A differential housing for an automatic transmission and a processing method thereof
By reinforcing the stiffeners and flanges on the differential housing and finishing with CNC machine tools, the problems of insufficient strength and large machining errors of the differential housing are solved, achieving a more efficient and precise differential housing. Integrated production prolongs the service life of the differential.
Patent Information
- Application Number
- CN202311296258.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-10-09
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2043-10-09
AI Technical Summary
The strength of the existing differential housing is insufficient, causing damage to the gears during operation, and the many steps in the processing method lead to large errors, which affects the service life and efficiency of the differential.
The differential housing for automatic transmissions and its processing method are adopted. Through casting, heat treatment, CNC machine tool finishing and electric welding of reinforcement sheets and flanges, the number of clamping times is reduced, the processing efficiency is improved and the strength of the housing is enhanced.
The strength and machining accuracy of the differential housing are improved, errors are reduced, the service life of the differential is extended, and operating efficiency is improved.
Smart Images

Figure CN117189845B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of differential production, in particular to a differential housing for an automatic transmission and a processing method thereof. Background Art
[0002] The differential is installed to adjust the speed difference between the left and right wheels, and the middle differential is added to adjust the speed difference between the front and rear wheels. With the rapid development of the automobile industry, the differential, as an important part of the automobile transmission system, its performance and quality have an important impact on the driving safety of the entire vehicle.
[0003] A differential case processing method with application number CN202010621964.3 is now retrieved, comprising the following steps: a. preparing a differential case blank; b. clamping and positioning with the outer circumferential surfaces of the left cylindrical section and the right cylindrical section of the differential case and the step surface formed between the left cylindrical section and the differential case as the clamping reference, and rough turning the circumferential surface and both side surfaces of the docking part of the differential case, and rough turning the circumferential surface on the right side of the docking part on the differential case to obtain a clamping circumferential surface; c. clamping and positioning with the circumferential surface for clamping and the right side surface of the docking part processed in step b as the clamping reference, and fine turning the inner hole, outer circle and end face of the left cylindrical section and the right cylindrical section; d. clamping and positioning with the left side surface and the outer circumferential surface of the docking part processed in step b as the clamping reference, and turning the ball hole and planetary shaft hole of the differential case; the present invention has the advantages of high machining accuracy, high machining efficiency and low machining cost.
[0004] The differential housing is an important component of the differential. The quality of the differential housing directly affects the service life of the differential. The existing differential is not strong enough, which causes damage to the differential housing when the gears inside the differential are running. At the same time, the processing method of the differential housing has many steps, which leads to large errors in the differential housing. For this reason, we propose a differential housing for an automatic transmission and a processing method thereof. Summary of the invention
[0005] The object of the present invention is to provide a differential case for an automatic transmission and a processing method thereof, so as to solve the problems raised in the above-mentioned background technology.
[0006] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a differential housing for an automatic transmission and a processing method thereof, comprising a shell body, a reinforcement sheet is welded on the surface of the shell body, a first end cover is installed at one edge of the shell body, an inner cavity for installing a gear is provided inside the shell body, a second end cover is installed at the other edge of the shell body, an oil filling hole is provided on one side of the first end cover, a first transmission channel is provided on one side of the shell body, and a second transmission channel is provided on the side of the shell body away from the first transmission channel.
[0007] Furthermore, a first half-shaft is installed inside the first transmission channel, and a second half-shaft is installed inside the second transmission channel.
[0008] Furthermore, a flange is installed around the first transmission channel, and mounting holes are distributed in an array around the flange.
[0009] Furthermore, an oil tank is provided at the edge of the second transmission channel, and bolt holes are distributed in an array around the oil tank.
[0010] A method for processing a differential housing for an automated transmission, the method comprising the following steps:
[0011] Step 1: Casting, obtaining a differential housing blank by casting;
[0012] Step 2: heat treatment, normalizing the differential case blank prepared in step 1, cooling it for standby use, then placing the cooled differential case blank on a grinder to grind the inner cavity of the differential case blank and the interior of the first transmission channel and the second transmission channel, and then manually cleaning the debris generated by grinding;
[0013] Step 3: The heat-treated differential housing blank is placed on a CNC machine tool to perform rough turning on the end surface of the housing body where the flange is installed;
[0014] Step 4: Rough machining is performed on the end surface of the housing body on which the oil tank is installed on a CNC machine tool;
[0015] Step 5: Finish turning the oil filling hole, the first end cover, the second end cover, the first transmission channel and the second transmission channel on the surface of the housing body;
[0016] Step 6: Finish the oil filling hole, mounting hole, bolt hole and the inner spherical surface of the shell body on the machining center;
[0017] Step 7: Use an electric welder to weld the reinforcement sheet to the surface of the housing body, and install the flange around the first transmission channel;
[0018] Step 8: Use an electric welder to weld the oil tank around the bolt holes, and connect the oil outlet pipe of the oil tank to the oil filling hole;
[0019] Step 9: Deburr and inspect the finished product.
[0020] Furthermore, the hardness of the differential case blank in step 1 is 156-197 HBS, and is cast using a sand mold mechanical molding.
[0021] Furthermore, the turning speed in step three and step four is 200-300r / min, the cutting force is 400-500N, the milling speed is 150-250r / min, the cutting force is 300-400N, the drilling speed is 100-150r / min, the cutting force is 200-300N, and the polishing speed is 100-150r / min, and the cutting force is 100-150N.
[0022] Furthermore, in the step five, the turning speed is 150-250r / min, the cutting force is 200-400N, the milling speed is 100-150r / min, the cutting force is 200-300N, the drilling speed is 70-120r / min, the cutting force is 150-250N, and the polishing speed is 100-150r / min, and the cutting force is 100-150N.
[0023] Furthermore, the normalizing treatment in step 2 is specifically as follows: heating the differential housing blank to 30-50 degrees Celsius above Ac, then keeping the temperature for 70-120 minutes and then cooling it with the furnace.
[0024] Compared with the prior art, the invention has the following beneficial effects: the differential housing for an automatic transmission and the processing method thereof have the following beneficial effects:
[0025] Firstly, the differential housing for the automatic transmission of the present invention is reinforced by a reinforcing sheet and a flange to ensure that the gears inside the differential will not be damaged under high-intensity operation, thereby improving the efficiency and quality of the differential operation. Secondly, the differential production steps are few, and multiple processing steps can be performed on a CNC lathe and a machining center without multiple transfers. This not only reduces the number of clamping times to improve efficiency, but also avoids errors on the differential housing caused by multiple clamping processes. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 This is a front structural schematic diagram of a differential housing for an automatic transmission of the present invention;
[0027] Figure 2 This is a schematic diagram of the end surface structure of a differential housing for an automatic transmission of the present invention;
[0028] Figure 3 The figure is a schematic diagram of the other side end surface structure of a differential housing for an automatic transmission of the present invention.
[0029] In the figure: 1. shell body; 2. reinforcement plate; 3. oil filling hole; 4. first end cover; 5. second end cover; 6. first transmission channel; 601. first half shaft; 7. second transmission channel; 701. second half shaft; 8. flange; 9. mounting hole; 10. oil tank; 11. bolt hole. DETAILED DESCRIPTION
[0030] In the description of the present invention, unless otherwise specified, "plurality" means two or more than two; the orientations or positional relationships indicated by the terms "upper", "lower", "left", "right", "inner", "outer", "front end", "rear end", "head", "tail", etc. are based on the orientations or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", "third", etc. are only used for descriptive purposes and cannot be understood as indicating or implying relative importance.
[0031] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "connected" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances. Embodiment 1:
[0032] like Figure 1-Figure 3 As shown, the present invention provides a technical solution: a differential housing for an automatic transmission and a processing method thereof, comprising a shell body 1, a reinforcing sheet 2 is welded on the surface of the shell body 1, and a first end cover 4 is installed at one side edge of the shell body 1, an inner cavity for installing a gear is provided inside the shell body 1, a second end cover 5 is installed at the other side edge of the shell body 1, an oil filling hole 3 is provided on one side of the first end cover 4, a first transmission channel 6 is provided on one side of the shell body 1, and a second transmission channel 7 is provided on the side of the shell body 1 away from the first transmission channel 6.
[0033] A first half shaft 601 is installed inside the first transmission channel 6 , and a second half shaft 701 is installed inside the second transmission channel 7 .
[0034] A flange 8 is installed around the first transmission channel 6 , and mounting holes 9 are distributed in an array around the flange 8 .
[0035] An oil tank 10 is disposed at the edge of the second transmission channel 7 , and bolt holes 11 are distributed in an array around the oil tank 10 . Embodiment 2:
[0036] A method for processing a differential housing for an automated transmission, the method comprising the following steps:
[0037] Step 1: Casting: a differential case blank is obtained by casting.
[0038] Step 2: heat treatment, normalizing the differential case blank prepared in step 1, cooling it for standby use, then placing the cooled differential case blank on a grinder to grind the inner cavity of the differential case blank and the interior of the first transmission channel 6 and the second transmission channel 7, and then manually cleaning the debris generated by grinding;
[0039] Step 3: The heat-treated differential housing blank is placed on a CNC machine tool to perform rough turning on the end surface of the housing body 1 on which the flange 8 is installed;
[0040] Step 4: Rough machining is performed on the end surface of the housing body 1 on which the oil tank 10 is installed on a CNC machine tool;
[0041] Step 5: fine-turning the oil filling hole 3, the first end cover 4, the second end cover 5, the first transmission channel 6 and the second transmission channel 7 on the surface of the housing body 1;
[0042] Step 6: Finish the oil filling hole 3, the mounting hole 9, the bolt hole 11 and the inner spherical surface of the housing body 1 on a machining center;
[0043] Step 7: Weld the reinforcing plate 2 to the surface of the housing body 1 by an electric welder, and install the flange 8 around the first transmission channel 6;
[0044] Step 8: Weld the oil tank 10 around the bolt hole 11 by an electric welder, and connect the oil outlet pipe of the oil tank 10 to the oil filling hole 3;
[0045] Step 9: Deburr and inspect the finished product.
[0046] The hardness of the differential housing blank in step 1 is 156-197 HBS, and it is cast by sand mold mechanical molding.
[0047] The turning speed in step 3 and step 4 is 200r / min, the cutting force is 400N, the milling speed is 150r / min, the cutting force is 300N, the drilling speed is 100r / min, the cutting force is 200N, and the polishing speed is 100r / min, and the cutting force is 100N.
[0048] In step five, the turning speed is 150r / min, the cutting force is 200N, the milling speed is 100r / min, the cutting force is 200N, the drilling speed is 70r / min, the cutting force is 150N, and the polishing speed is 100r / min, and the cutting force is 100N.
[0049] The normalizing treatment in step 2 is specifically as follows: heating the differential housing blank to 30-50 degrees Celsius above Ac, then keeping the temperature for 70-120 minutes and then cooling it with the furnace. Embodiment 3:
[0050] A method for processing a differential housing for an automated transmission, the method comprising the following steps:
[0051] Step 1: Casting: a differential case blank is obtained by casting.
[0052] Step 2: heat treatment, normalizing the differential case blank prepared in step 1, cooling it for standby use, then placing the cooled differential case blank on a grinder to grind the inner cavity of the differential case blank and the interior of the first transmission channel 6 and the second transmission channel 7, and then manually cleaning the debris generated by grinding;
[0053] Step 3: The heat-treated differential housing blank is placed on a CNC machine tool to perform rough turning on the end surface of the housing body 1 on which the flange 8 is installed;
[0054] Step 4: Rough machining is performed on the end surface of the housing body 1 on which the oil tank 10 is installed on a CNC machine tool;
[0055] Step 5: fine-turning the oil filling hole 3, the first end cover 4, the second end cover 5, the first transmission channel 6 and the second transmission channel 7 on the surface of the housing body 1;
[0056] Step 6: Finish the oil filling hole 3, the mounting hole 9, the bolt hole 11 and the inner spherical surface of the housing body 1 on a machining center;
[0057] Step 7: Weld the reinforcing plate 2 to the surface of the housing body 1 by an electric welder, and install the flange 8 around the first transmission channel 6;
[0058] Step 8: Weld the oil tank 10 around the bolt hole 11 by an electric welder, and connect the oil outlet pipe of the oil tank 10 to the oil filling hole 3;
[0059] Step 9: Deburr and inspect the finished product.
[0060] The hardness of the differential housing blank in step 1 is 156-197 HBS, and it is cast by sand mold mechanical molding.
[0061] The turning speed in step 3 and step 4 is 300r / min, the cutting force is 500N, the milling speed is 250r / min, the cutting force is 400N, the drilling speed is 150r / min, the cutting force is 300N, and the polishing speed is 150r / min, and the cutting force is 150N.
[0062] In step five, the turning speed is 250r / min, the cutting force is 400N, the milling speed is 150r / min, the cutting force is 300N, the drilling speed is 120r / min, the cutting force is 250N, and the polishing speed is 150r / min, the cutting force is 150N.
[0063] The normalizing treatment in step 2 is specifically as follows: heating the differential housing blank to 30-50 degrees Celsius above Ac, then keeping the temperature for 70-120 minutes and then cooling it with the furnace. Embodiment 4:
[0064] A method for processing a differential housing for an automated transmission, the method comprising the following steps:
[0065] Step 1: Casting, obtaining a differential housing blank by casting;
[0066] Step 2: heat treatment, normalizing the differential case blank prepared in step 1, cooling it for standby use, then placing the cooled differential case blank on a grinder to grind the inner cavity of the differential case blank and the interior of the first transmission channel 6 and the second transmission channel 7, and then manually cleaning the debris generated by grinding;
[0067] Step 3: The heat-treated differential housing blank is placed on a CNC machine tool to perform rough turning on the end surface of the housing body 1 on which the flange 8 is installed;
[0068] Step 4: Rough machining is performed on the end surface of the housing body 1 on which the oil tank 10 is installed on a CNC machine tool;
[0069] Step 5: fine-turning the oil filling hole 3, the first end cover 4, the second end cover 5, the first transmission channel 6 and the second transmission channel 7 on the surface of the housing body 1;
[0070] Step 6: Finish the oil filling hole 3, the mounting hole 9, the bolt hole 11 and the inner spherical surface of the housing body 1 on a machining center;
[0071] Step 7: Weld the reinforcing plate 2 to the surface of the housing body 1 by an electric welder, and install the flange 8 around the first transmission channel 6;
[0072] Step 8: Weld the oil tank 10 around the bolt hole 11 by an electric welder, and connect the oil outlet pipe of the oil tank 10 to the oil filling hole 3;
[0073] Step 9: Deburr and inspect the finished product.
[0074] The hardness of the differential housing blank in step 1 is 156-197 HBS, and it is cast by sand mold mechanical molding.
[0075] The turning speed in step 3 and step 4 is 250r / min, the cutting force is 450N, the milling speed is 200r / min, the cutting force is 350N, the drilling speed is 120r / min, the cutting force is 250N, and the polishing speed is 120r / min, and the cutting force is 120N.
[0076] In step five, the turning speed is 200r / min, the cutting force is 300N, the milling speed is 120r / min, the cutting force is 250N, the drilling speed is 100r / min, the cutting force is 200N, and the polishing speed is 120r / min, and the cutting force is 120N.
[0077] The normalizing treatment in step 2 is specifically as follows: heating the differential housing blank to 30-50 degrees Celsius above Ac, then keeping the temperature for 70-120 minutes and then cooling it with the furnace.
[0078] It is to be understood that the above embodiments are merely exemplary embodiments used to illustrate the principles of the present invention, but the present invention is not limited thereto. For those of ordinary skill in the art, various modifications and improvements can be made without departing from the spirit and essence of the present invention, and these modifications and improvements are also considered to be within the scope of protection of the present invention.
Claims
1. A method for processing a differential housing for an automated transmission, Features: The invention comprises a housing body (1), a reinforcement sheet (2) is welded on the surface of the housing body (1), a first end cover (4) is installed at the edge of one side of the housing body (1), an inner cavity for installing a gear is arranged inside the housing body (1), a second end cover (5) is installed at the edge of the other side of the housing body (1), an oil filling hole (3) is arranged on one side of the first end cover (4), a first transmission channel (6) is arranged on one side of the housing body (1), and a second transmission channel (7) is arranged on a side of the housing body (1) away from the first transmission channel (6), a first half shaft (601) is installed inside the first transmission channel (6), and a second half shaft (701) is installed inside the second transmission channel (7), a flange (8) is installed around the first transmission channel (6), and mounting holes (9) are arranged in an array around the flange (8), and an oil tank (10) is arranged at the edge of the second transmission channel (7), and bolt holes (11) are arranged in an array around the oil tank (10); The processing method comprises the following steps: Step 1: Casting: the differential housing blank is obtained by casting: Step 2: heat treatment, normalizing the differential case blank prepared in step 1, cooling it for use, then placing the cooled differential case blank on a grinder to grind the inner cavity of the differential case blank and the interior of the first transmission channel (6) and the second transmission channel (7), and then manually cleaning away the debris generated by the grinding; Step 3: The heat-treated differential housing blank is placed on a CNC machine tool to perform rough turning on the end surface of the housing body (1) on which the flange (8) is mounted; Step 4: Rough machining is performed on the end surface of the housing body (1) on which the oil tank (10) is mounted on a CNC machine tool; Step 5: fine-turning the oil injection hole (3), the first end cover (4), the second end cover (5), the first transmission channel (6) and the second transmission channel (7) on the surface of the housing body (1); Step 6: Finish the oil filling hole (3), the mounting hole (9), the bolt hole (11) and the inner spherical surface of the housing body (1) on a machining center; Step 7: Weld the reinforcing plate (2) to the surface of the housing body (1) using an electric welder, and install the flange (8) around the first transmission channel (6); Step 8: Weld the oil tank (10) around the bolt hole (11) using an electric welder, and connect the oil outlet pipe of the oil tank (10) to the oil filling hole (3); Step 9: Deburr and inspect the finished product; The hardness of the differential housing blank in step 1 is 156-197 HBS, and it is cast by sand mold mechanical molding; The turning speed in step 3 and step 4 is 200-300 r / min, the cutting force is 400-500 N, the milling speed is 150-250 r / min, the cutting force is 300-400 N, the drilling speed is 100-150 r / min, the cutting force is 200-300 N, the polishing speed is 100-150 r / min, and the cutting force is 100-150 N; The turning speed in the step 5 is 150-250r / min, the cutting force is 200-400N, the milling speed is 100-150r / min, the cutting force is 200-300N, the drilling speed is 70-120r / min, the cutting force is 150-250N, the polishing speed is 100-150r / min, and the cutting force is 100-150N; The normalizing treatment in step 2 is specifically as follows: heating the differential housing blank to 30-50 degrees Celsius above Ac, then keeping the temperature for 70-120 minutes and then cooling it with the furnace.
Citation Information
Patent Citations
Method for machining differential mechanism shell
CN111745165A
Differential case
CN109611538A
Differential mechanism shell machining process
CN112692520A
Differential inner rotating gear and machining method thereof
CN114508580A
Automobile drive axle differential case
CN209430712U