Electric field assisted crystal growth device and method
By introducing electric field-assisted technology into the silicon carbide crystal growth device, the electric field is used to ionize and evenly distribute the silicon carbide atmosphere in the lifting zone, solving the defect problem caused by uneven gas phase distribution in the traditional process and improving the crystal quality and growth rate.
Patent Information
- Application Number
- CN202410849749.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-27
- Publication Date
- 2024-10-01
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In the traditional silicon carbide crystal growth process, silicon carbide gas phase components easily form defects during the nucleation and deposition process in the growing crystal region due to uneven distribution of the atmosphere.
Design an electric field-assisted crystal growth device. By setting a cathode plate above the lifting zone and an anode plate below, a uniform electric field is formed to ionize the silicon carbide atmosphere and transport it to the crystal growth zone under the action of electric field force and temperature gradient. Uniform distribution of gas phase.
Through electric field-assisted technology, the quality of silicon carbide crystals is significantly improved, ensuring a more uniform distribution of the gas phase in the radial direction, thereby reducing crystal defects and improving the rate and quality of crystal growth.
Smart Images

Figure CN118727153A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductors, and in particular to an electric field assisted crystal growth device and method. Background Art
[0002] PVT physical vapor transport is a material synthesis technology used to grow high-quality crystals, especially for growing wide-bandgap semiconductor materials such as silicon carbide (SiC) and gallium nitride (GaN). The PVT method uses the process of material sublimation and condensation at high temperature to control the growth of crystals.
[0003] In the traditional silicon carbide crystal growth process, a method of heating silicon carbide powder in a crystal growth furnace is generally used for crystal growth. Specifically, the crystal growth furnace is heated, and the silicon carbide powder is heated and sublimated into a gas state in the crystal growth furnace. At this time, the silicon carbide gas phase components are in a state of extremely disturbed molecules under a high temperature environment, and reach the crystal growth area in the crystal growth furnace to form silicon carbide crystals. However, in the process of nucleation and formation of silicon carbide crystals in the crystal growth area, the atmosphere distribution of the silicon carbide gas phase components in a disturbed state is uneven, which is easy to form defects. Summary of the invention
[0004] The objectives of the present invention include, for example, providing an electric field assisted crystal growth device, which can transmit the atmosphere to the crystal growth area for deposition in a more uniform radial distribution through electric field assistance, thereby improving the quality of the crystal growth.
[0005] The embodiments of the present invention can be implemented as follows:
[0006] An electric field assisted crystal growth device, the electric field assisted crystal growth device comprising a crucible and a parallel plate capacitor;
[0007] The crucible is an insulating crucible, and the bottom of the crucible is a powder loading area for loading silicon carbide powder, the top of the crucible is a crystal growth area, and the area between the powder loading area and the crystal growth area is a sublimation area;
[0008] The parallel plate capacitor includes an anode plate and a cathode plate, wherein the anode plate is arranged below the rise zone, and the cathode plate is arranged above the rise zone. An electric field can be formed between the anode plate and the cathode plate to ionize the silicon carbide atmosphere in the rise zone to make it positively charged, and the charged silicon carbide atmosphere can be transmitted upward to the crystal growth zone for deposition under the combined action of the electric field force and the temperature gradient during the pre-growth stage and the main crystal growth stage.
[0009] In an optional embodiment, the anode plate is disposed on the outside of the crucible and is coaxial with the bottom wall of the crucible, and the cathode plate is disposed on the outside of the crucible and is coaxial with the top wall of the crucible.
[0010] In an optional embodiment, the anode plate and the cathode plate are graphite plates or metal plates.
[0011] In an optional embodiment, during the pre-growth stage, the potential difference between the anode plate and the cathode plate ranges from 400 V to 2000 V;
[0012] In the main crystal growth stage, the potential difference between the anode plate and the cathode plate ranges from 480V to 2400V;
[0013] The value of the potential difference between the anode plate and the cathode plate in the main crystal growth stage is greater than the value of the potential difference between the anode plate and the cathode plate in the pre-growth stage.
[0014] In an optional embodiment, the anode plate and the cathode plate are both arranged in the crucible, and the anode plate is arranged between the powder loading area and the rising area, and the cathode plate is arranged between the rising area and the crystal growth area, so that the electric field formed between the anode plate and the cathode plate is located in the rising area, and the anode plate and the cathode plate are both provided with corresponding and uniform flow holes, which allow the silicon carbide atmosphere to pass through
[0015] In the pre-growth stage, the potential difference between the anode plate and the cathode plate ranges from 100V to 500V, and in the main crystal growth stage, the potential difference between the anode plate and the cathode plate ranges from 120V to 600V, and the value of the potential difference between the anode plate and the cathode plate in the main crystal growth stage is greater than the value of the potential difference between the anode plate and the cathode plate in the pre-growth stage.
[0016] In an optional embodiment, the anode plate is arranged in the crucible and is located between the powder loading zone and the rising zone, and the cathode plate is arranged above the crystal growth zone, so that the electric field formed between the anode plate and the cathode plate is located in the rising zone and the crystal growth zone, and the anode plate is provided with a flow hole, so that the silicon carbide atmosphere can enter the rising zone through the flow hole;
[0017] In the pre-growth stage, the potential difference between the anode plate and the cathode plate ranges from 200V to 1000V, and in the main crystal growth stage, the potential difference between the anode plate and the cathode plate ranges from 240V to 1200V, and the potential difference between the anode plate and the cathode plate in the main crystal growth stage is greater than the potential difference between the anode plate and the cathode plate in the pre-growth stage.
[0018] In an optional embodiment, the anode plate and the cathode plate are both graphite meshes.
[0019] In an optional embodiment, the crucible is made of boron nitride ceramic material.
[0020] In a second aspect, the present application further provides a crystal growth method, which is applied to the electric field assisted crystal growth device described in the above optional embodiment, and the method comprises:
[0021] S1, preheating treatment, heating the temperature in the crucible to a first preset temperature, and evacuating the crucible to make the pressure in the crucible reach a first preset pressure.
[0022] S2. In the pre-growth stage, the temperature in the crucible is maintained at a first preset temperature, the pressure is maintained at a first preset pressure, and a first preset potential difference is applied to the anode plate and the cathode plate, so that the ionized charged silicon carbide atmosphere is transmitted to the crystal growth area for deposition under the action of the electric field force, and maintained for a first preset time.
[0023] S3, in the main crystal growth stage, the pressure in the crucible is reduced to maintain the pressure in the crucible at a second preset pressure, an axial temperature gradient is formed inside the crucible, and the potential difference between the anode plate and the cathode plate is increased to maintain the potential difference at the second preset potential difference, so that the ionized charged silicon carbide atmosphere is transmitted to the crystal growth area for deposition under the combined action of the electric field force and the temperature gradient, and maintained for the second preset time.
[0024] S4, annealing stage, increasing the pressure in the crucible to maintain the pressure in the crucible at a third preset pressure, lowering the temperature in the crucible, and making the potential difference between the anode plate and the cathode plate 0, and maintaining it for a third preset time.
[0025] The first preset temperature ranges from 2000°C to 2300°C, and the first preset pressure ranges from 10 2 Up to 10 4 The first preset time ranges from 3h to 5h, the second preset pressure ranges from 1Pa to 3000Pa, the second preset time ranges from 50h to 200h, and the third preset pressure ranges from 10 2 Pa to 10 4 Pa, the third preset time ranges from 5h to 20h.
[0026] The beneficial effects of the electric field assisted crystal growth device and method provided by the embodiments of the present invention include, for example:
[0027] The present application sets a cathode plate above the sublimation zone and an anode plate below the sublimation zone. During the crystal growth process, a uniform electric field can be formed in the sublimation zone by using the anode plate and the cathode plate. Since the silicon carbide atmosphere is in a gaseous state, it is easier to ionize and lose electrons and become positively charged under high temperature conditions than the powder in the powder loading zone, so it is relatively easy to ionize and charge the molecules and atoms in the silicon carbide gas phase component. In a uniform electric field, positively charged molecules and atomic groups will be subject to vertically upward electric field forces. Compared with the case without external electric field assistance, the gas phase in the device of the present invention can be transmitted to the growth zone more quickly, and its horizontal displacement will be less constrained by the electric field force. Therefore, the radial distribution of the gas phase in the sublimation zone will be more uniform, thereby improving the crystal quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.
[0029] Figure 1 A schematic diagram of the structure of an electric field assisted crystal growth device provided in Example 1 of the present invention;
[0030] Figure 2 A schematic diagram of the structure of an electric field assisted crystal growth device provided in Example 2 of the present invention;
[0031] Figure 3 This is a schematic diagram of the structure of the electric field assisted crystal growth device provided in Example 3 of the present invention.
[0032] Icons: 100 - electric field assisted crystal growth device; 110 - crucible; 111 - powder loading area; 113 - rise zone; 115 - crystal growth area; 130 - parallel plate capacitor; 131 - anode plate; 133 - cathode plate; 135 - through hole. DETAILED DESCRIPTION
[0033] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.
[0034] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0035] It should be noted that, in the absence of conflict, the features in the embodiments of the present invention may be combined with each other.
[0036] Example
[0037] Please refer to Figure 1 This embodiment provides an electric field assisted crystal growth device 100, which can make the silicon carbide atmosphere more evenly distributed in the rise zone 113 under the action of electric field assistance, and can accelerate the rising speed of the silicon carbide atmosphere, thereby improving the crystal growth rate and quality.
[0038] In this embodiment, the electric field assisted crystal growth device 100 includes a crucible 110 and a parallel plate capacitor 130; the crucible 110 is an insulating crucible 110, and the bottom of the crucible 110 is a powder loading area 111 for loading silicon carbide powder, the top of the crucible 110 is a crystal growth area 115, and the area between the powder loading area 111 and the crystal growth area 115 is a rise zone 113;
[0039] The parallel plate capacitor 130 includes an anode plate 131 and a cathode plate 133. The anode plate 131 is arranged below the uplift zone 113, and the cathode plate 133 is arranged above the uplift zone 113. An electric field can be formed between the anode plate 131 and the cathode plate 133 to ionize the silicon carbide atmosphere in the uplift zone 113 and make it positively charged. The charged silicon carbide atmosphere can be transmitted upward to the crystal growth zone 115 for deposition under the combined action of the electric field force and the temperature gradient during the pre-growth stage and the main crystal growth stage.
[0040] By arranging a cathode plate 133 above the sublimation zone 113 and an anode plate 131 below the sublimation zone 113, a uniform electric field can be formed in the sublimation zone 113 by using the anode plate 131 and the cathode plate 133 during the crystal growth process. Since the silicon carbide atmosphere is in a gaseous state, it is easier to ionize and lose electrons and become positively charged under high temperature conditions than the powder in the powder loading zone 111, so it is relatively easy to ionize and charge the molecules and atoms in the silicon carbide gas phase component. In a uniform electric field, positively charged molecules and atomic groups will be subject to vertically upward electric field forces. Compared with the case without external electric field assistance, the gas phase in the device of the present invention can be transmitted to the growth zone more quickly, and its displacement in the horizontal direction will be less constrained by the electric field force. Therefore, the radial distribution of the gas phase in the sublimation zone 113 will be more uniform, thereby improving the crystal quality.
[0041] It should be noted that the electrons moving in the electric field knock out the electrons in the gas phase atoms or molecules to form positive ions and electrons. The electrons will move toward the anode plate 131, and the positively charged ions will move toward the cathode plate 133. In this way, the silicon carbide atmosphere can be affected by the electric field force and the temperature gradient at the same time, so that the silicon carbide atmosphere can be transmitted faster during the rising process, thereby accelerating the deposition speed.
[0042] Example 1
[0043] In this embodiment, the anode plate 131 is disposed below the powder loading area 111, and the cathode plate 133 is disposed above the crystal growth area 115. This facilitates the installation of the anode plate 131 and the cathode plate 133.
[0044] Please refer to Figure 1 In this embodiment, the anode plate 131 is disposed outside the crucible 110 and is coaxial with the bottom of the crucible 110, and the cathode plate 133 is disposed outside the crucible 110 and is coaxial with the top wall of the crucible 110. The installation of the anode plate 131 and the cathode plate 133 does not affect the internal space of the crucible 110.
[0045] In this embodiment, the anode plate 131 and the cathode plate 133 are both graphite plates, which are provided with electrodes. The graphite plates used as the anode plate 131 and the cathode plate 133 have high temperature resistance and high specific surface area, which can significantly increase the capacitance value of the capacitor. Good electrical conductivity can effectively reduce the equivalent series resistance of the capacitor and improve its high frequency response capability.
[0046] Of course, in some embodiments of the present application, the anode plate 131 and the cathode plate 133 are also made of one of the following materials: tantalum carbide has a melting point of about 3880°C, hafnium carbide has a melting point of about 3890°C, niobium carbide has a melting point of about 3640°C, zirconium carbide has a melting point of about 3500°C, titanium carbide has a melting point of about 3140°C, and tungsten has a melting point of about 3680°C, rhenium has a melting point of about 3440°C, and other metals.
[0047] In this embodiment, the crucible 110 is made of an insulating and high temperature resistant material, such as a boron nitride ceramic material. Since boron nitride ceramic materials are insulating and high temperature resistant, existing crystal growth is made of graphite. The reason why the present application does not use a graphite crucible 110 is that when the electric field enters the inside of the graphite crucible 110, the strength of the electric field may be affected by the conductivity of the graphite. The free electrons inside the graphite will respond to the electric field and may generate current, which will shield a portion of the electric field, reducing the penetration of the electric field inside the graphite.
[0048] In this embodiment, in the pre-growth stage, the potential difference between the anode plate 131 and the cathode plate 133 ranges from 400 V to 2000 V. In the main crystal growth stage, the potential difference between the anode plate 131 and the cathode plate 133 ranges from 480 V to 2400 V. The value of the potential difference between the anode plate 131 and the cathode plate 133 in the main crystal growth stage is greater than the value of the potential difference between the anode plate 131 and the cathode plate 133 in the pre-growth stage.
[0049] For example, in one embodiment, the potential difference between the anode plate 131 and the cathode plate 133 is 1200V in the pre-growth stage, and the potential difference between the anode plate 131 and the cathode plate 133 is 1600V in the main growth stage.
[0050] Example 2
[0051] Please refer to Figure 2 In the present embodiment, the anode plate 131 and the cathode plate 133 are arranged in the crucible 110, the anode plate 131 is arranged between the powder loading zone 111 and the rising zone 113, and the cathode plate 133 is arranged between the rising zone 113 and the crystal growth zone 115, so that the electric field formed between the anode plate 131 and the cathode plate 133 is located in the rising zone 113, and the two anode plates 131 and the cathode plate 133 are both provided with corresponding and uniform flow holes 135, and the flow holes 135 allow the silicon carbide atmosphere to pass through.
[0052] That is, the anode plate 131 and the cathode plate 133 divide the chamber in the crucible 110 into three parts. The lower part of the anode plate 131 is the powder loading area 111, the area between the anode plate 131 and the cathode plate 133 is the rising area 113, and the upper part of the cathode plate 133 is the crystal growth area 115.
[0053] The anode plate 131 and the cathode plate 133 are arranged in this way to provide an electric field only in the ascending zone 113, which can prevent the charged ions in the powder in the powder loading zone 111 from being transmitted upward under the action of the electric field force, thereby affecting the quality of the crystal growth. Most importantly, the electric field is arranged inside the crucible 110 and is located on the upper and lower sides of the ascending zone 113, so that the distance between the anode plate 131 and the cathode plate 133 is closer. When the same ionization field strength is achieved, the voltage difference required to be applied to the anode plate 131 and the cathode plate 133 will be reduced, which can reduce energy consumption and reduce the processing requirements of the anode plate 131 and the cathode plate 133. Secondly, the anode plate 131 and the cathode plate 133 are provided with flow holes 135 and 130, which can be used as flow equalizing plates, and can further improve the uniformity of the silicon carbide atmosphere in the crystal growth zone 115. Thus, the overall flow equalization effect of double charging is achieved.
[0054] Furthermore, the electric field assisted crystal growth device also includes a fixed frame, and the anode plate 131 and the cathode plate 133 are fixed at both ends of the fixed frame according to a preset distance, and a limiting ring is set on the side wall of the crucible 110 to support the fixed frame and the anode plate 131 and the cathode plate 133 to form a whole, so that the whole is suspended in the crucible 110, and the side wall of the crucible 110 corresponding to the position of the anode plate 131 and the cathode plate 133 is provided with openings, and the electrodes are led out of the crucible 110 by the openings. The electrodes need to be sealed and insulated from the openings. The fixed frame can be made of high temperature resistant and insulating boron nitride ceramic material.
[0055] In one embodiment, the mounting frame can be cylindrical, and the hollow area of the cylinder forms a flow area for the silicon carbide atmosphere. The mounting frame is made of insulating material, such as ceramics, etc. The cathode plate 133 is installed at the top of the mounting frame, and the anode plate 131 is installed at the bottom of the mounting frame, and the three form a whole.
[0056] In this example, the anode plate 131 and the cathode plate 133 may be made of carbon plates, and uniform and dense micropores are opened thereon, so that the silicon carbide atmosphere can pass through. Of course, the anode plate 131 and the cathode plate 133 may also be made of graphite mesh.
[0057] Secondly, in this embodiment, the crucible 110 can be made of an insulating material, for example, the boron nitride ceramic material provided in the previous embodiment. A graphite crucible 110 can also be selected. When the graphite crucible 110 is selected, a high temperature resistant insulating coating needs to be provided in the crucible 110 to isolate the anode plate 131, the cathode plate 133 and the inner wall of the graphite crucible 110.
[0058] In this embodiment, since the distance between the anode plate 131 and the cathode plate 133 is short, the value of the potential difference to be applied is relatively small when the required electric field strength is achieved. In this embodiment, the value range of the potential difference between the anode plate 131 and the cathode plate 133 in the pre-growth stage is 100V to 500V, and the value range of the potential difference between the anode plate 131 and the cathode plate 133 in the main crystal growth stage is 120V to 600V, and the value of the potential difference between the anode plate 131 and the cathode plate 133 in the main crystal growth stage is greater than the value of the potential difference between the anode plate 131 and the cathode plate 133 in the pre-growth stage.
[0059] For example, in an optional embodiment, the potential difference between the anode plate 131 and the cathode plate 133 is 300V in the pre-growth stage, and the potential difference between the anode plate 131 and the cathode plate 133 is 400V in the main growth stage.
[0060] Example 3
[0061] Please refer to Figure 3 In the present embodiment, the anode plate 131 is arranged inside the crucible 110 and is located between the powder loading zone 111 and the crystal growth zone 113. The cathode plate 133 is arranged above the crystal growth zone 115 so that the electric field formed between the anode plate 131 and the cathode plate 133 is located in the crystal growth zone 113 and the crystal growth zone 115. The anode plate 131 is provided with a flow hole 135, which allows the silicon carbide atmosphere to enter the crystal growth zone 113 through the flow hole 135.
[0062] In this way, the electric field provided by the anode plate 131 and the cathode plate 133 fills the rise zone 113 and the crystal growth zone 115, so that the ionized and charged silicon carbide atmosphere can be transmitted to the crystal growth zone 115 under the action of the additional electric field force, thereby improving the gas phase transmission rate.
[0063] That is, the anode plate 131 is arranged inside the crucible 110, and an annular platform can be arranged inside the crucible 110 and a hole can be opened on the side wall. The electrode is installed in the hole and led out of the crucible 110, and after the silicon carbide powder is filled in the powder loading area 111, the anode plate 131 is installed on the annular boss, and the anode plate 131 and the electrode are connected. The cathode plate 133 is arranged above the outer top plate of the crucible 110. The electrode and the hole are insulated and sealed. In this embodiment, the modification can be made of a high temperature resistant insulating material, such as a boron nitride ceramic material.
[0064] Secondly, in an alternative embodiment, the crucible 110 includes a crucible body and a crucible cover. The crucible body can be made of an insulating boron nitride ceramic material, and the crucible cover is set to be made of graphite, and an electrode is set on the crucible cover, so that the cover can close the crucible body and can also be used as a cathode plate 133, saving parts and space, and reducing the distance between the anode plate 131 and the cathode plate 133.
[0065] In summary, the electric field assisted crystal growth device 100 provided in this embodiment can ionize and charge the silicon carbide atmosphere by providing an electric field by setting the anode plate 131 and the cathode plate 133, so that the ionized and charged silicon carbide atmosphere is constrained by the electric field force, and the radial movement is reduced, thereby providing uniformity of atmosphere distribution. The electric field can also provide an upward electric field for the atmosphere, thereby increasing the rate of upward transmission of the atmosphere, thereby improving the efficiency of crystal growth.
[0066] Please refer to Figures 1 to 3 Secondly, this embodiment also provides a crystal growth method, which is applied to the electric field assisted crystal growth device 100 of the above embodiment, and the method includes:
[0067] The method comprises:
[0068] S1, preheating treatment, heating the temperature inside the crucible 110 (110) to a first preset temperature, and evacuating the crucible 110 (110) to make the pressure inside the crucible 110 (110) reach a first preset pressure.
[0069] S2, pre-growth stage, the temperature in the crucible 110 (110) is maintained at a first preset temperature, the pressure is maintained at a first preset pressure, and a first preset potential difference is applied to the anode plate 131 and the cathode plate 133, so that the ionized charged silicon carbide atmosphere is transmitted to the crystal growth zone 115 (115) for deposition under the action of the electric field force, and maintained for a first preset time.
[0070] S3, the main crystal growth stage, reducing the pressure in the crucible 110 (110) to maintain the pressure in the crucible 110 (110) at a second preset pressure, forming an axial temperature gradient inside the crucible 110 (110), and increasing the potential difference between the anode plate 131 and the cathode plate 133 to maintain the potential difference at the second preset potential difference, so that the ionized charged silicon carbide atmosphere is transmitted to the crystal growth zone 115 (115) for deposition under the combined action of the electric field force and the temperature gradient, and maintained for a second preset time.
[0071] S4, annealing stage, increasing the pressure in the crucible 110 (110), maintaining the pressure in the crucible 110 (110) at a third preset pressure, lowering the temperature in the crucible 110 (110), and making the potential difference between the anode plate 131 and the cathode plate 133 0, and maintaining the third preset time.
[0072] The first preset temperature ranges from 2000°C to 2300°C, and the first preset pressure ranges from 10 2 Up to 10 4 The first preset time ranges from 3h to 5h, the second preset pressure ranges from 1Pa to 3000Pa, the second preset time ranges from 50h to 200h, and the third preset pressure ranges from 10 2 Pa to 10 4 Pa, the third preset time ranges from 5h to 20h.
[0073] The crystal growth method provided in this embodiment generates a uniform electric field by electrifying the anode plate 131 and the cathode plate 133, and ionizes the silicon carbide atmosphere by using the uniform electric field, so that the molecules and atoms in the silicon carbide atmosphere can be charged, so that the charged ions are bound by the electric field force, so that they are more evenly distributed in the radial direction. The electric field can also provide additional upward electric field force to the charged ions, thereby increasing the transmission speed.
[0074] In the pre-growth stage, due to the high pressure in the crucible 110, the mean free path of the silicon carbide atmosphere is very small and insufficient to rise to the growth zone. However, under the action of the additional continuous electric field force, the mean free path of the gas phase is increased, and the gas phase can be transported to the seed crystal to grow into a crystal. At this time, the temperature gradient has a smaller driving effect on the silicon carbide atmosphere. Under the drive of the additional electric field, the gas phase transport rate is relatively low, and the silicon carbide crystal growth rate is also low, so that a dense and high-quality silicon carbide buffer layer can be formed at this stage.
[0075] In the main crystal growth stage, the pressure in the crucible 110 is reduced, so that the mean free path of the silicon carbide gas phase components increases. Under the dual driving forces provided by the temperature gradient and the electric field, the gas phase transport rate will be faster, which can alleviate the congestion of the gas phase near the powder surface and the crystal growth rate will be faster. On the other hand, the uniform electric field can alleviate the radial gas phase non-uniformity caused by the radial temperature gradient, thereby reducing crystal defects.
[0076] It should be noted that the anode plate 131 and the cathode plate 133 are energized to form a potential difference U. The field strength between the positive plate and the negative plate is an electric field of E = U / d. The electrons in the electric field are accelerated by the electric field force of F = qE. The kinetic energy of the moving electrons is mv 2 / 2=m(v0+at) 2 / 2=m(v0+qUt / md) 2 / 2, v0 is the initial velocity of the electron entering the electric field, m is the mass of the electron, q is the charge constant, d is the distance between the anode plate 131 and the cathode plate 133, and t is the time for the electron to move after entering the electric field. The high-speed moving electrons collide with gas phase molecules and atoms. When the kinetic energy of the electrons is greater than the ionization energy I1 of the gas phase molecules and atoms, positive ions will be generated. As the desired gas phase components are ionized, the positive ions will be accelerated and transported to the growth interface for deposition under the action of the additional electric field.
[0077] It should also be noted that the values of the first preset potential difference and the second preset potential difference are determined by the setting position between the anode plate 131 and the cathode plate 133, and the specific parameters can be selected according to the corresponding parameters of the positions of the different anode plates 131 and cathode plates 133 in the above-mentioned electric field assisted crystal growth device.
[0078] In summary, the crystal growth method provided in this embodiment can make the atmosphere more uniformly distributed in the radial direction and improve the quality of the crystal growth through the assistance of the electric field.
[0079] The above are only specific embodiments of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed by the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the protection scope of the claims.
Claims
1. An electric field assisted crystal growth device, characterized in that: The electric field assisted crystal growth device comprises a crucible (110) and a parallel plate capacitor (130); The crucible (110) is insulated, and the bottom of the crucible (110) is a powder loading area (111) for loading silicon carbide powder, the top of the crucible (110) is a crystal growth area (115), and the area between the powder loading area (111) and the crystal growth area (115) is a rising area (113); The parallel plate capacitor (130) comprises an anode plate (131) and a cathode plate (133), wherein the anode plate (131) is arranged below the rise zone (113), and the cathode plate (133) is arranged above the rise zone (113). An electric field can be formed between the anode plate (131) and the cathode plate (133) to ionize the silicon carbide atmosphere in the rise zone (113) to be positively charged, and the charged silicon carbide atmosphere can be transmitted upward to the crystal growth zone (115) for deposition under the combined action of the electric field force and the temperature gradient during the pre-growth stage and the main crystal growth stage.
2. The electric field assisted crystal growth device according to claim 1, characterized in that: The anode plate (131) is arranged on the outside of the crucible (110) and is coaxial with the bottom wall of the crucible (110), and the cathode plate (133) is arranged on the outside of the crucible (110) and is coaxial with the top wall of the crucible (110).
3. The electric field assisted crystal growth device according to claim 2, characterized in that: The anode plate (131) and the cathode plate (133) are graphite plates or metal plates.
4. The electric field assisted crystal growth device according to claim 3, characterized in that: In the pre-growth stage, the potential difference between the anode plate (131) and the cathode plate (133) ranges from 400V to 2000V; In the main crystal growth stage, the potential difference between the anode plate (131) and the cathode plate (133) ranges from 480V to 2400V; The value of the potential difference between the anode plate (131) and the cathode plate (133) in the main crystal growth stage is greater than the value of the potential difference between the anode plate (131) and the cathode plate (133) in the pre-growth stage.
5. The electric field assisted crystal growth device according to claim 1, characterized in that: The anode plate (131) and the cathode plate (133) are both arranged in the crucible (110), and the anode plate (131) is arranged between the powder loading zone (111) and the rising zone (113), and the cathode plate (133) is arranged between the rising zone (113) and the crystal growth zone (115), so that the electric field formed between the anode plate (131) and the cathode plate (133) is located in the rising zone (113), and the anode plate (131) and the cathode plate (133) are both provided with a plurality of corresponding and uniform flow holes (135), and the flow holes (135) can allow silicon carbide atmosphere to pass through; In the pre-growth stage, the potential difference between the anode plate (131) and the cathode plate (133) ranges from 100V to 500V, and in the main crystal growth stage, the potential difference between the anode plate (131) and the cathode plate (133) ranges from 120V to 600V, and the value of the potential difference between the anode plate (131) and the cathode plate (133) in the main crystal growth stage is greater than the value of the potential difference between the anode plate (131) and the cathode plate (133) in the pre-growth stage.
6. The electric field assisted crystal growth device according to claim 1, characterized in that: The anode plate (131) is arranged in the crucible (110) and is located between the powder loading zone (111) and the rising zone (113); the cathode plate (133) is arranged above the crystal growth zone (115), so that the electric field formed between the anode plate (131) and the cathode plate (133) is located in the rising zone (113) and the crystal growth zone (115); the anode plate (131) is provided with a plurality of flow holes (135) so that the silicon carbide atmosphere can enter the rising zone (113) through the flow holes (135); In the pre-growth stage, the potential difference between the anode plate (131) and the cathode plate (133) ranges from 200V to 1000V, and in the main crystal growth stage, the potential difference between the anode plate (131) and the cathode plate (133) ranges from 240V to 1200V, and the potential difference between the anode plate (131) and the cathode plate (133) in the main crystal growth stage is greater than the potential difference between the anode plate (131) and the cathode plate (133) in the pre-growth stage.
7. The electric field assisted crystal growth device according to claim 5 or 6, characterized in that: The anode plate (131) and the cathode plate (133) are both graphite meshes.
8. The electric field assisted crystal growth device according to any one of claims 1 to 6, characterized in that: The crucible (110) is made of boron nitride ceramic material or a graphite crucible subjected to insulation treatment.
9. A crystal growth method, applied to the electric field assisted crystal growth device according to any one of claims 1 to 8, characterized in that: The method comprises: Preheating the crucible (110) to a first preset temperature, and evacuating the crucible (110) to make the pressure inside the crucible (110) reach a first preset pressure; In the pre-growth stage, the temperature in the crucible (110) is maintained at a first preset temperature, the pressure is maintained at a first preset pressure, and a first preset potential difference is applied to the anode plate (131) and the cathode plate (133), so that the ionized charged silicon carbide atmosphere is transmitted to the crystal growth area (115) under the action of the electric field force for deposition, and the first preset time is maintained; In the main crystal growth stage, the pressure in the crucible (110) is reduced to maintain the pressure in the crucible (110) at a second preset pressure, an axial temperature gradient is formed inside the crucible (110), and the potential difference between the anode plate (131) and the cathode plate (133) is increased to maintain the potential difference at the second preset potential difference, so that the ionized charged silicon carbide atmosphere is transmitted to the crystal growth zone (115) for deposition under the combined action of the electric field force and the temperature gradient, and is maintained for a second preset time; In an annealing stage, the pressure in the crucible (110) is increased so that the pressure in the crucible (110) is maintained at a third preset pressure, and the temperature in the crucible (110) is reduced, and the potential difference between the anode plate (131) and the cathode plate (133) is made zero and maintained for a third preset time; The first preset temperature ranges from 2000°C to 2300°C, and the first preset pressure ranges from 10 2 Up to 10 4 The first preset time ranges from 3h to 5h, the second preset pressure ranges from 1Pa to 3000Pa, the second preset time ranges from 50h to 200h, and the third preset pressure ranges from 10 2 Pa to 10 4 Pa, the third preset time ranges from 5h to 20h.
Citation Information
Patent Citations
Silicon carbide crystal growth device and growth method
CN116377566A
Silicon carbide crystal growth method and crystal growth device
CN116815319A
Silicon carbide crystal growth device with plasma electric field and method
CN116988147A
Crystal growth equipment capable of uniformly sublimating gas
CN220364624U
Producing a silicon carbide volume single crystal, comprises producing silicon carbide growth gaseous phase in crystal growth region of growth crucible, and growing the single crystal by deposition from silicon carbide growth gaseous phase
DE102009016131A1