A method and device for preparing anhydrous calcium chloride by autocatalytic coupling dehydration of carbon-containing mixed gas and hydrated calcium chloride

By using the self-catalytic coupling and dehydration method of carbon-containing mixture and hydrated calcium chloride under low temperature conditions, the problem of high energy consumption of the anhydrous calcium chloride preparation process is solved, and an efficient and low-cost preparation of anhydrous calcium chloride is achieved. It also provides new ways of hydrogen, improving economic benefits and industrial application value.

CN116395732BActive Publication Date: 2024-11-12BEIJING UNIV OF CHEM TECH +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310376819.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-04-11
Publication Date
2024-11-12
Estimated Expiration
2043-04-11

AI Technical Summary

Technical Problem

The existing anhydrous calcium chloride preparation process has high energy consumption, resulting in high production costs and little economic benefits, and lack of effective preparation methods under low temperature conditions.

Method used

The self-catalytic coupling and dehydration method of carbon-containing mixed gas and hydrated calcium chloride is adopted. By conducting an autocatalytic reaction under low temperature conditions, the dehydration temperature of calcium chloride is reduced, and the carbon-containing gas in the hydrogen production industry is used to carry out coupling reaction. High purity anhydrous calcium chloride and hydrogen gas are produced.

Benefits of technology

It greatly reduces the production temperature and energy consumption of anhydrous calcium chloride, improves economic benefits, and provides a new channel to remove CO from industrial exhaust gas, and prepares high-purity anhydrous calcium chloride and hydrogen to meet industrial needs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004170676580000051
    Figure BDA0004170676580000051
  • Figure BDA0004170676580000052
    Figure BDA0004170676580000052
  • Figure HDA0004170676600000011
    Figure HDA0004170676600000011
Patent Text Reader

Abstract

The present invention provides a method and device for preparing anhydrous calcium chloride by self-catalytic coupling dehydration of carbon-containing mixed gas and calcium chloride hydrate, and the specific steps are as follows: (1) grinding calcium chloride hydrate into powder and placing it in a quartz tube, (2) contacting calcium chloride hydrate with carbon-containing mixed gas at 50-250oC for reaction, controlling the gas flow rate to be 1mL / min-100mL / min, and the reaction time to be 0.5-20h, (3) cooling the sample to room temperature in the reaction atmosphere and taking it out, collecting it with a vacuum packaging bag, sealing and preserving it, and obtaining anhydrous calcium chloride product, (4) collecting the atmosphere after the reaction to obtain hydrogen. The technology of preparing anhydrous calcium chloride by self-catalytic coupling dehydration of carbon-containing mixed gas and calcium chloride hydrate proposed by the present invention establishes a new theory of inorganic salt dehydration autocatalytic effect based on coupling autocatalysis as the basic principle, and forms a new cognition of the dehydration process of calcium chloride hydrate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method and a device for preparing anhydrous calcium chloride by utilizing the autocatalytic coupling dehydration of carbon-containing mixed gas and hydrated calcium chloride. Background Art

[0002] Anhydrous calcium chloride can be widely used in the fields of food manufacturing, building materials, medicine, biology, etc. It can be used as a desiccant, dehydrating agent, antifreeze agent, and is also a raw material for producing calcium salts. It is a very important chemical reagent in production and life. At present, the most common process methods for preparing anhydrous calcium chloride in domestic industry mainly include (1) calcium chloride dihydrate (dehydration method); (2) spray drying dehydration method; (3) mother liquor method; (4) double decomposition method: (5) refining method. Calcium chloride dihydrate (dehydration method) method and spray drying method are high-temperature heating and drying to obtain anhydrous calcium chloride, but the energy consumption is high, resulting in little economic benefit during industrial production. For example, in Chinese patent CN210058176, a practical atomizing nozzle device for anhydrous calcium chloride fluidized bed drying granulation is designed, and the temperature reaches 250°C or above before granulation production can be carried out; in Chinese patent CN104495903, the mother liquor method produces calcium chloride and realizes waste recycling, but due to the low calcium chloride content of the waste liquid, evaporation requires a large amount of steam consumption, and sun drying occupies a large amount of land; the double decomposition method is mostly used in areas with by-product hydrochloric acid, for example, in Chinese patent CN104773750, industrial waste hydrochloric acid is used to produce anhydrous calcium chloride, but the cost is high and the product competitiveness is low; the refining method has low production cost and good product quality, but resources are limited and it is not suitable for industrial production. Therefore, it is of great significance to change the existing high-energy consumption process of preparing anhydrous calcium chloride and realize low-cost and high-efficiency mass production of anhydrous calcium chloride by optimizing production conditions.

[0003] The water-gas shift reaction is the reaction of CO and H 2 O forms CO 2 and H 2 Similarly, small carbon-containing molecules such as methanol, methane, and ethane can also react with H 2 O undergoes a catalytic reaction in the low temperature range to produce H 2 If this process can be coupled with the dehydration process of calcium chloride hydrate, the transformation coupling reaction of the carbon-containing gas and crystal water by the self-catalysis of the calcium chloride dehydration product can be efficiently carried out in the low temperature range with thermodynamic advantages, which is expected to effectively reduce the dehydration temperature and reduce the H 2 O to H 2 , improving the economic value of the process. In addition, the carbon-containing mixed gas can be derived from methanol reforming hydrogen production and its downstream hydrogen use industry, providing a new channel for removing a large amount of carbon monoxide, methanol and other carbon-containing gases in the tail gas of methanol reforming hydrogen production in industry. Summary of the invention

[0004] The present invention aims at the blank of preparing anhydrous calcium chloride by dehydrating calcium chloride under low temperature conditions, and provides a method and device for preparing anhydrous calcium chloride by autocatalytic coupling dehydration of carbon-containing mixed gas and hydrated calcium chloride. This technology greatly reduces the temperature of calcium chloride dehydration, prepares high-purity anhydrous calcium chloride under milder conditions, and greatly reduces industrial energy consumption. At the same time, this method can effectively remove a large amount of CO in methanol reforming hydrogen production and its downstream hydrogen use industry and prepare hydrogen at the same time, and has high economic value.

[0005] The present invention provides a method and device for preparing anhydrous calcium chloride by autocatalytic coupling dehydration of carbon-containing mixed gas and hydrated calcium chloride. The specific preparation steps are as follows:

[0006] A. Using carbon-containing mixed gas as raw material, and performing deoxygenation optimization treatment on the carbon-containing mixed gas to obtain treated carbon-containing mixed gas;

[0007] The carbon-containing mixed gas is selected from at least one of methanol, methane, ethane and carbon monoxide, and the remaining gas is the balance gas, which is usually selected from N 2 Or inert gas, the mixed gas can be derived from methanol reforming hydrogen production and its downstream hydrogen use industry, and the carbon-containing gas content is 1-100%.

[0008] The deoxidation optimization treatment step specifically utilizes 401 manganese-based deoxidizer for deoxidation. 401 manganese-based deoxidizer is a manganese-based metal oxide, which is used for deoxidation and purification of gases such as nitrogen and inert gases.

[0009] B. The carbon-containing mixed gas treated in step A is contacted with hydrated calcium chloride for reaction, and then cooled and collected under a reaction atmosphere to obtain anhydrous calcium chloride. Meanwhile, hydrogen can be obtained by collecting tail gas.

[0010] The hydrated calcium chloride refers to CaCl with two or more crystal waters. 2 ; The anhydrous calcium chloride refers to CaCl with less than one crystal water 2 ;

[0011] When the treated carbon-containing mixed gas contacts and reacts with calcium chloride hydrate, the gas flow rate is 1 mL / min-1000 L / min, preferably 10 mL / min-100 mL / min.

[0012] The concentration of the treated carbon-containing gas is 1%-100%, and the remaining gas is the balance gas, which is usually selected from N 2 Or inert gas, the mixed gas can come from methanol reforming hydrogen production and its downstream hydrogen use industry.

[0013] During the reaction, programmed heating is adopted, the heating rate is 0.1-100°C / min, the reaction temperature is 50-250°C, preferably 100-200°C, and the reaction time is 0.5-20h, preferably 0.5-4h.

[0014] During the reaction, the mixture was cooled to room temperature and quickly taken out, collected in a vacuum packaging bag, and sealed for storage.

[0015] During the reaction, the obtained anhydrous calcium chloride contains CaCl 2 The quality fraction is ≥96%.

[0016] During the reaction, the average hydrogen production of calcium chloride hydrate is 10-2000umol / g.

[0017] A method for preparing anhydrous calcium chloride by autocatalytic coupling dehydration of a carbon-containing mixed gas and hydrated calcium chloride, characterized in that the device used is as follows: comprising two or three gas cylinders, one of which is a balance gas, and the other or two are carbon-containing gases;

[0018] The carbon-containing gases are methane, ethane, and carbon monoxide, and the balance gas is N 2 or inert gas;

[0019] The gas cylinder is connected to the deoxygenation device, the deoxygenation device is connected to the reactor, pressure gauges are arranged before and after the reactor, and a gas collection tank is arranged after the reactor.

[0020] A method for preparing anhydrous calcium chloride by autocatalytic coupling dehydration of a carbon-containing mixed gas and hydrated calcium chloride, characterized in that the device used is as follows:

[0021] When the carbon-containing gas is methanol, there are two gas cylinders, one of which is the balance gas and the other is the carbon-containing gas;

[0022] Methanol liquid is passed through a vaporizing device and a heat-insulating gas path to obtain methanol gas;

[0023] The gas cylinder and the insulated gas line are connected to the deoxygenation device, the deoxygenation device is connected to the reactor, pressure gauges are provided before and after the reactor, and a gas collection tank is provided after the reactor. The preparation method is characterized in that: the present invention provides a method and device for preparing anhydrous calcium chloride by using carbon-containing mixed gas and hydrated calcium chloride to autocatalytically couple dehydration, and for the first time uses carbon-containing mixed gas to achieve autocatalytic reaction and synergistic dehydration, thereby efficiently preparing anhydrous calcium chloride. Through this method, the temperature of calcium chloride dehydration can be effectively reduced, energy consumption can be greatly reduced, and the production cost of preparing anhydrous calcium chloride is expected to be greatly reduced. In addition, the carbon-containing mixed gas used in this method can be derived from methanol reforming hydrogen production and its downstream hydrogen use industry, which greatly improves the economic benefits of this method, and hydrogen is produced at the same time, opening up a new idea for preparing hydrogen from inorganic substances containing crystal water, and providing a new channel for removing a large amount of carbon-containing gas from methanol reforming hydrogen production tail gas in industry.

[0024] Depend on Figure 1 The XRD spectrum shows that anhydrous calcium chloride was successfully prepared;

[0025] From the EDTA titration analysis in Table 1, it can be seen that the CaCl 2 The quality fraction is ≥96%, reaching the first-level industrial grade requirement.

[0026] From the hydrogen production analysis in Table 2, it can be seen that the method can produce hydrogen, and the average hydrogen production is 10-2000umol / g.

[0027] The present invention proposes a technology for preparing anhydrous calcium chloride by autocatalytic coupled dehydration of a carbon-containing mixed gas and hydrated calcium chloride, establishes a new theory of autocatalytic dehydration of inorganic salts based on coupled autocatalysis as the basic principle, and forms a new understanding of the dehydration process of hydrated calcium chloride. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 This is the XRD spectrum of anhydrous calcium chloride prepared in Example 2-5.

[0029] Figure 2 The invention relates to a device for preparing anhydrous calcium chloride by reacting carbon-containing mixed gas with hydrated calcium chloride for dehydration. DETAILED DESCRIPTION

[0030] In the following examples, the gas percentages are by volume.

[0031] Example 1

[0032] A. First, grind calcium chloride dihydrate into powder, weigh 0.4g of calcium chloride dihydrate into a quartz tube, heat and vaporize methanol to obtain methanol gas, and introduce carbon monoxide, and the reaction gas is strictly deoxygenated and optimized before entering the tube furnace, that is, deoxygenated using 401 manganese deoxidizer;

[0033] B. The methanol gas concentration in step A is selected to be 5% CH 3 OH / 5%CO / N 2 (balance gas); gas flow rate is 80 mL / min; the temperature is increased to 200°C at a heating rate of 10°C / min, and the reaction time is 2 h.

[0034] C. The sample in step B is cooled to room temperature in the reaction atmosphere, taken out, collected in a vacuum packaging bag, and sealed for storage to obtain anhydrous calcium chloride product. The atmosphere after the reaction is collected to obtain hydrogen.

[0035] Example 2

[0036] A. First, grind calcium chloride dihydrate into powder, weigh 0.4g of calcium chloride dihydrate into a quartz tube, and introduce methane gas. Before entering the tube furnace, the reaction gas is strictly deoxygenated and optimized. The processing steps are the same as those in Example 1;

[0037] B. The methane gas concentration in step A is selected to be 20% CH 4 / N 2 (balance gas), the gas flow rate is 40 mL / min, the temperature is increased to 50°C at a heating rate of 10°C / min, and the reaction time is 6 h.

[0038] C. The sample in step B is cooled to room temperature in the reaction atmosphere, taken out, collected in a vacuum packaging bag, and sealed for storage to obtain anhydrous calcium chloride product. The atmosphere after the reaction is collected to obtain hydrogen.

[0039] Example 3

[0040] A. First, grind calcium chloride dihydrate into powder, weigh 0.2g of calcium chloride dihydrate into a quartz tube, and introduce carbon monoxide gas, and strictly deoxygenate the reaction gas before entering the tube furnace to optimize the gas treatment, and the treatment steps are the same as those in Example 1;

[0041] B. The carbon monoxide gas concentration in step A is selected to be 70% CO / N 2 (balance gas); gas flow rate is 10mL / min; heating rate is 5℃ / min to 100℃, reaction time is 4h.

[0042] C. The sample in step B is cooled to room temperature in the reaction atmosphere, taken out, collected in a vacuum packaging bag, and sealed for storage to obtain anhydrous calcium chloride product. The atmosphere after the reaction is collected to obtain hydrogen.

[0043] Example 4

[0044] A. First, grind calcium chloride dihydrate into powder, weigh 0.4g of calcium chloride dihydrate into a quartz tube, and introduce a mixture of carbon monoxide and methane, and strictly deoxygenate the reaction gas before entering the tube furnace to optimize the gas treatment, and the treatment steps are the same as those in Example 1;

[0045] B. The ratio of carbon monoxide and methane mixed gas in step A is 1:1, 15% CO / 15% CH 4 / N 2 (balance gas); gas flow rate is 60mL / min; the temperature is increased to 200℃ at a heating rate of 5℃ / min, and the reaction time is 3h.

[0046] C. The sample in step B is cooled to room temperature in the reaction atmosphere, taken out, collected in a vacuum packaging bag, and sealed for storage to obtain anhydrous calcium chloride product. The atmosphere after the reaction is collected to obtain hydrogen.

[0047] Example 5

[0048] A. First, grind calcium chloride dihydrate into powder, weigh 0.4 g of calcium chloride dihydrate into a quartz tube, and introduce a mixture of carbon monoxide and ethane, and strictly deoxygenate the reaction gas before entering the tube furnace to optimize the gas treatment, and the treatment steps are the same as those in Example 1;

[0049] B. The ratio of carbon monoxide and ethane mixed gas in step A is 1:1, 1% CO / 1% C 2 H 6 / N 2 (balance gas); gas flow rate is 100mL / min; heating rate is 10℃ / min to 150℃, reaction time is 8h.

[0050] C. The sample in step B is cooled to room temperature in the reaction atmosphere, taken out, collected in a vacuum packaging bag, and sealed for storage to obtain anhydrous calcium chloride product. The atmosphere after the reaction is collected to obtain hydrogen.

[0051] Table 1: EDTA titration analysis of anhydrous calcium chloride prepared in Examples 1-5

[0052]

[0053] Table 2: Hydrogen production during the preparation of anhydrous calcium chloride in Examples 1-5

[0054]

Claims

1. A method for preparing anhydrous calcium chloride by autocatalytic coupling dehydration of a carbon-containing mixed gas and hydrated calcium chloride, characterized in that Here are the steps: A. Using a carbon-containing mixed gas as a raw material, and performing a deoxygenation optimization treatment on the carbon-containing mixed gas to obtain a treated carbon-containing mixed gas; the carbon-containing mixed gas is selected from at least one of methanol, methane, ethane, and carbon monoxide, the volume percentage of the carbon-containing gas is 1-100%, and the remaining gas is N2 or an inert gas; B. contacting the carbon-containing mixed gas treated in step A with hydrated calcium chloride to react; then cooling and collecting under a reaction atmosphere to obtain anhydrous calcium chloride, and collecting tail gas to obtain hydrogen; The specific reaction conditions are: When the mixed gas is selected as 5% CH3OH / 5% CO / N2; the gas flow rate is 80mL / min; the temperature is increased to 200℃ at a heating rate of 10℃ / min, and the reaction time is 2h; When the mixed gas is selected as 20% CH4 / N2, the gas flow rate is 40mL / min, the temperature is increased to 50℃ at a heating rate of 10℃ / min, and the reaction time is 6h; When the mixed gas is selected as 70% CO / N2; the gas flow rate is 10mL / min; the temperature is increased to 100℃ at a heating rate of 5℃ / min, and the reaction time is 4h; When the mixed gas is selected as 15% CO / 15% CH4 / N2; the gas flow rate is 60mL / min; the temperature is increased to 200℃ at a heating rate of 5℃ / min, and the reaction time is 3h; When the mixed gas is selected as a mixture of carbon monoxide and ethane in a ratio of 1:1, 1% CO / 1% C2H6 / N2; the gas flow rate is 100mL / min; the temperature is increased to 150℃ at a heating rate of 10℃ / min, and the reaction time is 8h.

2. The method according to claim 1, characterized in that In step B, the mixed gas may be derived from hydrogen production from methanol reforming or its downstream hydrogen-using industry.

3. The method according to claim 1, characterized in that In step B, during the reaction process, programmed heating is adopted, and the heating rate is 0.1-100°C / min.

4. A method as claimed in claim 1, characterized in that The apparatus used is as follows: it comprises two or three gas cylinders, one of which is a balance gas and one or two of which are carbon-containing gases; The carbon-containing gas is methane, ethane, carbon monoxide, and the balance gas is N2 or inert gas; The gas cylinder is connected to the deoxygenation device, the deoxygenation device is connected to the reactor, pressure gauges are arranged before and after the reactor, and a gas collection tank is arranged after the reactor.

5. A method as claimed in claim 1, characterized in that The equipment used is as follows: The carbon-containing gas is methanol, and there are two gas cylinders, one of which is the balance gas and the other is the carbon-containing gas; Methanol liquid is passed through a vaporizing device and a heat-insulating gas path to obtain methanol gas; The gas cylinder and the heat-insulated gas line are connected to the deoxygenation device, the deoxygenation device is connected to the reactor, pressure gauges are arranged before and after the reactor, and a gas collection tank is arranged after the reactor.