Middle frame, manufacturing method thereof and electronic equipment

Through mold processing and sandblasting and brushing, combined with inkjet printing decoration, the problem of complicated and high-cost processing of the middle frame groove in the existing technology is solved, and an efficient and low-cost three-dimensional texture appearance effect is achieved, which improves electronic equipment. aesthetics and productivity.

CN118720643APending Publication Date: 2024-10-01HUIZHOU VISION NEW TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410736491.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-06
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In the existing technology, the groove processing technology of the metal middle frame is complex and costly, and cannot effectively improve the aesthetic appearance.

Method used

Roughly processed profiles are processed using molds, combined with sandblasting and wire drawing, to achieve a grooved three-dimensional texture effect, and inkjet printing decoration processing can be used to simplify the process and improve production efficiency.

Benefits of technology

It realizes efficient and low-cost groove three-dimensional texture processing of the middle frame, improves the appearance aesthetics, simplifies the process flow, and improves processing efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118720643A_ABST
    Figure CN118720643A_ABST
Patent Text Reader

Abstract

The invention provides a middle frame, a manufacturing method of the middle frame and electronic equipment. The manufacturing method comprises the steps that a rough machining profile with a groove structure in the appearance face is manufactured through a mold; according to the required shape and the required size of the middle frame, the rough machining sectional material is manufactured into a middle sectional material; the appearance face of the middle profile is subjected to sand blasting treatment, and the middle profile subjected to sand blasting is obtained; the appearance face of the middle profile obtained after sand blasting is subjected to wire drawing treatment, and the middle profile obtained after wire drawing treatment is obtained; and performing post-treatment on the middle profile subjected to wire drawing treatment to obtain the middle frame. The technical problem that in the prior art, the technology is complex is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of electronic devices, and in particular to a middle frame and a manufacturing method thereof and an electronic device. Background Art

[0002] With the popularization of electronic devices, their appearance has become one of the important indicators for consumers to choose based on their increasingly powerful functions. The middle frame made of metal can enhance the beauty of the appearance. In the prior art, chemical etching is used to process a grooved three-dimensional texture on the appearance surface of the middle frame of the metal material to enhance the three-dimensional appearance; however, chemical etching first requires masking of the metal material, then engraving or developing the area to be etched on the surface, and then chemical etching is used to realize the groove, and finally the masking is removed to complete the groove texture setting. This type of conventional process operation is complicated. Summary of the invention

[0003] The main purpose of the present application is to provide a middle frame and a manufacturing method thereof and an electronic device, aiming to solve the technical problem of complex process existing in the prior art.

[0004] The present application proposes a method for manufacturing a middle frame, comprising:

[0005] A rough-machined profile having a groove structure on the exterior surface is produced by using a mold;

[0006] According to the required shape and size of the middle frame, the rough-processed profile is made into an intermediate profile;

[0007] Performing sandblasting on the exterior surface of the intermediate profile to obtain a sandblasted intermediate profile;

[0008] Performing wire drawing on the appearance surface of the sandblasted intermediate profile to obtain a wire drawing intermediate profile;

[0009] The intermediate profile after the wire drawing process is post-processed to obtain a middle frame.

[0010] Optionally, the post-processing of the intermediate profile after the wire drawing process includes:

[0011] The inner surface of the groove structure of the intermediate profile after the wire drawing process is subjected to inkjet printing decoration process.

[0012] Optionally, the post-processing of the intermediate profile after the wire drawing process further includes:

[0013] Before the inner surface of the groove structure of the intermediate profile after the wire drawing process is processed by the inkjet printing device, the surface of the intermediate profile after the wire drawing process is anodized.

[0014] Optionally, the post-processing of the intermediate profile after the wire drawing process further includes:

[0015] Before the inner surface of the groove structure of the intermediate profile after the wire drawing process is processed by the inkjet printing device, after the surface of the intermediate profile after the wire drawing process is anodized, the inner surface of the groove structure of the intermediate profile after the wire drawing process is plasma treated.

[0016] Optionally, while the inner surface of the groove structure of the intermediate profile after the wire drawing process is subjected to inkjet printing decoration treatment, the ink on the intermediate profile after the wire drawing process is subjected to curing treatment.

[0017] Optionally, there are multiple groove structures; wherein the depth of the groove structure is 0.5 to 0.8 mm; the width of the bottom groove wall of the groove structure is 0.7-1.0 mm; and the width of the convex surface connecting two adjacent groove structures is 1.0-2.0 mm.

[0018] Optionally, manufacturing the rough-processed profile into an intermediate profile according to the required shape and required size of the middle frame includes:

[0019] Straightening the rough-machined profile;

[0020] The straightened rough-processed profile is placed in an aging furnace and heated to a preset temperature, and kept at the temperature for a preset time to obtain a heat-treated rough-processed profile;

[0021] Performing surface treatment on the rough-machined profile after the heat treatment to obtain the rough-machined profile after the surface treatment;

[0022] The rough-processed profile after surface treatment is manufactured into an intermediate profile according to the required shape and size of the middle frame.

[0023] Optionally, after using a mold to produce a rough-machined profile with a groove structure on its exterior surface, and before producing the rough-machined profile into an intermediate profile according to the required shape and required size of the middle frame, the production method further includes: quenching the rough-machined profile taken out of the mold so that the rough-machined profile is in T5 or T6 state.

[0024] In a second aspect, the present application also proposes a middle frame made by the middle frame manufacturing method as described above.

[0025] In a third aspect, the present application also proposes an electronic device, comprising the middle frame as described above.

[0026] In the technical solution of the embodiment of the present application, a rough-machined profile with a groove structure on the appearance surface is directly processed by a mold; the rough-machined profile is processed to obtain an intermediate profile according to the required shape and required size of the middle frame; then the intermediate profile is successively sandblasted and wire-drawn to obtain the intermediate profile after wire-drawing, and the intermediate profile after wire-drawing is post-processed to obtain the middle frame; during the wire-drawing process, the sandblasted appearance of the original inner surface of the groove is not affected by wire-drawing, and the wire-drawing process will not destroy the main texture structure of the groove, so as to achieve the three-dimensional effect of the bright and matte appearance of the convex wire-drawn bright surface and the concave sandblasted matte surface. Compared with the chemical etching processing technology, in the technical solution provided by the embodiment of the present application, no masking treatment is required during the rough machining and fine machining of the groove, which is simpler in process and higher in processing efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying any creative work.

[0028] Figure 1 A schematic diagram of a process for manufacturing a middle frame provided in an embodiment of the present application;

[0029] Figure 2 A schematic diagram of a middle frame provided in an embodiment of the present application from one perspective;

[0030] Figure 3 for Figure 2 Schematic diagram of the middle AA section;

[0031] Figure 4 A partial schematic diagram of the appearance surface of the middle frame provided in an embodiment of the present application;

[0032] Figure 5 for Figure 1 A specific implementation flow chart of step S500;

[0033] Figure 6 for Figure 1 A specific implementation flow chart of step S200. DETAILED DESCRIPTION

[0034] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0035] It should be noted that all directional indications in the embodiments of the present application (such as up, down, left, right, front, back, etc.) are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.

[0036] In this application, unless otherwise clearly specified and limited, the terms "connection", "fixation", etc. should be understood in a broad sense. For example, "fixation" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0037] In addition, if there are descriptions involving "first", "second", etc. in the embodiments of the present application, the descriptions of "first", "second", etc. are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the meaning of "and / or" appearing in the full text includes three parallel schemes. Taking "A and / or B" as an example, it includes scheme A, or scheme B, or a scheme that satisfies both A and B. In addition, the technical solutions between the various embodiments can be combined with each other, but it must be based on the ability of ordinary technicians in the field to implement. When the combination of technical solutions is contradictory or cannot be implemented, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection required by this application.

[0038] At present, a large number of aluminum alloy (Al6061, Al6063, etc.) extruded materials are used in display frames such as TV, commercial display all-in-one machines, and smart education machines. Because this type of material has excellent molding performance and can achieve various surface treatment appearance effects, it is becoming more and more widely used. The traditional surface treatment of this type of frame is mainly brushed anode, sandblasted anode, spraying, electrophoresis, lamination and other processes. Among them, the surface after brushed anode and sandblasted anode treatment has a strong metallic texture, but the product appearance is highly homogenized; after spraying, electrophoresis, lamination and other processes, the surface of the aluminum material is covered with paint or decorative film, which cannot reflect the unique metallic texture and gloss of aluminum alloy, and the appearance is low-grade.

[0039] In order to improve the aesthetic appearance of electronic devices, grooves are processed on the appearance surface of the electronic devices so that they have groove textures and enhance their three-dimensional beauty. In the prior art, groove processing mainly includes CNC processing, laser processing and chemical etching. CNC processing has the disadvantage of low efficiency; laser processing is limited by processing equipment and cannot complete the processing of longer profiles, and there is a need for deep texture on the surface of aluminum materials, so the processing is time-consuming and the production efficiency is very low; therefore, chemical etching has become the main processing technology for the middle frame. However, during chemical etching, the metal material needs to be masked, and then the area on the surface that needs to be etched is engraved or developed, and then the groove is realized by chemical etching, and finally the masking is removed to complete the linear groove texture product. This process is complicated and the cost is high.

[0040] To this end, an embodiment of the present application provides a method for manufacturing a middle frame 100, which uses a mold, sandblasting and wire drawing to achieve a grooved three-dimensional texture effect of the middle frame 100. The process has high production efficiency, high yield, low cost, and no restriction on the processable length of the profile. Large, medium and small sized middle frames 100 can be achieved, especially for large-size display middle frames 100, which has the advantages of high production capacity and low cost.

[0041] Specifically, refer to Figure 1 As shown, the present application proposes a method for manufacturing a middle frame 100, comprising:

[0042] S100, using a mold to produce a rough-machined profile having an exterior surface 110 with a groove structure 111;

[0043] S200, manufacturing the rough-processed profile into an intermediate profile according to the required shape and size of the middle frame 100;

[0044] S300, performing sandblasting on the exterior surface 110 of the intermediate profile to obtain a sandblasted intermediate profile;

[0045] S400, performing wire drawing on the appearance surface 110 of the intermediate profile after sandblasting to obtain the intermediate profile after wire drawing;

[0046] S500 , performing post-processing on the intermediate profile after the wire drawing process to obtain the middle frame 100 .

[0047] In the technical solution of the embodiment of the present application, a rough-machined profile with a groove structure 111 on the appearance surface 110 is directly processed by a mold; the rough-machined profile is processed to obtain an intermediate profile according to the required shape and required size of the middle frame 100; then the intermediate profile is successively sandblasted and wire-drawn to obtain the intermediate profile after wire-drawing, and the intermediate profile after wire-drawing is post-processed to obtain the middle frame 100; during the wire-drawing process, the sandblasted appearance of the original inner surface of the groove (concave surface 111a) is not affected by wire-drawing, and the wire-drawing process will not destroy the main texture structure of the groove, so as to achieve the three-dimensional effect of the bright and matte appearance of the convex surface 111b and the sandblasted matte of the concave surface 111a. Compared with the chemical etching processing technology, in the technical solution provided by the embodiment of the present application, no shielding treatment is required during the rough machining and fine machining of the groove, which is simpler in process and higher in processing efficiency.

[0048] Compared with conventional processing technology, this application uses a mold structure and an extrusion process to complete the grooved three-dimensional texture appearance of the extruded aluminum surface. Since the groove structure 111 and the size characteristics are clearly defined, the entire appearance surface 110 can be sandblasted first, and then the convex surface 111b can be brushed without masking, thereby achieving a one-piece multi-effect three-dimensional texture appearance of the middle frame 100 (linear groove three-dimensional texture, convex surface 111b brushed bright surface, concave surface 111a sandblasted matte surface).

[0049] Generally speaking, the metal middle frame 100 of the electronic device uses aluminum or aluminum alloy as raw material, such as Al6061, Al6063, etc. In the process of using a mold to make a rough-processed profile with a groove structure 111 on the appearance surface 110, an extrusion mold is prepared in advance according to the cross-sectional design of the middle frame 100; the mold cavity of the extrusion mold has both the main cross-sectional structure of the middle frame 100 and the groove texture shape of the appearance surface 110; during the processing, the aluminum rod cast by the casting machine is heated to a certain temperature to reach the critical point of aluminum liquefaction, and then cut, hot sheared, and sent to the extruder, and the heated round cast rod is extruded from the mold by the extruder to obtain an aluminum extruded profile with groove texture characteristics on the surface.

[0050] like Figure 2 , Figure 3 to Figure 4As shown, an example of a cross-sectional structure of a middle frame 100 is shown; the appearance surface 110 of the middle frame 100 has a linearly arranged groove structure 111. The depth of these groove structures 111 is 0.5 to 0.8 mm. The width of the bottom groove wall (concave surface 111a) of the groove structure 111 is 0.7-1.0 mm. The width of the convex surface 111b (i.e., the appearance surface 110) connecting two adjacent groove structures 111 is 1.0-2.0 mm. When the wire drawing process is performed, the material thickness removal amount of the appearance surface 110 is usually 0.05 to 0.2 mm; since the depth of the groove structure 111 reaches more than 0.5 mm, the sandblasted appearance of the original concave surface 111a is not affected by the wire drawing, and the wire drawing process will not destroy the main texture structure of the groove.

[0051] In the prior art, the exterior surface 110 can also be partially decorated with colors; for example, the conventional processing technology realizes the appearance of a monochrome decorative line through a process of primary anodizing (color 1) + CNC high gloss machine to remove the oxide layer + secondary anodizing (color 2), but the conventional processing technology is complicated and has a long processing cycle. The more types of decorative line colors, the more anodizing treatments are performed, resulting in high costs. In some other technologies, a digital dispensing machine is used to fill the paint to achieve the decoration of the groove surface, but this method is prone to glue breakage or glue overflow, which seriously affects the appearance; and because this method is a drip coating method, on the one hand, the coating is thicker, and on the other hand, the coating is not fully atomized, which affects the curing effect of the coating, resulting in the adhesion cannot be guaranteed. There are also technologies that use silk screen printing or pad printing to achieve color decoration, but because the groove width of the invention is very narrow, only 0.7 to 1.0 mm, and the groove depth reaches 0.5 mm or more, the screen or pad printing rubber head cannot contact the inner surface of the groove, so the conventional means of silk screen printing or pad printing cannot achieve the ink or paint coating of the narrow groove concave surface 111a.

[0052] As an optional implementation of the above embodiment, Figure 4 As shown, the post-processing of the intermediate profile after the wire drawing process includes: S520, performing inkjet printing decoration processing on the inner surface of the groove structure 111 of the intermediate profile after the wire drawing process. In the technical solution of the embodiment of the present application, UV printing equipment is used to print UV ink on the inner surface of the linear groove of the middle frame 100, and the inner surface of the groove structure 111 is subjected to inkjet printing decoration processing. This method has high printing accuracy and high efficiency. In this technical solution, the inner surface of the groove structure 111 can also achieve gradient color and multi-color pattern processing at one time.

[0053] In some embodiments of the present application, the inner surface of the groove texture of the middle frame 100 is processed by UV printing process, so as to achieve the effect of local colored decorative lines. The product appearance effect is further improved on the basis of the integrated multi-effect three-dimensional texture. Compared with traditional multiple anodizing and CNC processing and digital dispensing, silk screen printing, pad printing and other traditional processes, this process is not limited by the site, has high processing accuracy and efficiency, and is more environmentally friendly.

[0054] In an embodiment, a monochrome inkjet printing decoration process can be performed, i.e., a decorative line of the same color is printed in each groove structure; a dual-color or multi-color inkjet printing decoration process can also be performed, i.e., decorative lines of different colors are printed in adjacent groove structures, such as printing decorative lines of different colors in two adjacent groove structures, or printing decorative lines of different colors in three adjacent groove structures.

[0055] As an optional implementation of the above embodiment, Figure 4 As shown, the post-processing of the intermediate profile after the wire drawing process also includes: before the inner surface of the groove structure 111 of the intermediate profile after the wire drawing process is processed by the inkjet printing device, S510, the surface of the intermediate profile after the wire drawing process is anodized. The surface of the intermediate profile is anodized to form an oxide film with both decorative and protective properties on the surface (including the inner surface of the groove structure 111). When coloring is required, it can be dyed after oxidation and then sealed; when silver white (original color) is required, it can be directly sealed after oxidation.

[0056] As an optional implementation of the above embodiment, Figure 5 As shown, the post-processing of the intermediate profile after the wire drawing process also includes: before the inner surface of the groove structure 111 of the intermediate profile after the wire drawing process is processed by the inkjet printing device, after the surface of the intermediate profile after the wire drawing process is anodized, S530, the inner surface of the groove structure 111 of the intermediate profile after the wire drawing process is plasma treated. The groove texture appearance surface 110 of the intermediate profile middle frame 100 after the anodization is plasma treated; specifically, in the embodiment, the low-temperature plasma treatment is used to make the material surface undergo multiple physical and chemical changes, introduce polar groups to the material surface to change its adhesion, so as to achieve the purpose of improving the adhesion between the ink and the metal anodized surface.

[0057] As an optional implementation of the above embodiment, while the inner surface of the groove structure 111 of the intermediate profile after the wire drawing process is subjected to inkjet printing decoration treatment, the ink on the intermediate profile after the wire drawing process is cured. In the embodiment, while the inkjet printing decoration process is being performed, the UV curing lamp provided by the equipment can be directly used to synchronously cure the ink on the product surface, thereby improving the processing efficiency and curing effect.

[0058] As an optional implementation of the above embodiment, Figure 6 As shown, the process of manufacturing the rough-processed profile into an intermediate profile according to the required shape and required size of the middle frame 100 includes:

[0059] S210, straightening the rough-machined profile;

[0060] S220, placing the straightened rough-processed profile into an aging furnace, heating it to a preset temperature, and keeping it at the temperature for a preset time, to obtain a heat-treated rough-processed profile;

[0061] S230, performing surface treatment on the rough-machined profile after the heat treatment to obtain the rough-machined profile after the surface treatment;

[0062] S240 , manufacturing the rough-processed profile after the surface treatment into an intermediate profile according to the required shape and required size of the middle frame 100 .

[0063] In an embodiment, the rough-machined profile is straightened to ensure that the profile is straight, which is convenient for making the shape of the middle frame 100. The straightened rough-machined profile is placed in an aging furnace and heated to a preset temperature and kept warm for a preset time to obtain a rough-machined profile after heat treatment, which significantly improves the mechanical properties of the profile, such as surface hardness and material strength. In an embodiment, the preset temperature and the holding time are determined according to the type of profile; for the T5 heat treatment state of 6063 aluminum extruded profile, the artificial aging treatment is usually preset for 2-3 hours and the preset temperature is about 200°C. Surface treatment includes surface grinding, burr treatment, etc. to remove profile marks and burrs.

[0064] Further, in an embodiment, after the surface treatment, the profile is subjected to bending, welding and other treatments according to the required shape and required size of the middle frame 100 to obtain an intermediate profile. For example, according to the required shape and required size of the middle frame 100, a 90° V-angle notch is punched at a position of the profile after surface treatment that matches the required shape and required size of the middle frame 100, and then the V-angle notch is bent 90° to form, for example, an intermediate profile (preliminary forming of the middle frame 100) with three sides (left side, sky side, right side) of a U-shape, and then a welding treatment is performed at the bending seam position, so that the intermediate profile structure is fixed and the stability is enhanced. In some embodiments, the V-angle notch is then bent 90° to form, for example, an intermediate profile (preliminary forming of the middle frame 100) with four sides (left side, sky side, right side, ground side), and then a welding treatment is performed at the bending seam position, so that the intermediate profile structure is fixed and the stability is enhanced. In some embodiments, the degree and bending angle of the V-angle notch are determined according to the shape of the middle frame 100. Generally speaking, the middle frame 100 is square in structure, so the degree and bending angle of the V-angle notch are 90 degrees.

[0065] In some embodiments, the rough-processed profile is led out by a tractor, cut by a hot saw to the length required for the middle frame 100, and then the profile is moved to a straightening machine for straightening. Then it is cut by a fixed-length saw and sent to the aging process. That is, in the embodiment, the processed rough-processed profile can meet the processing requirements of multiple middle frames 100, improve the needs of mass production, and improve efficiency. Then the rough-processed profile is sawn into multiple sections, each section meets the growth needs of a middle frame 100.

[0066] As an optional implementation of the above embodiment, after using a mold to produce a rough-machined profile having a groove structure 111 on the exterior surface 110, before the rough-machined profile is produced into an intermediate profile according to the required shape and required size of the middle frame 100, the production method further includes: quenching the rough-machined profile taken out of the mold so that the rough-machined profile is in a T5 or T6 state. The rough-machined profile is quenched so that the obtained rough-machined profile is in a T5 or T6 state, so that it has a good crystal phase structure and good mechanical properties.

[0067] In some embodiments, taking an aluminum (alloy) middle frame as an example, its main production steps include: extrusion molding of aluminum profile by extrusion die → quenching → sawing and straightening of aluminum profile → artificial aging heat treatment of aluminum profile → mechanical surface grinding → punching → bending → welding → sand blasting, wire drawing → anodizing → plasma surface cleaning → UV ink printing of colored decorative lines (ink simultaneous curing) → middle frame.

[0068] The embodiment of the present application further provides a middle frame 100 manufactured by using a part or all of the manufacturing method of the middle frame 100 of the embodiment described above. Figure 3As shown, the middle frame 100 has an appearance surface 110 and a functional screen-attaching surface 120. The display screen is attached to the functional screen-attaching surface 120. The appearance surface 110 has groove structures 111 arranged at intervals.

[0069] The embodiment of the present application also proposes an electronic device, including a middle frame 100. The specific structure of the middle frame 100 refers to the above embodiment. Since the middle frame 100 adopts all the technical solutions of all the above embodiments, it at least has all the beneficial effects brought by the technical solutions of the above embodiments, which will not be repeated here. In the embodiment, the electronic device can be a mobile phone, a tablet, a TV, an all-in-one commercial display machine, a smart education machine, etc.

[0070] The above description is only an optional embodiment of the present application, and does not limit the patent scope of the present application. All equivalent structural changes made by using the contents of the present application specification and drawings under the application concept of the present application, or directly / indirectly applied in other related technical fields are included in the patent protection scope of the present application.

Claims

1. A method for manufacturing a middle frame, characterized in that: include: A rough-machined profile having a groove structure on the exterior surface is produced by using a mold; According to the required shape and size of the middle frame, the rough-processed profile is made into an intermediate profile; Performing sandblasting on the exterior surface of the intermediate profile to obtain a sandblasted intermediate profile; Performing wire drawing on the appearance surface of the sandblasted intermediate profile to obtain a wire drawing intermediate profile; The intermediate profile after the wire drawing process is post-processed to obtain a middle frame.

2. The method for manufacturing the middle frame according to claim 1, characterized in that: The post-processing of the intermediate profile after the wire drawing process comprises: The inner surface of the groove structure of the intermediate profile after the wire drawing process is subjected to inkjet printing decoration process.

3. The method for manufacturing the middle frame according to claim 2, characterized in that: The post-processing of the intermediate profile after the wire drawing process further comprises: Before the inner surface of the groove structure of the intermediate profile after the wire drawing process is processed by the inkjet printing device, the surface of the intermediate profile after the wire drawing process is anodized.

4. The method for manufacturing the middle frame according to claim 3, characterized in that: The post-processing of the intermediate profile after the wire drawing process further comprises: Before the inner surface of the groove structure of the intermediate profile after the wire drawing process is processed by the inkjet printing device, after the surface of the intermediate profile after the wire drawing process is anodized, the inner surface of the groove structure of the intermediate profile after the wire drawing process is plasma treated.

5. The method for manufacturing the middle frame according to any one of claims 2 to 4, characterized in that: While the inner surface of the groove structure of the intermediate profile after the wire drawing process is subjected to inkjet printing decoration treatment, the ink on the intermediate profile after the wire drawing process is cured.

6. The method for manufacturing the middle frame according to claim 1, characterized in that: The number of the groove structures is multiple; wherein the depth of the groove structure is 0.5 to 0.8 mm; the width of the bottom groove wall of the groove structure is 0.7-1.0 mm; and the width of the convex surface connecting two adjacent groove structures is 1.0-2.0 mm.

7. The method for manufacturing the middle frame according to claim 1, characterized in that: The step of manufacturing the rough-processed profile into an intermediate profile according to the required shape and required size of the middle frame comprises: Straightening the rough-machined profile; The straightened rough-processed profile is placed in an aging furnace and heated to a preset temperature, and kept at the temperature for a preset time to obtain a heat-treated rough-processed profile; Performing surface treatment on the rough-machined profile after the heat treatment to obtain the rough-machined profile after the surface treatment; The rough-processed profile after surface treatment is manufactured into an intermediate profile according to the required shape and size of the middle frame.

8. The method for manufacturing the middle frame according to claim 1, characterized in that: After using a mold to produce a rough-machined profile with a groove structure on its exterior surface, before producing the rough-machined profile into an intermediate profile according to the required shape and required size of the middle frame, the production method also includes: quenching the rough-machined profile taken out of the mold so that the rough-machined profile is in T5 or T6 state.

9. A middle frame manufactured by the method for manufacturing a middle frame according to any one of claims 1 to 8.

10. An electronic device, characterized in that: Includes the middle frame described in claim 9.