MEMS acceleration and pressure integrated sensor and preparation method thereof

By using vertical integrated structure and sacrificial layer process in MEMS sensors, the mass blocks and cantilever beams of the accelerometer are fabricated above the sensitive film of the pressure sensor, which solves the problems of low integration degree and complex process of MEMS integrated sensors, and realizes the basic Savings of area and reducing production costs.

CN116750709BActive Publication Date: 2024-12-03NANJING GAOHUA TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310647135.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-06-02
Publication Date
2024-12-03
Estimated Expiration
2043-06-02

AI Technical Summary

Technical Problem

The degree of integration of existing MEMS integrated sensors is not high, resulting in large substrate area, high manufacturing cost, and complex process flow and difficult.

Method used

Using a vertical integrated structure, the mass and cantilever beam of the accelerometer are made above the sensitive film of the pressure sensor, and the preparation of the sensitive film is completed while releasing the mass and cantilever beam through the sacrificial layer process, simplifying the process flow.

Benefits of technology

Save 1/2 of the substrate area, improve the degree of integration of sensor chips, reduce production costs, simplify process flow, and improve economic benefits.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116750709B_ABST
    Figure CN116750709B_ABST
Patent Text Reader

Abstract

The embodiment of the present disclosure discloses a MEMS acceleration and pressure integrated sensor and a preparation method thereof. It includes: a first substrate, provided with a cavity; a buried oxide layer, a device layer and a first passivation layer arranged on the first substrate, the three corresponding to the cavity portion forming a sensitive film; a first piezoresistor and a first ohmic contact area, embedded in the surface of the device layer; a sacrificial layer, a structural layer and a second passivation layer arranged on the first passivation layer, the structural layer and the second passivation layer corresponding to the cavity portion suspended to form a mass block and a cantilever beam; a second piezoresistor and a second ohmic contact area, embedded in the surface of the suspended portion of the structural layer away from the first substrate; a lead layer and a metal filling layer, the lead layer is arranged on the surface of the second passivation layer, the metal filling layer is electrically connected to the lead layer, the first ohmic contact area and the second ohmic contact area respectively; a second substrate, connected to the surface of the first substrate away from the first passivation layer. Improve the degree of integration, reduce production costs, and simplify the process flow.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present disclosure belong to the technical field of sensor integration, and specifically relate to a MEMS acceleration and pressure integrated sensor and a preparation method thereof. Background Art

[0002] Sensors can convert physical quantity changes into electrical signal changes for easy measurement. Sensors manufactured based on MEMS technology have the advantages of small size, high precision, and easy integration. They are widely used in industrial control, environmental monitoring, aerospace, automotive electronics, etc. In many applications, it is often necessary to measure multiple physical quantities such as acceleration and pressure at the same time. MEMS integrated sensors can integrate multiple different types of MEMS sensors on the same chip to achieve simultaneous monitoring of multiple physical quantities. They have the advantages of small size and low unit cost, and have broad application prospects.

[0003] At present, common MEMS integrated sensors integrate the preparation processes of different sensors to achieve the simultaneous preparation of multiple MEMS sensors, but different sensors are still relatively independent parallel systems. They are horizontally arranged at different positions and occupy a certain area respectively.

[0004] Based on the above reasons, the current integration level of MEMS integrated sensors is not high, and they occupy a large substrate area, resulting in higher manufacturing costs. Summary of the invention

[0005] The embodiments of the present disclosure aim to solve at least one of the technical problems existing in the prior art, and disclose a MEMS acceleration and pressure integrated sensor and a preparation method thereof.

[0006] In a first aspect, an embodiment of the present disclosure provides a MEMS acceleration and pressure integrated sensor, the integrated sensor comprising:

[0007] A first substrate having a cavity extending through its thickness;

[0008] A buried oxide layer, a device layer and a first passivation layer are sequentially stacked on the first substrate, and the three layers corresponding to the cavity together form a sensitive film;

[0009] A first varistor and a first ohmic contact region are both embedded in a surface of the device layer facing away from the first substrate;

[0010] A sacrificial layer, a structural layer, and a second passivation layer are sequentially stacked on the first passivation layer, the sacrificial layer being located outside the cavity, so that the structural layer and the second passivation layer are partially suspended corresponding to the cavity to form a mass block and a cantilever beam;

[0011] A second varistor and a second ohmic contact region are both embedded in a surface of the structure layer of the suspended portion away from the first substrate;

[0012] A lead layer and a metal filling layer, wherein the lead layer is disposed on a surface of the second passivation layer away from the first substrate, and the metal filling layer is electrically connected to the lead layer, the first ohmic contact region, and the second ohmic contact region respectively;

[0013] The second substrate is connected to a surface of the first substrate facing away from the first passivation layer.

[0014] In some embodiments, the integrated sensor includes a plurality of first piezoresistors;

[0015] Each of the first varistors is located in a central area of ​​a corresponding side of the cavity.

[0016] In some embodiments, the plurality of first varistors are connected via a first Wheatstone bridge.

[0017] In some embodiments, the integrated sensor includes a plurality of second piezoresistors;

[0018] At least two of the second varistors are distributed in the stress concentration area of ​​the cantilever beam, and the remaining second varistors are distributed in the zero stress area of ​​the cantilever beam.

[0019] In some embodiments, the plurality of second varistors are connected via a second Wheatstone bridge.

[0020] In some embodiments, the at least two second varistors at the stress concentration region of the cantilever beam are symmetrically distributed; and / or,

[0021] The remaining second varistors at the zero stress region of the cantilever beam are symmetrically distributed.

[0022] In some embodiments, the metal filling layer penetrates the second passivation layer, the structural layer, and the first passivation layer.

[0023] In some embodiments, the integrated sensor further comprises an insulating layer;

[0024] The insulating layer is disposed around the metal filling layer.

[0025] In some embodiments, the sacrificial layer is formed of phosphosilicate glass; and / or the sacrificial layer has a thickness ranging from 1 μm to 10 μm.

[0026] In a second aspect, an embodiment of the present disclosure provides a method for preparing a MEMS acceleration and pressure integrated sensor, comprising:

[0027] Providing an SOI wafer; wherein the SOI wafer comprises a first substrate, a buried oxide layer and a device layer stacked in sequence;

[0028] Doping the surface of the device layer to form a first varistor and a first ohmic contact region respectively;

[0029] forming a first passivation layer on the surface of the device layer;

[0030] forming a sacrificial layer on the surface of the first passivation layer, and patterning the sacrificial layer to form an annular groove;

[0031] forming a structural layer on the surface of the sacrificial layer and in the annular groove;

[0032] forming a second varistor and a second ohmic contact area on the surface of the structural layer respectively;

[0033] forming a second passivation layer on the surface of the structural layer;

[0034] Patterning the second passivation layer, the structural layer, the sacrificial layer and the first passivation layer to form a first contact through hole corresponding to the first ohmic contact area;

[0035] forming an insulating layer on the inner sidewall of the first contact through hole, and filling the first contact through hole with a metal filling layer;

[0036] Patterning the second passivation layer to form a second contact hole corresponding to the second ohmic contact area;

[0037] forming a wiring layer on the second passivation layer;

[0038] Patterning the second passivation layer and the structural layer to define a proof mass and a cantilever beam region;

[0039] Patterning the surface of the first substrate facing away from the first passivation layer to obtain a through groove penetrating the thickness thereof;

[0040] Providing a second substrate, and connecting a surface of the second substrate to a surface of the first substrate facing away from the first passivation layer to form a cavity;

[0041] The sacrificial layer corresponding to the cavity portion is removed to release the mass block and the cantilever beam, and a sensitive film is formed at the same time, thereby completing the preparation of the MEMS acceleration and pressure integrated sensor.

[0042] The MEMS acceleration and pressure integrated sensor and its preparation method of the disclosed embodiment adopt a stacking method to make the mass block and cantilever beam of the accelerometer above the sensitive film of the pressure sensor. This vertical integration structure saves 1 / 2 of the substrate area, greatly improves the integration level of the sensor chip, reduces production costs, and improves economic benefits. In addition, the sacrificial layer process is also used to complete the preparation of the sensitive film while releasing the mass block and cantilever beam, which simplifies the process flow, reduces the process difficulty, reduces the production cost, and improves the economic benefits. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] The above and other features, advantages and aspects of the embodiments of the present disclosure will become more apparent with reference to the following detailed description in conjunction with the accompanying drawings. Throughout the accompanying drawings, the same or similar reference numerals represent the same or similar elements. It should be understood that the drawings are schematic and that components and elements are not necessarily drawn to scale.

[0044] Figure 1 is a cross-sectional view of a MEMS acceleration and pressure integrated sensor according to an embodiment of the present disclosure;

[0045] Figure 2 for Figure 1 A top view of the MEMS acceleration and pressure integrated sensor shown in FIG.

[0046] Figures 3 to 20 The present invention is a process flow chart of a method for preparing a MEMS acceleration and pressure integrated sensor according to an embodiment of the present invention. DETAILED DESCRIPTION

[0047] In order to enable those skilled in the art to better understand the technical solution of the present disclosure, the present disclosure is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0048] Embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although certain embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be construed as being limited to the embodiments set forth herein. On the contrary, these embodiments are provided to provide a more thorough and complete understanding of the present disclosure. It should be understood that the drawings and embodiments of the present disclosure are only for exemplary purposes and are not intended to limit the scope of protection of the present disclosure.

[0049] It should also be noted that, for ease of description, only the parts related to the present disclosure are shown in the drawings. In the absence of conflict, the embodiments and features in the embodiments of the present disclosure can be combined with each other.

[0050] The present disclosure will be described in detail below with reference to the accompanying drawings and in conjunction with embodiments.

[0051] like Figure 1 and Figure 2 As shown, an embodiment of the present disclosure relates to a MEMS acceleration and pressure integrated sensor, including: a first substrate 1, a buried oxide layer 2, a device layer 3, a first piezoresistor 4, a first ohmic contact area 5, a first passivation layer 6, a sacrificial layer 7, a structural layer 8, a second piezoresistor 9, a second ohmic contact area 10, a second passivation layer 11, an insulating layer 12, a metal filling layer 13, a lead layer 14 and a second substrate 15.

[0052] Please refer to Figure 1 The first substrate 1 is provided with a cavity 16 running through its thickness. In some embodiments, the material of the first substrate 1 is single crystal silicon with a thickness ranging from 200 μm to 1000 μm. The specific shape of the cavity 16 formed on the first substrate 1 is not limited. In some examples, the cavity 16 is located in the central area of ​​the first substrate 1 and has a rectangular shape.

[0053] Continue to refer Figure 1 , the buried oxide layer 2 is located above the first substrate 1. In some embodiments, the material of the buried oxide layer 2 is silicon oxide, and the thickness ranges from 0.1μm to 4μm. The device layer 3 is located above the buried oxide layer 2. In some embodiments, the material of the device layer 3 is single crystal silicon, and the thickness ranges from 0.2μm to 50μm. The first passivation layer 6 is located above the device layer 3. The function of the first passivation layer 6 is to achieve electrical isolation between the device layer 3 and the structural layer 8. In some embodiments, the material of the first passivation layer 6 is silicon nitride, and the thickness ranges from 0.2μm to 2μm. Figure 1 As shown, the first passivation layer 6 , the device layer 3 and the central portion of the buried oxide layer 2 facing the cavity 16 together form a sensitive film 17 .

[0054] Continue to refer Figure 1 , the first varistor 4 and the first ohmic contact area 5 are both embedded in the upper surface of the device layer 3. In some embodiments, there are multiple first varistor 4, and the example of four first varistor 4 is given. The four first varistor 4 are respectively arranged directly above the midpoint of the four sides of the cavity 16. The purpose of this is to arrange the first varistor 4 at the maximum stress of the sensitive film 17, so as to improve the sensitivity of the pressure sensor as much as possible. The four first varistor 4 is connected through the first Wheatstone bridge. The first ohmic contact area 5 is located at both ends of the first varistor 4, and its function is to realize the electrical interconnection between the first varistor 4 and the metal filling layer 13.

[0055] Next, continue to refer to Figure 1, the sacrificial layer 7 is located in the edge area above the first passivation layer 6. In some embodiments, the material of the sacrificial layer 7 is phosphosilicate glass (PSG) with a thickness ranging from 1 μm to 10 μm. The structural layer 8 is located above the sacrificial layer 7. In some embodiments, the material of the structural layer 8 is polysilicon with a thickness ranging from 3 μm to 20 μm. The second passivation layer 11 is located above the structural layer 8. The function of the second passivation layer 11 is to achieve electrical isolation between the lead layer 14 and the structural layer 8. In some embodiments, the material of the second passivation layer 11 is silicon nitride with a thickness ranging from 0.2 μm to 2 μm. Combined with Figure 2 Since the sacrificial layer 7 is only located at the edge region above the first passivation layer 6 , the second passivation layer 11 and the structural layer 8 are suspended at the position corresponding to the cavity 16 , thereby forming a mass block 18 and a cantilever beam 19 .

[0056] Then, if Figure 1 As shown, the second piezoresistors 9 and the second ohmic contact area 10 are both embedded in the upper surface of the structural layer 8 of the suspended portion. In some embodiments, there are multiple second piezoresistors 9, and an example is given with four second piezoresistors 9, wherein two second piezoresistors 9 are preferably symmetrically distributed in the stress concentration area on the cantilever beam 19, and the other two second piezoresistors 9 are preferably symmetrically distributed in the zero stress area on the cantilever beam 19, and the purpose of this is to maximize the sensitivity of the acceleration sensor. The second ohmic contact area 10 is located at both ends of the second piezoresistors 9, and its function is to realize the electrical interconnection between the second piezoresistors 9 and the lead layer 14.

[0057] Continue to refer Figure 1 The metal filling layer 13 is located at the end of the first ohmic contact region 5, and the material is at least one of W or Cu. In combination with the capabilities of the current deep trench etching and hole filling processes, the width is set to 2μm to 10μm; the function of the metal filling layer 13 is to realize the electrode lead-out of the first varistor 4. The insulating layer 12 is located around the metal filling layer 13, and the function of the insulating layer 12 is to realize the electrical isolation of the metal filling layer 13 and the structural layer 8. In some embodiments, the material of the insulating layer 12 is silicon dioxide, and the thickness ranges from 50nm to 500nm.

[0058] For reference Figure 1 and Figure 2 The lead layer 14 is located above the second passivation layer 11, and the function of the lead layer 14 is to realize the electrode lead-out of the metal filling layer 13 and the second varistor 9. In some embodiments, the material of the lead layer 14 is at least one of Al, Ti, Au, Cu, and Pt, preferably Au, and the thickness ranges from 100nm to 500nm.

[0059] like Figure 1As shown, the upper surface of the second substrate 15 is bonded to the lower surface of the first substrate 1 to achieve vacuum sealing of the cavity 16 and provide mechanical support for the sensor chip. In some embodiments, the material of the second substrate 15 is single crystal silicon or glass, preferably a BF33 glass sheet, with a thickness ranging from 200 μm to 2000 μm.

[0060] The working principle of the MEMS acceleration and pressure integrated sensor according to the embodiment of the present disclosure is described below:

[0061] like Figure 1 and Figure 2 As shown in the figure, when external pressure acts on the sensor, the sensitive film 17 deforms in proportion to the pressure, resulting in corresponding stress and strain around it. The resistance values ​​of the four first piezoresistors 4 located at the center of the four sides of the sensitive film 17 change under the action of the piezoresistance effect, and this change is converted into an electrical signal output through the Wheatstone bridge. Therefore, the magnitude of the pressure on the sensor can be obtained by measuring the electrical signal output of the first Wheatstone bridge.

[0062] When vertical acceleration acts on the sensor, due to the inertial force, the mass block 18 swings up and down, causing the cantilever beam 19 to deform in proportion to the acceleration, generating corresponding stress and strain on the cantilever beam 19, and the resistance of the two second piezoresistors 9 on the cantilever beam 19 changes under the action of the piezoresistive effect, and finally the resistance change is converted into an electrical signal output through the Wheatstone bridge. Therefore, the magnitude of the acceleration to which the sensor is subjected can be obtained by measuring the electrical signal output of the second Wheatstone bridge.

[0063] The MEMS acceleration and pressure integrated sensor of the disclosed embodiment adopts a stacking method to manufacture the mass block and cantilever beam of the accelerometer above the sensitive film of the pressure sensor. This vertical integration structure saves 1 / 2 of the substrate area, greatly improves the integration level of the sensor chip, reduces production costs, and improves economic benefits. In addition, the MEMS acceleration and pressure integrated sensor of the disclosed embodiment also utilizes a sacrificial layer process to complete the preparation of the sensitive film while releasing the mass block and cantilever beam, which simplifies the process flow, reduces the process difficulty, reduces production costs, and improves economic benefits.

[0064] Based on the same inventive concept, the embodiment of the present disclosure also provides a method for preparing a MEMS acceleration and pressure integrated sensor. The structure of the MEMS acceleration and pressure integrated sensor can refer to the relevant records in the previous text and will not be repeated here.

[0065] The method for preparing the MEMS acceleration and pressure integrated sensor of the embodiment of the present disclosure specifically comprises the following steps:

[0066] Step 1: Provide an SOI wafer; wherein the SOI wafer includes a first substrate, a buried oxide layer and a device layer stacked in sequence.

[0067] Specifically, in this step, Figure 3 As shown, the SOI wafer may be of N-type, and is provided with a first substrate 1, a buried oxide layer 2 and a device layer 3 from bottom to top. In this embodiment, the thickness of the first substrate 1 is 300 μm, the thickness of the buried oxide layer 2 is 2 μm, and the thickness of the device layer 3 is 10 μm.

[0068] Step 2: doping the surface of the device layer to form a first varistor.

[0069] Specifically, in this step, Figure 4 As shown, the first varistor 4 is formed on the upper surface of the device layer 3 by photolithography and boron ion implantation (light boron).

[0070] Step three: doping the surface of the device layer to form a first ohmic contact region.

[0071] Specifically, in this step, Figure 5 As shown, a first ohmic contact region 5 is formed on the upper surface of the device layer 3 by photolithography and boron ion implantation (concentrated boron).

[0072] Step 4: forming a first passivation layer on the surface of the device layer.

[0073] Specifically, in this step, Figure 6 As shown, silicon nitride with a thickness of 300 nm is deposited on the device layer 3 as the first passivation layer 6 by plasma enhanced chemical vapor deposition (PECVD).

[0074] Step five: forming a sacrificial layer on the surface of the first passivation layer.

[0075] Specifically, in this step, Figure 7 As shown, PSG (phosphosilicate glass) with a thickness of 5 μm is in-situ doped and deposited as the sacrificial layer 7 by high density plasma chemical vapor deposition (HDP CVD).

[0076] Step six: patterning the sacrificial layer to form an annular groove.

[0077] Specifically, in this step, Figure 8 As shown, an annular groove is formed on the PSG sacrificial layer 7 by photolithography and HF etching.

[0078] Step seven: forming a structural layer on the surface of the sacrificial layer and in the annular groove.

[0079] Specifically, in this step, Fig. 9 As shown, polysilicon with a thickness of 12 μm is deposited on the PSG sacrificial layer 7 as the structural layer 8 by low pressure chemical vapor deposition (LPCVD).

[0080] Step eight, forming a second varistor and a second ohmic contact area on the surface of the structural layer respectively.

[0081] Specifically, in this step, Fig.10 As shown, a second varistor 9 and a second ohmic contact region 10 are formed on the upper surface of the polysilicon structure layer 8 by photolithography and two boron ion implantations, and then annealed at 1000° C. for 30 minutes.

[0082] Step nine: forming a second passivation layer on the surface of the structural layer.

[0083] Specifically, in this step, Fig.11 As shown, silicon nitride with a thickness of 300 nm is deposited on the polysilicon structure layer 8 by PECVD as the second passivation layer 11 .

[0084] Step ten: patterning the second passivation layer, the structural layer, the sacrificial layer and the first passivation layer to form a first contact hole corresponding to the first ohmic contact area.

[0085] Specifically, in this step, Fig.12 As shown, photolithography is performed, the second passivation layer 11 is etched by reactive ion etching (RIE), the polysilicon structure layer 8 is etched by inductively coupled plasma (ICP), the PSG sacrificial layer 7 is corroded by HF, and the first passivation layer 6 is etched by RIE to finally form a first contact through hole.

[0086] Step 11: forming an insulating layer on the inner side wall of the first contact hole.

[0087] Specifically, in this step, Fig.13 As shown, through a low-temperature oxidation process, a 500nm thick silicon dioxide is deposited on the upper surface of the second passivation layer 11 and in the first contact hole as an insulating layer 12, and the silicon dioxide in the vertical direction is etched away by ion beam etching (IBE), leaving only the silicon dioxide insulating layer 12 on the side wall of the first contact hole.

[0088] Step twelve: filling a metal filling layer in the first contact through hole.

[0089] Specifically, in this step, Fig.14 As shown, metal tungsten is filled in the first contact hole as the metal filling layer 13 through a tungsten hole filling process.

[0090] Step 13: patterning the second passivation layer to form a second contact hole corresponding to the second ohmic contact area.

[0091] Specifically, in this step, Fig.15 As shown, the second passivation layer 11 is etched by RIE to form a second contact hole.

[0092] Step 14: forming a wiring layer on the second passivation layer.

[0093] Specifically, in this step, Fig.16 As shown, Cr with a thickness of 20 nm and Au with a thickness of 200 nm are prepared on the second passivation layer 11 by magnetron sputtering and photolithography etching as the lead layer 14 .

[0094] Step 15: Patterning the second passivation layer and the structural layer to define the mass block and cantilever beam regions.

[0095] Specifically, in this step, Fig.17 As shown, the quality block and the cantilever beam area are defined by photolithography and patterning, the second passivation layer 12 is etched by RIE, and then the polysilicon structure layer 8 is etched by ICP.

[0096] Step 16: Patterning the surface of the first substrate facing away from the first passivation layer to obtain through grooves penetrating the thickness of the first substrate.

[0097] Specifically, in this step, Fig.18 As shown, the lower surface of the first substrate 1 is patterned by photolithography, and deep silicon etching is performed by ICP process until the buried oxide layer 2 stops.

[0098] Step 17: Provide a second substrate, and connect a surface of the second substrate to a surface of the first substrate facing away from the first passivation layer to form a cavity.

[0099] Specifically, in this step, Fig.19 As shown, a 500 μm thick BF33 glass sheet is selected as the second substrate 15 , and the lower surface of the first substrate 1 is closely attached to the second substrate 15 through an anodic bonding process to form a cavity 16 .

[0100] Step 18: remove the sacrificial layer corresponding to the cavity portion, release the mass block and the cantilever beam, and simultaneously form a sensitive film to complete the preparation of the MEMS acceleration and pressure integrated sensor.

[0101] Specifically, in this step, Fig. 20 As shown, the PSG sacrificial layer 7 is corroded by HF to release the mass block 18 and the cantilever beam 19, and the sensitive film 17 is formed at the same time, thereby completing the preparation of the MEMS acceleration and pressure integrated sensor.

[0102] The preparation method of the MEMS acceleration and pressure integrated sensor of the disclosed embodiment adopts a stacking method to make the mass block and cantilever beam of the accelerometer above the sensitive film of the pressure sensor. This vertical integration structure saves 1 / 2 of the substrate area, greatly improves the integration level of the sensor chip, reduces production costs, and improves economic benefits. In addition, the sacrificial layer process is also used to complete the preparation of the sensitive film while releasing the mass block and the cantilever beam, which simplifies the process flow, reduces the process difficulty, reduces the production cost, and improves the economic benefits.

[0103] It is to be understood that the above embodiments are merely exemplary embodiments used to illustrate the principles of the present disclosure, but the present disclosure is not limited thereto. For those of ordinary skill in the art, various modifications and improvements can be made without departing from the spirit and substance of the present disclosure, and these modifications and improvements are also considered to be within the scope of protection of the present disclosure.

Claims

1. A MEMS acceleration and pressure integrated sensor, characterized in that: The integrated sensor comprises: A first substrate having a cavity extending through its thickness; A buried oxide layer, a device layer and a first passivation layer are sequentially stacked on the first substrate, and the three layers corresponding to the cavity together form a sensitive film; A first varistor and a first ohmic contact region are both embedded in a surface of the device layer facing away from the first substrate; A sacrificial layer, a structural layer, and a second passivation layer are sequentially stacked on the first passivation layer, the sacrificial layer being located outside the cavity, so that the structural layer and the second passivation layer are partially suspended corresponding to the cavity to form a mass block and a cantilever beam; A second varistor and a second ohmic contact region are both embedded in a surface of the structure layer of the suspended portion away from the first substrate; A lead layer and a metal filling layer, wherein the lead layer is disposed on a surface of the second passivation layer away from the first substrate, and the metal filling layer is electrically connected to the lead layer, the first ohmic contact region, and the second ohmic contact region respectively; The second substrate is connected to a surface of the first substrate facing away from the first passivation layer.

2. The MEMS acceleration and pressure integrated sensor according to claim 1, characterized in that: The integrated sensor includes a plurality of first piezoresistors; Each of the first varistors is located in a central area of ​​a corresponding side of the cavity.

3. The MEMS acceleration and pressure integrated sensor according to claim 2, characterized in that: The plurality of first varistors are connected via a first Wheatstone bridge.

4. The MEMS acceleration and pressure integrated sensor according to claim 1, characterized in that: The integrated sensor includes a plurality of second piezoresistors; At least two of the second varistors are distributed in the stress concentration area of ​​the cantilever beam, and the remaining second varistors are distributed in the zero stress area of ​​the cantilever beam.

5. The MEMS acceleration and pressure integrated sensor according to claim 4, characterized in that: The plurality of second varistors are connected via a second Wheatstone bridge.

6. The MEMS acceleration and pressure integrated sensor according to claim 4, characterized in that: The at least two second varistors at the stress concentration region of the cantilever beam are symmetrically distributed; and / or, The remaining second varistors at the zero stress region of the cantilever beam are symmetrically distributed.

7. The MEMS acceleration and pressure integrated sensor according to any one of claims 1 to 6, characterized in that: The metal filling layer penetrates the second passivation layer, the structural layer and the first passivation layer.

8. The MEMS acceleration and pressure integrated sensor according to claim 7, characterized in that: The integrated sensor further comprises an insulating layer; The insulating layer is disposed around the metal filling layer.

9. The MEMS acceleration and pressure integrated sensor according to any one of claims 1 to 6, characterized in that: The sacrificial layer is made of phosphosilicate glass; and / or the sacrificial layer has a thickness ranging from 1 μm to 10 μm.

10. A method for preparing a MEMS acceleration and pressure integrated sensor, characterized in that: include: Providing an SOI wafer; wherein the SOI wafer comprises a first substrate, a buried oxide layer and a device layer stacked in sequence; Doping the surface of the device layer to form a first varistor and a first ohmic contact region respectively; forming a first passivation layer on the surface of the device layer; forming a sacrificial layer on the surface of the first passivation layer, and patterning the sacrificial layer to form an annular groove; forming a structural layer on the surface of the sacrificial layer and in the annular groove; forming a second varistor and a second ohmic contact area on the surface of the structural layer respectively; forming a second passivation layer on the surface of the structural layer; Patterning the second passivation layer, the structural layer, the sacrificial layer and the first passivation layer to form a first contact through hole corresponding to the first ohmic contact area; forming an insulating layer on the inner sidewall of the first contact through hole, and filling the first contact through hole with a metal filling layer; Patterning the second passivation layer to form a second contact hole corresponding to the second ohmic contact area; forming a wiring layer on the second passivation layer; Patterning the second passivation layer and the structural layer to define a proof mass and a cantilever beam region; Patterning the surface of the first substrate facing away from the first passivation layer to obtain a through groove penetrating the thickness thereof; Providing a second substrate, and connecting a surface of the second substrate to a surface of the first substrate facing away from the first passivation layer to form a cavity; The sacrificial layer corresponding to the cavity portion is removed to release the mass block and the cantilever beam, and a sensitive film is formed at the same time, thereby completing the preparation of the MEMS acceleration and pressure integrated sensor.