Antibacterial and breathable knitted fabric and preparation method thereof

By using antibacterial and breathable reinforced components and modified porous silica structure in knitted fabrics, combined with a blended textile fabric with multiple fibers, the problem of insufficient antibacterial and breathable properties of knitted fabrics is solved, and efficient antibacterial and ultraviolet resistance is achieved.

CN118560124BActive Publication Date: 2024-11-19SICHUAN TINGMANYI TECH GRP CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411029941.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-30
Publication Date
2024-11-19
Estimated Expiration
2044-07-30

AI Technical Summary

Technical Problem

In the antibacterial treatment of existing knitted fabrics, the UV resistance of haloamine antibacterial agents has poor UV resistance, which affects its antibacterial properties. Traditional fabrics are easy to absorb sweat, causing bacteria to grow, affecting health.

Method used

Antibacterial breathable enhancement components are grafted to form an antibacterial surface layer, and the pyrimidine ring, coumarin structure and quaternary ammonium salt structure in the modified porous silica structure and the antibacterial components are combined with nylon, cotton, and linseed Blend with bamboo fiber to improve antibacterial and breathable properties.

Benefits of technology

It significantly improves the antibacterial properties and breathability of knitted fabrics, enhances UV resistance, reduces quaternary ammonium salt photolysis, and improves the stability and wearable comfort of the fabric.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 1SNDGO8GMQBSIDLXXJFEJAORBIGERY7F7RB7KX70
    Figure 1SNDGO8GMQBSIDLXXJFEJAORBIGERY7F7RB7KX70
  • Figure 1Y2VP9DZTUX3A2GG1NG8YLRGSDPO6VJZRBKRJRGP
    Figure 1Y2VP9DZTUX3A2GG1NG8YLRGSDPO6VJZRBKRJRGP
  • Figure URDPF7B7SGLV6QUWOAERJ9CSJLGXC4FSD7MSMQ6P
    Figure URDPF7B7SGLV6QUWOAERJ9CSJLGXC4FSD7MSMQ6P
Patent Text Reader

Abstract

The invention relates to an antibacterial and breathable knitted fabric and a preparation method thereof, belonging to the technical field of textiles, comprising a fabric base layer and an antibacterial surface layer; the antibacterial surface layer is formed by grafting an antibacterial liquid containing an antibacterial and breathable enhancing component onto an antibacterial fiber; the fabric base layer is made of the following fiber blends by weight: 40-50 parts of nylon fiber and 25-35 parts of polyester fiber; the antibacterial fiber is made of the following fiber blends by weight: 40-60 parts of cotton fiber, 10-20 parts of flax fiber and 25-55 parts of bamboo fiber; in the invention, the antibacterial liquid contains the antibacterial and breathable enhancing component, the shell of the component is a porous silica structure modified by KH-550, the core is an antibacterial component, the antibacterial component contains a pyrimidine ring, a coumarin structure, a Schiff base structure and a quaternary ammonium salt structure, and the antibacterial property, ultraviolet resistance and breathability of the knitted fabric are improved through the synergistic effect of each group of the antibacterial and breathable enhancing component.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of textiles, and in particular relates to an antibacterial and breathable knitted fabric and a preparation method thereof. Background Art

[0002] Knitted fabrics have the advantages of moisture absorption, breathability, soft texture, and comfort, and are widely used in clothing, home textiles and other products. Commonly used knitted fabrics are made of pure cotton fabrics, which easily absorb sweat from the human body. Not only are they not breathable, but sweat remains on clothing and skin, which can easily breed bacteria and produce odor, thus affecting health.

[0003] In the prior art, the antibacterial treatment of knitted fabrics is generally achieved by using antibacterial finishing agents and antibacterial fiber materials. Among them, halamine antibacterial agents have the advantages of long-lasting high efficiency, low toxicity, renewability, and broad-spectrum antibacterial, and are widely used in antibacterial textiles. Due to the presence of NX bonds in halamine antibacterial agents themselves, their UV resistance is poor, which seriously affects their antibacterial properties.

[0004] Therefore, in order to improve the wearing experience, developing a knitted fabric with good breathability, good UV resistance and strong antibacterial properties is a technical problem that needs to be solved urgently. Summary of the invention

[0005] The purpose of the present invention can be achieved through the following technical solutions:

[0006] An antibacterial and breathable knitted fabric comprises a fabric base layer and an antibacterial surface layer; the antibacterial surface layer is formed by grafting an antibacterial liquid onto an antibacterial fiber; the fabric base layer is made of a blend of the following fibers by weight: 40-50 parts of nylon fiber and 25-35 parts of polyester fiber; the antibacterial fiber is made of a blend of the following fibers by weight: 40-60 parts of cotton fiber, 10-20 parts of flax fiber and 25-55 parts of bamboo fiber;

[0007] The preparation method of the antibacterial and breathable knitted fabric comprises the following steps:

[0008] Step S1, preparing a fabric base layer: blending nylon fiber and polyester fiber by weight, and then weaving them into a knitted fabric layer by a large circular machine to obtain a fabric base layer;

[0009] Step S2, blending cotton fiber, flax fiber and bamboo fiber by weight to obtain antibacterial fiber;

[0010] Step S3, immersing the antibacterial fiber prepared in step S2 in an antibacterial liquid, padding, pre-baking, baking, washing with water for several times, and drying to obtain an antibacterial surface layer;

[0011] Step S4, connecting the fabric base layer prepared in step S1 and the antibacterial surface layer prepared in step S3 by suturing to obtain an antibacterial and breathable knitted fabric.

[0012] Furthermore, in step S3, the impregnation and rolling are two-impregnation and two-rolling, and the specific operation is: the impregnated antibacterial fiber is impregnated and rolled by a rolling car, the impregnation time is 10-30min, the impregnation pressure is 0.1-0.3MPa, the rolling rate is 70-80%, the pre-drying temperature is 85-95℃, the time is 5-10min, the baking temperature is 140-150℃, the time is 3-5min, and the drying temperature is 45-55℃.

[0013] Furthermore, the method for preparing the antibacterial liquid comprises the following steps:

[0014] Add the antibacterial breathable enhancement component into deionized water, heat it to 55-65° C., stir it evenly, and obtain an antibacterial liquid, wherein the mass ratio of the antibacterial breathable enhancement component to the deionized water is 3-5:60-80.

[0015] Furthermore, the preparation method of the antibacterial breathable enhancement component comprises the following steps:

[0016] The porous core-shell particles are vacuum dried to constant weight, then added to an ethanol aqueous solution with a mass fraction of 65-75%, ultrasonically dispersed evenly, and the siloxane alcohol solution is added while stirring, and the temperature is raised to 60-70°C, and stirred for reaction for 4-6 hours. After the reaction is completed, the particles are cooled to room temperature, washed with ethanol several times, centrifuged, and vacuum dried to obtain an antibacterial breathable enhancement component;

[0017] Among them, the amount ratio of porous core-shell particles, ethanol aqueous solution with a mass fraction of 65-75% and siloxane alcohol solution is 3-5g:35-45mL:12.6-13mL, and the amount ratio of siloxane and ethanol in the siloxane alcohol solution is 0.6-1.0mL:12mL. In the above reaction process, the porous core-shell particles are modified by siloxane, which improves the dispersibility and compatibility of the porous core-shell particles, and obtains an antibacterial and breathable enhanced component containing amino groups on the surface, which paves the way for subsequent reactions.

[0018] Furthermore, the siloxane is KH-550.

[0019] Furthermore, the method for preparing the porous core-shell particles comprises the following steps:

[0020] Step A1, adding 2-amino-4-hydroxy-6-methylpyrimidine to ethanol, adding a mixed solution a of p-dimethylaminobenzaldehyde, glacial acetic acid and ethanol dropwise while stirring, heating to reflux and stirring to react for 8-12h, and after the reaction is completed, removing the solvent by distillation under reduced pressure, and drying to obtain a Schiff base monomer, wherein the amount ratio of 2-amino-4-hydroxy-6-methylpyrimidine, ethanol and the mixed solution a is 2-4g:40-60mL:28mL, and the amount ratio of p-dimethylaminobenzaldehyde, glacial acetic acid and ethanol in the mixed solution a is 2.4-4.8g:2mL:26mL. In the above reaction process, glacial acetic acid is used as a catalyst, and 2-amino-4-hydroxy-6-methylpyrimidine reacts with p-dimethylaminobenzaldehyde to obtain a Schiff base monomer;

[0021] The structural formula of the Schiff base monomer is shown below:

[0022]

[0023] Step A2, adding Schiff base monomer, coumarin-3-carboxylic acid and p-toluenesulfonic acid to anhydrous DMF, heating to 65-75°C, stirring for reaction for 8-9h, and after the reaction, removing anhydrous DMF by rotary evaporation to obtain a coumarin derivative, wherein the amount ratio of Schiff base monomer, coumarin-3-carboxylic acid, p-toluenesulfonic acid and anhydrous DMF is 2-4g:1.5-3.1g:0.04-0.06g:40-60mL. In the above reaction process, with anhydrous DMF as solvent and p-toluenesulfonic acid as catalyst, the Schiff base monomer and coumarin-3-carboxylic acid undergo esterification reaction to obtain a coumarin derivative, and the structural formula of the coumarin derivative is as follows:

[0024]

[0025] Step A3, dissolving the coumarin derivative in anhydrous DMF, adding 1-chlorohexane, heating to 70-80°C, stirring for reaction for 4-6h, removing the anhydrous DMF by rotary evaporation, and drying to obtain an antibacterial component, wherein the amount ratio of the coumarin derivative, anhydrous DMF and 1-chlorohexane is 1.4-2.8g:50-60mL:3-5mL. In the above reaction process, with anhydrous DMF as solvent, the coumarin derivative and 1-chlorohexane undergo Menshutkin reaction to obtain the antibacterial component;

[0026] The structural formula of the antibacterial component is as follows:

[0027]

[0028] Step A4, dissolving alkyl orthosilicate in ethanol aqueous solution, adding antibacterial component, ultrasonically dispersing evenly, adjusting the solution pH to 8-9, adding porogen and emulsifier, emulsifying reaction at a speed of 12000-15000rpm for 3-5min, centrifuging, washing, and drying to obtain porous core-shell particles, wherein the amount ratio of alkyl orthosilicate, ethanol aqueous solution, antibacterial component, porogen and emulsifier is 6-12mL: 30-40mL: 1-2g: 1.5-2.5g: 0.6-0.8mL. In the above reaction process, alkyl orthosilicate is used as raw material and antibacterial component is used as inner core, and porous core-shell particles with porous silica outer layer and antibacterial component inner core are obtained by sol-gel method.

[0029] Furthermore, the drying temperature in step A1 is 45-55° C., and the drying time is 10-12 h.

[0030] Furthermore, the drying temperature in step A3 is 40-60° C., and the drying time is 6-8 hours.

[0031] Furthermore, in step A4, the alkyl orthosilicate is ethyl orthosilicate or methyl orthosilicate.

[0032] Furthermore, in step A4, the mass ratio of ethanol to deionized water in the ethanol aqueous solution is 1:2-4.

[0033] Furthermore, in step A4, the drying temperature is 55-65° C., and the drying time is 8-12 h.

[0034] Furthermore, in step A4, the porogen is polyethylene glycol octylphenyl ether or hexadecyltrimethylammonium bromide.

[0035] Furthermore, in step A4, the emulsifier is at least one of Tween-20, Tween-40, and Tween-60.

[0036] Compared with the prior art, the present invention has the following beneficial effects: in order to improve the antibacterial property and air permeability of knitted fabrics, the present invention grafts an antibacterial liquid containing an antibacterial air permeability enhancement component onto an antibacterial fiber to form an antibacterial surface layer; the outer shell of the antibacterial air permeability enhancement component is a porous silica structure modified by KH-550, and the inner core is an antibacterial component; the antibacterial component contains a pyrimidine ring, a coumarin structure, a Schiff base structure and a quaternary ammonium salt structure with good antibacterial properties; at the same time, the presence of the porous silica in the outer shell not only has good ultraviolet resistance, but also reduces the occurrence of photolysis of the quaternary ammonium salt structure in the inner core, thereby further improving the antibacterial property of the knitted fabric; moreover, it also has good air permeability, thereby improving the air permeability of the knitted fabric. DETAILED DESCRIPTION

[0037] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0038] Preparation Example 1

[0039] This preparation example provides a method for preparing porous core-shell particles, comprising the following steps:

[0040] Step A1, add 2 g of 2-amino-4-hydroxy-6-methylpyrimidine to 40 mL of ethanol, add dropwise a mixture of 2.4 g of p-dimethylaminobenzaldehyde, 2 mL of glacial acetic acid and 26 mL of ethanol while stirring, raise the temperature to reflux and stir to react for 8 h, after the reaction is completed, remove the solvent by distillation under reduced pressure, and then place at 45 ° C. and vacuum dry for 10 h to obtain a Schiff base monomer;

[0041] Step A2, add 3 g of Schiff base monomer, 1.5 g of coumarin-3-carboxylic acid and 0.04 g of p-toluenesulfonic acid into 40 mL of anhydrous DMF, heat to 65° C., stir and react for 8 h. After the reaction is completed, remove the anhydrous DMF by rotary evaporation to obtain a coumarin derivative;

[0042] Step A3, dissolving 1.4 g of the coumarin derivative in 50 mL of anhydrous DMF, adding 3 mL of 1-chlorohexane, heating to 70° C., stirring for 4 h, removing the anhydrous DMF by rotary evaporation, and drying at 40° C. for 6 h to obtain an antibacterial component;

[0043] Step A4, dissolve 6mL of tetraethyl orthosilicate in 30mL of ethanol aqueous solution, add 1g of antibacterial component, disperse evenly by ultrasonication, adjust the pH of the solution to 8, add polyethylene glycol octylphenyl ether and Tween-20, emulsify and react at a speed of 12000rpm for 3min, wash with ethanol 3 times, and dry at 55°C for 8h to obtain porous core-shell particles, wherein the mass ratio of ethanol to deionized water in the ethanol aqueous solution is 1:2.

[0044] Preparation Example 2

[0045] This preparation example provides a method for preparing porous core-shell particles, comprising the following steps:

[0046] Step A1, add 3 g of 2-amino-4-hydroxy-6-methylpyrimidine to 50 mL of ethanol, add dropwise a mixture of 3.6 g of p-dimethylaminobenzaldehyde, 2 mL of glacial acetic acid and 26 mL of ethanol while stirring, raise the temperature to reflux and stir to react for 10 hours, after the reaction is completed, remove the solvent by distillation under reduced pressure, then wash with ethanol and deionized water 4 times in sequence, and then place at 50° C. and vacuum dry for 11 hours to obtain a Schiff base monomer;

[0047] Step A2, add 3 g of Schiff base monomer, 2.3 g of coumarin-3-carboxylic acid and 0.05 g of p-toluenesulfonic acid into 50 mL of anhydrous DMF, heat to 70° C., stir and react for 8.5 h. After the reaction is completed, remove the anhydrous DMF by rotary evaporation to obtain a coumarin derivative;

[0048] Step A3, dissolving 2.1 g of coumarin derivative in 55 mL of anhydrous DMF, adding 4 mL of 1-chlorohexane, heating to reflux and stirring to react for 5 h, removing anhydrous DMF by rotary evaporation, and drying at 60° C. for 7 h to obtain an antibacterial component;

[0049] Step A4, dissolve 9mL of ethyl orthosilicate in 35mL of 45% ethanol aqueous solution, add 1.5g of antibacterial component, disperse evenly by ultrasonication, adjust the pH of the solution to 8.5 with 1M sodium hydroxide solution, add 2.0g of hexadecyltrimethylammonium bromide and 0.7mL of Tween-40, emulsify and react at a speed of 13500rpm for 4min, wash with ethanol 4 times, and dry at 60°C for 10h to obtain porous core-shell particles, wherein the mass ratio of ethanol to deionized water in the ethanol aqueous solution is 1:3.

[0050] Preparation Example 3

[0051] This preparation example provides a method for preparing porous core-shell particles, comprising the following steps:

[0052] Step A1, add 4 g of 2-amino-4-hydroxy-6-methylpyrimidine to 60 mL of ethanol, add dropwise a mixture of 4.8 g of p-dimethylaminobenzaldehyde, 2 mL of glacial acetic acid and 26 mL of ethanol while stirring, raise the temperature to reflux and stir to react for 12 h, after the reaction is completed, remove the solvent by distillation under reduced pressure, then wash with ethanol and deionized water for 5 times in sequence, and then place at 55° C. and vacuum dry for 12 h to obtain a Schiff base monomer;

[0053] Step A2, add 4 g of Schiff base monomer, 3.1 g of coumarin-3-carboxylic acid and 0.06 g of p-toluenesulfonic acid into 60 mL of anhydrous DMF, heat to 75° C., stir and react for 9 h. After the reaction is completed, remove the anhydrous DMF by rotary evaporation to obtain a coumarin derivative;

[0054] Step A3, dissolving 2.8 g of the coumarin derivative in 60 mL of anhydrous DMF, adding 5 mL of 1-chlorohexane, heating to 80° C., stirring for 6 h, removing the anhydrous DMF by rotary evaporation, and drying at 65° C. for 8 h to obtain an antibacterial component;

[0055] Step A4, dissolve methyl orthosilicate in 40 mL of ethanol aqueous solution, add 2 g of antibacterial component, disperse evenly by ultrasonication, adjust the solution pH to 9, add hexadecyltrimethylammonium bromide and Tween-60, emulsify and react at a speed of 15000 rpm for 5 min, wash with ethanol 5 times, and dry at 65°C for 12 h to obtain porous core-shell particles, wherein the mass ratio of ethanol to deionized water in the ethanol aqueous solution is 1:4.

[0056] Preparation Example 4

[0057] This preparation example provides a method for preparing an antibacterial liquid, comprising the following steps:

[0058] Step B1, put 3g of the porous core-shell particles prepared in Preparation Example 1 into a vacuum drying oven at 80°C, dry to constant weight, then place it in 35mL of 65% ethanol aqueous solution, ultrasonically disperse it evenly, add 0.6mL of KH-550 and 12mL of ethanol mixture dropwise while stirring, control the dripping within 10min, heat to 60°C, stir and react for 5h, after the reaction is completed, cool to room temperature, wash the solution with ethanol 3 times, centrifuge, and dry it at 60°C in vacuum for 16h to obtain an antibacterial breathable enhancement component;

[0059] Step B2: Add 90 g of the antibacterial breathable enhancement component into 1.8 L of deionized water, heat to 55° C., and stir evenly to obtain an antibacterial solution.

[0060] Preparation Example 5

[0061] This preparation example provides a method for preparing an antibacterial liquid, comprising the following steps:

[0062] Step B1, put 4g of the porous core-shell particles prepared in Preparation Example 1 into a vacuum drying oven at 80°C, dry to constant weight, then place it in 40mL of 70% ethanol aqueous solution, ultrasonically disperse it evenly, add 0.8mL of KH-550 and 12mL of ethanol mixture dropwise while stirring, control the dripping within 10min, heat to 65°C, stir and react for 5h, after the reaction is completed, cool to room temperature, wash the solution with ethanol 4 times, centrifuge, and vacuum dry at 70°C for 18h to obtain an antibacterial breathable enhancement component;

[0063] Step B2: Add 120 g of the antibacterial breathable enhancement component into 2.1 L of deionized water, heat to 60° C., and stir evenly to obtain an antibacterial solution.

[0064] Preparation Example 6

[0065] This preparation example provides a method for preparing an antibacterial liquid, comprising the following steps:

[0066] Step B1, put 5g of the porous core-shell particles prepared in Preparation Example 1 into a vacuum drying oven at 80°C, dry to constant weight, then place it in 45mL of 75% ethanol aqueous solution, ultrasonically disperse it evenly, add 1.0mL of KH-550 and 12mL of ethanol mixture dropwise while stirring, control the dripping within 10min, heat to 70°C, stir and react for 6h, after the reaction is completed, cool to room temperature, wash the solution with ethanol 5 times, centrifuge, and vacuum dry at 80°C for 20h to obtain an antibacterial breathable enhancement component;

[0067] Step B2: Add 150 g of the antibacterial breathable enhancement component into 2.4 L of deionized water, heat to 65° C., and stir evenly to obtain an antibacterial solution.

[0068] The present embodiment provides an antibacterial and breathable knitted fabric, comprising a fabric base layer and an antibacterial surface layer; the fabric base layer is made of a blend of the following fibers by weight: 40 parts of nylon fiber and 25 parts of polyester fiber; the antibacterial fiber is made of a blend of the following fibers by weight: 40 parts of cotton fiber, 10 parts of flax fiber and 25 parts of bamboo fiber;

[0069] The preparation method of the antibacterial and breathable knitted fabric comprises the following steps:

[0070] Step S1, preparing a fabric base layer: blending nylon fiber and polyester fiber by weight, and then weaving them into a knitted fabric layer by a large circular machine to obtain a fabric base layer;

[0071] Step S2, blending cotton fiber, flax fiber and bamboo fiber by weight to obtain antibacterial fiber;

[0072] Step S3, immersing the antibacterial fiber prepared in step S2 into the antibacterial solution prepared in Preparation Example 4, and then performing double immersion and double rolling by a rolling car, controlling the immersion time to be 10 minutes, the immersion and rolling pressure to be 0.1 MPa, the rolling rate to be 70%, and then pre-baking at 85°C for 8 minutes, baking at 140°C for 5 minutes, washing with water 3 times, and then drying at 50°C to obtain an antibacterial surface layer;

[0073] Step S4, connecting the fabric base layer prepared in step S1 and the antibacterial surface layer prepared in step S3 by suturing to obtain an antibacterial and breathable knitted fabric.

[0074] The present embodiment provides an antibacterial and breathable knitted fabric, comprising a fabric base layer and an antibacterial surface layer; the fabric base layer is made of a blend of the following fibers by weight: 45 parts of nylon fiber and 30 parts of polyester fiber; the antibacterial fiber is made of a blend of the following fibers by weight: 50 parts of cotton fiber, 15 parts of flax fiber and 40 parts of bamboo fiber;

[0075] The preparation method of the antibacterial and breathable knitted fabric comprises the following steps:

[0076] Step S1, preparing a fabric base layer: blending nylon fiber and polyester fiber by weight, and then weaving them into a knitted fabric layer by a large circular machine to obtain a fabric base layer;

[0077] Step S2, blending cotton fiber, flax fiber and bamboo fiber by weight to obtain antibacterial fiber;

[0078] Step S3, immersing the antibacterial fiber prepared in step S2 into the antibacterial solution prepared in Preparation Example 5, and then performing double immersion and double rolling by a rolling car, controlling the immersion time to be 20 minutes, the immersion and rolling pressure to be 0.2 MPa, the rolling rate to be 75%, and then pre-baking at 90°C for 8 minutes, baking at 145°C for 3 minutes, washing with water 4 times, and then drying at 50°C to obtain an antibacterial surface layer;

[0079] Step S4, connecting the fabric base layer prepared in step S1 and the antibacterial surface layer prepared in step S3 by suturing to obtain an antibacterial and breathable knitted fabric.

[0080] The present embodiment provides an antibacterial and breathable knitted fabric, comprising a fabric base layer and an antibacterial surface layer; the fabric base layer is made of a blend of the following fibers by weight: 50 parts of nylon fiber and 35 parts of polyester fiber; the antibacterial fiber is made of a blend of the following fibers by weight: 60 parts of cotton fiber, 20 parts of flax fiber and 55 parts of bamboo fiber;

[0081] The preparation method of the antibacterial and breathable knitted fabric comprises the following steps:

[0082] Step S1, preparing a fabric base layer: blending nylon fiber and polyester fiber by weight, and then weaving them into a knitted fabric layer by a large circular machine to obtain a fabric base layer;

[0083] Step S2, blending cotton fiber, flax fiber and bamboo fiber by weight to obtain antibacterial fiber;

[0084] Step S3, immersing the antibacterial fiber prepared in step S2 into the antibacterial solution prepared in Preparation Example 6, and then performing double immersion and double rolling by a rolling car, controlling the immersion time to be 30 minutes, the immersion and rolling pressure to be 0.3 MPa, the rolling rate to be 80%, and then pre-baking at 95°C for 10 minutes, baking at 150°C for 5 minutes, washing with water 5 times, and then drying at 55°C to obtain an antibacterial surface layer;

[0085] Step S4, connecting the fabric base layer prepared in step S1 and the antibacterial surface layer prepared in step S3 by suturing to obtain an antibacterial and breathable knitted fabric.

[0086] Comparative Example 1

[0087] Comparative Example 1 Compared with Example 1, in the process of preparing porous core-shell particles, 2-aminopyrimidine was used instead of 2-amino-4-hydroxy-6-methylpyrimidine, and other conditions remained unchanged.

[0088] Comparative Example 2

[0089] Comparative Example 2 Compared with Example 1, in the process of preparing the porous core-shell particles, benzaldehyde was used instead of p-dimethylaminobenzaldehyde, and other conditions remained unchanged.

[0090] Comparative Example 3

[0091] Comparative Example 3 Compared with Example 1, in the process of preparing the porous core-shell particles, dodecyltrimethylammonium chloride was used instead of the antibacterial component, and other conditions remained unchanged.

[0092] Performance Testing

[0093] The following performance tests were performed on the knitted fabrics prepared in Examples 1-3 and Comparative Examples 1-3:

[0094] Antibacterial rate: According to the national standard GB / T 20944.2-2007 "Evaluation of antibacterial properties of textiles Part 2: Absorption method", the antibacterial quantitative test was carried out, and the antibacterial performance was compared after 100 washings. The washing method was based on GB / T8629-2001 "Household washing and drying procedures for textile testing" using a type B agitator washing machine and washing procedure 8B. The ultraviolet protection factor and ultraviolet transmittance of textiles were tested with reference to "GB / T 18830-2009 Evaluation of the anti-ultraviolet performance of textiles". The air permeability of the sample was tested with an air permeability tester with reference to GB / T5453-1997 "Determination of air permeability of textile fabrics". The same sample was tested 10 times at different parts and the average value was taken. The specific performance test results are shown in Table 1 below;

[0095] Table 1

[0096]

[0097] From the data in Table 1, it can be seen that by comparing Example 1 with Comparative Example 1, the knitted fabric in Example 1 has more excellent antibacterial performance and UV resistance, which is because the 2-amino-4-hydroxy-6-methylpyrimidine in Example 1 can undergo esterification reaction with coumarin-3-carboxylic acid in the subsequent reaction process, thereby improving the synergistic effect of the coumarin structure and the pyrimidine ring, thereby significantly improving the antibacterial performance and UV resistance of the knitted fabric. By comparing Example 1 with Comparative Example 2, it can be seen that the knitted fabric in Example 1 has more excellent antibacterial performance, which is due to the good antibacterial performance of the quaternary ammonium salt structure in Example 1. By comparing Example 1 with Comparative Example 3, it can be seen that the knitted fabric in Example 1 has more excellent antibacterial performance and UV resistance, which is because in Example 1, the antibacterial component in the kernel not only contains Schiff base structure, coumarin structure and pyrimidine ring with good antibacterial performance, but also the ester group and ether bond thereon can produce stable hydrogen bonding with the surface of the antibacterial fiber, further improving its antibacterial stability after multiple washings, and at the same time, the coumarin ring structure also has good UV resistance, further improving the UV resistance of the fabric.

[0098] In the description of the specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.

[0099] The above contents are merely examples and explanations of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the invention or exceed the scope defined by the claims, they shall all fall within the protection scope of the present invention.

Claims

1. An antibacterial and breathable knitted fabric, characterized in that it comprises a fabric base layer and an antibacterial surface layer; the antibacterial surface layer is firstly prepared by mixing an antibacterial breathable enhancement component and deionized water to obtain an antibacterial liquid, and then grafted to an antibacterial fiber to form; the fabric base layer is made of the following fiber blends by weight: 40-50 parts of nylon fiber and 25-35 parts of polyester fiber; the antibacterial fiber is made of the following fiber blends by weight: 40-60 parts of cotton fiber, 10-20 parts of flax fiber and 25-55 parts of bamboo fiber; The method for preparing the antibacterial breathable enhanced component comprises the following steps: The porous core-shell particles are vacuum dried to constant weight, then added to an ethanol aqueous solution with a mass fraction of 65-75%, ultrasonically dispersed evenly, and the siloxane alcohol solution is added dropwise while stirring, and the temperature is raised to 60-70°C, and stirred for reaction for 4-6 hours. After the reaction is completed, the particles are cooled to room temperature, washed with ethanol several times, centrifuged, and vacuum dried to obtain an antibacterial breathable enhancement component; The method for preparing the porous core-shell particles comprises the following steps: Step A1, adding 2-amino-4-hydroxy-6-methylpyrimidine to ethanol, adding dropwise a mixed solution a of p-dimethylaminobenzaldehyde, glacial acetic acid and ethanol while stirring, heating to reflux and stirring to react for 8-12h, after the reaction is completed, removing ethanol by reduced pressure distillation, and vacuum drying to obtain a Schiff base monomer, wherein the amount ratio of 2-amino-4-hydroxy-6-methylpyrimidine, ethanol and the mixed solution a is 2-4g:40-60mL:28mL, and the amount ratio of p-dimethylaminobenzaldehyde, glacial acetic acid and ethanol in the mixed solution a is 2.4-4.8g:2mL:26mL; Step A2, adding Schiff base monomer, coumarin-3-carboxylic acid and p-toluenesulfonic acid to anhydrous DMF, heating to 65-75°C, stirring and reacting for 8-9h, and after the reaction, removing anhydrous DMF by rotary evaporation to obtain a coumarin derivative, wherein the amount ratio of Schiff base monomer, coumarin-3-carboxylic acid, p-toluenesulfonic acid and anhydrous DMF is 2-4g:1.5-3.1g:0.04-0.06g:40-60mL; Step A3, dissolving the coumarin derivative in anhydrous DMF, adding 1-chlorohexane, heating to 70-80°C, stirring for 4-6h, removing the anhydrous DMF by rotary evaporation, and drying to obtain an antibacterial component, wherein: The usage ratio of the coumarin derivative, anhydrous DMF and 1-chlorohexane is 1.4-2.8 g: 50-60 mL: 3-5 mL; Step A4, dissolving alkyl orthosilicate in ethanol aqueous solution, adding antibacterial components, ultrasonically dispersing evenly, adjusting the solution pH to 8-9, adding porogens and emulsifiers, and performing emulsification reaction at a speed of 12000-15000 rpm for 3-5 min, centrifuging, washing, and drying to obtain porous core-shell particles, wherein the amount ratio of alkyl orthosilicate, ethanol aqueous solution, antibacterial components, porogens, and emulsifiers is 6-12 mL: 30-40 mL: 1-2 g: 1.5-2.5 g: 0.6-0.8 mL.

2. The antibacterial and breathable knitted fabric according to claim 1, characterized in that: The usage ratio of the porous core-shell particles, the ethanol aqueous solution and the siloxane alcohol solution is 3-5 g: 35-45 mL: 12.6-13 mL.

3. A method for preparing the antibacterial and breathable knitted fabric according to any one of claims 1 to 2, characterized in that: The following steps are involved: Step S1, preparing a fabric base layer: blending nylon fiber and polyester fiber by weight, and then weaving them into a knitted fabric layer by a large circular machine to obtain a fabric base layer; Step S2, blending cotton fiber, flax fiber and bamboo fiber by weight to obtain antibacterial fiber; Step S3, immersing the antibacterial fiber prepared in step S2 in an antibacterial liquid, padding, pre-baking, baking, washing with water for several times, and drying to obtain an antibacterial surface layer; Step S4, connecting the fabric base layer prepared in step S1 and the antibacterial surface layer prepared in step S3 by suturing to obtain an antibacterial and breathable knitted fabric.

Citation Information

Cited By

  • Antibacterial and breathable cotton yarn textile fabric for mothers and infants and preparation method of antibacterial and breathable cotton yarn textile fabric

    CN120608360A