Electrolytic cell ratio solvent for measuring water content of rubber and NMP mixture by volumetric method
By using a solvent mixed with anhydrous methanol and xylene in a ratio of 7:3, combined with the reaction analysis of Karl Fischer reagent, the problem of inaccurate measurement of the moisture content of hydrogenated nitrile rubber in the lithium battery cathode slurry was solved, achieving a more accurate Moisture measurement and simplified preparation process.
Patent Information
- Application Number
- CN202211554266.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-12-06
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2042-12-06
AI Technical Summary
In the existing technology, when measuring the moisture content of hydrogenated nitrile rubber in the lithium battery cathode slurry, the solvent reacts with water or acid, causing the measurement to fail and the volumetric measurement to be inaccurate.
Use anhydrous methanol and xylene mixed in a ratio of 7:3 as the solvent, and automatically analyze the moisture content through the Karl Fischer reagent reaction to ensure measurement accuracy.
The accurate measurement of the moisture content of hydrogenated nitrile rubber is achieved, the preparation process is simplified, and the accuracy and practicality of the measurement are improved.
Abstract
Description
Technical Field
[0001] The invention relates to an electrolytic cell proportioning solvent, in particular to an electrolytic cell proportioning solvent for measuring the water content of a rubber and NMP mixed liquid by a volumetric method. Background Art
[0002] There are two methods for measuring moisture: volumetric method and coulometric method. The coulometric method is very effective for measuring low-content moisture and will not react with Karl Fischer reagent to precipitate other substances. The volumetric method has a good quantitative effect on measuring the moisture content of some rubber products that are not very soluble. Lithium battery positive electrode slurry has strict requirements on moisture content. Having a method to measure its moisture content has a certain supporting role in production process control and parameter adjustment.
[0003] ARC-080A is made of N-methylpyrrolidone (NMP) dissolved hydrogenated nitrile rubber (H-NBR) to make additive slurry, which is sold to lithium battery manufacturers for the homogenization and dispersion of positive electrode materials and conductive agents (CNT and other materials) to improve production efficiency, save energy and reduce emissions. In the production process, the water content is measured by the volumetric method. During the measurement, the solute in the solvent will cause the solute (H-NBR) to precipitate when it encounters water or acid, resulting in measurement failure.
[0004] In summary, the present invention provides an electrolytic cell proportioning solvent for measuring the water content of a mixture of rubber and NMP by a volumetric method. Summary of the invention
[0005] In view of the deficiencies in the prior art, the present invention aims to provide an electrolytic cell ratio solvent for measuring the moisture content of a rubber and NMP mixture by a volumetric method. The preparation method is simple. A solution prepared by selecting xylene and anhydrous methanol can be used as a dissolving solvent of the electrolytic cell. When ARC-080A is injected into the electrolytic cell, it is first dissolved and dispersed, and then water molecules enter the electrolytic cell and react with the Karl Fischer reagent that automatically enters. The instrument automatically analyzes the moisture content of ARC-080A according to the amount of Karl Fischer reagent added, and the measurement result is more accurate.
[0006] In order to achieve the above object, the present invention is implemented through the following technical scheme: the electrolytic cell ratio solvent for measuring the water content of the rubber and NMP mixture by volumetric method includes the following components in the following ratio: anhydrous methanol: xylene = 7:3.
[0007] The method for preparing an electrolytic cell ratio solvent for measuring the water content of a rubber and NMP mixed solution by a volumetric method comprises the following steps:
[0008] 1. Prepare a mixture of anhydrous methanol and xylene: prepare a mixed solution of anhydrous methanol and xylene in a fume hood at a ratio of 7:3;
[0009] 2. Pre-treatment:
[0010] Measure the amount of mixed solvent suitable for instrument titration and add it to the electrolysis bottle, turn on the stirring rotor and set the appropriate speed. Wait for the instrument to automatically inject Karl Fischer reagent so that the display interface is lower than 20ul / min and an alarm prompts that the test environment is stable, then enter the calibration stage;
[0011] 3. Calibration:
[0012] After the instrument is stable, inject 1 microliter of pure water. If the instrument automatically analyzes the water content and it is about 1000000ppm, the calibration is considered successful.
[0013] 4. Measurement:
[0014] Weigh an appropriate amount of sample (0.5g-1g), then quickly inject the sample from the injection port, open the sample editing box, enter the sample mass on the numeric keypad, start pre-titration and display the curve, display the result after the titration, repeat the sample 3 times to get the moisture content of the measured sample.
[0015] The capacity of the electrolytic bottle is 50-75 ml.
[0016] Beneficial effects of the present invention: The preparation method of the present invention is simple, and a mixture of NMP and hydrogenated nitrile rubber (H-NBR) can be dissolved and dispersed evenly in a mixed solution of xylene and anhydrous methanol in a ratio of 7:3, and then the water content (ppm) of the solution can be calculated by injecting the volume of Karl Fischer reagent under stirring at a certain speed, so that the measurement is more accurate and practical. DETAILED DESCRIPTION
[0017] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods.
[0018] This specific implementation adopts the following technical solution: the electrolytic cell ratio solvent for measuring the water content of the rubber and NMP mixture by volumetric method includes the following components in the following ratio: anhydrous methanol: xylene = 7:3.
[0019] The method for preparing an electrolytic cell ratio solvent for measuring the water content of a rubber and NMP mixed solution by a volumetric method comprises the following steps:
[0020] 1. Prepare a mixture of anhydrous methanol and xylene: prepare a mixed solution of anhydrous methanol and xylene in a fume hood at a ratio of 7:3;
[0021] 2. Pre-treatment:
[0022] Measure the amount of mixed solvent suitable for instrument titration and add it into the electrolysis bottle (50-75) ml, turn on the stirring rotor and set the appropriate speed. After the instrument automatically injects Karl Fischer reagent so that the display interface is lower than 20ul / min and an alarm prompts that the test environment is stable, you can enter the calibration stage;
[0023] 3. Calibration:
[0024] After the instrument is stable, inject 1 microliter of pure water. If the instrument automatically analyzes the water content and it is about 1000000ppm, the calibration is considered successful.
[0025] 4. Measurement:
[0026] Weigh an appropriate amount of sample (0.5g-1g), then quickly inject the sample from the injection port, open the sample editing box and enter the sample mass on the numeric keypad, start pre-titration and display the curve, display the result after the titration, repeat the sample 3 times to get the moisture content of the measured sample.
[0027] In this specific embodiment, a mixture of anhydrous methanol and xylene in a ratio of 7:3 can be used to dissolve and disperse a mixture of NMP and hydrogenated nitrile rubber (H-NBR) evenly, and then the water content (ppm) of the solution can be calculated by injecting the volume of Karl Fischer reagent under stirring at a certain speed. The preparation method is simple, the measurement result is more accurate, and the practicability is strong.
[0028] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. The electrolytic cell ratio solvent for measuring the water content of the rubber and NMP mixture by volumetric method is characterized in that: The composition comprises the following components in the following ratio: anhydrous methanol: xylene = 7:3, and the preparation method thereof comprises the following steps: (1) Prepare a mixed solution of anhydrous methanol and xylene: prepare a mixed solution of anhydrous methanol and xylene in a ratio of 7:3 in a fume hood; (2) Pre-treatment: Measure the amount of mixed solvent suitable for instrument titration and add it to the electrolysis bottle, turn on the stirring rotor and set the appropriate speed. Wait for the instrument to automatically inject Karl Fischer reagent so that the display interface is lower than 20ul / min and an alarm prompts that the test environment is stable, then enter the calibration stage; (3) Calibration: After the instrument is stable, inject 1 microliter of pure water. If the instrument automatically analyzes the water content and it is about 1000000ppm, the calibration is considered successful. (4) Measurement: Weigh an appropriate amount of sample (0.5g-1g), then quickly inject the sample from the injection port, open the sample editing box, enter the sample mass on the numeric keyboard, start pre-titration and display the curve, and display the result after the titration. Repeat the sample 3 times to get the moisture content of the measured sample. The capacity of the electrolytic bottle is 50-75 ml.
Citation Information
Patent Citations
Method for detecting moisture of ethylene sulfate
CN113671110A
Predispersant composition, and electrode and secondary battery including the same
CN114174384A