A sample test piece fixing device for corrosion test

By designing a sample test piece fixing device for power plant site, and using the cooperation of slider components and support components, the stable fixation of metal test piece in a high-temperature and high-pressure steam environment is achieved, and the problem of difficulty in fixing test piece on power plant site is solved. Real experimental data are provided and the risk of failure caused by scale is reduced.

CN115672433BActive Publication Date: 2024-11-15XIAN THERMAL POWER RES INST CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211020013.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-08-24
Publication Date
2024-11-15
Estimated Expiration
2042-08-24

AI Technical Summary

Technical Problem

At the power plant site, it is difficult to fix the metal test piece in a high-speed flowing high-temperature and high-pressure steam environment, making it difficult to perform oxidation and corrosion experiments.

Method used

A sample test piece fixing device including a main rod, a slider assembly, a support assembly and a support frame is designed. Through the cooperation of the slider assembly and the support assembly, the top rod slides radially along the main rod and abuts with the inner wall of the pipe, and combines the Support frame fixing device to achieve stable fixation of sample test pieces.

Benefits of technology

The device can fix the sample test piece in a high-speed flowing high-temperature and high-pressure steam environment to avoid swing or collision, provide real experimental data on power plant conditions, reduce the probability of failure caused by scale, and is cheap and easy to operate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115672433B_ABST
    Figure CN115672433B_ABST
Patent Text Reader

Abstract

The invention discloses a sample test piece fixing device for corrosion experiments, comprising a main rod, and a slider assembly, a support assembly and a support frame arranged thereon; a plurality of sample test pieces are fixed on the column rod and located between the support assembly and the support frame, a plurality of push rods are evenly distributed circumferentially on the support assembly, the slider assembly is connected to the support assembly, the slider assembly moves along the axial direction of the main rod so that the end of the push rod abuts against the inner wall of the pipeline, the push rod is driven radially to move by sliding, and the entire fixing device is fixed in combination with the support frame, the fixing device can adjust the contact pressure between the push rod and the pipe wall through the slider assembly, and the fixing device can adapt to pipelines of different diameters, the sample test piece is fixed by the fixing device so that it will not swing or collide under the flushing of high-temperature and high-pressure steam flowing at high speed, which is of great significance for studying the anti-oxidation corrosion performance of metal materials and reducing the probability of accidents caused by oxide scale.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the research field of high-temperature oxidation corrosion of metal materials, and in particular to a sample test piece fixing device used for corrosion experiments. Background Art

[0002] In order to reduce environmental pollution, reduce greenhouse gas emissions, and improve the power generation efficiency of coal-fired power generating units, most coal-fired power plants adopt the method of increasing steam pressure and temperature parameters to improve the power generation efficiency of thermal power units. However, with the increase of steam pressure and temperature, the boilers, turbines and other systems of power plant units have been in service for a long time under high temperature and high pressure steam environment. The reheater tubes, turbine valve stems, valve sleeves and other components are very easy to be oxidized and corroded, and a thick oxide layer is formed on the metal surface. In addition, the oxide scale on the inner wall of the boiler reheater tube is very easy to peel off and cause problems such as steam pipe blockage, overheating, pipe burst, and turbine main steam valve jamming and solid particle erosion (SPE). Therefore, studying the generation and peeling mechanism of oxide scale is of great significance to reducing a series of problems caused by oxide scale shedding in power plants.

[0003] At present, the research on the high-temperature oxidation corrosion resistance of metal materials is mostly carried out in the laboratory. The experimental conditions are quite different from the actual conditions of the power plant, which has a great impact on the formation and peeling of oxide scale on the surface of metal materials. Therefore, it is of great significance to carry out oxidation corrosion experiments on metal materials on-site in the power plant. However, in the actual operating environment of the power plant, high-temperature and high-pressure steam flows at high speed in the boiler reheater pipe, which has a great impact on the metal test piece and is difficult to fix. Summary of the invention

[0004] In view of the problems existing in the prior art, the present invention provides a sample test piece fixing device for corrosion experiments to solve the problem in the prior art that the test piece cannot be fixed in a pipeline with high-speed flowing high-temperature and high-pressure steam.

[0005] The present invention is achieved through the following technical solutions:

[0006] A sample test piece fixing device for a corrosion experiment comprises a main rod, a slider assembly, a support assembly and a support frame;

[0007] The support assembly and the support frame are arranged on the main rod at intervals along the axial direction of the main rod. A plurality of sample test pieces are sleeved on the main rod at intervals and are located between the support assembly and the support frame. A plurality of push rods are evenly distributed on the circumference of the support assembly. The slider assembly is sleeved on the column rod and is located in the slide groove of the support assembly. The lower end of the push rod is connected to the slider assembly. When the slider assembly moves in the slide groove along the axial direction of the main rod, the push rod can slide radially along the main rod and abut against the inner wall of the pipe.

[0008] Preferably, the support assembly comprises a fixing plate and a support rod;

[0009] The fixed plate is fixedly sleeved on the main rod, and multiple support rods are arranged circumferentially along the radial direction of the pipeline and are evenly distributed on the side wall of the fixed plate. The support rod is provided with a mandrel hole coaxial with the mandrel, and the mandrel is installed in the mandrel hole. A slide groove is provided at the lower end of each support rod, and the upper end of the slide groove is connected with the mandrel hole. The slider assembly is sleeved on the column rod and is located in multiple slide grooves.

[0010] Preferably, the slider assembly comprises a wedge-shaped slider and a connecting plate;

[0011] The top surface of the wedge-shaped slider is an inclined surface and is inclined along the axial direction of the main rod. Multiple wedge-shaped sliders are evenly distributed on the main rod and installed in the slide groove. The connecting plate is sleeved on the column rod and is located at the end of the wedge-shaped slider away from the sample test piece. The end surface of the connecting plate is fixedly connected to the ends of the multiple wedge-shaped sliders.

[0012] Preferably, the wedge-shaped sliding block is connected to the lower end of the push rod via a sliding groove.

[0013] Preferably, the slide groove is a T-shaped groove.

[0014] Preferably, a spring is sleeved on the main rod, and the spring is located on a side of the fixing plate close to the sample test piece. One end of the spring close to the sample test piece is fixedly connected to the main rod, and the other end of the spring abuts against the end of the wedge-shaped slider.

[0015] Preferably, a threaded sleeve is also provided on the main rod, which is connected to the main rod through an internal thread and is located at the end of the slider assembly.

[0016] Preferably, the support frame includes a fixed connecting plate and support legs, the fixed connecting plate is mounted on the main rod by a threaded sleeve, a plurality of support legs are evenly distributed circumferentially on the edge of the fixed connecting plate, one end of the support leg is fixedly connected to the side wall of the fixed connecting plate, and the other end extends radially along the pipe.

[0017] Preferably, a ball screw is embedded in the end of the supporting leg, and the ball screw is used to abut against the inner wall of the pipe.

[0018] Preferably, a sleeve is provided between two adjacent sample test pieces.

[0019] Compared with the prior art, the present invention has the following beneficial technical effects:

[0020] The present invention provides a sample specimen fixing device for corrosion experiments, comprising a main rod, and a slider assembly, a support assembly and a support frame arranged thereon; a plurality of sample specimens are fixed on the column rod and located between the support assembly and the support frame, a plurality of push rods are evenly distributed circumferentially on the support assembly, the slider assembly is connected to the support assembly, the slider assembly moves along the axial direction of the main rod so that the end of the push rod abuts against the inner wall of the pipeline, the push rod is driven to move radially by sliding, and the entire fixing device is fixed in combination with the support frame, the fixing device can adjust the contact pressure between the push rod and the pipe wall through the slider assembly, and the fixing device can adapt to pipelines of different diameters, the sample specimen is fixed by the fixing device, so that it will not swing or collide under the flushing of high-speed high-temperature and high-pressure steam, and valuable experimental data of metal materials after operation under actual working conditions of power plants can be obtained. The fixing device has low cost, simple operation, and is easy to manufacture, and is of great significance for studying the anti-oxidation corrosion performance of metal materials and reducing the probability of accidents caused by oxide scale. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 It is a schematic diagram of the structure of the fixing device of the present invention;

[0022] Figure 2 is a cross-sectional view of a support assembly of the present invention;

[0023] Figure 3 It is a structural schematic diagram of the front support frame of the present invention;

[0024] Figure 4 It is a schematic diagram of the connection between the wedge-shaped slider and the push rod of the present invention;

[0025] Figure 5 It is a structural schematic diagram of the slider assembly of the present invention;

[0026] Figure 6 It is a front view of the rear support frame of the present invention;

[0027] Figure 7 It is a side view of the rear support frame of the present invention.

[0028] In the figure: 1. pipe; 2. threaded sleeve; 3. slider assembly; 4. support assembly; 5. spring; 6. sample specimen; 7. sleeve; 8. main rod; 9. support frame; 10. ball screw; 41. fixing plate; 42. support rod; 43. push rod; 44. wedge-shaped slider; 45. push rod hole; 46. slide groove; 47. connecting plate. DETAILED DESCRIPTION

[0029] The present invention will be further described in detail below in conjunction with the accompanying drawings, which are intended to explain the present invention rather than to limit it.

[0030] See also Figure 1-7A sample specimen fixing device for a corrosion experiment includes a main rod 1, a slider assembly 3, a support assembly 4 and a support frame 9.

[0031] The support assembly 4 and the support frame 9 are arranged on the main rod 1 at intervals along the axial direction of the main rod. A plurality of sample test pieces 6 are sleeved on the main rod 1 at intervals and are located between the support assembly 4 and the support frame 9. A plurality of push rods 43 are evenly distributed on the circumference of the support assembly 4. The slider assembly 3 is sleeved on the column rod and is located in the slide groove of the support assembly 4. The lower end of the push rod is connected to the slider assembly 3. When the slider assembly 3 moves in the slide groove along the axial direction of the main rod, the push rod can slide radially along the main rod and abut against the inner wall of the pipe.

[0032] The support assembly includes a fixed plate 41 and a support rod 42. The fixed plate 41 is annular and fixedly sleeved on the main rod 1. Multiple support rods are arranged circumferentially along the radial direction of the pipeline and are evenly distributed on the side wall of the fixed plate. The support rod is provided with a mandrel hole 45 coaxial with the mandrel. The mandrel 43 is installed in the mandrel hole 45. A slide groove 46 is provided at the lower end of each support rod 42 and passes through the fixed plate. The upper end of the slide groove is connected to the mandrel hole, and the lower end of the slide groove passes through the inner ring wall of the fixed plate. The slider assembly 3 is sleeved on the column rod and is located in multiple slide grooves.

[0033] The slider assembly 3 includes a wedge-shaped slider 44 and a connecting plate 47. The top surface of the wedge-shaped slider 44 is an inclined surface and is inclined along the axial direction of the main rod. It is located at one end of the sample test piece near the center of the main rod. The number of wedge-shaped sliders 44 is the same as the number of slide grooves. Multiple wedge-shaped sliders 44 are evenly distributed on the main rod and installed in the slide groove. The connecting plate 47 is sleeved on the column rod and is located at one end of the wedge-shaped slider 44 away from the sample test piece 6. The end surface of the connecting plate 47 is fixedly connected to the end of the multiple wedge-shaped sliders; the multiple wedge-shaped sliders 44 are connected by the connecting plate 47 to form a slide groove assembly, so that the multiple wedge-shaped sliders 44 can be moved synchronously, and the multiple push rods can be controlled synchronously so that the multiple push rods are simultaneously in contact with the inner wall of the pipeline, thereby ensuring the stability of the fixing device in the pipeline and avoiding movement under the impact of high-speed airflow.

[0034] The top surface of the wedge-shaped slide is provided with a T-slot, and the lower end of the push rod is provided with a T-block that cooperates with it. The lower end of the push rod is connected to the wedge block slider through the T-block, so that the push rod can be driven to reciprocate radially along the pipeline through the wedge-shaped slider.

[0035] The main rod is also provided with a threaded sleeve 2, which is connected to the main rod through an internal thread and is located at the end of the connecting plate 47. The main rod is also provided with a spring 5, which is located on the side of the fixing plate 41 close to the sample specimen 6. One end of the spring close to the sample specimen 6 is fixedly connected to the main rod, and the other end of the spring abuts against the end of the wedge-shaped slider. When the threaded sleeve 2 rotates and moves toward the sample specimen 6, a thrust is applied to the wedge-shaped slider to make it move synchronously. During the movement of the wedge-shaped slider, the spring is compressed, and at the same time, the lower end of the push rod gradually moves along the inclined surface of the wedge-shaped slider. Under the action of the inclined surface, the push rod moves along the radial direction of the main rod toward the inner wall of the pipeline 1 until the end of the push rod extends out of the support rod 42 for a certain length and abuts against the inner wall of the pipeline, thereby fixing the entire fixing device to the pipeline.

[0036] Both ends of the spring are provided with positioning plates, which are sleeved on the column rod. The positioning plate close to the sample specimen 6 is fixedly connected to the main rod, and the other positioning plate is slidably connected to the main rod. The end of the wedge-shaped slider abuts against the end face of the positioning plate, which can effectively ensure that the forces on multiple wedge-shaped sliders are the same. After the test is completed, the threaded sleeve 2 is loosened and the spring is reset. Under the action of the elastic force, the slider assembly 3 moves in the opposite direction, and the push rod is separated from the inner wall of the pipe through the T-block.

[0037] The support frame 9 is detachably connected to the main rod to realize the installation of the sample specimen 6 on the main rod. The support frame 9 includes a fixed connecting plate and support legs. The fixed connecting plate is mounted on the main rod 1 through a threaded sleeve. A plurality of support legs are evenly distributed around the edge of the fixed connecting plate. One end of the support leg is fixedly connected to the side wall of the fixed connecting plate, and the other end extends radially along the pipeline. It should be noted that the free ends of the plurality of support legs form a radius slightly smaller than the inner diameter of the pipeline. A ball screw 10 is embedded in the end of the support leg. The diameter formed by the balls of the plurality of ball screws 10 is larger than the inner wall of the pipeline. The support frame 9 is supported in the pipeline by the ball screw 10, and then combined with the support assembly 4 to realize the fixation of the entire device.

[0038] In this embodiment, the number of the support rods 42 and the number of the support legs on the support assembly 4 and the support frame 9 are both three.

[0039] See also Figure 1 Six sample test pieces 6 are sleeved on the main rod, and a sleeve 7 is set between two adjacent sample test pieces. The sleeve is sleeved on the main rod, and the two sleeves at both ends are fixedly connected to the main rod in a detachable manner to ensure that the sample test pieces are in a stable state on the main rod during the corrosion test.

[0040] The following is a detailed description of the method for using a sample test piece fixing device for a corrosion experiment provided by the invention, as follows:

[0041] Step 1: Separate the support frame from the main rod, and put the sample specimen 6 and the sleeve on the main rod in sequence. During the installation process, ensure that the sample specimen 6 and the sleeve are in close contact with each other, and weld the two sleeves at both ends to the main rod to prevent the sample specimen from moving under high-speed airflow, and then install the support frame at the end of the main rod.

[0042] Step 2: Install the fixture obtained in step 1 into the pipeline 1.

[0043] First, insert one end of the support frame of the fixing device into the pipe, and make the ball of the ball screw abut against the inner wall of the pipe until the support assembly enters the pipe.

[0044] Then, rotate the threaded sleeve to move it along the axial direction of the main rod and move it toward the direction of the sample specimen. The threaded sleeve drives the slider assembly to move synchronously, and the wedge-shaped slider drives the push rod to move toward the inside of the pipe until the end of the push rod abuts against the inside of the pipe. At this time, the spring is compressed, and the two ends of the main rod are supported in the pipe by the support assembly and the support frame. It should be noted that the support frame plays an auxiliary supporting role to prevent the radial shaking of the main rod. The pressure applied by the wedge-shaped slider to make the end of the push rod of the support assembly abut against the inner wall of the pipe is the core of realizing the fixation of the entire fixing device to the pipe.

[0045] During the installation process, the threaded sleeve is located at the mouth of the pipe, which makes it easy to rotate it using tools to achieve the fixing and removal of the fixture. After the fixture is fixed to the pipe, the pipe is reset and fixed by welding to ensure the air tightness of the pipe.

[0046] The above contents are only for explaining the technical idea of ​​the present invention and cannot be used to limit the protection scope of the present invention. Any changes made on the basis of the technical solution in accordance with the technical idea proposed by the present invention shall fall within the protection scope of the claims of the present invention.

Claims

1. A sample specimen fixing device for a corrosion test, characterized in that: It comprises a main rod (8), a slider assembly (3), a support assembly (4) and a support frame (9); The support assembly (4) and the support frame (9) are arranged on the main rod (8) at intervals along the axial direction of the main rod; a plurality of sample test pieces (6) are sleeved on the main rod (8) at intervals and are located between the support assembly (4) and the support frame (9); a plurality of push rods (43) are evenly distributed on the circumference of the support assembly (4); the slider assembly (3) is sleeved on the main rod and is located in the slide groove of the support assembly (4); the lower end of the push rod is connected to the slider assembly (3); when the slider assembly (3) moves in the slide groove along the axial direction of the main rod, the push rod can slide along the radial direction of the main rod and abut against the inner wall of the pipe; The support assembly comprises a fixing plate (41) and a support rod (42); The fixing plate (41) is fixedly sleeved on the main rod (8), and a plurality of support rods are arranged circumferentially and evenly distributed on the side wall of the fixing plate along the radial direction of the pipeline. A mandrel hole (45) coaxial with the mandrel is provided in the support rod, and the mandrel (43) is installed in the mandrel hole (45). A slide groove (46) is provided at the lower end of each support rod (42), and the upper end of the slide groove is connected to the mandrel hole. The slider assembly (3) is sleeved on the main rod and is located in the plurality of slide grooves; The slider assembly (3) comprises a wedge-shaped slider (44) and a connecting plate (47); The top surface of the wedge-shaped slider (44) is an inclined surface and is inclined along the axial direction of the main rod. A plurality of wedge-shaped sliders (44) are evenly distributed on the main rod and installed in the slide groove. The connecting plate (47) is sleeved on the main rod and is located at one end of the wedge-shaped slider (44) away from the sample test piece (6). The end surface of the connecting plate (47) is fixedly connected to the ends of the plurality of wedge-shaped sliders. The main rod is also sleeved with a spring (5), which is located on a side of the fixed plate (41) close to the sample test piece (6), one end of the spring close to the sample test piece (6) is fixedly connected to the main rod, and the other end of the spring abuts against the end of the wedge-shaped slider; The main rod is also provided with a threaded sleeve (2), which is connected to the main rod through an internal thread and is located at the end of the slider assembly; The support frame (9) comprises a fixed connection plate and support legs. The fixed connection plate is mounted on the main rod (8) by means of a threaded sleeve. A plurality of support legs are evenly distributed around the edge of the fixed connection plate. One end of the support leg is fixedly connected to the side wall of the fixed connection plate, and the other end extends radially along the pipeline. A ball screw (10) is embedded at the end of the support leg, and the ball screw is used to abut against the inner wall of the pipeline.

2. A sample specimen fixing device for corrosion test according to claim 1, characterized in that: The wedge-shaped sliding block is connected to the lower end of the push rod through a sliding groove.

3. A sample specimen fixing device for corrosion test according to claim 2, characterized in that: The slide groove is a T-shaped groove.

4. A sample specimen fixing device for corrosion test according to claim 1, characterized in that: A sleeve (7) is arranged between two adjacent sample test pieces.