A flat paper tube

By applying a heat seal coating on the paper layer of the food packaging paper tube and setting an anti-permeability layer on the inner wall, the separation problem caused by water vapor at the upper and lower openings of the paper tube is solved, extending the service life and improving the waterproof performance.

CN114803045BActive Publication Date: 2024-11-05DUOPU PRINTING DESIGN (SHENZHEN) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210556890.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-05-19
Publication Date
2024-11-05
Estimated Expiration
2042-05-19

AI Technical Summary

Technical Problem

After long-term use of the existing food packaging paper tube, due to exposure to air at the upper and lower openings, it is easy to separate multiple layers of paper due to water vapor and other reasons, causing rupture problems.

Method used

A flat rolled paper tube design with at least two layers of paper, wherein the first heat seal coating is coated in the outer edges of the first and second regions along the width direction of the paper layer, and is solidified by heating to tighten the paper and a second heat seal coating is applied at the first side of the second area and the second side of the first area to enhance adhesion, while an anti-permeability layer and a barrier layer are provided on the inner wall of the paper tube to prevent Moisture permeation.

Benefits of technology

Effectively prevent the separation of paper layers at the upper and lower openings of the paper tube, extend the service life, and prevent moisture from penetrating when filling oily or rich in moisture, improving the waterproof performance and stability of the paper tube.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114803045B_ABST
    Figure CN114803045B_ABST
Patent Text Reader

Abstract

The present application provides a flat rolled paper tube, comprising at least two layers of paper rolled flat; any of the paper layers comprises a first region for rolling to form the paper tube body, and a second region for rolling to form the paper tube end cap; wherein, along the width direction of the paper layer, the first region and the second region are coated with a first heat-seal coating at the opposite outer edges, so that when the multiple layers of the paper layers are rolled on a heated core, the first heat-seal coating can seal the outer wall of the paper tube. The above scheme is to coat the first heat-seal coating at the opposite outer edges of the first region and the second region along the width direction of the paper layer, so that when the multiple layers of paper layers are rolled on the heated core, the heated core solidifies the first heat-seal coating at the outer edges of the first region and the second region so that the multiple layers of paper layers are tightly adhered to each other.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present application relates to the field of packaging technology, and in particular to a flat roll paper tube. [Background technology]

[0002] In the field of food packaging, paper packaging cans are usually used to hold food. In the production process of existing food packaging paper tubes, multiple paper layers are usually rolled flat and pressed together by hot pressing. During the use of the pressed paper tube, since the upper and lower openings of the paper tube are exposed to the air, after long-term use, the upper and lower openings of the paper tube may rupture due to moisture in the air, resulting in the separation of multiple paper layers. [Summary of the invention]

[0003] In view of this, it is necessary to provide a flat rolled paper tube that can prevent the upper and lower openings of the paper tube from breaking to solve the above problems.

[0004] An embodiment of the present application provides a flat-rolled paper tube, comprising at least two paper layers flat-rolled;

[0005] Any of the paper layers comprises a first region for winding to form the paper tube body, and a second region for winding to form the paper tube end cap;

[0006] Wherein, along the width direction of the paper layer, the first area and the second area are coated with a first heat-sealing coating at the opposite outer edge portions, so that when the multiple paper layers are wound on the heated core, the first heat-sealing coating can seal the outer wall of the paper tube.

[0007] In at least one embodiment of the present application, the second region has a first side extending outwardly from the first region;

[0008] The second region is coated with a second heat-sealing coating at the position of the first side edge, and the second heat-sealing coating is used to adhere the first side edge to the tube body of the wound paper tube.

[0009] In at least one embodiment of the present application, the ratio of the length of the first side to the width of the paper layer is 1 / 20-2 / 3.

[0010] In at least one embodiment of the present application, the first region has a second side extending outwardly along the first side;

[0011] The first region is coated with a third heat-sealing coating at the second side edge position, which is used to adhere the second side edge to the tube body of the wound paper tube.

[0012] In at least one embodiment of the present application, the ratio of the length of the second side to the length of the paper layer is 1 / 2-2 / 3.

[0013] In at least one embodiment of the present application, the paper tube further comprises a barrier layer wound around the inner layer of the paper tube and an anti-permeation layer detachably wound around the inner layer of the barrier layer;

[0014] A fixed structure is arranged on the side of the barrier layer away from the paper layer, and the anti-permeability layer is sleeved on the fixed structure and is wound around the inner layer of the barrier layer according to the fixed structure.

[0015] In at least one embodiment of the present application, the fixing structure includes a first fixing member and a second fixing member protruding from the barrier layer;

[0016] The anti-permeability layer is provided with a first fixing hole, and the anti-permeability layer is sleeved on the first fixing member through the first fixing hole;

[0017] The second fixing member is provided with a second fixing hole, and the second fixing member is sleeved on the first fixing member through the second fixing hole to press the anti-permeability layer onto the inner wall of the barrier layer.

[0018] In at least one embodiment of the present application, the second fixing member is made of a flexible material.

[0019] In at least one embodiment of the present application, the barrier layer is provided with folds;

[0020] The barrier layer can be folded along the fold to form a first barrier layer and a second barrier layer stacked on each other;

[0021] The first barrier layer is attached to the inner wall of the paper layer, and the fixing structure is arranged on the inner wall of the second barrier layer.

[0022] In at least one embodiment of the present application, the first barrier layer and the second barrier layer are made of elastic plastic material.

[0023] This application has at least the following beneficial effects:

[0024] 1. By coating the first heat-sealing coating on the outer edges of the first region and the second region relative to each other along the width direction of the paper layer, when the multiple paper layers are wound on the heated core, the heated core solidifies the first heat-sealing coating on the outer edges of the first region and the second region so that the multiple paper layers are tightly adhered to each other, thereby bonding and fastening the multiple paper layers at the openings at the upper and lower ends of the formed paper tube, thereby preventing the problem of paper layers being damaged and separated due to the upper and lower ends of the paper tube being exposed to the air.

[0025] 2. By coating the second heat-sealing coating at the first side edge of the second region and the second side edge of the first region, the tightness of the bonding between each two paper layers is further ensured. After the multiple paper layers are wound on the core, the first side edge and the second side edge of the outermost paper layer are adhered to the paper tube body by the second heat-sealing coating, so as to prevent the first side edge and the second side edge from flying off and separating relative to the tube body due to water vapor in the air, thereby ensuring the quality of the tube body and extending the service life of the tube body.

[0026] 3. By setting the width ratio of the first side edge to the paper layer to 1 / 20-2 / 3 and the length ratio of the second side edge to the paper layer to 1 / 2-2 / 3, the thickness of the wound paper tube end cap and the length of the end cap extending outward from the tube body are ensured, thereby preventing the end cap from being damaged due to being too long or too thin.

[0027] 4. By setting an anti-permeation layer on the inner wall of the paper tube, when the paper tube contains oily objects or other objects with water, it is prevented that the water in the object penetrates the paper tube and softens the paper tube, thereby causing the paper tube to be unable to be reused. Furthermore, a barrier layer made of plastic material is set between the anti-permeation layer and the paper layer, so that when there is too much water in the paper tube and penetrates the anti-permeation layer, the barrier layer can further prevent water from penetrating. And by setting a fixing structure on the inner wall of the barrier layer, by sleeve-mounting the first fixing hole on the anti-permeation layer on the first fixing member, and by sleeve-mounting the second fixing hole on the second fixing member on the first fixing member or removing it from the first fixing member, the installation and removal of the anti-permeation layer is realized, by tearing the anti-permeation layer off the inner wall of the paper layer, and adhering a new anti-permeation layer to the inner layer of the paper layer by hot pressing or gluing, so as to replace the anti-permeation layer, so as to solve the problem in the prior art that the paper tube cannot be used due to the inability to replace the anti-permeation layer and the anti-permeation layer being penetrated by water after the paper tube is used for a long time, so as to extend the service life of the paper tube.

[0028] 5. By extending the first fixing member from the barrier layer toward the axial direction of the paper tube, the multiple anti-permeation layers are stacked on each other to increase their thickness, thereby increasing their thickness and improving the anti-permeation performance. A stopper, a fixing member and a first fixing member are arranged on the first barrier layer to prevent the impact of the liquid from both sides when the paper tube is loaded with liquid, thereby increasing the stability of the anti-permeation layer. Furthermore, by arranging the fixing member parallel to the barrier layer, the thickness of the placement groove is uniform, thereby facilitating the placement of the anti-permeation layer.

[0029] 6. The barrier layer is folded along the crease to form a first barrier layer and a second barrier layer which are stacked on each other, and the first barrier layer and the second barrier layer are made of elastic plastic material, so that the first barrier layer and the second barrier layer generate a mutual force at the folded portion, and when the paper tube is deformed by an external force, the first barrier layer located at the deformed portion pushes the paper layer outward under the action of its own elastic force and the elastic force of the second barrier layer to restore the original state, thereby preventing the paper tube from being damaged or affecting its aesthetics due to deformation of its appearance due to impact.

Brief Description of the Drawings

[0030] Figure 1 It is a schematic diagram of the three-dimensional structure of a paper tube in one embodiment of the present application.

[0031] Figure 2 This is a schematic diagram of the three-dimensional structure of a paper tube in another embodiment of the present application.

[0032] Figure 3 This is a schematic diagram of the three-dimensional structure of the paper tube in the third embodiment of the present application.

[0033] Figure 4 for Figure 1 A top view of the paper tube shown.

[0034] Figure 5 for Figure 4 Schematic diagram of the barrier layer before folding.

[0035] Figure 6 for Figure 4 Schematic diagram of the barrier layer after folding.

[0036] Figure 7 for Figure 5 A schematic diagram of the first barrier layer and the second barrier layer being bent at a crease is shown.

[0037] Figure 8 for Figure 5 A cross-sectional view of the barrier layer, anti-permeation layer, fixing structure and adhesive layer when they are combined.

[0038] Fig. 9 for Figure 4 An expanded view of the paper layers shown.

[0039] Fig.10 for Figure 1 The forming process of the paper tube is shown.

[0040]

Main component symbol description

[0041] 100, paper tube; 100a, paper layer; 10, tube body; 10a, first area; 11a, second side; 20, end cap; 20a, second area; 21a, first side; 30, first heat-seal coating; 40, second heat-seal coating; 50, third heat-seal coating; 60, barrier layer; 60a, fold; 61, first barrier layer; 62, second barrier layer; 70, anti-permeation layer; 71, first fixing hole; 71a, fitting surface; 72, first end; 72a, first surface; 72b, second surface; 73, second end; 73a, third surface; 73b, fourth surface; 80, fixing structure; 80a, accommodating groove; 80b, placement groove; 81, first fixing member; 82, second fixing member; 82a, stopper; 82b, fixing portion; 821, second fixing hole; 90, adhesive layer. [Specific implementation method]

[0042] The embodiments of the present application will be described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all the embodiments.

[0043] It should be noted that when a component is considered to be "connected" to another component, it may be directly connected to the other component or there may be a central component at the same time. When a component is considered to be "located on" another component, it may be directly located on the other component or there may be a central component at the same time. The terms "top", "bottom", "upper", "lower", "left", "right", "front", "back", and similar expressions used herein are for illustrative purposes only.

[0044] An embodiment of the present application provides a flat-rolled paper tube, comprising at least two layers of paper rolled flat; any of the paper layers comprises a first area for rolling to form the paper tube body, and a second area for rolling to form the paper tube end cover; wherein, along the width direction of the paper layer, the first area and the second area are coated with a first heat-sealing coating on the opposite outer edge portions, so that when the multiple layers of the paper layers are rolled on a heated tube core, the first heat-sealing coating can seal the outer side wall of the paper tube.

[0045] The above scheme applies the first heat-seal coating on the outer edge portions of the first region and the second region relative to each other along the width direction of the paper layer, so that when the multiple paper layers are wound on the heated core, the heated core solidifies the first heat-seal coating on the outer edges of the first region and the second region so that the multiple paper layers are tightly bonded to each other.

[0046] Some embodiments of the present application are described in detail below in conjunction with the accompanying drawings. In the absence of conflict, the following embodiments and features in the embodiments can be combined with each other.

[0047] See also Figure 1 , Figure 2 and Figure 3 The present application provides a flat roll paper tube 100, comprising at least two paper layers 100a flatly rolled to form a container for placing food or cosmetics. Preferably, the number of paper layers 100a is four layers to form a paper tube 100 with a certain thickness. It is understood that the number of paper layers 100a is not limited thereto, and in order to meet the placement requirements of different objects, the number of paper layers 100a can also be two layers, three layers, five layers, etc.

[0048] In a specific embodiment, the paper layer 100a is coated white paper.

[0049] It should be noted that the above-mentioned paper tube 100 is formed by flat rolling of at least two paper layers 100a. Among them, at least two paper layers 100a need to be wound on a core or a mold, and the rotation of the mold drives the rotation of the paper layer 100a to form the corresponding paper tube 100. And the shape of the final paper tube 100 is consistent with the shape of the core or mold on which it is wound, that is, when the shape of the core or mold is a cylinder, the wound paper tube 100 is a cylindrical can. When the shape of the core or mold is a rectangular body, the wound paper tube 100 is a rectangular can. When the core or mold is an ellipse, the wound paper tube 100 is an ellipse.

[0050] Please combine Figure 1 - Fig.10 , any paper layer 100a includes a first area 10a for winding into the above-mentioned tube body 10, and a second area 20a for winding into the above-mentioned end cap 20. So that the multi-layer paper layer 100a can form the above-mentioned paper tube 100 by winding. Preferably, the first area 10a and the second area 20a of the paper layer 100a are rectangular paper layers 100a, so that the first area 10a and the second area 20a can be evenly wound on the tube core or the mold. It can be understood that since the first area 10a and the second area 20a on any paper layer 100a are different parts connected on the same paper, that is, in the production process of the paper tube 100, the tube body 10 part and the end cap 20 part of the paper tube 100 are an integrally formed structure, thereby avoiding the cumbersome operation of separately forming the tube body 10 and the end cap 20 and then fixing the tube body 10 and the end wall, reducing the production process steps, thereby improving the production efficiency and saving labor costs.

[0051] In a specific embodiment, the second area 20a is a rectangular block-shaped paper layer 100a extending outward from one side or two opposite sides of the first area 10a, so as to form an end cover 20 portion having a smaller diameter than the tube body 10 in the paper tube 100 formed by winding, so that a cover body can be provided on the end cover 20 to achieve sealing and opening and closing of the paper tube 100, so as to facilitate the placement of food.

[0052] Further, the second region 20a has a first side edge 21a extending outwardly along the first region 10a. Preferably, the ratio of the length of the first side edge 21a to the width of the paper layer 100a is 1 / 20-2 / 3, so that in the tube body 10 and the end cap 20 formed by winding the first region 10a and the second region 20a, the end cap 20 will not extend a large distance relative to the tube body 10, thereby reducing the overall height of the end cap 20 when the amount of paper is constant, and lowering the center of gravity of the end cap 20 as a whole, thereby increasing the strength of the end cap 20 and reducing the probability of the end cap 20 being damaged.

[0053] In a specific embodiment, the length of the first side 21a can be set to 10mm-120mm, and the width of the paper layer 100a can be set to 15mm-200mm. It is understandable that the length of the first side 21a and the width of the paper layer 100a can be specified to corresponding sizes according to the requirements of specific products.

[0054] Furthermore, the first region 10a has a second side edge 11a extending outwardly along the first side edge 21a, that is, the first side edge 21a and the second side edge 11a are two lines intersecting at the corner where the first region 10a and the second region 20a form a height difference. Preferably, the first side edge 21a is perpendicular to the second side edge 11a. Preferably, the ratio of the length of the second side edge 11a to the length of the paper layer 100a is 1 / 2-2 / 3. Within this range, the length of the second region 20a occupies a certain proportion of the total length of the paper layer 100a, so that after the paper layer 100a is wound to form the paper tube 100, the end cap 20 is guaranteed to have a certain thickness, thereby further preventing the end cap 20 from being damaged. At this time, the vacancy formed by the diameter difference between the end cap 20 and the tube body 10 can be covered by the cover body, so that it is convenient for the cover body to block the inner cavity of the tube body 10, and the strength of the end cap 20 can be guaranteed, and the quality of the paper tube 100 is guaranteed on the premise of improving the performance of the paper tube 100.

[0055] In a specific embodiment, the length of the second side 11a can be set to 40mm-140mm, and the length of the second area 20a can be set to 40mm-130mm. It is understandable that the length of the second side 11a and the length of the second area 20a can be specified to corresponding sizes according to the requirements of specific products.

[0056] It should be noted that during the production process of the paper tube 100, that is, during the flat rolling process of the paper layer 100a, an opening is formed at the upper end or the upper and lower ends of the paper tube 100, and no sealing operation is performed on the stacked ends of the multiple paper layers 100a at the opening, and the multiple paper layers 100a are directly exposed to the air at the opening. Due to the presence of more water vapor and some corrosive gases in the air, the multiple paper layers 100a may be broken at the opening, that is, the multiple paper layers 100a may be separated from each other.

[0057] In order to prevent the problem of the multi-layer paper layers 100a being separated from each other and to reduce the usage of the first heat-sealing coating 30, the first heat-sealing coating 30 is coated on the outer edge portions of the first region 10a and the second region 20a relative to each other, so that when the multi-layer paper layers 100a are wound on a heated core or mold, the first heat-sealing coating 30 can seal the outer wall of the paper tube 100.

[0058] It should be noted that the first heat-sealing coating 30 is a coating that can be cured by heating to play a bonding role, such as some organic polymers. In the process of winding the multi-layer paper layer 100a, by arranging the first heat-sealing coating 30 between every two paper layers 100a, during the lamination process of the multi-layer paper layer 100a, when the cylinder core or the mold is heated to achieve the hot pressing function, the first heat-sealing coating 30 arranged between every two paper layers 100a is cured to achieve the fixation between the two adjacent paper layers 100a. When the first heat-sealing coating 30 is fully covered on the side of each paper layer 100a, the use amount of the first heat-sealing coating 30 will increase significantly, thereby causing waste of the first heat-sealing coating 30 in the large-scale production process of the paper tube 100, thereby increasing the production cost.

[0059] In one embodiment, the first heat-sealing coating 30 is applied only to the outer edge portions of the first region 10a and the second region 20a, and the whole is hot pressed, that is, the core or mold is heated and the multi-layer paper layers 100a are pressed together, so as to ensure the stability of the connection between each two adjacent paper layers 100a. For other parts of the tube body 10 except the upper and lower edge portions, the tightness of the connection between the two adjacent paper layers 100a can be achieved by hot pressing. Since the first heat-sealing coating 30 is applied to the outer edge portions of the first region 10a and the second region 20a, the two adjacent paper layers 100a are bonded by the first heat-sealing coating 30 after heating and curing, so as to prevent the problem of delamination of the outer paper layer 100a caused by the action of external water vapor or other corrosive gases, thereby ensuring the use quality of the paper tube 100 and extending the service life of the paper tube 100.

[0060] In another embodiment, in addition to coating the first heat-sealing layer on the opposite outer edge portions of the first region 10a and the second region 20a, the first heat-sealing coating 30 may be coated alternately in other inner regions except the first region 10a and the second region 20a to further enhance the fastness of the connection between the two adjacent paper layers 100a.

[0061] Furthermore, in a specific embodiment, along the width direction of the paper layer 100a, the width of the first heat-sealing coating 30 is 2mm-5mm, so that the outer edge parts of the two adjacent paper layers 100a are tightly sealed by applying the first heat-sealing coating 30 of the above width. It can be understood that the coating width of the first heat-sealing coating 30 can be determined according to the corrosion resistance strength and corresponding service life of the paper tube 100 to be manufactured. When the corrosion resistance of the paper tube 100 required is strong, the first heat-sealing coating 30 with a width of 5mm can be selected. When the corrosion resistance of the paper tube 100 required is weak, the first heat-sealing coating 30 with a width of 2mm can be selected.

[0062] Please refer to Figure 1 and Fig. 9 In order to better prevent the outermost side wall of the paper tube 100 from flying up relative to the tube body 10 and damaging the quality of the paper tube 100, the second area 20a is coated with a second heat-sealing coating 40 at the position of the first side edge 21a, so that when the second area 20a is wound, the outermost end of the second area 20a can be adhered to the tube body 10 of the wound paper tube 100 through the second heat-sealing coating 40.

[0063] It should be noted that, since the length of the second region 20a is shorter than that of the first region 10a, when the first region 10a and the second region 20a are wound together, the second region 20a is wound first, and at this time, the outermost end wall of the second region 20a is attached to the end cap 20 formed by the second region 20a. At this time, the outermost end wall of the second region 20a will not be wound together with the first region 10a, that is, after the winding is completed, the outer end wall of the second region 20a is exposed to the air, and the stratification problem occurs under the action of water vapor and corrosive gases in the air. The present application applies the second heat-sealing coating 40 at the first side edge 21a of the second region 20a, and heats the core or mold to cure the second heat-sealing coating 40, so that the outer end wall of the second region 20a is attached to the end cap 20 formed by the winding of the second region 20a.

[0064] In one embodiment, the lower end of the second heat-sealing coating 40 is flush with the lower end of the first side 21a, and the upper end of the second heat-sealing coating 40 is coated to the position of the first heat-sealing coating 30. At this time, since the entire first side 21a is coated with the second heat-sealing coating 40, the stability of the first side 21a and the end cap 20 after winding is ensured.

[0065] In another embodiment, the upper end of the second heat-seal coating 40 is coated to the position of the first heat-seal coating 30, and the lower end is located above the lower end of the first side 21a. It should be noted that, since the first region 10a and the second region 20a are integrally arranged, the lower end point of the first side 21a is directly connected to the first region 10a. When the number of turns wound in the first region 10a is greater than the number of turns wound in the first region 10a, the lower end point of the first side 21a is fixed to the first region 10a, and the upper end point of the first side 21a is arranged to float relative to the lower end point, so that the paper layer 100a in the region of the upper end of the first side 21a is greatly affected by water vapor in the air. By coating the second heat-seal coating 40 at the position of the upper end of the first side 21a, the overall adhesion effect of the first side 21a is ensured, and the use of the second heat-seal coating 40 at the lower end of the first side 21a can be reduced, which reduces the use of materials and reduces production costs.

[0066] Furthermore, along the length direction of the paper tube 100, the width of the second heat-seal coating 40 is 2 mm to 5 mm, so that the paper layer 100a of the second region 20a at the position of the first side edge 21a is tightly sealed on the end cover 20 by applying the second heat-seal coating 40 of the above width. It can be understood that the coating width of the second heat-seal coating 40 can be determined according to the corrosion resistance strength and corresponding service life of the paper tube 100 to be manufactured. When the corrosion resistance of the paper tube 100 required is strong, the second heat-seal coating 40 with a width of 5 mm can be selected. When the corrosion resistance of the paper tube 100 required is weak, the second heat-seal coating 40 with a width of 2 mm can be selected.

[0067] In one embodiment, the first heat-seal coating 30 is a coating that can be cured by heating to provide an adhesive effect, such as some organic polymers.

[0068] Furthermore, in order to better prevent the multiple paper layers 100a on the paper tube 100 from delaminating, the first area 10a is coated with a third heat-sealing coating 50 at the second side edge 11a to adhere the third side edge to the wound tube body 10.

[0069] It should be noted that, since the length of the first region 10a is longer than that of the second region 20a, when the first region 10a is wound, the number of windings of the first region 10a is greater than that of the second region 20a, resulting in the first region 10a forming an outermost paper layer 100a on the outer surface of the end cap 20 after winding. The outermost paper layer 100a forms a second side edge 11a on the outer surface of the end cap 20 after winding, and the second side edge 11a is exposed to the air, and is easily damaged by the action of water vapor and corrosive gases in the air, resulting in burrs. The present application applies a third heat-sealing coating 50 at the position of the second side edge 11a of the first region 10a, so as to adhere the third side edge exposed to the air to the tube body 10 after winding. Preferably, the length of the third heat-sealing coating 50 is equal to the length of the third side edge, so as to completely adhere the third side edge to the end cap 20, thereby maximizing the sealing of the third side edge.

[0070] Furthermore, along the width direction of the paper tube 100, the width of the third heat-sealing coating 50 is 2 mm to 5 mm, so that the second side 11a exposed to the air is adhered to the end cover 20 by coating the third heat-sealing coating 50 of the above width. It can be understood that the coating width of the third heat-sealing coating 50 can be determined according to the corrosion resistance and corresponding service life of the paper tube 100 to be manufactured. When the corrosion resistance of the paper tube 100 required is strong, the third heat-sealing coating 50 with a width of 5 mm can be selected. When the corrosion resistance of the paper tube 100 required is weak, the third heat-sealing coating 50 with a width of 2 mm can be selected.

[0071] In one embodiment, the third heat-seal coating 50 is a coating that can be cured by heating to provide an adhesive effect, such as some organic polymers.

[0072] Please combine Figure 4 The paper tube 100 further includes a barrier layer 60 wound on the inner layer of the paper tube 100. By providing the barrier layer 60 on the inner wall of the paper tube 100, when the paper tube 100 contains oily food or cosmetics that are easy to remain and adhere to the inner wall of the paper tube 100, the problem of the paper tube 100 being only usable once due to the adherence of the contained materials to the inner wall of the paper tube 100 is prevented, so that the paper tube 100 can be recycled for multiple times to reduce the use cost.

[0073] Preferably, the barrier layer 60 is formed of long-fiber coated paper to play a barrier role, preventing the inner wall of the paper tube 100 from sticking to the residue of objects placed in the inner cavity of the tube body 10, which would cause the paper tube 100 to be used only once. It can also be used to prevent the penetration of external air, water vapor and water.

[0074] Furthermore, the paper tube 100 also includes an anti-permeation layer 70 detachably wound around the inner layer of the barrier layer 60. A fixed structure 80 is provided on the side of the barrier layer 60 away from the paper layer 100a, and the anti-permeation layer 70 is sleeved on the fixed structure 80 and wound around the inner layer of the barrier layer according to the fixed structure 80. By arranging the anti-permeation layer 70 on the inner wall of the paper tube 100, when the paper tube 100 contains oily objects or other objects with water, it is prevented that the water in the objects penetrates the paper tube 100 and softens the paper tube 100, thereby causing the problem that the paper tube 100 cannot be reused. In one embodiment, the anti-permeation layer 70 is a paper layer structure with a smooth surface. It should be noted that the above scheme arranges a barrier layer 60 made of plastic material between the anti-permeation layer 70 and the paper layer 100a, so that when there is too much water in the paper tube 100 and penetrates the anti-permeation layer 70, the barrier layer 60 can further prevent water from penetrating.

[0075] Furthermore, the fixing structure 80 includes a first fixing member 81 and a second fixing member 82 protruding from the barrier layer 60. The anti-permeation layer 70 is provided with a first fixing hole 71, and the anti-permeation layer 70 is sleeved on the first fixing member 81 through the first fixing hole 71. The second fixing member 82 is provided with a second fixing hole 821, and the second fixing member 82 is sleeved on the first fixing member 81 through the second fixing hole 821, so as to press the anti-permeation layer 70 onto the inner wall of the barrier layer. The above scheme realizes installation and removal of the anti-permeation layer 70 by arranging a fixing structure 80 on the inner wall of the barrier layer 60, by sleeve-mounting the first fixing hole 71 on the anti-permeation layer 70 on the first fixing piece 81, and by sleeve-mounting the second fixing hole 821 on the second fixing piece 82 on the first fixing piece 81 or removing it from the first fixing piece 81, and by tearing off the anti-permeation layer 70 from the inner wall of the paper layer 100a and adhering a new anti-permeation layer 70 to the inner layer of the paper layer 100a by hot pressing or gluing to replace the anti-permeation layer 70, so as to solve the problem in the prior art that the paper tube 100 cannot be used due to the inability to replace the anti-permeation layer 70 and the anti-permeation layer 70 being penetrated by water after the paper tube 100 is used for a long time, so as to extend the service life of the paper tube 100.

[0076] In one embodiment, the first fixing member 81 is made of a hard material to facilitate the installation of the anti-permeation layer 70 and prevent the anti-permeation layer 70 from falling off due to the first fixing member 81 being relatively soft.

[0077] Furthermore, in order to prevent the problem of poor anti-permeability performance caused by the anti-permeability layer 70 being too thin, the first fixing member 81 extends from the barrier layer 60 toward the axis of the paper tube 100, so that multiple anti-permeability layers 70 can be stacked on each other and are sleeved on the first fixing member 81 through the first fixing hole 71 on each anti-permeability layer 70, so as to increase the thickness of the inner anti-permeability layer 70 of the paper tube 100, thereby increasing the anti-permeability performance of the paper tube 100.

[0078] Furthermore, when a liquid substance, such as liquid milk, is placed in the paper tube 100, in order to prevent the liquid in the paper tube 100 from being intentionally shaken or rotated by human factors, which may cause the liquid to penetrate into the inner surface of the adhesive opening of the anti-permeation layer 70 due to the centrifugal force of the shaking or rotation, thereby causing the anti-permeation layer 70 to separate from the barrier layer 60, the second fixing member 82 includes a stopper 82a provided on the barrier layer 60 and a fixing member 82b provided on the stopper 82a. Specifically, the stopper 82a and the fixing member 82b are arranged to surround the first fixing member 81, so that when the liquid impacts the first fixing member 81 along the stopper 82a, the stopper 82a can stop the liquid to prevent the liquid from contacting the anti-permeation layer 70 sleeved on the first fixing member 81, thereby effectively avoiding the problem of the anti-permeation layer 70 separating from the barrier layer 60 due to the liquid penetrating into the anti-permeation layer 70. The anti-permeation layer 70 is mounted on the first fixing member 81 through the first fixing hole 71, so that when the anti-permeation layer 70 is subjected to circumferential force, the first fixing member 81 can pull the anti-permeation layer 70 to prevent the anti-permeation layer 70 from falling off due to impact.

[0079] Furthermore, in order to prevent the liquid from impacting along the first fixing member 81 toward the stopper 82a and infiltrating into the anti-permeation layer 70, thereby causing the anti-permeation layer 70 to separate from the barrier layer 60, a receiving groove 80a for receiving the anti-permeation layer 70 is provided between the first fixing member 81 and the stopper 82a, and a placement groove 80b communicating with the receiving groove 80a is formed between the first fixing member 81 and the fixing portion 82b. Preferably, the placement groove 80b is closer to the axis of the paper tube 100 than the receiving groove 80a. When the anti-permeation layer 70 is fixedly attached to the barrier layer 60, the first fixing hole 71 on the anti-permeation layer 70 is sleeved on the first fixing member 81, and the opening of the anti-permeation layer 70 is located in the receiving groove 80a. Therefore, when the liquid impacts the direction of the stopper 82a along the first fixing member 81, since the first fixing member 81 protrudes out of the barrier layer 60, the first fixing member 81 stops and weakens the impact force of the liquid, so that the liquid can only penetrate from the placement groove 80b to the containing groove 80a, and since the second fixing hole 821 is opened on the fixing part 82b, the liquid part entering from the placement groove 80b flows out through the second fixing hole 821. Due to the weakening of the impact force of the liquid, the reduction of the liquid volume, and the inability of the liquid to directly impact the opening of the anti-permeation layer 70, and the anti-permeation layer 70 is fixed on the barrier layer by hot pressing or gluing, the liquid cannot easily penetrate into the inner surface of the anti-permeation layer 70, thereby further increasing the tightness of the connection between the anti-permeation layer 70 and the barrier layer 60, and extending the service life of the paper tube 100. In addition, by setting the above-mentioned fixing structure 80, the paper tube 100 can be suitable for the placement of various liquid substances, thereby increasing the applicability of the paper tube 100.

[0080] Furthermore, the fixing part 82b is arranged parallel to the barrier layer 60, so that each part of the placement groove 80b is arranged at an equal interval, so that when the anti-permeation layer 70 is placed through the placement groove 80b, the problem of difficulty in placing the anti-permeation layer 70 due to the local narrowness of the placement groove 80b is avoided, the production difficulty of the paper tube 100 is reduced, the processing efficiency of the paper tube 100 is improved, and the labor cost is reduced. In one embodiment, the second fixing member 82 is made of a flexible material, such as rubber, so that in the process of pressing the anti-permeation layer 70 to the paper layer 100a through the first fixing member 81 and the second fixing member 82, it is easy to twist the second fixing member 82 to achieve the fixing or removal of the first fixing member 81 and the second fixing member 82.

[0081] See also Figure 8 In order to better prevent the anti-permeation layer 70 from being separated from the barrier layer 60 due to the impact force of the liquid in the paper tube 100, the anti-permeation layer 70 includes a first end 72 and a second end 73 arranged at opposite ends thereof. When the anti-permeation layer 70 is fixed to the fixing structure 80 on the second barrier layer 62, the anti-permeation layer 70 surrounds and adheres to the inner wall of the second barrier layer 62. The opposite end surfaces of the first end 72 and the second end 73 are respectively adhered to the opposite side surfaces of the stopper 82a, so that when the liquid in the paper tube 100 rotates, the rotating liquid directly impacts the stopper 82a, but cannot directly impact the opening surface of the first end 72 and the second end 73, thereby preventing the first end 72 and the second end 73 from being separated from the second barrier layer 62 due to the liquid impacting the opening of the first end 72 or the second end 73 and penetrating into the first end 72 and the second end 73.

[0082] Further, the first fixing hole 71 is formed on the first end portion 72, so that when the first end portion 72 is fixed to the second barrier layer 62, the first end portion 72 is inserted into the placement groove 80b, and the first fixing hole 71 on the first end portion 72 is sleeved on the first fixing member 81, so as to achieve the fixation of the first end portion 72. Preferably, when the first end portion 72 is fixed to the first fixing member 81, the length of the first end portion 72 protruding from the first fixing member 81 is equal to the length of the accommodating groove 80a, so that the opening of the first end portion 72 is completely attached to the stopper 82a, thereby preventing the liquid in the paper tube 100 from directly impacting the opening of the first end portion 72 and penetrating into the first end portion 72 when impacting along the first fixing member 81 toward the stopper 82a, thereby preventing the first end portion 72 from being separated from the second barrier layer 62.

[0083] Furthermore, the first end portion 72 has a fitting surface 71a surrounding the inner wall of the first fixing hole 71, and when the first fixing hole 71 is mounted on the first fixing component 81, the fitting surface 71a fits on the outer wall of the first fixing component 81, thereby avoiding the generation of a gap between the anti-permeability layer 70 and the first fixing component 81, and avoiding the problem of damage to the anti-permeability layer 70 due to long-term impact of liquid on the above gap.

[0084] In a specific embodiment, the first end portion 72 has a first surface 72a facing the second barrier layer 62, and the first end portion 72 has a second surface 72b facing the stopper 82a. Preferably, the first surface 72a is bonded to the second barrier layer 62 by glue, and the second surface 72b is bonded to the stopper 82a by glue, so that when the first end portion 72 is fixed to the second barrier layer 62, the first surface 72a is attached to the second barrier layer 62 and there is no gap between the first surface 72a and the second barrier layer 62, and the second surface 72b is attached to the stopper 82a and there is no gap between the stopper 82a. Therefore, when the paper tube 100 is shaken, the liquid in the paper tube 100 is prevented from penetrating through the above-mentioned gap to the bonding portion between the first surface 72a and the second barrier layer 62, and penetrating to the bonding portion between the second surface 72b and the stopper 82a, thereby preventing the anti-permeation layer 70 from separating from the second barrier layer 62.

[0085] Specifically, in the process of fixing the first end portion 72 to the second barrier layer 62, the first end portion 72 is first placed along the placement groove 80. When the end of the first end portion 72 faces the accommodation groove 80a, the first surface 72a is pressed against the second barrier layer 62 and the second surface 72b is pressed against the stopper 82a by extending the elongated needle into the fixing structure 80. Preferably, glue is applied on the first surface 72a and the second surface 72b so that the first surface 72a is fixed to the second barrier layer 62 and the second surface 72b is fixed to the stopper 82a.

[0086] Furthermore, the second end portion 73 has a third surface 73a facing the second barrier layer 62 and a fourth surface 73b facing the stopper 82a. Preferably, when the second end portion 73 is fixed to the second barrier layer 62, the third surface 73a is attached to the second barrier layer 62 and there is no gap between the third surface 73a and the second barrier layer 62, and the fourth surface 73b is attached to the stopper 82a and there is no gap between the fourth surface 73b and the stopper 82a, so as to prevent the problem that the second end portion 73 is separated from the second barrier layer 62 due to liquid penetrating into the above-mentioned gap.

[0087] Furthermore, the barrier layer 60 is provided with a fold 60a, and the barrier layer 60 can be folded along the fold 60a to form a first barrier layer 61 and a second barrier layer 62 which are stacked on each other. The first barrier layer 61 is attached to the inner wall of the paper layer 100a, and the fixing structure 80 is arranged on the inner wall of the second barrier layer 62. Furthermore, the first barrier layer 61 and the second barrier layer 62 are made of elastic plastic material. It should be noted that, please refer to Figure 7 The above scheme is to fold the barrier layer 60 along the crease 60a to form a first barrier layer 61 and a second barrier layer 62 which are stacked on each other, and use elastic plastic material to make the above first barrier layer 61 and the second barrier layer 62, so that when the first barrier layer 61 and the second barrier layer 62 are folded along the crease 60a, the first barrier layer 61 and the second barrier layer 62 have the property of restoring their original state, that is, elastic deformation ability, so that the first barrier layer 61 is subjected to a force away from the axis of the paper tube 100, that is, F2 in the figure, and the second barrier layer 62 is subjected to a force toward the axis of the paper tube 100, that is, F1 in the figure. When the paper tube 100 is deformed by external or internal force, the first barrier layer 61 or the second barrier layer 62 located at the deformed position pushes the paper layer 100a outward or inward under the action of its own elastic force to restore the original state, thereby preventing the paper tube 100 from being damaged or affecting its aesthetics due to deformation of its appearance caused by impact or internal extrusion.

[0088] Furthermore, the paper tube 100 further includes an adhesive layer 90, which is disposed on the first barrier layer 61, and the first barrier layer 61 is adhered to the inner wall of the paper layer 100a through the adhesive layer 90. Preferably, the adhesive layer 90 is a glue layer.

[0089] Furthermore, the stop portion 82a is arranged at the position of the above-mentioned fold 60a to limit the position where the adhesive layer 90 is applied when it is applied to the first barrier layer 61, thereby preventing the adhesive layer 90 from being applied to the corner between the first barrier layer 61 and the second barrier layer 62 after folding, thereby preventing the adhesive layer 90 from being wasted. This saves material usage and reduces production costs.

[0090] It should be noted that the bonding area between the first barrier layer 61 and the paper layer 100a is the area where the first barrier layer 61 and the paper layer 100a face each other. When the first barrier layer 61 is partially flipped and is not facing the paper layer, the adhesive layer 90 coated on the first barrier layer 61 cannot contact and bond with the paper layer 100a.

[0091] In one embodiment, the barrier layer 60 is detachably disposed in the inner cavity of the tube body 10, so that after packaging food or cosmetics, the barrier layer 60 can be taken out from the inner cavity of the tube body 10 and replaced to achieve the reuse of the paper tube 100, thereby reducing the use cost of the paper tube 100. In addition, the small amount of use of the paper tube 100 reduces the abuse of resources, saves energy, and purifies the environment.

[0092] Furthermore, the barrier layer 60 and the multi-layer paper layer 100a are made of elastic materials, so that when the paper tube 100 is small in size, the material placed in the tube body 10 can be squeezed out by squeezing the tube body 10, thereby increasing the comfort of the user. After squeezing, the tube body 10 and the barrier layer 60 disposed in the inner cavity of the tube body 10 can also recover under the effect of their own elasticity, thereby facilitating the next use of the paper tube 100, better reducing the use of the paper tube 100, better saving resources, and purifying the environment.

[0093] The above scheme applies the first heat-seal coating 30 to the outer edges of the first region 10a and the second region 20a along the width direction of the paper layer 100a, so that when the multi-layer paper layer 100a is wound on the heated core, the heated core solidifies the first heat-seal coating 30 located at the outer edges of the first region 10a and the second region 20a so that the multi-layer paper layers 100a are tightly bonded to each other, thereby bonding and fastening the multi-layer paper layers 100a at the openings at the upper and lower ends of the formed paper tube 100, thereby preventing the paper layers 100a from being damaged and separated due to the upper and lower ends of the paper tube 100 being exposed to the air. In addition, along the width direction of the paper layer 100a, the width of the first heat-seal coating 30 is set to 2mm-5mm, so as to ensure that the first heat-seal coating 30 is applied to the entire range of the paper layer 100a, under the premise of ensuring that the two adjacent paper layers 100a are bonded and fastened, thereby reducing the cost.

[0094] The above is only an implementation method of the present application. It should be pointed out that a person skilled in the art can make improvements without departing from the inventive concept of the present application, but these improvements are within the scope of protection of the present application.

Claims

1. A flat paper tube, characterized in that: It comprises at least two layers of paper rolled flat; Any of the paper layers comprises a first region for winding to form the paper tube body, and a second region for winding to form the paper tube end cap; Wherein, along the width direction of the paper layer, the first area and the second area are coated with a first heat-sealing coating at the opposite outer edges, so that when the multiple paper layers are wound on the heated core, the first heat-sealing coating can seal the outer wall of the paper tube; The second region has a first side extending outwardly from the first region; The second region is coated with a second heat-sealing coating at the position of the first side edge, and the second heat-sealing coating is used to adhere the first side edge to the tube body of the wound paper tube; The paper tube further comprises a barrier layer wound around the inner layer of the paper tube and an anti-permeation layer detachably wound around the inner layer of the barrier layer; A fixed structure is provided on the side of the barrier layer facing away from the paper layer, and the anti-permeability layer is sleeved on the fixed structure and wound around the inner layer of the barrier layer according to the fixed structure; The fixing structure includes a first fixing member and a second fixing member protruding from the barrier layer; the anti-permeability layer is provided with a first fixing hole, and the anti-permeability layer is sleeved on the first fixing member through the first fixing hole; the second fixing member is provided with a second fixing hole, and the second fixing member is sleeved on the first fixing member through the second fixing hole, so as to press the anti-permeability layer onto the inner wall of the barrier layer; The second fixing member includes a stopper portion provided on the barrier layer and a fixing portion provided on the stopper portion; the stopper portion and the fixing portion surround the first fixing member; The anti-permeation layer includes a first end portion and a second end portion provided at opposite ends thereof, and the opposite end surfaces of the first end portion and the second end portion are respectively attached to the opposite side surfaces of the stopper portion; The barrier layer is provided with a fold; the barrier layer can be folded along the fold to form a first barrier layer and a second barrier layer stacked on each other; the first barrier layer is attached to the inner wall of the paper layer, and the fixing structure is arranged on the inner wall of the second barrier layer; A receiving groove for receiving the anti-permeation layer is arranged between the first fixing member and the stopper, and a placement groove communicating with the receiving groove is formed between the first fixing member and the fixing member, and the placement groove is closer to the axis of the paper tube than the receiving groove. When the anti-permeation layer is fixedly attached to the barrier layer, the first fixing hole on the anti-permeation layer is sleeved on the first fixing member, and the opening of the anti-permeation layer is located in the receiving groove, so that when the liquid impacts the direction of the stopper along the first fixing member, the first fixing member protrudes out of the barrier layer, and the first fixing member stops and weakens the impact of the liquid, so that the liquid penetrates from the placement groove to the receiving groove, and the second fixing hole is opened on the fixing member so that the liquid part entering the placement groove flows out through the second fixing hole; The first fixing hole is opened on the first end portion, so that when the first end portion is fixed on the second barrier layer, the first end portion is extended into the placement groove, and the first fixing hole on the first end portion is sleeved on the first fixing member to achieve the fixation of the first end portion. When the first end portion is fixed on the first fixing member, the length of the first end portion protruding from the first fixing member is equal to the length of the accommodating groove, so that the opening portion of the first end portion is completely fitted on the stopper, thereby preventing the liquid in the paper tube from directly impacting the opening portion of the first end portion and penetrating into the first end portion when impacting along the first fixing member toward the stopper, thereby preventing the first end portion from being separated from the second barrier layer.

2. The flat roll paper tube according to claim 1, characterized in that: The ratio of the length of the first side to the width of the paper layer is 1 / 20-2 / 3.

3. The flat roll paper tube according to claim 1, characterized in that: The first region has a second side edge extending outwardly from the first side edge; The first region is coated with a third heat-sealing coating at the second side edge position, which is used to adhere the second side edge to the tube body of the wound paper tube.

4. The flat roll paper tube according to claim 3, characterized in that: The ratio of the second side edge to the length of the paper layer is 1 / 2-2 / 3.

5. The flat roll paper tube according to claim 1, characterized in that: The second fixing member is made of a flexible material.

6. The flat roll paper tube according to claim 1, characterized in that: The first barrier layer and the second barrier layer are made of elastic plastic material.