Fan-out packaging method

By layering photoresist to form barrier components and conductive pillars, combined with a heat sink structure, the problems of chip misalignment and heat dissipation within the packaging structure are solved, achieving higher stability and heat dissipation performance.

CN114512410BActive Publication Date: 2024-11-08NANTONG FUJITSU MICROELECTRONICS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111671818.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-31
Publication Date
2024-11-08
Estimated Expiration
2041-12-31

AI Technical Summary

Technical Problem

In traditional fan-out packaging methods, shrinkage of the molding compound within the packaging structure causes chip misalignment, affecting lifespan and resulting in poor heat dissipation performance.

Method used

Layered positive and negative photoresists are used to form barrier components and conductive pillars, which, combined with a heat sink structure, restrict material deformation and achieve three-dimensional vertical interconnection.

Benefits of technology

This reduces the probability of chip warpage and improves the heat dissipation and stability of fan-out devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114512410B_ABST
    Figure CN114512410B_ABST
Patent Text Reader

Abstract

The present application discloses a fan-out packaging method, which includes: arranging a first chip, a plurality of blocking members, and a plurality of conductive pillars on a first surface of a carrier; wherein the blocking member has a conductive property, and the blocking member and the conductive pillar are simultaneously formed by means of a positive photoresist and a negative photoresist that are stacked; the plurality of blocking members are arranged around the side periphery of the first chip, the plurality of conductive pillars are arranged around the side periphery of the plurality of blocking members, and the height of the conductive pillars is greater than the height of the blocking members; and a first heat sink is arranged on one side of the non-functional surface of the first chip. In the above manner, the present application can reduce the probability of chip warping and improve the heat dissipation performance of fan-out devices.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor packaging technology, and in particular to a fan-out packaging method. Background Art

[0002] After the chip is encapsulated in the traditional fan-out packaging method, the plastic encapsulation material in the packaging structure shrinks and deforms, which can easily cause the chip to shift in the packaging structure, reducing the service life of the chip. In addition, the performance of the fan-out device is easily affected by the poor heat dissipation performance of the traditional fan-out packaging device. Summary of the invention

[0003] The main technical problem solved by the present application is to provide a fan-out packaging method, which can reduce the probability of chip warping and improve the heat dissipation effect of fan-out devices.

[0004] In order to solve the above technical problems, a technical solution adopted in the present application is: to provide a fan-out packaging method, comprising: arranging a first chip, a plurality of blocking members and a conductive column on the first surface of a carrier; wherein the blocking member has conductive properties, and the blocking member and the conductive column are formed simultaneously by means of a stacked positive photoresist and a negative photoresist; the plurality of blocking members are arranged around the side periphery of the first chip, the plurality of conductive columns are arranged around the side periphery of the plurality of blocking members, and the height of the conductive column is greater than the height of the blocking member; and a first heat sink is arranged on one side of the non-functional surface of the first chip.

[0005] Among them, the step of simultaneously forming the blocking member and the conductive column with the help of stacked positive photoresist and negative photoresist includes: successively forming a first photoresist layer and a second photoresist layer on the first surface of a carrier; wherein, one of the first photoresist layer and the second photoresist layer is a positive photoresist, and the other is a negative photoresist; and the second photoresist layer covers the side of the first photoresist layer and the surface of the first photoresist layer facing away from the carrier; the first photoresist layer and the second photoresist layer are simultaneously exposed and developed, a plurality of first vias are formed on the first photoresist layer, and a plurality of second vias are formed on the second photoresist layer located on the periphery of the side of the first photoresist layer; wherein the height of the second via is greater than the height of the first via; forming the blocking member in the first via, and simultaneously forming the conductive column in the second via; removing the first photoresist layer and the second photoresist layer.

[0006] Wherein, after the step of removing the first photoresist layer and the second photoresist layer, it includes: arranging a first chip in the area surrounded by the multiple blocking members; or, before the step of successively forming the first photoresist layer and the second photoresist layer on the first surface of the carrier, it includes: arranging a first chip on the first surface of the carrier; wherein, when the first photoresist layer and the second photoresist layer are formed on the first surface of the carrier, the second photoresist layer is away from the carrier on the side facing away from the carrier relative to the first chip on the side facing away from the carrier.

[0007] Among them, the first chip includes a functional surface and a non-functional surface arranged opposite to each other, and a conductive bump is arranged on the functional surface of the first chip; the step of arranging the first chip on the first surface of the carrier board includes: making the non-functional surface of the first chip face the first carrier board, and a second heat sink is arranged between the non-functional surface of the first chip and the first carrier board.

[0008] Among them, the step of setting a first heat sink on the non-functional side of the first chip includes: forming insulating glue at least on the side periphery of the first chip and the side periphery of the blocking member, and the blocking member and the first chip form an integral structure through the insulating glue; making the side of the carrier with the first chip facing the conductive substrate, and the conductive column and the conductive bump are electrically connected to the conductive substrate; removing the carrier; setting a first heat sink on the non-functional side of the first chip; wherein the conductive column is exposed from the first heat sink.

[0009] The heat sink includes a base plate and a plurality of side plates extending from the base plate; the orthographic projection of the base plate on the conductive substrate covers the first chip and the blocking member, and the side plates penetrate the gap between the blocking member and the conductive column and contact the conductive substrate.

[0010] Among them, before the step of setting a first heat sink on the non-functional side of the first chip, it includes: forming an insulating layer on the side of the carrier where the first chip is set, and the first chip, the blocking member and the conductive column form an integral structure through the insulating layer; removing the carrier.

[0011] A first rewiring layer is formed on a side of the insulating layer away from the carrier, and the first rewiring layer is electrically connected to one end of the conductive column and a functional surface of the first chip.

[0012] Wherein, the orthographic projection of the first heat sink on the insulating layer covers the first chip, the blocking member and a portion of the conductive column adjacent to the blocking member; or, after the step of removing the carrier, it also includes: arranging a second rewiring layer at the other end of the conductive column, the second rewiring layer is electrically connected to the conductive column; the orthographic projection of the first heat sink on the insulating layer covers the first chip and the blocking member.

[0013] After the step of arranging a first heat sink on one side of the non-functional surface of the first chip, the method further includes: arranging a first electrical connector and a second electrical connector on both sides of the conductive column in the length direction.

[0014] The beneficial effects of the present application are as follows: Different from the prior art, the present application forms blocking members and conductive pillars at the same time by using stacked positive photoresists and negative photoresists. Multiple blocking members and multiple conductive pillars are equivalent to cofferdam walls, which help to limit the movement of materials in the insulating layer to reduce the deformation of the insulating layer due to material shrinkage, thereby reducing the probability of chip warping; and the conductive pillars can realize a three-dimensional vertical interconnection structure, which is conducive to reducing the height of the fan-out device. In addition, the heat dissipation performance of the fan-out device is greatly improved by providing a first heat sink and a second heat sink. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work. Among them:

[0016] Figure 1 It is a flow chart of an implementation method of a fan-out packaging method of the present application;

[0017] Figure 2 yes Figure 1 Step S101 corresponds to a flowchart of an implementation method;

[0018] Figure 3 yes Figure 2 Step S201 corresponds to a cross-sectional structural schematic diagram of an implementation method;

[0019] Figure 4 yes Figure 2 Step S202 corresponds to a cross-sectional structural schematic diagram of an implementation method;

[0020] Figure 5 yes Figure 2 Step S202 corresponds to a cross-sectional structural schematic diagram of another embodiment;

[0021] Figure 6 yes Figure 2 Step S203 corresponds to a cross-sectional structural schematic diagram of an implementation method;

[0022] Figure 7 yes Figure 1 Step S102 corresponds to a cross-sectional structural schematic diagram of an implementation method;

[0023] Figure 8 yes Figure 1 Step S103 corresponds to a cross-sectional structural schematic diagram of an implementation method;

[0024] Fig. 9 yes Figure 1 Step S104 corresponds to a cross-sectional structural schematic diagram of an implementation method;

[0025] Fig.10 yes Figure 1 Step S105 corresponds to a cross-sectional structural schematic diagram of an implementation method;

[0026] Fig.11 is a schematic cross-sectional structural diagram corresponding to an embodiment after step S105;

[0027] Fig.12 It is a flow chart of another implementation method of the fan-out packaging method of the present application;

[0028] Fig.13 yes Fig.12 Step S301 corresponds to a cross-sectional structural schematic diagram of an implementation method;

[0029] Fig.14 yes Fig.12 Step S302 corresponds to a cross-sectional structural schematic diagram of an implementation method;

[0030] Fig.15 yes Fig.12 Step S303 corresponds to a cross-sectional structural schematic diagram of an implementation method;

[0031] Fig.16 yes Fig.12 Step S303 corresponds to a cross-sectional structural schematic diagram of another embodiment. DETAILED DESCRIPTION

[0032] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0033] See also Figure 1 , Figure 1 1 is a flow chart of an embodiment of a fan-out packaging method of the present application, the method comprising:

[0034] S101: Disposing a plurality of blocking members and a plurality of conductive pillars on a first surface of a carrier.

[0035] See also Figure 2 , Figure 2 for Figure 1 Step S101 in the flowchart corresponds to an implementation method, and the specific implementation process of step S101 includes:

[0036] S201: forming a first photoresist layer and a second photoresist layer on a first surface of a carrier in sequence.

[0037] See also Figure 3 , Figure 3 for Figure 2 Step S201 corresponds to a schematic cross-sectional structure diagram of an embodiment, and the specific implementation process of step S201 includes: setting a carrier 10, the carrier 10 includes a first surface 11 and a second surface 12 arranged opposite to each other, and the flatness of the first surface 11 is relatively high. Among them, the material of the carrier 10 can be a hard material such as metal, plastic, etc. Further, a first photoresist layer 20 and a second photoresist layer 30 are successively formed on one side of the first surface 11 of the carrier 10. Among them, one of the first photoresist layer 20 and the second photoresist layer 30 is a positive photoresist, and the other is a negative photoresist, and the second photoresist layer 30 covers the side of the first photoresist layer 20 and the surface of the first photoresist layer 20 away from the carrier 10. Specifically, the positive photoresist is insoluble in the developer before exposure treatment, and can be dissolved in the developer after exposure treatment; the negative photoresist is soluble in the developer before exposure treatment, and is insoluble in the developer after exposure treatment. Step S202 is facilitated by forming a first photoresist layer 20 and a second photoresist layer 30 .

[0038] S202: performing exposure and development processing on the first photoresist layer and the second photoresist layer simultaneously to form a plurality of first via holes and a plurality of second via holes.

[0039] When the first photoresist layer 20 is a positive photoresist and the second photoresist layer 30 is a negative photoresist, please refer to Figure 4 , Figure 4 for Figure 2The step S202 in the figure corresponds to a schematic cross-sectional structure diagram of an embodiment. The specific implementation process of step S202 includes: exposing and developing the first photoresist layer 20 and the second photoresist layer 30 at the same time to form a plurality of first via holes 22 on the first photoresist layer 20, and forming a plurality of second via holes 32 on the second photoresist layer 30 located on the side periphery of the first photoresist layer 20. The formation of the plurality of first via holes 22 and the plurality of second via holes 32 facilitates the execution of step S203. The height of the second via hole 32 is greater than the height of the first via hole 22. Specifically, as Figure 4 As shown in the middle figure a, a mask plate 50 with a plurality of openings 52 is arranged on the side of the second photoresist layer 30 away from the carrier 10; the mask plate 50 is removed after the side of the mask plate 50 away from the carrier 10 is exposed, and the first photoresist layer 20 and the second photoresist layer 30 are simultaneously developed. In response to the second photoresist layer 30 being a negative photoresist, the second photoresist layer 30 located outside the corresponding area of ​​the opening 52 is removed after the development process. Among them, a plurality of second vias 32 are formed in the corresponding area of ​​the second photoresist layer 30 located on the outer periphery of the side of the first photoresist layer 20 and removed. In response to the first photoresist layer 20 being a positive photoresist, for the opening 52 whose orthographic projection on the first photoresist layer 20 is located in the first photoresist layer 20, the first photoresist layer 20 at the corresponding position is removed under the action of development after exposure to form a first via 22. In addition, there is no longer a photoresist layer connected to the second photoresist layer 30 at the corresponding position of the opening 52 whose orthographic projection on the first photoresist layer 20 is located in the first photoresist layer 20, and the part of the second photoresist layer 30 is also removed. After the first photoresist layer 20 and the part of the second photoresist layer 30 are removed, as shown in FIG. Figure 4 As shown in Figure b.

[0040] When the first photoresist layer 20 is a negative photoresist and the second photoresist layer 30 is a positive photoresist, please refer to Figure 5 , Figure 5 for Figure 2 Step S202 in the figure corresponds to a cross-sectional structural schematic diagram of another embodiment. Specifically, the specific implementation process of step S202 includes: Figure 5As shown in the middle figure a, specifically, a mask plate 50 with a plurality of openings 52 is provided on the side of the second photoresist layer 30 away from the carrier 10. The side of the mask plate 50 away from the carrier 10 is subjected to an exposure process; after the exposure process is completed, the mask plate 50 is removed, and the first photoresist layer 20 and the second photoresist layer 30 are simultaneously subjected to a development process. In response to the second photoresist layer 30 being a positive photoresist, the second photoresist layer 30 located at the periphery of the side of the first photoresist layer 20 and at the position corresponding to the opening 52 is removed after exposure and development to form a plurality of second vias 32. For the openings 52 whose orthographic projections on the first photoresist layer 20 are located within the first photoresist layer 20, the second photoresist layer 30 at the corresponding positions is removed through exposure and development. In addition, the first photoresist layer 20 corresponding to the areas enclosed by the openings 52 is not exposed because it is blocked by the mask 50. Moreover, since the first photoresist layer 20 is a negative photoresist layer, the first photoresist layer 20 corresponding to the middle area enclosed by the openings 52 is also removed to form the first via 22. Since the second photoresist layer 30 at the corresponding positions of the openings 52 is removed through development, and the first photoresist layer 20 corresponding to the middle area enclosed by the openings 52 is removed through development, there is no longer any photoresist layer connected to the second photoresist layer 30 at the middle area enclosed by the openings 52, and this part of the second photoresist layer 30 is also removed. After part of the first photoresist layer 20 and part of the second photoresist layer 30 are removed through exposure and development, as shown in FIG. Figure 5 As shown in Figure b.

[0041] S203: forming a blocking member and a conductive pillar, and removing the first photoresist layer and the second photoresist layer.

[0042] See also Figure 6 , Figure 6 for Figure 2 Step S203 in the figure corresponds to a schematic cross-sectional structure diagram of an embodiment. The specific implementation process of step S203 includes: filling the first via hole 22 and the second via hole 32 with conductive material at the same time to form a blocking member 24 and a conductive column 34. Specifically, the conductive column 34 is arranged around the periphery of the blocking member 24, and the height of the conductive column 34 is higher than that of the blocking member 24. The blocking member 24 has conductive properties. Among them, the above-mentioned conductive material can be one or more of titanium, tantalum, chromium, tungsten, copper, aluminum, nickel, gold, etc., preferably titanium or copper. The three-dimensional vertical interconnection structure of the fan-out device can be realized by the conductive column 34, and the blocking member 24 helps to improve the stability of the fan-out device. Further, the first photoresist layer 20 and the second photoresist layer 30 are removed to expose the blocking member 24 and the conductive column 34 to help perform step S102.

[0043] S102: Setting a first chip.

[0044] See also Figure 7, Figure 7 for Figure 1 Step S102 corresponds to a schematic cross-sectional structure diagram of an embodiment, and the specific implementation process of step S102 includes: arranging a first chip 100 in an area surrounded by a plurality of blocking members 24. The first chip 100 includes a functional surface 101 and a non-functional surface 102 disposed opposite to each other, and a conductive bump 105 is disposed on the functional surface 101 of the first chip 100. The conductive bump 105 is electrically connected to the pad 103 on the functional surface 101 of the first chip 100, and one end of the conductive bump 105 is flush with the end of the conductive column 34 away from the carrier 10. Specifically, the non-functional surface 102 of the first chip 100 is directed toward the carrier 10, and a second heat sink 110 is disposed between the non-functional surface 102 of the first chip 100 and the carrier 10 to achieve a certain heat dissipation effect on the first chip 100. The material of the second heat sink 110 may be a metal material such as single element indium, indium alloy, silver alloy, or an organic material; when the material of the second heat sink 110 is a metal material, a flux is required to remove the oxide layer and foreign matter on the surface of the metal heat sink material and improve the wettability and weldability when forming the second heat sink 110. S103: Form an insulating glue at least on the side periphery of the first chip and the side periphery of the blocking member.

[0045] See also Figure 8 , Figure 8 for Figure 1 Step S103 in the figure corresponds to a schematic cross-sectional structure diagram of an embodiment. The specific implementation process of step S103 includes: forming an insulating layer 60 at least on the side periphery of the first chip 100 and the side periphery of the blocking member 24, and the blocking member 24 and the first chip 100 form an integral structure through the insulating layer 60. Specifically, the insulating layer 60 can be formed by filling a colloid, or the side of the carrier 10 provided with the first chip 100 can be plastic-sealed to form the insulating layer 60. The insulating layer 60 is flush with the end of the blocking member 24 away from the carrier 10. By forming the insulating layer 60, at least the blocking member 24 and the first chip 100 can be fixed and protected to a certain extent.

[0046] S104: a conductive substrate is provided, and the side of the carrier on which the first chip is provided faces the conductive substrate.

[0047] See also Fig. 9 , Fig. 9 for Figure 1The step S104 in the figure corresponds to a schematic cross-sectional structure diagram of an embodiment. The step S104 specifically includes: providing a conductive substrate 70, on which a plurality of solders 72 are provided, so that the side of the carrier 10 provided with the first chip 100 faces the conductive substrate 70. The conductive pillars 34 and the conductive bumps 105 are electrically connected to the conductive substrate 70 through the solders 72, so that the first chip 100 is connected to the conductive substrate 70, and information exchange can be performed.

[0048] S105: removing the carrier board, and disposing a first heat sink on the non-functional surface of the first chip.

[0049] See also Fig.10 , Fig.10 for Figure 1 Step S105 in the figure corresponds to a schematic diagram of a cross-sectional structure of an embodiment. The specific implementation process of step S105 includes: removing the carrier 10, setting a first heat sink 120 on the side of the non-functional surface 102 of the first chip 100, and the conductive column 34 is exposed from the first heat sink 120. Among them, the material of the first heat sink 120 can be a metal material such as single element indium, indium alloy, silver alloy, etc., or it can be an organic material; when the material of the first heat sink 120 is a metal material, when forming the first heat sink 120, it is necessary to use a flux to remove the oxide layer and foreign matter on the surface of the metal heat dissipation material, and improve the wettability and weldability. In addition, the first heat sink 120 includes a bottom plate 122 and a plurality of side plates 124 extending from the bottom plate. Among them, the orthographic projection of the bottom plate 122 on the conductive substrate 70 covers the first chip 100 and the blocking member 24, and the side plate 124 penetrates the gap between the blocking member 24 and the conductive column 34 and contacts the conductive substrate 70. By providing the first heat sink 120 including the bottom plate 122 and the plurality of side plates 124, it is helpful to further improve the heat dissipation effect of the fan-out device by increasing the area of ​​the heat sink, and the design of the plurality of side plates 124 also helps to protect the device to a certain extent, avoiding a short circuit between the blocking member 24 and the conductive column 34 due to being too close. Of course, in other embodiments, the first heat sink 120 may also include only the bottom plate 122, and the present application is not limited to this.

[0050] For further information, see Fig.11 , Fig.11 for Figure 1The schematic diagram of the cross-sectional structure after step S105 in one embodiment corresponds to the embodiment. After step S105, it also includes: setting a first electrical connector 160 and a second electrical connector 180 on both sides of the length direction of the conductive column 34. The first electrical connector 160 is electrically connected to the end of the conductive column 34 away from the conductive substrate 70 through a plurality of solder balls 170; the second electrical connector 180 is electrically connected to the conductive substrate 70 through a plurality of solder balls 170. Through the first electrical connector 160 and the second electrical connector 180, the substrate or other chips can be connected to the first chip 100.

[0051] The present application forms the blocking member 24 and the conductive pillar 34 by stacking positive photoresist and negative photoresist, which helps to limit the movement of the material in the insulating layer 60, so as to reduce the deformation of the insulating layer due to material shrinkage, and reduce the probability of chip warping; and the conductive pillar 34 can realize a three-dimensional vertical interconnection structure, which is conducive to reducing the height of the fan-out device. In addition, the heat dissipation performance of the fan-out device is greatly improved by providing the first heat sink 120 and the second heat sink 110.

[0052] In another embodiment, before step S105, an insulating layer 60 is formed on the side of the carrier 10 where the first chip 100 is disposed, and the first chip 100, the blocking member 24 and the conductive pillar 34 form an integral structure through the insulating layer 60. Fig.12 , Fig.12 This is a flow chart of another embodiment of the fan-out packaging method of the present application. The specific implementation process of this embodiment includes:

[0053] S301: forming an insulating layer on a side of the carrier where the first chip is disposed.

[0054] See also Fig.13 , Fig.13 for Fig.12 Step S301 in the figure corresponds to a schematic cross-sectional structure diagram of an embodiment. The specific implementation process of S301 includes: forming an insulating layer 60 on the side of the carrier 10 where the first chip 100 is provided. Specifically, the insulating layer 60 can be formed by filling an insulating material on the side of the carrier 10 where the first chip 100 is provided, and the first chip 100, the blocking member 24 and the conductive column 34 form an integral structure through the insulating layer 60, and the insulating layer 60 plays a certain role in fixing and protecting the first chip 100, the blocking member 24 and the conductive column 34. Among them, one end of the conductive column 34 and the conductive bump 105 are exposed from the insulating layer 60. Optionally, the insulating layer 60 can be formed by filling a colloid, and the surface of the insulating layer 60 is processed by a scraper to expose the conductive column 34 and the conductive bump 105; the side of the carrier 10 where the first chip 100 is provided can also be plastic-sealed to form the insulating layer 60, and the insulating layer 60 is polished from the side of the insulating layer 60 away from the carrier 10 to expose the conductive column 34 and the conductive bump 105.

[0055] S302: forming a first redistribution layer on a side of the insulating layer facing away from the carrier.

[0056] See also Fig.14 , Fig.14 for Fig.12 The step S302 corresponds to a schematic cross-sectional structure diagram of an embodiment. The specific implementation process of the step S302 includes: forming a first rewiring layer 80 on the side of the insulating layer 60 away from the carrier 10, and the first rewiring layer 80 is electrically connected to one end of the conductive column 34 and the functional surface 101 of the first chip 100. Specifically, the first rewiring layer 80 is electrically connected to the first chip 100 through the conductive bump 105. The first rewiring layer 80 is provided to facilitate the connection of the first chip 100 with other devices.

[0057] S303: Disposing a first heat sink on one side of the non-functional surface of the first chip.

[0058] See also Fig.15 , Fig.15 for Fig.12 Step S303 in the figure corresponds to a schematic cross-sectional structure diagram of an embodiment. The specific implementation process of step S303 includes: removing the carrier 10, and setting a first heat sink 120 on the side of the non-functional surface 102 of the first chip 100. Among them, the orthographic projection of the first heat sink 120 on the insulating layer 60 covers the first chip 100, the blocking member 24, and part of the conductive column 34 adjacent to the blocking member 24, that is, the first heat sink 120 is in contact with the blocking member 24, part of the conductive column 34, and the second heat sink 110, which helps to dissipate the overall heat of the packaged fan-out device and further improves the heat dissipation effect.

[0059] For further information, please refer to Fig.15 In this embodiment, step S303 further includes providing a first electrical connector 160 and a second electrical connector 180 on both sides of the length direction of the conductive pillar 34. A plurality of solder balls 150 are provided between the first rewiring layer 80 and the first electrical connector 160, and between the end of the conductive pillar 34 away from the first rewiring layer 80 and the second electrical connector 180, so as to help the electrical connector connect to the first rewiring layer 80 or the conductive pillar 34 at the corresponding position. The first electrical connector 160 and the second electrical connector 180 are provided to facilitate the connection of the fan-out device with the substrate or other chips.

[0060] Optionally, see Fig.16 , Fig.16 for Fig.12Step S303 corresponds to a schematic cross-sectional structure diagram of another embodiment. In this application mode, the first heat sink 120 does not contact the conductive column 34. Specifically, the carrier 10 is removed, and the first heat sink 120 is arranged on the side of the non-functional surface 102 of the first chip 100. Among them, the orthographic projection of the first heat sink 120 on the insulating layer 60 covers the first chip 100 and the blocking member 24. Further, a second rewiring layer 90 is arranged at one end of the conductive column 34, and the second rewiring layer 90 is electrically connected to the conductive column 34. Among them, the surface of the second rewiring layer 90 facing away from the conductive column 34 is flush with the surface of the first heat sink 120 facing away from the first chip 100, and the second rewiring layer 90 is not arranged in the area covered by the first heat sink 120. By setting the second rewiring layer 90, other chips or devices can be connected to the first chip 100.

[0061] For further information, please refer to Fig.16 In this embodiment, step S303 further includes disposing a first electrical connection body 160 and a second electrical connection body 180 on both sides of the length direction of the conductive pillar 34. A plurality of solder balls 150 are disposed between the first rewiring layer 80 and the first electrical connection body 160, and between the second rewiring layer 90 and the second electrical connection body 180, so as to facilitate the electrical connection body to be connected to the first rewiring layer 80 or the second rewiring layer 90 at the corresponding position.

[0062] In this embodiment, the first chip 100 , the blocking member 24 and the conductive pillar 34 are formed into an integral structure through the insulating layer 60 , and the first heat sink 120 is provided to further improve the heat dissipation effect of the fan-out device.

[0063] In addition, in another embodiment, the first chip may be first set on the carrier, and then stacked positive and negative photoresist layers may be formed on one side of the carrier where the first chip is set, and multiple blocking members and conductive columns may be formed through the positive and negative photoresist layers to execute steps S103 to S105.

[0064] In another embodiment, in step S102, the functional surface of the first chip can also be facing the carrier, and a first heat sink and a second heat sink can be further arranged on the non-functional surface of the first chip, and the insulating layer can play a certain fixing and protecting role for at least the first chip, the blocking member and the conductive column.

[0065] The above description is only an implementation method of the present application, and does not limit the patent scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the present application specification and drawings, or directly or indirectly used in other related technical fields, are also included in the patent protection scope of the present application.

Claims

1. A fan-out packaging method, characterized in that: include: A first chip, a plurality of blocking members and a plurality of conductive pillars are arranged on a first surface of a carrier; wherein the blocking members have conductive properties, and the blocking members and the conductive pillars are simultaneously formed by means of a positive photoresist and a negative photoresist that are stacked; the plurality of blocking members are arranged around the periphery of the side surfaces of the first chip, the plurality of conductive pillars are arranged around the periphery of the side surfaces of the plurality of blocking members, and the height of the conductive pillars is greater than the height of the blocking members, an insulating layer is formed around the periphery of the side surfaces of the first chip and the blocking members, and the blocking members and the first chip form an integral structure through the insulating layer; Disposing a first heat sink on one side of the non-functional surface of the first chip; Among them, the step of simultaneously forming the blocking member and the conductive column with the help of stacked positive photoresist and negative photoresist includes: successively forming a first photoresist layer and a second photoresist layer on the first surface of a carrier; wherein, one of the first photoresist layer and the second photoresist layer is a positive photoresist, and the other is a negative photoresist; and the second photoresist layer covers the side of the first photoresist layer and the surface of the first photoresist layer facing away from the carrier; the first photoresist layer and the second photoresist layer are simultaneously exposed and developed, a plurality of first vias are formed on the first photoresist layer, and a plurality of second vias are formed on the second photoresist layer located on the periphery of the side of the first photoresist layer; wherein the height of the second via is greater than the height of the first via; forming the blocking member in the first via, and simultaneously forming the conductive column in the second via; removing the first photoresist layer and the second photoresist layer.

2. The fan-out packaging method according to claim 1, characterized in that: After the step of removing the first photoresist layer and the second photoresist layer, the method further comprises: arranging a first chip in an area surrounded by the plurality of blocking members; Alternatively, before the step of successively forming the first photoresist layer and the second photoresist layer on the first surface of the carrier, the step includes: arranging a first chip on the first surface of the carrier; wherein, when the first photoresist layer and the second photoresist layer are formed on the first surface of the carrier, the second photoresist layer is away from the carrier on a side facing away from the carrier relative to the first chip on a side facing away from the carrier.

3. The fan-out packaging method according to claim 1, characterized in that: The first chip includes a functional surface and a non-functional surface disposed opposite to each other, and a conductive bump is disposed on the functional surface of the first chip; the step of disposing the first chip on the first surface of the carrier board includes: The non-functional surface of the first chip faces the carrier board, and a second heat sink is arranged between the non-functional surface of the first chip and the carrier board.

4. The fan-out packaging method according to claim 3, characterized in that: The step of providing a first heat sink on the non-functional surface of the first chip comprises: An insulating layer is formed at least on the periphery of the side of the first chip and the periphery of the side of the blocking member, and the blocking member and the first chip form an integral structure through the insulating layer; The side of the carrier board provided with the first chip faces the conductive substrate, and the conductive pillars and the conductive bumps are electrically connected to the conductive substrate; removing the carrier plate; A first heat sink is disposed on one side of the non-functional surface of the first chip; wherein the conductive column is exposed from the first heat sink.

5. The fan-out packaging method according to claim 4, characterized in that: The first heat sink includes a bottom plate and a plurality of side plates extending from the bottom plate; The orthographic projection of the bottom plate on the conductive substrate covers the first chip and the blocking member, and the side plate passes through the gap between the blocking member and the conductive column and contacts the conductive substrate.

6. The fan-out packaging method according to claim 3, characterized in that: Before the step of providing a first heat sink on the non-functional surface of the first chip, the method includes: An insulating layer is formed on one side of the carrier board where the first chip is arranged, and the first chip, the blocking member and the conductive column form an integral structure through the insulating layer; The carrier plate is removed.

7. The fan-out packaging method according to claim 6, characterized in that: Before the step of removing the carrier board, the method includes: A first rewiring layer is formed on a side of the insulating layer away from the carrier, and the first rewiring layer is electrically connected to one end of the conductive column and a functional surface of the first chip.

8. The fan-out packaging method according to claim 7, characterized in that: The orthographic projection of the first heat sink on the insulating layer covers the first chip, the blocking member, and a portion of the conductive column adjacent to the blocking member; or, After the step of removing the carrier, the method further includes: providing a second rewiring layer at the other end of the conductive pillar, wherein the second rewiring layer is electrically connected to the conductive pillar; An orthographic projection of the first heat sink on the insulating layer covers the first chip and the blocking member.

9. The fan-out packaging method according to any one of claims 1 to 8, characterized in that: After the step of providing a first heat sink on one side of the non-functional surface of the first chip, the method further includes: A first electrical connector and a second electrical connector are respectively disposed on both sides of the conductive column in the length direction.