A method for sealing a vehicle body lap weld

By filling the weld sealant in the depression at the overlapping part of the vehicle body, and using acupressure sealant to close the opening and extruded weld sealant, the problem of flow deformation of the weld sealant is solved, and a better sealing effect is achieved.

CN116532336BActive Publication Date: 2024-11-19DONGFENG LIUZHOU MOTOR
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310367624.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-04-07
Publication Date
2024-11-19
Estimated Expiration
2043-04-07

AI Technical Summary

Technical Problem

When the weld sealant is sealed with a width or diameter of more than 3mm when the multi-layer board overlapping part forms a depression with a width or diameter of more than 3mm, the weld sealant is prone to flow and deform to the opening, resulting in poor weld sealing effect.

Method used

Fill the weld sealant in the depression, and plug the acupressure sealant at the opening to close the opening, so that the acupressure sealant extruded the weld sealant fills the inner cavity of the depression, and then the outer periphery of the acupressure sealant and multiple layers are placed on the outer periphery of the acupressure sealant. Weld sealant is applied to the fitting seam of the board and heated to cure.

Benefits of technology

Through the extrusion of the acupressure sealant, the weld sealant can fully fill the weld, improve the sealing effect, avoid the sealant flowing outward, and enhance the sealing performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116532336B_ABST
    Figure CN116532336B_ABST
Patent Text Reader

Abstract

The invention relates to the field of vehicle engineering technology, and in particular to a method for sealing a vehicle body overlap weld. The method for sealing a vehicle body overlap weld comprises the following steps: firstly, a weld sealant is filled in a recessed portion; then, a finger pressure sealant is inserted at the opening of the recessed portion, the finger pressure sealant can shape and seal the opening of the recessed portion, and the finger pressure sealant squeezes the weld sealant in the recessed portion, so that the weld sealant fills the inner cavity of the recessed portion and each weld; then, the weld sealant is applied to the periphery of the finger pressure sealant and the fitting seams of each multilayer board, and finally, the weld sealant is heated and cured; the finger pressure sealant restricts the weld sealant in the recessed portion, thereby preventing the weld sealant from flowing outward, and under the squeezing action of the finger pressure sealant, the weld sealant can fully fill each weld, thereby improving the weld sealing effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of vehicle engineering, and in particular to a method for sealing a vehicle body lap weld. Background Art

[0002] The automobile body is made of multiple steel plates laser welded together. Laser welding has high requirements for assembly quality. In order to meet the requirements of laser welding and ensure the strength requirements of the weld, the current body structure mostly adopts an overlap structure. The overlap of the multi-layer plate will form a concave part with a width or diameter greater than 3mm, such as Figure 1 As shown, a first recessed portion 300 opening toward the upper right side is formed between the hood hinge 1, the A-pillar inner plate 23, the A-pillar middle plate 22 and the A-pillar outer plate 21, the width of the first recessed portion 300 is greater than 3 mm, the weld between the hood hinge 1 and the A-pillar inner plate 23 is located on the left side of the first recessed portion 300, the weld between the A-pillar inner plate 23 and the A-pillar middle plate 22 is located at the bottom of the first recessed portion 300, and the weld between the A-pillar outer plate 21 and the A-pillar middle plate 22 is located on the right side of the first recessed portion 300. If effective measures are not taken to seal the gaps at each weld, it will not only affect the comfort of the whole vehicle, resulting in a reduction in the sound insulation and noise reduction function of the vehicle, but also cause the steel plate at the weld to rust due to being soaked in rainwater, causing perforation corrosion, and causing the vehicle to be scrapped in advance.

[0003] At present, the recessed parts with a width or diameter greater than 3mm formed at the overlapped parts of the multi-layer boards are mostly sealed by applying weld sealant; however, due to the good fluidity of the weld sealant, after application and before curing, the opening of the recessed part is in an open state due to the movement or shaking of the vehicle body, and the flow resistance of the weld sealant at the opening of the recessed part is small, and the flow resistance of the weld sealant in the narrower weld part is large. Therefore, the weld sealant is easy to flow and deform toward the opening, resulting in the weld sealant being unable to fully fill the weld or the recessed part, and the welding seam sealing effect is poor. Summary of the invention

[0004] The technical problem to be solved by the present invention is: at present, when the overlapping parts of the multi-layer boards form a recessed part with a width or diameter greater than 3mm and are sealed by applying weld sealant, the weld sealant easily flows and deforms toward the opening, resulting in the weld sealant being unable to fully fill the weld or fill the recessed part, and the sealing effect of the weld is poor.

[0005] In order to solve the above technical problems, the purpose of the present invention is to provide a method for sealing a vehicle body overlap weld, which is used to seal a recessed portion with a width or diameter greater than 3 mm formed by overlapping multi-layer panels of a vehicle body, comprising the following steps:

[0006] Step S1, filling the recessed portion with weld sealant;

[0007] Step S2, inserting finger-pressure sealant at the opening of the recessed portion to close the opening of the recessed portion, and allowing the finger-pressure sealant to squeeze the weld sealant in the recessed portion so that the inner cavity of the recessed portion is filled with the weld sealant;

[0008] Step S3, applying weld sealant on the outer periphery of the finger pressure sealant and the joint seams of each of the multilayer boards;

[0009] Step S4, heating and curing the weld sealant and the finger pressure sealant.

[0010] As a preferred solution, in step S4, heating and curing the weld sealant includes:

[0011] Step S41, pre-drying to dry the surface layer of the weld sealant and the finger pressure sealant;

[0012] Step S42, spray painting the vehicle body surface;

[0013] Step S43, drying, to dry the paint on the surface of the vehicle body, the inner layer of the finger-pressure sealant and the inner layer of the weld sealant.

[0014] As a preferred solution, in step S41, the pre-drying parameters are: keeping warm at 110° C. to 130° C. for 8 to 20 minutes;

[0015] In step S43, the drying parameters are: keeping warm at 135° C. to 140° C. for 40 to 50 minutes.

[0016] As a preferred solution, the step S1 includes:

[0017] Step S0, performing electrophoretic coating on the vehicle body and drying.

[0018] As a preferred solution, after step S41 and before step S42, grinding is also included to remove particles or flow marks on the electrophoretic paint of the vehicle body.

[0019] As a preferred solution, in step S1, a mobile glue pump is used to fill the weld sealant into the recessed portion.

[0020] As a preferred solution, in step S3, a brush is used to evenly apply the weld sealant to the outer periphery of the finger pressure sealant and the fitting seams of each of the multilayer boards.

[0021] As a preferred solution, the step S4 includes:

[0022] Step S5: performing a weld sealing test on the vehicle body.

[0023] As a preferred solution, the vehicle body is subjected to a sealing test by means of a rain test to detect whether water seepage occurs in each of the recessed portions.

[0024] Compared with the prior art, the present invention has the following beneficial effects:

[0025] The method for sealing the overlapped weld of a vehicle body of the present invention comprises the following steps: firstly, a weld sealant is filled in a recessed portion; then, a finger pressure sealant is inserted at the opening of the recessed portion, the finger pressure sealant can shape and seal the opening of the recessed portion, and the finger pressure sealant squeezes the weld sealant in the recessed portion, so that the weld sealant fills the inner cavity of the recessed portion and each weld; then, the weld sealant is applied to the periphery of the finger pressure sealant and the fitting seams of each multilayer board, and finally, the weld sealant is cured by heating; the finger pressure sealant restricts the weld sealant in the recessed portion, thereby preventing the weld sealant from flowing outward, and under the squeezing action of the finger pressure sealant, the weld sealant can fully fill each weld, thereby improving the weld sealing effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 This is a schematic structural diagram of a vehicle body lap weld sealing method before weld sealing in Embodiment 1 of the present invention;

[0027] Figure 2 This is a schematic diagram of the structure after the weld is sealed in Embodiment 1 of the method for sealing the lap weld of a vehicle body according to the present invention;

[0028] Figure 3 This is a schematic structural diagram of a vehicle body lap weld sealing method before the weld is sealed in Embodiment 2 of the present invention;

[0029] Figure 4 It is a schematic diagram of the structure after the weld is sealed in the second embodiment of the method for sealing the overlap weld of the vehicle body of the present invention;

[0030] In the figure, 1, hood hinge; 21, A-pillar outer panel; 22, A-pillar middle panel; 23, A-pillar inner panel; 3, front panel; 4, front longitudinal beam reinforcement plate; 100, first finger-pressure sealant; 200, weld sealant; 300, first recessed portion; 400, second recessed portion; 500, second finger-pressure sealant. DETAILED DESCRIPTION

[0031] The specific implementation of the present invention is further described in detail below in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention.

[0032] In the description of the present invention, it should be understood that the orientation or positional relationship indicated by the terms "upper", "lower", "left", "right", "top", "bottom", etc. is based on the orientation or positional relationship shown in the accompanying drawings, and is only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention. It should be understood that the terms "first", "second", etc. are used in the present invention to describe various information, but such information should not be limited to these terms, which are only used to distinguish the same type of information from each other. For example, without departing from the scope of the present invention, the "first" information may also be referred to as the "second" information, and similarly, the "second" information may also be referred to as the "first" information.

[0033] Embodiment 1

[0034] like Figure 1 , Figure 2 As shown, a method for sealing a vehicle body overlap weld of the present invention is used to seal the weld in the first recessed portion 300 at the mounting base of the hood hinge 1, and to seal the weld formed between the hood hinge 1, the A-pillar inner plate 23, the A-pillar middle plate 22 and the A-pillar outer plate 21. A first recessed portion 300 opening toward the upper right side is formed between the hood hinge 1, the A-pillar inner plate 23, the A-pillar middle plate 22 and the A-pillar outer plate 21, and the width of the first recessed portion 300 is greater than 3 mm. The weld between the hood hinge 1 and the A-pillar inner plate 23 is located on the left side of the first recessed portion 300, the weld between the A-pillar inner plate 23 and the A-pillar middle plate 22 is located at the bottom of the first recessed portion 300, and the weld between the A-pillar outer plate 21 and the A-pillar middle plate 22 is located on the right side of the first recessed portion 300, comprising the following steps:

[0035] Step S1, filling the first recessed portion 300 with weld sealant 200;

[0036] Step S2, inserting the first finger-pressed sealant 100 at the opening of the first recessed portion 300 to close the opening of the first recessed portion 300, and making the first finger-pressed sealant 100 squeeze the weld sealant 200 in the first recessed portion 300, so that the inner cavity of the first recessed portion 300 is filled with the weld sealant 200; specifically, the first finger-pressed sealant 100 can close the opening of the first recessed portion 300, and can squeeze the weld sealant 200 in the first recessed portion 300, so that the weld sealant can flow out. The welds between the hood hinge 1 and the A-pillar inner panel 23, the welds between the A-pillar inner panel 23 and the A-pillar middle panel 22, and the welds between the A-pillar outer panel 21 and the A-pillar middle panel 22 are filled, so that each weld in the first recessed portion 300 is filled. When the vehicle body is moved to the heating and curing station, the weld sealant 200 in the first recessed portion 300 is constrained by the first finger pressure sealant 100, and the weld sealant in the first recessed portion 300 flows out through the opening of the first recessed portion 300, thereby ensuring the sealing effect.

[0037] Step S3, applying weld sealant to the joints between the outer periphery of the first finger-pressed sealant 100 and the hood hinge 1, and the outer periphery of the first finger-pressed sealant 100 and the A-pillar outer panel 21;

[0038] Step S4, heating and curing the weld sealant 200, and heating and curing the weld sealant coated on the outside of the first finger pressure sealant 100 and the first finger pressure sealant 100.

[0039] Wherein, in step S4, heating and curing the weld sealant comprises:

[0040] Step S41, pre-drying to dry the surface layer of the weld sealant and the first finger-pressure sealant 100; specifically, pre-drying can shape the weld sealant and the first finger-pressure sealant 100 in the first recessed portion 300 to avoid damage before painting.

[0041] Step S42, spraying paint on the vehicle body surface;

[0042] Step S43, drying, to dry the paint on the vehicle body surface, the inner layer of the finger pressure sealant and the inner layer of the weld sealant. Specifically, drying can completely cure the paint on the vehicle body surface, the first finger pressure sealant 100 and the weld sealant in the first recessed portion 300, and curing the paint on the vehicle body surface, the first finger pressure sealant 100 and the weld sealant in the first recessed portion 300 at the same station not only saves costs, but also avoids the influence of repeated heating on the painted surface or the first finger pressure sealant 100 and the weld sealant in the first recessed portion 300.

[0043] The parameters of the pre-baking are: keeping warm at 110°C to 130°C for 8 to 20 minutes; in step S43, the parameters of the baking are: keeping warm at 135°C to 140°C for 40 to 50 minutes. Specifically, if the pre-baking temperature is too low or the insulation time is insufficient, the first finger-pressed sealant 100 and the weld sealant in the first recessed portion 300 and the weld sealant outside the first finger-pressed sealant 100 will not be sufficiently cured, resulting in damage to the first finger-pressed sealant 100 and the weld sealant outside the first finger-pressed sealant 100 during subsequent painting or polishing. When the pre-drying temperature is too high or the insulation time is too long, the first finger-pressure sealant 100 and the weld sealant located in the first recessed portion 300 and the weld sealant located outside the first finger-pressure sealant 100 will be completely cured. When the painted surface is subsequently cured, the first finger-pressure sealant 100 and the weld sealant located in the first recessed portion 300 and the weld sealant located outside the first finger-pressure sealant 100 will be heated again, causing the first finger-pressure sealant 100 and the weld sealant located in the first recessed portion 300 and the weld sealant located outside the first finger-pressure sealant 100 to age. In this embodiment, the temperature is kept at 110°C to 130°C for 8 to 20 minutes. In step S43, the drying parameters are: keeping at 135°C to 140°C for 40 to 50 minutes. This ensures that the first finger-pressure sealant 100 and the weld sealant located in the first recessed portion 300 and the weld sealant located outside the first finger-pressure sealant 100 meet the curing requirements after pre-drying and drying and will not be affected by excessive heating, and also ensures that the painted surface can be fully cured.

[0044] In this embodiment, before step S1, the following steps are included:

[0045] Step S0, electrophoresis coating and drying the vehicle body. The surface cleanliness of the vehicle body after electrophoresis coating and drying is high, which ensures the bonding force between the first finger-pressure sealant 100 and the weld sealant in the first recessed portion 300 and the vehicle body.

[0046] After step S41 and before step S42, polishing is also included to remove particles or flow marks on the electrophoretic paint of the vehicle body to ensure the quality of the painted surface after painting.

[0047] In this embodiment, in step S1, a mobile glue pump is used to fill the weld sealant into the recessed portion.

[0048] In this embodiment, in step S3, the weld sealant is evenly applied to the outer periphery of the finger pressure sealant and the joint seams of each multilayer board using a brush pen. The weld sealant is applied with a brush pen so that the weld sealant is applied more evenly.

[0049] To ensure the sealing effect, step S4 includes:

[0050] Step S5: performing a weld sealing test on the vehicle body.

[0051] Specifically, in this embodiment, the sealing test of the vehicle body is performed by means of a rain test to detect whether water seepage occurs in each recessed portion.

[0052] To verify the sealing effect, in this embodiment, a mobile glue pump is used at the plugging cover installation station to spray weld sealant in the first recessed part 300 of 20 car bodies, and then the glue coating station is entered. At the glue coating station, finger-pressure sealant is used for plugging; thereafter, weld sealant is applied at the joint between the outer periphery of the first finger-pressure sealant 100 and the hood hinge 1, and the joint between the outer periphery of the first finger-pressure sealant 100 and the A-pillar outer panel 21, and then pre-drying, painting, and drying are carried out in sequence. After drying, the car body is modified and loaded into the final assembly. When the final assembly is off the line, it is subjected to a rain test. The rain test results show that the 20 pre-coated car bodies of this model no longer have water ingress, and the failure rate is zero. The glue coating status of the water-ingressed car bodies is checked. Visual inspection did not find problems such as surface glue cracking and glue separation. After removing the fender, it was checked that the finger-pressure sealant was fixed and not offset, and the welds in the first recessed part 300 and the first recessed part 300 were filled with weld sealant.

[0053] Embodiment 2

[0054] The difference between this embodiment and the first embodiment is that Figure 3 , Figure 4 As shown, the vehicle body overlap weld sealing method of the present invention can be used to seal the second recessed portion 400 at the overlapped portion of the A-pillar, the side panel, the cabin longitudinal beam and the front risk lower cross beam, the width of the second recessed portion 400 is greater than 3 mm, and a second recessed portion 400 with an opening facing upward is formed between the A-pillar outer plate 21, the A-pillar middle plate 22, the A-pillar inner plate 23 and the front longitudinal beam reinforcement plate 4, the bottom wall of the second recessed portion 400 is the front wheel hub cover plate, and welds exist between the front wheel hub cover plate and the A-pillar inner plate 23, the A-pillar middle plate 22, the A-pillar outer plate 21 and the front longitudinal beam reinforcement plate 4. In the embodiment, the weld sealant is first sprayed in the second recessed portion 400, and then the pinched second finger-pressure sealant 500 is inserted into the top opening of the second recessed portion 400. Thereafter, the weld sealant is applied to the joints between the second finger-pressure sealant 500 and the A-pillar outer panel 21, the A-pillar middle panel 22, the A-pillar inner panel 23 and the front longitudinal beam reinforcement plate 4. Finally, the entire vehicle body is dried to cure the second finger-pressure sealant 500, the weld sealant in the second recessed portion 400 and the weld sealant outside the second finger-pressure sealant 500.

[0055] In summary, the method for sealing the overlapped weld of a vehicle body of the present invention first fills the recessed portion with weld sealant; then, finger pressure sealant is inserted at the opening of the recessed portion, the finger pressure sealant can shape and seal the opening of the recessed portion, and the finger pressure sealant squeezes the weld sealant in the recess so that the weld sealant fills the inner cavity of the recessed portion and each weld; then, weld sealant is applied to the periphery of the finger pressure sealant and the fitting seams of each multilayer board, and finally, the weld sealant is heated and cured; the finger pressure sealant restricts the weld sealant in the recessed portion, thereby preventing the weld sealant from flowing outward, and under the squeezing action of the finger pressure sealant, the weld sealant can fully fill each weld, thereby improving the weld sealing effect.

[0056] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and substitutions can be made without departing from the technical principles of the present invention. These improvements and substitutions should also be regarded as the scope of protection of the present invention.

Claims

1. A method for sealing a vehicle body overlap weld, used for sealing a recessed portion with a width or diameter greater than 3 mm formed by overlapping multi-layer panels of a vehicle body, characterized in that: The vehicle body lap weld sealing method is used to seal a first recessed portion (300) formed between a hood hinge (1), an A-pillar inner plate (23), an A-pillar middle plate (22) and an A-pillar outer plate (21) and opening toward the upper right side; and comprises the following steps: Step S1, filling the recessed portion with weld sealant; Step S2, plugging the opening of the recessed portion with a first finger-pressure sealant (100) to close the opening of the recessed portion, and allowing the finger-pressure sealant to squeeze the weld sealant in the recess, so that the inner cavity of the recessed portion is filled with the weld sealant; the first finger-pressure sealant (100) closes the opening of the first recessed portion (300), and can squeeze the weld sealant (200) in the first recessed portion (300), so that the weld sealant (200) can flow to the weld between the hood hinge (1) and the A-pillar inner panel (23), the weld between the A-pillar inner panel (23) and the A-pillar middle panel (22), and the weld between the A-pillar outer panel (21) and the A-pillar middle panel (22), so that each weld in the first recessed portion (300) is filled; Step S3, applying weld sealant on the outer periphery of the finger pressure sealant and the joint seams of each of the multilayer boards; Step S4, heating and curing the weld sealant and the finger pressure sealant; The step S1 includes: Step S0, performing electrophoretic coating on the vehicle body and drying.

2. The method for sealing a vehicle body lap weld according to claim 1, characterized in that: In the step S4, heating and curing the weld sealant comprises: Step S41, pre-drying to dry the surface layer of the weld sealant and the finger pressure sealant; Step S42, spray painting the vehicle body surface; Step S43, drying, to dry the paint on the surface of the vehicle body, the inner layer of the finger-pressure sealant and the inner layer of the weld sealant.

3. The method for sealing a vehicle body lap weld according to claim 2, characterized in that: In step S41, the pre-drying parameters are: keeping warm at 110°C to 130°C for 8min to 20min; In step S43, the drying parameters are: keeping warm at 135° C. to 140° C. for 40 to 50 minutes.

4. The method for sealing a vehicle body lap weld according to claim 1, characterized in that: After step S41 and before step S42, grinding is also included to remove particles or flow marks on the electrophoretic paint of the vehicle body.

5. The method for sealing a vehicle body lap weld according to claim 1, characterized in that: In the step S1, a mobile glue pump is used to fill the weld sealant into the recessed portion.

6. The method for sealing a vehicle body lap weld according to claim 1, characterized in that: In the step S3, a brush is used to evenly apply the weld sealant to the outer periphery of the finger pressure sealant and the joint seams of each of the multilayer boards.

7. The method for sealing a vehicle body lap weld according to claim 1, characterized in that: The step S4 comprises: Step S5: performing a weld sealing test on the vehicle body.