A kind of black plum residue xanthate material and its preparation method and application

By preparing the ebony residue xanthate material and using it to efficiently remove heavy metals in heavy metal-contaminated soil, the problem of low removal efficiency of waste biomass source solubilizer materials in the existing technology has been solved, and the efficient removal of heavy metals in the soil has been achieved. Resource reuse reduces restoration costs and pollution risks.

CN117138759BActive Publication Date: 2024-10-29INST OF SOIL SCI CHINESE ACAD OF SCI
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311120155.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-09-01
Publication Date
2024-10-29
Estimated Expiration
2043-09-01

AI Technical Summary

Technical Problem

Existing waste biomass source solubilizer materials have low removal efficiency of heavy metals, and their removal and reuse process of heavy metals in soil elution waste liquid have not been effectively studied, which limits their application in the reduction and remediation of heavy metal-contaminated soil in cultivated land. .

Method used

By alkalizing and yellowing the ebony dregs with sodium hydroxide and carbon disulfide, and then adding magnesium sulfate for ion exchange and setting reaction, the ebony dregs xanthate material is prepared to improve its removal rate of heavy metals and achieve Its application and recycling in heavy metal contaminated soil.

Benefits of technology

The ebony residue xanthate material significantly improves the removal rate of heavy metals and can efficiently remove heavy metals in the soil. Its preparation method is recyclable, reducing remediation costs and reducing the risk of secondary pollution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117138759B_ABST
    Figure CN117138759B_ABST
Patent Text Reader

Abstract

The present invention belongs to the technical field of soil treatment, and provides a xanthate material of ebony residues, and a preparation method and application thereof. The preparation method of the xanthate material of ebony residues provided by the present invention comprises the following steps: mixing ebony residues with a first sodium hydroxide solution, alkalizing, and obtaining alkalized ebony residues; mixing the alkalized ebony residues, a second sodium hydroxide solution, and carbon disulfide, and performing yellowing; after the yellowing, adding a magnesium sulfate solution to the obtained yellowing liquid, performing ion exchange and shaping reaction, and obtaining the xanthate material of ebony residues. The preparation method provided by the present invention alkalizes the ebony residues, can decompose the fibers in the ebony residues, and release a large number of hydroxyl groups; then performing yellowing, and then grafting the active groups onto the ebony residues through the decomposed hydroxyl groups, providing sites for the subsequent complexation of heavy metals, thereby improving the heavy metal removal rate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of soil treatment, and in particular to a xanthate material of ebony dregs, and a preparation method and application thereof. Background Art

[0002] Waste biomass-derived solubilizing materials based on chemical solubilization methods are considered to be an emerging green, low-carbon and sustainable mild remediation technology due to their advantages of being environmentally friendly, low-cost and resource-recycling, and they overcome the shortcomings of soil structure destruction (acid and alkali), soil nutrient loss, poor degradability (EDTA) and high application cost (EDDS) after soil remediation using traditional inorganic and synthetic cleaning agents. However, the current research on the reduction of heavy metals by waste biomass-derived solubilizing materials is still very limited, mainly because the existing waste biomass-derived solubilizing materials have the problem of low efficiency in removing heavy metals.

[0003] Soil cleaning can effectively repair soil contaminated by heavy metals, and the treatment, recycling and reuse of elution waste liquid is an effective way to reduce the risk of secondary pollution of surrounding soil and groundwater, reduce the cost of remediation and realize the reuse of waste resources. However, the current soil remediation research mainly focuses on the soil heavy metal cleaning process, while the removal and reuse of heavy metals in soil elution waste liquid using friendly waste biomass as materials has not yet been carried out, and the solubilization and discharge of heavy metals in cultivated soil and elution liquid based on biomass solubilizers and their leaching residues. The chain-type synergistic reduction and remediation effect, microscopic mechanism and soil environmental quality risk assessment model have not been reported. This has also become a technical bottleneck limiting the application of this technology in the reduction and remediation of cultivated heavy metal contaminated soil. Therefore, it is crucial to screen and modify and optimize agricultural and forestry biomass adsorption materials with a wide range of sources, economic availability and high efficiency for the rapid and effective removal and resource reuse of heavy metals in elution waste liquid after farmland soil leaching. Summary of the invention

[0004] In view of this, the object of the present invention is to provide a xanthate material of ebony dregs and a preparation method and application thereof. The xanthate material of ebony dregs obtained by the preparation method provided by the present invention has a high removal rate of heavy metals and can be recycled.

[0005] In order to achieve the above-mentioned object of the invention, the present invention provides the following technical solutions:

[0006] The present invention provides a method for preparing a xanthate material of ebony dregs, comprising the following steps:

[0007] Mixing the ebony residue with the first sodium hydroxide solution and alkalizing to obtain alkalized ebony residue;

[0008] The alkalized ebony residue, the second sodium hydroxide solution and carbon disulfide are mixed to perform xantholysis;

[0009] After the yellowing, a magnesium sulfate solution is added to the obtained yellowing liquid to carry out ion exchange and setting reaction to obtain the black plum residue xanthate material.

[0010] Preferably, the mass concentration of the first sodium hydroxide solution is 10-30%, and the dosage ratio of the ebony residue to the first sodium hydroxide solution is 10g:200mL-10g:400mL;

[0011] The alkalization temperature is room temperature, the time is 12 to 48 hours, and the alkalization is carried out under stirring, and the stirring speed is 100 to 250 rpm.

[0012] Preferably, the mass concentration of the second sodium hydroxide solution is 5-20%, and the usage ratio of the ebony residue, the second sodium hydroxide solution and carbon disulfide is 10g:200mL:10mL-10g:400mL:10mL;

[0013] The yellowing temperature is room temperature, the time is 3 to 6 hours, and the yellowing is carried out under stirring.

[0014] Preferably, the mass concentration of the magnesium sulfate solution is 5-10%, the dosage ratio of the ebony residue to the magnesium sulfate solution is 10g:100mL-10g:150mL; the temperature of the ion exchange and shaping reaction is room temperature, and the time is 0.5-2h; the ion exchange and shaping reaction is carried out under stirring.

[0015] Preferably, after the ion exchange and shaping reaction, the method further comprises: filtering, washing and drying the obtained ion exchange and shaping reaction liquid in sequence.

[0016] Preferably, the method for preparing the ebony residue comprises the following steps:

[0017] Mixing black plums with water and performing extraction to obtain black plum residue;

[0018] Mixing the ebony residue with water and performing extraction to obtain the ebony residue;

[0019] During the extraction, the ratio of the black plum to water is 1g:10mL to 1g:30mL, the extraction temperature is 80 to 100°C, and the extraction time is 1 to 6h;

[0020] During the extraction, the ratio of the black plum residue to water is 25g:1L-100g:1L, and the extraction method is shaking on a shaking table; the shaking table has an oscillation temperature of 22-28°C, a rotation speed of 120-180rpm, and a time of 1-6h.

[0021] The present invention also provides a xanthate material of ebony residues obtained by the preparation method described in the above technical scheme.

[0022] The present invention also provides the use of the black plum medicinal residue xanthate material described in the above technical solution in heavy metal contaminated soil.

[0023] Preferably, the steps include:

[0024] Mixing the xanthate material of the ebony residue, the heavy metal-contaminated soil to be treated and a liquid solvent for solubilization treatment;

[0025] The dosage ratio of the ebony residue xanthate material, the heavy metal contaminated soil to be treated and the liquid solvent is 1g:2g:40mL to 1g:400g:400mL;

[0026] The liquid solvent is water or a filtrate obtained by solubilization treatment;

[0027] The solubilization treatment time is 0.5 to 3 hours.

[0028] Preferably, after the solubilization treatment, the method further comprises: filtering the obtained solubilization treatment liquid to obtain a filtrate; mixing the filtrate, the ebony residue xanthate material and the heavy metal contaminated soil to be treated, and performing a solubilization treatment again to achieve recycling of the filtrate.

[0029] The present invention provides a method for preparing a xanthate material of ebony residues, comprising the following steps: mixing ebony residues with a first sodium hydroxide solution, alkalizing, and obtaining alkalized ebony residues; mixing the alkalized ebony residues, a second sodium hydroxide solution, and carbon disulfide, and performing xanthation; after the xanthation, adding a magnesium sulfate solution to the obtained xanthate solution, performing ion exchange and shaping reactions, and obtaining the xanthate material of ebony residues. The preparation method provided by the present invention alkalizes the ebony residues, can decompose the fibers in the ebony residues, and release a large number of hydroxyls; then performing xanthation, and then grafting active groups onto the ebony residues through the decomposed hydroxyls, providing sites for subsequent complexation of heavy metals, and thus improving the heavy metal removal rate. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 It is a flow chart for the preparation of xanthate materials of ebony dregs;

[0031] Figure 2 The following are the SEM photos and EDS spectra of Wumei medicinal residue;

[0032] Figure 3 SEM photos and EDS spectra of xanthate materials of Wumei medicinal residues

[0033] Figure 4The removal effect of Cd in alkaline soil and acidic soil by direct solubilization of the solution and its effluent is shown in the figure;

[0034] Figure 5 This is a diagram showing the removal effect of Cd in alkaline and acidic soils by composite solubilization of the solution and its effluent. DETAILED DESCRIPTION

[0035] The present invention provides a method for preparing a xanthate material of ebony dregs, comprising the following steps:

[0036] Mixing the ebony residue with the first sodium hydroxide solution and alkalizing to obtain alkalized ebony residue;

[0037] The alkalized ebony residue, the second sodium hydroxide solution and carbon disulfide are mixed to perform xantholysis;

[0038] After the yellowing, a magnesium sulfate solution is added to the obtained yellowing liquid to carry out ion exchange and setting reaction to obtain the black plum residue xanthate material.

[0039] In the present invention, unless otherwise specified, the raw materials used in the present invention are preferably commercially available products.

[0040] Figure 1 This is a flow chart for the preparation of ebony dregs xanthate materials. Figure 1 The preparation process of xanthate material from ebony residue is described in detail.

[0041] The invention mixes the ebony residues with a first sodium hydroxide solution and performs alkalization to obtain the alkalized ebony residues.

[0042] In the present invention, the method for preparing the ebony dregs preferably comprises the following steps:

[0043] Mixing black plums with water and performing extraction to obtain black plum residue;

[0044] The ebony residue is mixed with water and extracted to obtain the ebony residue.

[0045] In the present invention, during the extraction, the ratio of the amount of the ebony and water is preferably 1g:10mL~1g:30mL, more preferably 1g:15mL~1g:25mL; the temperature of the extraction is preferably 80~100°C, more preferably 90°C; the time is preferably 1~6h, more preferably 3h. In the present invention, during the extraction, the ratio of the amount of the ebony residue and water is preferably 25g:1L~100g:1L, more preferably 50g:1L, the extraction method is preferably shaking; the temperature of the shaking table is preferably 22~28°C; the rotation speed is preferably 120~180rpm; the time is preferably 1~6h, more preferably 3h.

[0046] In the present invention, the mass concentration of the first sodium hydroxide solution is preferably 10-30%, and more preferably 20%; the dosage ratio of the ebony residue to the first sodium hydroxide solution is preferably 10g:200mL-10g:400mL, and more preferably 10g:250mL-10g:350mL.

[0047] In the present invention, the alkalization temperature is preferably room temperature; the time is preferably 12 to 48 hours, more preferably 24 hours; the alkalization is preferably carried out under stirring; the stirring speed is preferably 100 to 250 rpm, more preferably 150 to 200 rpm.

[0048] After the alkalization, the present invention preferably further comprises filtering the obtained alkalized liquid, washing and drying the obtained filter residue. In the present invention, the filtration is preferably bag filtration. In the present invention, the washing agent is preferably water, and the water is preferably distilled water; the number of washings is preferably 3 times. In the present invention, the drying temperature is preferably 60°C, and the drying time is preferably 15h.

[0049] After obtaining the alkalized black plum residue, the present invention mixes the alkalized black plum residue, a second sodium hydroxide solution and carbon disulfide to perform xantholysis.

[0050] In the present invention, the mass concentration of the second sodium hydroxide solution is preferably 5 to 20%, and more preferably 10 to 15%. In the present invention, the usage ratio of the ebony residue, the second sodium hydroxide solution and carbon disulfide is preferably 10g:200mL:10mL to 10g:400mL:10mL.

[0051] In the present invention, the yellowing temperature is preferably room temperature; the time is preferably 3 to 6 hours; and the yellowing is preferably carried out under stirring.

[0052] After the yellowing, the present invention adds a magnesium sulfate solution to the obtained yellowing liquid to carry out ion exchange and shaping reaction to obtain the black plum residue xanthate material.

[0053] In the present invention, the mass concentration of the magnesium sulfate solution is preferably 5-10%, and the dosage ratio of the ebony residue to the magnesium sulfate solution is preferably 10g:100mL-10g:150mL. In the present invention, the temperature of the ion exchange and shaping reaction is preferably room temperature; the time is preferably 0.5-2h; and the ion exchange and shaping reaction is preferably carried out under stirring.

[0054] After the ion exchange and shaping reaction, the present invention preferably further comprises: filtering, washing and drying the obtained ion exchange and shaping reaction liquid in sequence. The present invention does not specifically limit the amount and number of reagents for the washing, and washing until the pH is close to neutral. In the present invention, the drying temperature is preferably room temperature.

[0055] The present invention also provides a xanthate material of ebony residues obtained by the preparation method described in the above technical scheme.

[0056] The present invention also provides the use of the black plum medicinal residue xanthate material described in the above technical solution in heavy metal contaminated soil.

[0057] In the present invention, when the ebony residue xanthate material is applied to heavy metal contaminated soil, the method preferably includes the following steps:

[0058] The xanthate material of ebony residue, the heavy metal contaminated soil to be treated and a liquid solvent are mixed for solubilization treatment.

[0059] In the present invention, the liquid solvent is water or a filtrate obtained by solubilization treatment.

[0060] In the present invention, the dosage ratio of the ebony residue xanthate material, the heavy metal contaminated soil to be treated and the liquid solvent is preferably 1g:2g:40mL to 1g:400g:400mL, and more preferably 1g:20g:40mL.

[0061] In the present invention, the solubilization treatment time is preferably 0.5 to 3 hours, more preferably 1 hour.

[0062] After the solubilization treatment, the present invention preferably further comprises: filtering the obtained solubilization treatment liquid to obtain a filtrate; mixing the filtrate, the black plum residue xanthate material and the heavy metal contaminated soil to be treated, and performing a solubilization treatment again to achieve recycling of the filtrate.

[0063] In the present invention, the dosage ratio of the filtrate, the ebony residue xanthate material and the heavy metal contaminated soil to be treated is preferably adjusted according to actual conditions.

[0064] The ebony residue xanthate material provided by the present invention and its preparation method and application are described in detail below in conjunction with the embodiments, but they should not be construed as limiting the scope of protection of the present invention.

[0065] The main materials used in the following examples are:

[0066] The test soils were real heavy metal contaminated soils, and the test soils were alkaline soils (Gansu Baiyin dryland gray calcium soil: N 36°31′59", E 104°9′6") and acidic soils (Jiangsu Taicang farmland paddy soil: 31°22′08″N, 121°06′48″E). The pH of the alkaline soil was 8.78, and the Cd content was 0.78 mg / kg. The pH of the acidic soil was 6.51, and the Cd content was 0.79 mg / kg.

[0067] Wumei was purchased from Heentang Co., Ltd., Bozhou City, Anhui Province.

[0068] Carbon disulfide (CS2) was purchased from Sinopharm Group.

[0069] Dicarboxymethylalanine (MGDA) was purchased from Shandong Taihe Water Treatment Co., Ltd.

[0070] Example 1

[0071] Preparation of xanthate material from ebony dregs:

[0072] Take 10.00g of black plum residue (RPM) and pass it through a 10-mesh sieve, place it in a 1.00L large beaker, add 200.00mL of NaOH solution with a mass concentration of 20.0%, and stir for 24h in an electric stirrer at 200rpm (S212-90B, Shanghai Shensheng Biotechnology Co., Ltd.) for alkalization. After the alkalization is completed, filter it with a bag filter and wash it with distilled water for 3 times, and dry it below 60℃ for 15h to obtain the alkalized black plum residue. At room temperature and pressure, the alkalized black plum residue was placed in a 1.00L beaker, 200.00mL of 10.0% NaOH solution was added, 10.00mL CS2 was added, and the mixture was stirred at room temperature for 3h for yellowing. After yellowing, 100.0mL of 5.0% MgSO4 solution was added, and the mixture was stirred for 30min. After filtration, the residue was rinsed with water until the pH was close to neutral, and dried at room temperature to obtain the black plum residue xanthate material (RPMX).

[0073] The method for obtaining the ebony dregs comprises the following steps:

[0074] Wash the black plums, dry them in an oven at 60°C, and crush them through a 2mm sieve. The crushed black plums are processed according to the traditional Chinese medicine decoction method, that is, the medicine-water ratio is 1:30 (g / v), 8g of the crushed black plums are weighed and placed in a 250mL conical flask, 240mL of deionized water is added, and the mixture is heated in a water bath and extracted at a constant temperature of 90°C for 3h, left to cool, filtered after cooling, and dried to obtain the black plum residue.

[0075] Weigh 30.00 g of ebony residue and put it into a 500.00 mL plastic bottle, add 300 mL of deionized water (the ratio of ebony residue to water is 1:10), shake in a shaker at 28°C and 180 rpm for 3 h, filter, and dry the resulting filter residue to obtain ebony residue.

[0076] Test Case

[0077] Characterization and adsorption properties of xanthate from ebony residue

[0078] Scanning electron microscope energy spectrum (SEM-EDS) analysis:

[0079] Unmodified ebony residue (RPM) and ebony residue xanthate material (RPMX) were freeze-dried and ground to obtain powders. After gold spraying, the morphology was collected and analyzed using a cold field emission scanning electron microscope (HITACHI S-4800, SEM, Japan).

[0080] SEM and EDS were used to characterize the microstructure and element distribution of ebony residue and ebony residue xanthate materials. Figure 2 and Figure 3 shown. Figure 2 The SEM and EDS images of Wumei medicinal residue are shown below. Figure 2 In the middle, the left picture is the SEM picture, and the right picture is the EDS picture. Figure 3 These are the SEM and EDS images of the xanthate material of the ebony dregs. Figure 3 The left picture is the SEM picture, and the right picture is the EDS picture. Figure 2 The left picture shows that the surface structure of RPM is orderly and smooth. Figure 3 The left figure shows that the structure of the ebony residue xanthate material (RPMX) has changed greatly compared to RPM. The surface is loose, the layers are more, there are more protruding particles, and the specific surface area is increased. The possible reason for this phenomenon is that during the alkalization and xanthation treatment, part of the hemicellulose and lignin in the ebony residue were removed, and the structure between each single fiber was loose. At the same time, the composition structure of cellulose was changed, and the xanthate group was introduced. Na + Mg 2+ All of them were successfully connected to the material surface, enhancing the adsorption capacity of RPMX for Cd in the effluent.

[0081] Adsorption performance of ebony residue xanthate material on Cd in wastewater:

[0082] Weigh 20.00 mg CdCl2 into a 1000 mL volumetric flask, add deionized water to make up to volume, and prepare a 20 mg / L CdCl2 solution. Take 20.00 mL of the prepared 20 mg / L CdCl2 solution into a 50 mL centrifuge tube, add 0.50 g RPM and RPMX respectively, oscillate in a centrifuge for 3 h, centrifuge and filter, measure the Cd content in the solution by ICP-MS, calculate the adsorption capacity of the xanthate of the ebony residue for Cd, and repeat the experiment three times.

[0083] The Cd adsorption capacity of ebony residue and ebony residue xanthate materials for self-prepared Cd solution was compared, and the results are shown in Table 1.

[0084] Table 1 Adsorption effect of the residues of Wumei medicinal residues on Cd before and after modification

[0085]

[0086] Note: RPM: residue extracted from ebony dregs; RPMX: modified ebony dregs xanthate.

[0087] As can be seen from Table 1, the Cd adsorption capacity of the ebony residue xanthate material (RPMX) is significantly improved compared with the ebony residue (RPM), and the adsorption and removal efficiency of Cd increases from 13.6% to 91.5%, proving that the xanthate treatment can effectively improve the adsorption capacity of ebony residue for Cd. Under the condition of 1:40 dosage, the adsorption capacity of RPMX for Cd is 6.40 mg / g.

[0088] Example 3

[0089] Purification effect and circulation method of solubilized effluent

[0090] Preparation of black plum residue solubilizer: weigh 30.00g black plum and put it into a 1.00L plastic bottle, add 900.00mL deionized water, put it into a 90℃ water bath, extract it at constant temperature for 3h, filter it with a filter bag to get the filter residue, dry it naturally and crush it to get black plum residue with a particle size of 2mm; do three groups of parallel, and get a total of 90.00g black plum residue. Weigh 15.00g black plum residue and put it into a 500.00mL plastic bottle, add 300mL deionized water, shake it in a shaker at 28℃ and 180rpm for 3h, and get a black plum residue solubilizer with a concentration of 50g / L. Do three groups of parallel, and get a total of 600mL black plum residue solubilizer.

[0091] Dicarboxymethylalanine (MGDA) and 50 g / L of Prunus mume residue solubilizer were mixed at a dosage ratio of 0.34 g:1 L to obtain a biodegradable composite solubilizer (RPMG3).

[0092] The biodegradable composite solubilizer RPMG3 was used to solubilize alkaline soil and acidic soil under the optimized solubilization conditions (pH 5.0, liquid-to-soil ratio 2:1, time 1h). After the treatment, the waste liquid was collected by centrifugation and filtration as the solubilization discharge liquid.

[0093] RPMX and the solubilized effluent were mixed at a ratio of 1 g:40 mL, shaken in a shaker at 180 rpm for 3 h for purification, and centrifuged to obtain a solubilized and purified effluent; the Cd concentration in the solubilized and purified effluent was determined.

[0094] The above process is called one solubilization and one purification, and the same solubilization and purification process is combined into a set of cyclic solubilization processes.

[0095] The primary solubilization and purification effluent was subjected to recycling tests under the optimized solubilization conditions (pH 5.0, liquid-to-soil ratio 2:1, time 1h) in the following two ways:

[0096] (1) Direct circulation: the once-solubilized and once-purified effluent is directly solubilized with untreated alkaline soil and acidic soil, and the solubilized effluent is mixed with RPMX for purification; the soil solubilization is repeated twice and the effluent purification is repeated once, which are recorded as secondary solubilization, secondary purification, and tertiary solubilization, respectively.

[0097] After the first purification and the second purification, the removal rate of cadmium in the solubilized effluent obtained after the solubilization treatment is shown in Table 2.

[0098] Table 2 Removal effect of RPMX on Cd solubilization in effluent

[0099]

[0100] Note: Lowercase letters in the same column indicate significant differences between means.

[0101] It can be seen from Table 2 that the removal efficiency of Plum dregs xanthate material (RPMX) for Cd solubilization in alkaline soil and acidic soil effluent can reach 97.0% to 99.4%, and the Cd concentration in the purified solubilized effluent reaches the standard value of agricultural irrigation water quality (Cd 0.01 mg / L).

[0102] The removal rates of cadmium in alkaline soil and acidic soil after the first, second and third solubilization treatments are as follows: Figure 4 As shown. Figure 4It can be seen that the purified solubilized effluent still has a certain ability to remove Cd in untreated alkaline soil and acidic soil. However, compared with the single solubilization, the removal efficiency of Cd has decreased significantly, and with the increase in the number of solubilization times, the removal efficiency of Cd has also continued to decrease, and the residual Cd concentration in the soil still exceeds the screening value (Cd, 0.60 mg / kg). The main reason for this phenomenon is that the concentrations of effective ingredients such as soluble organic carbon (DOC) and MGDA in the biodegradable composite solubilizer RPMG3 decrease with the increase in the number of cycles. Therefore, direct circulation solubilization after the solubilization effluent is purified is not suitable for actual field applications.

[0103] (2) Composite cycle: The once-solubilized and once-purified effluent was mixed with a biodegradable composite solubilizer (RPMG3) at a volume ratio of 1:1, 1:1.5, and 1:2, respectively, to obtain a mixed composite solubilizer; the mixed composite solubilizer was solubilized with untreated alkaline soil and acidic soil, and the obtained solubilized effluent was mixed with RPMX for purification; the soil solubilization was repeated twice and the effluent purification was repeated once, which were recorded as secondary solubilization, secondary purification, and tertiary solubilization, respectively.

[0104] After the solubilization effluent was purified once and twice, the removal rate of cadmium in the solubilized effluent obtained after solubilization treatment is shown in Table 3. After the solubilization treatment once, twice and three times, the removal rate of cadmium in alkaline soil and acidic soil is shown in Table 3. Figure 5 shown.

[0105] Table 3 Removal effect of RPMX on Cd solubilization in effluent

[0106]

[0107] Note: Lowercase letters in the same column indicate significant differences between means.

[0108] From Table 3 and Figure 5It can be seen that after the first solubilization, the Cd content in the effluent was between 0.25mg / L and 0.26mg / L, and the Cd adsorption removal effect of RPMX on the solubilized effluent was stable at more than 93.4%. After purification by RPMX, the Cd content in the effluent was not detected, meeting the agricultural irrigation water quality standard value (Cd 0.01mg / L, GB5084-2021). When the purified effluent was mixed with the RPMG3 stock solution at a ratio of 1:1, 1:1.5, and 1:2, it was found that the removal efficiency of Cd by the second and third solubilizations was lower than that of the first solubilization. However, with the increase in the number of solubilizations, the removal efficiency of soil Cd by the biodegradable composite solubilizer was relatively stable between 26.3% and 30.1%, and the residual Cd content in the soil was reduced to below the screening value, so that the soil could meet the safety production and utilization standards. When the effluent and RPMG3 stock solution were mixed in a volume ratio of 1:2, the removal efficiency of Cd in the soil was optimal through compound circulation solubilization. This was mainly because the addition of stock solution to the effluent directly supplemented the amount of substances in the solution that could undergo complexation reactions with Cd, and with the increase in the supplement ratio, the removal efficiency of Cd was significantly improved.

[0109] Table 4 gives the field application costs of MGDA in the combined cycle.

[0110] Table 4 Field application cost of MGDA in compound cycle

[0111]

[0112]

[0113] From Table 4, we can find that the 1:1 compound circulation solubilization can not only ensure that alkaline soil and acidic soil meet the safe production conditions, but also reduce the field application cost by 50% (from 930.90 yuan to 465.45 yuan) when repairing the second mu of polluted farmland soil. With the increase of the repair area, the average repair cost per mu of land is also decreasing. Therefore, the compound circulation clean soil after the compound Chinese medicine residue solubilizer and its effluent purification is an economical, efficient, simple and convenient soil leaching and repair technology with potential application prospects.

[0114] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. A method for preparing a xanthate salt material of ebony dregs, characterized in that: The following steps are involved: Mixing the ebony residue with the first sodium hydroxide solution and alkalizing to obtain alkalized ebony residue; The alkalized ebony residue, the second sodium hydroxide solution and carbon disulfide are mixed to perform xantholysis; After the yellowing, a magnesium sulfate solution is added to the obtained yellowing liquid to carry out ion exchange and setting reaction to obtain the black plum residue xanthate material; The mass concentration of the first sodium hydroxide solution is 20%, and the amount ratio of the ebony residue to the first sodium hydroxide solution is 10g:200mL; The alkalization temperature is room temperature, the time is 24 hours, and the alkalization is carried out under stirring conditions, and the stirring speed is 100-250 rpm; The mass concentration of the second sodium hydroxide solution is 10%, and the amount ratio of the ebony residue, the second sodium hydroxide solution and carbon disulfide is 10g:200mL:10mL; The yellowing temperature is room temperature, the time is 3 hours, and the yellowing is carried out under stirring; The mass concentration of the magnesium sulfate solution is 5%, and the dosage ratio of the ebony residue to the magnesium sulfate solution is 10g:100mL; the temperature of the ion exchange and shaping reaction is room temperature, and the time is 0.5h; the ion exchange and shaping reaction are carried out under stirring; The method for obtaining the ebony dregs comprises the following steps: The black plums were cleaned and dried in an oven at 60°C, then crushed and passed through a 2mm sieve. The crushed black plums were processed according to the traditional Chinese medicine decoction method, i.e., the medicine-water ratio was 1:30g / v. 8g of the crushed black plums were weighed and placed in a 250mL conical flask, 240mL of deionized water was added, and the mixture was heated in a water bath and extracted at a constant temperature of 90°C for 3h. The mixture was allowed to stand and cool, filtered after cooling, and dried to obtain the black plum residue.

2. The preparation method according to claim 1, characterized in that: After the ion exchange and shaping reaction, the method further comprises: filtering, washing and drying the obtained ion exchange and shaping reaction liquid in sequence.

3. The xanthate material of ebony residues obtained by the preparation method according to any one of claims 1 to 2.

4. Application of the xanthate material of the ebony residues according to claim 3 in heavy metal contaminated soil.

5. The use according to claim 4, characterized in that: The following steps are involved: Mixing the xanthate material of the ebony residue, the heavy metal-contaminated soil to be treated and a liquid solvent for solubilization treatment; The dosage ratio of the ebony residue xanthate material, the heavy metal contaminated soil to be treated and the liquid solvent is 1g:2g:40mL~1g:400g:400mL; The liquid solvent is water or a filtrate obtained by solubilization treatment; The solubilization treatment time is 0.5 to 3 hours.

6. The use according to claim 5, characterized in that: After the solubilization treatment, the method further includes: filtering the obtained solubilization treatment liquid to obtain a filtrate; mixing the filtrate, the black plum medicinal residue xanthate material and the heavy metal contaminated soil to be treated, and performing a solubilization treatment again to achieve the recycling of the filtrate.

Citation Information

Patent Citations

  • Preparation method and application of corn stalk cellulose xanthic acid magnesium salt

    CN105080511A

  • Method for removing soil heavy metals by utilizing agricultural and forestry waste leaching liquor