A production and processing molding device for phase change energy storage material and a material molding method thereof

By introducing an L-shaped scraper and heat collection chamber into the processing and forming device of phase change energy storage materials, the automatic cleaning of rectangular molds is realized, the material adhesion problem is solved, the production efficiency and cleaning effect are improved, and energy saving and environmental protection is achieved.

CN118456752BActive Publication Date: 2024-11-22YANGZHOU HANJIANG YANGZI AUTOMOTIVE INTERIOR ACCESSORIES CO L
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410721233.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-06-05
Publication Date
2024-11-22
Estimated Expiration
2044-06-05

AI Technical Summary

Technical Problem

In the existing processing and forming methods of phase change energy storage materials, rectangular molds are prone to material adhesion problems during demolding, which leads to difficulty in cleaning the mold, especially during mass production, which requires frequent cleaning to maintain the demolding effect.

Method used

A production and processing forming device including a hot press, an L-shaped scraper and a heat collecting chamber is designed. The heat compressor is used to heat and extrude the press plate. The scraper automatically rotates and cleans the inner wall of the mold, and the heat collecting chamber recycles heat for the scraper power to realize Automated cleaning and energy saving.

Benefits of technology

It effectively solves the problem of rectangular mold cleaning, realizes automatic cleaning, improves production efficiency and cleaning effect, reduces dependence on electrical systems, and is energy-saving and environmentally friendly.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118456752B_ABST
    Figure CN118456752B_ABST
Patent Text Reader

Abstract

The present invention belongs to the technical field of phase change energy storage materials, specifically, a production and processing molding device of phase change energy storage materials and a material molding method thereof, the molding device comprising a hot press and a mold, the mold is in a rectangular shape with an open top, the hot press is internally provided with a pressing plate, a bracket is arranged on the outside of the hot press; a transmission component for transporting the mold; a scraper movably arranged on the bracket; the phase change energy storage material is prepared by a pressing molding method, by setting an L-shaped scraper, the scraper can be driven to rotate by simply starting the rotation of the rotating seat, and the movement trajectory of the scraper is rectangular, and with the L-shaped design of the scraper, the inner side wall and the inner bottom wall of the mold can be fully scraped and cleaned without dead corners, the cleaning effect on the rectangular mold is better, and the operation is convenient, and the heat emitted by the mold is recovered by setting a heat collection chamber to provide power for the scraper, thereby eliminating the need for an additional electrical system for driving the scraper, which is energy-saving and environmentally friendly.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of phase change energy storage materials, in particular to a production, processing and molding device of phase change energy storage materials and a material molding method thereof. Background Art

[0002] Phase change energy storage materials use the latent heat released and absorbed during the phase change process to store and release energy. Conventional processing and molding methods for phase change energy storage materials include compression molding, which is to load the mixed phase change energy storage material into a mold and shape it by applying external pressure.

[0003] A patent document with publication number CN115011312B discloses a method for preparing a shaped high thermal conductivity phase change energy storage material, the preparation method comprising: first pouring an organic phase change material into a mold and heating it to a liquid state; then adding a thermal conductive material powder to the surface of the liquid organic phase change material; secondly applying pressure using a pressing plate so that the organic phase change material infiltrates into the thermal conductive material, fully mixing, cooling, demolding and shaping, and then a high thermal conductivity phase change energy storage material can be obtained. In the preparation method of the present invention, the phase change material has been shaped after demolding and can directly enter the packaging process, simplifying the production process.

[0004] The above technical solution still has some problems in practical application. It uses a rectangular mold to press and mold the phase change energy storage material. Affected by the characteristics of paraffin itself, some phase change energy storage materials may adhere to the inner wall of the mold during demolding. In batch or assembly line production, the mold needs to be reused. Before each use of the mold, it should be ensured that there is no residue or dirt on the surface to reduce adhesion in the mold to maintain the subsequent demolding effect. For rectangular molds, cleaning the inner wall is more troublesome, and the above technical solution does not effectively solve this problem.

[0005] To this end, the present invention provides a production, processing and molding device for a phase change energy storage material and a material molding method thereof. Summary of the invention

[0006] In order to make up for the deficiencies of the prior art, at least one technical problem raised in the background technology is solved.

[0007] The technical solution adopted by the present invention to solve its technical problem is: a production, processing and molding device of a phase change energy storage material described in the present invention includes a hot press and a mold, the mold is in a rectangular shape with an open top, a pressing plate is movably provided inside the hot press, the pressing plate is used to extrude and mold the material placed inside the mold, the pressing plate is provided with ventilation holes, a heating unit for heating the mold is provided inside the hot press, and also includes: a bracket arranged on the outside of the hot press; a transmission component for transporting the mold; a scraper movably provided on the bracket, and the scraper is L-shaped.

[0008] Preferably, the bracket is provided with a guiding mechanism for guiding the scraper, and the guiding mechanism includes: a swivel seat rotatably provided on the bracket; a lifting plate movably inserted inside the swivel seat, the lifting plate slides longitudinally inside the swivel seat, and the scraper is slidably provided at the bottom end of the lifting plate; and a first spring provided on the scraper.

[0009] Preferably, the guide mechanism also includes: a fixed guide rail fixed to the bracket; a movable guide rail slidably arranged on the fixed guide rail; a slider slidably arranged on the movable guide rail; a movable rod movably inserted into the inside of the rotating seat, the movable rod slides horizontally inside the rotating seat, and the end of the movable rod is rotatably connected to the slider; a second spring arranged on the rotating seat for pushing the movable rod to extend outward.

[0010] Preferably, it also includes a control mechanism, which includes: a push plate slidably arranged on the bracket, the push is used to drive the lifting plate to move up and down; a detection plate slidably arranged on the bracket, the mold passes through the detection plate during the transportation process; a support spring for pushing the detection plate up; and a stroke amplification component, after the detection plate moves, the push plate is driven to move through the stroke amplification component.

[0011] Preferably, the transmission assembly includes a first transmission belt and a second transmission belt, and the first transmission belt and the second transmission belt are respectively aligned with the detection plate before and after lifting.

[0012] Preferably, the stroke amplification component includes: a driving gear, an adjusting gear and a driven gear that are rotatably arranged on the bracket, the driving gear and the adjusting gear are transmitted through a chain belt, and the adjusting gear is meshed with the driven gear for transmission; a first tooth segment arranged on the detection plate, the first tooth segment is meshed with the driving gear; a second tooth segment arranged on the push plate, the second tooth segment is meshed with the driven gear.

[0013] Preferably, the control mechanism also includes: a clockwork assembly arranged on the detection plate, the output shaft of the clockwork assembly is slidably connected to the swivel seat, and a gear ring is provided on the output shaft of the clockwork assembly; a non-return pawl arranged on the push plate, and the non-return pawl is meshingly connected to the gear ring; a heat engine arranged on the bracket, and the input shaft of the clockwork assembly is inserted into the output end of the heat engine.

[0014] Preferably, the control mechanism further includes: a heat collection chamber arranged outside the hot press, the heat collection chamber being used to place the mold taken out of the hot press; and a heat pipe, through which the heat in the heat collection chamber is transferred to the heat engine.

[0015] A method for forming a phase change energy storage material, the method adopts the production and processing forming device of the phase change energy storage material described above, and comprises the following steps:

[0016] Step 1: pour the organic phase change material into a mold, and place the mold in a hot press to heat it until the organic phase change material is in a liquid state;

[0017] Step 2: Spread the thermal conductive material on the surface of the liquid organic phase change material;

[0018] Step 3: Use a pressing plate that matches the size of the mold to extrude the material inside the mold so that the thermal conductive material and the liquid organic phase change material are mixed;

[0019] Step 4: Take the mold out of the hot press and send it into the solar collector for preliminary cooling. At the same time, use the heat engine to recover the heat emitted by the mold in the solar collector;

[0020] Step 5: Take the mold out of the solar collector, place it in an external environment to cool to room temperature, and then demould to obtain a formed phase change energy storage material;

[0021] Step 6: Use a scraper to scrape and clean the mold after demoulding;

[0022] Step 7: Repeat steps 1 to 6, and reuse the mold to continuously produce phase change energy storage materials.

[0023] Preferably, in the step 1, the organic phase change material is paraffin, and in the step 2, the thermal conductive material is a mixture of expanded graphite powder, graphene powder, aluminum powder and gamma iron oxide powder.

[0024] The beneficial effects of the present invention are as follows:

[0025] 1. The production and processing molding device of a phase change energy storage material and its material molding method described in the present invention prepare the phase change energy storage material by a compression molding method. By setting an L-shaped scraper, the scraper can be driven to rotate by simply starting the rotation of the swivel seat, and the movement trajectory of the scraper is rectangular. Combined with the L-shaped design of the scraper, the inner side wall and the inner bottom wall of the mold can be fully scraped and cleaned without dead corners. The cleaning effect on rectangular molds is better and the operation is convenient.

[0026] 2. The production, processing and molding device of phase change energy storage materials and the material molding method thereof described in the present invention use a spring to provide the power required for the scraper to rotate, and use a detection plate to determine the position status of the mold to be cleaned. When the mold moves to the detection plate, the detection plate is pressed down and drives the spring assembly, the push plate and the lifting plate to move down, releasing the non-return state of the spring assembly and driving the scraper to insert into the mold. Then, the spring assembly can drive the scraper to rotate for cleaning, thereby realizing the automatic coordination between the scraper and the mold, and the overall device can be automatically reset, with a high degree of automation.

[0027] 3. The production, processing and molding device of a phase change energy storage material and its material molding method described in the present invention provide a heat collection chamber to initially cool down the mold after hot pressing, and recover the heat emitted by the mold to provide power for the rotating scraping and brushing of the scraper, thereby eliminating the need for an additional electrical system to drive the scraper, thereby saving energy and being environmentally friendly. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] The present invention will be further described below in conjunction with the accompanying drawings.

[0029] Figure 1 is a three-dimensional diagram of the first embodiment of the present invention;

[0030] Figure 2 It is a three-dimensional diagram of the internal structure of the heat press and the bracket and the heat collection chamber;

[0031] Figure 3 It is a three-dimensional diagram of the guiding mechanism and the control mechanism;

[0032] Figure 4 It is an exploded diagram of the guiding mechanism and the local control mechanism;

[0033] Figure 5 This is an exploded view of the detection board and stroke amplification assembly;

[0034] Figure 6 This is a bottom view of the test board;

[0035] Figure 7 It is a schematic diagram of the check pawl and mainspring assembly;

[0036] Figure 8 It is an exploded view of the swivel seat, spring assembly and heat engine;

[0037] In the figure: 1. hot press; 11. pressing plate; 12. vent; 2. mold; 3. bracket; 4. transmission component; 41. first transmission belt; 42. second transmission belt; 5. scraper; 6. guide mechanism; 61. swivel seat; 62. lifting plate; 63. first spring; 64. fixed guide rail; 65. movable guide rail; 66. slider; 67. movable rod; 68. second spring; 7. control mechanism; 71. push plate; 72. detection plate; 73. support spring; 74. stroke amplification component; 741. driving gear; 742. adjusting gear; 743. driven gear; 744. first tooth segment; 745. second tooth segment; 75. spring component; 751. input shaft; 752. output shaft; 753. gear ring; 76. check pawl; 77. heat engine; 771. output end; 78. heat collecting chamber; 79. heat pipe. DETAILED DESCRIPTION

[0038] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods.

[0039] Embodiment 1

[0040] like Figure 1-4 As shown, a production and processing molding device of a phase change energy storage material according to an embodiment of the present invention comprises a hot press 1 and a mold 2, wherein the mold 2 is rectangular with an open top, and a pressing plate 11 is movably provided inside the hot press 1, and the pressing plate 11 is used to extrude and mold the material placed inside the mold 2, and a vent hole 12 is provided on the pressing plate 11, and a heating unit for heating the mold 2 is provided inside the hot press 1, and further comprises:

[0041] A support 3 arranged outside the hot press 1;

[0042] A transmission component 4 for transporting the mold 2;

[0043] A scraper 5 is movably arranged on the bracket 3, and the scraper 5 is L-shaped.

[0044] Specifically, the heating unit is preferably but not limited to an electric heating structure, the bracket 3 is located on the right side of the hot press 1, and the transmission component 4 adopts a transmission belt structure. The materials required for the production of phase change energy storage materials include paraffin, expanded graphite powder, graphene powder, aluminum powder and gamma iron oxide powder. When producing phase change energy storage materials, the mold 2 is placed in the hot press 1, and paraffin with a melting point of 54°C is poured into the rectangular mold 2. At this time, the pressing plate 11 is located above the mold 2, the heating unit of the hot press 1 is started, the mold 2 is heated to 65°C, and a mixture of expanded graphite powder, graphene powder, aluminum powder and gamma iron oxide powder is poured onto the upper surface of the paraffin and flattened, the pressing plate 11 is started and slowly pressed vertically downward to press the mixture powder toward the paraffin. After the pressing is completed, the phase change energy storage material formed by the mixture and the paraffin is no longer fluid, the mold 2 is taken out of the hot press 1, and solidified and formed after cooling at room temperature for one hour. Finally, the solidified material is taken out of the mold 2 and demolded to obtain a shaped phase change energy storage material.

[0045] During batch or assembly line production, the mold 2 needs to be reused. Before each use of the mold 2, it should be ensured that there is no residue or dirt on its surface to reduce adhesion, thereby maintaining the subsequent demolding effect. Due to the characteristics of the paraffin itself, part of the phase change energy storage material may adhere to the inner wall of the mold 2 during demolding. Therefore, the mold 2 after demolding needs to be cleaned; during cleaning, the demolded mold 2 is placed on the transmission component 4, and the mold 2 moves from right to left along the transmission component 4 to below the scraper 5, and then the scraper 5 is started to move downward so that the scraper 5 is inserted into the mold 2. The longitudinal side edge of the L-shaped scraper 5 contacts the longitudinal inner wall of the mold 2, and the bottom edge of the scraper 5 contacts the inner bottom wall of the mold 2. Then, the scraper 5 is started to move. The L-shaped scraper 5 can be set to scrape and clean the inner side wall and the inner bottom wall of the mold 2 at the same time, and the cleaning speed is faster. After cleaning the mold 2, the mold 2 can be sent to the hot press 1 for the molding of the phase change energy storage material.

[0046] like Figure 2-4 As shown, the bracket 3 is provided with a guiding mechanism 6 for guiding the scraper 5, and the guiding mechanism 6 includes: a rotating seat 61 rotatably arranged on the bracket 3; a lifting plate 62 movably inserted into the inside of the rotating seat 61, the lifting plate 62 slides longitudinally inside the rotating seat 61, and the scraper 5 is slidingly arranged at the bottom end of the lifting plate 62; and a first spring 63 arranged on the scraper 5.

[0047] Specifically, the rotating seat 61 can rotate in the horizontal direction, the lifting plate 62 can move up and down relative to the rotating seat 61, and the scraper 5 can move horizontally relative to the lifting seat. Under the push of the first spring 63, the longitudinal side of the scraper 5 is close to the inner wall of the mold 2.

[0048] like Figure 2-4As shown, the guide mechanism 6 also includes: a fixed guide rail 64 fixedly connected to the bracket 3; a movable guide rail 65 slidably arranged on the fixed guide rail 64; a slider 66 slidably arranged on the movable guide rail 65; a movable rod 67 movably inserted into the inside of the rotating seat 61, the movable rod 67 slides horizontally inside the rotating seat 61, and the end of the movable rod 67 is rotatably connected to the slider 66; a second spring 68 arranged on the rotating seat 61 for pushing the movable rod 67 to extend outward.

[0049] Specifically, the swivel seat 61 is arranged at the center of the rectangle formed by the fixed guide rail 64 and the movable guide rail 65. After the swivel seat 61 rotates, the slider 66 is driven to move by the movable rod 67. The slider 66 moves along the fixed guide rail 64 and the movable guide rail 65, and its movement trajectory is rectangular. The movement trajectory of the longitudinal side of the scraper 5 is also rectangular. The movement trajectory of the scraper 5 is designed to match the inner wall size of the mold 2; therefore, it is only necessary to start the rotation of the swivel seat 61 to drive the scraper 5 to rotate, and during the rotation of the scraper 5, its longitudinal side is always in contact with the inner wall of the mold 2, so as to comprehensively scrape and clean the inner wall of the mold 2 without dead corners, and the cleaning effect on the rectangular mold 2 is better and the operation is convenient.

[0050] like Figure 3-6 As shown, it also includes a control mechanism 7, which includes: a push plate 71 slidably arranged on the bracket 3, and the push is used to drive the lifting plate 62 to move up and down; a detection plate 72 slidably arranged on the bracket 3, and the mold 2 passes through the detection plate 72 during the transportation process; a support spring 73 for pushing the detection plate 72 to move upward; and a stroke amplification component 74. After the detection plate 72 moves, the push plate 71 is driven to move through the stroke amplification component 74.

[0051] Specifically, a disc is provided on the top of the lifting plate 62, and a recessed slot is provided on the bottom end of the push plate 71. The disc is inserted into the slot. After the push plate 71 moves up and down, the lifting plate 62 is driven to move up and down through the cooperation between the disc and the slot. The lifting plate 62 can rotate during the movement, thereby driving the scraper 5 to rotate.

[0052] like Figure 1-2 As shown, the transmission assembly 4 includes a first transmission belt 41 and a second transmission belt 42, and the first transmission belt 41 and the second transmission belt 42 are respectively aligned with the detection plate 72 before and after lifting.

[0053] Specifically, the transmission component 4 is located on the right side of the hot press 1, and the first conveyor belt 41 and the second conveyor belt 42 are respectively located on the right and left sides of the detection plate 72. Initially, the support spring 73 pushes the empty detection plate 72 upward. At this time, the first conveyor belt 41 is highly aligned with the detection plate 72, and the mold 2 after demolding is placed on the right end of the first conveyor belt 41. The mold 2 can be directly conveyed to the detection plate 72 along the first conveyor belt 41. The weight of the mold 2 causes the detection plate 72 to move downward. After the detection plate 72 moves downward, it is aligned with the second conveyor belt 42, and the cleaned mold 2 is continued to be conveyed to the left through the second conveyor belt 42, so as to facilitate the cleaned mold 2 to be sent into the hot press 1 on the left.

[0054] like Figure 3-5 As shown, the stroke amplification component 74 includes: a driving gear 741, an adjusting gear 742 and a driven gear 743 rotatably arranged on the bracket 3, the driving gear 741 and the adjusting gear 742 are transmitted through a chain belt, and the adjusting gear 742 is meshed and transmitted with the driven gear 743; a first tooth segment 744 arranged on the detection plate 72, the first tooth segment 744 is meshed and connected with the driving gear 741; a second tooth segment 745 arranged on the push plate 71, the second tooth segment 745 is meshed and connected with the driven gear 743.

[0055] Specifically, the stroke amplification component 74 adopts the amplification principle of gear transmission. After the detection plate 72 moves up and down, the push plate 71 and the lifting plate 62 are driven to move up and down synchronously through the action of the gear structure; after the mold 2 is placed on the detection plate 72, the detection plate 72 is driven to move downward, and this stroke is A. The stroke of the scraper 5 inserted into the interior of the mold 2 is B, and the stroke B is greater than the stroke A; through the amplification effect of the gear structure, after the detection plate 72 moves downward, it can drive the scraper to move a longer distance, so that the bottom edge of the scraper can contact the inner bottom wall of the mold 2, thereby ensuring that the scraping and brushing cleaning work of the mold 2 can be carried out normally.

[0056] like Figure 3-8 As shown, the control mechanism 7 also includes: a clockwork assembly 75 arranged on the detection plate 72, the output shaft 752 of the clockwork assembly 75 is slidably connected with the rotating seat 61, and a gear ring 753 is provided on the output shaft 752 of the clockwork assembly 75: a non-return pawl 76 arranged on the push plate 71, and the non-return pawl 76 is meshingly connected with the gear ring 753; a heat engine 77 arranged on the bracket 3, and the input shaft 751 of the clockwork assembly 75 is inserted into the output end 771 of the heat engine 77.

[0057] Specifically, the clockwork assembly 75 is provided with a structure to prevent over-tightening, and the toothed ring 753 and the non-return pawl 76 form a one-way rotating structure. The clockwork assembly 75 is always connected to the rotating seat 61 as the detection plate 72 moves up and down; the heat engine 77 is preferably, but not limited to, an organic Rankine cycle device or a Stirling engine, and can utilize heat of about 50°. The output end 771 of the heat engine 77 is a rotating structure. After heat is provided to the heat engine 77, the heat engine 77 can be started. Initially, the non-return pawl 76 contacts the toothed ring 753 to prevent the clockwork assembly 75 from rotating and releasing energy. After the heat engine 77 receives the heat and starts, the output end 771 of the heat engine 77 rotates. In the initial state, the input shaft 751 of the clockwork assembly 75 is plugged into the output end 771 of the heat engine 77. After the output end 771 rotates, it drives the input shaft 751 to rotate, thereby tightening the clockwork assembly 75;

[0058] After the mold 2 moves onto the detection plate 72, the detection plate 72 moves downward and drives the clockwork assembly 75, the push plate 71 and the lifting plate 62 to move downward. After the lifting plate 62 moves downward, it drives the scraper 5 to be inserted into the mold 2. After the clockwork assembly 75 moves downward, its input shaft 751 is separated from the output end 771 of the heat engine 77. After the push plate 71 moves downward, the check pawl 76 is also staggered up and down with the gear ring 753. Then, the clockwork assembly 75 can release energy and rotate. The output shaft 752 of the clockwork assembly 75 drives the swivel seat 61 to rotate. The rotating swivel seat 61 drives the scraper 5 to scrape and clean the mold 2. In this way, the function of the scraper 5 automatically moving down to the inside of the mold 2 for scraping and cleaning is realized, and the degree of automation is high.

[0059] like Figure 1-2 As shown, the control mechanism 7 also includes: a heat collection chamber 78 arranged on the outside of the hot press 1, and the heat collection chamber 78 is used to place the mold 2 taken out from the hot press 1; a heat pipe 79, and the heat in the heat collection chamber 78 is transmitted to the heat engine 77 via the heat pipe 79.

[0060] Specifically, after the mold 2 in the hot press 1 completes the pressing, the temperature of the mold 2 is relatively high. The mold 2 is taken out of the hot press 1 and placed in the heat collection chamber 78 for preliminary cooling. The heat emitted by the mold 2 is recovered through the heat collection chamber 78 and transmitted to the heat engine 77. The heat engine 77 then tightens the clockwork assembly 75 to store energy, so that after the demolded mold 2 moves to the detection seat, it can provide power for the scraper 5; after the mold 2 in the heat collection chamber 78 is cooled to a certain temperature, the mold 2 is taken out of the heat collection chamber 78, and the mold 2 is cooled to room temperature under the external environment, and then the demolding work can be carried out; by setting the heat collection chamber 78, during the forming process of the phase change energy storage material, the self-gravity of the mold 2 is used to drive the scraper to move down to the inside of the mold 2, so that the scraper and the mold 2 are automatically matched, and the heat of the mold 2 is recovered to provide power for the rotating scraping work of the scraper, eliminating the need for an additional electrical system for driving the scraper, which is energy-saving and environmentally friendly.

[0061] Embodiment 2

[0062] A method for forming a phase change energy storage material, the method adopts the production and processing forming device of the phase change energy storage material described above, and comprises the following steps:

[0063] Step 1: pour the organic phase change material into the mold 2, and place the mold 2 into the hot press 1 to heat it until the organic phase change material is in liquid state;

[0064] Step 2: Spread the thermal conductive material on the surface of the liquid organic phase change material;

[0065] Step 3: using a pressing plate 11 that matches the size of the mold 2 to extrude the material inside the mold 2, so that the thermal conductive material and the liquid organic phase change material are mixed;

[0066] Step 4: Take the mold 2 out of the hot press 1 and send it into the heat collection chamber 78 for preliminary cooling. At the same time, use the heat engine 77 to recover the heat emitted by the mold 2 in the heat collection chamber 78.

[0067] Step 5: Take the mold 2 out of the heat collection chamber 78, place it in an external environment to cool to room temperature, and then demould to obtain a formed phase change energy storage material;

[0068] Step 6: Use the scraper 5 to scrape and clean the mold 2 after demoulding;

[0069] Step 7: Repeat steps 1 to 6, and reuse the mold 2 to continuously produce the phase change energy storage material.

[0070] In the step 1, the organic phase change material is paraffin, and in the step 2, the thermal conductive material is a mixture of expanded graphite powder, graphene powder, aluminum powder and gamma iron oxide powder.

[0071] Working principle: When producing phase change energy storage materials, put the mold 2 into the hot press 1, and pour paraffin with a melting point of 54°C into the rectangular mold 2. At this time, the pressing plate 11 is located above the mold 2, and the heating unit of the hot press 1 is started to heat the mold 2 to 65°C. Pour a mixture of expanded graphite powder, graphene powder, aluminum powder and gamma iron oxide powder onto the upper surface of the paraffin and flatten it. Start the pressing plate 11 to slowly press down vertically to press the mixed powder toward the paraffin. After the pressing is completed, the phase change energy storage material formed by the mixture and the paraffin has no fluidity. Take the mold 2 out of the hot press 1 and place it in the heat collection chamber 78 for preliminary cooling. The heat emitted by the mold 2 is recovered through the heat collection chamber 78 and transmitted to the heat engine 77. After the heat engine 77 receives the heat and starts, the output end 771 of the heat engine 77 rotates to tighten the clockwork assembly 75.

[0072] After the mold 2 in the heat collection chamber 78 is cooled to a certain temperature, the mold 2 is taken out from the heat collection chamber 78, and the mold 2 is cooled to room temperature under the external environment. After cooling at room temperature for one hour, the mold is solidified and formed. Finally, the solidified material is taken out from the mold 2, and the mold is demolded to obtain a fixed phase change energy storage material.

[0073] The demoulded mold 2 is placed at the right end of the first conveyor belt 41. The mold 2 can be directly transferred to the detection plate 72 along the first conveyor belt 41. The weight of the mold 2 causes the detection plate 72 to move downward. After the detection plate 72 moves downward, the clockwork assembly 75, the push plate 71 and the lifting plate 62 are driven to move downward.

[0074] After the lifting plate 62 moves downward, it drives the scraper 5 to be inserted into the mold 2, the longitudinal side of the scraper 5 contacts the inner side wall of the mold 2, and the bottom edge of the scraper 5 contacts the inner bottom wall of the mold 2;

[0075] After the clockwork assembly 75 moves downward, its input shaft 751 is separated from the output end 771 of the heat engine 77;

[0076] After the push plate 71 moves downward, the non-return pawl 76 is also staggered with the toothed ring 753, and then the clockwork assembly 75 can release energy and rotate, and the output shaft 752 of the clockwork assembly 75 drives the rotating seat 61 to rotate, and the rotating rotating seat 61 drives the scraper 5 to scrape and clean the mold 2;

[0077] After the inspection plate 72 moves downward, it is aligned with the second conveyor belt 42, and the cleaned mold 2 is further conveyed to the left by the second conveyor belt 42, so that the cleaned mold 2 can be sent to the hot press 1 on the left side to work again;

[0078] After the cleaned mold 2 is removed from the detection plate 72, the detection plate 72 moves upward and resets, and drives the clockwork assembly 75, the push plate 71 and the lifting plate 62 to move upward and reset, so as to clean the next mold 2 after demoulding.

[0079] The above shows and describes the basic principles, main features and advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A production and processing device for phase change energy storage materials, characterized in that: The invention comprises a hot press (1) and a mold (2), wherein the mold (2) is in a rectangular shape with an open top, a pressing plate (11) is movably provided inside the hot press (1), and the pressing plate (11) is used to extrude and mold materials placed inside the mold (2), and a vent hole (12) is provided on the pressing plate (11). The hot press (1) is provided with a heating unit for heating the mold (2), and further comprises: A support (3) arranged outside the hot press (1); A transmission component (4) for transporting the mold (2); a scraper (5) movably mounted on the bracket (3), the scraper (5) being in an L shape; The support (3) is provided with a guide mechanism (6) for guiding the scraper (5), and the guide mechanism (6) comprises: Rotating a rotating seat (61) disposed on the support (3); A lifting plate (62) movably inserted into the rotating seat (61), the lifting plate (62) slides longitudinally inside the rotating seat (61), and the scraper (5) is slidably arranged at the bottom end of the lifting plate (62); A first spring (63) provided on the scraper (5); The guiding mechanism (6) further comprises: A fixed guide rail (64) fixedly connected to the bracket (3); A movable guide rail (65) slidably arranged on the fixed guide rail (64); A slider (66) slidably disposed on the movable guide rail (65); A movable rod (67) movably inserted into the rotating seat (61), the movable rod (67) slides transversely inside the rotating seat (61), and the end of the movable rod (67) is rotatably connected to the slider (66); A second spring (68) is provided on the rotating seat (61) and is used to push the movable rod (67) to extend outward.

2. The production and processing device for phase change energy storage material according to claim 1, characterized in that: It also includes a control mechanism (7), wherein the control mechanism (7) includes: A push plate (71) slidably disposed on the bracket (3), the push plate being used to drive the lifting plate (62) to move up and down; a detection plate (72) slidably arranged on the support (3), wherein the mold (2) passes through the detection plate (72) during transportation; A support spring (73) for pushing the detection plate (72) upward; A stroke amplifying component (74), wherein after the detection plate (72) moves, the push plate (71) is driven to move via the stroke amplifying component (74).

3. The production and processing device for phase change energy storage material according to claim 2, characterized in that: The transmission assembly (4) comprises a first transmission belt (41) and a second transmission belt (42), wherein the first transmission belt (41) and the second transmission belt (42) are respectively aligned with the detection plate (72) before and after lifting.

4. The production and processing device for phase change energy storage material according to claim 3, characterized in that: The stroke amplification component (74) comprises: Rotating a driving gear (741), an adjusting gear (742), and a driven gear (743) provided on the bracket (3), wherein the driving gear (741) and the adjusting gear (742) are transmitted via a chain belt, and the adjusting gear (742) and the driven gear (743) are meshed for transmission; A first tooth segment (744) provided on the detection plate (72), the first tooth segment (744) being meshingly connected with the driving gear (741); A second tooth segment (745) is provided on the push plate (71), and the second tooth segment (745) is meshingly connected with the driven gear (743).

5. The production and processing device for phase change energy storage material according to claim 4, characterized in that: The control mechanism (7) further comprises: A clockwork assembly (75) is disposed on the detection plate (72), wherein an output shaft (752) of the clockwork assembly (75) is slidably connected to the rotating seat (61), and a gear ring (753) is disposed on the output shaft (752) of the clockwork assembly (75): a non-return pawl (76) provided on the push plate (71), the non-return pawl (76) being meshingly connected with the toothed ring (753); A heat engine (77) is arranged on the bracket (3), and the input shaft (751) of the clockwork assembly (75) is plugged into the output end (771) of the heat engine (77).

6. The production and processing device for phase change energy storage material according to claim 5, characterized in that: The control mechanism (7) further comprises: a heat collection chamber (78) disposed outside the hot press (1), the heat collection chamber (78) being used to place the mold (2) taken out of the hot press (1); A heat conducting pipe (79), wherein the heat in the heat collecting chamber (78) is transferred to the heat engine (77) via the heat conducting pipe (79).

7. A method for forming a phase change energy storage material, the method using the production and processing forming device of a phase change energy storage material according to claim 6, characterized in that: The following steps are involved: Step 1: pouring the organic phase change material into a mold (2), placing the mold (2) into a hot press (1) for heating until the organic phase change material is in a liquid state; Step 2: Spread the thermal conductive material on the surface of the liquid organic phase change material; Step 3: using a pressing plate (11) having a size matching that of the mold (2) to extrude the material inside the mold (2) so that the thermal conductive material and the liquid organic phase change material are mixed; Step 4: taking the mold (2) out of the hot press (1) and sending it into a heat collecting chamber (78) for preliminary cooling; at the same time, using a heat engine (77) to recover the heat emitted by the mold (2) in the heat collecting chamber (78); Step 5: taking the mold (2) out of the heat collection chamber (78), placing it in an external environment to cool to room temperature, and demoulding to obtain a molded phase change energy storage material; Step 6: Use a scraper (5) to scrape and clean the mold (2) after demoulding; Step 7: Repeat steps 1 to 6, and reuse the mold (2) to continuously produce the phase change energy storage material.

8. A phase change energy storage material molding method according to claim 7, characterized in that: In the step 1, the organic phase change material is paraffin, and in the step 2, the thermal conductive material is a mixture of expanded graphite powder, graphene powder, aluminum powder and gamma iron oxide powder.

Citation Information

Cited By

  • Production, processing and forming device for phase-change energy storage material and material forming method of phase-change energy storage material

    CN120080480A