A high temperature resistant flame retardant cable and preparation method thereof
By using composite flame retardant and specific polymer materials, combined with extrusion granulation process, the problem of poor high-temperature flame retardant performance of existing cables is solved, and efficient and stable flame retardant performance and good mechanical properties are achieved. .
Patent Information
- Application Number
- CN202410115865.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-29
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2044-01-29
AI Technical Summary
In the prior art, cables with poor high temperature flame retardant performance are difficult to meet the flame retardant requirements of cable outer sheath, and excessive amount of flame retardant added will affect the overall performance of the cable.
Using composite flame retardants, including composite flame retardants and modified magnesium hydroxide, combined with ethylene-vinyl acetate copolymer, ethylene-octene copolymer and maleic anhydride grafted ethylene-vinyl acetate copolymer and other materials, through double- The process of roll-opening mixer and twin-screw extruder is melt blended and extruded to form high-temperature flame retardant cables.
It significantly improves the high-temperature flame retardant performance of cables, improves the mechanical properties and flame retardant performance of materials, and simplifies the production process and improves production efficiency.
Smart Images

Figure CN117887164B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of cable preparation, and in particular to a high temperature resistant flame retardant cable and a preparation method thereof. Background Art
[0002] Wires and cables play an indispensable role in daily life and industry, but long-term overload operation of cables, short circuit failure caused by insulation damage, external fire and heat sources, etc. may cause fires in cables, resulting in significant losses. At present, flame-retardant cables are usually made by extrusion process on the outer sheath of cables. Flame-retardant cables usually use polyolefin materials represented by ethylene-vinyl acetate copolymer and thermoplastic polyolefin elastomer as matrix resin. Since both have the characteristics of high combustion heat release, low carbonization, and easy generation of molten droplets, their flame retardancy faces great challenges. In order to meet the flame retardant requirements of cable outer sheaths, flame retardants are compounded with matrix resins.
[0003] However, a large amount of flame retardant added will affect the comprehensive performance of the cable, and the effect of a single flame retardant is not obvious. At present, the compounding of hydroxide flame retardants and synergistic flame retardants has become a major trend. The cables made using the existing flame retardant synergistic compound system have poor high temperature flame retardant performance. Therefore, it is necessary to provide a high temperature resistant flame retardant cable and a preparation method thereof to solve the above problems. Summary of the invention
[0004] In view of the deficiencies in the prior art, an object of the present invention is to provide a high temperature resistant flame retardant cable and a preparation method thereof.
[0005] A high temperature resistant flame retardant cable comprises the following raw materials in weight ratio: 20-40 parts of compound flame retardant, 10-30 parts of ethylene-vinyl acetate copolymer, 10-30 parts of ethylene-octene copolymer, 10-30 parts of maleic anhydride grafted ethylene-vinyl acetate copolymer, 10-30 parts of wear resistance agent, 0.5-2 parts of silane coupling agent, 0.5-2 parts of lubricant and 0.1-3 parts of antioxidant.
[0006] Furthermore, the composite flame retardant comprises a composite flame retardant and modified magnesium hydroxide, and the mass ratio of the composite flame retardant to the modified magnesium hydroxide is 1:6-9.
[0007] Furthermore, the vinyl acetate content of the ethylene-vinyl acetate copolymer is 30%-60%, and the Shore hardness of the ethylene-octene copolymer is 50-75A.
[0008] Furthermore, the anti-wear agent is hollow microspheres with a particle size in the range of 2-20 microns, the lubricant is one or more of polysiloxane, erucamide, and zinc stearate, and the antioxidant is one or more of hindered phenol antioxidants, phosphite antioxidants, and hindered amine antioxidants.
[0009] A preparation method of a high-temperature resistant flame-retardant cable comprises the following steps: adding a composite flame retardant, modified magnesium hydroxide, ethylene-vinyl acetate copolymer, ethylene-octene copolymer, maleic anhydride grafted ethylene-vinyl acetate copolymer, hollow microspheres, silane coupling agent, lubricant and antioxidant into a double-roll mill for melt blending, transferring the materials into a twin-screw extruder for extrusion granulation, placing the masterbatch into a pipe extruder after drying, melt extruding, molding, and cooling to room temperature to obtain the high-temperature resistant flame-retardant cable.
[0010] Furthermore, the temperature of the twin-screw extruder is set to 140-160° C., the feeding frequency is 25-35 Hz, and the screw speed is 260-300 r / min.
[0011] Furthermore, the preparation method of the composite flame retardant is as follows: 5-5.5 parts by mass of terephthalaldehyde is dissolved in a solvent and put into a reaction bottle, 3.9-4.2 parts by mass of 4,4-diaminodiphenylmethane dissolved in the solvent is slowly dripped into the reactor, stirred at 300-500r / min, nitrogen is introduced and the temperature is raised to 60-70°C for reaction for 1-2h, after the reaction is completed, the system is filtered and the precipitate is washed with ethanol, and an intermediate is obtained after drying; the intermediate is mixed with a solvent, 0.88-0.96 The solvent solution of 1-1.2 parts by weight of diethylenetriamine is stirred and mixed, and a solvent solution of 1-1.2 parts by weight of cyanuric chloride is added dropwise, the mixed solution is poured into a microwave reactor, microwaved at 70-80°C for 1-2h, and then transferred to a reaction bottle, cooled to room temperature, 1-1.2 parts by weight of DOPO flame retardant is dissolved in the solvent, and slowly added dropwise to the reaction bottle, the temperature is raised to 60-70°C, and the reaction is continued for 4-5h, filtered and washed under reduced pressure, the filter cake is dried at 70-80°C for 6-8h, and the composite flame retardant is obtained after grinding.
[0012] Furthermore, the solvent is anhydrous ethanol.
[0013] Furthermore, the preparation method of the composite flame retardant also includes pretreatment of raw materials: putting cyanuric chloride into a purification bottle, placing a matching watch glass on the purification bottle, heating the purification bottle to sublime the cyanuric chloride, then cooling it to the bottom of the watch glass, scraping off the cyanuric chloride on the bottom of the watch glass, and using it immediately after preparation.
[0014] Furthermore, the preparation method of the modified magnesium hydroxide is as follows: 150-160 parts by mass of sodium hydroxide and 25-30 parts by mass of urea are dissolved in 50-70 parts by volume of deionized water to prepare a mixed alkaline solution, which is stored for standby use; 450-500 parts by volume of a 2 mol / L magnesium chloride solution is slowly added dropwise to the mixed alkaline solution, and stirred for 1-1.5 hours to obtain a mixed solution; 6-6.5 parts by mass of sodium stearate are weighed and dissolved in 50-70 parts by volume of hot water, and the mixture is added dropwise to the mixed solution, and the mixture is continuously stirred for 0.5-1 hour. The reaction temperature is 55-60° C., and the product is centrifugally washed with hot deionized water for 3-5 times, dried at 60-65° C. for 10-12 hours, and then crushed to obtain modified magnesium hydroxide.
[0015] Furthermore, the high temperature resistant and flame retardant cable is used for cable assembly, and the specific steps are as follows:
[0016] 1. Wire drawing: Under normal temperature conditions, use a wire drawing machine to draw metal rods (copper and aluminum) into metal wires;
[0017] 2. Single wire annealing: heat the wire to a certain temperature and then cool it at an appropriate speed;
[0018] 3. Conductor twisting: twist multiple metal wires into a conductor in a specified direction;
[0019] 4. Insulation extrusion: use an extruder to directly extrude the insulation layer;
[0020] 5. Cabling: Multi-core cables use a cabling machine to twist the insulated cores into round cable cores in a certain arrangement and pitch, including filling and binding;
[0021] 6. Inner sheath extrusion: use an extruder to directly extrude the inner sheath;
[0022] 7. Armor: a layer of metal or other material outside the inner sheath of the cable;
[0023] 8. Outer sheath extrusion: The high temperature resistant and highly flame retardant cable is used as the outer sheath, and the cable is made by extrusion process.
[0024] The beneficial effects achieved by the present invention are as follows: 1. The present invention prepares a new type of composite flame retardant and combines it with modified magnesium hydroxide to form a composite flame retardant system, thereby improving the high temperature flame retardant performance of the cable; firstly, terephthalaldehyde, diethylenetriamine and cyanuric chloride and other raw materials are used to prepare the Schiff base flame retardant polymer, and DOPO flame retardant is added in the later stage of the preparation reaction to effectively combine the two to prepare a composite flame retardant.
[0025] 2. The present invention uses urea and sodium stearate as modifiers and adopts a precipitation method to prepare modified magnesium hydroxide with irregular particles and good dispersibility, while improving the hydrophobicity of magnesium hydroxide and its compatibility in polymers, thereby achieving the effect of improving the mechanical and flame retardant properties of cable materials.
[0026] 3. The present invention uses a microwave method to prepare a Schiff base flame retardant polymer, and utilizes the unique thermal effect and non-thermal effect of microwave synthesis to make the reactant ions and polar molecules move in opposite directions, thereby increasing the probability of collision between reactant molecules and thereby improving the reaction efficiency.
[0027] 4. The cable raw materials used in the present invention have good compatibility, and the formed composite material has stable structure and performance.
[0028] 5. The method used in the present invention is simple to operate, has high production efficiency, high yield, and convenient post-processing. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 This is a principle block diagram of a method for preparing a high temperature resistant flame retardant cable used in an embodiment of the present invention. DETAILED DESCRIPTION
[0030] The present invention is further described in detail below in conjunction with specific embodiments.
[0031] Example 1: A high temperature resistant flame retardant cable, comprising the following raw materials in weight ratio: 28 parts of a compound flame retardant, 20 parts of ethylene-vinyl acetate copolymer with a vinyl acetate content of 40%, 20 parts of ethylene-octene copolymer with a Shore hardness of 50-75A, 20 parts of maleic anhydride grafted ethylene-vinyl acetate copolymer, 15 parts of an anti-wear agent, 0.7 parts of a silane coupling agent, 0.7 parts of a lubricant and 1 part of an antioxidant; the compound flame retardant comprises a composite flame retardant and modified magnesium hydroxide, and the mass ratio of the composite flame retardant to the modified magnesium hydroxide is 1:6; the anti-wear agent is a hollow microsphere with a particle size in the range of 2-20 microns, the lubricant is polysiloxane, and the antioxidant is a hindered phenol antioxidant.
[0032] A method for preparing a high temperature resistant flame retardant cable, such as Figure 1 As shown, the method comprises the following steps: adding a composite flame retardant, modified magnesium hydroxide, ethylene-vinyl acetate copolymer, ethylene-octene copolymer, maleic anhydride grafted ethylene-vinyl acetate copolymer, hollow microspheres, silane coupling agent, lubricant and antioxidant into a twin-roll mill for melt blending, transferring the materials into a twin-screw extruder for extrusion granulation, wherein the temperature of the twin-screw extruder is set to 140° C., the feeding frequency is 25 Hz, and the screw speed is 260 r / min; after drying, placing the masterbatch in a pipe extruder, melt extruding, molding, and cooling to room temperature to obtain a high temperature resistant flame retardant cable.
[0033] The preparation method of the composite flame retardant is as follows:
[0034] Put cyanuric chloride into a purification bottle, put a matching watch glass on the purification bottle, heat the purification bottle to make the cyanuric chloride sublime, then cool it to the bottom of the watch glass, perform recrystallization purification, scrape off the cyanuric chloride at the bottom of the watch glass, and use it immediately;
[0035] 5 parts by weight of terephthalaldehyde are dissolved in anhydrous ethanol and put into a reaction bottle, 3.9 parts by weight of 4,4-diaminodiphenylmethane dissolved in anhydrous ethanol is slowly dripped into the reactor, stirred at 300 r / min, nitrogen is introduced and the temperature is raised to 60°C for reaction for 1 hour, TLC is used to monitor the progress of the reaction during the reaction, and the reaction produces a yellow precipitate. After the reaction is completed, the system is filtered and the precipitate is washed with ethanol, and the intermediate is obtained after drying; the intermediate is mixed with anhydrous ethanol, an anhydrous ethanol solution containing 0.88 parts by weight of diethylenetriamine is dripped, stirred and mixed, an anhydrous ethanol solution containing 1 part by weight of cyanuric chloride is added dropwise, the mixed solution is poured into a microwave reactor, microwaved at 70°C for 1 hour, and then transferred to a reaction bottle, cooled to room temperature, 1 part by weight of DOPO flame retardant is dissolved in anhydrous ethanol, slowly dripped into the reaction bottle, heated to 60°C and continued to react for 4 hours, filtered and washed under reduced pressure, the filter cake is dried at 70°C for 6 hours, and the composite flame retardant is obtained after grinding.
[0036] The amount of anhydrous ethanol used to dissolve the material each time is 30 parts by volume.
[0037] The preparation method of modified magnesium hydroxide is as follows: 150 parts by mass of sodium hydroxide and 25 parts by mass of urea are dissolved in 50 parts by volume of deionized water to prepare a mixed alkaline solution, which is stored for standby use; 450 parts by volume of a 2 mol / L magnesium chloride solution is slowly dropped into the mixed alkaline solution, and stirred for 1 hour to obtain a mixed solution; 6 parts by mass of sodium stearate are weighed and dissolved in 50 parts by volume of hot water, and the solution is dropped into the mixed solution, and the mixture is continuously stirred for 0.5 hours. The reaction temperature is 55° C., and the product is centrifugally washed with hot deionized water for 3 times, dried at 60° C. for 10 hours, and then crushed to obtain modified magnesium hydroxide.
[0038] Example 2: A high temperature resistant flame retardant cable, comprising the following raw materials in weight ratio: 35 parts of a compound flame retardant, 30 parts of ethylene-vinyl acetate copolymer with a vinyl acetate content of 40%, 30 parts of ethylene-octene copolymer with a Shore hardness of 50-75A, 25 parts of maleic anhydride grafted ethylene-vinyl acetate copolymer, 20 parts of an anti-wear agent, 1 part of a silane coupling agent, 1 part of a lubricant and 1.5 parts of an antioxidant; the compound flame retardant comprises a composite flame retardant and modified magnesium hydroxide, and the mass ratio of the composite flame retardant to the modified magnesium hydroxide is 1:6; the anti-wear agent is hollow microspheres with a particle size in the range of 2-20 microns, the lubricant is polysiloxane, and the antioxidant is a hindered phenol antioxidant.
[0039] A method for preparing a high temperature resistant flame retardant cable, such as Figure 1As shown, the method comprises the following steps: adding a composite flame retardant, modified magnesium hydroxide, ethylene-vinyl acetate copolymer, ethylene-octene copolymer, maleic anhydride grafted ethylene-vinyl acetate copolymer, hollow microspheres, silane coupling agent, lubricant and antioxidant into a twin-roll mill for melt blending, transferring the materials into a twin-screw extruder for extrusion granulation, wherein the temperature of the twin-screw extruder is set to 140° C., the feeding frequency is 25 Hz, and the screw speed is 260 r / min; after drying, placing the masterbatch in a pipe extruder, melt extruding, molding, and cooling to room temperature to obtain a high temperature resistant flame retardant cable.
[0040] The preparation method of the composite flame retardant is as follows:
[0041] Put cyanuric chloride into a purification bottle, put a matching watch glass on the purification bottle, heat the purification bottle to make the cyanuric chloride sublime, then cool it to the bottom of the watch glass, perform recrystallization purification, scrape off the cyanuric chloride at the bottom of the watch glass, and use it immediately;
[0042] 5.5 parts by mass of terephthalaldehyde were dissolved in anhydrous ethanol and put into a reaction bottle. 4.2 parts by mass of 4,4-diaminodiphenylmethane dissolved in anhydrous ethanol was slowly added dropwise to the reactor, stirred at 300 r / min, nitrogen was introduced and the temperature was raised to 60°C for reaction for 1 hour. During the reaction, the progress of the reaction was monitored by TLC. A yellow precipitate was produced by the reaction. After the reaction was completed, the system was filtered and the precipitate was washed with ethanol and dried to obtain an intermediate. The intermediate was mixed with anhydrous ethanol and 0. 96 parts by weight of anhydrous ethanol solution of diethylenetriamine was stirred and mixed, and 1.2 parts by weight of anhydrous ethanol solution of cyanuric chloride was added dropwise. The mixed solution was poured into a microwave reactor, and after microwave irradiation at 70°C for 1 hour, it was transferred to a reaction bottle and cooled to room temperature. 1.2 parts by weight of DOPO flame retardant was dissolved in anhydrous ethanol and slowly added dropwise to the reaction bottle. After heating to 60°C, the reaction was continued for 4 hours, filtered and washed under reduced pressure, and the filter cake was dried at 70°C for 6 hours. The composite flame retardant was obtained after grinding.
[0043] The amount of anhydrous ethanol used to dissolve the material each time is 30 parts by volume.
[0044] The preparation method of modified magnesium hydroxide is as follows: 160 parts by mass of sodium hydroxide and 30 parts by mass of urea are dissolved in 70 parts by volume of deionized water to prepare a mixed alkaline solution, which is stored for standby use; 500 parts by volume of a 2 mol / L magnesium chloride solution is slowly dropped into the mixed alkaline solution, and stirred for 1 hour to obtain a mixed solution; 6.5 parts by mass of sodium stearate are weighed and dissolved in 70 parts by volume of hot water, and the solution is dropped into the mixed solution, and the mixture is continuously stirred for 0.5 hours. The reaction temperature is 55° C., and the product is centrifugally washed with hot deionized water for 3 times, dried at 60° C. for 10 hours, and then crushed to obtain modified magnesium hydroxide.
[0045] Example 3: A high temperature resistant flame retardant cable, comprising the following raw materials in weight ratio: 28 parts of compound flame retardant, 20 parts of ethylene-vinyl acetate copolymer with 40% vinyl acetate content, 20 parts of ethylene-octene copolymer with Shore hardness of 50-75A, 20 parts of maleic anhydride grafted ethylene-vinyl acetate copolymer, 15 parts of wear agent, 0.7 parts of silane coupling agent, 0.7 parts of lubricant and 1 part of antioxidant; the compound flame retardant comprises a composite flame retardant and modified magnesium hydroxide, and the mass ratio of the composite flame retardant to the modified magnesium hydroxide is 1:6; the wear agent is hollow microspheres with a particle size in the range of 2-20 microns, the lubricant is polysiloxane, and the antioxidant is a hindered phenol antioxidant.
[0046] A method for preparing a high temperature resistant flame retardant cable, such as Figure 1 As shown, the method comprises the following steps: adding a composite flame retardant, modified magnesium hydroxide, ethylene-vinyl acetate copolymer, ethylene-octene copolymer, maleic anhydride grafted ethylene-vinyl acetate copolymer, hollow microspheres, silane coupling agent, lubricant and antioxidant into a twin-roll mill for melt blending, transferring the materials into a twin-screw extruder for extrusion granulation, wherein the temperature of the twin-screw extruder is set to 150° C., the feeding frequency is 30 Hz, and the screw speed is 280 r / min; after drying, placing the masterbatch in a pipe extruder, melt extruding, molding, and cooling to room temperature to obtain a high temperature resistant flame retardant cable.
[0047] The preparation method of the composite flame retardant is as follows:
[0048] Put cyanuric chloride into a purification bottle, put a matching watch glass on the purification bottle, heat the purification bottle to make the cyanuric chloride sublime, then cool it to the bottom of the watch glass, perform recrystallization purification, scrape off the cyanuric chloride at the bottom of the watch glass, and use it immediately;
[0049] 5 parts by weight of terephthalaldehyde were dissolved in anhydrous ethanol and put into a reaction bottle. 3.9 parts by weight of 4,4-diaminodiphenylmethane dissolved in anhydrous ethanol was slowly added dropwise to the reactor, stirred at 400 r / min, nitrogen was introduced and the temperature was raised to 65°C for reaction for 1.5 hours. During the reaction, the progress of the reaction was monitored by TLC. A yellow precipitate was produced by the reaction. After the reaction was completed, the system was filtered and the precipitate was washed with ethanol and dried to obtain an intermediate. The intermediate was mixed with anhydrous ethanol and 0. 88 parts by mass of anhydrous ethanol solution of diethylenetriamine were stirred and mixed, and 1 part by mass of anhydrous ethanol solution of cyanuric chloride was added dropwise, and the mixed solution was poured into a microwave reactor, and microwaved at 75°C for 1.5 hours, and then transferred to a reaction bottle, cooled to room temperature, and 1 part by mass of DOPO flame retardant was dissolved in anhydrous ethanol, and slowly added dropwise to the reaction bottle, and the temperature was raised to 65°C and the reaction was continued for 4.5 hours, and the mixture was filtered and washed under reduced pressure. The filter cake was dried at 80°C for 7 hours and ground to obtain a composite flame retardant.
[0050] The amount of anhydrous ethanol used to dissolve the material each time is 30 parts by volume.
[0051] The preparation method of modified magnesium hydroxide is as follows: 150 parts by mass of sodium hydroxide and 25 parts by mass of urea are dissolved in 50 parts by volume of deionized water to prepare a mixed alkaline solution, which is stored for standby use; 450 parts by volume of a 2 mol / L magnesium chloride solution is slowly dropped into the mixed alkaline solution, and stirred for 1 hour to obtain a mixed solution; 6 parts by mass of sodium stearate are weighed and dissolved in 50 parts by volume of hot water, and the solution is dropped into the mixed solution, and the mixture is continuously stirred for 1 hour. The reaction temperature is 60°C, and the product is centrifugally washed with hot deionized water for 5 times, dried at 65°C for 12 hours, and then crushed to obtain modified magnesium hydroxide.
[0052] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A high temperature resistant flame retardant cable, characterized in that: The invention comprises the following raw materials in weight ratio: 20-40 parts of compound flame retardant, 10-30 parts of ethylene-vinyl acetate copolymer, 10-30 parts of ethylene-octene copolymer, 10-30 parts of maleic anhydride grafted ethylene-vinyl acetate copolymer, 10-30 parts of anti-wear agent, 0.5-2 parts of silane coupling agent, 0.5-2 parts of lubricant and 0.1-3 parts of antioxidant; The composite flame retardant comprises a composite flame retardant and modified magnesium hydroxide, wherein the mass ratio of the composite flame retardant to the modified magnesium hydroxide is 1:6-9; the preparation method of the composite flame retardant comprises: dissolving 5-5.5 parts by mass of terephthalaldehyde in a solvent and putting the mixture into a reaction bottle, slowly dropping 3.9-4.2 parts by mass of 4,4-diaminodiphenylmethane dissolved in the solvent into a reactor, stirring at 300-500 r / min, introducing nitrogen and heating to 60-70°C for reaction for 1-2h, filtering the system after the reaction is completed, washing the precipitate with ethanol, and drying to obtain an intermediate; The mixture is mixed with a solvent, a solvent solution containing 0.88-0.96 parts by mass of diethylenetriamine is added dropwise, the mixture is stirred and mixed, a solvent solution containing 1-1.2 parts by mass of cyanuric chloride is added dropwise, the mixed solution is poured into a microwave reactor, microwaved at 70-80° C. for 1-2 hours, and then transferred to a reaction bottle, cooled to room temperature, 1-1.2 parts by mass of DOPO flame retardant is dissolved in the solvent, and the mixture is slowly added dropwise to the reaction bottle, the mixture is heated to 60-70° C., and the reaction is continued for 4-5 hours, the mixture is filtered and washed under reduced pressure, and the filter cake is dried at 70-80° C. for 6-8 hours, and the composite flame retardant is obtained after grinding; The preparation method of the modified magnesium hydroxide comprises: weighing 150-160 parts by mass of sodium hydroxide and 25-30 parts by mass of urea, dissolving them in 50-70 parts by volume of deionized water, preparing a mixed alkaline solution, and storing it for use; slowly dropping 450-500 parts by volume of a 2 mol / L magnesium chloride solution into the mixed alkaline solution, stirring for 1-1.5 hours to obtain a mixed solution; weighing 6-6.5 parts by mass of sodium stearate, dissolving it in 50-70 parts by volume of hot water, dropping it into the mixed solution, continuously stirring for 0.5-1 hour, the reaction temperature is 55-60° C., the product is centrifugally washed with hot deionized water for 3-5 times, dried at 60-65° C. for 10-12 hours, and then crushed to obtain the modified magnesium hydroxide.
2. A high temperature resistant flame retardant cable according to claim 1, characterized in that: The vinyl acetate content of the ethylene-vinyl acetate copolymer is 30%-60%, and the Shore hardness of the ethylene-octene copolymer is 50-75A.
3. A high temperature resistant flame retardant cable according to claim 1, characterized in that: The anti-wear agent is hollow microspheres with a particle size in the range of 2-20 microns, the lubricant is one or more of polysiloxane, erucamide, and zinc stearate, and the antioxidant is one or more of hindered phenol antioxidants, phosphite antioxidants, and hindered amine antioxidants.
4. The high temperature resistant flame retardant cable according to claim 1, characterized in that: The solvent is anhydrous ethanol.
5. The high temperature resistant flame retardant cable according to claim 1, characterized in that: The preparation method of the composite flame retardant also includes pretreatment of raw materials: putting cyanuric chloride into a purification bottle, placing a matching watch glass on the purification bottle, heating the purification bottle to sublime the cyanuric chloride, then cooling it at the bottom of the watch glass, scraping off the cyanuric chloride at the bottom of the watch glass, and using it immediately after preparation.
6. The method for preparing a high temperature resistant flame retardant cable according to claim 1, characterized in that: The following steps are involved: The composite flame retardant, modified magnesium hydroxide, ethylene-vinyl acetate copolymer, ethylene-octene copolymer, maleic anhydride grafted ethylene-vinyl acetate copolymer, hollow microspheres, silane coupling agent, lubricant and antioxidant are added to a double-roll mill for melt blending, and the materials are transferred to a twin-screw extruder for extrusion granulation. After drying, the masterbatch is placed in a pipe extruder, melt-extruded, molded, and cooled to room temperature to obtain a high temperature resistant flame retardant cable.
7. The method for preparing a high temperature resistant flame retardant cable according to claim 6, characterized in that: The temperature of the twin-screw extruder is set at 140-160° C., the feeding frequency is 25-35 Hz, and the screw speed is 260-300 r / min.
Citation Information
Patent Citations
Highly-elastic, wear-resistant, low-smoke, zero-halogen and flame-retardant cable material
CN103483675A
Cited By
Flame-retardant cable and processing method
CN121768758A