Manufacturing process of framework for fiber-optic gyroscope

By using metal materials and flame-retardant, heat-insulating and vibration-isolating material layers on the skeleton of the fiber optic gyroscope, combined with the process of silicone adhesives, the stability problem of the fiber optic gyroscope in temperature and vibration environments is solved, and its accuracy and reliability are improved. sex.

CN118706101APending Publication Date: 2024-09-27BEIJING PENGZHENG HUAXING PHOTOELECTRIC TECH CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410732572.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-06
Publication Date
2024-09-27

AI Technical Summary

Technical Problem

The existing fiber optic gyroscope skeleton manufacturing process has an adverse effect on the fiber ring when the temperature changes, resulting in unstable performance of the fiber optic gyroscope in temperature and vibration environments in medium and high-precision applications.

Method used

The metal material of the outer frame and the inner frame is used, combined with the flame-retardant, heat-insulating and vibration-isolating material layer and the silica gel layer. Through heating and moisture removal treatment and the use of silicone adhesive, an optical fiber ring is formed and a zero-bias test is performed to ensure the reliability of the fiber optic gyro. Temperature stability and vibration resistance.

Benefits of technology

It effectively reduces the temperature drift and vibration effects of fiber optic gyroscopes, improves measurement accuracy and mechanical reliability, simplifies the production process and reduces costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118706101A
    Figure CN118706101A
Patent Text Reader

Abstract

The invention discloses a manufacturing process of a framework for a fiber-optic gyroscope, and relates to the technical field of fiber-optic gyroscopes, and the manufacturing process comprises the following steps: S1, framework composition: the framework for the fiber-optic gyroscope is composed of an outer framework, an inner framework and an annular groove opening used for mounting an optical fiber ring, and a flame-retardant heat-insulation vibration-isolation material layer is arranged in the annular groove; an adhesive layer for bonding is coated on the flame-retardant heat-insulation vibration-isolation material layer; s2, preparing an optical fiber ring; s3, inspection is carried out; and S4, bonding is completed. The organic silicon adhesive is an adhesive cured at room temperature, the problem that a traditional organic silicon adhesive needs to be heated and cured is solved, the bonding process is simplified, the production period is shortened, the production cost is reduced, the product quality is improved, the color layer is arranged on the surface of each optical fiber, and the optical fiber has the advantages of being uniform in temperature distribution, small in stress, resistant to vibration, resistant to impact and the like. After the fiber-optic gyroscope is applied, the temperature drift and vibration influence of the gyroscope can be effectively reduced, and the mechanical reliability of the fiber-optic gyroscope is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of fiber optic gyroscopes, and in particular to a manufacturing process of a skeleton for a fiber optic gyroscope. Background Art

[0002] Fiber optic gyroscope is a new type of angular rate sensor that uses the Sagnac effect to convert the introduced rotational angular rate into phase drift. In the early 20th century, physicists discovered in experiments that the optical interference phenomenon was affected by the rotational angular rate, which inspired people to measure the rotational angular rate through the optical interference phenomenon. As a new type of all-solid-state inertial instrument, fiber optic gyroscope has no moving parts and wear parts compared to traditional gyroscopes. It has the advantages of low cost, long life, light weight, high reliability, and fast startup speed. It has been widely used in many military and civilian fields. Fiber optic gyroscope is an optoelectronic inertial sensitive device based on the Sagnac effect. The Sagnac effect is a pure spatial delay that is independent of the medium. The light emitted from the same light source is split into two beams of light with the same characteristics, which propagate in opposite directions in the same closed optical path and finally converge to the original splitting point. However, if the plane where the closed optical path is located rotates relative to the inertial space, the optical paths propagated by the positive and negative beams will be different, resulting in an optical path difference. The fiber optic gyroscope is a device for measuring the angular velocity of the carrier relative to the inertial space. It eliminates the disadvantages of the motion mechanism of traditional mechanical gyroscopes and laser gyroscopes. With its advantages of all-solid-state, high reliability, large dynamic range, fast start-up, and high sensitivity, it can be widely used in navigation, aviation, aerospace, oil exploration and other fields. As a new generation of important inertial measurement devices, medium and low precision fiber optic gyroscopes have been mass-produced and widely used. However, in medium and high precision application fields such as ship navigation, due to the sensitivity of fiber optic gyroscopes to environmental factors such as temperature and vibration, it has been difficult to ensure its performance in practical applications. In order to solve this phenomenon, the present invention provides a manufacturing process for the skeleton of a fiber optic gyroscope. The following problems exist in the prior art:

[0003] 1. In the existing manufacturing process of fiber optic gyroscope skeleton, the optical fiber is generally directly wound on the skeleton of the fiber optic loop. After the optical fiber is wound with one or more layers, a layer of film is placed on it. The film material has different temperature characteristics from the optical fiber and the fixing glue, which will directly have an adverse effect on the fiber optic loop when the temperature changes. Summary of the invention

[0004] In order to solve the above technical problems, the technical solution adopted by the present invention is:

[0005] A manufacturing process for a skeleton for an optical fiber gyroscope comprises the following steps:

[0006] S1. Framework composition: The framework of the fiber optic gyroscope is composed of an outer framework, an inner framework and an annular groove opening for installing an optical fiber ring. The inner part of the annular groove is provided with a flame retardant, heat insulation and vibration isolation material layer, and a glue layer for bonding is coated on the flame retardant, heat insulation and vibration isolation material layer;

[0007] S2. Prepare the optical fiber ring: clean the optical fiber ring skeleton, heat and dehumidify the optical fiber ring skeleton and the optical fiber, wrap the prepared optical fiber around the skeleton, bond each layer of the optical fiber layer with an organic silicone adhesive, and provide a color layer on the surface of each optical fiber;

[0008] S3. Inspection: Perform zero bias test on the prepared fiber optic ring to determine whether the fiber optic gyroscope has oscillation phenomenon. Perform zero bias test on the fiber optic ring assembly of each axis. If oscillation phenomenon exists, adjust the frequency difference and re-perform zero bias test until the fiber optic gyroscope has no oscillation phenomenon.

[0009] S4. Complete bonding: Apply curing glue on the upper end face of the optical fiber ring, use a special transparent positioning and molding tool to position and press it, and put it in a curing box for curing.

[0010] A further improvement of the technical solution of the present invention is that the height and width of the S1 annular groove are respectively 10 mm larger than the width and thickness of the optical fiber ring, the outer skeleton and the inner skeleton are made of metal, the material of the flame retardant, heat insulating and vibration isolating material layer is flame retardant polyurethane, the glue layer is silicone, and the thickness of the flame retardant, heat insulating and vibration isolating material layer is 3 mm.

[0011] A further improvement of the technical solution of the present invention is that S2 winds the colored optical fiber on the skeleton of the optical fiber gyroscope, and uses the optical fiber ring skeleton to wind two polarization-maintaining optical fibers respectively using the same process to form two optical fiber rings, and the number of layers of the two optical fiber rings and the number of turns of the optical fiber on each layer are the same.

[0012] A further improvement of the technical solution of the present invention is that: the optical fiber ring is potted, silicone adhesive is filled in the gap of the optical fiber ring, silicone adhesive is applied to each layer of optical fiber after it is wound, and the next layer is wound before the silicone adhesive dries, and the optical fibers between each layer are bonded to each other and kept in fixed position after bonding.

[0013] A further improvement of the technical solution of the present invention is that the starting point of the optical fiber winding is located at the tooling of the optical fiber ring skeleton, the optical fiber is divided into two sections from the midpoint, the optical fiber on one side of the midpoint is wound clockwise, and it is wound from top to bottom to the tooling at the lower edge of the optical fiber ring skeleton to form an optical fiber layer. When the optical fiber is colored, a fiber coloring machine is used to control the tension of the optical fiber to be maintained between 6 and 9 grams, and it is placed to dry after coloring.

[0014] A further improvement of the technical solution of the present invention is that after S4 is cured, the positioning and molding tooling is removed, the space is filled with cured glue, and after the glue is filled, the optical fiber ring is directly turned over, and the optical fiber ring is reversely positioned and bonded to the frame to complete the bonding of the optical fiber ring and the frame.

[0015] Due to the adoption of the above technical solution, the present invention has the following technical advances compared with the prior art:

[0016] 1. The present invention provides a manufacturing process for a skeleton for a fiber optic gyroscope, wherein a flame retardant, heat-insulating and vibration-isolating material layer is provided inside the annular groove, and a rubber layer for bonding is applied on the flame retardant, heat-insulating and vibration-isolating material layer. The outer skeleton and the inner skeleton are made of metal, the material of the flame retardant, heat-insulating and vibration-isolating material layer is flame retardant polyurethane, the rubber layer is silicone, the thickness of the flame retardant, heat-insulating and vibration-isolating material layer is 3 mm, and the heat insulation layer is placed between the skeleton-free fiber ring and the metal shell. Since the thermal conductivity of the heat insulation layer is much lower than that of the metal shell, the heat transfer can be slowed down, and the temperature difference between the upper and lower parts of the ring body can be reduced. The use of organic silicon adhesive as a room temperature curing adhesive solves the problem that the traditional organic silicone adhesive needs to be heated and cured, simplifies the bonding process, shortens the production cycle, reduces production costs, and improves product quality.

[0017] 2. The present invention provides a manufacturing process for a skeleton for an optical fiber gyroscope. The bonding of the ring and the skeleton is a key process for forming an optical fiber gyroscope. After bonding, the temperature performance and vibration and impact resistance of the optical fiber gyroscope are one of the most important indicators for measuring the optical fiber gyroscope. When preparing the optical fiber ring, the optical fiber ring skeleton is cleaned, the optical fiber ring skeleton and the optical fiber are heated and dehumidified, and the prepared optical fiber is wrapped around the skeleton. There is a bonding silicone adhesive between each layer of the optical fiber layer, and a color layer is provided on the surface of each optical fiber. The optical fiber has the characteristics of uniform temperature distribution, low stress, vibration resistance, and impact resistance. After application, the temperature drift and vibration influence of the gyroscope can be effectively reduced. The optical fiber gyroscope ring is manufactured by using colored optical fiber without laying a film, avoiding the influence of the introduction of film materials on the optical fiber ring, thereby reducing the measurement accuracy error of the optical fiber gyroscope, reducing the loss of the optical fiber gyroscope ring, and improving the temperature stability, measurement repeatability and sensitivity of the optical fiber gyroscope. Direct bonding between layers is used to improve the mechanical reliability of the optical fiber gyroscope ring, thereby improving the mechanical reliability of the optical fiber gyroscope. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a schematic diagram of the overall process structure of the manufacturing process of the skeleton for the fiber optic gyroscope of the present invention;

[0019] Figure 2 The figure is a schematic diagram of the process structure of preparing the optical fiber ring according to the present invention. DETAILED DESCRIPTION

[0020] The present invention is further described in detail below in conjunction with embodiments:

[0021] like Figure 1-2 As shown, the present invention provides a manufacturing process for a skeleton for an optical fiber gyroscope, comprising the following steps:

[0022] S1. Framework composition: The framework of the fiber optic gyroscope is composed of an outer framework, an inner framework and an annular groove opening for installing an optical fiber ring. The inner part of the annular groove is provided with a flame retardant, heat insulation and vibration isolation material layer, and a glue layer for bonding is coated on the flame retardant, heat insulation and vibration isolation material layer;

[0023] S2. Prepare the optical fiber ring: clean the optical fiber ring skeleton, heat and dehumidify the optical fiber ring skeleton and the optical fiber, wrap the prepared optical fiber around the skeleton, bond each layer of the optical fiber layer with an organic silicone adhesive, and provide a color layer on the surface of each optical fiber;

[0024] S3. Inspection: Perform zero bias test on the prepared fiber optic ring to determine whether the fiber optic gyroscope has oscillation phenomenon. Perform zero bias test on the fiber optic ring assembly of each axis. If oscillation phenomenon exists, adjust the frequency difference and re-perform zero bias test until the fiber optic gyroscope has no oscillation phenomenon.

[0025] S4. Complete bonding: Apply curing glue on the upper end face of the optical fiber ring, use a special transparent positioning and molding tool to position and press it, and put it in a curing box for curing.

[0026] In this implementation case, the flame retardant heat insulation and vibration isolation material layer is made of flame retardant polyurethane, the adhesive layer is silicone, the thickness of the flame retardant heat insulation and vibration isolation material layer is 3 mm, and the thermal insulation layer is placed between the skeleton-free optical fiber ring and the metal shell. Since the thermal conductivity of the thermal insulation layer is much lower than that of the metal shell, it can slow down the transfer of heat and reduce the temperature difference between the upper and lower parts of the ring body. The use of organic silicon adhesive as a room temperature curing adhesive solves the problem that traditional organic silicone adhesives need to be heated and cured, simplifies the bonding process, shortens the production cycle, reduces production costs, and improves product quality.

[0027] like Figure 1-2As shown, the present invention provides a technical solution: preferably, the height and width of the annular groove S1 are respectively greater than the width and thickness of the optical fiber ring by 10 mm, the outer frame and the inner frame are made of metal, the material of the flame retardant, heat-insulating and vibration-isolating material layer is flame retardant polyurethane, the glue layer is silica gel, and the thickness of the flame retardant, heat-insulating and vibration-isolating material layer is 3 mm, S2 winds the colored optical fiber on the skeleton of the optical fiber gyroscope, and uses the optical fiber ring skeleton to wind two polarization-maintaining optical fibers respectively using the same process to form two optical fiber rings, the number of layers of the two optical fiber rings is the same as the number of turns of the optical fiber on each layer, the optical fiber ring is potted, and the silicone adhesive is filled in the gap of the optical fiber ring, and each layer of the optical fiber is coated with organic adhesive after winding. Silicone adhesive, wind the next layer before the silicone adhesive dries, the optical fibers between each layer are bonded to each other, and the position is kept fixed after bonding. The starting point of the optical fiber winding is located at the tooling of the optical fiber ring skeleton. The optical fiber is divided into two sections from the midpoint, and the optical fiber on one side of the midpoint is wound clockwise, and it is wound from top to bottom to the lower edge tooling of the optical fiber ring skeleton to form an optical fiber layer. When the optical fiber is colored, a fiber optic coloring machine is used to control the tension of the optical fiber to be maintained between 6 and 9 grams. After coloring, it is placed to dry. After S4 is cured, the positioning molding tool is removed, and the cured glue is filled in the blank. After the glue is filled, the optical fiber ring is directly turned over, and the optical fiber ring is reversely positioned and bonded to the skeleton to complete the bonding of the optical fiber ring and the skeleton.

[0028] In this embodiment, a color layer is provided on the surface of each optical fiber, which has the characteristics of uniform temperature distribution, low stress, vibration resistance, impact resistance, etc. After application, it can effectively reduce the temperature drift and vibration influence of the gyroscope. The fiber optic gyroscope ring is manufactured by using colored optical fiber without laying a film, thereby avoiding the influence of the introduction of film material on the optical fiber ring, thereby reducing the measurement accuracy error of the fiber optic gyroscope, reducing the loss of the fiber optic gyroscope ring, and improving the temperature stability, measurement repeatability and sensitivity of the fiber optic gyroscope. Direct bonding between layers is used to improve the mechanical reliability of the fiber optic gyroscope ring, thereby improving the mechanical reliability of the fiber optic gyroscope.

[0029] The working principle of the manufacturing process of the skeleton for the fiber optic gyroscope is described in detail below.

[0030] like Figure 1-2As shown, the skeleton of the fiber optic gyroscope is composed of an outer skeleton, an inner skeleton and an annular groove opening for installing an optical fiber ring. The inner part of the annular groove is provided with a flame retardant, heat-insulating and vibration-isolating material layer, and a glue layer for bonding is coated on the flame retardant, heat-insulating and vibration-isolating material layer. The height and width of the annular groove are respectively 10 mm larger than the width and thickness of the optical fiber ring. The outer skeleton and the inner skeleton are made of metal, the material of the flame retardant, heat-insulating and vibration-isolating material layer is flame retardant polyurethane, the glue layer is silicone, the thickness of the flame retardant, heat-insulating and vibration-isolating material layer is 3 mm, and the insulation layer is placed between the skeleton-free optical fiber ring and the metal shell.Since the thermal conductivity of the insulation layer is much lower than that of the metal shell, it can slow down the transfer of heat and reduce the temperature difference between the upper and lower parts of the ring body. The use of silicone adhesives as room temperature curing adhesives solves the problem that traditional silicone adhesives need to be heated and cured, simplifies the bonding process, shortens the production cycle, reduces production costs, and improves product quality. The fiber optic ring skeleton is cleaned, the fiber optic ring skeleton and the optical fiber are heated and dehumidified, and the prepared optical fiber is wrapped around the skeleton. There is a bonding silicone adhesive between each layer of the optical fiber layer, and a color layer is provided on the surface of each optical fiber. The colored optical fiber is wound on the skeleton of the fiber optic gyroscope, and the fiber optic ring skeleton is used to collect Two polarization-maintaining optical fibers are wound using the same process to form two optical fiber rings. The number of layers of the two optical fiber rings is the same as the number of turns of the optical fiber on each layer. The optical fiber rings are potted and filled with silicone adhesive in the gaps of the optical fiber rings. After each layer of optical fiber is wound, silicone adhesive is applied. The next layer is wound before the silicone adhesive dries. The optical fibers between each layer are bonded to each other and the positions are kept fixed after bonding. The starting point of the optical fiber winding is located at the tooling of the optical fiber ring skeleton. The optical fiber is divided into two sections from the midpoint. The optical fiber on one side of the midpoint is wound in a clockwise direction and wound from top to bottom to the tooling at the lower edge of the optical fiber ring skeleton to form an optical fiber layer. Fiber coloring is used when the optical fiber is colored. The machine controls the tension of the optical fiber to be kept between 6 and 9 grams. After coloring, it is placed to dry. Each optical fiber surface is provided with a color layer, which has the characteristics of uniform temperature distribution, small stress, vibration resistance, and impact resistance. After application, it can effectively reduce the temperature drift and vibration influence of the gyroscope. The colored optical fiber does not need to be laid with a film to manufacture the optical fiber gyroscope ring, which avoids the influence of the introduction of film materials on the optical fiber ring, thereby reducing the measurement accuracy error of the optical fiber gyroscope, reducing the loss of the optical fiber gyroscope ring, and improving the temperature stability, measurement repeatability and sensitivity of the optical fiber gyroscope. Direct bonding between layers is used to improve the mechanical stability of the optical fiber gyroscope ring. Reliability, thereby improving the mechanical reliability of the fiber optic gyroscope, conduct a zero bias test on the prepared fiber optic ring to determine whether the fiber optic gyroscope has oscillation phenomenon, conduct a zero bias test on the fiber optic ring assembly of each axis, if there is oscillation phenomenon, adjust the frequency difference and re-test the zero bias until the fiber optic gyroscope does not have oscillation phenomenon, apply curing glue on the upper end face of the fiber optic fiber ring, use a special transparent positioning molding tool to position and press, put it in a curing box for curing, remove the positioning molding tool after S4 curing, fill the blank with curing glue, turn the fiber optic ring over directly after filling the glue, and reverse the fiber optic ring to bond it to the skeleton to complete the bonding of the fiber optic ring and the skeleton.

[0031] The above generally describes the present invention in detail, but it is obvious to a person skilled in the art that some modifications or improvements can be made to the present invention. Therefore, modifications or improvements that do not depart from the spirit of the present invention are within the scope of protection of the present invention.

Claims

1. A manufacturing process for a fiber optic gyroscope frame, comprising the following steps, characterized in that: S1. Framework composition: The framework of the fiber optic gyroscope is composed of an outer framework, an inner framework and an annular groove opening for installing an optical fiber ring. The inner part of the annular groove is provided with a flame retardant, heat insulation and vibration isolation material layer, and a glue layer for bonding is coated on the flame retardant, heat insulation and vibration isolation material layer; S2. Prepare the optical fiber ring: clean the optical fiber ring skeleton, heat and dehumidify the optical fiber ring skeleton and the optical fiber, wrap the prepared optical fiber around the skeleton, bond each layer of the optical fiber layer with an organic silicone adhesive, and provide a color layer on the surface of each optical fiber; S3. Inspection: Perform zero bias test on the prepared fiber optic ring to determine whether the fiber optic gyroscope has oscillation phenomenon. Perform zero bias test on the fiber optic ring assembly of each axis. If oscillation phenomenon exists, adjust the frequency difference and re-perform zero bias test until the fiber optic gyroscope has no oscillation phenomenon. S4. Complete bonding: Apply curing glue on the upper end face of the optical fiber ring, use a special transparent positioning and molding tool to position and press it, and put it in a curing box for curing.

2. The manufacturing process of a fiber optic gyroscope frame according to claim 1, characterized in that: The height and width of the S1 annular groove are respectively 10 mm larger than the width and thickness of the optical fiber ring. The outer frame and the inner frame are made of metal. The material of the flame retardant, heat insulating and vibration isolating material layer is flame retardant polyurethane. The glue layer is silicone. The thickness of the flame retardant, heat insulating and vibration isolating material layer is 3 mm.

3. The manufacturing process of a skeleton for an optical fiber gyroscope according to claim 1, characterized in that: S2 winds the colored optical fiber on the frame of the optical fiber gyroscope, and uses the optical fiber ring frame to wind two polarization-maintaining optical fibers respectively using the same process to form two optical fiber rings. The number of layers of the two optical fiber rings and the number of turns of the optical fiber on each layer are the same.

4. The manufacturing process of a skeleton for an optical fiber gyroscope according to claim 3, characterized in that: The optical fiber ring is potted and filled with silicone adhesive in the gap of the optical fiber ring. After each layer of optical fiber is wound, the silicone adhesive is applied, and the next layer is wound before the silicone adhesive dries. The optical fibers between each layer are bonded to each other and kept in fixed position after bonding.

5. The manufacturing process of a skeleton for an optical fiber gyroscope according to claim 4, characterized in that: The starting point of optical fiber winding is located at the tooling of the optical fiber ring skeleton. The optical fiber is divided into two sections from the midpoint. The optical fiber on one side of the midpoint is wound clockwise, and then wound from top to bottom to the tooling at the lower edge of the optical fiber ring skeleton to form an optical fiber layer. When coloring the optical fiber, a fiber optic coloring machine is used to control the tension of the optical fiber to be maintained between 6 and 9 grams. After coloring, it is placed to dry.

6. The manufacturing process of a fiber optic gyroscope frame according to claim 1, characterized in that: After S4 is cured, remove the positioning and molding tooling, fill the blanks with cured glue, and directly flip the fiber optic ring after filling, and bond the fiber optic ring to the frame in the reverse position to complete the bonding of the fiber optic ring and the frame.

Citation Information

Cited By

  • Fiber arrangement structure of three-axis integrated fiber-optic gyroscope

    CN120907525A