A method for preparing a piezoelectric ceramic material doped with barium strontium titanate

By introducing screening steps in the preparation process of piezoelectric ceramic materials, the screening mechanism of the molding equipment is used to detect and remove ceramic parts with unqualified quality, the problem of quality error during the molding process is solved, and the stability and consistency of ceramic parts are achieved. , ensuring product performance and quality.

CN118495944BActive Publication Date: 2024-11-08NANTONG INST OF TECH
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410959288.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-17
Publication Date
2024-11-08
Estimated Expiration
2044-07-17

AI Technical Summary

Technical Problem

In the preparation process of piezoelectric ceramic materials, the quality errors during the molding process will affect the sintering process, resulting in unstable finished product quality, and it is difficult for the prior art to effectively screen out ceramic parts with unqualified quality.

Method used

The screening step is introduced between the press forming step and the sintering step. The ceramic parts are quality tested and screened through the screening mechanism of the molding equipment to remove ceramic parts with unqualified quality, ensuring the quality stability and consistency of the production process.

Benefits of technology

Through the introduction of screening steps, the quality control of ceramic parts is achieved, ensuring the performance and quality requirements of the final product, avoiding the increase in manual processes, and improving the automation and efficiency of the production process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118495944B_ABST
    Figure CN118495944B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of piezoelectric ceramic material preparation, and discloses a method for preparing a piezoelectric ceramic material doped with barium strontium titanate. The piezoelectric ceramic material has a chemical formula of Ba 1‑x Sr x TiO3, which is made of ferroelectric materials BaTiO3 and SrTiO3 by doping rare earth elements and solid phase sintering, wherein x represents the ratio of strontium Sr to barium Ba; specifically includes corresponding preparation methods and molding equipment. The present invention pushes the pressed ceramic parts from the molding mechanism to the discharging position through the molding mechanism, and the ceramic parts arrive at the screening mechanism position, and the screening mechanism is responsible for quality inspection and screening of the formed ceramic parts; the entire pressing and molding process, through the orderly combination of molding, filling and screening links, realizes the transformation process from powder to molded parts, and strictly controls the quality of the ceramic parts at each step to ensure that the final product meets the expected performance and quality requirements.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of piezoelectric ceramic material preparation, and in particular to a method for preparing a piezoelectric ceramic material doped with barium strontium titanate. Background Art

[0002] Piezoelectric ceramic materials doped with barium strontium titanate usually have excellent piezoelectric and dielectric properties and are suitable for various piezoelectric devices and sensors. The purpose of doping is usually to improve the specific properties of the material or increase its scope of application. Doping can be the addition of a small amount of other elements, such as rare earth elements or transition metal oxides, to adjust the material's lattice structure, electrical properties and sintering behavior.

[0003] When piezoelectric ceramic products are prepared by a solid-phase method, the molding process is generally carried out by pressing and molding through a mold. If there is a quality error in the mold pressing and molding process, it will lead to molding errors in the subsequent sintering process, which will ultimately affect the quality of the finished product. At the same time, the weight of the piezoelectric ceramic does not change much before and after the sintering step. Therefore, it is of great significance to screen the molded ceramic parts after the pressing and molding step. Summary of the invention

[0004] The purpose of the present invention is to provide a technical solution, adding a screening step between the pressing step and the sintering step, screening the formed ceramic parts according to their quality differences, and removing ceramic parts with large quality errors, so as to solve the problems in the prior art raised in the above background technology.

[0005] To achieve the above object, the present invention adopts the following technical solutions:

[0006] A method for preparing a piezoelectric ceramic material doped with barium strontium titanate, wherein the piezoelectric ceramic material has a chemical formula of Ba 1-x Sr x TiO3, which is made of ferroelectric materials BaTiO3 and SrTiO3 by doping rare earth elements and solid phase sintering, where x represents the ratio of strontium Sr to barium Ba;

[0007] The preparation method comprises the following steps:

[0008] S1. Raw material preparation and ingredient mixing, selecting the required starting materials, including raw materials of barium strontium titanate and dopants; weighing the raw materials according to a predetermined chemical ratio, and mixing them evenly to ensure that the dopant is evenly dispersed in the barium strontium titanate matrix;

[0009] S2. ball milling, putting the mixed powder into a ball mill, adding an appropriate amount of grinding solvent, and using ball milling media for ball milling to obtain fine and uniform powder particles;

[0010] S3 drying, the ball-milled slurry is dried to remove the solvent and obtain a dry powder;

[0011] S4. Compression molding, the pre-sintered powder is molded, the compression molding step uses a molding device, the molding device generates green ceramic parts while screening out unqualified ceramic parts to ensure quality stability and consistency during the production process;

[0012] S5. Sintering: The green ceramic parts are sintered in a high-temperature furnace. The sintering temperature and holding time are optimized and adjusted according to the specific formula and required performance. During the sintering process, the powder particles are combined into a dense ceramic body through solid-state diffusion.

[0013] Preferably, the compression molding comprises the following steps:

[0014] The molding equipment uses a molding die to press and mold the powder raw materials into preliminary ceramic parts. The ceramic parts are pushed out of the molding die and intermittently conveyed in sequence. During the conveying process, the mass of each ceramic part is measured in sequence, and the ceramic parts with a mass within the error range are transmitted to the next process, and the ceramic parts with a mass outside the error range are removed.

[0015] Preferably, a molding device for a piezoelectric ceramic material is provided, wherein the molding device comprises:

[0016] Forming mechanism, feeding mechanism and screening mechanism;

[0017] The forming mechanism is used to press the ceramic powder into a round cake-shaped ceramic piece;

[0018] The feeding mechanism is used for filling the barium strontium titanate-doped piezoelectric ceramic powder and pushing the pressed ceramic parts from the forming mechanism to the discharging position;

[0019] The screening mechanism is arranged at the discharging position, and the screening mechanism performs quality inspection on the ceramic pieces formed by the forming mechanism, screens out ceramic pieces with unqualified quality, and continuously conveys ceramic pieces with qualified quality to the next process.

[0020] Preferably, the screening mechanism uses the push of the feeding mechanism to cooperate with the intermittent conveying component to intermittently convey the plurality of ceramic pieces, and a screening mechanism is provided on the conveying path of the ceramic pieces, and the screening mechanism sequentially screens the intermittently conveyed ceramic pieces;

[0021] The screening mechanism includes a conveying platform, an intermittent conveying component and a weighing component. The conveying platform is provided with a limited edge to form a conveying path for the ceramic pieces. The intermittent conveying component is provided on the conveying path for the ceramic pieces to control the intermittent conveying of the ceramic pieces. The weighing component weighs the intermittently conveyed ceramic pieces in sequence.

[0022] Preferably, the conveying platform is provided with a clearance hole on the conveying path, and the weighing assembly is arranged at the position of the clearance hole. The weighing assembly includes a load-bearing plate and a weight sensor. The upper surface of the load-bearing plate is higher than the conveying platform. When a single ceramic piece is conveyed and stops on the upper surface of the load-bearing plate, the weight sensor weighs the single ceramic piece.

[0023] Preferably, the intermittent conveying assembly includes a separating rotating member, a ratchet and a movable pawl, the separating rotating member and the ratchet are coaxially positioned and installed, the ratchet is rotatably installed on the conveying platform, the movable pawl is rotatably installed on the conveying platform and can be reset by a reset spring, and a cam for rotating the movable pawl and a driving motor for driving the movable pawl to rotate are also rotatably installed on the conveying platform; as the cam rotates, the movable pawl intermittently jumps, causing the ratchet and the separating rotating member to intermittently rotate, so as to realize intermittent conveying of ceramic parts.

[0024] Preferably, it includes a removal component, which is located on one side of the intermittent conveying component. The ceramic parts weighed and measured by the weighing component are intermittently conveyed by the intermittent conveying component once and then arrive at the workstation of the removal component. The removal component includes a linear push rod and a push plate. The removal component pushes the ceramic parts with unqualified quality out of the conveying path through the linear push rod and the push plate.

[0025] Preferably, the carrying plate and the conveying platform are provided with powder leakage holes along the conveying path of the ceramic parts, and the excess raw material powder of the ceramic parts during the conveying process leaks out through the powder leakage holes, thereby avoiding excessive accumulation of powder affecting the accuracy of the weighing component.

[0026] Preferably, the molding mechanism comprises a machine platform, on which a molding pressure head and a molding groove are arranged, and an ejection structure is arranged in the molding groove;

[0027] The feeding mechanism includes a feeding box and a filling pipe. The feeding box moves back and forth on the machine platform through a linear motion module. A positioning rod for reciprocating positioning of the linear motion module is provided on the machine platform. A pushing plate is provided on the side of the feeding box.

[0028] The powder raw materials of the ceramic parts are filled into the forming tank through the filling pipe and the loading box. When the loading box returns to the initial position from above the forming tank, the powder in the forming tank is scraped flat. After the ceramic parts are formed by the forming head and the forming tank, the pressed ceramic parts are ejected from the forming tank and pushed to the conveying path by the pushing plate.

[0029] Technical effects and advantages of the present invention: Compared with the prior art, the method for preparing a piezoelectric ceramic material doped with barium strontium titanate proposed by the present invention has the following advantages:

[0030] The present invention pushes the pressed ceramic pieces from the forming mechanism to the discharging position through the forming mechanism, and the ceramic pieces arrive at the screening mechanism position, and the screening mechanism is responsible for quality inspection and screening of the formed ceramic pieces; by measuring the quality of individual ceramic pieces in turn, the ceramic pieces with qualified quality will continue to be transported to the next process, and the ceramic pieces with unqualified quality will be automatically screened out, ensuring the quality stability and consistency in the production process; the entire pressing and forming process, through the orderly combination of the forming, filling and screening links, realizes the transformation process from powder to formed pieces, and strictly controls the quality of the ceramic pieces at each step to ensure that the final product meets the expected performance and quality requirements;

[0031] By combining the separation rotating part with the ratchet structure, the intermittent jumping of the movable pawl causes the ratchet and the separation rotating part to rotate intermittently, so as to realize the intermittent conveying of ceramic parts. Combined with the special structure of the carrying plate, it is convenient to weigh the ceramic parts one by one in sequence. At the same time, by removing components, the ceramic parts whose mass exceeds the error range are eliminated without adding additional manual processes. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1 is a flow chart of a method for preparing a piezoelectric ceramic material according to the present invention;

[0033] Figure 2 It is one of the structural schematic diagrams of the molding equipment in the present invention;

[0034] Figure 3 This is the second structural schematic diagram of the molding equipment in the present invention;

[0035] Figure 4 This is the third structural schematic diagram of the molding equipment in the present invention;

[0036] Figure 5 It is a schematic diagram of the top view of the structure of the molding device of the present invention;

[0037] Figure 6 It is a front structural schematic diagram of the molding device of the present invention;

[0038] Figure 7 For the present invention Figure 6 A schematic diagram of the enlarged structure at A in the middle;

[0039] Figure 8 It is a schematic diagram of the structure of the intermittent conveying component in the present invention;

[0040] Fig. 9 It is a structural schematic diagram of the load-bearing plate in the present invention;

[0041] Fig.10 This is one of the bottom structure schematic diagrams of the molding device of the present invention;

[0042] Fig.11This is the second schematic diagram of the bottom structure of the molding device of the present invention;

[0043] In the figure:

[0044] 1. Forming mechanism; 2. Feeding mechanism; 3. Screening mechanism;

[0045] 11. Machine platform; 12. Forming press head; 13. Forming tank;

[0046] 21. Feeding box; 22. Filling pipe; 23. Linear motion module; 24. Positioning rod; 25. Pushing plate;

[0047] 31. Conveying platform; 32. Limiting edge; 33. Intermittent conveying assembly; 34. Clearance hole; 35. Carrying plate; 36. Display screen; 37. Powder leakage hole; 38. Weighing assembly; 39. Removal assembly;

[0048] 331, separating rotating member; 332, ratchet; 333, movable pawl; 334, driving motor; 335, cam; 336, return spring. DETAILED DESCRIPTION

[0049] The subject matter described herein will now be discussed with reference to example embodiments. It should be understood that the discussion of these embodiments is only to enable those skilled in the art to better understand and implement the subject matter described herein, and the functions and arrangements of the elements discussed may be changed without departing from the scope of protection of the contents of this specification. Each example may omit, replace or add various processes or components as needed. In addition, the features described relative to some examples may also be combined in other examples.

[0050] The invention provides Figure 1-Figure 11 As shown, a method for preparing a piezoelectric ceramic material doped with barium strontium titanate, the piezoelectric ceramic material having a chemical formula of Ba 1-x Sr x TiO3, which is made of ferroelectric materials BaTiO3 and SrTiO3 by doping rare earth elements and solid phase sintering, where x represents the ratio of strontium Sr to barium Ba;

[0051] like Figure 1 , the preparation method comprises the following steps:

[0052] S1. Raw material preparation and ingredient mixing: select the required starting materials, including the raw materials of barium strontium titanate and dopants (such as rare earth elements, transition metal oxides, etc.); weigh the raw materials according to the predetermined chemical ratio and mix them evenly; ensure that the dopants are evenly dispersed in the barium strontium titanate matrix;

[0053] S2. ball milling: put the mixed powder into a ball mill, add an appropriate amount of grinding solvent (such as alcohol or water), and use ball milling media (such as zirconia grinding balls) to perform ball milling to obtain fine and uniform powder particles;

[0054] S3 drying, the ball-milled slurry is dried to remove the solvent and obtain a dry powder;

[0055] S4. Compression molding, the pre-sintered powder is molded and pressed into a green ceramic part, the pressing step uses a molding device, the molding device generates green ceramic parts while screening out unqualified ceramic parts to ensure quality stability and consistency during the production process;

[0056] S5. Sintering: The green ceramic parts are sintered in a high-temperature furnace. The sintering temperature and holding time need to be optimized and adjusted according to the specific formula and required performance. During the sintering process, the powder particles are combined into a dense ceramic body through solid-state diffusion.

[0057] The pressing step can be performed by dry pressing, isostatic pressing, extrusion and other methods to form ceramic parts. In the actual preparation scenario, it is most common to directly use a mold for pressing. The pressing method using a molding mold includes the following steps:

[0058] The molding equipment uses a molding die to press and mold the powder raw materials into preliminary ceramic parts. The ceramic parts are pushed out of the molding die and intermittently conveyed in sequence. During the conveying process, the mass of each ceramic part is measured in sequence, and the ceramic parts with a mass within the error range are transmitted to the next process, and the ceramic parts with a mass outside the error range are removed.

[0059] like Figure 2-Figure 4 According to the specific steps of compression molding using a molding die, corresponding molding equipment needs to be equipped. The following provides a specific implementation method; a molding equipment including a piezoelectric ceramic material, the molding equipment includes:

[0060] Forming mechanism 1, feeding mechanism 2 and screening mechanism 3;

[0061] The forming mechanism 1 is used to press the ceramic powder into a round cake-shaped ceramic piece;

[0062] The feeding mechanism 2 is used for filling the barium strontium titanate-doped piezoelectric ceramic powder and pushing the pressed ceramic parts from the forming mechanism 1 to the discharging position;

[0063] The screening mechanism 3 is arranged at the discharging position, and the screening mechanism 3 performs quality inspection on the ceramic pieces formed by the forming mechanism 1, and screens out ceramic pieces with unqualified quality, while continuing to convey ceramic pieces with qualified quality to the next process.

[0064] Working principle: The pre-prepared ceramic powder is placed into the forming mold through the forming mechanism 1. The forming mechanism 1 uses the pressure and the mold to press the powder into a round ceramic piece. The key to this step is to ensure that the ceramic powder can fully fill the mold and is subjected to sufficient pressure to ensure the shape and density of the final molded part; through the feeding mechanism 2, piezoelectric ceramic powder doped with strontium barium titanate is filled into the mold. The filling process requires precise control of the amount of powder to ensure the accurate material ratio of the molded part. After the filling is completed, the forming mechanism 1 pushes the pressed ceramic part from the forming mechanism 1 to the discharge position The ceramic pieces arrive at the screening mechanism 3, which is responsible for quality inspection and screening of the formed ceramic pieces; by measuring the quality of individual ceramic pieces in turn, the ceramic pieces with qualified quality will continue to be transported to the next process, while the ceramic pieces with unqualified quality will be automatically screened out to ensure the quality stability and consistency in the production process; the entire pressing and molding process, through the orderly combination of molding, filling and screening, realizes the transformation process from powder to molded parts, and strictly controls the quality of ceramic pieces at each step to ensure that the final product meets the expected performance and quality requirements.

[0065] like Figure 4 Regarding the structure of the molding die, the molding mechanism 1 includes a machine table 11, on which a molding pressure head 12 and a molding groove 13 are provided, and an ejection structure is provided in the molding groove 13;

[0066] The feeding mechanism 2 includes a feeding box 21 and a filling pipe 22. The feeding box 21 reciprocates on the machine table 11 through a linear motion module 23. A positioning rod 24 for reciprocating positioning of the linear motion module 23 is provided on the machine table 11. A pushing plate 25 is provided on the side of the feeding box 21.

[0067] The powder raw materials of the ceramic parts are filled into the molding groove 13 through the filling pipe 22 and the loading box 21. When the loading box 21 returns to the initial position from above the molding groove 13, the powder in the molding groove 13 is scraped flat. After the ceramic parts are formed by the molding pressure head 12 and the molding groove 13, the pressed ceramic parts are ejected from the molding groove 13 and pushed to the conveying path by the pushing plate 25.

[0068] like Figure 5-Figure 7 , with respect to the operation mode and specific structure of the above-mentioned screening mechanism 3, the following specific implementation is provided; the screening mechanism 3 uses the push of the feeding mechanism 2 to cooperate with the intermittent conveying component 33 to intermittently convey a plurality of ceramic pieces, and the screening mechanism 3 is arranged on the conveying path of the ceramic pieces, and the screening mechanism 3 sequentially screens the intermittently conveyed ceramic pieces;

[0069] The screening mechanism 3 includes a conveying platform 31, an intermittent conveying component 33 and a weighing component 38. The conveying platform 31 is provided with a limited edge 32 to form a conveying path for the ceramic pieces. The intermittent conveying component 33 is arranged on the conveying path for the ceramic pieces to control the intermittent conveying of the ceramic pieces. The weighing component 38 weighs the intermittently conveyed ceramic pieces in sequence.

[0070] Specifically, a display screen 36 is provided on the conveying platform 31, and the weighing result of the weighing component 38 is displayed in real time on the display screen 36. A PLC controller is also included. The PLC controller can compare the weighing result data of the weighing component 38 with a preset data range. If the value exceeds the range, the removal component 39 is triggered with a delay. When the intermittent conveying component 33 conveys the ceramic parts to the removal component 39 station, the removal component 39 pushes the ceramic parts out of the conveying path. If the quality is within the error range, it is conveyed normally until the next process.

[0071] The conveying platform 31 is provided with a clearance hole 34 on the conveying path, and the weighing assembly 38 is arranged at the position of the clearance hole 34. The weighing assembly 38 includes a carrying plate 35 and a weight sensor. The upper surface of the carrying plate 35 is higher than the conveying platform 31. When a single ceramic piece is conveyed and stops on the upper surface of the carrying plate 35, the weight sensor weighs the single ceramic piece.

[0072] like Figure 5-Figure 9 The carrier plate 35 and the conveying platform 31 are provided with powder leakage holes 37 along the conveying path of the ceramic parts. During the conveying process of the ceramic parts, the excess raw material powder is leaked out through the powder leakage holes 37 to avoid excessive accumulation of powder affecting the accuracy of the weighing component 38. Specifically, the shape of the carrier plate 35 is as follows: Fig. 9 As shown, both sides of the load-bearing plate 35 are arranged as slopes, and the bottom surface height of the load-bearing plate 35 is arranged flush with the conveying platform 31. The ceramic pieces on the conveying platform 31 are pushed through the load-bearing plate 35 in sequence. When they are pushed to the upper surface of the load-bearing plate 35, the ceramic pieces on the load-bearing plate 35 are higher than the conveying platform 31, and the weighing assembly 38 only weighs one ceramic piece separately.

[0073] like Figure 8, the following specific implementation scheme is provided for the intermittent conveying component 33, the intermittent conveying component 33 includes a separating rotating member 331, a ratchet 332 and a movable pawl 333, the separating rotating member 331 and the ratchet 332 are coaxially positioned and installed, the ratchet 332 is rotatably installed on the conveying platform 31, the movable pawl 333 is rotatably installed on the conveying platform 31 and can be reset by a reset spring 336, and a cam 335 for rotating the movable pawl 333 and a driving motor 334 for driving the movable pawl 333 to rotate are also rotatably installed on the conveying platform 31; as the cam 335 rotates, the movable pawl 333 intermittently jumps, causing the ratchet 332 and the separating rotating member 331 to intermittently rotate, so as to realize intermittent conveying of ceramic parts.

[0074] like Figure 4 and Figure 5 For the above-mentioned screening method, it is necessary to cooperate with the corresponding removal component 39, otherwise the weighed unqualified ceramic parts will be mixed with the qualified ceramic parts, affecting the subsequent process, including the removal component 39, the removal component 39 is located on one side of the intermittent conveying component 33, and the ceramic parts weighed and measured by the weighing component 38 are intermittently conveyed in the intermittent conveying component 33 and then arrive at the workstation of the removal component 39, the removal component 39 includes a linear push rod and a push plate, and the removal component 39 pushes the unqualified ceramic parts out of the conveying path through the linear push rod and the push plate; the ceramic parts whose quality exceeds the error range are removed by the removal component 39 without adding additional manual processes.

[0075] The above describes an embodiment of the present embodiment, but the present embodiment is not limited to the above-mentioned specific implementation methods. The above-mentioned specific implementation methods are merely illustrative and not restrictive. Under the guidance of the present embodiment, ordinary technicians in this field can also make many forms, all of which are within the protection of the present embodiment.

Claims

1. A method for preparing a piezoelectric ceramic material doped with barium strontium titanate, wherein the piezoelectric ceramic material has the general chemical formula of Ba 1- x Sr x TiO 3 , which is made of ferroelectric material BaTiO 3 and SrTiO 3 It is made by doping rare earth elements and solid phase sintering, where x represents the ratio of strontium Sr to barium Ba. Features: The preparation method comprises the following steps: S1. Raw material preparation and ingredient mixing, select the required starting materials, including raw materials and dopants of barium strontium titanate; weigh the raw materials and mix them evenly to ensure that the dopant is evenly dispersed in the barium strontium titanate matrix; S2. ball milling, placing the mixed powder into a ball mill, adding a grinding solvent and using a ball milling medium to perform ball milling to obtain a powder; S3 drying, the ball-milled powder is dried to remove the solvent and obtain a dry powder; S4. Compression molding, the pre-sintered powder is molded and pressed into a green ceramic part, the pressing step uses a molding device, the molding device generates green ceramic parts while screening out unqualified ceramic parts to ensure quality stability and consistency during the production process; S5. Sintering, sintering the green ceramic piece after forming in a high temperature furnace, the sintering temperature and holding time are optimized and adjusted according to the specific formula and required performance; during the sintering process, the powder particles are combined into a dense ceramic body through solid-state diffusion; Compression molding includes the following steps: The molding equipment uses a molding die to press the powder raw material into a preliminary ceramic part. The ceramic part is pushed out of the molding die and is intermittently conveyed in sequence. During the conveying process, the mass of each ceramic part is measured in sequence. The ceramic parts with a mass within the error range are transferred to the next process, and the ceramic parts with a mass outside the error range are removed. A molding device comprising a piezoelectric ceramic material, the molding device comprising: A forming mechanism (1), a feeding mechanism (2) and a screening mechanism (3); The forming mechanism (1) is used to press the ceramic powder into a round cake-shaped ceramic piece; The feeding mechanism (2) is used to fill the barium strontium titanate-doped piezoelectric ceramic powder and to push the pressed ceramic piece from the forming mechanism (1) to the discharging position; The screening mechanism (3) is arranged at the material discharging position, and the screening mechanism (3) performs quality inspection on the ceramic pieces formed by the forming mechanism (1), screens out ceramic pieces with unqualified quality, and continuously conveys ceramic pieces with qualified quality to the next process; The screening mechanism (3) uses the push of the feeding mechanism (2) in conjunction with the intermittent conveying component (33) to intermittently convey a plurality of ceramic pieces. The screening mechanism (3) is provided on the conveying path of the ceramic pieces, and the screening mechanism (3) sequentially screens the intermittently conveyed ceramic pieces. The screening mechanism (3) comprises a conveying platform (31), an intermittent conveying component (33) and a weighing component (38); the conveying platform (31) is provided with a limited edge (32) to form a conveying path for the ceramic pieces; the intermittent conveying component (33) is provided on the conveying path for the ceramic pieces to control the intermittent conveying of the ceramic pieces; and the weighing component (38) weighs the intermittently conveyed ceramic pieces in sequence; The conveying platform (31) is provided with a clearance hole (34) on the conveying path, the weighing assembly (38) is arranged at the position of the clearance hole (34), the weighing assembly (38) comprises a bearing plate (35) and a weight sensor, the upper surface of the bearing plate (35) is higher than the conveying platform (31), and when a single ceramic piece is conveyed and stops on the upper surface of the bearing plate (35), the weight sensor weighs the single ceramic piece; The intermittent conveying assembly (33) comprises a separating rotating member (331), a ratchet (332) and a movable pawl (333); the separating rotating member (331) and the ratchet (332) are coaxially mounted; the ratchet (332) is rotatably mounted on the conveying platform (31); the movable pawl (333) is rotatably mounted on the conveying platform (31) and is resettable and rotatable by a reset spring (336); a cam (335) for rotating the movable pawl (333) and a driving motor (334) for driving the movable pawl (333) to rotate are also rotatably mounted on the conveying platform (31); as the cam (335) rotates, the movable pawl (333) intermittently jumps, causing the ratchet (332) and the separating rotating member (331) to intermittently rotate, thereby realizing intermittent conveying of ceramic pieces; The invention comprises a removal component (39), wherein the removal component (39) is located at one side of the intermittent conveying component (33), and the ceramic pieces weighed and measured by the weighing component (38) are intermittently conveyed by the intermittent conveying component (33) once and then arrive at the workstation of the removal component (39), wherein the removal component (39) comprises a linear push rod and a push plate, and the removal component (39) pushes the ceramic pieces with unqualified quality out of the conveying path through the linear push rod and the push plate.

2. The method for preparing a piezoelectric ceramic material doped with barium strontium titanate according to claim 1, It is characterized in that The carrying plate (35) and the conveying platform (31) are provided with powder leakage holes (37) along the conveying path of the ceramic pieces. During the conveying process of the ceramic pieces, excess raw material powder is leaked out through the powder leakage holes (37), thereby preventing excessive accumulation of powder from affecting the accuracy of the weighing component (38).

3. A method for preparing a piezoelectric ceramic material doped with barium strontium titanate according to claim 1 or 2, It is characterized in that The molding mechanism (1) comprises a machine platform (11), the machine platform (11) being provided with a molding pressure head (12) and a molding groove (13), and an ejection structure being provided in the molding groove (13); The feeding mechanism (2) comprises a feeding box (21) and a filling pipe (22); the feeding box (21) moves back and forth on the machine platform (11) via a linear motion module (23); a positioning rod (24) is provided on the machine platform (11) for positioning the linear motion module (23) in reciprocating motion; and a pushing plate (25) is provided on the side of the feeding box (21); The powder raw material of the ceramic part is filled into the molding groove (13) through the filling pipe (22) and the loading box (21). When the loading box (21) returns to the initial position from above the molding groove (13), the powder in the molding groove (13) is scraped flat. After the ceramic part is molded by the molding head (12) and the molding groove (13), the pressed ceramic part is ejected from the molding groove (13) and pushed to the conveying path by the pushing plate (25).

Citation Information

Patent Citations

  • Automatic weighing transmission quality control system for powder compacting product

    CN101498601A

  • Barium strontium titanate doped high dielectric property ferroelectric ceramic material and preparation thereof

    CN101503293A

  • Ceramic resistor formula, processing technology and equipment

    CN114524670A

  • Ceramic rock plate forming equipment and preparation method

    CN115946225A

  • Automatic mold pressing and detecting system for ceramic cushion block and working method of automatic mold pressing and detecting system

    CN118219389A