Electrode assembly and method for manufacturing the same
By adopting a first electrode in a monolithic form and multiple double-sided electrodes, combined with a monolithic form of the diaphragm and insulating part, the problem of damage to the electrode assembly in a tape pasting process is solved, achieving higher energy density and simplified Manufacturing process.
Patent Information
- Application Number
- CN202180005872.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-03-04
- Filing Date
- 2021-02-26
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2041-02-26
AI Technical Summary
Existing electrode components are prone to wrinkles, expansion or delamination during tape sticking or delamination, resulting in damage to the electrode, slow production speed and low alignment.
The first electrode in the form of a monolithic and a plurality of double-sided electrodes are folded inward and outward by predetermined intervals, combined with the monolithic membrane, avoiding the use of tape to fix it, and adding insulating parts to prevent short circuits.
Effectively prevent electrode damage, improve energy density, simplify manufacturing process, save processing time, and enhance the structural stability and alignment of electrode assembly.
Smart Images

Figure CN114600289B_ABST
Abstract
Description
Technical Field
[0002] CROSS-REFERENCE TO RELATED APPLICATIONS
[0003] This application claims the benefit of priority from Korean Patent Application No. 10-2020-0027431, filed on Mar. 4, 2020, which is hereby incorporated by reference in its entirety. Technical Field
[0004] The present invention relates to an electrode assembly and a method for manufacturing the same, and more particularly, to an electrode assembly and a method for manufacturing the same capable of preventing damage to an electrode such as wrinkles or swelling on the electrode due to a taping process or deintercalation of an active material of the electrode. Background Art
[0005] Generally, secondary batteries include nickel-cadmium batteries, nickel-hydrogen batteries, lithium-ion batteries and lithium-ion polymer batteries. Such secondary batteries are being used in small products such as digital cameras, P-DVDs, MP3Ps, mobile phones, PDAs, portable game devices, power tools, electric bicycles (E-bikes), and large products that require high power such as electric vehicles and hybrid vehicles, power storage devices for storing surplus power or renewable energy, and backup power storage devices.
[0006] In order to manufacture a secondary battery, the electrode assembly is contained in a battery case, and an electrolyte is injected, and then the battery case is sealed. In addition, in order to manufacture an electrode assembly, first, a positive electrode active material slurry is applied to a positive electrode current collector, and a negative electrode active material slurry is applied to a negative electrode current collector to manufacture a positive electrode and a negative electrode, respectively. A separator is inserted between the positive electrode and the negative electrode to manufacture an electrode assembly. Such electrode assemblies are divided into various types. For example, various types of electrode assemblies include: a simple stacking type electrode assembly, in which a positive electrode, a separator, and a negative electrode simply intersect and are stacked continuously without manufacturing a unit cell; a laminated and stacked (L&S) type electrode assembly, in which a laminated and stacked type electrode assembly, a unit cell is first manufactured using a positive electrode, a separator, and a negative electrode, and then stacked; and a stacked and folded (S&F) type electrode assembly, in which a plurality of unit cells are attached to one surface of a long length separator at predetermined intervals and are repeatedly folded from one end of the separator in the same direction.
[0007] Figure 1 is a perspective view of an electrode assembly 30 according to the prior art, and Figure 2 is a front view of an electrode assembly 30 according to the prior art.
[0008] The existing simple stacking type or laminated and stacked type electrode assembly 30 has a simple structure and a high electrolyte impregnation degree, but has the problem that the manufacturing speed is slow and the alignment degree is reduced. In order to maintain the alignment of the plurality of stacked electrodes of the electrode assembly 30 and the separator, a tape pasting process is performed. Then, as Figure 1 As illustrated in FIG. 1 , the tape 31 is attached to each of both surfaces of the top surface and the bottom surface of the electrode assembly 30 and some portions thereof.
[0009] However, in the simple stacking type or the laminated and stacked type electrode assembly 30, each of the negative electrode and the separator has a width relatively wider than that of the positive electrode. Therefore, since the peripheral portion protrudes to the outside, if the tape 31 is attached, there is a problem that the electrode is damaged, such as wrinkling or swelling or delamination of the electrode active material.
[0010] Furthermore, in the electrolyte injection process or the degassing process, the tape 31 may be detached later. In particular, since the gas in the housing must be discharged to the outside in the degassing process, there is a problem that the tape 31 is more easily detached due to the gas flow.
[0011] The stacked and folded type electrode assembly has a high manufacturing speed and high structural stability, but has problems in that the processing is complicated and the degree of alignment and electrolyte impregnation is reduced. Summary of the invention
[0012] Technical issues
[0013] An object of the present invention to solve the above problems is to provide an electrode assembly capable of preventing electrode damage such as wrinkles or swelling on the electrode due to a taping process or delamination of an active material of the electrode and a method of manufacturing the same.
[0014] The objects of the present invention are not limited to the above-mentioned objects, but other objects not described herein will be clearly understood by those skilled in the art from the following description.
[0015] Technical Solution
[0016] An electrode assembly according to an embodiment of the present invention for achieving the above purpose includes: a first electrode, which is formed in a single-piece form and is repeatedly folded inward and outward at a predetermined interval; a second electrode, which is formed in multiple pieces and is respectively inserted in the space formed by folding the first electrode; and a separator, which is formed in a single-piece form and is inserted between the first electrode and the second electrode to repeatedly fold inward and outward at a predetermined interval together with the first electrode, wherein the first electrode is a single-sided electrode in which a first electrode active material is applied only to one surface of a first electrode current collector, and the second electrode is a double-sided electrode in which a second electrode active material is applied to both surfaces of a second electrode current collector.
[0017] In addition, the second electrodes may be inserted only in the spaces formed by folding the first electrodes inwardly.
[0018] In addition, the separator may be interposed between one surface of the first electrode coated with the first electrode active material and the second electrode.
[0019] In addition, an insulating portion formed in the form of a single film may be provided on the other surface of the first electrode where the separator is not provided.
[0020] In addition, the insulating portion may include at least one of polyethylene terephthalate (PET), polypropylene (PP), or polytetrafluoroethylene (PTFE).
[0021] A method for manufacturing an electrode assembly according to an embodiment of the present invention for achieving the above purpose includes the following steps: stacking a separator formed in a single-piece form on one surface of a first electrode formed in a single-piece form in the same direction; arranging a plurality of second electrodes formed in a single-piece form on the separator at predetermined intervals to form an electrode stack; and folding the first electrode and the separator inward and outward to fold the electrode stack, wherein the first electrode is a single-sided electrode in which a first electrode active material is applied only to one surface of a first electrode current collector, and the second electrode is a double-sided electrode in which a second electrode active material is applied to both surfaces of a second electrode current collector.
[0022] In addition, in the step of stacking the separator, the separator is stacked on one surface of the first electrode on which the first electrode active material may be coated.
[0023] In addition, the predetermined interval may be longer than the length of the second electrode.
[0024] In addition, the method may further include the steps of coating an insulating material on the other surface of the first electrode not coated with the first electrode active material and drying the coated insulating material to form an insulating portion before folding the electrode stack.
[0025] In addition, the step of forming the insulating portion may be performed before the step of providing the second electrode.
[0026] In addition, in the step of folding the electrode stack, the first electrode and each region of the separator at one end where the second electrode is provided may be folded inward, and the first electrode and each region of the separator at the other end where the second electrode is provided may be folded outward.
[0027] Details of other implementations are included in the detailed description and accompanying drawings.
[0028] Beneficial Effects
[0029] According to the embodiment of the present invention, there are at least the following effects.
[0030] Since the first electrode is formed in a single-piece form, it is not necessary to fix the electrode assembly using a tape, and thus it is possible to prevent damage to the electrode (such as wrinkles or swelling on the electrode or delamination of an electrode active material).
[0031] In addition, since the first electrode is a single-sided electrode, unnecessary electrode active materials may not be formed on the outermost side of the electrode assembly to improve energy density relative to volume.
[0032] In addition, since it is not necessary to first manufacture unit cells, continuous processing can be easily performed and processing time can be saved.
[0033] The effects of the present invention are not limited to the above-mentioned description, and therefore, more varied effects are involved in this specification. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 is a stereoscopic view of an electrode assembly according to the prior art.
[0035] Figure 2 is a front view of an electrode assembly according to the prior art.
[0036] Figure 3 is a schematic diagram illustrating an electrode stack according to an embodiment of the present invention.
[0037] Figure 4 is a schematic diagram illustrating a shape in which an electrode stack according to an embodiment of the present invention is folded.
[0038] Figure 5 is a schematic diagram of an electrode assembly according to an embodiment of the present invention.
[0039] Figure 6 is a schematic diagram of an electrode stack according to another embodiment of the present invention.
[0040] Figure 7 is a schematic diagram illustrating a shape in which an electrode stack according to another embodiment of the present invention is folded.
[0041] Figure 8 is a schematic diagram of an electrode assembly according to another embodiment of the present invention. DETAILED DESCRIPTION
[0042] The advantages and features of the present invention and their implementation methods will be explained by the following embodiments described with reference to the accompanying drawings. However, the present invention can be implemented in different ways and should not be understood as being limited to the embodiments set forth herein. On the contrary, these embodiments are provided so that the present disclosure will be thorough and complete, and the scope of the present invention will be fully conveyed to those skilled in the art. In addition, the present invention is limited only by the scope of the claims. The same reference numerals always refer to the same elements.
[0043] Unless the terms used in the present invention are defined differently, all terms used herein (including technical terms and scientific terms) have the same meaning as commonly understood by those skilled in the art. In addition, unless clearly and obviously defined in the specification, the terms defined in the commonly used dictionaries are not ideally or excessively interpreted as having a formal meaning.
[0044] In the following description, technical terms are only used to illustrate specific exemplary embodiments, rather than to limit the present invention. In this specification, unless otherwise specified, terms in the singular may include plural forms. The meaning of "include" and / or "comprising" does not exclude other components besides the mentioned components.
[0045] Hereinafter, preferred embodiments will be described in detail with reference to the accompanying drawings.
[0046] Figure 3 is a schematic diagram illustrating an electrode stack 11 according to an embodiment of the present invention.
[0047] According to an embodiment of the present invention, since the first electrode 101 is formed in a single-piece form, it is not necessary to use tape to fix the electrode to the electrode assembly, thereby preventing the electrode from being damaged (such as wrinkles or swelling on the electrode or delamination of the active material of the electrode). In addition, since the first electrode 101 is a single-sided electrode, unnecessary electrode active materials may not be formed on the outermost side of the electrode assembly 10 to increase the energy density relative to the volume. In addition, since it is not necessary to first manufacture a unit cell, continuous processing can be easily performed and processing time can be saved.
[0048] To this end, the manufacturing method of the electrode assembly 10 according to an embodiment of the present invention includes: a step of stacking a separator 103 formed in a single-piece form on one surface of a first electrode 101 formed in a single-piece form in the same direction; a step of arranging a plurality of second electrodes 102 at predetermined intervals on the separator 103 to form an electrode stack 11; and a step of folding the first electrode 101 and the separator 103 inwardly and outwardly to fold the electrode stack 11, wherein the first electrode 101 is a single-sided electrode in which the first electrode active material 1012 is applied only to one surface of the first electrode current collector 1011, and the second electrode 102 is a double-sided electrode in which the second electrode active material 1022 is applied to both surfaces of the second electrode current collector 1021.
[0049] The electrode assembly 10 manufactured by the above method according to an embodiment of the present invention includes: a first electrode 101, which is formed in a single-piece form and is repeatedly folded inward and outward at a predetermined interval; a second electrode 102, which is formed in multiple pieces and is respectively inserted in the space formed by folding the first electrode 101; and a separator 103, which is formed in a single-piece form and is inserted between the first electrode 101 and the second electrode 102, so as to be repeatedly folded inward and outward at a predetermined interval together with the first electrode 101, wherein the first electrode 101 is a single-sided electrode in which the first electrode active material 1012 is applied only to one surface of the first electrode current collector 1011, and the second electrode 102 is a double-sided electrode in which the second electrode active material 1022 is applied to both surfaces of the second electrode current collector 1021.
[0050] As described above, in order to manufacture the electrode assembly 10, first, the positive electrode active material slurry is applied to the positive electrode current collector, and the negative electrode active material slurry is applied to the negative electrode current collector to manufacture the positive electrode and the negative electrode, respectively. The separator 103 is interposed between the positive electrode and the negative electrode, and the separator 103 and the electrodes can be stacked to manufacture the electrode assembly 10.
[0051] The two electrodes, the positive electrode and the negative electrode, used in the present invention are not particularly limited, and the electrode active material can be prepared into a shape that is bonded to the electrode current collector according to a typical method known in the art. Here, the positive electrode can be manufactured by, for example, applying a slurry mixed with a positive electrode active material, a conductive agent, and a binder to the positive electrode current collector, and then drying and pressing the slurry. At this time, if necessary, the slurry may also include a filler. The positive electrode can be manufactured in a sheet form and mounted on a roller.
[0052] The thickness of the positive electrode current collector is generally 3 μm to 500 μm. The positive electrode current collector is generally made of a material having high conductivity without causing chemical changes. Such a material may be surface-treated with, for example, stainless steel, aluminum, nickel, titanium, calcined carbon, or aluminum or stainless steel having a surface treatment with carbon, nickel, titanium, silver, etc. on its surface, but is not limited thereto. In addition, the positive electrode current collector may have fine unevenness on its surface to increase the adhesion of the positive electrode active material. In addition, the positive electrode current collector may have various shapes such as a film, a sheet, a foil, a mesh, a porous body, a foam, a non-woven fabric, and the like.
[0053] In the case of a lithium secondary battery, the positive electrode active material may include a layered compound such as lithium cobalt oxide (LiCoO2), lithium nickel oxide (LiNiO2), or a substituted compound containing one or more transition metals; such as Li 1+x Mn 2-x Lithium manganese oxides such as LiMnO4 (x is 0 to 0.33), LiMnO3, LiMn2O3, LiMnO2, etc.; lithium copper oxide (Li2CuO2); vanadium oxides such as LiV3O8, LiFe3O4, V2O5, Cu2V2O7, etc.; 1-x M x Ni-type lithium nickel oxide represented by O2 (M = Co, Mn, Al, Cu, Fe, Mg, B or Ga, and x = 0.01 to 0.3); represented by the chemical formula LiMn 2-x M x Lithium manganese composite oxide represented by LiMn2O4 (M = Co, Ni, Fe, Cr, Zn or Ta, and x = 0.01 to 0.1) or Li2Mn3MO8 (M = Fe, Co, Ni, Cu or Zn); LiMn2O4 in which part of Li is replaced by alkaline earth ions; disulfide; Fe2(MoO4)3, etc. However, the embodiment is not limited thereto.
[0054] The conductive agent is usually added at 1 wt % to 50 wt % of the total weight of the mixture including the positive electrode active material. The conductive agent is often made of a material that has conductivity without causing chemical changes. The conductive agent may include, for example, a conductive material such as: graphite such as natural graphite and artificial graphite; carbon black such as acetylene black, ketjen black, furnace black, channel black, lamp black, and thermal black; conductive fibers such as carbon fibers and metal fibers; metal powders such as fluorocarbon, aluminum, and nickel powders; conductive whiskers such as zinc oxide and potassium titanate; conductive oxides such as titanium oxide; or polyphenylene derivatives.
[0055] The binder is a component that assists the active material to be combined with the conductive agent and with the current collector, and is generally added at 1% to 50% by weight of the total weight of the mixture including the positive electrode active material. Examples of binders may include polyvinylidene fluoride, polyvinyl alcohol, carboxymethyl cellulose (CMC), starch, hydroxypropyl cellulose, regenerated cellulose, polyvinyl pyrrolidone, tetrafluoroethylene, polyethylene, polypropylene, ethylene-propylene-diene terpolymer (EPDM), sulfonated EPDM, styrene-butadiene rubber, fluororubber, various copolymers, etc.
[0056] The filler may be used as a component to hinder the expansion of the positive electrode. In addition, if the filler is a fiber material that does not cause chemical changes, a common filler may be used. Examples of the filler may include olefin polymers such as polyethylene and polypropylene; and fiber materials such as glass fiber and carbon fiber.
[0057] For example, the negative electrode can be manufactured by coating the negative electrode active material onto the negative electrode current collector, and then drying and pressing the negative electrode active material. If necessary, the negative electrode active material may optionally include a conductive agent, a binder, a filler, etc. The negative electrode can be manufactured in a sheet form and mounted on a roller.
[0058] The thickness of the negative electrode current collector is generally 3 μm to 500 μm. The negative electrode current collector is generally made of a material that has conductivity and does not cause chemical changes. Examples of materials include copper, stainless steel, aluminum, nickel, titanium, calcined carbon, copper or stainless steel with a surface treated with carbon, nickel, titanium, silver, etc., or aluminum-cadmium alloy. In addition, the negative electrode current collector may have fine unevenness on its surface to increase the binding force of the negative electrode active material. In addition, the negative electrode current collector may have various shapes such as a film, a sheet, a foil, a mesh, a porous body, a foam or a non-woven fabric.
[0059] The negative electrode active material may include, for example, carbon such as non-graphitizable carbon, graphite-like carbon, etc.; such as LixFe2O3 (0≤x≤1), Li x WO2(0≤x≤1), Sn x Me 1-x Me' y O z(Me: Mn, Fe, Pb, Ge; Me': Al, B, P, Si, elements of Group I, Group II and Group III in the periodic table, halogens; 0 < x ≤ 1; 1 ≤ y ≤ 3; 1 ≤ z ≤ 8) metal composite oxides such as these; lithium metal; lithium alloy; silicon-based alloy; tin-based alloy; metal oxides such as SnO, SnO2, PbO, PbO2, Pb2O3, Pb3O4, Sb2O3, Sb2O4, Sb2O5, GeO, GeO2, Bi2O3, Bi2O4, Bi2O5; conductive polymers such as polyacetylene; Li-Co-Ni-based materials, etc.
[0060] A known polyolefin separator 103 or a composite separator 103 having an organic and inorganic composite layer formed on an olefin-based material can be used as the separator 103 provided between the positive electrode and the negative electrode to insulate the electrodes from each other, but it is not particularly limited.
[0061] The electrode assembly 10 having the above structure is accommodated in a battery case. Then, an electrolytic solution is injected, and the battery case is sealed to manufacture a secondary battery.
[0062] According to an embodiment of the present invention, the first electrode 101 may be a positive electrode, and the second electrode 102 may be a negative electrode, but it is not limited thereto. For example, the first electrode 101 may be a negative electrode, and the second electrode 102 may be a positive electrode.
[0063] First, as Figure 3 illustrated in, one separator 103 formed in a single-piece form is stacked on one surface of the first electrode 101 formed in a single-piece form in the same direction. Here, the first electrode 101 is a single-sided electrode in which the first electrode active material 1012 is coated only on one surface of the first electrode current collector 1011. Therefore, the first electrode active material 1012 is formed on one surface of the first electrode 101, and the first electrode active material 1012 is not formed on the other surface of the first electrode 101. As a result, the first electrode current collector 1011 is exposed to the outside. The separator 103 formed in a single-piece form is preferably stacked on the one surface of the first electrode 101 coated with the first electrode active material 1012.
[0064] Then, a plurality of second electrodes 102 formed in plurality are arranged to be separated from each other by a predetermined interval on the separator 103 to form an electrode stack 11. Here, the second electrode 102 is a double-sided electrode in which the second electrode active material 1022 is coated on both surfaces of the second electrode current collector 1021. Therefore, the second electrode active material 1022 is formed on both one side and the other side of the second electrode 102.
[0065] It is preferred that the predetermined interval is longer than the length of the second electrode 102. If the predetermined interval is shorter than the length of the second electrode 102, the second electrode 102 is unevenly aligned when the electrode stack 11 is stacked later, and thus protrudes outward. However, if the predetermined interval is longer than the length of the second electrode 102, the second electrode 102 is evenly aligned to reduce the volume, and the area where the second electrode 102 and the first electrode 101 overlap each other increases, so that the energy density is increased.
[0066] Figure 4 is a schematic diagram illustrating a folded shape of an electrode stack 11 according to an embodiment of the present invention.
[0067] like Figure 4 As illustrated in , the electrode stack 11 is folded by folding the first electrode 101 and the separator 103 inwardly and outwardly. That is, in the electrode stack 11, one side of the sheet stacked with the first electrode 101 and the separator 103 is folded inwardly and then folded outwardly in the opposite direction, and then the process is repeated alternately. In addition, the sheet is folded continuously from one side thereof to the other side. At this time, in the first electrode 101 and the separator 103, each of the regions IA where one end 1023 of the second electrode 102 is located can be folded inwardly, and each of the regions OA where the other end 1024 of the second electrode 102 is located can be folded outwardly. That is, the inward folding region and the outward folding region in the first electrode 101 and the separator 103 can be determined according to the position of the second electrode 102.
[0068] Herein, inward folding refers to folding in a direction in which the first electrode 101 surrounds the second electrode 102. Therefore, when inward folding is performed, the separator 103 and the first electrode 101 are sequentially stacked on both surfaces of the second electrode 102. In addition, as an opposite concept of inward folding, outward folding refers to folding in a direction in which the first electrode 101 excludes the second electrode 102. Therefore, when outward folding is performed, the first electrode current collectors 1011 exposed through the other surface of the first electrode 101 are stacked on each other.
[0069] Figure 5 is a schematic diagram of an electrode assembly 10 according to an embodiment of the present invention.
[0070] like Figure 5 As illustrated in the figure, the electrode assembly 10 according to the embodiment of the present invention can be manufactured by the above method. The electrode assembly 10 includes a first electrode 101, a second electrode 102 and a separator 103. The first electrode 101 is a single-sided electrode in which the first electrode active material 1012 is applied only to one surface of the first electrode current collector 1011, and the second electrode 102 is a double-sided electrode in which the second electrode active material 1022 is applied to both surfaces of the second electrode current collector 1021.
[0071] The first electrode 101 is formed in a single sheet form and repeatedly folds inward and outward at a predetermined interval. The second electrode 102 is formed as a plurality of electrodes respectively inserted in the space formed by folding the first electrode 101. In particular, it is preferred that the second electrode 102 is inserted only in the space formed by folding the first electrode 101 inward. The separator 103 is formed in a single sheet form, inserted between the first electrode 101 and the second electrode 102, and repeatedly folds inward and outward at a predetermined interval together with the first electrode 101. In particular, the separator 103 is inserted between one surface of the first electrode 101 coated with the first electrode active material 1012 and the second electrode 102.
[0072] Typically, the two outermost surfaces of the electrode assembly are not used to generate electricity. However, in the electrode assembly 10 according to an embodiment of the present invention, as shown in FIG. Figure 5 , the first electrode current collector 1011 of the first electrode 101 as a single-sided electrode is exposed on both outermost surfaces. Therefore, since the first electrode active material 1012 is not formed on both outermost surfaces that do not generate power, energy density can be increased.
[0073] However, according to an embodiment of the present invention, since the electrode current collectors are also stacked on each other at the outward folded portion of the first electrode 101, the outward folded portion is not used to generate electricity. However, generally, the electrode active material is much thicker than the electrode current collector in the electrode. Therefore, even if the outward folded portion of the first electrode 101 does not generate electricity, the thickness is much thinner, thereby reducing the volume. That is, the energy density relative to the volume can be further improved.
[0074] In addition, since the first electrode 101 and the separator 103 are formed in a single piece, it is not necessary to use a tape to fix the electrode to the electrode assembly, thereby preventing damage to the electrode, such as wrinkles or swelling on the electrode or delamination of the active material of the electrode. In addition, since it is not necessary to first manufacture a unit cell, continuous processing can be easily performed and processing time can be saved.
[0075] Figure 6 is a schematic diagram of an electrode stack 11 a according to another embodiment of the present invention.
[0076] When a secondary battery is actually used, a malfunction may occur due to a collision with the outside. For example, a sharp object may penetrate the secondary battery, and thus, the positive electrode and the negative electrode may directly contact each other to cause a short circuit. Due to the short circuit, a large amount of gas may be generated at a high speed in a short time, and a high temperature may occur. In addition, a large explosion may occur, causing a major malfunction.
[0077] According to another embodiment of the present invention, Figure 6As illustrated in FIG. 1 , before folding the electrode stack 11a, an insulating material may be applied to the other surface of the first electrode 101 that is not coated with the first electrode active material 1012, and then dried to form an insulating portion. The insulating material may be a non-conductive nonconductor with poor conductivity, and may include at least one of polyethylene terephthalate (PET), polypropylene (PP), or polytetrafluoroethylene (PTFE).
[0078] The insulating portion 104 may be formed just before the electrode stack 11a is folded after the electrode stack 11a is formed. However, it is preferred that the insulating portion 104 is formed before the first electrode 101 and the diaphragm 103 are stacked and the second electrode 102 is set. In addition, it is more preferred that the insulating portion 104 is formed before the diaphragm 103 is stacked on the first electrode 101. In order to coat the insulating material on the first electrode 101 and then dry the coated insulating material, the top surface and the bottom surface of the first electrode 101 must be reversed. That is, the insulating material must be coated in a state where one surface of the first electrode 101 faces the lower side and the other surface of the first electrode 101 faces the upper side. This is done because, as the number of objects stacked on one surface of the first electrode 101 decreases, it is easier to perform the process of flipping the first electrode 101 and the process of coating the insulating material.
[0079] Figure 7 is a schematic diagram illustrating a folded shape of an electrode stack according to another embodiment of the present invention, and Figure 8 is a schematic diagram of an electrode assembly according to another embodiment of the present invention.
[0080] like Figure 7 As illustrated in FIG. 1 , the electrode stack 11a is folded by folding the first electrode 101 and the separator 103 inwardly and outwardly. Figure 8 As illustrated in the figure, an electrode assembly 10a according to another embodiment of the present invention can be manufactured by the above method. In the first electrode 101 included in the electrode assembly 10a, an insulating portion 104 formed in the form of a single film is provided on the other surface where the diaphragm 103 is not provided. In addition, the insulating portion 104 may be a non-conductive non-conductor with poor conductivity, and may include at least one of polyethylene terephthalate (PET), polypropylene (PP) or polytetrafluoroethylene (PTFE). That is, in another electrode assembly 10a according to the present invention, the insulating portion 104 formed on the other surface of the first electrode 101 as a single-sided electrode is exposed to the two outermost surfaces. In addition, the insulating portions 104 are stacked on each other at the outward folded portion of the first electrode 101.
[0081] According to another embodiment of the present invention, even if a sharp nail penetrates the secondary battery, a short circuit between the positive electrode and the negative electrode can be prevented to reduce heat generation and also reduce the risk of explosion.
[0082] Those skilled in the art of the present invention will appreciate that the present invention can be performed in other specific forms without changing the technical ideas or essential features. Therefore, the embodiments disclosed above will be regarded as illustrative rather than restrictive. Therefore, the scope of the present invention is defined by the appended claims rather than the exemplary embodiments described above and herein. Various modifications made within the meaning of the equivalents of the claims of the present invention and within the claims will be regarded as within the scope of the present invention.
[0083] [Description of Reference Signs]
[0084] 10, 30: electrode assembly 11: electrode stack
[0085] 101: first electrode 1011: first electrode current collector
[0086] 1012: first electrode active material 102: second electrode
[0087] 1021: Second electrode current collector 1022: Second electrode active material
[0088] 1023: one end of the second electrode 1024: the other end of the second electrode
[0089] 103: diaphragm 104: insulation part
[0090] 31: Tape
Claims
1. A secondary battery, the secondary battery include: a battery case and an electrode assembly, the electrode assembly being accommodated in the battery case and an electrolyte being injected into the battery case; Wherein, the electrode assembly comprises: a first electrode formed in a single sheet form and repeatedly folded inwardly and outwardly at predetermined intervals; a second electrode formed in plural and respectively inserted in spaces formed by folding the first electrode; and a separator formed in a single-sheet form and interposed between the first electrode and the second electrode so as to be repeatedly folded inwardly and outwardly at predetermined intervals together with the first electrode; wherein the first electrode is a single-sided electrode in which the first electrode active material is coated only on one surface of the first electrode current collector, and The second electrode is a double-sided electrode in which the second electrode active material is coated on both surfaces of the second electrode current collector. wherein the separator is interposed between a surface of the first electrode coated with the first electrode active material and the second electrode, wherein the insulating portion formed in the form of a single film is provided on the other surface of the first electrode where the diaphragm is not provided, wherein the insulating portions are stacked on each other at the outwardly folded portion of the first electrode, The inward folding refers to folding in a direction in which the first electrode surrounds the second electrode, and The outward folding refers to folding in a direction in which the first electrode current collectors exposed through the surfaces of the first electrodes are stacked on each other.
2. The secondary battery according to claim 1, in, The second electrodes are inserted only in the spaces formed by folding the first electrodes inwardly.
3. The secondary battery according to claim 1, in, The insulating part includes at least one of polyethylene terephthalate (PET), polypropylene (PP) or polytetrafluoroethylene (PTFE).
4. The secondary battery according to claim 1, in, The predetermined interval is longer than a length of the second electrode.
5. A method for manufacturing a secondary battery, the method The following steps are involved: stacking a separator formed in a monolithic form on one surface of a first electrode formed in a monolithic form in the same direction; disposing a plurality of second electrodes at predetermined intervals on the separator to form an electrode stack; coating an insulating material on the other surface of the first electrode not coated with the first electrode active material and drying the coated insulating material to form an insulating portion, and folding the insulating portion, the first electrode, and the separator inwardly and outwardly to fold the electrode stack to form an electrode assembly, The electrode assembly is housed in a battery case, an electrolyte is injected into the battery case, and then the battery case is sealed, wherein the first electrode is a single-sided electrode in which the first electrode active material is coated only on one surface of the first electrode current collector, and The second electrode is a double-sided electrode in which the second electrode active material is coated on both surfaces of the second electrode current collector. The inward folding refers to folding in a direction in which the first electrode surrounds the second electrode, and The outward folding refers to folding in a direction in which the first electrode current collectors exposed through the surfaces of the first electrodes are stacked on each other.
6. The method according to claim 5, in, In the step of stacking the separator, the separator is stacked on one surface of the first electrode on which the first electrode active material is coated.
7. The method according to claim 5, in, The predetermined interval is longer than a length of the second electrode.
8. The method according to claim 5, in, The step of forming the insulating portion is performed before the step of providing the second electrode.
9. The method according to claim 5, in, In the step of folding the electrode stack, the first electrode and regions of one end of the separator where the second electrode is provided are folded inward, and the first electrode and regions of the other end of the separator where the second electrode is provided are folded outward.