One-step extrusion molding processing equipment and processing method for wood-plastic door

By adopting a mixing technology of a combination of screw motor and a stirring rod in the wood-plastic door processing equipment, combining extrusion and cooling systems, the problems of uneven mixing of raw materials and blockage are solved, the quality and production efficiency of wood-plastic doors are improved, and high efficiency is achieved cooling and quality inspection.

CN118438632BActive Publication Date: 2024-11-22ZHEJIANG QIDE NEW MATERIAL CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202410663694.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-05-27
Publication Date
2024-11-22
Estimated Expiration
2044-05-27

AI Technical Summary

Technical Problem

It is difficult for existing wood-plastic door processing equipment to crush and mix raw materials, resulting in uneven material layout, affecting the quality of wood-plastic doors and blockage of the feed port.

Method used

A single-time extrusion processing equipment of wood plastic doors is designed, using a screw motor and a mixing rod, which rotates the mixing rod through bevel gear transmission, and the movable rod and the fixed column come into contact with the material, combining the extrusion roller and the pulley. Crush and mix, and efficient cooling and surface moisture removal through synchronous wheel sets and water absorption rollers.

Benefits of technology

The full mixing and extrusion of materials is achieved, the quality and production efficiency of wood-plastic doors are improved, the blockage problem is avoided, and the flatness and quality of the product are ensured through testing instruments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118438632B_ABST
    Figure CN118438632B_ABST
Patent Text Reader

Abstract

The present invention discloses a one-time extrusion molding processing equipment for wood-plastic doors and a processing method thereof, which relates to the technical field of wood-plastic door processing, and comprises an extruder and a feed port, wherein a screw motor is installed on the top of the extruder, and a screw body is fixedly connected to the output end of the screw motor. The one-time extrusion molding processing equipment for wood-plastic doors starts a first driving motor to drive a bevel gear set to rotate, and the bevel gear set drives a stirring rod to rotate. When the stirring rod rotates, the movable rod also rotates around the axis of the stirring rod. When the connecting column on one side of the movable rod contacts the fixed column annularly arranged inside the feeding barrel, the movable rod rotates by itself, so that two mixing forms can be formed in the feeding barrel, so that the contact between the material mixing is more frequent, and the mixing effect of the material is improved. Thus, through the above operation, the materials entering the extrusion molding equipment can be fully mixed, and the extrusion molding effect of the wood-plastic door can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of wood-plastic door processing, in particular to one-step extrusion molding processing equipment for wood-plastic doors and a processing method thereof. Background Art

[0002] Wood-plastic door is a new type of environmentally friendly building material, which is composed of wood and plastic. It has the texture of solid wood and the durability of plastic. It is widely used in home decoration and construction. When processing wood-plastic door, you first need to add PVC powder, stabilizer calcium acid and other materials into the extruder, extrude the wood-plastic door through the mold, and cool it into shape through the cooling mechanism.

[0003] For example, the publication number CN208881144U discloses a wood plastic powder molding device, the main structure of which includes an extruder, the extruder includes a fuselage, a feeding part, a deceleration drive part, a distribution box and an extrusion part; the feeding part includes a feeding hopper and a feeder, and the feeding hopper is a screw conveyor; the wood plastic powder mixed with additives enters the screw conveyor from the feeding hopper, and the screw conveyor continuously conveys the wood plastic powder to the extrusion part; the deceleration drive part transmits power to the first extrusion screw and the second extrusion screw in the extrusion part through the distribution box, and through the extrusion and conveying of the first extrusion screw and the second extrusion screw and the heating in the extrusion part, the wood plastic powder is fully foamed and extruded into the mold. In the wood plastic powder molding device in the utility model, the wood plastic powder is conveyed forward by the screw conveyor and the screw, and there is no situation of clogging the inside of the extruder, so the wood plastic powder can be used directly.

[0004] When the above patent processes the wood-plastic door through the extruder, it only drives the stirring shaft to rotate in a single direction through the motor to mix the materials at the feed port. The mixing form is relatively simple, and other raw materials such as wood-plastic powder and additives will clump when added to the extruder. If they are not crushed and mixed, the wood-plastic door extruded from the extruder will have uneven distribution of various materials, thereby affecting the quality of the wood-plastic door. The materials at the feed port are generally directly fed into the extruder. The concentrated feeding of these materials will cause the feed port to be blocked, affecting the discharge of the material. Summary of the invention

[0005] The object of the present invention is to provide a one-step extrusion molding processing equipment for wood-plastic doors and a processing method thereof, so as to solve the problem that the existing extrusion molding processing equipment mentioned in the above background technology is difficult to grind and mix the raw materials.

[0006] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a one-time extrusion molding processing equipment for wood-plastic doors, comprising an extruder and a feed port, a screw motor is installed on the top of the extruder, the output end of the screw motor is fixedly connected to a screw body, the outer side of the screw body is movably connected to a connecting cylinder through a bearing, a heating cylinder is fixed to the outer side of the connecting cylinder, a feeding cylinder is penetrated through the top of the connecting cylinder, a cooling platform is arranged on one side of the extruder, a molding die is installed on the top of the cooling platform, one side of the molding die is fixedly connected to the connecting cylinder, a shaping die is fixed on the other side of the molding die, a cooling pool is fixed on the upper end face of the cooling platform away from the molding die,

[0007] A cold water tank is fixed inside the cooling table, and a water pipe is connected to the bottom of the cold water tank through a pipeline and a water pump, one end of the water pipe is fixedly connected to the top of the cooling pool, the cold water tank and the top of the cooling table are both provided with drainage holes, and a through hole matching the drainage hole on the top of the cooling table is provided at the bottom of the cooling pool. A first driving motor is installed on one side of the feeding barrel, and the output end of the first driving motor is fixedly connected to a first bevel gear through an output shaft, and a second bevel gear is meshedly connected to the outer side of the first bevel gear, and a stirring rod is fixedly connected to one side of the second bevel gear, and the bottom of the second bevel gear is connected to the The feeding barrel is movably connected, and the outer side of the stirring rod is movably connected with a movable rod through a rotating shaft, one end of the movable rod is fixedly connected to a connecting column, and a fixed column is fixedly connected to a position near the connecting column inside the feeding barrel, and multiple groups of fixed columns are provided. The outer side of the fixed column is wrapped with rubber, and a lever is welded and fixed to the top of the stirring rod, and the top of the lever is connected to an extrusion plate through a ball rolling, and the top of the extrusion plate is provided with a rotating groove matching the ball, the top of the ball is fixedly connected to the feed port, and the bottom of the feed port is fixedly connected to the feeding barrel, and the bottom of the feed port is provided with a through groove for discharging.

[0008] Preferably, a fixed plate is provided on the top of the extrusion plate, and the top of the fixed plate is fixedly connected to the feeding barrel, the inside of the feed port is movably connected to an extrusion roller through a rotating shaft, one end of the extrusion roller is fixedly connected to a second pulley, the outer side of the second pulley is sleeved with a belt body, one side of the belt body is sleeved with a first pulley, and the inside of the first pulley is fixedly connected to the output shaft of the first drive motor.

[0009] Preferably, one side of the cooling table is fixedly connected to a second drive motor through a bracket, the output end of the second drive motor is fixedly connected to a first synchronous wheel, the outer side of the first synchronous wheel is sleeved with a first synchronous belt, the middle part of the first synchronous belt is sleeved with a second synchronous wheel, the side of the first synchronous belt away from the first synchronous wheel is sleeved with a third synchronous wheel, one side of the first synchronous wheel is fixedly connected to a driving gear, and the outer side of the driving gear is meshingly connected to a driven gear.

[0010] Preferably, one side of the driven gear is fixedly connected to the first water-absorbing roller via a transmission shaft, one end of the first water-absorbing roller is movably connected to the first fixing frame via a rotating shaft, a second fixing frame is fixed to the bottom of the first fixing frame, the interior of the first fixing frame is fixedly connected to the first extrusion block, a first drainage groove is provided on one side of the first drainage groove, a water collecting box is provided on one side of the water collecting box, and one side of the water collecting box is fixedly connected to the first fixing frame.

[0011] Preferably, one side of the water collecting box is connected to the cold water tank through a pipe, one side of the driving gear is fixedly connected to the second water absorption roller, one end of the second water absorption roller is movably connected to the second fixed frame through a rotating shaft, the interior of the second fixed frame is fixedly connected to the second extrusion block, and a second drainage groove is provided on the side of the second fixed frame close to the second extrusion block, one side of the third synchronous wheel is fixedly connected to a connecting rod, one side of the connecting rod is fixedly connected to a fourth synchronous wheel, the outer side of the fourth synchronous wheel is sleeved with a second synchronous belt, one side of the second synchronous belt is sleeved with a fifth synchronous wheel, one side of the fifth synchronous wheel and the second synchronous wheel are both fixedly connected to the first connecting rod through a connecting shaft, and one side of the two groups of first connecting rods are movably connected to the second connecting rod through a rotating shaft.

[0012] Preferably, one side of the second connecting rod is movably connected to a fixed block via a rotating shaft, a sliding groove for sliding the fixed block is provided inside the cooling pool, the other side of the second connecting rod is movably connected to a gear body via a rotating shaft, one side of the gear body is movably connected to a toggle shaft via a rotating shaft, and a protrusion is fixedly connected to the middle of the connecting rod.

[0013] Preferably, a spoiler is provided on one side of the protrusion, and both sides of the bottom of the spoiler are movably connected to the cooling pool through a rotating shaft. A first spring is fixedly connected to one side of the spoiler, and one end of the first spring is fixedly connected to the cooling pool.

[0014] Preferably, a first pull rope is fixedly connected to one side of the fixed block, a first pull rope is wound around the outer side of the first pull rope, both sides of the first pulley form a rotating structure with the cooling pool through a rotating shaft, one end of the first pull rope is fixedly connected to the first detector, a through hole is provided inside the first detector for sliding of a limit rod, both ends of the limit rod are fixedly connected to the cooling pool, a second pull rope is fixedly connected to one side of the first detector, a second pull rope and a third pulley are wound around the outer side of the second pull rope, and one side of the second pulley and the third pulley are movably connected to the cooling pool through a rotating shaft.

[0015] Preferably, one end of the second pull rope is fixedly connected to the second detector, a round hole for sliding the slide rod is opened inside the second detector, both ends of the slide rod are fixedly connected to the cooling pool, a tension spring is sleeved on the outer side of the slide rod, one end of the tension spring is fixedly connected to the second detector, and the other end of the tension spring is fixedly connected to the cooling pool, pressure sensors are fixed inside the first detector and the second detector, a second spring is fixed on the top of the pressure sensor, a connecting block is fixed on one end of the second spring, movable grooves are opened inside the first detector and the second detector, and the movable grooves are slidably connected to the connecting block.

[0016] A one-step extrusion molding method for a wood-plastic door comprises the following steps:

[0017] S1: Add materials into the feeding barrel, and start the first driving motor to drive the stirring rod to mix the materials in the feeding barrel;

[0018] S2: Start the screw motor to drive the screw body to rotate, and extrude the material entering the connecting barrel into the forming mold;

[0019] S3: The material is formed through the forming mold, and the formed wood-plastic door will enter the shaping mold for shaping;

[0020] S4: The formed WPC door can be cooled by the cooling pool to complete the extrusion molding process of the WPC door.

[0021] Compared with the prior art, the present invention has the following beneficial effects:

[0022] 1. In order to ensure that the material is completely mixed when it contacts the screw body, the first drive motor is started to drive the bevel gear set to rotate, and the bevel gear set drives the stirring rod to rotate. When the stirring rod rotates, the movable rod will also rotate around the axis of the stirring rod. When the connecting column on one side of the movable rod contacts the fixed column arranged in an annular manner inside the feeding barrel, the movable rod will rotate on its own. In this way, two mixing forms can be formed in the feeding barrel, making the contact between the material mixing more frequent and improving the mixing effect of the material. In this way, the materials entering the extrusion molding equipment can be fully mixed through the above operation, and the extrusion molding effect of the wood-plastic door can be improved.

[0023] 2. By starting the second driving motor to drive the synchronous wheel group to rotate, the second synchronous wheel in the synchronous wheel group can drive the first connecting rod and the second connecting rod to rotate, thereby pulling the fixed block to slide back and forth, and at the same time, the second connecting rod can pull the gear body and the toggle shaft to move back and forth, and the gear body will mesh with the rack plate during the movement. When the toggle shaft moves toward the side with higher water temperature in the cooling pool, the toggle shaft can push cold water into the side with high water temperature in the cooling pool to cool the WPC door. The first water absorption roller and the second water absorption roller can be driven by the linkage component to remove moisture from the surface of the WPC door. In this way, the WPC door processed in the extrusion molding processing equipment can be efficiently cooled through the above operation, and the moisture on the surface of the cooled WPC board can be absorbed, which is convenient for subsequent processing.

[0024] 3. When the fixed block moves in the direction away from the shaping mold, the first detector will be pulled to move by the first pull rope. When the first detector moves, the second detector will be pulled to move by the second pull rope and the tension spring will be stretched. When the fixed block moves in the direction, the tension spring will be reset and pull the second detector to move. The second detector can pull the first detector to reset by the second pull rope and the first pull rope. In this way, when the fixed block moves back and forth, the first detector and the second detector will also move back and forth and detect the flatness of the passing wood-plastic door. In this way, through the above operation, the extrusion molding processing equipment can detect the wood-plastic door when it is produced, so as to ensure the quality of the wood-plastic door produced by the extrusion molding processing equipment. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 It is a three-dimensional schematic diagram of the present invention;

[0026] Figure 2 It is a three-dimensional cross-sectional schematic diagram of the present invention;

[0027] Figure 3 It is a three-dimensional cross-sectional schematic diagram of the feed port of the present invention;

[0028] Figure 4 It is a top view of a three-dimensional cross-sectional schematic diagram of a feeding cylinder of the present invention;

[0029] Figure 5 It is a three-dimensional schematic diagram of the feed port of the present invention;

[0030] Figure 6 It is a three-dimensional schematic diagram of the movable rod of the present invention;

[0031] Figure 7 It is a three-dimensional schematic diagram of the cooling stage of the present invention;

[0032] Figure 8 It is a three-dimensional cross-sectional schematic diagram of the cooling stage of the present invention;

[0033] Fig. 9 It is a three-dimensional cross-sectional schematic diagram of the cooling pool of the present invention;

[0034] Fig.10 It is a three-dimensional schematic diagram of the first synchronous belt of the present invention;

[0035] Fig.11 It is a three-dimensional schematic diagram of the shift shaft of the present invention;

[0036] Fig.12 It is a three-dimensional cross-sectional schematic diagram of a first fixing frame of the present invention;

[0037] Fig.13 It is an enlarged schematic diagram of A of the present invention;

[0038] Fig.14 It is a three-dimensional schematic diagram of the slide bar of the present invention;

[0039] Fig.15 It is a three-dimensional cross-sectional schematic diagram of the first detector of the present invention.

[0040] In the figure: 1, extruder; 2, screw motor; 3, screw body; 4, connecting cylinder; 5, heating cylinder; 6, feeding cylinder; 7, cooling table; 8, forming mold; 9, shaping mold; 10, cooling pool; 11, water pipe; 12, first drive motor; 13, first bevel gear; 14, second bevel gear; 15, stirring rod; 16, movable rod; 17, connecting column; 18, fixed column; 19, lever; 20, extrusion plate; 21, ball; 22, fixed plate; 23, feed port; 24, extrusion roller; 25, first pulley; 26, belt body; 27, second pulley; 28, second drive motor; 29, first synchronous wheel; 30, first synchronous belt; 31, second synchronous wheel; 32, third synchronous wheel; 33, driving gear; 34, driven gear; 35, first water suction roller; 36, first The fixing frame; 37, the first extrusion block; 38, the first drainage trough; 39, the water collecting box; 40, the second extrusion block; 41, the second water suction roller; 42, the second fixing frame; 43, the second drainage trough; 44, the first connecting rod; 45, the second connecting rod; 46, the fixing block; 47, the gear body; 48, the toggle shaft; 49, the rack plate; 50, the connecting rod; 51, the protrusion; 52, the spoiler; 53, the first spring; 54, the first pull rope; 55, the first pulley; 56, the first detector; 57, the second pull rope; 58, the second pulley; 59, the third pulley; 60, the second detector; 61, the sliding rod; 62, the tension spring; 63, the limit rod; 64, the pressure sensor; 65, the second spring; 66, the connecting block; 67, the cold water tank; 68, the fourth synchronous wheel; 69, the second synchronous belt; 70, the fifth synchronous wheel. DETAILED DESCRIPTION

[0041] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0042] See also Figure 1 - Fig.15 The present invention provides a technical solution: a one-time extrusion molding processing equipment for wood-plastic doors, comprising an extruder 1 and a feed port 23, a screw motor 2 is installed on the top of the extruder 1, the output end of the screw motor 2 is fixedly connected with a screw body 3, the outer side of the screw body 3 is movably connected with a connecting cylinder 4 through a bearing, a heating cylinder 5 is fixed on the outer side of the connecting cylinder 4, a feeding cylinder 6 is penetrated through the top of the connecting cylinder 4, a cooling platform 7 is arranged on one side of the extruder 1, a molding die 8 is installed on the top of the cooling platform 7, one side of the molding die 8 is fixedly connected with the connecting cylinder 4, a shaping die 9 is fixed on the other side of the molding die 8, and a cooling pool 10 is fixed on the side of the upper end surface of the cooling platform 7 away from the molding die 8;

[0043] A cold water tank 67 is fixed inside the cooling table 7, and a water pipe 11 is connected to the bottom of the cold water tank 67 through a pipeline and a water pump, and one end of the water pipe 11 is fixedly connected to the top of the cooling pool 10. Drainage holes are provided on the cold water tank 67 and the top of the cooling table 7, and a through hole matching the drainage hole on the top of the cooling table 7 is provided at the bottom of the cooling pool 10. A first drive motor 12 is installed on one side of the feeding barrel 6, and the output end of the first drive motor 12 is fixedly connected to the first bevel gear 13 through an output shaft, and the outer side of the first bevel gear 13 is meshingly connected to the second bevel gear 14, and one side of the second bevel gear 14 is fixedly connected to a stirring rod 15, and the bottom of the second bevel gear 14 is movably connected to the feeding barrel 6 through a connecting shaft and a bearing, and the outer side of the stirring rod 15 is movably connected to a movable rod 16 through a rotating shaft, and one end of the movable rod 16 is fixedly connected to a connecting column 17, and a fixed column 18 is fixedly connected to a position near the connecting column 17 inside the feeding barrel 6, and the fixed column 18 is provided with a plurality of groups, and the outer side of the fixed column 18 Wrapped with rubber, a lever 19 is welded and fixed on the top of the stirring rod 15, and the top of the lever 19 is connected to an extrusion disk 20 through a ball rolling, and a rotating groove matching the ball 21 is opened on the top of the extrusion disk 20, and the top of the ball 21 is fixedly connected to the feed port 23, and the bottom of the feed port 23 is fixedly connected to the feeding barrel 6, and a through groove for discharging is opened at the bottom of the feed port 23; a fixed disk 22 is arranged on the top of the extrusion disk 20, and the top of the fixed disk 22 is fixedly connected to the feeding barrel 6, and the inside of the feed port 23 is movably connected to an extrusion roller 24 through a rotating shaft, and one end of the extrusion roller 24 is fixedly connected to a second pulley 27, and the outer side of the second pulley 27 is sleeved with a belt body 26, and one side of the belt body 26 is sleeved with a first pulley 25, and the inside of the first pulley 25 is fixedly connected to the output shaft of the first drive motor 12, and the first bevel gear 13 and the second bevel gear 14 constitute a meshing transmission structure, and the stirring rod 15 constitutes a rotating structure with the movable rod 16 through a rotating shaft;

[0044] In specific implementation, when the wood-plastic door is produced, the raw materials need to be extruded and molded by the extruder 1 and the mold. In order to ensure that the material is completely mixed when it contacts the screw body 3, by starting the first drive motor 12, the first drive motor 12 can drive the first bevel gear 13 to mesh with the second bevel gear 14, and the second bevel gear 14 can drive the stirring rod 15 to rotate. When the stirring rod 15 rotates, the movable rod 16 will also rotate around the axis of the stirring rod 15. When the connecting column 17 on one side of the movable rod 16 contacts the fixed column 18 arranged in an annular manner inside the feeding barrel 6, the movable rod 16 will rotate on its own. In this way, two mixing forms can be formed in the feeding barrel 6, so that the contact between the mixed materials is more frequent, and the mixing effect of the materials is improved;

[0045] At the same time, the first driving motor 12 will also drive the first pulley 25 to rotate, so that the first pulley 25 drives the second pulley 27 to rotate through the belt body 26, and the squeezing roller 24 connected to one side of the second pulley 27 will also rotate accordingly. When the material enters the feed port 23, it will fall into the groove of the squeezing roller 24. When the squeezing roller 24 rotates, the material can be squeezed with the inner wall of the feed port 23, so that the materials that are bonded together are separated and the materials are crushed once.

[0046] While rotating, the stirring rod 15 will also contact the inner wall of the extrusion disk 20 through the ball on the top of the fixed column 18, pushing the extrusion disk 20 to rotate around the ball 21, and the rotating extrusion disk 20 will be close to the fixed disk 22. When the material enters the top of the extrusion disk 20 through the drop groove at the bottom of the feed port 23, the extrusion disk 20 will push the material to contact the conical surface at the bottom of the fixed disk 22, and grind the material twice. After the crushed material is mixed by the stirring rod 15 and the movable rod 16 at the bottom, it can be evenly mixed before the material contacts the screw body 3. In this way, the material entering the extrusion molding equipment can be fully mixed through the above operation, thereby improving the extrusion molding effect of the wood-plastic door.

[0047] See also Figure 1 , Figure 2 , Figure 7 , Figure 8 , Fig. 9 , Fig.10 , Fig.11 , Fig.12 and Fig.13A second driving motor 28 is fixedly connected to one side of the cooling table 7 through a bracket, a first synchronous wheel 29 is fixedly connected to the output end of the second driving motor 28, a first synchronous belt 30 is sleeved on the outer side of the first synchronous wheel 29, a second synchronous wheel 31 is sleeved on the middle part of the first synchronous belt 30, a third synchronous wheel 32 is sleeved on the side of the first synchronous belt 30 away from the first synchronous wheel 29, a driving gear 33 is fixedly connected to one side of the first synchronous wheel 29, and a driven gear 34 is meshedly connected to the outer side of the driving gear 33; a first water-absorbing roller 35 is fixedly connected to one side of the driven gear 34 through a transmission shaft, and one end of the first water-absorbing roller 35 is movably connected to the third water-absorbing roller 35 through a rotating shaft. A fixing frame 36, a second fixing frame 42 is fixed to the bottom of the first fixing frame 36, a first extrusion block 37 is fixedly connected to the inside of the first fixing frame 36, a first drainage groove 38 is provided on one side of the first fixing frame 36 close to the first extrusion block 37, a water collecting box 39 is provided on one side of the first drainage groove 38, and one side of the water collecting box 39 is fixedly connected to the first fixing frame 36; one side of the water collecting box 39 is connected to the cold water tank 67 through a pipeline, a second water suction roller 41 is fixedly connected to one side of the driving gear 33, one end of the second water suction roller 41 is movably connected to the second fixing frame 42 through a rotating shaft, and the second fixing frame 42 is fixedly connected to the inside of the second extrusion block 37. The pressing block 40, a second drainage groove 43 is provided on one side of the second fixing frame 42 near the second extrusion block 40, a connecting rod 50 is fixedly connected to one side of the third synchronous wheel 32, a fourth synchronous wheel 68 is fixedly connected to one side of the connecting rod 50, a second synchronous belt 69 is sleeved on the outer side of the fourth synchronous wheel 68, a fifth synchronous wheel 70 is sleeved on one side of the second synchronous belt 69, the fifth synchronous wheel 70 and one side of the second synchronous wheel 31 are fixedly connected to the first connecting rod 44 through a connecting shaft, and one side of the two groups of first connecting rods 44 are movably connected to the second connecting rod 45 through a rotating shaft; one side of the second connecting rod 45 is movably connected to the fixed block 46 through a rotating shaft, and the cooling pool A slide groove for sliding the fixed block 46 is provided inside 10, the other side of the second connecting rod 45 is movably connected to the gear body 47 through a rotating shaft, one side of the gear body 47 is movably connected to the toggle shaft 48 through a rotating shaft, and a protrusion 51 is fixedly connected to the middle of the connecting rod 50; a spoiler 52 is provided on one side of the protrusion 51, and the two sides of the bottom of the spoiler 52 are movably connected to the cooling pool 10 through a rotating shaft, one side of the spoiler 52 is fixedly connected to the first spring 53, one end of the first spring 53 is fixedly connected to the cooling pool 10, the driving gear 33 and the driven gear 34 form an engaging transmission structure, and the first connecting rod 44 forms a rotating structure with the second connecting rod 45 through the rotating shaft.

[0048] In specific implementation, when the wood-plastic door is produced, the raw materials need to be extruded and formed by the cooperation of the extruder 1 and the mold. The formed wood-plastic door needs to enter the cooling pool 10 for cooling. The cooling pool 10 discharges the water flow into the cold water tank 67 through the through groove at the bottom for cooling, and then the cooled water flow is discharged into the cooling pool 10 through the water pump and the water pipe 11. Since the side of the cooling pool 10 close to the shaping mold 9 first contacts the extruded wood-plastic door, the water temperature on the side of the cooling pool 10 close to the shaping mold 9 will be higher. In order to reduce the temperature on this side and improve the cooling effect on the wood-plastic door, the first synchronous wheel 29 is driven to rotate by starting the second drive motor 28. The first synchronous wheel 29 can drive the second synchronous wheel 31 and the third synchronous wheel 32 to rotate synchronously through the first synchronous belt 30. The diameter of the second synchronous wheel 31 located in the middle is larger than the first synchronous wheel 29 and the third synchronous wheel 32, so the first synchronous wheel 29. The second synchronous wheel 31 and the third synchronous wheel 32 rotate synchronously. When the second synchronous wheel 31 rotates, it will drive the first connecting rod 44 to rotate and pull the second connecting rod 45 to rotate. The second connecting rod 45 can pull the fixed block 46 to slide back and forth in the slide grooves on both sides of the inner wall of the cooling pool 10. At the same time, the second connecting rod 45 can pull the gear body 47 and the toggle shaft 48 to reciprocate. The gear body 47 will mesh with the rack plate 49 during the movement, so that the rack plate 49 drives the toggle shaft 48 to rotate. In this way, the toggle shaft 48 can continuously reciprocate and rotate in the cooling pool 10. When the third synchronous wheel 32 rotates, it will drive the fourth synchronous wheel 68 to rotate through the connecting rod 50. The fourth synchronous wheel 68 transmits power to the fifth synchronous wheel 70 through the second synchronous belt 69, so that the fifth synchronous wheel 70 drives the first connecting rod 44 of another group to rotate, and maintains the stability of the toggle shaft 48 when it moves.

[0049] When the toggle shaft 48 moves toward the side of the cooling pool 10 where the water temperature is higher, due to the meshing of the gear body 47 and the rack plate 49, the arc-shaped concave surface of the outer arc plate will contact the water flow when the toggle shaft 48 rotates, generating a larger thrust, thereby pushing the cold water into the side of the cooling pool 10 where the water temperature is higher. At the same time, the rotating toggle shaft 48 will also push the cold water close to the water surface to the bottom, so that the cold water quickly contacts the wood-plastic door, pushing the wood-plastic door to cool. When the toggle shaft 48 is away from the side of the cooling pool 10 where the water temperature is higher, the arc-shaped convex surface of the outer arc plate of the toggle shaft 48 will contact the water flow, and the thrust generated at this time is smaller, which can reduce the amount of cold water pushed back.

[0050] At the same time, the third synchronous wheel 32 will also drive the connecting rod 50 to rotate when rotating. The connecting rod 50 can move the spoiler 52 to rotate through the arc-shaped protrusion 51 in the middle, so that it pushes the first spring 53 to shrink. When the arc-shaped protrusion 51 is disconnected from the first spring 53, the first spring 53 will reset and drive the spoiler 52 to reset. At this time, the spoiler 52 can push the water flow at the bottom of the WPC door to flow, pushing the water flow on the cold water side to the hot water side. At the same time, the pushed water flow will impact the bottom of the WPC door, so that the water flow with a slower flow speed will quickly contact the WPC door and take away the heat on the WPC door.

[0051] When the wood plastic door is cooled, it will contact the sponge on the outside of the first water absorption roller 35 and the second water absorption roller 41. At this time, the rotating first synchronous wheel 29 will drive the driving gear 33 to mesh with the driven gear 34, driving the first water absorption roller 35 and the second water absorption roller 41 to rotate in the opposite direction, and the rotating sponge will absorb the water droplets adhered to the cooled wood plastic door. After the sponge on the outside of the first water absorption roller 35 rotates and contacts the first extrusion block 37, the sponge will deform, squeeze out the absorbed water, and flow into the water collection box 39 through the first drainage groove 38. The water collected in the water collection box 39 The water will be introduced into the cold water tank 67 through a pipe on one side for recovery, and the second water absorption roller 41 will also come into contact with the second extrusion block 40 when rotating, thereby squeezing out the absorbed water and directly introducing it into the cold water tank 67 through the second drainage groove 43. In this way, the water absorption effect of the sponge on the outer sides of the first water absorption roller 35 and the second water absorption roller 41 can be maintained, and the water droplets adhered to the wood-plastic door can be effectively absorbed. In this way, through the above operation, the wood-plastic door processed in the extrusion molding processing equipment can be efficiently cooled, and the moisture on the surface of the cooled wood-plastic board can be absorbed, which is convenient for subsequent processing.

[0052] See also Fig. 9 , Fig.14 and Fig.15A first pull rope 54 is fixedly connected to one side of the fixed block 46, and a first pulley 55 is wound around the outer side of the first pull rope 54. Both sides of the first pulley 55 form a rotating structure with the cooling pool 10 through a rotating shaft. One end of the first pull rope 54 is fixedly connected to a first detector 56. A through hole for sliding a limit rod 63 is provided inside the first detector 56. Both ends of the limit rod 63 are fixedly connected to the cooling pool 10. A second pull rope 57 is fixedly connected to one side of the first detector 56. A second pulley 58 and a third pulley 59 are wound around the outer side of the second pull rope 57. One side of the second pulley 58 and the third pulley 59 are movably connected to the cooling pool 10 through a rotating shaft; one end of the second pull rope 57 is fixedly connected to a second detector 60. The second detector 60 A round hole is provided inside for the sliding rod 61 to slide, and both ends of the sliding rod 61 are fixedly connected to the cooling pool 10. A tension spring 62 is sleeved on the outer side of the sliding rod 61, one end of the tension spring 62 is fixedly connected to the second detector 60, and the other end of the tension spring 62 is fixedly connected to the cooling pool 10. A pressure sensor 64 is fixed inside the first detector 56 and the second detector 60, a second spring 65 is fixed on the top of the pressure sensor 64, and a connecting block 66 is fixed at one end of the second spring 65. A movable groove is provided inside the first detector 56 and the second detector 60, and the movable groove is slidably connected to the connecting block 66. The sliding rod 61 and the second detector 60 constitute a sliding structure, and the first pulley 55 constitutes a rotating structure with the cooling pool 10 through a rotating shaft.

[0053] In specific implementation, when the wood-plastic door is produced, the raw material needs to be extruded and molded by the cooperation of the extruder 1 and the mold. When the fixed block 46 moves in the direction away from the shaping mold 9, the first detector 56 will be pulled to move by the first pull rope 54. The first pulley 55 can reduce the friction of the movement of the first pull rope 54 and change the pulling direction of the first pull rope 54. When the first detector 56 moves, the second detector 60 will also be pulled to move by the second pull rope 57. The second pulley 58 and the third pulley 59 can guide the second pull rope 57. When the second pull rope 57 moves, the tension spring 62 can be stretched. When the fixed block 46 moves in the direction close to the shaping mold 9, the tension spring 62 will be reset and pull the second detector 60 to move. The second detector 60 can be reset by pulling the first detector 56 by the second pull rope 57 and the first pull rope 54.

[0054] In this way, when the fixed block 46 moves back and forth, the first detector 56 and the second detector 60 will also move back and forth. During the movement of the two, the ball bearings on the connecting block 66 on one side will contact the wood-plastic door sent out from the shaping mold 9. When in contact, the second spring 65 will be squeezed due to the squeezing, and the second spring 65 will transfer the pressure to the pressure sensor 64 for detection. When the wood-plastic door bends or the surface is dented, the connecting block 66 will move, thereby changing the pressure on the pressure sensor 64. At this time, it can be detected that there is a problem with the production of the wood-plastic door, which can help the staff to promptly discover the problems with the extrusion molding processing equipment. In this way, through the above operation, the extrusion molding processing equipment can be tested when producing the wood-plastic door, thereby ensuring the quality of the wood-plastic door produced by the extrusion molding processing equipment.

[0055] A one-step extrusion molding method for a wood-plastic door comprises the following steps:

[0056] S1: Add materials into the feeding barrel 6, and start the first driving motor 12 to drive the stirring rod 15 to mix the materials in the feeding barrel 6;

[0057] S2: Start the screw motor 2 to drive the screw body 3 to rotate, and extrude the material entering the connecting tube 4 into the forming mold 8;

[0058] S3: The material is molded by the molding die 8, and the molded wood-plastic door enters the shaping die 9 for shaping;

[0059] S4: The formed WPC door can be cooled by the cooling pool 10 to complete the extrusion molding process of the WPC door.

[0060] In summary, by adding the material into the feeding barrel 6 and starting the screw motor 2 to drive the screw body 3 to rotate, the screw body 3 can transport the material and extrude it, the heating barrel 5 can heat the material in the connecting barrel 4, and when the material contacts the forming mold 8, the screw body 3 will push the material into the forming mold 8 for forming processing. After the material is in the shaping mold 9, it will be further shaped and cooled once. After entering the cooling pool 10, the wood-plastic door will be completely cooled. The contents not described in detail in this description belong to the prior art known to professional and technical personnel in this field.

[0061] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A one-step extrusion molding processing device for a wood-plastic door, comprising an extruder (1) and a feed inlet (23), characterized in that: A screw motor (2) is installed on the top of the extruder (1), the output end of the screw motor (2) is fixedly connected to a screw body (3), the outer side of the screw body (3) is movably connected to a connecting cylinder (4) through a bearing, a heating cylinder (5) is fixed to the outer side of the connecting cylinder (4), a feeding cylinder (6) penetrates the top of the connecting cylinder (4), a cooling table (7) is provided on one side of the extruder (1), a molding die (8) is installed on the top of the cooling table (7), one side of the molding die (8) is fixedly connected to the connecting cylinder (4), the other side of the molding die (8) is fixed with a shaping die (9), and a cooling pool (10) is fixed on the side of the upper end surface of the cooling table (7) away from the molding die (8); A cold water tank (67) is fixed inside the cooling table (7), the bottom of the cold water tank (67) is connected to a water pipe (11) via a pipeline and a water pump, one end of the water pipe (11) is fixedly connected to the top of the cooling pool (10), the cold water tank (67) and the top of the cooling table (7) are both provided with drainage holes, the bottom of the cooling pool (10) is provided with a through hole matching the drainage hole on the top of the cooling table (7), a first drive motor (12) is installed on one side of the feeding barrel (6), the output end of the first drive motor (12) is fixedly connected to a first bevel gear (13) via an output shaft, the outer side of the first bevel gear (13) is meshingly connected to a second bevel gear (14), one side of the second bevel gear (14) is fixedly connected to a stirring rod (15), the bottom of the second bevel gear (14) is movably connected to the feeding barrel (6) via a connecting shaft and a bearing, the outer side of the stirring rod (15) is movably connected to A movable rod (16), one end of which is fixedly connected to a connecting column (17), a fixed column (18) is fixedly connected to a position near the connecting column (17) inside the feeding barrel (6), and a plurality of fixed columns (18) are provided. The outer side of the fixed column (18) is wrapped with rubber. A lever (19) is welded and fixed to the top of the stirring rod (15), and the top of the lever (19) is connected to an extrusion disk (20) through a ball rolling. The top of the extrusion disk (20) is provided with a rotating groove matching a ball (21). The top of the ball (21) is fixedly connected to a feed port (23), and the bottom of the feed port (23) is fixedly connected to the feeding barrel (6). The bottom of the feed port (23) is provided with a through groove for discharging. When the connecting column (17) on one side of the movable rod (16) contacts the fixed column (18) arranged in an annular manner inside the feeding barrel (6), the movable rod (16) will rotate.

2. The one-step extrusion molding equipment for wood-plastic doors according to claim 1 is characterized in that: A fixed disk (22) is arranged on the top of the extrusion disk (20), the top of the fixed disk (22) is fixedly connected to the feeding barrel (6), the inside of the feed port (23) is movably connected to an extrusion roller (24) via a rotating shaft, one end of the extrusion roller (24) is fixedly connected to a second belt pulley (27), the outer side of the second belt pulley (27) is sleeved with a belt body (26), one side of the belt body (26) is sleeved with a first belt pulley (25), and the first belt pulley (25) is fixedly connected to the output shaft of the first drive motor (12).

3. The one-step extrusion molding equipment for wood-plastic doors according to claim 1 is characterized in that: A second drive motor (28) is fixedly connected to one side of the cooling table (7) via a bracket, a first synchronous wheel (29) is fixedly connected to the output end of the second drive motor (28), a first synchronous belt (30) is sleeved on the outer side of the first synchronous wheel (29), a second synchronous wheel (31) is sleeved on the middle part of the first synchronous belt (30), a third synchronous wheel (32) is sleeved on the side of the first synchronous belt (30) away from the first synchronous wheel (29), a driving gear (33) is fixedly connected to one side of the first synchronous wheel (29), and a driven gear (34) is meshedly connected to the outer side of the driving gear (33).

4. The one-step extrusion molding equipment for wood-plastic doors according to claim 3 is characterized in that: One side of the driven gear (34) is fixedly connected to a first water-absorbing roller (35) via a transmission shaft; one end of the first water-absorbing roller (35) is movably connected to a first fixing frame (36) via a rotating shaft; a second fixing frame (42) is fixed to the bottom of the first fixing frame (36); a first extrusion block (37) is fixedly connected inside the first fixing frame (36); a first drainage groove (38) is provided on one side of the first fixing frame (36) close to the first extrusion block (37); a water collecting box (39) is provided on one side of the first drainage groove (38); one side of the water collecting box (39) is fixedly connected to the first fixing frame (36).

5. The one-step extrusion molding equipment for wood-plastic doors according to claim 4 is characterized in that: One side of the water collecting box (39) is connected to the cold water tank (67) through a pipeline, one side of the driving gear (33) is fixedly connected to a second water absorbing roller (41), one end of the second water absorbing roller (41) is movably connected to a second fixing frame (42) through a rotating shaft, the interior of the second fixing frame (42) is fixedly connected to a second extrusion block (40), a second drainage groove (43) is provided on one side of the second fixing frame (42) close to the second extrusion block (40), and one side of the third synchronous wheel (32) is fixedly connected to a second extrusion block (40). A connecting rod (50) is fixedly connected to one side of the connecting rod (50), a fourth synchronous wheel (68) is fixedly connected to one side of the connecting rod (50), a second synchronous belt (69) is sleeved on the outer side of the fourth synchronous wheel (68), a fifth synchronous wheel (70) is sleeved on one side of the second synchronous belt (69), the fifth synchronous wheel (70) and one side of the second synchronous wheel (31) are both fixedly connected to a first connecting rod (44) via a connecting shaft, and one side of the two sets of first connecting rods (44) are both movably connected to a second connecting rod (45) via a rotating shaft.

6. The one-step extrusion molding equipment for wood-plastic doors according to claim 5, characterized in that: One side of the second connecting rod (45) is movably connected to a fixed block (46) via a rotating shaft, a sliding groove for sliding the fixed block (46) is provided inside the cooling pool (10), the other side of the second connecting rod (45) is movably connected to a gear body (47) via a rotating shaft, one side of the gear body (47) is movably connected to a shifting shaft (48) via a rotating shaft, and a protrusion (51) is fixedly connected to the middle of the connecting rod (50).

7. The one-step extrusion molding equipment for wood-plastic doors according to claim 6 is characterized in that: A spoiler (52) is provided on one side of the protrusion (51), and two sides of the bottom of the spoiler (52) are movably connected to the cooling pool (10) via a rotating shaft. A first spring (53) is fixedly connected to one side of the spoiler (52), and one end of the first spring (53) is fixedly connected to the cooling pool (10).

8. The one-step extrusion molding equipment for wood-plastic doors according to claim 6 is characterized by: A first pull rope (54) is fixedly connected to one side of the fixed block (46), a first pulley (55) is wound around the outer side of the first pull rope (54), and two sides of the first pulley (55) form a rotating structure with the cooling pool (10) via a rotating shaft. One end of the first pull rope (54) is fixedly connected to a first detector (56), and a through hole for a limit rod (63) to slide is provided inside the first detector (56), and two ends of the limit rod (63) are fixedly connected to the cooling pool (10). A second pull rope (57) is fixedly connected to one side of the first detector (56), and a second pulley (58) and a third pulley (59) are wound around the outer side of the second pull rope (57), and one side of the second pulley (58) and the third pulley (59) are movably connected to the cooling pool (10) via a rotating shaft.

9. The one-step extrusion molding equipment for wood-plastic doors according to claim 8, characterized in that: One end of the second pull rope (57) is fixedly connected to the second detector (60), and a round hole for the sliding rod (61) to slide is provided inside the second detector (60), and both ends of the sliding rod (61) are fixedly connected to the cooling pool (10), and a tension spring (62) is sleeved on the outer side of the sliding rod (61), and one end of the tension spring (62) is fixedly connected to the second detector (60), and the other end of the tension spring (62) is fixedly connected to the cooling pool (10), and a pressure sensor (64) is fixed inside the first detector (56) and the second detector (60), and a second spring (65) is fixed on the top of the pressure sensor (64), and a connecting block (66) is fixed at one end of the second spring (65), and a movable groove is provided inside the first detector (56) and the second detector (60), and the movable groove is slidably connected to the connecting block (66).

10. A one-step extrusion molding method for a wood-plastic door, using the one-step extrusion molding equipment for a wood-plastic door according to any one of claims 1 to 9, characterized in that: The following steps are involved: S1: adding materials into the feeding barrel (6), and starting the first driving motor (12) to drive the stirring rod (15) to mix the materials in the feeding barrel (6); S2: starting the screw motor (2) to drive the screw body (3) to rotate, thereby extruding the material entering the connecting cylinder (4) into the forming die (8); S3: The material is molded by a molding mold (8), and the molded wood-plastic door enters a shaping mold (9) for shaping; S4: The formed wood-plastic door can be cooled by the cooling pool (10), thereby completing the extrusion molding process of the wood-plastic door.

Citation Information

Patent Citations

  • The invention discloses a wood-plastic powder forming device

    CN208881144U

  • Anti-blocking dredging silo device

    CN115556252A

  • Double-screw extruder for producing double-wall corrugated pipe

    CN117565352A

  • Wood -plastic wallboard's production system

    CN206416548U

  • The utility model discloses a granulating device for engineering plastics

    CN208867372U