Solar cell metallization sintering method and processing device

Through split-beam laser-induced sintering technology, the problems of reduced contact capability and insufficient processing rate in traditional sintering technology are solved, more efficient metallization sintering of solar cells is achieved, and productivity and economic benefits are improved.

CN117790625BActive Publication Date: 2024-10-01DR LASER TECH(WUXI) CO LTD

Patent Information

Application Number
CN202311784722.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2023-10-26
Filing Date
2023-12-23
Publication Date
2024-10-01
Estimated Expiration
2043-12-23

AI Technical Summary

Technical Problem

It is difficult for traditional airflow thermal cycle sintering furnaces to form good ohmic contact. With laser-induced sintering technology, after the spot size exceeds a certain size, the contact capability is significantly reduced, and the processing rate is insufficient, affecting production capacity and economic benefits.

Method used

Laser-induced sintering technology in the form of split beam is used to generate multiple split beams through the laser, and the beam spacing and scanning speed are controlled to ensure that the contact capability is not reduced and the processing rate is increased, including using the first electrode and the second electrode to contact the surface of the cell respectively. With the pre-cured electrode on the back, the laser beam is split into multiple split beams to scan the surface of the cell. The distance between adjacent split beams is larger than the spot size, and the current micro-channels are not connected to each other, which improves the efficiency of laser-induced sintering.

Benefits of technology

It effectively improves the contact characteristics and processing speed of solar cells, improves production capacity and economic benefits, and ensures higher photoelectric conversion efficiency and lower contact resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117790625B_ABST
    Figure CN117790625B_ABST
Patent Text Reader

Abstract

The present application proposes a method for metallization sintering of solar cell and a processing device thereof, the method comprising: using a first electrode and a second electrode to contact the pre-cured electrodes on the upper and lower surfaces of the cell respectively, while the upper and lower surfaces of the cell are electrically connected, a laser generates a laser beam, controls the laser beam to split into multiple split beams, and the multiple split beams simultaneously scan the cell, generating unbalanced photogenerated carriers in the area of ​​the cell irradiated by the multiple split beams, the PN junction under the pre-cured electrode maintains a current path state, the interval between adjacent split beams is greater than or equal to the spot size, and the current micro-paths generated by the multiple split beams are not conductive to each other on the vertical section of the solar cell. Among them, the multiple split beams are controlled to scan the cell along a preset path to complete the surface scanning of the entire cell. Under the premise of improving the contact of the solar cell, this method can further improve the processing rate of laser induced sintering.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the field of photovoltaic cell technology, and specifically, relates to a method for metallization sintering of a solar cell and a processing device thereof. Background Art

[0002] The contact resistance between the surface electrode and the back electrode of a crystalline silicon solar cell has a great influence on the fill factor and conversion efficiency. The lower the contact resistance, the higher the fill factor and conversion efficiency. Reducing the contact resistance has become an urgent need for major battery manufacturers. On the other hand, in order to pursue higher conversion efficiency, the square resistance of the emitter in the surface electrode of a crystalline silicon solar cell is getting higher and higher, making it difficult to form a lower contact resistance. It is difficult to form a good ohmic contact when sintering the slurry on the cell in a traditional airflow thermal cycle sintering furnace.

[0003] In order to reduce the contact resistance on the surface of the semiconductor layer, laser induced sintering technology is used to excite the battery carriers through laser, and they flow in a directed manner under the action of the reverse voltage of the external electric field to form a loop. When the loop current flows through the interface between the metal and the silicon wafer, a more obvious thermal effect is generated due to the large contact resistance between the metal and the silicon wafer. The heat can further promote the mutual diffusion of the metal and the silicon wafer, thereby obtaining a better semiconductor surface metallization contact effect and a good passivation effect, which increases the opening voltage by more than 5mV and the battery efficiency by more than 0.2%.

[0004] In laser induced sintering technology, laser is used as a channel to open the electrical circuit, and the spot size affects the area of ​​the circuit conduction. When the existing spot size is small, the efficiency improvement difference in the processing area is small. When it exceeds a certain size, the efficiency improvement ability of the processing area will be significantly reduced. After in-depth research and comparison by the applicant, it was found that: since the spot size obviously exceeds a certain size, the number of grid lines covered by the spot increases and the coverage area becomes larger, the grid line voltage division will become uneven, and the ability to improve contact will become weaker; at the same time, when the spot area becomes larger, the area of ​​reverse conduction becomes larger, the current will increase, and then the transmission current carried by the grid line will increase, and the heat generation will increase, causing the grid line to overburn.

[0005] Due to the limitation of spot size, laser induced sintering technology urgently needs to develop new technical solutions to ensure that the ability to improve contact will not be weakened, while further improving the processing rate, productivity and economic benefits. Summary of the invention

[0006] In view of this, the present application provides a method for rapidly improving the metal contact formed by laser induced sintering of solar cells. Specifically, a method for optimizing the grid line contact characteristics of solar cells using laser induced sintering technology in the form of a split beam, and a corresponding device are proposed.

[0007] As one aspect, a method for metallization sintering of a solar cell is proposed, comprising: using a first electrode and a second electrode to contact a pre-cured electrode on the upper surface and the lower surface of the cell respectively, while the upper and lower surfaces of the cell are electrically connected, a laser generates a laser beam, and the laser beam is controlled to be split into multiple split beams, the multiple split beams simultaneously scan the cell, and unbalanced photogenerated carriers are generated in the area of ​​the cell irradiated by the multiple split beams, the PN junction under the pre-cured electrode maintains a current path state, the interval between adjacent split beams is greater than or equal to the spot size, and the current micro-paths generated by the multiple split beams are not conductive to each other on the vertical section of the solar cell; the pre-cured electrode is obtained after the conductive paste on the upper surface and the lower surface of the cell is pre-cured;

[0008] The step of controlling the laser beam to split into a plurality of split beams, wherein the plurality of split beams simultaneously scan the cell sheet comprises:

[0009] The first electrode is brought into contact with the main grid line in the pre-cured electrode on the upper surface of the cell, and multiple split light beams are controlled to scan the upper surface of the cell along a preset path to complete the surface scanning of the entire cell.

[0010] Furthermore, the scanning speed of the multiple split light beams on the solar cell is ≤200m / s.

[0011] Furthermore, the scanning speed of the multiple split light beams on the solar cell is ≤80m / s.

[0012] Furthermore, the interval between adjacent split light beams is greater than 10 mm.

[0013] Furthermore, the interval between adjacent split beams is less than 120 mm, and / or the spot of the split beam is less than 25 mm in area. 2 spot of light.

[0014] Furthermore, the laser beam generated by the laser is a continuous laser beam or a pulsed laser beam.

[0015] Furthermore, after the laser generates a laser beam, it is first expanded and then split into multiple split beams. The scanning rate and scanning direction of the multiple split beams are then controlled by a galvanometer. The multiple split beams are emitted to the upper surface of the battery cell through a field lens.

[0016] Furthermore, the method of controlling the laser beam to split into a plurality of split beams includes any one of splitting by a wedge-shaped reflector, splitting by geometric space or splitting by diffraction.

[0017] Furthermore, the battery cell is a battery cell of standard size; or a standard battery cell formed by splicing a plurality of slices.

[0018] Furthermore, the battery cell is a standard battery cell formed by splicing a plurality of split slices, and each of the plurality of split light beams irradiates a surface of a split slice respectively.

[0019] Furthermore, the wavelength of the laser is 355nm-2500nm, and the power of the laser is less than 6000W.

[0020] Furthermore, the splitting efficiency of the laser beam into multiple split light beams is greater than 80%.

[0021] Furthermore, the splitting efficiency of the laser beam into multiple split light beams is greater than 95%.

[0022] As another aspect, a processing device for metallization sintering of solar cell is proposed, including: a laser module and a voltage module, the laser module at least includes a laser, a spectrometer, and a laser scanning component, the laser generates a laser beam, the spectrometer splits the laser beam into multiple spectrometer beams, and the laser scanning component controls the multiple spectrometer beams to simultaneously scan the cell; the voltage module at least includes a constant voltage source, a first electrode and a second electrode, the first electrode and the second electrode are respectively used to contact the pre-cured electrodes on the upper surface and the lower surface of the cell to be processed, when the multiple spectrometer beams scan the cell simultaneously, the voltage module applies a constant voltage to the cell.

[0023] Furthermore, the spectroscopic device is a diffraction spectroscopic device.

[0024] Furthermore, the interval between adjacent split light beams is at least the spot size of the split light beam and at most half the size of the solar cell.

[0025] The beneficial effect of the present application is that by proposing a method and a processing device for metallization sintering of solar cell sheets, under the premise of improving the contact of solar cells, by effectively implementing multi-beam processing, the processing rate of laser induced sintering is further improved, and the production capacity and economic benefits are improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] In order to more clearly illustrate the technical solutions in the embodiments of the present application or the related technologies, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying any creative work.

[0027] The structures, proportions, sizes, etc. illustrated in the drawings of this specification are only used to match the contents disclosed in the specification so as to facilitate understanding and reading by persons familiar with this technology. They are not used to limit the conditions under which this application can be implemented, and therefore have no substantive technical significance. Any structural modification, change in proportion or adjustment of size, without affecting the effects and purposes that can be achieved by this application, should still fall within the scope of the technical contents disclosed in this application.

[0028] Figure 1 A schematic diagram of the structure of a processing device for metallization sintering of a solar cell according to an embodiment of the present application;

[0029] Figure 2 A schematic diagram of the effect of a split beam scanning a solar cell at intervals provided in the present application;

[0030] Figure 3 A schematic diagram of the effect of a split beam scanning a complete solar cell provided in the present application;

[0031] Figure 4 The optical path principle diagram of the light splitting method using a wedge-shaped reflector;

[0032] Figure 5 This is the principle diagram of the optical path using spatial geometric splitting method. DETAILED DESCRIPTION

[0033] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the embodiments in the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.

[0034] In order to make the above-mentioned objects, features and advantages of the present application more obvious and easy to understand, the present application is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0035] The present application provides a method for metallization sintering of a solar cell, comprising: using a first electrode and a second electrode to contact a precured electrode on the upper surface and the lower surface of the cell respectively, while the upper and lower surfaces of the cell are electrically connected, a laser generates a laser beam, controls the laser beam to split into multiple split beams, and the multiple split beams simultaneously scan the cell, generating unbalanced photogenerated carriers in the area of ​​the cell irradiated by the multiple split beams, a PN junction under the precured electrode maintains a current path state, the interval between adjacent split beams is greater than or equal to the spot size, and the current micropaths generated by the multiple split beams are not connected to each other on the vertical cross section of the solar cell; the precured electrode is obtained after the conductive paste on the upper surface and the lower surface of the cell is precured;

[0036] Among them, controlling the laser beam to split into multiple split beams, and the multiple split beams simultaneously scanning the cell includes: contacting the first electrode with the main grid line in the pre-cured electrode on the upper surface of the cell, controlling the multiple split beams to scan the cell along a preset path, and completing the surface scanning of the entire cell. The preset path can be parallel or perpendicular to the secondary grid line, or in the form of any fold line or other path to complete the surface scanning of the entire cell, or the entire cell can be divided into several areas, each area is scanned by an optional path, and the scanning of each area is completed one by one to complete the scanning of the entire cell.

[0037] Through the above-mentioned method of metallization sintering of solar cell sheets, the laser beam is split to obtain multiple split beams, and the intervals of the split beams are controlled (to meet the process effect requirements and match the processing graphics). Under the premise of improving the contact of solar cells, the processing rate of laser induced sintering is further improved, thereby improving production capacity and economic benefits.

[0038] Furthermore, the light output effect of the laser beam after splitting is consistent with that of a single beam without splitting, and the functionality is consistent. Increasing the laser power makes the total energy of the n split beams n times that of a single beam, and keeping the other parameters of the split beams and the processing form unchanged, maintains the same process effect as a single beam without splitting.

[0039] Specifically, the interval between adjacent split beams is greater than or equal to the spot size, which should be reasonably understood as the interval between adjacent split beams is greater than or equal to the maximum side length or maximum diameter value of the regular spot. For example, when the spot is a square spot or a rectangular spot, the interval between adjacent split beams is greater than or equal to the maximum side length of the spot. For example, when the spot is a circular spot or an elliptical spot, the interval between adjacent split beams is greater than or equal to the long diameter value. Generally speaking, under this adjacent beam multi-distance constraint condition, the current micro-paths generated by multiple adjacent split beams are not conductive to each other on the vertical section of the solar cell. It can be understood that the larger the beam spot spacing, the smaller the mutual influence of the current micro-paths generated by the split beams, which is limited to not exceeding the maximum effective distance of the split beams, such as 120mm. Generally, when the splitting spacing exceeds half of the cell, the actual scanning range of the galvanometer will be larger than half of the cell area, and the laser will scan outside the cell, which increases the processing time and wastes laser energy. In addition, when the splitting spacing is too large, the field of view of the optical system is too large, which increases the system aperture requirements and reduces the economic efficiency.

[0040] More specifically, the interval between adjacent split beams is set to be greater than 10 mm, preferably ≥ 15 mm, to reduce the current micro-paths formed under the irradiation of the light spot from the path disturbance existing when the carriers diffuse disorderly. And, more importantly, to avoid the increase of current concentration density caused by the beams being too close, which may cause the grid lines in the nearby area to burn out when the local area is overheated.

[0041] Furthermore, in the above method, the scanning speed of the multiple split beams on the cell is ≤200m / s, and the effective processing time is controlled to be ≥10μs, so as to ensure that after the beams in each area of ​​the cell are scanned, the atoms of the pre-cured electrode and the cell diffuse with each other, which can significantly improve the conversion efficiency of the cell by more than 0.1%. Since the non-equilibrium carriers generated by the laser irradiation solar cell are in the non-electric field direction, the time for the carrier recombination to relax to the equilibrium state can usually reach the microsecond level. However, when the laser beam scanning rate exceeds a certain value, the efficiency improvement ability will be reduced to a certain extent. This is because at low speed, the time the spot passes is sufficient (the spot size divided by the speed), that is, the effective processing time is guaranteed, and if the scanning speed is increased, the effective processing time is reduced, resulting in a worse processing effect. The scanning speed corresponds to the processing time, and the performance improvement corresponding to the processing time is two groups of factors that need to be comprehensively considered. In a complete set of processing equipment systems, the processing time can usually be matched with the laser scanning processing module through various automation devices, and the performance improvement brought by laser scanning needs to be guaranteed. In order to better ensure that the contact characteristics of solar cells can be improved with high reliability and high uniformity, preferably, the scanning speed of the multiple split light beams on the cell in the present application is ≤25m / s, thereby controlling the effective processing time to be ≥60μs; or the scanning speed of the multiple split light beams on the cell is ≤60m / s, thereby controlling the effective processing time to be ≥25μs; to ensure that the final photoelectric conversion efficiency of the cell is improved by more than 0.2-0.3%.

[0042] Among them, the pre-curing treatment is, for example, placing the battery cell in a sintering furnace to control the heating time and heating temperature, and heating the slurry on the surface of the battery cell to obtain a pre-cured electrode in the desired state. When the laser beam scans the battery cell, the first electrode and the second electrode are respectively connected to the power supply, and respectively contact the pre-cured electrodes on the upper and lower surfaces of the battery cell, and the battery cell is scanned while the first electrode and the second electrode are respectively electrically connected to the upper and lower surfaces of the battery cell. Among them, the first electrode includes at least one strip electrode, and the structure of the first electrode includes: an elastic probe row structure (that is, a plurality of elastic probes arranged in a collinear manner are connected under a probe bracket, and the plurality of probes are in contact with the battery cell), or an elastic conductive wire, or a long strip of elastic electrode sheet (the electrode sheet and the battery cell can be in surface contact). The electrode structure in the first electrode is not limited to this. The structural form of the second electrode can also be various, such as a conductive plate or a probe row, as long as the second electrode can achieve electrical contact with the pre-cured electrode on the lower surface of the battery cell.

[0043] As another embodiment, the interval between adjacent split beams is less than 120 mm, and / or the spot of the split beam has a spot area of ​​less than 25 mm. 2 By controlling the spot size within this range, the production capacity requirements can be met while ensuring the processing effect (the efficiency improvement capability will not be significantly reduced, and the contact improvement capability will not be weakened).

[0044] As another embodiment, the laser beam generated by the laser is a continuous laser beam or a pulsed laser beam, that is, both a continuous laser beam and a pulsed laser beam are possible. When a continuous laser beam is used as a light source, the carrier diffusion flow under the pre-cured electrode on the upper surface and the pre-cured electrode on the lower surface of the solar cell is kept completely turned on, and the carrier concentration at the turned-on point is always kept constant.

[0045] As another embodiment, after the laser generates a laser beam, it is first expanded and then split into multiple split beams. The scanning rate and scanning direction of the multiple split beams are then controlled by a galvanometer. The multiple split beams are emitted to the upper surface of the battery cell through a field lens.

[0046] As another embodiment, the battery cell is a standard battery cell with a size of 182mmx182mm or 210mmx210mm or other standard battery cells available on the market; or a standard battery cell formed by splicing multiple slices. In other words, the metallization method is not only applicable to standard battery cells, but also to multi-slice battery cells, and has a wide range of application scenarios.

[0047] As another embodiment, the cell is a standard cell formed by splicing multiple slices, and each of the multiple split beams irradiates the surface of a slice. By controlling the interval of the split beams, laser induced sintering can be performed on multiple slices at the same time, further improving the production capacity.

[0048] As another embodiment, the wavelength of the laser is 355nm-2500nm, and the power of the laser is less than 6000W.

[0049] As another embodiment, the splitting efficiency of the laser beam into multiple split beams is greater than 80% to control the influence of the loop channel formed by the secondary light on the process effect. Preferably, the splitting efficiency of the laser beam into multiple split beams is greater than 95% to better control the influence of the loop channel formed by the secondary light on the process effect. When the splitting efficiency of the split beam is low, a small part of the secondary light and higher-order secondary light, secondary light and other non-target beams irradiate the pn junction area of ​​the solar cell, which will affect the number of photogenerated carriers and further affect the effect of laser-assisted sintering.

[0050] As another aspect of this application, Figure 1As shown, a processing device for metallization sintering of solar cell is proposed, including: a laser module and a voltage module, the laser module at least includes a laser 110, a spectrometer 120, and a laser scanning assembly 130, the laser 110 generates a laser beam, the spectrometer 120 splits the laser beam into multiple spectrometer beams, and the laser scanning assembly 120 controls the multiple spectrometer beams to scan the cell at the same time; the laser scanning assembly 120 includes a field mirror and a galvanometer, and the galvanometer controls the scanning rate and scanning direction of the multiple spectrometer beams after the spectrometer beams are split, and the multiple spectrometer beams are emitted to the upper surface of the cell through the field mirror. The voltage module at least includes a constant voltage source 210, a first electrode 220 and a second electrode 230, and the first electrode 220 and the second electrode 230 are used to contact the pre-cured electrodes on the upper and lower surfaces of the cell to be processed, respectively, and when the multiple spectrometer beams scan the cell at the same time, the voltage module applies a constant voltage to the cell.

[0051] During operation, the first electrode 220 and the second electrode 220 are used to contact the pre-cured electrodes on the upper and lower surfaces of the battery cell respectively. When the upper and lower surfaces of the battery cell are electrically connected, the voltage module applies a constant voltage to the battery cell. The laser 110 generates a laser beam which is split into multiple split beams through the splitter device 120. The laser scanning component 130 controls the multiple split beams to scan the battery cell at the same time. Unbalanced photogenerated carriers are generated in the area of ​​the battery cell irradiated by the multiple split beams, and the PN junction under the pre-cured electrode maintains a current path state.

[0052] Through the processing device for metallization sintering of solar cell sheets, the processing rate of laser induced sintering can be further improved under the premise of improving the contact of solar cells, thereby increasing production capacity and economic benefits.

[0053] Furthermore, the processing device also includes a beam expander 120 to change the diameter and divergence angle of the laser beam, and utilize the magnification effect of the optical path in the optical path design to adjust the required interval of the split light beam to meet the actual process requirements.

[0054] For the specific laser beam splitting method, this application uses examples to illustrate, and this example does not exclude other forms of splitting methods, as long as they can meet the actual splitting needs of this application. For example, wedge reflector splitting, geometric space splitting, etc. The specific implementation scheme is as follows:

[0055] Solution 1: Wedge-shaped reflector beam splitting

[0056] like Figure 4As shown, a laser beam is incident on a reflector with a wedge angle of w. The glass refractive index of the reflector is n. The beam is divided into two beams of equal power at the S1 surface, where beam 1 is directly reflected and beam 2 is reflected by S2 and then transmitted through S1. After calculation, the angle between beam 1 and beam 2 is approximately θ=2.36*n*w. For a given splitting angle θ, it is sufficient to select a suitable wedge angle w and refractive index n.

[0057] Solution 2: Spatial geometric spectrometry

[0058] The geometric splitting method can be achieved by placing several sub-light sources in parallel according to the required splitting spacing, and focusing them separately through focusing mirrors installed on the paths of each split beam to obtain the required splitting quantity and spacing.

[0059] like Figure 5 As shown, a laser beam is incident on a beam splitter and is split into two beams of equal power, one of which is a reflected beam 1 and the other is a transmitted beam 2. The two sub-beams pass through corresponding reflectors 1 and 2 respectively. By adjusting the angles of reflectors 1 and 2, any desired beam splitting angle θ can be achieved.

[0060] That is to say, the optical splitter 120 can obtain multiple split light beams with equal power by wedge-shaped reflection splitting or spatial geometric splitting, or by phase modulation.

[0061] Preferably, as another embodiment, the spectrometer 120 is a diffraction spectrometer. When using a diffraction spectrometer, the spacing D of the split beams is proportional to the angle θ between the split beams and the focal length EFFL of the focusing system, D = EFFL * f (θ), where f (θ) is determined by the image height relationship of the focusing system: commonly used relationships are: f (θ) = θ, f (θ) = tan θ, f (θ) = sin θ, etc. Under the given splitting spacing and system focal length requirements, the required angle between the split beams can be calculated using the imaging principle to obtain the required spacing of the split beams.

[0062] As another embodiment, the interval between adjacent split light beams is at least the spot size of the split light beams and at most half the size of the solar cell.

[0063] Example 1

[0064] A 1mmx1mm square spot is used to process a 210mmx210mm silicon wafer. The processing method is front scanning. A total of 210 laser lines need to be processed. If there is no light splitting, 210 scans are required. The scanning speed is 20m / s, and the required laser power is 300W. The time required for a single scan is 2600ms.

[0065] Using the split beam solution for processing, the interval between the two split beams is 105mm, and a total of 105 scans are required to complete the processing. At a scanning speed of 20m / s, the required laser power is 600W, and the time required to complete the processing of the entire silicon wafer is 1300ms;

[0066] Example 2

[0067] A 1mmx3mm square spot is used to process a 210mmx210mm silicon wafer. The processing method is front scanning. A total of 70 laser lines need to be processed. If there is no light splitting, 70 scans are required. The scanning speed is 20m / s, and the required laser power is 900W. The time required for a single scan is 875ms.

[0068] The processing is performed using a beam splitting solution, with the interval between the two beam splitting beams being 105 mm, and a total of 35 scans are required to complete the processing. At a scanning speed of 20 m / s, the required laser power is 1800 W, and the time required to complete the processing of the entire silicon wafer is 440 ms.

[0069] Example 3

[0070] The wavelength of the infrared continuous light is 1030nm, and the laser power is 1000W. The size of the square spot is 1.75mmx1.75mm, the processing power is 550W, the processing speed is 25m / s, the splitting efficiency is 99%, the number of splits is 3, and the splitting spacing is 21mm. The scanning length is 190mm, and the effect of scanning once is as follows Figure 2 As shown, the three line types (straight line, dotted line, and dash-dot line) are three beam splitting spot paths. To fill the beam splitting spacing, 12 scans are required (21mm / 1.75mm=12 scanning lines). At this time, one cycle is 63mm. Three groups are scanned in this way. Figure 3 As shown, it can cover an area of ​​190mmx190mm. Using this optical solution, it is possible to process cells with specifications such as 182mmx182mm, 182mmx183.75mm, 182mmx188mm, and other sizes less than 189mmx190mm.

[0071] It should be noted that Figure 2 and Figure 3 The three line types are just for illustration of the three beams of light. If they were all the same line type, it would be inconvenient to illustrate. In fact, the characteristics of the three beams of light are the same, and the scanning method is the same.

[0072] Of course, the number of split beams is not limited to this, and the above embodiments are only for illustration. By scanning the solar cell with the above-mentioned various split beams, the photoelectric conversion efficiency can be effectively improved under the action of the electric field. The complete set of solar cell processing equipment using this technology lays a solid technical foundation for the industrialization of solar cell metallization technology.

[0073] In this specification, each embodiment is described in a progressive, parallel, or progressive and parallel manner. Each embodiment focuses on the differences from other embodiments, and the same or similar parts between the embodiments can be referred to each other. For the device disclosed in the embodiment, since it corresponds to the method disclosed in the embodiment, the description is relatively simple, and the relevant parts can be referred to the method part.

[0074] The above description of the disclosed embodiments enables those skilled in the art to implement or use the present application. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present application. Therefore, the present application will not be limited to the embodiments shown herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A method for metallization sintering of solar cell sheets, characterized in that: include: A pre-cured electrode is used in which the first electrode and the second electrode contact the upper surface and the lower surface of the solar cell respectively. When the upper and lower surfaces of the solar cell are electrically connected, a laser generates a laser beam, and the laser beam is controlled to be split into multiple split beams. The multiple split beams scan the solar cell at the same time, and unbalanced photogenerated carriers are generated in the area of ​​the solar cell irradiated by the multiple split beams. The PN junction under the pre-cured electrode maintains a current path state, the interval between adjacent split beams is greater than or equal to the spot size, the interval between adjacent split beams is greater than 10mm, and the current micro-paths generated by the multiple split beams are not connected to each other on the vertical section of the solar cell; the interval between adjacent split beams is less than 120mm, and / or the spot of the split beam is a spot area less than 25mm 2 The pre-cured electrode is obtained by pre-curing the conductive paste on the upper surface and the lower surface of the cell; The step of controlling the laser beam to split into a plurality of split beams, wherein the plurality of split beams simultaneously scan the cell sheet comprises: The first electrode is contacted with the main grid line in the pre-cured electrode on the upper surface of the cell, and multiple split light beams are controlled to scan the upper surface of the cell along a preset path to complete the surface scanning of the entire cell.

2. The method for metallization sintering of solar cell according to claim 1, characterized in that: The scanning speed of multiple split beams on the battery cell is ≤200m / s.

3. The method for metallization sintering of solar cell according to claim 1, characterized in that: The scanning speed of multiple split beams on the battery cell is ≤80m / s.

4. The method for metallization sintering of solar cell according to claim 1, characterized in that: The laser beam generated by the laser is a continuous laser beam or a pulsed laser beam.

5. The method for metallization sintering of solar cell according to claim 1, characterized in that: After the laser generates a laser beam, it is first expanded and then split into multiple split beams. The scanning rate and scanning direction of the multiple split beams are then controlled by a galvanometer. The multiple split beams are emitted to the upper surface of the battery cell through a field lens.

6. The method for metallization sintering of solar cell according to claim 1, characterized in that: The method of controlling the laser beam to split into multiple split beams includes any one of splitting by a wedge-shaped reflector, splitting by geometric space or splitting by diffraction.

7. The method for metallization sintering of solar cell according to claim 1, characterized in that: The battery cell is a battery cell of standard size; or a standard battery cell formed by splicing a plurality of sub-cells.

8. The method for metallization sintering of solar cell according to claim 1, characterized in that: The battery cell is a standard battery cell formed by splicing a plurality of split slices, and each of the plurality of split light beams irradiates the surface of a split slice respectively.

9. The method for metallization sintering of solar cell according to claim 1, characterized in that: The wavelength of the laser is 355nm~2500nm, and the power of the laser is less than 6000W.

10. The method for metallization sintering of solar cell according to claim 1, characterized in that: The splitting efficiency of the laser beam into multiple split light beams is greater than 80%.

11. The method for metallization sintering of solar cell according to claim 9, characterized in that: The splitting efficiency of the laser beam into multiple split light beams is greater than 95%.

12. A processing device for metallizing and sintering a solar cell used to complete the method for metallizing and sintering a solar cell according to any one of claims 1 to 11, characterized in that: The processing device for metallization sintering of solar cell comprises: a laser module and a voltage module, wherein the laser module comprises at least a laser, a spectrometer, and a laser scanning assembly, wherein the laser generates a laser beam, and the spectrometer splits the laser beam into a plurality of spectrometer beams, wherein the interval between adjacent spectrometer beams is greater than or equal to the spot size, and the interval between adjacent spectrometer beams is greater than 10 mm, and the current micro-paths generated by the plurality of spectrometer beams are not connected to each other on the vertical section of the solar cell, and the laser scanning assembly controls the plurality of spectrometer beams to scan the cell at the same time; The voltage module at least includes a constant voltage source, a first electrode and a second electrode, wherein the first electrode and the second electrode are respectively used to contact the pre-cured electrodes on the upper surface and the lower surface of the battery cell to be processed. When multiple beams of the split light beams scan the battery cell simultaneously, the voltage module applies a constant voltage to the battery cell.

13. The processing device for metallization sintering of solar cell according to claim 12, characterized in that: The spectroscopic device is a diffraction spectroscopic device.

14. The processing device for metallization sintering of solar cell according to claim 12, characterized in that: The interval between adjacent split light beams is at least the spot size of the split light beams and at most half the size of the solar cell.

Citation Information

Patent Citations

  • Method for improving the ohmic contact behavior between a contact grid and an emitter layer of a silicon solar cell

    CN111742417A

  • Solar cell preparation method with laser processing

    CN115799394A

  • Laser multi-beam processing device and solar cell multi-beam processing method

    CN116038106A

Cited By

  • Method and processing device for improving laser-assisted sintering contact uniformity

    CN119967936A

  • A method and a processing apparatus for improving contact uniformity in laser-assisted sintering

    CN119967936B