Environment-friendly methanol fuel and preparation method thereof

By adding components such as ammonia, low-carbon alcohol, hydrogen peroxide and composite nanoparticles to methanol fuel, the problems of difficult cold start and insufficient combustion of methanol fuel are solved, and its calorific value, octane number and environmental performance are improved. Achieving more complete combustion and reducing pollutant emissions.

CN118725923AInactive Publication Date: 2024-10-01ORUILICHUANG (SHAANXI) BIOTECHNOLOGY CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411076288.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-07
Publication Date
2024-10-01
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Methanol fuel has problems such as difficulty in cold starting, low calorific value, low octane number, and incomplete combustion during the use of automotive fuel, which affects its application efficiency and environmental performance.

Method used

Pretreated multi-walled carbon nanotubes and potassium sodium tartrate are added to the copper sulfate aqueous solution as chelating agents, the pH is adjusted with sodium hydroxide, and oxidized in oxygen to obtain multi-walled carbon nanotubes-copper oxide nanomaterials, which are then passed through Cetyltrimethylammonium bromide assists Ce(NO3)3·6H2O, Y(NO3)3·6H2O, Mn (NO3)2 is dispersed, ammonium carbonate and ammonia are added, left to stand and calcined to obtain manganese- and yttrium-doped multi-walled carbon nanotubes-copper oxide-cerium oxide composite nanoparticles, combined with levulinic acid and ethanol esterification reaction, A bifunctional additive is formed, and finally components such as methanol, ammonia, low-carbon alcohol, hydrogen peroxide, and composite nanoparticles are mixed to prepare environmentally friendly methanol fuel.

Benefits of technology

It improves the ignition time, stability, octane number, oxidation resistance and lubricity of methanol fuel, promotes the complete combustion of methanol, reduces pollutant emissions, and improves the environmental protection and performance of the fuel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118725923A_ABST
    Figure CN118725923A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of energy and chemical industry, and discloses an environment-friendly methanol fuel and a preparation method thereof. The environment-friendly methanol fuel is prepared from the following components in parts by weight: 100 to 150 parts of methanol, 30 to 40 parts of ammonia water, 10 to 18 parts of low-carbon alcohol, 15 to 25 parts of hydrogen peroxide, 6 to 10 parts of composite nanoparticles, 1.5 to 5.5 parts of an anti-freezing agent, 2.5 to 8.5 parts of a preservative, 2.0 to 3.5 parts of ethylene glycol monobutyl ether, 1.8 to 3.6 parts of ethyl tert-butyl ether, 5 to 11.5 parts of sweet orange peel oil, 2 to 4.5 parts of catechol and 3.5 to 6.5 parts of a difunctional aid. The environment-friendly methanol fuel disclosed by the invention can be combusted more sufficiently in the use process, and has good stability, octane number, oxidation resistance and lubricity.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of energy chemical industry, and in particular to an environmentally friendly methanol fuel and a preparation method thereof. Background Art

[0002] Methanol fuel is a new type of fuel system that uses methanol as fuel. Methanol is a colorless, toxic, flammable liquid that can be prepared by chemical synthesis or biological fermentation. Compared with traditional fuels, methanol fuel has the following advantages: 1) Methanol is a renewable fuel that can be prepared by biological fermentation and other methods, and has high sustainability; 2) The combustion products of methanol are mainly carbon dioxide and water, with less harmful gases emitted and less pollution to the environment; 3) Methanol has high combustion energy and can provide higher power output and combustion efficiency; 4) Methanol has stable physical properties and is easy to store and transport. Methanol fuel has been widely used in automobiles, ships, generators and other fields. At the same time, with the enhancement of environmental awareness and changes in energy demand, methanol fuel will also be more widely used and developed in the future. However, when methanol fuel is used as automobile fuel, it has problems such as difficulty in cold start, low calorific value, low octane number, and incomplete combustion. Summary of the invention

[0003] In order to solve the above technical problems, the present invention provides a method for preparing an environmentally friendly methanol fuel, comprising the following steps:

[0004] Step (1) adding pretreated multi-walled carbon nanotubes to a copper sulfate aqueous solution, using potassium sodium tartrate as a chelating agent, adjusting the pH of the mixed solution with sodium hydroxide, then adding formaldehyde aqueous solution to react, and then oxidizing in oxygen to obtain a multi-walled carbon nanotube-copper oxide nanomaterial;

[0005] In the above process, copper oxide nanoparticles are deposited on the multi-walled carbon nanotubes to obtain multi-walled carbon nanotube-copper oxide nanomaterials.

[0006] Step (2) Ce(NO 3 ) 3 6H 2 O、Y(NO 3 ) 3 6H 2 O、Mn(NO 3 ) 2 Dispersing in deionized water, adding multi-walled carbon nanotube-copper oxide nanomaterials, dropping ammonium carbonate and ammonia water, standing, filtering, washing, drying, and calcining to obtain composite nanoparticles;

[0007] In the above process, the composite nanoparticles of multi-walled carbon nanotubes-copper oxide-cerium oxide doped with manganese and yttrium were obtained by assisting the impregnation with hexadecyltrimethylammonium bromide.

[0008] Step (3) using levulinic acid and ethanol as reactants and p-toluenesulfonic acid as a catalyst, and performing a reflux reaction to obtain ethyl levulinate; then using ethyl levulinate and N-phenyl-p-phenylenediamine as reactants and p-toluenesulfonic acid as a catalyst, and continuing the reflux reaction to obtain a bifunctional auxiliary agent;

[0009] In the above process, levulinic acid and ethanol undergo esterification reaction to obtain ethyl levulinate; C=O of ethyl levulinate reacts with the amino group of N-phenyl-p-phenylenediamine to obtain a bifunctional auxiliary agent.

[0010] Step (4) at room temperature and pressure, firstly mix methanol and ammonia water and stir until they are uniform, then add low-carbon alcohol, continue stirring, and then add hydrogen peroxide, composite nanoparticles, antifreeze, preservative, ethylene glycol monobutyl ether, ethyl tert-butyl ether, sweet orange peel oil, catechol, and bifunctional additives, stir until they are uniform, and obtain environmentally friendly methanol fuel.

[0011] In the above environmentally friendly methanol fuels: ammonia water can be converted into nitrogen dioxide under the catalytic action of composite nanoparticles, and nitrogen dioxide can promote the ignition of methanol and shorten the ignition delay time; low-carbon alcohols can increase the combustion calorific value of methanol, improve low-temperature performance, and improve cold start problems; hydrogen peroxide can shorten the ignition delay time; copper oxide and cerium oxide in composite nanoparticles can not only be used as catalysts for methanol combustion, but cerium oxide can also be used as a catalyst for the catalytic conversion of ammonia water. At the same time, copper oxide can also play a lubricating role in methanol fuel; multi-walled carbon nanotubes in composite nanoparticles can improve the lubricity of methanol fuel; composite nanoparticles are synthesized through The addition of hexadecyltrimethylammonium bromide can improve the dispersibility of composite nanoparticles in methanol fuel; ethylene glycol monobutyl ether as a cosolvent can improve the dispersibility of each component in the fuel; ethyl tert-butyl ether can improve the anti-knock property and octane number of methanol fuel; sweet orange peel oil as a natural additive can improve the octane number of methanol fuel; catechol as a natural antioxidant additive can improve the stability and antioxidant property of methanol fuel; bifunctional additives can not only improve the antioxidant property of methanol fuel, but also have a good lubricating effect; preservatives can prevent methanol fuel from corroding the automobile engine system; antifreeze can improve the low-temperature resistance of methanol fuel.

[0012] Preferably, in step (1), the preparation method of the pretreated multi-walled carbon nanotubes is as follows: the multi-walled carbon nanotubes are heat treated at 400-450°C for 30-40 min, then washed with acetone, then treated with 30-33 vol% HCl acid for 15-25 min, and finally treated with HNO 3 / H 2SO 4 The mixed solution is treated with acid at 60-80° C. for 20-40 minutes and then washed with deionized water to obtain pretreated multi-walled carbon nanotubes.

[0013] Preferably, in step (1), the copper sulfate aqueous solution is obtained by mixing anhydrous copper sulfate and deionized water in a mass ratio of 3.5:100-150; the pH of the mixed solution is adjusted to 12-12.5 with sodium hydroxide; the oxidation conditions are: oxidation in oxygen at 140-160° C. for 60-90 min; the amount ratio of copper sulfate, pretreated multi-walled carbon nanotubes, potassium sodium tartrate, and formaldehyde aqueous solution is 35-75 kg: 0.9-1.8 kg: 170-340 kg: 200-400 L.

[0014] Preferably, in step (2), Ce(NO 3 ) 3 6H 2 O、Y(NO 3 ) 3 6H 2 O、Mn(NO 3 ) 2 The mass ratio of hexadecyltrimethylammonium bromide and multi-walled carbon nanotube-copper oxide nanomaterials is 2.7-2.9:0.18-0.26:0.13-0.2:3.1-3.3:10.3-15.5; the pH is maintained at 8.2-8.7 during the addition of ammonium carbonate and ammonia water; and the standing time is 10-14 hours.

[0015] Preferably, in step (2), the drying conditions are: drying at 60-80°C for 20-30h; the calcination conditions are: first calcining at 550-600°C for 3-4h, and then calcining at 700-800°C for 18-24h.

[0016] Preferably, in step (3), the mass ratio of levulinic acid, ethanol and p-toluenesulfonic acid is 11.6-17.4:5.2-10.5:3.2-3.8; the reflux reaction conditions of levulinic acid and ethanol are: reflux reaction at 190-210° C. for 5.5-6.5 h.

[0017] Preferably, in the step (3), the mass ratio of ethyl levulinate, N-phenyl-p-phenylenediamine and p-toluenesulfonic acid is 14.4-28.8:22.1-45:4.5-6.5; the reflux reaction conditions of ethyl levulinate and N-phenyl-p-phenylenediamine are: reflux reaction at 190-210° C. for 7-9 hours.

[0018] Preferably, in step (4), the content of each component is, by weight:

[0019] 100-150 parts of methanol, 30-40 parts of ammonia water, 10-18 parts of low-carbon alcohols, 15-25 parts of hydrogen peroxide, 6-10 parts of composite nanoparticles, 1.5-5.5 parts of antifreeze, 2.5-8.5 parts of preservatives, 2.0-3.5 parts of ethylene glycol monobutyl ether, 1.8-3.6 parts of ethyl tert-butyl ether, 5-11.5 parts of sweet orange peel oil, 2-4.5 parts of catechol, and 3.5-6.5 parts of bifunctional additives.

[0020] Preferably, in step (4), the preservative comprises methyl eugenol; and the low-carbon alcohol is obtained by mixing ethanol, propanol, glycerol and isobutanol in a mass ratio of 5:2:1:3.

[0021] The environmentally friendly methanol fuel is prepared by the method for preparing the environmentally friendly methanol fuel.

[0022] Compared with the prior art, the present invention has the following beneficial effects:

[0023] 1. The present invention improves the quality of methanol fuel, shortens the ignition time of methanol fuel, improves its stability, octane number, antioxidant property and lubricity, and at the same time, promotes the full combustion of methanol fuel, reduces the emission of pollutants, and is more environmentally friendly by adding ammonia water, low-carbon alcohol, hydrogen peroxide, composite nanoparticles, antifreeze, preservatives, ethylene glycol monobutyl ether, ethyl tert-butyl ether, sweet orange peel oil, catechol, bifunctional additives, etc. to methanol fuel.

[0024] 2. The composite nanoparticles in the present invention are composite nanoparticles of multi-walled carbon nanotubes-copper oxide-cerium oxide doped with manganese and yttrium. The components synergistically improve the lubricity of methanol fuel, shorten the ignition time, and promote the complete combustion of methanol. The doping of manganese and yttrium further improves the catalytic activity of the composite nanoparticles.

[0025] 3. The bifunctional additive of the present invention has excellent antioxidant and lubricating effects, and can cooperate with catechol and composite nanoparticles to better improve the antioxidant and lubricating properties of methanol fuel. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 This is a process flow chart of the preparation of the environmentally friendly methanol fuel of the present invention;

[0027] Figure 2 It is a comparison chart of the combustion value test of the environmentally friendly methanol fuel of Examples 1-3 and Comparative Examples 1-7 in the present invention;

[0028] Figure 3 It is a comparison chart of the friction coefficient test of the environmentally friendly methanol fuel of Examples 1-3 and Comparative Examples 1-7 in the present invention;

[0029] Figure 4 It is a schematic diagram of the synthesis of the bifunctional auxiliary agent of the present invention. DETAILED DESCRIPTION

[0030] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0031] Example 1

[0032] This embodiment discloses a method for preparing an environmentally friendly methanol fuel, comprising the following steps:

[0033] Step (1) The multi-walled carbon nanotubes were heat treated at 400°C for 30 min, washed with acetone, treated with 30 vol% HCl for 15 min, and finally treated with HNO 3 / H 2 SO 4 The mixed solution was treated with acid at 60°C for 20 minutes, and then washed with deionized water to obtain pretreated multi-walled carbon nanotubes; anhydrous copper sulfate was dissolved in deionized water at a mass ratio of 3.5:100, and ultrasonically treated for 30 minutes at 30KHz, and then the pretreated multi-walled carbon nanotubes and potassium sodium tartrate were added, and the pH of the mixed solution was adjusted to 12 with sodium hydroxide, and then 37wt% formaldehyde aqueous solution was added under 30KHz ultrasonic conditions, and the ultrasonic treatment was continued for 30 minutes. After the reaction was completed, the reaction product was washed with deionized water, and then oxidized in oxygen at 140°C for 60 minutes to obtain multi-walled carbon nanotube-copper oxide nanomaterials; wherein the amount ratio of anhydrous copper sulfate, pretreated multi-walled carbon nanotubes, potassium sodium tartrate, and formaldehyde aqueous solution was 35kg:0.9kg:170kg:200L.

[0034] Step (2) 2.7 kg Ce(NO 3 ) 3 6H 2 O, 0.18kg Y(NO 3 ) 3 6H 2 O, 0.13kg Mn(NO 3 ) 2, 3.1 kg of hexadecyltrimethylammonium bromide was dispersed in deionized water, stirred at a speed of 200 r / min, and then 10.3 kg of multi-walled carbon nanotube-copper oxide nanomaterial was added, and stirring was continued. During the stirring process, excess ammonium carbonate and ammonia water were added dropwise, and the pH was kept at 8.2 during the addition process. After the addition was completed, it was allowed to stand for 10 hours, filtered, and the filter residue was washed with distilled water until the pH value of the washing liquid remained unchanged. It was first dried at 60°C for 20 hours, then calcined at 550°C for 3 hours, and finally calcined at 700°C for 18 hours to obtain composite nanoparticles.

[0035] Step (3) 11.6 kg of levulinic acid and 5.2 kg of ethanol are mixed, and then 3.2 kg of p-toluenesulfonic acid is added, and the mixture is refluxed at 190° C. for 5.5 h. After the reaction is completed, excess ethanol is removed by rotary evaporation, and the reaction product is washed with deionized water and ethyl acetate to obtain an organic layer, and the ethyl acetate in the organic layer is removed by rotary evaporation to obtain ethyl levulinate; 14.4 kg of ethyl levulinate and 22.1 kg of N-phenyl-p-phenylenediamine are added to a sufficient amount of ethanol, and then 4.5 kg of p-toluenesulfonic acid is added, and the mixture is refluxed at 190° C. for 7 h. After the reaction is completed, the ethanol is removed by rotary evaporation, and the reaction product is washed with deionized water and ethyl acetate to obtain a bifunctional auxiliary agent.

[0036] Step (4) at room temperature and pressure, firstly mix 100 kg of methanol and 30 kg of ammonia water and stir until uniform, then add 10 kg of low-carbon alcohol, continue stirring, then add 15 kg of hydrogen peroxide, 6 kg of composite nanoparticles, 1.5 kg of antifreeze, 2.5 kg of methyl eugenol, 2.0 kg of ethylene glycol monobutyl ether, 1.8 kg of ethyl tert-butyl ether, 5 kg of sweet orange peel oil, 2 kg of catechol, and 3.5 kg of bifunctional additives, stir until uniform, and obtain environmentally friendly methanol fuel; wherein the low-carbon alcohol is obtained by mixing ethanol, propanol, glycerol and isobutanol in a mass ratio of 5:2:1:3.

[0037] Example 2

[0038] This embodiment discloses a method for preparing an environmentally friendly methanol fuel, comprising the following steps:

[0039] Step (1) The multi-walled carbon nanotubes were heat treated at 450°C for 40 min, washed with acetone, treated with 33 vol% HCl for 25 min, and finally treated with HNO 3 / H 2 SO 4The mixed solution was treated with acid at 80°C for 40 minutes, and then washed with deionized water to obtain pretreated multi-walled carbon nanotubes; anhydrous copper sulfate was dissolved in deionized water at a mass ratio of 3.5:150, and ultrasonically treated for 60 minutes at 40KHz, and then the pretreated multi-walled carbon nanotubes and potassium sodium tartrate were added, and the pH of the mixed solution was adjusted to 12.5 with sodium hydroxide, and then a 37wt% formaldehyde aqueous solution was added under 40KHz ultrasonic conditions, and the ultrasonic treatment was continued for 60 minutes. After the reaction was completed, the reaction product was washed with deionized water, and then oxidized in oxygen at 160°C for 90 minutes to obtain a multi-walled carbon nanotube-copper oxide nanomaterial; wherein the amount ratio of anhydrous copper sulfate, pretreated multi-walled carbon nanotubes, potassium sodium tartrate, and formaldehyde aqueous solution was 75kg:1.8kg:340kg:400L.

[0040] Step (2) 2.9 kg Ce(NO 3 ) 3 6H 2 O, 0.26kg Y(NO 3 ) 3 6H 2 O, 0.2kg Mn(NO 3 ) 2 , 3.3 kg of hexadecyltrimethylammonium bromide was dispersed in deionized water, stirred at a speed of 400 r / min, and then 15.5 kg of multi-walled carbon nanotube-copper oxide nanomaterial was added, and stirring was continued. During the stirring process, excess ammonium carbonate and ammonia water were added dropwise, and the pH was kept at 8.7 during the addition process. After the addition was completed, it was allowed to stand for 14 hours, filtered, and the filter residue was washed with distilled water until the pH value of the washing liquid remained unchanged. It was first dried at 80°C for 30 hours, then calcined at 600°C for 4 hours, and finally calcined at 800°C for 24 hours to obtain composite nanoparticles.

[0041] Step (3) 17.4 kg of levulinic acid and 10.5 kg of ethanol are mixed, and then 3.8 kg of p-toluenesulfonic acid is added, and the mixture is refluxed at 210° C. for 6.5 h. After the reaction is completed, excess ethanol is removed by rotary evaporation, and the reaction product is washed with deionized water and ethyl acetate to obtain an organic layer, and the ethyl acetate in the organic layer is removed by rotary evaporation to obtain ethyl levulinate; 28.8 kg of ethyl levulinate and 45 kg of N-phenyl-p-phenylenediamine are added to a sufficient amount of ethanol, and then 6.5 kg of p-toluenesulfonic acid is added, and the mixture is refluxed at 210° C. for 9 h. After the reaction is completed, the ethanol is removed by rotary evaporation, and the reaction product is washed with deionized water and ethyl acetate to obtain a bifunctional auxiliary agent.

[0042] Step (4) at room temperature and pressure, firstly mix 150kg of methanol and 40kg of ammonia water and stir until uniform, then add 18kg of low-carbon alcohol, continue stirring, then add 25kg of hydrogen peroxide, 10kg of composite nanoparticles, 5.5kg of antifreeze, 8.5kg of methyl eugenol, 3.5kg of ethylene glycol monobutyl ether, 3.6kg of ethyl tert-butyl ether, 11.5kg of sweet orange peel oil, 4.5kg of catechol, and 6.5kg of bifunctional additives, stir until uniform, and obtain environmentally friendly methanol fuel.

[0043] Example 3

[0044] This embodiment discloses a method for preparing an environmentally friendly methanol fuel, comprising the following steps:

[0045] Step (1) The multi-walled carbon nanotubes were heat treated at 420°C for 35 min, washed with acetone, treated with 31.5 vol% HCl acid for 20 min, and finally treated with HNO 3 / H 2 SO 4 The mixed solution was treated with acid at 70°C for 30 minutes, and then washed with deionized water to obtain pretreated multi-walled carbon nanotubes; anhydrous copper sulfate was dissolved in deionized water at a mass ratio of 3.5:125, and ultrasonically treated at 35KHz for 45 minutes, and then the pretreated multi-walled carbon nanotubes and potassium sodium tartrate were added, and the pH of the mixed solution was adjusted to 12.2 with sodium hydroxide, and then a 37wt% formaldehyde aqueous solution was added under 35KHz ultrasonic conditions, and the ultrasonic treatment was continued for 45 minutes. After the reaction was completed, the reaction product was washed with deionized water, and then oxidized in oxygen at 150°C for 75 minutes to obtain multi-walled carbon nanotube-copper oxide nanomaterials; wherein the amount ratio of anhydrous copper sulfate, pretreated multi-walled carbon nanotubes, potassium sodium tartrate, and formaldehyde aqueous solution was 55kg:1.3kg:205kg:300L.

[0046] Step (2) 2.8 kg Ce(NO 3 ) 3 6H 2 O, 0.22kg Y(NO 3 ) 3 6H 2 O, 0.16kg Mn(NO 3 ) 2, 3.2 kg of hexadecyltrimethylammonium bromide was dispersed in deionized water, stirred at a speed of 300 r / min, and then 12.9 kg of multi-walled carbon nanotube-copper oxide nanomaterial was added, and stirring was continued. During the stirring process, excess ammonium carbonate and ammonia water were added dropwise, and the pH was kept at 8.5 during the addition process. After the addition was completed, it was allowed to stand for 12 hours, filtered, and the filter residue was washed with distilled water until the pH value of the washing liquid remained unchanged. It was first dried at 70°C for 25 hours, and then calcined at 575°C for 3.5 hours, and finally calcined at 750°C for 21 hours to obtain composite nanoparticles.

[0047] Step (3) 14.5 kg of levulinic acid and 7.4 kg of ethanol are mixed, and then 3.5 kg of p-toluenesulfonic acid is added, and the mixture is refluxed at 200° C. for 6 h. After the reaction is completed, excess ethanol is removed by rotary evaporation, and the reaction product is washed with deionized water and ethyl acetate to obtain an organic layer, and the ethyl acetate in the organic layer is removed by rotary evaporation to obtain ethyl levulinate; 21.6 kg of ethyl levulinate and 33.5 kg of N-phenyl-p-phenylenediamine are added to a sufficient amount of ethanol, and then 5.5 kg of p-toluenesulfonic acid is added, and the mixture is refluxed at 200° C. for 8 h. After the reaction is completed, the ethanol is removed by rotary evaporation, and the reaction product is washed with deionized water and ethyl acetate to obtain a bifunctional auxiliary agent.

[0048] Step (4) at room temperature and pressure, firstly mix 125kg of methanol and 35kg of ammonia water and stir until uniform, then add 14kg of low-carbon alcohol, continue stirring, then add 20kg of hydrogen peroxide, 8kg of composite nanoparticles, 3.5kg of antifreeze, 5.5kg of methyl eugenol, 2.7kg of ethylene glycol monobutyl ether, 2.7kg of ethyl tert-butyl ether, 8.2kg of sweet orange peel oil, 3.2kg of catechol, and 5kg of bifunctional additive, stir until uniform, and obtain environmentally friendly methanol fuel.

[0049] Comparative Example 1

[0050] Comparative Example 1 Compared with Example 3, no bifunctional additive is added to the environmentally friendly methanol fuel in Comparative Example 1, and other conditions remain unchanged.

[0051] Comparative Example 2

[0052] Comparative Example 2 Compared with Example 3, no composite nanoparticles are added to the environmentally friendly methanol fuel in Comparative Example 2, and other conditions remain unchanged.

[0053] Comparative Example 3

[0054] Comparative Example 3 Compared with Example 3, in Comparative Example 3, Y(NO 3 ) 3 6H 2 O, other conditions remain unchanged.

[0055] Comparative Example 4

[0056] Comparative Example 4 Compared with Example 3, in Comparative Example 4, no Mn(NO) was added during the preparation of the composite nanoparticles. 3 ) 2 , other conditions remain unchanged.

[0057] Comparative Example 5

[0058] Comparative Example 5 Compared with Example 3, in Comparative Example 5, hexadecyltrimethylammonium bromide was not added during the preparation of the composite nanoparticles, and other conditions remained unchanged.

[0059] Comparative Example 6

[0060] Comparative Example 6 Compared with Example 3, in Comparative Example 6, Ce (NO 3 ) 3 6H 2 O, other conditions remain unchanged.

[0061] Comparative Example 7

[0062] Comparative Example 7 Compared with Example 3, in Comparative Example 7, pretreated multi-walled carbon nanotubes are used instead of multi-walled carbon nanotube-copper oxide nanomaterials during the preparation of composite nanoparticles, and other conditions remain unchanged.

[0063] In the above embodiments and comparative examples, the multi-walled carbon nanotubes are fibrous in shape, with an average fiber length of 8 μm and an average fiber diameter of 150 nm, and are from Shanghai Waidian International Trading Co., Ltd.

[0064] Experimental example

[0065] 1. Lubrication performance test: Referring to the method in "Lubricating oil friction coefficient determination method (four-ball method)" SH / T0762-2005, the friction coefficient of the environmentally friendly methanol fuel of Examples 1-3 and Comparative Examples 1-7 was tested. The test results are shown in Table 1:

[0066] Table 1

[0067]

[0068] From the test results in Table 1, it can be seen that the environmentally friendly methanol fuels prepared in Examples 1-7 of the present invention have excellent lubricity. From the comparison between Comparative Examples 1 and 2 and Example 3, it can be seen that the addition of bifunctional additives and composite nanoparticles helps to improve the lubricity of methanol fuel; from the comparison between Comparative Example 5 and Example 3, it can be seen that the composite nanoparticles prepared with the assistance of hexadecyltrimethylammonium bromide improve the lubricity of methanol fuel by improving the dispersibility of the composite nanoparticles in methanol fuel; from the comparison between Comparative Examples 6 and 7 and Example 3, it can be seen that the components of copper oxide and cerium oxide in the composite nanoparticles have a positive effect on improving the lubricity of methanol fuel.

[0069] 2. Combustion sufficiency test: According to the national standard GB 16663-1996 "Alcohol-based liquid fuel", the combustion value and stability of the environmentally friendly methanol fuel of Examples 1-3 and Comparative Examples 1-7 were tested. The test results are shown in Table 2:

[0070] Table 2

[0071]

[0072] From the test results in Table 2, it can be seen that the environmentally friendly methanol fuel prepared by Examples 1-7 of the present invention can burn more fully. From the comparison of Comparative Examples 1 and 2 with Example 3, it can be seen that the addition of bifunctional additives and composite nanoparticles can promote the combustion of methanol fuel; from the comparison of Comparative Examples 3, 4, 6, and 7 with Example 3, it can be seen that the components of copper oxide and cerium oxide in the composite nanoparticles and the doping of manganese and yttrium are all conducive to the full combustion of methanol fuel; from the comparison of Comparative Example 5 with Example 3, it can be seen that the composite nanoparticles prepared with the assistance of hexadecyltrimethylammonium bromide can further improve the combustion completeness of methanol fuel.

[0073] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A method for preparing environmentally friendly methanol fuel, It is characterized in that The following steps are involved: Step (1) adding pretreated multi-walled carbon nanotubes to a copper sulfate aqueous solution, using potassium sodium tartrate as a chelating agent, adjusting the pH of the mixed solution with sodium hydroxide, then adding formaldehyde aqueous solution to react, and then oxidizing in oxygen to obtain a multi-walled carbon nanotube-copper oxide nanomaterial; Step (2) Ce(NO 3 ) 3 6H 2 O、Y(NO 3 ) 3 6H 2 O、Mn(NO 3 ) 2 Dispersing in deionized water, adding multi-walled carbon nanotube-copper oxide nanomaterials, dropping ammonium carbonate and ammonia water, standing, filtering, washing, drying, and calcining to obtain composite nanoparticles; Step (3) using levulinic acid and ethanol as reactants and p-toluenesulfonic acid as a catalyst, and performing a reflux reaction to obtain ethyl levulinate; then using ethyl levulinate and N-phenyl-p-phenylenediamine as reactants and p-toluenesulfonic acid as a catalyst, and continuing the reflux reaction to obtain a bifunctional auxiliary agent; Step (4) at room temperature and pressure, firstly mix methanol and ammonia water and stir until they are uniform, then add low-carbon alcohol, continue stirring, and then add hydrogen peroxide, composite nanoparticles, antifreeze, preservative, ethylene glycol monobutyl ether, ethyl tert-butyl ether, sweet orange peel oil, catechol, and bifunctional additives, stir until they are uniform, and obtain environmentally friendly methanol fuel.

2. The method for preparing the environmentally friendly methanol fuel according to claim 1, It is characterized in that In the step (1), the preparation method of the pretreated multi-walled carbon nanotubes is as follows: the multi-walled carbon nanotubes are heat treated at 400-450°C for 30-40 minutes, then washed with acetone, then treated with 30-33 vol% HCl acid for 15-25 minutes, and finally treated with HNO 3 / H 2 SO 4 The mixed solution is treated with acid at 60-80° C. for 20-40 minutes and then washed with deionized water to obtain pretreated multi-walled carbon nanotubes.

3. The method for preparing the environmentally friendly methanol fuel according to claim 1, It is characterized in that In the step (1), the copper sulfate aqueous solution is obtained by mixing anhydrous copper sulfate and deionized water in a mass ratio of 3.5:100-150; the pH of the mixed solution is adjusted to 12-12.5 with sodium hydroxide; the oxidation conditions are: oxidation in oxygen at 140-160° C. for 60-90 min; the amount ratio of copper sulfate, pretreated multi-walled carbon nanotubes, potassium sodium tartrate, and formaldehyde aqueous solution is 35-75 kg: 0.9-1.8 kg: 170-340 kg: 200-400 L.

4. The method for preparing the environmentally friendly methanol fuel according to claim 1, It is characterized in that In the step (2), Ce(NO 3 ) 3 6H 2 O、Y(NO 3 ) 3 6H 2 O、Mn(NO 3 ) 2 The mass ratio of hexadecyltrimethylammonium bromide and multi-walled carbon nanotube-copper oxide nanomaterials is 2.7-2.9:0.18-0.26:0.13-0.2:3.1-3.3:10.3-15.5; the pH is maintained at 8.2-8.7 during the addition of ammonium carbonate and ammonia water; and the standing time is 10-14 hours.

5. The method for preparing the environmentally friendly methanol fuel according to claim 1, It is characterized in that In the step (2), the drying conditions are: drying at 60-80°C for 20-30h; the calcination conditions are: first calcining at 550-600°C for 3-4h, and then calcining at 700-800°C for 18-24h.

6. The method for preparing the environmentally friendly methanol fuel according to claim 1, It is characterized in that In the step (3), the mass ratio of levulinic acid, ethanol and p-toluenesulfonic acid is 11.6-17.4:5.2-10.5:3.2-3.8; the reflux reaction conditions of levulinic acid and ethanol are: reflux reaction at 190-210° C. for 5.5-6.5 hours.

7. The method for preparing the environmentally friendly methanol fuel according to claim 1, It is characterized in that In the step (3), the mass ratio of ethyl levulinate, N-phenyl-p-phenylenediamine and p-toluenesulfonic acid is 14.4-28.8:22.1-45:4.5-6.5; the reflux reaction conditions of ethyl levulinate and N-phenyl-p-phenylenediamine are: reflux reaction at 190-210° C. for 7-9 hours.

8. The method for preparing the environmentally friendly methanol fuel according to claim 1, It is characterized in that In the step (4), the contents of the components are, by weight, 100-150 parts of methanol, 30-40 parts of ammonia water, 10-18 parts of low-carbon alcohols, 15-25 parts of hydrogen peroxide, 6-10 parts of composite nanoparticles, 1.5-5.5 parts of antifreeze, 2.5-8.5 parts of preservative, 2.0-3.5 parts of ethylene glycol monobutyl ether, 1.8-3.6 parts of ethyl tert-butyl ether, 5-11.5 parts of sweet orange peel oil, 2-4.5 parts of catechol, and 3.5-6.5 parts of a bifunctional additive.

9. The method for preparing the environmentally friendly methanol fuel according to claim 1, It is characterized in that In the step (4), the preservative includes methyl eugenol; and the low-carbon alcohol is obtained by mixing ethanol, propanol, glycerol and isobutanol in a mass ratio of 5:2:1:

3.

10. An environmentally friendly methanol fuel prepared by the method according to any one of claims 1 to 9.

Citation Information

Cited By

  • Combustion aid suitable for methanol fuel as well as preparation method and application of combustion aid

    CN122563636A