One-step production process of magnesium stearate
Through one-step process and special equipment, environmental pollution and heavy metal residues in magnesium stearate production are solved, efficient and low-cost magnesium stearate production are achieved, and the lubricating performance and yield of the product are improved.
Patent Information
- Application Number
- CN202310948535.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-07-31
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing magnesium stearate production process has problems such as environmental pollution, long production cycle, high energy consumption, and heavy metal residues. The two-step process equipment has large investment, insufficient reaction, and uneven quality.
Using one-step process and specialized equipment, including glass reactors, centrifuges, dialysis purification devices, ovens, vibrating screens and high-energy ball mills, the heavy metal removal and particle size adjustment are achieved through the coating layer adsorption of catalysts and modified sepiolite adsorbents. , produce high-efficiency, low-heavy metal content of magnesium stearate finished products.
It realizes clean, environmentally friendly, time-saving and labor-saving magnesium stearate production, reduces heavy metal residues, improves the lubricating performance and yield of the product, and reduces the production cycle.
Smart Images

Figure CN117019032B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of organic synthesis, and in particular to a one-step production process for producing magnesium stearate. Background Art
[0002] The prior art mostly adopts a two-step production process, i.e., saponification reaction and double decomposition reaction to prepare magnesium stearate. Its production process produces a large amount of wastewater and waste inorganic salts, seriously pollutes the environment, and has the disadvantages of long production cycle, time-consuming and labor-intensive, high energy consumption, and difficult to manage. A small number of production companies adopt a dry production process, which has special requirements for equipment, large equipment investment, and has the disadvantages of insufficient reaction, uneven quality, unstable product quality, and long production cycle, thereby limiting the production scale. It is necessary to provide a clean, environmentally friendly, pollution-free, time-saving and labor-saving production process to replace the existing production process. The one-step production process of magnesium stearate can solve the disadvantages of the above two-step process.
[0003] At the same time, the sodium soap, the intermediate product of the two-step process, has high gelation energy, low solubility, and a viscous solution. It is easy to form stearic acid to synthesize acidic soap and is also easily salted out, which reduces the reaction activity. Nickel and cadmium elements are also easily introduced into the feed of the two-step process, resulting in heavy metal residues in the finished product. Summary of the invention
[0004] In order to solve the technical problems of heavy metal residue in magnesium stearate and two-step preparation of magnesium stearate in the prior art, the present invention provides a one-step production process and equipment for producing magnesium stearate.
[0005] In a first aspect, the present invention provides a one-step production device for producing magnesium stearate, comprising a glass reactor, a centrifuge, a dialysis purification device, an oven, a vibrating screen, a high-energy ball mill, a liquid inlet pipeline and a liquid infusion pipeline.
[0006] A stirring assembly is arranged at the top opening of the body of the glass reactor, and stirring blades of the stirring assembly extend from the top opening to the body of the glass reactor. A coating layer is arranged in the inner cavity of the body of the glass reactor, and the coating layer is an adhesive / PVA-boric acid / porous aluminum oxide foil layer. The PVA-boric acid hydrogel is used to seal the adsorption holes of the porous aluminum oxide foil layer and is evenly bonded to the porous aluminum oxide foil layer. The PVA-boric acid hydrogel has a large number of hydrogen bonds, so that the body of the glass reactor can tightly adsorb impurities.
[0007] The dialysis purification device includes an electrode substrate and a composite dialysis porous membrane layer. The composite dialysis porous membrane layer is a multilayer membrane structure of an outer protective film / PVA-boric acid sealing layer / diaphragm / solution layer of an iron-modified sepiolite adsorbent / diaphragm. The two layers of the diaphragm are sealed at the edges, the solution layer of the iron-modified sepiolite adsorbent is sealed and bonded to the outer protective film through the PVA-boric acid sealing layer, and the composite dialysis porous membrane layer is concave to form a dialysate receiving cavity.
[0008] Preferably, the thickness of the PVA-boric acid sealing layer is 1.5-3 mm.
[0009] Preferably, the solution layer containing the iron-modified sepiolite adsorbent contains 18-22 g / L of sepiolite adsorbent.
[0010] Furthermore, the iron-modified sepiolite adsorbent is a fibrous, chain-structured magnesium silicate with a structural formula of Si 12 Mg 8 O 30 (OH) 4 (OH 2 ) 4 •8H 2 O. Modification by iron ions can produce acid ions when iron ions are hydrolyzed and replace the Mg in the sepiolite structure. 2+ ions, micropores are transformed into mesopores, and iron ions are converted into Fe(OH) 3 During the electrodialysis process, heavy metal ions enter between the diaphragms and react with the iron-modified sepiolite adsorbent. + Ion or Mg 2+ Ion replacement, adsorption on the sepiolite. At the same time, PVA-boric acid seals the pores, and a large number of hydrogen bonds inside PVA-boric acid can adsorb and fix the sepiolite adsorbed with heavy metal ions.
[0011] The glass reactor transports the reaction product to the centrifuge through the infusion pipeline for dispersed centrifugation, and the centrifuge is passed into the dialysis purification device. After the dialysis purification device purifies the centrifuge to remove heavy metal elements, the centrifuge is placed in an oven for drying to obtain a coarse-grained magnesium stearate powder. The coarse-grained magnesium stearate powder is sieved and then subjected to high-energy ball milling to obtain a finished magnesium stearate product.
[0012] Preferably, the finished magnesium stearate has a particle size of 350-1560 nm and a bulk density of 0.085-0.25 g / mL. -1 Finished product.
[0013] By adopting high-energy ball milling and adjusting the high-energy ball milling parameters, magnesium stearate with small particle size can be obtained. The smaller the particle size, the less obvious the agglomeration phenomenon is, and the better the lubrication performance of magnesium stearate as a tablet is; at the same time, the smaller the bulk density, the fluffier the particle stacking is, and the better the lubrication performance is.
[0014] In a second aspect, the present invention provides a one-step production process for producing magnesium stearate, and provides a one-step production device for producing magnesium stearate, specifically comprising the following steps:
[0015] S100: weigh 65-80% of stearic acid, 25-30% of deionized water, 8-15% of magnesium hydroxide, and 0.6-1.0% of catalyst hydrogen peroxide, dissolve the magnesium hydroxide in the deionized water, and add alkali solution to adjust the pH to 10.5-11;
[0016] S200: placing the catalyst hydrogen peroxide in a glass reactor, stirring to allow the catalyst hydrogen peroxide to wet the coating layer of the inner cavity of the glass reactor, then adding stearic acid, stirring, heating to a temperature of 80-90° C., and completely dissolving the stearic acid, adding the magnesium hydroxide dissolved in deionized water in step S100, stirring fully, and maintaining the temperature at 80-90° C. When the pH value drops to 7.5-8, adding deionized water to the glass reactor to cool it down, and stirring fully to make it have a certain fluidity;
[0017] S300: The reaction product of step S200 is transported to a centrifuge through an infusion pipeline for dispersion and centrifugation. The speed of the centrifuge is controlled at 450-600 rpm. The centrifuge is passed into a dialysis purification device, the power is turned on, and the dialysis purification device purifies the centrifuge to remove heavy metal elements. The reaction is performed for 1.5-2 hours, and then the centrifuge is placed in an oven for drying to obtain a coarse-particle magnesium stearate powder. The drying temperature is controlled at 80-105°C.
[0018] S400: Placing the coarse-grained magnesium stearate powder in a vibrating screen for sieving, and passing through 100-150 mesh screens respectively, and sieving out powders of different particle sizes respectively, placing the powders of different particle sizes sifted out by the sifting ...
[0019] The beneficial effects achieved by the present invention are:
[0020] 1) Using 0.6%-1.0% weight ratio of hydrogen peroxide catalyst, within this mass range, the yield is high and the yield is stable;
[0021] 2) The hydrogen peroxide catalyst is introduced into the glass reactor to allow the catalyst hydrogen peroxide to wet the coating layer on the four walls of the glass reactor. The coating layer can enrich the catalyst hydrogen peroxide to avoid the heat release during the formation of magnesium stearate, which causes the catalyst hydrogen peroxide to decompose directly before catalysis;
[0022] 3) The coating layer is enriched with catalyst hydrogen peroxide, which can improve the temperature tolerance of the reaction system, allowing the reaction to proceed at a higher temperature and ensuring that the catalyst hydrogen peroxide will not decompose;
[0023] 4) The coating layer is a sandwich glue structure: adhesive / PVA-boric acid / porous aluminum foil layer. At the same time, the dialysis purification device adds a modified sepiolite adsorbent. By adjusting the thickness of PVA-boric acid and whether to add the modified sepiolite adsorbent, the heavy metal content in the finished product is controlled to be less than 9ppm;
[0024] 5) Screen the powder through the vibrating screen with 100-150 mesh screens, and screen out the powders with different particle sizes. High-energy ball milling with a ball-to-material ratio of (5-12):1, the ball milling time is 3-6 hours, and the ball milling time and ball milling ratio are adjusted according to the different particle sizes screened out to obtain a particle size of 350-1560nm and a bulk density of 0.085-0.25g / mL. -1 Finished magnesium stearate product. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0026] Figure 1 This is a production process flow chart of magnesium stearate produced by one-step method in this embodiment;
[0027] Figure 2 This is a structural diagram of the production equipment for producing magnesium stearate in one step in this embodiment. DETAILED DESCRIPTION
[0028] In order to more clearly understand the above-mentioned purpose, features and advantages of the present invention, the present invention is further described below in conjunction with the accompanying drawings and embodiments. It should be noted that the embodiments of the present application and the features in the embodiments can be combined with each other without conflict.
[0029] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments.
[0030] Example 1: A one-step production process for magnesium stearate is provided, the flow chart is as follows Figure 1 .
[0031] At the same time, we also provide one-step production equipment for magnesium stearate, such as Figure 2 .
[0032] Specific steps:
[0033] S100: According to the weight fraction, 70 kg of stearic acid, 30 kg of deionized water, 12 kg of magnesium hydroxide, and 0.6-1.0 kg of catalyst hydrogen peroxide with a purity of 98% are weighed, dissolved in the deionized water, and alkali solution is added dropwise to adjust the pH to 10.5-11;
[0034] S200: Open the liquid valve, and introduce the hydrogen peroxide catalyst into the glass reactor 5 through the catalyst feed pipe 1. The stirring assembly 7 stirs for 30 minutes to allow the catalyst hydrogen peroxide to wet the coating layer 6 on the four walls of the body of the glass reactor 5. The hydrogen peroxide is filled in the PVA-boric acid in the adhesive / PVA-boric acid / porous aluminum oxide foil layer of the coating layer 6 and the pores of the porous aluminum oxide foil layer. The PVA-boric acid hydrogel is used to seal the adsorption pores of the porous aluminum oxide foil layer and is evenly bonded to the porous aluminum oxide foil layer. The coating layer can enrich the catalyst hydrogen peroxide to avoid the heat release during the formation of magnesium stearate, which causes the catalyst hydrogen peroxide to directly decompose before catalysis.
[0035] Open the liquid valve, add stearic acid to the glass reactor 5 through the organic liquid inlet pipe 2, stir the stirring assembly 7 for 30 minutes, heat to a temperature of 80-90° C., and wait until the stearic acid is completely dissolved. Open the liquid valve, add the magnesium hydroxide dissolved in the deionized water in step S100 through the inorganic liquid inlet pipe 3, stir the stirring assembly 7 sufficiently, and keep the temperature at 80-90° C. When the pH value drops to 7.5-8, pump the deionized water into the glass reactor 5 through the air pump 12 to cool it down, and stir it sufficiently to make it have a certain fluidity;
[0036] S300: The reaction product of step S200 is transported to a centrifuge 8 through a liquid infusion pipeline 4 for dispersion and centrifugation. The speed of the centrifuge 8 is controlled at 450-600 rpm. The centrifuge is passed into a dialysis purification device 9. The power is turned on. The dialysis purification device 9 purifies the centrifuge to remove heavy metal elements. The reaction is performed for 1.5-2 hours. The centrifuge is then placed in an oven 10 for drying to obtain a coarse-grained magnesium stearate powder. The drying temperature is controlled at 80°C.
[0037] S400: The coarse-grained magnesium stearate powder is drawn into the vibrating screen 11 for sieving, and is passed through 100, 120, and 150 mesh screens respectively, and powders of different particle sizes are sieved out in three grades. The powders of different particle sizes sieved out by the graded screens are placed in a high-energy ball mill (not shown) for high-energy ball milling to obtain the magnesium stearate finished product.
[0038] Among them, the ball-to-material ratio is (5-12):1, the ball milling time is 3-6 hours, and the ball milling time and ball milling ratio are adjusted according to the different particle sizes screened out. The higher the mesh number of the sieve, the ball milling time is slightly reduced, and the ball-to-material ratio can be slightly reduced.
[0039] Example 2: Effect of adjusting catalyst content on yield
[0040] In Example 1, step S100 is selected without adding hydrogen peroxide catalyst as a control group;
[0041] By weight fraction, in step S100 in Example 1, 0.2%, 0.4%, 0.6%, 0.8%, and 1.0% of catalyst hydrogen peroxide were selected as experimental groups, and a certain reaction time was controlled to test the output yield. The data are shown in Table 1.
[0042] Table 1:
[0043]
[0044] It can be seen from Table 1 that with the addition of catalyst at the same reaction time, the yield is better than that of the control group without the addition of catalyst; at the same time, the more catalyst is added, the higher the yield is, and within the range of 0.6%-1.0%, the yield is high and stable.
[0045] In Example 1, step S100 chose not to add a hydrogen peroxide catalyst, and the yield was tested at different reaction times. The data are shown in Table 2.
[0046] Table 2:
[0047]
[0048] As shown in Table 2, without adding catalyst hydrogen peroxide, the reaction yield must reach 95% and at least 7 hours of reaction time is required, which is not conducive to large-scale production.
[0049] Example 3: Effect of adjusting reaction time on yield
[0050] In step S200 of Example 1, the reaction time was adjusted from 5 min to 20 min, the reaction temperature was controlled to be the same at 90° C., and the same dosage of 1.0% catalyst hydrogen peroxide was added to test the effect of the reaction time on the yield. The data are shown in Table 3.
[0051] Table 3:
[0052]
[0053] The reaction process can reach a yield of 99.8% within 10 minutes. The reasons are as follows: 1) a 1.0% dosage of hydrogen peroxide catalyst is added; 2) when the hydrogen peroxide catalyst is introduced into the glass reactor, the stirring assembly is stirred for 30 minutes to allow the catalyst hydrogen peroxide to wet the coating layer on the four walls of the glass reactor body. The coating layer can enrich the catalyst hydrogen peroxide to avoid the heat release during the formation of magnesium stearate, which causes the catalyst hydrogen peroxide to decompose directly before catalysis; 3) the coating layer is enriched with the catalyst hydrogen peroxide, which can improve the temperature resistance of the reaction system, so that the reaction can be carried out at a higher temperature and ensure that the catalyst hydrogen peroxide will not decompose.
[0054] Example 4: Testing the effects of different coating thicknesses and the presence or absence of modified sepiolite dialysis purification on heavy metal residues
[0055] The coating layer has a sandwich glue structure: PVA-boric acid and porous aluminum oxide foil layers in the adhesive / PVA-boric acid / porous aluminum oxide foil layer. The thickness of the porous aluminum oxide foil layer is adjusted to 2mm, 3mm, 4mm, 5mm, and 6mm, and the thickness of the PVA-boric acid film layer is 0.5mm, 1mm, and 1.5mm. The coating layer is applied to the glass reactor body. At the same time, the dialysis purification process is tested whether modified sepiolite is added between the diaphragm layers, and the heavy metal residues in the finished product under different conditions are tested.
[0056] The main heavy metals are chromium and nickel. After the finished product is made, atomic absorption spectrometry combined with mass spectrometry is used to test the residual heavy metal elements.
[0057] Table 4:
[0058]
[0059] The PVA-boric acid membrane layer was controlled to be 1 mm, modified sepiolite was added between the dialysis purification process, the reaction time was controlled to be 15 min and the hydrogen peroxide catalyst dosage was 1%, the thickness of the porous aluminum oxide foil layer was adjusted, and the yield data was tested. As shown in Table 4, there was no significant linear relationship between the thickness of the porous aluminum oxide foil layer and the yield, and there was no significant linear relationship between the heavy metal content and the thickness of the aluminum oxide foil layer.
[0060] Table 5:
[0061]
[0062] The porous aluminum foil layer was controlled to be 5 mm, modified sepiolite was added between the dialysis purification process, the reaction time was controlled to be 15 min and the hydrogen peroxide catalyst dosage was 1%, the thickness of the PVA-boric acid film was adjusted, and the yield data were tested. As shown in Table 5, there was a significant positive linear correlation between the thickness of the PVA-boric acid film and the yield, and there was also a significant positive linear correlation between the heavy metal content and the thickness of the PVA-boric acid film. This was mainly due to the large number of hydrogen bonds in the PVA-boric acid film, which increased the adsorption of heavy metal inorganic salt impurities in the feed and the reaction feed residues, increased the purity of the finished product, and at the same time enhanced the adsorption of heavy metal elements, which further increased the yield of the finished product.
[0063] The magnesium stearate prepared in this embodiment has a high yield, a rapid reaction process, and a heavy metal content in the product is significantly lower than 9ppm. At the same time, through high-energy ball milling, the obtained product has excellent wetting properties, a particle size of 350-1560nm, and a bulk density of 0.085-0.25g / mL. -1 Finished magnesium stearate product.
[0064] Through the above specific implementations, those skilled in the art can easily implement the present invention. However, it should be understood that the present invention is not limited to the above specific implementations. On the basis of the disclosed implementations, those skilled in the art can arbitrarily combine different technical features to achieve different technical solutions.
Claims
1. A one-step production process for magnesium stearate, characterized in that: Providing a production equipment for preparing the magnesium stearate, comprising a glass reactor containing a coating layer, a centrifuge, a dialysis purification device, an oven, a vibrating screen, a high-energy ball mill, a liquid inlet pipeline and a liquid infusion pipeline; The steps are: S100: weigh 65-80% of stearic acid, 25-30% of deionized water, 8-15% of magnesium hydroxide, and 0.6-1.0% of catalyst hydrogen peroxide, dissolve the magnesium hydroxide in the deionized water, and add alkali solution to adjust the pH to 10.5-11; S200: placing the catalyst hydrogen peroxide in the glass reactor, stirring, allowing the catalyst hydrogen peroxide to wet the coating layer in the inner cavity of the glass reactor body, then adding the stearic acid, stirring, heating until the stearic acid is completely dissolved, adding the magnesium hydroxide dissolved in the deionized water in step S100, stirring and heating fully, and when the pH value drops to 7.5-8, adding deionized water to the glass reactor to cool down; the coating layer of the glass reactor body is a sandwich structure of adhesive / PVA-boric acid / porous aluminum oxide foil layer, and the PVA-boric acid is used to seal the adsorption holes of the porous aluminum oxide foil layer and is evenly bonded to the porous aluminum oxide foil layer; S300: The reaction product of step S200 is transported to the centrifuge through the infusion pipeline for dispersion centrifugation, the speed of the centrifuge is controlled at 450-600 rpm, the centrifuge is passed into the dialysis purification device, the power is turned on, the dialysis purification device purifies the centrifuge to remove heavy metal elements, the reaction is performed for 1.5-2 hours, and then the centrifuge is placed in the oven for drying to obtain a coarse-grained magnesium stearate powder; S400: Placing the coarse-grained magnesium stearate powder in the vibrating screen for sieving, respectively passing through a 100-150 mesh screen, and sieving out powders of different particle sizes, and placing the sifted powders of different particle sizes in the high-energy ball mill for high-energy ball milling to obtain the magnesium stearate finished product.
2. The production process for producing magnesium stearate by one-step method as claimed in claim 1, characterized in that: In step S200, the temperature is heated to 80-90°C to dissolve the stearic acid.
3. The production process for producing magnesium stearate in one step as claimed in claim 1, characterized in that: The reaction temperature is maintained at 80-90° C., and the magnesium hydroxide is added in step S200 to react.
4. The production process for producing magnesium stearate in one step as claimed in claim 1, characterized in that: The drying temperature is controlled at 80-105℃.
5. The production process for producing magnesium stearate by one-step method as claimed in claim 1, characterized in that: The ball-to-material ratio of high-energy ball milling is (5-12):1, and the ball milling time is 3-6 hours.
6. The production process for producing magnesium stearate in one step as claimed in claim 5, characterized in that: According to the different particle sizes of magnesium stearate powder screened out by graded screening, the ball milling time and ball-to-material ratio were adjusted to obtain a particle size of 350-1560nm and a bulk density of 0.085-0.25g / mL -1 Finished magnesium stearate product.
7. The production process for producing magnesium stearate in one step as claimed in claim 1, characterized in that: The thickness of the PVA-boric acid is 0.5-1.5 mm.
8. The production process for producing magnesium stearate in one step as claimed in claim 1, characterized in that: The dialysis purification device comprises an electrode substrate and a composite dialysis porous membrane layer, wherein the composite dialysis porous membrane layer is a multilayer membrane structure of an outer protective film / PVA-boric acid sealing layer / diaphragm / solution layer of an iron-modified sepiolite adsorbent / diaphragm; The two layers of the diaphragm are sealed to seal the solution layer of the iron-modified sepiolite adsorbent, and are bonded to the outer protective film through the PVA-boric acid sealing layer. The composite dialysis porous membrane layer is concave to form a dialysis liquid receiving cavity.
9. The production process for producing magnesium stearate in one step as claimed in claim 8, characterized in that: The solution layer of the iron-modified sepiolite adsorbent contains 18-22 g / L of sepiolite adsorbent; and the thickness of the PVA-boric acid sealing layer is 1.5-3 mm.