Vacuum sealing tool and sealing method thereof

By using a combination of deformable parts and solder in the vacuum sealing tooling, the automatic welding and packaging of the diaphragm and the plate is realized, which solves the problem of long time and low efficiency caused by separate degassing and exhausting of the reference cavity of the thin film vacuum gauge. Ensures efficient vacuum compliance.

CN118730387APending Publication Date: 2024-10-01北京晶芯电子有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410755731.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-12
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In the prior art, the degassing and exhausting of the reference cavity of the thin film vacuum gauge are performed separately, which results in a long process time, low production efficiency and easily leads to problems such as substandard vacuum degree.

Method used

Vacuum sealing tooling is used, including fixing parts, deformation parts and solder. By heating in a vacuum furnace, the deformation parts shrink and the solder contacts the electrode plate, thereby realizing automatic welding and packaging of the diaphragm and the electrode plate, simplifying the process and improving vacuum Spend.

Benefits of technology

The process flow is simplified, the production efficiency is improved, the sufficient vacuum degree of the reference cavity is ensured, and the problem of substandard vacuum degree caused by separate degassing and exhausting is solved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118730387A_ABST
    Figure CN118730387A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of capacitive vacuum gauge sealing, and provides a vacuum sealing tool and a sealing method thereof.The vacuum sealing tool comprises a first fixing piece, a second fixing piece, welding flux and a deformation piece; the top of the first fixing piece is used for arranging a diaphragm of the capacitive vacuum gauge; the second fixing piece is arranged above the first fixing piece, a mounting groove is formed in the bottom of the first fixing piece, and the mounting groove is used for mounting a polar plate of the capacitive vacuum gauge; the solder is used for surrounding the edge position of the upper side of the diaphragm; the deformation piece is arranged between the first fixing piece and the second fixing piece, and the two ends of the deformation piece abut against the first fixing piece and the second fixing piece respectively. The deformation piece can be switched between an original long state and a deformation state along with the change of the environment temperature so as to adjust the distance between the first fixing piece and the welding flux. According to the vacuum sealing tool, the technological process of vacuumizing and sealing of the reference cavity can be completed in sequence by heating in the vacuum furnace, the technological process is simple, and multiple times of air exhausting and exhausting are not needed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of capacitive vacuum gauge sealing, and in particular to a vacuum sealing tool and a sealing method thereof. Background Art

[0002] The thin film capacitance vacuum gauge uses the elastic diaphragm to deform under the action of pressure difference, thereby causing the capacitance of the capacitor composed of the diaphragm and the fixed electrode to change. By measuring the change in capacitance, the pressure difference can be characterized and the vacuum degree can be measured. Compared with other types of vacuum gauges, it has the advantages of high measurement accuracy, good linearity, good output repeatability and long-term stability, and the measurement results are independent of gas composition and type. It is widely used in vacuum measurement, surface treatment, coating equipment, aerospace and other fields. The core of the thin film vacuum gauge is to use an elastic diaphragm to divide the shell gauge into two small chambers. One side is connected to the measured system as a process chamber, and the other side is used as a reference chamber. The reference chamber is sealed with a high vacuum, which is called an absolute pressure capacitance vacuum gauge. The vacuum degree in the reference chamber will affect the accuracy and range of the vacuum gauge.

[0003] In the related art, the production process of the reference cavity of a high-precision thin-film vacuum gauge usually includes the following steps: degassing the workpiece to accelerate the gas release inside the reference cavity, then using oxygen-free copper as a sealing material to seal the reference cavity, and finally connecting the reference cavity to an exhaust device for exhaust. The degassing and exhaust are carried out separately, the process time is long, the production efficiency is low, and it is easy for the vacuum degree to fail to meet the standard due to insufficient degassing. Summary of the invention

[0004] The present invention provides a vacuum sealing tool and a sealing method thereof, which are used to solve the problems in the prior art of producing a reference chamber of a thin film vacuum gauge, in which degassing and exhaust are performed separately, the process time is long, the production efficiency is low, and the vacuum degree does not meet the standard due to insufficient degassing.

[0005] In a first aspect, the present invention provides a vacuum sealing tool, comprising:

[0006] A first fixing member, wherein the top of the first fixing member is used to set a diaphragm of a capacitive vacuum gauge;

[0007] A second fixing member, the second fixing member is arranged above the first fixing member, and a mounting groove is configured at the bottom of the first fixing member, and the mounting groove is used to mount the electrode plate of the capacitive vacuum gauge;

[0008] Solder, the solder is used to surround the edge position of the upper side of the diaphragm;

[0009] A deformable member, wherein the deformable member is disposed between the first fixing member and the second fixing member, and two ends of the deformable member are respectively in contact with the first fixing member and the second fixing member; the deformable member can switch between an original length state and a deformed state as the ambient temperature changes, so as to adjust the distance between the first fixing member and the solder;

[0010] When the ambient temperature is lower than the first temperature, the deformable member is in the original length state, and there is a gap between the solder and the electrode plate in the mounting groove; when the ambient temperature reaches the first temperature, the deformable member is in a deformed state, and the deformable member contracts to make the solder close to the first fixing member, and the solder is used to abut against the electrode plate in the mounting groove.

[0011] According to the vacuum sealing tool of the present invention, the deformable member is a memory alloy spring, and the first temperature is the martensitic transformation point of the memory alloy spring.

[0012] According to the vacuum sealing tool of the present invention, there are a plurality of the deformable members, and the plurality of the deformable members are arranged around the edge of the first fixing member.

[0013] According to the vacuum sealing tool of the present invention, the solder is provided with exhaust holes / notches penetrating in the horizontal direction.

[0014] According to the vacuum sealing tool of the present invention, there are a plurality of exhaust holes / notches, and the plurality of exhaust holes / notches are arranged at intervals along the circumference of the solder.

[0015] In a second aspect, the present invention further provides a sealing method using any one of the above-mentioned vacuum sealing tools, comprising:

[0016] The diaphragm and the solder are sequentially stacked on the first fixing member, the electrode plate is installed in the installation groove, the second fixing member is arranged above the first fixing member through the deformable member, and the diaphragm and the electrode plate are aligned;

[0017] The vacuum sealing tool is moved into a vacuum furnace, and the vacuum sealing tool is heated. When the temperature in the furnace reaches a second temperature, the temperature in the furnace is kept unchanged; the second temperature is lower than the first temperature;

[0018] When the vacuum degree in the furnace reaches a preset vacuum degree, the temperature in the furnace is continuously increased until the deformable member is deformed so that the solder abuts against the electrode plate, and the solder melts and seals the diaphragm and the electrode plate;

[0019] The temperature in the furnace is lowered to cool and solidify the solder.

[0020] According to the sealing method of the present invention, the step of sequentially stacking the diaphragm and the solder on the first fixing member comprises:

[0021] The solder is formed on top of the membrane by screen printing.

[0022] According to the sealing method of the present invention, the solder includes an annular portion and a plurality of raised portions spaced apart at the top of the annular portion, and the gaps between adjacent raised portions form exhaust gaps; the step of forming the solder on the top of the diaphragm by screen printing includes:

[0023] forming the annular portion on the top of the diaphragm by screen printing;

[0024] A plurality of protrusions are formed on the top of the annular portion by screen printing.

[0025] According to the sealing method of the present invention, the two ends of the deformable member are fixedly connected to the first fixing member and the second fixing member respectively, and when the vacuum degree in the furnace reaches a preset vacuum degree, the temperature in the furnace is continuously increased until the deformable member is deformed so that the solder abuts against the electrode plate, and the solder melts and seals the diaphragm and the electrode plate, the step includes:

[0026] Raising the temperature in the furnace to a third temperature, and maintaining the temperature in the furnace at the third temperature until the solder melts and seals the diaphragm and the electrode plate;

[0027] At the third temperature, the deformable member contracts to pull the first fixing member, pressing the electrode plate tightly against the top of the solder.

[0028] According to the sealing method of the present invention, before the steps of sequentially stacking the diaphragm and the solder on the first fixing member, installing the electrode plate in the mounting groove, arranging the second fixing member above the first fixing member through the deformable member, and aligning the diaphragm and the electrode plate, the method comprises:

[0029] The electrode plate, the diaphragm and the vacuum sealing tool are cleaned to ensure that there is no oil stain and impurities on the surface.

[0030] The vacuum sealing tool of the present invention is used to hold the diaphragm and the electrode plate of the capacitive vacuum gauge by arranging a first fixing member and a second fixing member, respectively, so that the diaphragm and the electrode plate can maintain relative positions, and solder is arranged between the diaphragm and the electrode plate, so that the diaphragm and the electrode plate can be welded and packaged in a vacuum furnace later to form a reference cavity of the capacitive vacuum gauge; at the same time, a deformation member is arranged between the first fixing member and the second fixing member to support the second fixing member; when the temperature in the vacuum furnace is lower than the first temperature, the deformation member maintains its original length, so that there is a gap between the solder and the electrode plate, so that the electrode plate and the solder are heated and vacuumed; after the temperature in the vacuum furnace is heated to the first temperature, the deformation member switches to a deformation state, and contracts so that the electrode plate and The solders are brought close to each other, thereby bringing the solder and the electrode plates close to each other until the solder and the electrode plates abut against each other, thereby enabling the solder, the electrode plates and the diaphragm to enclose and form a reference cavity, so that the solder can be subsequently melted to seal the electrode plates and the diaphragm, thereby sealing the reference cavity. It can be seen from the above that by using the vacuum sealing tool of the present invention, it is only necessary to evacuate the vacuum furnace during the heating process, and after reaching a sufficient temperature, the solder and the electrode plates will automatically approach and complete the sealing between the electrode plates and the diaphragm. The process flow is simple, and there is no need for multiple degassing and exhausting. This effectively solves the problem that in the prior art, when producing the reference cavity of a thin film vacuum gauge, degassing and exhausting are carried out separately, the process time is long, the production efficiency is low, and the vacuum degree is easily substandard due to insufficient degassing. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] In order to more clearly illustrate the technical solutions in the present invention or the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0032] Figure 1 is a schematic diagram of a vacuum sealing tool, a diaphragm and a plate when the deformable member provided by an embodiment of the present invention is in an original length state;

[0033] Figure 2 is a schematic diagram of a vacuum sealing tool, a diaphragm and a plate when the deformable member provided by an embodiment of the present invention is in a deformed state;

[0034] Figure 3 is a schematic diagram of a solder provided by an embodiment of the present invention;

[0035] Figure 4 is a flow chart of a sealing method provided by an embodiment of the present invention;

[0036] Figure 5 is a schematic diagram of a screen printing plate for printing annular parts provided by an embodiment of the present invention;

[0037] Figure 6 It is a schematic diagram of a screen printing plate for printing raised portions provided in an embodiment of the present invention.

[0038] Reference numerals:

[0039] 1. Vacuum sealing tooling;

[0040] 11. first fixing member; 111. mounting groove;

[0041] 12. A second fixing member;

[0042] 13. solder; 131. exhaust notch; 132. annular portion; 133. raised portion;

[0043] 14. Deformed parts;

[0044] 2. Diaphragm; 3. Plate. DETAILED DESCRIPTION

[0045] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be clearly and completely described below in conjunction with the drawings of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0046] Combine the following Figure 1-3 The vacuum sealing tool provided by the present invention is described.

[0047] like Figure 1 and Figure 2 As shown, the vacuum sealing tool 1 provided by the present invention comprises: a first fixing member 11, a second fixing member 12, a solder 13, and a deforming member 14; the top of the first fixing member 11 is used to set the diaphragm 2 of the capacitive vacuum gauge; the second fixing member 12 is set above the first fixing member 11, and the bottom of the first fixing member 11 is configured with a mounting groove 111, and the mounting groove 111 is used to install the electrode plate 3 of the capacitive vacuum gauge; the solder 13 is used to surround the edge position of the upper side of the diaphragm 2; the deforming member 14 is set between the first fixing member 11 and the second fixing member 12, and the deforming member 14 The two ends are respectively abutted against the first fixing member 11 and the second fixing member 12; the deformable member 14 can switch between the original length state and the deformed state as the ambient temperature changes, so as to adjust the distance between the first fixing member 11 and the solder 13; when the ambient temperature is lower than the first temperature, the deformable member 14 is in the original length state, and there is a gap between the solder 13 and the electrode plate 3 in the mounting groove 111; when the ambient temperature reaches the first temperature, the deformable member 14 is in the deformed state, the deformable member 14 contracts to make the solder 13 close to the first fixing member 11, and the solder 13 is used to abut against the electrode plate 3 in the mounting groove 111.

[0048] In this embodiment, a first fixing member 11 and a second fixing member 12 are provided, wherein the first fixing member 11 is used to support the diaphragm 2 of the capacitive vacuum gauge, and a mounting groove 111 is provided at the bottom of the second fixing member 12 for fixing the electrode plate 3 of the capacitive vacuum gauge; the second fixing member 12 is provided above the first fixing member 11 so that the diaphragm 2 and the electrode plate 3 can be arranged relative to each other, and a solder 13 is provided between the diaphragm 2 and the electrode plate 3 so that the two can be subsequently sealed to form a reference cavity of the capacitive vacuum gauge; at the same time, a deformable member 14 is provided between the first fixing member 11 and the second fixing member 12 to support the second fixing member 12, and the deformable member 14 can adjust the deformation state with temperature, and stretch or shrink to adjust the distance between the first fixing member 11 and the solder 13, thereby adjusting the distance between the solder 13 and the electrode plate 3 in the mounting groove 111, so as to evacuate or seal the electrode plate 3 and the diaphragm 2.

[0049] Specifically, after the vacuum sealing tool 1, the electrode 3 and the diaphragm 2 are assembled, they are usually placed in a vacuum furnace and heated and evacuated at the same time; when the furnace temperature is lower than the first temperature, the deformable member 14 is in the original length state and can maintain the original length, so that a sufficient distance is maintained between the first fixing member 11 and the second fixing member 12, so that a certain gap can be maintained between the solder 13 and the electrode 3, so that the gas and moisture between the solder 13, the diaphragm 2 and the electrode 3 can be extracted through the gap between the solder 13 and the electrode 3, so that a sufficient vacuum degree is achieved in the solder 13, the diaphragm 2 and the electrode 3; when the furnace temperature is heated to the first temperature, the deformable member 14 switches to the deformed state, and contracts to make the second fixing member 12 fall toward the first fixing member 11, so that the solder 13 and the electrode 3 are close to each other until the solder 13 and the electrode 3 abut against each other, and then the solder 13, the electrode 3 and the diaphragm 2 can be surrounded to form a reference cavity, so that the subsequent melting of the solder 13 seals the electrode 3 and the diaphragm 2 and seals the reference cavity.

[0050] The vacuum sealing tool 1 of the present invention is used to accommodate the diaphragm 2 and the electrode plate 3 of the capacitive vacuum gauge by providing a first fixing member 11 and a second fixing member 12, respectively, so that the diaphragm 2 and the electrode plate 3 can maintain relative positions, and a solder 13 is provided between the diaphragm 2 and the electrode plate 3, so that the diaphragm 2 and the electrode plate 3 can be subsequently welded and packaged in a vacuum furnace to form a reference cavity of the capacitive vacuum gauge; at the same time, a deformation member 14 is provided between the first fixing member 11 and the second fixing member 12 to support the second fixing member 12; when the temperature in the vacuum furnace is lower than the first temperature, the deformation member 14 maintains its original length, so that there is a gap between the solder 13 and the electrode plate 3, so that the electrode plate 3 and the solder 13 can be heated and evacuated; after the temperature in the vacuum furnace is heated to the first temperature, the deformation member 14 switches to the deformation state and closes. The electrode plate 3 and the solder 13 are contracted to be close to each other, thereby making the solder 13 and the electrode plate 3 close to each other until the solder 13 and the electrode plate 3 abut each other, and then the solder 13, the electrode plate 3 and the diaphragm 2 can be surrounded to form a reference cavity, so that the solder 13 is subsequently melted to seal the electrode plate 3 and the diaphragm 2, and the reference cavity is sealed; it can be seen from the above that by using the vacuum sealing tool 1 of the present invention, it is only necessary to evacuate the vacuum furnace during the heating process, and after reaching a sufficient temperature, the solder 13 and the electrode plate 3 will automatically approach and complete the sealing between the electrode plate 3 and the diaphragm 2. The process flow is simple, and there is no need for multiple degassing and exhausting. It effectively solves the problem that when producing the reference cavity of the thin film vacuum gauge in the prior art, the degassing and exhausting are carried out separately, the process time is long, the production efficiency is low, and it is easy to cause the vacuum degree to fail to meet the standard due to insufficient degassing.

[0051] Specifically, in some embodiments, the deformable member 14 is a memory alloy spring, and the first temperature is the martensitic transformation point of the memory alloy spring.

[0052] Memory alloy springs are made of shape memory alloy wire, which utilizes the memory effect of shape memory alloy. They remain in the hard phase within a specific temperature range, that is, they maintain their original length; outside the temperature range, they transform into the martensite phase (soft phase), that is, they become deformed and can be deformed.

[0053] The deformation member 14 of this embodiment adopts a memory alloy spring. The length of the memory alloy spring is not affected by factors other than temperature. It has good wear resistance and corrosion resistance. The state change lag is small after the temperature changes, which is convenient for temperature control. The first temperature in the above embodiment is the martensitic transformation point of the memory alloy spring. When the ambient temperature is lower than the first temperature, the memory alloy spring remains in the hard phase and maintains the original length state; when the ambient temperature reaches the first temperature, the memory alloy spring changes into the martensitic phase, that is, switches to the deformation state.

[0054] In some embodiments, Figure 1 and Figure 2 As shown, there are a plurality of deformable members 14 , and the plurality of deformable members 14 are disposed around the edge of the first fixing member 11 .

[0055] In this embodiment, by arranging multiple first fixing members 11 around the first fixing member 11, the second fixing member 12 can be supported from multiple supporting points, so that the supporting points of the second fixing member 12 are more evenly dispersed, and the entire supporting structure is more stable and reliable. After the deformable member 14 is deformed after being heated, the falling of the second fixing member 12 is also smoother and more stable, with a simple structure and strong practicality.

[0056] Specifically, in some embodiments not shown, positioning holes are provided on the first fixing member 11 and the second fixing member 12 at positions corresponding to the deformable member 14, and both ends of the deformable member 14 are respectively inserted into the positioning holes of the first fixing member 11 and the second fixing member 12 to position and install the deformable member 14.

[0057] In some embodiments, Figure 3 As shown, the solder 13 is provided with an exhaust hole or exhaust notch 131 penetrating in the horizontal direction.

[0058] In this embodiment, a through exhaust hole or exhaust gap 131 is provided on the solder 13. After the ambient temperature reaches the first temperature, the deformable member 14 switches to the deformed state and contracts to make the second fixing member 12 fall toward the first fixing member 11, so that the solder 13 and the electrode plate 3 are close to each other until the solder 13 and the electrode plate 3 abut against each other. Then, the residual gas and moisture in the reference cavity formed by the solder 13, the electrode plate 3 and the diaphragm 2 can continue to be discharged through the exhaust hole or exhaust gap 131, further improving the vacuum degree in the reference cavity. After the ambient temperature reaches the melting point of the solder 13, the solder 13 melts and fills the closed exhaust hole or exhaust gap 131, so that the reference cavity is closed, with a simple structure and good use effect.

[0059] Optionally, in some embodiments, Figure 3 As shown, there are a plurality of exhaust holes or exhaust gaps 131 , and the plurality of exhaust holes or exhaust gaps 131 are arranged at intervals along the circumference of the solder 13 .

[0060] In this embodiment, a plurality of exhaust holes or exhaust gaps 131 are arranged at intervals along the circumference of the solder 13 , so that the gas or moisture in the reference cavity is discharged through the exhaust holes or exhaust gaps 131 in all directions, and the exhaust efficiency is higher.

[0061] In some embodiments not shown, a positioning groove is provided at the top of the first fixing member 11 corresponding to the position of the diaphragm 2 , and the positioning groove is used to set the diaphragm 2 .

[0062] In this embodiment, a positioning groove is provided on the top of the first fixing member 11, and the positioning groove is adapted to the outer shape of the diaphragm 2. When the diaphragm 2 and the electrode plate 3 need to be sealed, the diaphragm 2 is placed in the positioning groove to limit the position of the diaphragm 2, so that the diaphragm 2 and the electrode plate 3 can be subsequently aligned with each other and the relative position of the diaphragm 2 and the electrode plate 3 can be maintained to avoid displacement of the diaphragm 2 during the sealing process.

[0063] Second, as Figure 4 As shown, the present invention also provides a sealing method using the vacuum sealing tool 1 provided in any of the above embodiments. By adopting the vacuum sealing tool 1 of the above embodiment, the sealing method of the present invention also has the advantages of the above embodiment, which will not be repeated here. The sealing method of the present invention comprises the following steps:

[0064] Step S101: stack the diaphragm and the solder on the first fixing member in sequence, install the electrode plate in the installation groove, set the second fixing member above the first fixing member through the deformation member, and align the diaphragm and the electrode plate.

[0065] Step S102: Move the vacuum sealing tool into the vacuum furnace, heat the vacuum sealing tool, and when the temperature in the furnace reaches a second temperature, keep the temperature in the furnace unchanged; the second temperature is lower than the first temperature.

[0066] Step S103: When the vacuum degree in the furnace reaches a preset vacuum degree, the temperature in the furnace is continuously increased until the deformable member is deformed so that the solder abuts against the electrode plate, and the solder melts and seals the diaphragm and the electrode plate.

[0067] Step S104: lowering the temperature in the furnace to cool and solidify the solder.

[0068] Before sealing the diaphragm 2 and the electrode plate 3, the diaphragm 2 and the solder 13 are placed on the first fixing member 11 in sequence. It is easy to understand that the diaphragm 2 can be placed on the first fixing member 11 first, and then the solder 13 is arranged on the diaphragm 2; or the solder 13 can be fixed on the diaphragm 2 first, and then the solder 13 and the diaphragm 2 are placed on the first fixing member 11 as a whole; for example, the solder 13 can be coated on the diaphragm 2.

[0069] After the diaphragm 2 and the solder 13 are arranged, the deformable member 14 can be arranged on the first fixing member 11 so as to arrange the second fixing member 12. After the electrode plate 3 is installed in the installation groove 111 of the second fixing member 12, the second fixing member 12 is arranged on the upper end of the deformable member 14, and the diaphragm 2 and the electrode plate 3 are aligned with each other so as to seal the diaphragm 2 and the electrode plate 3 later.

[0070] After completing the assembly of the vacuum sealing tool 1, the diaphragm 2 and the electrode plate 3, the vacuum sealing tool 1 can be placed in a vacuum furnace and heated so that the gas and moisture in the vacuum sealing tool 1 can evaporate and be discharged. When the vacuum furnace reaches the second temperature, the furnace temperature is kept unchanged. Since the second temperature is lower than the first temperature, the deformable part 14 remains in its original length, so that there is still a gap between the solder 13 and the electrode plate 3, so that the residual gas between the diaphragm 2, the solder 13 and the electrode plate 3 can be continuously discharged to reach a preset vacuum degree, so that the vacuum degree can meet the measurement standard of the capacitive vacuum gauge.

[0071] After the vacuum degree in the furnace reaches the preset vacuum degree, the vacuum furnace can be controlled to continue to increase the furnace temperature until the furnace temperature reaches the first temperature. After reaching the first temperature, the deformable member 14 switches from the original length state to the deformed state, and the deformable member 14 contracts, causing the second fixing member 12 to fall toward the first fixing member 11 until the top of the solder 13 and the bottom of the electrode plate 3 are in contact. Then, heating is continued to melt the solder 13 in the vacuum furnace and seal it with the diaphragm 2 and the electrode plate 3.

[0072] After the solder 13 melts and seals the diaphragm 2 and the electrode 3, the vacuum furnace can be controlled to cool down to cool and solidify the solder 13. The solidified solder 13 is fixed to the diaphragm 2 and the electrode 3, thereby completely sealing the reference cavity between the diaphragm 2 and the electrode 3. After the solder 13 is completely solidified, the sealing between the diaphragm 2 and the electrode 3 is completed.

[0073] In a specific embodiment, the second temperature is 100°C, the first temperature is 110°C, and the preset vacuum degree is 10 - 6 When the vacuum furnace is heated up, after the furnace temperature reaches 100°C, the vacuum furnace is kept warm for at least one hour. When the vacuum degree in the furnace reaches 10 -6 torr, the furnace temperature can be continued to be increased. When the furnace temperature reaches 110°C, the deformable member 14 is deformed, the second fixing member 12 and the electrode plate 3 fall down and abut against the solder 13. The temperature is continued to be increased until the solder 13 melts and is sealed with the electrode plate 3 and the diaphragm 2. Then the furnace temperature is lowered to allow the solder 13 to cool and solidify to form a vacuum reference cavity.

[0074] In some embodiments, the two ends of the deformable member 14 are fixedly connected to the first fixing member 11 and the second fixing member 12 respectively. Step S103: when the vacuum degree in the furnace reaches a preset vacuum degree, the temperature in the furnace is continuously increased until the deformable member is deformed so that the solder abuts against the electrode plate, and the solder melts and seals the diaphragm and the electrode plate, including the following steps:

[0075] The temperature in the furnace is raised to the third temperature, and the temperature in the furnace is maintained at the third temperature until the solder melts and is sealed with the diaphragm and the electrode plate.

[0076] At the third temperature, the deformable member contracts to pull the first fixing member, pressing the electrode plate against the top of the solder.

[0077] In this embodiment, after the temperature in the furnace reaches the preset temperature, the temperature in the furnace is raised to the third temperature. At the third temperature, the deformable member 14 will shrink under the action of the temperature, causing the first fixing member 11 to fall, thereby driving the electrode plate 3 to fall and abut against the top of the solder 13. At the same time, since the deformable member 14 is fixedly connected to the first fixing member 11 and the second fixing member 12, the deformable member 14 can further generate a certain pulling force on the first fixing member 11, thereby pressing the electrode plate 3 against the top of the solder 13, and ensuring that the electrode plate 3 and the solder 13 can fit closely during the melting of the solder 13, further ensuring the sealing of the solder 13 and the electrode plate 3. At the same time, by setting the third temperature, it is possible to avoid the temperature in the furnace from being raised too high, thereby avoiding wasting energy or damaging the tooling and materials due to excessive temperature.

[0078] Specifically, in some embodiments, the step of sequentially stacking the diaphragm and the solder on the first fixing member includes:

[0079] Solder is screen printed on top of the membrane.

[0080] When the diaphragm 2 and the solder 13 are arranged on the first fixing member 11, the solder 13 can be arranged on the diaphragm 2 first, and then the solder 13 and the diaphragm 2 are installed on the first fixing member 11 as a whole. Preferably, the solder 13 can be printed on the top of the diaphragm 2 by screen printing. Specifically, firstly, a corresponding screen printing plate is made according to the shape of the solder 13, and the screen printing plate is covered on the diaphragm 2, and then the welding material (such as glass powder slurry) is coated on the diaphragm 2 by the screen printing plate, so as to form the solder 13 on the diaphragm 2. By using screen printing, the solder 13 is formed on the diaphragm 2, so that the solder 13 can fit the diaphragm 2 tightly, the sealing is good, and the screen printing plate can be used repeatedly, which is convenient for repeated batch operations.

[0081] Specifically, in some embodiments, Figure 3 As shown, the solder 13 includes an annular portion 132 and a plurality of protrusions 133 spaced apart on the top of the annular portion 132 , and gaps between adjacent protrusions 133 form exhaust gaps 131 .

[0082] The steps of forming solder on top of the membrane by screen printing include:

[0083] A ring-shaped portion is formed on top of the membrane by screen printing.

[0084] A plurality of protrusions are formed on the top of the annular portion by screen printing.

[0085] In this embodiment, a plurality of protrusions 133 are constructed on the top of the annular portion 132 to form an exhaust gap 131. After the ambient temperature reaches the first temperature, the deformable member 14 switches to the deformed state and contracts to make the second fixing member 12 fall toward the first fixing member 11, so that the solder 13 and the electrode plate 3 are close to each other until the solder 13 and the electrode plate 3 abut against each other. The residual gas and moisture in the reference cavity formed by the solder 13, the electrode plate 3 and the diaphragm 2 can continue to be discharged through the exhaust gap 131, further improving the vacuum degree in the reference cavity; after the ambient temperature reaches the melting point of the solder 13, the solder 13 melts and fills the closed exhaust gap 131, so that the reference cavity is closed, the structure is simple, and the use effect is good. At the same time, since the protrusion 133 is located at the top of the annular portion 132, it is also convenient to form the solder 13 on the top of the diaphragm 2 by screen printing.

[0086] Specifically, the solder 13 can be formed by screen printing twice. During the first screen printing, the printing pattern on the screen printing plate used corresponds to the annular portion 132 (eg, Figure 5 As shown), so that the welding material is coated on the top of the diaphragm 2 to form an annular portion 132; during the second screen printing, the printing pattern on the screen printing plate used corresponds to the raised portion 133, so that the welding material is coated on the top of the annular portion 132 to form a plurality of raised portions 133 (as shown). Figure 6 As shown), solder 13 is formed; the entire process is short, easy to operate, and convenient for mass production.

[0087] In some embodiments, Figure 4 As shown, step S101: stacking the diaphragm and the solder on the first fixing member in sequence, installing the electrode plate in the mounting groove, setting the second fixing member above the first fixing member through the deformation member, and aligning the diaphragm and the electrode plate, includes the following steps:

[0088] Step S090: Clean the plate, diaphragm and vacuum sealing tooling to ensure that there is no oil or impurities on the surface.

[0089] Before assembling the electrode plate 3, the diaphragm 2 and the vacuum sealing tool 1, each component needs to be cleaned to avoid residual oil, impurities, etc. on the surface, to ensure that there is no dirt in the final reference cavity, so as to ensure the quality of the vacuum gauge.

[0090] The above described embodiments are merely illustrative, and some or all of the modules may be selected according to actual needs to achieve the purpose of the embodiments. Those skilled in the art may understand and implement the embodiments without creative effort.

[0091] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A vacuum sealing tool, characterized in that: include: A first fixing member, wherein the top of the first fixing member is used to set a diaphragm of a capacitive vacuum gauge; A second fixing member, the second fixing member is arranged above the first fixing member, and a mounting groove is configured at the bottom of the first fixing member, and the mounting groove is used to mount the electrode plate of the capacitive vacuum gauge; Solder, the solder is used to surround the edge position of the upper side of the diaphragm; A deformable member, wherein the deformable member is disposed between the first fixing member and the second fixing member, and two ends of the deformable member are respectively in contact with the first fixing member and the second fixing member; the deformable member can switch between an original length state and a deformed state as the ambient temperature changes, so as to adjust the distance between the first fixing member and the solder; When the ambient temperature is lower than the first temperature, the deformable member is in the original length state, and there is a gap between the solder and the electrode plate in the mounting groove; When the ambient temperature reaches the first temperature, the deformable member is in a deformed state, and the deformable member contracts to make the solder close to the first fixing member, and the solder is used to abut against the electrode plate in the mounting groove.

2. The vacuum sealing tool according to claim 1, characterized in that: The deformable member is a memory alloy spring, and the first temperature is a martensitic transformation point of the memory alloy spring.

3. The vacuum sealing tool according to claim 1, characterized in that: There are a plurality of the deformable members, and the plurality of the deformable members are arranged around the edge of the first fixing member.

4. The vacuum sealing tool according to claim 1, characterized in that: The solder is provided with exhaust holes / notches penetrating in the horizontal direction.

5. The vacuum sealing tool according to claim 4, characterized in that: There are a plurality of exhaust holes / notches, and the plurality of exhaust holes / notches are arranged at intervals along the circumference of the solder.

6. A sealing method using the vacuum sealing tool according to any one of claims 1 to 5, characterized in that: include: The diaphragm and the solder are sequentially stacked on the first fixing member, the electrode plate is installed in the installation groove, the second fixing member is arranged above the first fixing member through the deformable member, and the diaphragm and the electrode plate are aligned; The vacuum sealing tool is moved into a vacuum furnace, and the vacuum sealing tool is heated, and when the temperature in the furnace reaches a second temperature, the temperature in the furnace is kept unchanged; the second temperature is lower than the first temperature; When the vacuum degree in the furnace reaches a preset vacuum degree, the temperature in the furnace is continuously increased until the deformable member is deformed so that the solder abuts against the electrode plate, and the solder melts and seals the diaphragm and the electrode plate; The temperature in the furnace is lowered to cool and solidify the solder.

7. The sealing method according to claim 6, characterized in that: The two ends of the deformable member are respectively fixedly connected to the first fixing member and the second fixing member. When the vacuum degree in the furnace reaches a preset vacuum degree, the temperature in the furnace is continuously increased until the deformable member is deformed so that the solder abuts against the electrode plate, and the solder melts and seals the diaphragm and the electrode plate, comprising: Raising the temperature in the furnace to a third temperature, and maintaining the temperature in the furnace at the third temperature until the solder melts and seals the diaphragm and the electrode plate; At the third temperature, the deformable member contracts to pull the first fixing member, pressing the electrode plate tightly against the top of the solder.

8. The sealing method according to claim 6, characterized in that: The step of sequentially stacking the diaphragm and the solder on the first fixing member comprises: The solder is formed on top of the membrane by screen printing.

9. The sealing method according to claim 7, characterized in that: The solder comprises an annular portion and a plurality of raised portions spaced apart on the top of the annular portion, wherein the gaps between adjacent raised portions form exhaust gaps; The step of forming the solder on the top of the diaphragm by screen printing comprises: forming the annular portion on the top of the diaphragm by screen printing; A plurality of protrusions are formed on the top of the annular portion by screen printing.

10. The sealing method according to claim 6, characterized in that: Before the steps of sequentially stacking the diaphragm and the solder on the first fixing member, installing the electrode plate in the mounting groove, arranging the second fixing member above the first fixing member through the deformable member, and aligning the diaphragm and the electrode plate, the method includes: The electrode plate, the diaphragm and the vacuum sealing tool are cleaned to ensure that there is no oil stain and impurities on the surface.