Deposition equipment and method for controlling thickness uniformity of wafer deposited film
By dynamically adjusting the wafer bearing angle and the reaction gas flow ratio of the deposition equipment, the problem of film thickness non-uniformity during the wafer deposition process is solved, and high-quality and uniform deposition of the film is achieved, which is suitable for complex semiconductor device manufacturing.
Patent Information
- Application Number
- CN202410917090.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-10
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2044-07-10
AI Technical Summary
During the wafer deposition process, it is difficult to effectively control the deposition thickness consistency of wafer films due to non-uniform film thickness problems caused by gas flow, temperature gradients or differences in reactant arrival paths.
A deposition equipment including an equipment rack, a limit bar, a deposition seat, a gas guide seat and a wafer positioning component was designed. By dynamically adjusting the wafer carrying angle and the reaction gas flow ratio, the film thickness and refraction were analyzed using a spectral reflection module. rate, achieving multi-stage control of thin film deposition.
It effectively reduces edge effects and center accumulation, improves the overall film quality, ensures that the film on the surface and inside of the wafer is uniform, and meets the manufacturing requirements of complex semiconductor devices.
Smart Images

Figure CN118460990B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of wafer manufacturing equipment, and in particular relates to a deposition device and a method for controlling the uniformity of the thickness of a wafer deposited film. Background Art
[0002] In wafer production, wafer thin film uniformity is a key indicator in the vapor deposition process, and generally requires that the thickness of each area of the thin film be consistent; and the uniformity of the thin film is mainly affected by the thin film deposition process and equipment, including factors such as gas flow, process temperature, gas spray uniformity, plasma concentration distribution, etc., all of which will affect the final formation of the film quality; in the prior art, the wafer deposition process adopts the method of wafer rotation and revolution to improve the uniformity of thin film deposition, however, in the horizontal deposition process of the wafer, it is very easy to obtain different deposition effects in the wafer area near the edge or the middle due to differences in gas flow, temperature gradient or the path of the reaction material reaching the wafer surface, resulting in uneven wafer film thickness; therefore, it is necessary to provide a deposition device and method for controlling the uniformity of wafer deposited film thickness to solve the problems raised in the above background technology. Summary of the invention
[0003] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a deposition device for controlling the uniformity of the thickness of a thin film deposited on a wafer, comprising: an equipment frame and a limiting bar, a deposition seat is horizontally fixed inside the equipment frame, a plurality of wafer loading spaces are distributed circumferentially inside the deposition seat, and is used to synchronously carry a plurality of wafers; the limiting bar is vertically fixed to one side of the equipment frame, a gas guide seat is arranged above the deposition seat in the equipment frame, the gas guide seat is slidably mounted on the limiting bar, and is sealed and assembled with the deposition seat to form a gas reaction chamber; a gas supply pipe is vertically connected to the middle part of the lower part of the deposition seat, and is used to transport reaction gas, one end of the gas supply pipe is connected to the gas reaction chamber, and a gas exhaust pipe is arranged on one side of the deposition seat, and a vacuum pump is vertically connected to the gas exhaust pipe through a tee;
[0004] A wafer positioning assembly is provided at each wafer loading position in the deposition seat, and the wafer positioning assembly provides horizontal or inclined multi-angle loading for the wafer in different stages of the wafer deposition process;
[0005] A spectral reflection module is provided in the deposition seat. The spectral reflection module calculates the thickness and refractive index of the thin film deposited on the wafer at different preset angles through the reflectivity of light of different wavelengths on the surface of the thin film in combination with a thin film theoretical model, and analyzes the thin film uniformity characteristic data corresponding to the deposition at each angle; a control unit is provided on the equipment rack. The control unit dynamically adjusts the wafer bearing angle in combination with the thin film uniformity characteristic data corresponding to the deposition at each angle in different stages of the wafer deposition process, so that the wafer is always at the optimal angle for thin film deposition.
[0006] Further, preferably, the wafer positioning assembly comprises:
[0007] The carriers are multiple and distributed in a circle, a carrier plate is arranged at the center of the deposition seat, and the carriers are embedded and fixed on the carrier plate;
[0008] A rotating shaft seat is rotatably connected in the carrier, the rotating shaft seat is in a hemispherical structure, and a gear groove is provided on its lower surface, a driving tooth is installed in the carrier, and the driving tooth meshes with the gear groove;
[0009] A negative pressure plate is coaxially mounted on the rotating shaft seat, and a plurality of air holes are formed on the negative pressure plate;
[0010] The built-in motor is installed in the rotating shaft seat, the negative pressure plate is rotatably connected to the rotating shaft seat, and the output end of the built-in motor is fixed to the negative pressure plate.
[0011] Further, as a preference, a main shaft is vertically rotatably connected in the deposition seat, the upper end of the main shaft is fixed to the carrier plate, and a driving part is installed in the deposition seat, and the driving part is connected to the main shaft for transmission through gear meshing;
[0012] An air guide tube is fixed cocentrically within the main shaft, and the upper end of the air supply tube is sealed and rotatably connected to the air guide tube;
[0013] An air guide ring is fixed on the outer circumference of the carrier in the deposition seat, a plurality of guide holes are opened on the air guide ring, and an air cavity is arranged below the air guide ring in the deposition seat, and the air exhaust pipe is horizontally connected to one side of the air cavity.
[0014] Further, preferably, a flow cavity is provided inside the carrier, and a plurality of rows of holes are distributed on the inner wall of the carrier, the rows of holes are connected to the flow cavity, connecting tubes are arranged in the deposition seat, one end of the connecting tubes is connected to the flow cavity, and the other end of each connecting tube is connected to the gas exhaust pipe through a collecting seat, and a bronchus is provided on the side of the collecting seat away from the connecting tube.
[0015] Further, as a preference, an airtight seat is transversely fixed on the deposition seat, the airtight seat is connected with the gas exhaust pipe, a direct current cavity is centrally arranged in the airtight seat, a through hole connected with the airtight seat is provided on the side wall of the direct current cavity, a direct current tube is slidably connected in the direct current cavity, one end of the direct current tube is slidably connected with the bronchial tube on the current collecting seat, an isolation ring is fixed in the direct current cavity, a cut-off ring is sleeved on the direct current tube, and the cut-off ring is in sliding contact with the isolation ring;
[0016] A blocking shaft is fixed in the direct current cavity, one end of the blocking shaft penetrates into the direct current tube, the interior of the direct current tube is set as a variable diameter hole, and the blocking shaft can be slidably and sealingly matched with the variable diameter hole in the direct current tube;
[0017] The airtight seat is provided with a flow hole connected with the air cavity.
[0018] Further, preferably, the diameter of the guide hole on the air guide ring close to the air exhaust pipe is smaller than the diameter of the guide hole far from the air exhaust pipe.
[0019] Further, as a preference, a cooler is provided above the interior of the air guide seat, a heat conduction plate is fixed below the cooler, and an air flow plate is suspended in the air guide seat, and spray holes are circumferentially distributed at different diameter length positions on the air flow plate;
[0020] A rotating tube is vertically penetrated through the middle of the airflow plate, and the lower end of the rotating tube is detachably and sealingly connected to the air guide tube in the deposition seat.
[0021] Further, as a preference, the airflow plate is rotatably mounted in an air guide seat, and a control motor for driving the airflow plate to rotate is mounted on the air guide seat;
[0022] A plurality of adjustment rings of different diameter lengths are rotatably connected to the airflow plate, each of the adjustment rings is provided with a transfer hole corresponding to the spray hole, and the adjustment rings are independently deflected and adjusted so that the spray holes at different diameter lengths are connected or staggered with the transfer holes.
[0023] Further, as a preference, a deposition method for controlling the uniformity of the thickness of a thin film deposited on a wafer comprises the following steps:
[0024] S1. Wafer placement: multiple wafers are placed on the wafer loading space of the deposition seat by a vacuum fixture. At this time, the wafers can be fixed by negative pressure adsorption through the air holes on the negative pressure plate. Then, the air guide seat and the deposition seat are sealed and assembled, and the inside is vacuumed by a vacuum pump;
[0025] S2. In the initial deposition stage of the wafer, the wafer on the wafer positioning assembly is placed horizontally, the carrier in the deposition seat rotates continuously, and the negative pressure plate can be driven to rotate by the built-in motor, so that the wafer can rotate while revolving. At this time, the gas delivery pipe carries out the initial stage of reaction gas delivery and adjusts the flow rate of the reaction gas. After being controlled by the temperature of the heat conduction plate, the reaction gas passes downward through the nozzles of the air flow plate to achieve initial thin film deposition;
[0026] S3. Multi-stage deposition: To increase the deposition rate and ensure deposition thickness and uniformity, the wafer positioning assembly gradually changes the wafer carrying angle to form multiple different stages of wafer deposition. In each stage, the wafer can still revolve in the carrier, and the negative pressure plate controls the wafer rotation. At this time, the reaction gas can be sprayed to the wafer from the nozzles at different diameter positions, so that a more uniform and controllable film thickness is formed on the wafer surface.
[0027] S4. Control of gas flow direction. In each stage, after the reaction gas flows through the wafer surface, a part of it can enter the gas cavity through the guide hole on the gas guide ring, and enter the gas exhaust pipe through the gas-tight seat, while the other part of the reaction gas can enter the flow cavity through the discharge hole on the inner wall of the carrier, and then enter the direct current pipe through the current collecting seat, and finally flow into the gas exhaust pipe; thereby controlling and adjusting the flow ratio of the reaction gas in the two flow paths, so as to realize the control of the flow rate of the reaction gas on the wafer surface and effectively adjust the film deposition speed;
[0028] S5. At the end of deposition, the wafer is placed horizontally, and step S2 is repeated while adjusting the parameters of wafer rotation speed, reaction gas flow rate and temperature so that a deposited film with uniform properties is formed on the wafer surface.
[0029] Compared with the prior art, the present invention has the following beneficial effects:
[0030] In the present invention, wafer thin film deposition is divided into multiple stages of deposition. The initial stage is horizontal deposition, so that a relatively uniform thin film can be quickly formed on the wafer surface to establish a basic thin film layer. In the subsequent stages, the wafer bearing angle is gradually changed by a wafer positioning component, thereby effectively reducing edge effects and center accumulation and improving the overall film quality. The two flow paths located in the deposition seat can respectively discharge the reaction gas, so that the flow ratio of the reaction gas in the two flow paths can be controlled and adjusted to achieve the control of the flow rate of the reaction gas on the wafer surface, effectively adjust the film deposition speed and the reaction gas flow direction, and more accurately control the film characteristics to meet the manufacturing requirements of diversified and complex semiconductor devices. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figure 1 It is a structural schematic diagram of the present invention;
[0032] Figure 2 It is a structural schematic diagram of the carrier plate in the present invention;
[0033] Figure 3 It is a schematic diagram of the structure of the deposition base and the wafer positioning assembly in the present invention;
[0034] Figure 4 It is a structural schematic diagram of the tilt-adjustable lower rotating shaft seat in the present invention;
[0035] Figure 5 for Figure 4 The enlarged schematic diagram at A in the middle;
[0036] Figure 6 It is a structural schematic diagram of the air guide seat in the present invention;
[0037] Figure 7 It is a schematic diagram of the structure of the adjustment ring and the airflow plate in the present invention;
[0038] In the figure: 1. Equipment rack; 11. Air exhaust pipe; 12. Air supply pipe; 13. Vacuum pump; 2. Air guide seat; 21. Cooler; 22. Heat conduction plate; 23. Air flow plate; 24. Rotating pipe; 25. Adjusting ring; 26. Nozzle; 27. Adapter hole; 3. Deposition seat; 31. Carrier; 32. Spindle; 33. Driving unit; 34. Air guide ring; 35. Guide hole; 36. Air cavity; 4. Wafer positioning assembly; 41. Carrier; 42. Rotating shaft seat; 43. Driving gear; 44. Negative pressure plate; 45. Flow cavity; 46. Exhaust hole; 47. Connecting pipe; 5. Airtight seat; 51. DC cavity; 52. Through hole; 53. DC pipe; 54. Isolation ring; 55. Blocking shaft. DETAILED DESCRIPTION
[0039] See also Figure 1-Figure 7 In an embodiment of the present invention, a deposition device for controlling the uniformity of the thickness of a thin film deposited on a wafer comprises: an equipment frame 1 and a limiting bar, wherein a deposition seat 3 is horizontally fixed inside the equipment frame 1, and a plurality of wafer loading spaces are distributed on the circumference of the deposition seat 3 for synchronously carrying a plurality of wafers; the limiting bar is vertically fixed to one side of the equipment frame 1, and a gas guide seat 2 is arranged above the deposition seat 3 in the equipment frame 1, and the gas guide seat 2 is slidably mounted on the limiting bar and is sealed and assembled with the deposition seat 3 to form a gas reaction chamber; a gas supply pipe 12 is vertically connected to the middle part of the lower part of the deposition seat 3 for conveying reaction gas, one end of the gas supply pipe 12 is connected to the gas reaction chamber, and a gas exhaust pipe 11 is arranged on one side of the deposition seat 3, and a vacuum pump 13 is vertically connected to the gas exhaust pipe 11 through a tee; the vacuum pump is used to vacuum the inside of the gas reaction chamber;
[0040] A wafer positioning assembly 4 is provided at each wafer loading position in the deposition seat 3, and the wafer positioning assembly 4 provides horizontal or inclined multi-angle loading for the wafer in different stages of the wafer deposition process;
[0041] A spectral reflection module is provided in the deposition seat 3. The spectral reflection module calculates the thickness and refractive index of the thin film deposited on the wafer at different preset angles through the reflectivity of light of different wavelengths on the film surface and in combination with the thin film theoretical model, and analyzes the thin film uniformity characteristic data corresponding to each angle of deposition; a control unit is provided on the equipment frame 1. The control unit dynamically adjusts the wafer carrying angle in different stages of the wafer deposition process in combination with the thin film uniformity characteristic data corresponding to each angle of deposition, so that the wafer is always deposited at the optimal angle for thin film deposition, that is, the wafer deposition process is divided into multiple deposition stages, and the wafer can be deposited at the optimal loading angle in each deposition stage, so as to more accurately control the growth conditions of the thin film, such as deposition rate, thickness uniformity, step coverage, etc., so as to achieve better film quality at the microscopic level, thereby reducing edge effects and center accumulation phenomena, and ensuring that the film is uniform and consistent on the entire wafer surface and even inside the three-dimensional structure.
[0042] In this embodiment, the wafer positioning component 4 includes:
[0043] The carriers 41 are multiple and distributed in a circle. A carrier plate 31 is disposed at the center of the deposition seat 3. The carriers 41 are embedded and fixed on the carrier plate 31.
[0044] A rotating shaft seat 42 is rotatably connected in the carrier 41. The rotating shaft seat 42 is in a hemispherical structure, and a gear groove is provided on its lower surface. A driving tooth 43 is installed in the carrier 41, and the driving tooth 43 is meshed with the gear groove; thereby, the rotating shaft seat is driven to deflect through the driving tooth, so as to adjust the wafer carrying angle;
[0045] A negative pressure plate 44 is coaxially mounted on the rotating shaft seat 42, and a plurality of air holes are formed on the negative pressure plate 44; the negative pressure plate can fix the wafer by negative pressure adsorption through the air holes;
[0046] The built-in motor is installed in the rotating shaft seat 42, the negative pressure plate 44 is rotatably connected to the rotating shaft seat 42, and the output end of the built-in motor is fixed to the negative pressure plate 44, so that the negative pressure plate is driven to rotate by the built-in motor to realize self-rotation during wafer deposition.
[0047] As a preferred embodiment, a main shaft 32 is vertically rotatably connected in the deposition seat 3, the upper end of the main shaft 32 is fixed to the carrier 31, and a driving part 33 is installed in the deposition seat 3, and the driving part 33 is connected to the main shaft 32 through gear meshing for transmission; thus, the revolution of the wafer during deposition is realized by the rotation of the main shaft (that is, the center of the carrier is the rotation center);
[0048] An air guide tube is fixed cocentrically within the main shaft 32, and the upper end of the air supply tube 12 is sealed and rotatably connected to the air guide tube;
[0049] An air guide ring 34 is fixed on the outer circumference of the carrier plate 31 in the deposition seat 3, and a plurality of guide holes 35 are opened on the air guide ring 34. An air cavity 36 is provided below the air guide ring 34 in the deposition seat 3, and the gas exhaust pipe 11 is horizontally connected to one side of the gas cavity 36. That is to say, the reaction gas entering the gas reaction chamber can enter the gas cavity through the guide holes on the air guide ring so as to be discharged from the gas exhaust pipe, thereby realizing the internal flow of the reaction gas.
[0050] In this embodiment, a flow cavity 45 is provided inside the carrier 41, and a plurality of row holes 46 are distributed on the inner wall of the carrier 41, and the row holes 46 are connected to the flow cavity 45. A connecting tube 47 is arranged in the deposition seat 3, and one end of the connecting tube 47 is connected to the flow cavity 45, and the other end of each connecting tube 47 is connected to the gas exhaust pipe 11 through a collector seat. A bronchus is provided on the side of the collector away from the connecting tube 47. When the wafer positioning assembly controls the wafer to be loaded at an angle, a part of the reaction gas can enter the flow cavity through the row holes, and finally flow into the gas exhaust pipe for discharge, thereby realizing sufficient flow of the reaction gas along the surface of the wafer. At this time, the continuous rotation of the wafer can improve the deposition efficiency and ensure the deposition uniformity.
[0051] In this embodiment, an airtight seat 5 is transversely fixed on the deposition seat 3, and the airtight seat 5 is connected to the gas exhaust pipe 11. A direct current cavity 51 is arranged at the center of the airtight seat 5. A through hole 52 connected to the airtight seat 5 is opened on the side wall of the direct current cavity 51. A direct current tube 53 is slidably connected in the direct current cavity 51. One end of the direct current tube 53 is slidably connected to the bronchus on the collecting seat. An isolation ring 54 is fixed in the direct current cavity 51. A cut-off ring is sleeved on the direct current tube 53. The cut-off ring is in sliding contact with the isolation ring 54.
[0052] A blocking shaft 55 is fixed in the DC cavity 51, and one end of the blocking shaft 55 extends into the DC tube 53. The interior of the DC tube 53 is set as a variable diameter hole, and the blocking shaft 55 can slide and seal with the variable diameter hole in the DC tube 53; that is, by adjusting the sliding of the DC tube (which can be electrically controlled or driven by a telescopic rod, which belongs to the prior art and will not be repeated here), the flow ratio of the reaction gas in the air cavity and the collector is controlled, so that the flow rate of the reaction gas on the wafer surface is accurately controlled, and the deposition rate can be effectively controlled.
[0053] The airtight seat 5 is provided with a flow hole connected to the air cavity 36 .
[0054] In this embodiment, the diameter of the guide hole 35 on the gas guide ring 34 close to the gas exhaust pipe 11 is smaller than the diameter of the guide hole 35 far from the gas exhaust pipe 11, thereby improving the flow uniformity of the reaction gas in the deposition seat.
[0055] As a preferred embodiment, a cooler 21 is provided on the upper part of the air guide seat 2, a heat conduction plate 22 is fixed below the cooler 21, and an air flow plate 23 is suspended in the air guide seat 2, and spray holes 26 are distributed circumferentially at different diameter length positions on the air flow plate 23;
[0056] A rotating tube 24 is vertically penetrated through the middle of the airflow plate 23 , and the lower end of the rotating tube 24 is detachably and sealingly connected to the air guide tube in the deposition seat 3 .
[0057] In this embodiment, the air flow plate 23 is rotatably mounted in the air guide seat 2, and a control motor for driving the air flow plate 23 to rotate is mounted on the air guide seat 2, so that the air flow plate can rotate to guide air;
[0058] A plurality of adjustment rings 25 with different diameter lengths are rotatably connected to the airflow plate 23, and each of the adjustment rings 25 is provided with a transfer hole 28 corresponding to the nozzle hole 26. The adjustment rings 25 are independently deflected and adjusted so that the nozzle holes 26 at different diameter length positions are connected or staggered with the transfer holes 28. In particular, when the wafer is loaded at an angle, the reaction gas is vertically sprayed through the nozzle holes at different spatial positions, which can effectively and accurately control the film properties.
[0059] In this embodiment, a deposition method for controlling the uniformity of the thickness of a thin film deposited on a wafer comprises the following steps:
[0060] S1. Wafer placement: multiple wafers are placed on the wafer loading space of the deposition seat 3 by a vacuum fixture. At this time, the wafers can be fixed by negative pressure adsorption through the air holes on the negative pressure plate 44; then the air guide seat 2 and the deposition seat 3 are sealed and assembled to create a dust-free and controllable environment. The vacuum pump 13 evacuates the inside of the deposition chamber to form a highly clean and vacuum environment, removes the air and other impurity gases in the deposition chamber, and creates the necessary low-oxygen and low-impurity environment for subsequent chemical reactions or material deposition;
[0061] S2. In the initial deposition stage of the wafer, the wafer on the wafer positioning assembly 4 is placed horizontally, the carrier plate 31 in the deposition seat 3 rotates continuously, and the negative pressure plate 44 can be driven to rotate by the built-in motor, so that the wafer can rotate while orbiting. At this time, the gas supply pipe 12 carries out the initial stage of reaction gas delivery and adjusts the flow rate of the reaction gas. After the temperature is controlled by the heat conduction plate 22, the reaction gas passes downward through the nozzles 26 of the air flow plate 23 to achieve initial thin film deposition; placing the wafer horizontally is conducive to the uniform distribution of gas on the wafer surface, so as to obtain a more uniform film thickness during the thin film deposition process, that is, on the horizontal plane, the gas flow is more likely to form a uniform laminar flow, reduce eddy currents and dead zones, and ensure that the quality of the deposits received by each wafer area is consistent;
[0062] S3. Multi-stage deposition. To increase the deposition rate and ensure the deposition thickness and uniformity, the wafer positioning component 4 is used to gradually change the wafer carrying angle to form multiple different stages of wafer deposition. In each stage, the wafer can still revolve in the carrier 31, and the negative pressure plate 44 controls the wafer rotation. At this time, the reaction gas can be sprayed to the wafer from the nozzles 26 at different diameter positions, so that a more uniform and controllable film thickness is formed on the wafer surface. By adjusting the angle of the wafer, the reaction gas can act on the wafer surface from different angles and distances, which can more effectively fill the microscopic depressions on the wafer surface and eliminate the shadow effect, thereby obtaining a more uniform film thickness. By adjusting the angle and distance of the gas spray according to the requirements of different deposition stages, the growth dynamics of the film can be finely controlled to optimize the deposition rate while maintaining or improving the crystal quality of the film.
[0063] S4. Control of gas flow direction. In each stage, after the reaction gas flows through the wafer surface, a part of the reaction gas can enter the gas cavity 36 through the guide hole 35 on the gas guide ring 34, and enter the gas exhaust pipe 11 through the airtight seat 5, while another part of the reaction gas can enter the flow cavity 45 through the discharge hole 46 on the inner wall of the carrier 41, and then enter the direct current pipe 53 through the current collector, and finally flow into the gas exhaust pipe 11; thereby, the flow ratio of the reaction gas in the two flow paths is controlled and adjusted, so as to realize the control of the flow rate of the reaction gas on the wafer surface and effectively adjust the film deposition speed;
[0064] S5. At the end of deposition, the wafer is placed horizontally, and step S2 is repeated while adjusting the parameters of wafer rotation speed, reaction gas flow rate and temperature so that a deposited film with uniform properties is formed on the wafer surface.
[0065] What is described above is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A deposition device for controlling the uniformity of the thickness of a thin film deposited on a wafer, characterized in that: It includes: An equipment frame (1) and a limit bar, wherein a deposition seat (3) is horizontally fixed inside the equipment frame (1), and a plurality of wafer loading spaces are distributed on the inner circumference of the deposition seat (3) for synchronously carrying a plurality of wafers; the limit bar is vertically fixed to one side of the equipment frame (1), and a gas guide seat (2) is arranged above the deposition seat (3) in the equipment frame (1), and the gas guide seat (2) is slidably mounted on the limit bar and is sealed and assembled with the deposition seat (3) to form a gas reaction chamber; a gas supply pipe (12) is vertically connected to the middle of the lower part of the deposition seat (3) for conveying reaction gas, and one end of the gas supply pipe (12) is connected to the gas reaction chamber, and a gas exhaust pipe (11) is arranged on one side of the deposition seat (3), and a vacuum pump (13) is vertically connected to the gas exhaust pipe (11) through a three-way connection; A wafer positioning assembly (4) is provided at each wafer loading position in the deposition seat (3), and the wafer positioning assembly (4) provides horizontal or inclined multi-angle loading for the wafer in different stages of the wafer deposition process; The deposition seat (3) is provided with a spectral reflection module, which calculates the thickness and refractive index of the thin film deposited on the wafer at different preset angles by using the reflectivity of light of different wavelengths on the thin film surface in combination with a thin film theoretical model, and analyzes the thin film uniformity characteristic data corresponding to the deposition at each angle; the equipment frame (1) is provided with a control unit, which dynamically adjusts the wafer bearing angle in combination with the thin film uniformity characteristic data corresponding to the deposition at each angle in different stages of the wafer deposition process, so that the wafer is always at the optimal angle for thin film deposition; The wafer positioning component (4) comprises: The carriers (41) are multiple and distributed in a circle, a carrier plate (31) is arranged at the center of the deposition seat (3), and the carriers (41) are embedded and fixed on the carrier plate (31); A rotating shaft seat (42) is rotatably connected in the carrier (41); the rotating shaft seat (42) is in a hemispherical structure and has a gear groove on its lower surface; a driving tooth (43) is installed in the carrier (41), and the driving tooth (43) meshes with the gear groove; A negative pressure plate (44) is coaxially mounted on the rotating shaft seat (42), and a plurality of air holes are formed on the negative pressure plate (44); A built-in motor is installed in the rotating shaft seat (42), the negative pressure plate (44) is rotationally connected to the rotating shaft seat (42), and the output end of the built-in motor is fixed to the negative pressure plate (44); A main shaft (32) is vertically rotatably connected in the deposition seat (3), the upper end of the main shaft (32) is fixed to the carrier plate (31), and a driving part (33) is installed in the deposition seat (3), and the driving part (33) is connected to the main shaft (32) for transmission through gear meshing; An air guide tube is fixed coaxially within the main shaft (32), and the upper end of the air supply tube (12) is sealed and rotatably connected to the air guide tube; An air guide ring (34) is fixedly provided on the outer circumference of the carrier plate (31) in the deposition seat (3), a plurality of guide holes (35) are provided on the air guide ring (34), and an air cavity (36) is provided below the air guide ring (34) in the deposition seat (3), and the air exhaust pipe (11) is horizontally connected to one side of the air cavity (36).
2. The deposition device for controlling the uniformity of the thickness of a thin film deposited on a wafer according to claim 1, characterized in that: A flow cavity (45) is provided inside the carrier (41), and a plurality of rows of holes (46) are distributed on the inner wall of the carrier (41), the rows of holes (46) being connected to the flow cavity (45), a connecting tube (47) is arranged inside the deposition seat (3), one end of the connecting tube (47) is connected to the flow cavity (45), and the other end of each connecting tube (47) is connected to the gas exhaust pipe (11) through a current collecting seat, and a bronchus is provided on a side of the current collecting seat away from the connecting tube (47).
3. The deposition device for controlling the uniformity of the thickness of a thin film deposited on a wafer according to claim 2, characterized in that: An airtight seat (5) is transversely fixed on the deposition seat (3), the airtight seat (5) is connected to the gas exhaust pipe (11), a direct current cavity (51) is arranged at the center of the airtight seat (5), a through hole (52) connected to the airtight seat (5) is opened on the side wall of the direct current cavity (51), a direct current tube (53) is slidably connected in the direct current cavity (51), one end of the direct current tube (53) is slidably connected to the bronchial tube on the current collecting seat, an isolation ring (54) is fixed in the direct current cavity (51), a cut-off ring is sleeved on the direct current tube (53), and the cut-off ring is in sliding contact with the isolation ring (54); A blocking shaft (55) is fixed in the direct current cavity (51), one end of the blocking shaft (55) is inserted into the direct current tube (53), the interior of the direct current tube (53) is provided with a variable diameter hole, and the blocking shaft (55) can be slidably and sealingly matched with the variable diameter hole in the direct current tube (53); The airtight seat (5) is provided with a flow hole connected to the air cavity (36).
4. The deposition device for controlling the uniformity of the thickness of a thin film deposited on a wafer according to claim 2, characterized in that: The diameter of the guide hole (35) on the air guide ring (34) close to the air exhaust pipe (11) is smaller than the diameter of the guide hole (35) far from the air exhaust pipe (11).
5. The deposition device for controlling the uniformity of the thickness of a thin film deposited on a wafer according to claim 3, characterized in that: A cooler (21) is provided above the interior of the air guide seat (2), a heat conduction plate (22) is fixed below the cooler (21), and an air flow plate (23) is suspended in the air guide seat (2), and spray holes (26) are distributed circumferentially at positions of different diameter lengths on the air flow plate (23); A rotating tube (24) is vertically penetrated through the middle of the airflow plate (23), and the lower end of the rotating tube (24) is detachably and sealingly connected to the air guide tube in the deposition seat (3).
6. The deposition device for controlling the uniformity of the thickness of a thin film deposited on a wafer according to claim 5, characterized in that: The airflow plate (23) is rotatably mounted in the air guide seat (2), and a control motor for driving the airflow plate (23) to rotate is mounted on the air guide seat (2); A plurality of adjustment rings (25) of different diameter lengths are rotatably connected to the airflow plate (23), each of the adjustment rings (25) being provided with a transfer hole (27) corresponding to the spray hole (26), and the adjustment rings (25) are independently deflected and adjusted so that the spray holes (26) at different diameter length positions are connected or staggered with the transfer holes (27).
7. A deposition method for controlling the uniformity of the thickness of a thin film deposited on a wafer, which adopts the deposition device for controlling the uniformity of the thickness of a thin film deposited on a wafer as claimed in any one of claims 5 to 6, characterized in that: It includes the following steps: S1. Wafer placement: multiple wafers are placed on the wafer loading space of the deposition seat (3) by means of a vacuum fixture. At this time, the wafers can be fixed by negative pressure adsorption through the air holes on the negative pressure plate (44); then the air guide seat (2) and the deposition seat (3) are sealed and assembled, and the inside is evacuated by a vacuum pump (13); S2. In the initial deposition stage of the wafer, the wafer on the wafer positioning assembly (4) is placed horizontally, the carrier (31) in the deposition seat (3) is continuously rotating, and the negative pressure plate (44) can be driven to rotate by the built-in motor, so that the wafer can rotate while orbiting. At this time, the air supply pipe (12) performs the initial stage of reaction gas delivery and adjusts the flow rate of the reaction gas. After the reaction gas passes through the temperature control of the heat conduction plate (22), it passes downward through the nozzles (26) of the air flow plate (23) to achieve initial thin film deposition; S3. Multi-stage deposition. To increase the deposition rate and ensure deposition thickness and uniformity, the wafer positioning component (4) gradually changes the wafer carrying angle to form multiple different stages of wafer deposition. In each stage, the wafer can still revolve in the carrier (31), and the negative pressure plate (44) controls the wafer rotation. At this time, the reaction gas can be sprayed onto the wafer from the nozzles (26) at different diameter positions, so that a uniform and controllable film thickness is formed on the wafer surface. S4. Control of gas flow direction. In each stage, after the reaction gas flows through the surface of the wafer, a portion of the reaction gas enters the gas cavity (36) through the guide hole (35) on the gas guide ring (34), and enters the gas exhaust pipe (11) through the gas-tight seat (5), while another portion of the reaction gas enters the flow cavity (45) through the discharge hole (46) on the inner wall of the carrier (41), and then enters the direct current pipe (53) through the current collecting seat, and finally flows into the gas exhaust pipe (11); thereby controlling and adjusting the flow ratio of the reaction gas in the two flow paths, so as to realize the control of the flow rate of the reaction gas on the wafer surface and effectively adjust the film deposition speed; S5. At the end of deposition, the wafer is placed horizontally, and step S2 is repeated while adjusting the parameters of wafer rotation speed, reaction gas flow rate and temperature so that a deposited film with uniform properties is formed on the wafer surface.