier.
[0008] Preferably, the method of immersing the carrier structure and the support in a debonding solution and stirring the debonding solution comprises:
[0009] Place a magnetic stirring bar in the stirring tank;
[0010] Covering the magnetic stirring bar with a first cleaning basket;
[0011] placing the slide structure and the support member on the first cleaning basket;
[0012] using a second cleaning basket to cover the slide structure and the support member;
[0013] Pour the debonding solution into the stirring tank, so that the slide structure and the support are immersed in the debonding solution;
[0014] The stirring cylinder is placed on a magnetic stirrer, and the magnetic stirrer provides a rotational driving force to the magnetic stirrer.
[0015] Preferably, the support member comprises a support plate and a positioning column provided on the support plate, and a radial cross-sectional area of the positioning column is smaller than an area of the through hole.
[0016] Preferably, the carrier is one of a silicon substrate, a glass substrate, and an SOI substrate.
[0017] Preferably, the temperature of the debonding solution is greater than 50°C.
[0018] Preferably, the rotation rate of the magnetic stirrer is greater than 80 rad / s.
[0019] Preferably, the first cleaning flower basket and the second cleaning flower basket are made of polytetrafluoroethylene.
[0020] Preferably, the stirring tank is made of quartz.
[0021] Compared to the prior art, the debonding method for a temporarily bonded carrier structure provided by the present invention forms through-holes in a predetermined area of the carrier wafer to increase the contact area between the bonding adhesive and the debonding solution, thereby allowing the debonding solution to easily infiltrate the bonding adhesive and increasing the speed of dissolving the bonding adhesive. Furthermore, during the debonding process, the support member passes through the through-holes in the wafer to form the entire carrier structure. Therefore, after the wafer and carrier are separated, the wafer may fall onto the support member while the carrier continues to be supported by the support member, thereby accelerating the dissolution rate of the remaining bonding adhesive.
[0022] In addition, by stirring the debonding solution to accelerate the dissolution rate of the bonding glue, the flow of the debonding solution prevents the bonding glue particles from being deposited on the wafer surface, thereby improving the cleanliness of the wafer surface and facilitating subsequent processes. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 is a flow chart of a debonding method of a temporarily bonded slide structure according to an embodiment of the present invention;
[0024] Figure 22 is a schematic diagram of the operation of a debonding method of a temporarily bonded wafer structure according to an embodiment of the present invention. DETAILED DESCRIPTION
[0025] To make the objectives, technical solutions, and advantages of the present invention more apparent, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings. Examples of these preferred embodiments are illustrated in the accompanying drawings. The embodiments of the present invention shown in and described with reference to the accompanying drawings are merely exemplary, and the present invention is not limited to these embodiments.
[0026] It should also be noted that, in order to avoid obscuring the present invention due to unnecessary details, the accompanying drawings only show structures and / or processing steps closely related to the solutions according to the present invention, while other details that are not closely related to the present invention are omitted.
[0027] In response to the existing technical problems in the background technology, this embodiment provides the following specific solutions.
[0028] like Figure 1 As shown, this embodiment provides a method for debonding a temporarily bonded carrier structure, the debonding method comprising:
[0029] Step S1: forming a through hole in a preset area of a wafer of a carrier structure.
[0030] Step S2: Place the wafer carrier structure upside down on a support member so that a contact area between the support member and the wafer carrier structure is located within the through hole, and the contact area is smaller than an area of the through hole.
[0031] Step S3: immersing the wafer carrier structure and the support member in a debonding solution, and stirring the debonding solution to dissolve the temporary bonding glue between the wafer of the wafer carrier structure and the wafer carrier.
[0032] Compared with the prior art, the debonding method of the temporarily bonded carrier structure of the present embodiment forms a through hole on a preset area of the wafer of the carrier structure, thereby increasing the contact area between the bonding glue and the debonding solution, so that the debonding solution can easily infiltrate the bonding glue, thereby improving the speed of dissolving the bonding glue. Moreover, during the debonding process, the support member is made into the entire carrier structure through the through hole on the wafer. Therefore, after the wafer and the carrier are separated, the wafer may fall on the support member, and the carrier continues to be supported by the support member, thereby accelerating the dissolution rate of the remaining bonding glue. Not only that, while accelerating the dissolution rate of the bonding glue by stirring the debonding solution, the flow of the debonding solution prevents the bonding glue particles from being deposited on the wafer surface, thereby improving the cleanliness of the wafer surface, so as to facilitate the subsequent process.
[0033] Preferably, combined Figure 2As shown, in this embodiment, the method of immersing the carrier structure A and the support member B in a debonding solution and stirring the debonding solution includes:
[0034] Step S31 , placing a magnetic stirring bar 2 in a stirring tank 1 ; wherein the stirring tank 1 is made of quartz.
[0035] Step S32: Use a first cleaning basket 3 (multiple through holes are not shown in the figure) to cover the magnetic stirring bar 2; wherein the first cleaning basket 3 is made of polytetrafluoroethylene.
[0036] Step S33 : placing the slide structure A and the support member B on the first cleaning basket 3 .
[0037] Step S34: Use a second cleaning basket 4 (multiple through holes not shown in the figure) to cover the wafer carrier structure A and the support member B; wherein the second cleaning basket 4 is made of polytetrafluoroethylene.
[0038] Step S35 , pouring the debonding solution (not shown) into the stirring tank 1 , immersing the carrier structure A and the support member B in the debonding solution; wherein the temperature of the debonding solution is greater than 50° C.
[0039] Step S36: placing the stirring cylinder 1 on a magnetic stirrer (not shown in the figure), and providing a rotational driving force to the magnetic stirrer 2 through the magnetic stirrer; wherein the rotation rate of the magnetic stirrer 2 is greater than 80 rad / s.
[0040] Specifically, the support member B of this embodiment includes a support plate B1 and positioning posts B2 disposed on the support plate B1. When the wafer carrier structure A is inverted on the support member B, the positioning posts B2 are located within the through-hole a of the wafer A1. The radial cross-sectional area of the positioning posts B2 is smaller than the area of the through-hole a. The wafer carrier A2 of the wafer carrier structure A is preferably a silicon substrate, a glass substrate, or an SOI substrate.
[0041] It should be noted that, in this document, relational terms such as first and second, etc., are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply the existence of any such actual relationship or order between these entities or operations. Moreover, the terms "comprises," "comprising," or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article, or device comprising a series of elements includes not only those elements, but also other elements not explicitly listed, or elements inherent to such process, method, article, or device. In the absence of further limitations, an element defined by the phrase "comprising a ..." does not exclude the presence of other identical elements in the process, method, article, or device comprising the element.
[0042] While embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions, and variations may be made to these embodiments without departing from the principles and spirit of the invention, and that the scope of the invention is defined by the appended claims and their equivalents.
Claims
1. A method for debonding a temporarily bonded carrier structure, characterized in that: The debonding method comprises: forming a through hole in a predetermined area of the wafer of the carrier structure; Inverting the slide structure onto a support member so that a contact area between the support member and the slide structure is located within the through hole, and the contact area is smaller than an area of the through hole; Immersing the wafer carrier structure and the support member in a debonding solution, and stirring the debonding solution to dissolve the temporary bonding glue between the wafer of the wafer carrier structure and the wafer carrier; The method of immersing the carrier structure and the support member in a debonding solution and stirring the debonding solution comprises: Place a magnetic stirring bar in the stirring tank; Using a first cleaning basket to cover the magnetic stirring bar; placing the slide structure and the support member on the first cleaning basket; Pour the debonding solution into the stirring tank, so that the slide structure and the support member are immersed in the debonding solution; The stirring cylinder is placed on a magnetic stirrer, and the magnetic stirrer provides a rotational driving force to the magnetic stirrer.
2. The debonding method according to claim 1, characterized in that: The method of immersing the carrier structure and the support member in a debonding solution and stirring the debonding solution further comprises: The second cleaning basket is used to cover the slide structure and the support.
3. The debonding method according to claim 1 or 2, characterized in that: The support member includes a support plate and a positioning column arranged on the support plate, and a radial cross-sectional area of the positioning column is smaller than an area of the through hole.
4. The debonding method according to claim 3, characterized in that: The carrier is one of a silicon substrate, a glass substrate and an SOI substrate.
5. The debonding method according to claim 4, characterized in that: The temperature of the debonding solution is greater than 50°C.
6. The debonding method according to claim 2, characterized in that: The rotation speed of the magnetic stirrer is greater than 80 rad / s.
7. The debonding method according to claim 6, characterized in that: The first cleaning flower basket and the second cleaning flower basket are made of polytetrafluoroethylene.
8. The debonding method according to claim 7, characterized in that: The stirring cylinder is made of quartz.