A MOCVD device for real-time monitoring of epitaxial wafer cracks
By using high-definition cameras and light sensors in the MOCVD equipment to analyze the surface change information of the epitaxial wafer, calculate the crack reflection value, and adjust the equipment parameters in real time, the problem of cracks in the epitaxial wafer during the heating and cooling processes is solved and the generation of defective products is reduced. Improved production efficiency and economy.
Patent Information
- Application Number
- CN202410243642.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-04
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2044-03-04
AI Technical Summary
In MOCVD equipment, epitaxial wafers are prone to cracks during the heating and cooling processes, leading to batch production of defective products and economic losses. Current technology is difficult to monitor and correct in real time.
A MOCVD equipment for real-time monitoring of epitaxial wafer cracks is designed. It uses an analysis unit combined with a high-definition camera and a light sensor to obtain and analyze the surface change information of the epitaxial wafer, including phase transfer, surface reflectivity and scattering intensity information, to calculate the crack response. value, real-time adjustment of equipment operating parameters to avoid cracks.
Real-time monitoring and correction of epitaxial wafer cracks is achieved, reducing the generation of defective products, improving production efficiency and economy, providing more comprehensive and accurate crack detection results, and avoiding unnecessary detection and energy consumption.
Smart Images

Figure CN118109899B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of metal organic chemical vapor deposition, in particular to a MOCVD device for real-time monitoring of crack conditions of an epitaxial wafer. Background Art
[0002] MOCVD is the abbreviation of Metal Organic Chemical Vapor Deposition. It is a technology used to grow thin films and crystals, and is widely used in the fields of semiconductors and optoelectronics. MOCVD equipment is the equipment used to perform this deposition process.
[0003] Epitaxial wafers usually refer to thin films or crystal layers grown on the surface of a substrate. These layers are called epilayers because they are deposited on the surface of the substrate, extending the structure of the original crystal. The characteristics of epitaxial wafers (such as thickness, composition, crystal structure, etc.) are usually achieved by controlling various parameters in the MOCVD process, such as the flow rate of precursor gases, reaction temperature and pressure, etc.
[0004] During the growth process of the epitaxial wafer, cracks in the film will occur due to the quality mismatch during the heating process and the thermal mismatch during the cooling process. Once cracks occur, defective products will be produced in batches, resulting in a large amount of economic losses. Therefore, it is necessary to propose an MOCVD device that can monitor the crack situation of the epitaxial wafer in real time.
[0005] In view of the above technical defects, a solution of a MOCVD device for real-time monitoring of cracks in epitaxial wafers is proposed. Summary of the invention
[0006] To solve the above problems, the present invention provides the following technical solutions: an MOCVD device for real-time monitoring of cracks in epitaxial wafers, comprising a device body, a growth reaction chamber and an annealing chamber arranged inside the device body, a heater being arranged inside the growth reaction chamber, a cooler being arranged inside the annealing chamber, and a finished product recovery chamber for storing products being arranged inside the device body;
[0007] The analysis unit includes a collection component and a feedback adjustment module. The collection component includes a high-definition camera and a light sensor. The high-definition camera and the light sensor are used to record the crack conditions of the epitaxial wafer.
[0008] Furthermore, a robotic arm is disposed inside the main body of the device, a transfer bracket is disposed at the end of the robotic arm, the robotic arm is located between the growth reaction chamber and the annealing chamber, and a phase transfer reference surface is disposed beside the robotic arm.
[0009] Furthermore, a top cover is provided on the top of the device body, the high-definition camera and the light sensor are both provided on the bottom of the top cover, and an illumination light source is also provided on the bottom of the top cover.
[0010] Furthermore, the feedback adjustment module includes a controller, and the controller is electrically connected to the high-definition camera, the light sensor and the device body.
[0011] The present invention also discloses a monitoring method for MOCVD equipment for real-time monitoring of cracks in epitaxial wafers, comprising the following steps:
[0012] Obtain surface change information of epitaxial wafers through high-definition cameras;
[0013] Making judgment on the acquired surface change information;
[0014] Measuring the morphological change information of the epitaxial wafer by means of a light sensor, wherein the morphological change information includes phase shift information, surface reflectivity information, and scattering intensity information;
[0015] Analyze and classify the acquired morphological change information;
[0016] The operating parameters of the device body are adjusted according to the morphological change information.
[0017] Furthermore, the step of determining the acquired surface change information includes:
[0018] The controller obtains the surface change information of the epitaxial wafer collected by the high-definition camera in real time;
[0019] If the surface change information of the epitaxial wafer collected this time does not change from the surface change information collected last time, it is determined that the working state is normal, and further detection of the subsequent light sensor is not triggered;
[0020] If the surface change information of the epitaxial wafer collected this time is different from the surface change information collected last time, it is determined that the working state is abnormal, triggering further detection by subsequent light sensors.
[0021] Furthermore, the step of measuring the morphological change information of the epitaxial wafer by means of a light sensor comprises:
[0022] Providing constant light intensity through lighting source;
[0023] The light sensor illuminates the surface of the epitaxial wafer at an appropriate angle, and the scattering intensity information of each epitaxial wafer surface is determined by the intensity of the scattered light received by the light sensor. The change of the scattering intensity information is positively correlated with the crack.
[0024] The angle of the light sensor is adjustable. By adjusting the incident angle of the light sensor, the reflected light on the surface of the epitaxial wafer can be obtained. The surface reflectivity information can be obtained through the intensity of the reflected light received by the light sensor.
[0025] The illumination light source is divided into two beams, one irradiates the surface of the epitaxial wafer, and the other directly irradiates the phase shift reference surface. The controller obtains and analyzes the interference pattern of the two beams of light to obtain the phase shift information.
[0026] Furthermore, the step of analyzing and classifying the acquired morphological change information includes:
[0027] The acquired phase shift information, surface reflectivity information and scattering intensity information are substituted into the crack reflection value calculation model to obtain the crack reflection value, wherein the calculation formula of the crack reflection value calculation model is:
[0028]
[0029] Among them, L is the crack reflection value, η1, ω1 and They are the phase shift information, surface reflectivity information and scattering intensity information of the epitaxial wafer, and G1, P1 and T1 are the influence weights of the phase shift information, surface reflectivity information and scattering intensity information of the epitaxial wafer on the crack reflection value.
[0030] Furthermore, the steps for determining and classifying the crack reflection value L are as follows:
[0031] If L≤0.36, it can be determined that the cause of the crack is the mismatch of the quality during the heating process.
[0032] If L>1.45, it can be determined that the cause of the cracks is the thermal mismatch during the cooling process.
[0033] Furthermore, the step of adjusting the operating parameters of the device body according to the adjustment difference information includes:
[0034] When it is determined that the film cracks are caused by the mismatch of the character during the heating process, the epitaxial structure growth parameters are continuously adjusted, and the parameter adjustment range is adjusted by 0.3% L each time until no new cracks appear;
[0035] When it is determined that the film cracks are caused by the mismatch of the character during the cooling process, the epitaxial structure growth parameters are continuously adjusted, and the parameter adjustment range is adjusted by 0.27% L each time until no new cracks appear;
[0036] After crack conditions are detected multiple times, the adjustment parameters are accumulated and the optimal operating parameters are determined, and the controller records the parameters.
[0037] Compared with the prior art, the present invention has the following beneficial effects:
[0038] 1. In the present invention, the state of the epitaxial wafer inside the device body can be monitored in real time through the acquisition component, and the crack conditions of the epitaxial wafer can be recorded through the high-definition camera and the light sensor. The controller can adjust the operating parameters of the device body in real time according to the state of the epitaxial wafer crack. When a crack appears in a certain epitaxial wafer, the operating parameters are corrected in time to avoid the mass production of defective products and prevent a large amount of economic losses.
[0039] 2. In the present invention, when the surface change information of the epitaxial wafer has not changed from the information collected last time, the method determines that the working state is normal and there is no need to trigger further detection of subsequent light sensors. This intelligent judgment can save resources, avoid unnecessary detection and energy consumption, and improve the efficiency and economy of the method.
[0040] 3. This method combines phase shift information, surface reflectivity information and scattering intensity information, and substitutes them into the crack reflection value calculation model to comprehensively analyze the morphological changes of the epitaxial wafer from multiple aspects. Such a comprehensive analysis can provide more comprehensive and accurate crack detection results. By calculating the crack reflection value, the crack situation is quantified, so that the existence and severity of the crack can be quantitatively evaluated. This quantitative evaluation helps to more accurately understand the quality status of the epitaxial wafer. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] In order to facilitate understanding by those skilled in the art, the present invention is further described below in conjunction with the accompanying drawings;
[0042] Figure 1 It is a schematic diagram of the top view of the structure of the present invention;
[0043] Figure 2 It is a schematic diagram of the overall structure of the present invention;
[0044] Figure 3 It is a schematic diagram of the structure of the mechanical arm in the present invention;
[0045] Figure 4 It is a schematic diagram of the structure of the top cover plate in the present invention;
[0046] Figure 5 for Figure 4 Enlarged view of point A in the middle;
[0047] Figure 6 The diagram is a schematic diagram of a monitoring method of an MOCVD device for real-time monitoring of crack conditions of an epitaxial wafer in the present invention.
[0048] Figure numerals: 1. Equipment body; 2. Robotic arm; 3. Transfer bracket; 4. Growth reaction chamber; 5. Annealing chamber; 6. Heater; 7. Cooler; 8. Finished product recovery chamber; 9. Top cover; 10. High-definition camera; 11. Light sensor; 12. Light source. DETAILED DESCRIPTION
[0049] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0050] Example 1
[0051] See also Figure 1-Figure 5 , a MOCVD device for real-time monitoring of cracks in epitaxial wafers, comprising a device body 1, and also comprising a growth reaction chamber 4 and an annealing chamber 5 arranged inside the device body 1, wherein a heater 6 is arranged inside the growth reaction chamber 4, and a cooler 7 is arranged inside the annealing chamber 5, and a finished product recovery chamber 8 for storing products is also arranged inside the device body 1;
[0052] The analysis unit includes a collection component and a feedback adjustment module. The collection component includes a high-definition camera 10 and a light sensor 11. The high-definition camera 10 and the light sensor 11 are both used to record the crack conditions of the epitaxial wafer.
[0053] In the present invention, the state of the epitaxial wafer inside the device body 1 can be monitored in real time through the acquisition component, and the crack conditions of the epitaxial wafer can be recorded through the high-definition camera 10 and the light sensor 11. The controller can adjust the operating parameters of the device body 1 in real time according to the state of the epitaxial wafer cracks. When a crack appears in an epitaxial wafer, the operating parameters are corrected in time to avoid the mass production of defective products and prevent large economic losses.
[0054] See also Figure 1-Figure 3 A robotic arm 2 is arranged inside the device body 1, a transfer bracket 3 is arranged at the end of the robotic arm 2, the robotic arm 2 is located between the growth reaction chamber 4 and the annealing chamber 5, a phase transfer reference surface is arranged on the side of the robotic arm 2, a top cover plate 9 is arranged on the top of the device body 1, the high-definition camera 10 and the light sensor 11 are arranged at the bottom of the top cover plate 9, and an illumination light source 12 is also arranged at the bottom of the top cover plate 9, and the feedback adjustment module includes a controller, and the controller is electrically connected to the high-definition camera 10, the light sensor 11 and the device body 1.
[0055] It should be noted that: by arranging a mechanical arm 2 inside the device body 1, a transfer bracket 3 is provided at the end thereof, so that samples or devices can be flexibly transferred between the growth reaction chamber 4 and the annealing chamber 5, thereby improving the operating efficiency and flexibility of the device, and a phase transfer reference surface is arranged beside the mechanical arm 2, which helps to ensure the sample position and phase control during the growth or annealing process;
[0056] A top cover plate 9 is provided on the top of the device body 1, and a high-definition camera 10, a light sensor 11 and an illumination light source 12 are placed at the lower part of the cover plate. Such a configuration can provide real-time monitoring and control of the internal process of the reaction chamber, which helps to maintain the stability and controllability of the preparation conditions. By electrically connecting the high-definition camera 10, the light sensor 11 and the device body 1 to the controller, these components can exchange information quickly and reliably, which helps to realize intelligent control and monitoring of the device. The feedback adjustment module enables the present invention to have the ability of feedback control, and the growth reaction process can be adjusted according to the real-time monitoring information, thereby improving the consistency and quality of the preparation.
[0057] Example 2
[0058] The difference between this embodiment and embodiment 1 is that, please refer to Figure 6 The present invention also discloses a monitoring method for MOCVD equipment for real-time monitoring of cracks in epitaxial wafers, comprising the following steps:
[0059] Acquire surface change information of the epitaxial wafer by a high-definition camera 10;
[0060] Making judgment on the acquired surface change information;
[0061] Measuring the morphological change information of the epitaxial wafer by means of the light sensor 11, wherein the morphological change information includes phase shift information, surface reflectivity information and scattering intensity information;
[0062] Analyze and classify the acquired morphological change information;
[0063] The operating parameters of the device body 1 are adjusted according to the morphological change information.
[0064] It should be noted that the present invention can obtain the surface change information and morphological change information of the epitaxial wafer in real time through the high-definition camera 10 and the light sensor 11, and realize continuous monitoring of the state of the epitaxial wafer. The morphological change information obtained by the light sensor 11 includes phase shift information, surface reflectivity information and scattering intensity information, which can provide a multi-dimensional reference for the surface state and quality of the epitaxial wafer. The obtained morphological change information is analyzed and classified, and various conditions of the epitaxial wafer surface can be identified through algorithms or models, and can be automatically classified;
[0065] Adjustment difference information is obtained based on the classification results. The operating parameters of the equipment body 1 are adjusted using this information, and the equipment can be automatically feedback-adjusted to avoid or reduce the occurrence of problems such as epitaxial wafer cracks, thereby improving the efficiency and quality of epitaxial wafer growth. Through real-time monitoring and intelligent analysis, problems can be identified before cracks occur in the epitaxial wafer, and timely measures can be taken to make adjustments, thereby avoiding unnecessary losses and providing early warning of problems that may occur during the epitaxial wafer growth process.
[0066] Specifically, the step of judging the acquired surface change information includes:
[0067] The controller acquires the surface change information of the epitaxial wafer collected by the high-definition camera 10 in real time;
[0068] If the surface change information of the epitaxial wafer collected this time does not change from the surface change information collected last time, it is determined that the working state is normal, and the subsequent light sensor 11 is not triggered for further detection;
[0069] If the surface change information of the epitaxial wafer collected this time is different from the surface change information collected last time, it is determined that the working state is abnormal, and further detection by the subsequent light sensor 11 is triggered.
[0070] By acquiring the surface change information of the epitaxial wafer collected by the high-definition camera 10 in real time, the state of the epitaxial wafer can be monitored and judged immediately, which can help take timely actions when problems occur, reduce production interruptions and the generation of defective products. When the collected surface change information of the epitaxial wafer is different from the information collected last time, the method automatically determines that the working state is abnormal and triggers further detection by the subsequent light sensor 11, which can reduce human errors and missed detections, and improve the reliability and accuracy of the monitoring method;
[0071] When the surface change information of the epitaxial wafer has not changed from the information collected last time, the method determines that the working state is normal and there is no need to trigger further detection of the subsequent light sensor 11. This intelligent judgment can save resources, avoid unnecessary detection and energy consumption, and improve the efficiency and economy of the method. Combined with the data of the high-definition camera 10 and the light sensor 11, the method can comprehensively monitor the surface changes of the epitaxial wafer, so as to better understand the status of the epitaxial wafer and make timely adjustments. This comprehensive monitoring can effectively prevent the occurrence of problems such as cracks in the epitaxial wafer and improve production quality and stability.
[0072] Specifically, the step of measuring the morphological change information of the epitaxial wafer by the light sensor 11 includes:
[0073] Providing a constant illumination intensity through the illumination light source 12;
[0074] The light sensor 11 irradiates the surface of the epitaxial wafer at an appropriate angle, and the scattering intensity information of each epitaxial wafer surface is determined by the intensity of the scattered light received by the light sensor 11, and the change of the scattering intensity information is positively correlated with the crack;
[0075] The angle of the light sensor 11 is adjustable. By adjusting the incident angle of the light sensor 11, the reflected light on the surface of the epitaxial wafer can be obtained. The surface reflectivity information can be obtained through the intensity of the reflected light received by the light sensor 11.
[0076] The illumination light source 12 is divided into two beams, one irradiates the surface of the epitaxial wafer, and the other directly irradiates the phase shift reference surface. The controller obtains and analyzes the interference pattern of the two beams of light to obtain the phase shift information.
[0077] It should be noted that the method uses the light sensor 11 to achieve high-precision measurement of changes in epitaxial wafer surface morphology. By receiving the intensity information of scattered light and reflected light on the epitaxial wafer surface, it can accurately capture small changes in the epitaxial wafer surface, including defects such as cracks. This monitoring method can achieve real-time monitoring of epitaxial wafer crack conditions. The rapid response capability of the light sensor 11 enables the method to instantly capture changes in epitaxial wafer surface morphology, thereby promptly discovering and handling problems. The light sensor 11 is a non-contact detection method that does not require direct contact with the epitaxial wafer surface, avoiding possible damage to the epitaxial wafer. This non-contact detection can not only protect the integrity of the epitaxial wafer, but also improve production efficiency.
[0078] The angle-adjustable design of the light sensor 11 enables the method to flexibly adjust the incident angle as needed to obtain scattered light and reflected light information at different angles. This flexibility enables the monitoring method to adapt to changes in surface characteristics of different epitaxial wafers. The illumination light source 12 is divided into two beams and passes through a phase shift reference surface to generate an interference pattern. The interference pattern of the two beams is acquired and analyzed by the controller to obtain phase shift information. This interference pattern analysis can further improve the detection precision and accuracy of epitaxial wafer surface morphological changes. Specifically, the steps of analyzing and classifying the acquired morphological change information include:
[0079] The acquired phase shift information, surface reflectivity information and scattering intensity information are substituted into the crack reflection value calculation model to obtain the crack reflection value, wherein the calculation formula of the crack reflection value calculation model is:
[0080] Among them, L is the crack reflection value, η1, ω1 and They are the phase shift information, surface reflectivity information and scattering intensity information of the epitaxial wafer respectively, and G1, P1 and T1 are the influence weights of the phase shift information, surface reflectivity information and scattering intensity information of the epitaxial wafer on the crack reflection value respectively.
[0081] Furthermore, the steps for determining and classifying the crack reflection value L are as follows:
[0082] If L≤0.36, it can be determined that the cause of the crack is the mismatch of the quality during the heating process.
[0083] If L>1.45, it can be determined that the cause of the cracks is the thermal mismatch during the cooling process.
[0084] It is worth mentioning that this method combines phase shift information, surface reflectivity information and scattering intensity information, and substitutes them into the crack reflection value calculation model to comprehensively analyze the morphological changes of the epitaxial wafer from multiple aspects. Such a comprehensive analysis can provide more comprehensive and accurate crack detection results. By calculating the crack reflection value, the crack situation is quantified, so that the existence and severity of the crack can be quantitatively evaluated. This quantitative evaluation helps to more accurately understand the quality status of the epitaxial wafer, so as to take corresponding measures.
[0085] This method introduces the calculation of crack reflection value and considers the influence weights of phase transfer information, surface reflectivity information and scattering intensity information on the crack reflection value. Therefore, it can comprehensively consider the influence of various factors on the crack formation, so as to better understand the causes and mechanisms of crack formation. By judging and classifying the crack reflection value, the causes of crack formation can be further analyzed to distinguish the cracks caused by quality mismatch during heating and thermal mismatch during cooling, which is helpful for in-depth understanding of the crack formation mechanism and can guide subsequent process optimization and control.
[0086] Because it is based on a real-time monitoring method, it can monitor and analyze the early stages of crack formation, which helps to detect crack problems in a timely manner and take corresponding countermeasures to avoid further crack expansion and cause product quality problems.
[0087] Specifically, the step of adjusting the operating parameters of the device body 1 according to the adjustment difference information includes:
[0088] When it is determined that the film cracks are caused by the mismatch of the character during the heating process, the epitaxial structure growth parameters are continuously adjusted, and the parameter adjustment range is adjusted by 0.3% L each time until no new cracks appear;
[0089] When it is determined that the film cracks are caused by the mismatch of the character during the cooling process, the epitaxial structure growth parameters are continuously adjusted, and the parameter adjustment range is adjusted by 0.27% L each time until no new cracks appear;
[0090] After crack conditions are detected multiple times, the adjustment parameters are accumulated and the optimal operating parameters are determined, and the controller records the parameters.
[0091] Fine adjustment: By adjusting the epitaxial structure growth parameters according to the crack determination, the operating parameters of the equipment body 1 can be finely adjusted. The range of each adjustment is based on the percentage of the crack reflection value. This fine adjustment method can more accurately control the growth process of the epitaxial wafer and help avoid the recurrence of cracks.
[0092] This method adopts different adjustment strategies and parameter ranges for cracks caused by quality mismatch during the heating process and the cooling process. This targeted adjustment can more effectively deal with crack problems caused by different reasons, improve the targetedness and effectiveness of the adjustment, and when cracks are detected multiple times, the parameters are adjusted cumulatively and the optimal operating parameters are determined. This iterative optimization process can gradually improve the equipment operating parameters to make it more adaptable to the needs of epitaxial wafer growth, thereby reducing the possibility of cracks and improving the quality and yield of epitaxial wafers. The controller records the optimal operating parameters, which is convenient for subsequent management and traceability. The recorded parameters can be used as a reference to help operators better understand the operating status of the equipment and make timely adjustments and maintenance. Because it is based on a real-time monitoring method, it can make timely adjustments and processing when crack problems occur to avoid more serious impacts caused by crack expansion. This real-time and responsiveness help to ensure the stability of the production process and product quality.
[0093] The preferred embodiments of the present invention disclosed above are only used to help explain the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to only specific implementation methods. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.
Claims
1. A monitoring method for an MOCVD device for real-time monitoring of cracks in an epitaxial wafer, the device comprising a device body (1), and also comprising a growth reaction chamber (4) and an annealing chamber (5) arranged inside the device body (1), wherein a heater (6) is arranged inside the growth reaction chamber (4), and a cooler (7) is arranged inside the annealing chamber (5), and a finished product recovery chamber (8) for storing products is also arranged inside the device body (1); An analysis unit, the analysis unit comprising a collection component and a feedback adjustment module, the collection component comprising a high-definition camera (10) and a light sensor (11), the high-definition camera (10) and the light sensor (11) both being used to record crack conditions of the epitaxial wafer; A top cover plate (9) is arranged on the top of the device body (1), the high-definition camera (10) and the light sensor (11) are arranged on the bottom of the top cover plate (9), and an illumination light source (12) is also arranged on the bottom of the top cover plate (9); the device is characterized in that: The following steps are involved: Acquiring surface change information of the epitaxial wafer by means of a high-definition camera (10); Making judgment on the acquired surface change information; Measuring morphological change information of the epitaxial wafer by means of a light sensor (11), wherein the morphological change information includes phase shift information, surface reflectivity information, and scattering intensity information; Analyze and classify the acquired morphological change information; Adjusting the operating parameters of the device body (1) according to the morphological change information; The step of judging the acquired surface change information comprises: The controller acquires in real time the surface change information of the epitaxial wafer collected by the high-definition camera (10); If the surface change information of the epitaxial wafer collected this time does not change from the surface change information collected last time, it is determined that the working state is normal, and no further detection of the subsequent light sensor (11) is triggered; If the surface change information of the epitaxial wafer collected this time is different from the surface change information collected last time, it is determined that the working state is abnormal, and further detection by the subsequent light sensor (11) is triggered; The step of measuring the morphological change information of the epitaxial wafer by means of a light sensor (11) comprises: Providing a constant light intensity through an illumination light source (12); The light sensor (11) irradiates the surface of the epitaxial wafer at an appropriate angle, and the scattering intensity information of the surface of each epitaxial wafer is determined by the intensity of the scattered light received by the light sensor (11), and the change of the scattering intensity information is positively correlated with the crack; The angle of the light sensor (11) is designed to be adjustable, and the incident angle of the light sensor (11) is adjusted to obtain reflected light from the surface of the epitaxial wafer, and surface reflectivity information is obtained through the intensity of the reflected light received by the light sensor (11); The illumination light source (12) is divided into two beams, one of which irradiates the surface of the epitaxial wafer and the other directly irradiates the phase shift reference surface. The controller obtains and analyzes the interference pattern of the two beams of light to obtain phase shift information. The steps of analyzing and classifying the acquired morphological change information include: The acquired phase shift information, surface reflectivity information and scattering intensity information are substituted into the crack reflection value calculation model to obtain the crack reflection value, wherein the calculation formula of the crack reflection value calculation model is: ; Where: L is the crack reflection value, , and They are the phase shift information, surface reflectivity information and scattering intensity information of the epitaxial wafer. , and are the influence weights of the phase shift information, surface reflectivity information and scattering intensity information of the epitaxial wafer on the crack reflection value; The steps for determining and classifying the crack reflection value L are as follows: like , it can be determined that the cause of the cracks is the mismatch of the quality during the heating process; like , it can be determined that the cause of the cracks is the thermal mismatch during the cooling process.
2. The method for monitoring MOCVD equipment for real-time monitoring of cracks in epitaxial wafers according to claim 1, characterized in that: The step of adjusting the operating parameters of the device body (1) according to the adjustment difference information comprises: When it is determined that the film cracks are caused by lattice mismatch during the heating process, the epitaxial structure growth parameters are continuously adjusted, and the parameter adjustment range is adjusted by 0.3%L each time until no new cracks appear; When it is determined that the film cracks are caused by the mismatch of the character during the cooling process, the epitaxial structure growth parameters are continuously adjusted, and the parameter adjustment range is adjusted by 0.27%L each time until no new cracks appear; After crack conditions are detected multiple times, the adjustment parameters are accumulated and the optimal operating parameters are determined, and the controller records the parameters.