Metal gate structure and forming method thereof

By using the composite barrier layer formed by the atomic layer deposition process in the metal gate structure of the integrated circuit, the solid solution properties of titanium nitride and silicon nitride are used to solve the problem of damage to the titanium nitride layer during the etching process and reduce the It reduces the risk of leakage and simplifies the process to form a thinner work function layer.

CN118737818APending Publication Date: 2024-10-01SHANGHAI INTEGRATED CIRCUIT RESEARCH & DEVELOPMENT CENTER CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202310349422.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In integrated circuit manufacturing, in a metal gate structure with a high dielectric constant dielectric layer and a metal material, the titanium nitride layer is easily damaged during the etching process, resulting in an increased risk of leakage.

Method used

An atomic layer deposition process is used to form a composite barrier layer on the gate dielectric layer, and titanium nitride is formed by introducing interstitial solid solution element silicon as a barrier layer to protect the gate dielectric layer, and its greater etching selectivity is used to prevent damage.

Benefits of technology

It effectively reduces the risk of leakage of the metal gate structure and simplifies the etching process of the work function layer to form a thinner work function layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118737818A_ABST
    Figure CN118737818A_ABST
Patent Text Reader

Abstract

The invention provides a metal gate structure and a forming method thereof, and the forming method comprises the steps: providing a substrate, forming a gate trench on the substrate, and covering the inner wall of the gate trench with a gate dielectric layer; forming a composite barrier layer on the surface of the gate dielectric layer, wherein the composite barrier layer is formed by introducing an interstitial solid solution element silicon in the process of forming titanium nitride by adopting an atomic layer deposition process; a plurality of work function layers are formed on the composite barrier layer to form a metal gate structure, and the composite barrier layer protects the gate dielectric layer when etching the work function layers. In the invention, the composite barrier layer has the characteristics of silicon nitride with an amorphous structure and titanium nitride with a crystal structure, the silicon nitride with the amorphous structure has relatively high etching resistance relative to the work function layer, and the barrier characteristic of titanium nitride on metal ions in the work function layer is reserved, so that the gate dielectric layer is prevented from being damaged, and the metal ions are prevented from entering the gate dielectric layer; and thus, the electric leakage risk caused thereby is prevented.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of integrated circuit manufacturing, and in particular to a metal gate structure and a forming method thereof. Background Art

[0002] In the field of integrated circuit technology, with the development of technology, the characteristic size of field effect transistors continues to shrink, and the thickness of the gate oxide layer continues to shrink. However, if the thickness of the gate oxide layer is too thin, it will cause obvious carrier tunneling effect, resulting in a rapid increase in gate leakage current. Therefore, the use of a metal gate structure composed of a high dielectric constant dielectric layer and a metal material has gradually become a trend.

[0003] Taking the formation of the above-mentioned metal gate structure by the gate-last process as an example, first, a gate dielectric layer and a titanium nitride layer are sequentially formed in a number of gate trenches on the substrate, wherein the titanium nitride layer is used as a barrier layer to protect the gate dielectric layer, and then a P-type work function layer or an N-type work function layer is formed to cover the titanium nitride layer, and then the work function layer in part of the gate trench is removed and a work function layer of the opposite type is formed, wherein in the process of removing the P-type work function layer or the N-type work function layer, the titanium nitride layer is also very susceptible to damage, thereby affecting its blocking protection effect and increasing the leakage risk of the metal gate structure (device). Summary of the invention

[0004] An object of the present invention is to provide a metal gate structure and a method for forming the same, so as to reduce the leakage risk of the metal gate structure.

[0005] In order to solve the above technical problems, the present invention provides a method for forming a metal gate structure, comprising:

[0006] Providing a substrate, wherein a gate trench is formed on the substrate, and an inner wall of the gate trench is covered with a gate dielectric layer;

[0007] forming a composite barrier layer on the surface of the gate dielectric layer, wherein the composite barrier layer is formed by introducing interstitial solid solution element silicon during the process of forming titanium nitride by atomic layer deposition;

[0008] A plurality of work function layers are formed on the composite barrier layer to form the metal gate structure, wherein the composite barrier layer protects the gate dielectric layer when etching the work function layer.

[0009] Optionally, the gate dielectric layer includes an interface layer and a high dielectric constant dielectric layer formed in sequence.

[0010] Optionally, the composite barrier layer is formed by stacking a plurality of barrier layers, and the steps of forming each barrier layer include:

[0011] Passing titanium source gas to the surface of the gate dielectric layer to adsorb the titanium source, and performing a purge operation on the gate dielectric layer;

[0012] Introducing nitrogen source gas into the surface of the gate dielectric layer to adsorb the nitrogen source to react with the titanium source, and performing a purge operation on the gate dielectric layer;

[0013] A silicon source gas is introduced into the surface of the gate dielectric layer to adsorb the silicon source to react with the titanium source and the nitrogen source, and a purge operation is performed on the gate dielectric layer to form the barrier layer.

[0014] Optionally, the thickness of the composite barrier layer is 10 angstroms to 30 angstroms.

[0015] Optionally, the flow rate and time of the nitrogen source gas are greater than the flow rate and time of the silicon source gas, and the flow rate and time of the silicon source gas are greater than the flow rate and time of the titanium source gas.

[0016] Optionally, the titanium source gas includes titanium tetrachloride, and the flow rate of the titanium source gas is 30 sccm to 50 sccm; the nitrogen source gas includes ammonia, and the flow rate of the nitrogen source gas is 3500 sccm to 4000 sccm; the silicon source gas includes monosilane, and the flow rate of the silicon source gas is 200 sccm to 500 sccm.

[0017] Optionally, argon is used as the purge gas to perform the purge operation.

[0018] Optionally, after forming the composite barrier layer, an amorphous silicon layer is formed to cover the composite barrier layer and the surface of the substrate, and after performing an annealing process, the amorphous silicon layer is removed.

[0019] Optionally, the gate trench includes a first gate trench and a second gate trench, and after forming the composite barrier layer in the first gate trench and the second gate trench, the step of forming the metal gate structure includes:

[0020] Forming an etch stop layer to cover the inner walls of the first gate trench and the second gate trench, wherein the material of the etch stop layer is different from the material of the composite barrier layer and the material of the etch stop layer includes metal nitride;

[0021] Forming a first type work function layer to cover the first gate trench and the etching stop layer in the second gate trench;

[0022] Forming a patterned mask to cover the second gate trench and expose the first gate trench, using the patterned mask and the metal halide to remove the first type work function layer and the etch stop layer in the first gate trench, and staying on the surface of the composite barrier layer;

[0023] forming a second type work function layer to cover the inner wall of the first gate trench;

[0024] The patterned mask is removed, and gate metal is filled in the first gate trench and the second gate trench to form the metal gate structure.

[0025] According to another aspect of the present invention, a metal gate structure is further provided, comprising:

[0026] A substrate, wherein a surface of the substrate has a gate trench;

[0027] A gate dielectric layer covering an inner wall of the gate trench;

[0028] A composite barrier layer covers the surface of the gate dielectric layer, and the composite barrier layer is formed by introducing interstitial solid solution element silicon during the process of forming titanium nitride by atomic layer deposition process;

[0029] A work function layer covers the composite barrier layer.

[0030] To sum up, in the metal gate structure provided by the present invention, a composite barrier layer is arranged between the gate dielectric layer and the work function layer. The composite barrier layer is formed by introducing interstitial solid solution element silicon in the process of forming titanium nitride by atomic layer deposition process. The composite barrier layer can be regarded as amorphous silicon nitride and crystalline titanium nitride formed by solid solution at the atomic level, so that the composite barrier layer has the characteristics of both, that is, the larger etching selectivity (etching resistance) of the amorphous silicon nitride relative to the work function layer is utilized, and the blocking property of titanium nitride to metal ions in the work function layer is retained, thereby preventing damage to the gate dielectric layer and metal ions from entering the gate dielectric layer, thereby preventing the risk of leakage caused thereby, and the etching process of the work function layer can also be simplified, thereby forming a thinner work function layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Those skilled in the art should understand that the drawings are provided for a better understanding of the present invention, but do not constitute any limitation on the scope of the present invention.

[0032] Figure 1 is a flow chart of a method for forming a metal gate structure provided in Embodiment 1;

[0033] Figure 2a to Figure 2i This is a schematic structural diagram corresponding to the corresponding steps of the method for forming a metal gate structure provided in the first embodiment.

[0034] In the attached figure:

[0035] 10-substrate; 11-gate trench; 11a-first gate trench; 11b-second gate trench; 12-active area; 12a-first active area; 12b-second active area; 21-gate dielectric layer; 22-composite barrier layer; 22a-barrier layer; 31-etching stop layer; 32-P-type work function layer; 33-patterned mask; 34-N-type work function layer; 35-gate metal; D1-first direction; D2-second direction. DETAILED DESCRIPTION

[0036] In order to make the purpose, advantages and features of the present invention clearer, the present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be noted that the drawings are all in a very simplified form and are not drawn to scale, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention. In addition, the structure shown in the drawings is often a part of the actual structure. In particular, the emphasis of each drawing is different, and sometimes different scales are used.

[0037] As used in the present invention, the singular forms "one", "an", and "the" include plural objects, the term "or" is usually used to include the meaning of "and / or", the term "several" is usually used to include the meaning of "at least one", and the term "at least two" is usually used to include the meaning of "two or more". In addition, the terms "first", "second", and "third" are used only for descriptive purposes and cannot be understood as indicating or implying relative importance or implicitly indicating the number of indicated technical features. Therefore, the features defined as "first", "second", and "third" may explicitly or implicitly include one or at least two of the features, unless the content clearly indicates otherwise.

[0038] Embodiment 1

[0039] Figure 1 It is a flow chart of the method for forming a metal gate structure provided in the first embodiment.

[0040] like Figure 1 As shown, the method for forming a metal gate structure provided in this embodiment includes:

[0041] S01: providing a substrate, wherein a gate trench is formed on the substrate, and an inner wall of the gate trench is covered with a gate dielectric layer;

[0042] S02: forming a composite barrier layer on the surface of the gate dielectric layer, wherein the composite barrier layer is formed by introducing interstitial solid solution element silicon during the process of forming titanium nitride by an atomic layer deposition process;

[0043] S03: forming a plurality of work function layers on the composite barrier layer to form the metal gate structure, wherein the composite barrier layer protects the gate dielectric layer when etching the work function layer.

[0044] Figure 2a to Figure 2i The structural schematic diagram corresponding to the corresponding steps of the method for forming the metal gate structure provided in this embodiment, next, Figure 2a to Figure 2i The method for forming the metal gate structure is described in detail.

[0045] First, please refer to Figure 2a and Figure 2b , perform step S01, provide a substrate 10, a gate trench 11 is formed on the substrate 10, and the inner wall of the gate trench 11 is covered with a gate dielectric layer 21.

[0046] The substrate 10 may be any suitable base material known to those skilled in the art, for example, at least one of the following materials: silicon, silicon on insulator, stacked silicon on insulator, stacked silicon germanium on insulator, silicon germanium on insulator, and germanium on insulator, etc. In this embodiment, the material of the substrate 10 is described by taking silicon (silicon substrate) as an example.

[0047] In this embodiment, a metal gate structure of a planar transistor is used as an example for explanation. The substrate 10 may be formed with an active region 12 ( Figure 2b The gate dielectric layer 21 is formed to cover the inner wall of the gate trench 11, i.e., the surface of the conductive channel. The gate dielectric layer 21 includes an interface layer and a high dielectric constant layer formed in sequence, the interface layer covers the inner wall of the gate trench 11, and the material thereof may be, for example, silicon oxide, and the high dielectric constant layer covers the surface of the interface layer, and the material thereof may be, for example, hafnium oxide. After the high dielectric constant layer is formed, an annealing process may be performed to solidify it.

[0048] For details, please continue to refer to Figure 2a and Figure 2b , Figure 2a A top view diagram is shown. Figure 2b for Figure 2aIn the cross-sectional view of the embodiment, the active region 12 includes a first active region 12a and a second active region 12b. The first active region 12a and the second active region 12b have opposite conductivity types and are used to form transistors of different conductivity types. Correspondingly, a first gate trench 11a is provided on the first active region 12a, and a second gate trench 11b is provided on the second active region 12b. Figure 2c and Figure 2d , executing step S02, forming a composite barrier layer 22 on the surface of the gate dielectric layer 21, the composite barrier layer 22 is formed by introducing interstitial solid solution element silicon in the process of forming titanium nitride by atomic layer deposition process.

[0049] in, Figure 2c for Figure 2b The composite barrier layer 22 may have a thickness of 10 angstroms to 20 angstroms and is formed by stacking a plurality of barrier layers 22a. Each barrier layer 22a may include 1 to 2 atomic layers. The interstitial solid solution formed by titanium, silicon and nitrogen may react with nitrogen to form titanium nitride with an amorphous structure. The composite barrier layer 22 may be regarded as titanium nitride with an amorphous structure doped with silicon nitride with an amorphous structure, or titanium nitride with a crystalline structure introduced into silicon nitride with an amorphous structure. Thus, the barrier layer 22a formed may have the characteristics of both, that is, utilizing the larger etching selectivity of silicon nitride with an amorphous structure relative to the work function layer and maintaining the characteristics of titanium nitride.

[0050] Specifically, the steps of forming each barrier layer 22a by using the atomic layer deposition process may include:

[0051] S021: introducing a titanium source gas to the surface of the gate dielectric layer 21 to adsorb the titanium source, and performing a purge operation on the gate dielectric layer 21;

[0052] S022: introducing nitrogen source gas to the surface of the gate dielectric layer 21 to adsorb the nitrogen source and react with the titanium source, and performing a purge operation on the gate dielectric layer 21;

[0053] S023: introducing silicon source gas to the surface of the gate dielectric layer 21 to adsorb the silicon source and react with the titanium source and the nitrogen source, and performing a purge operation on the gate dielectric layer 21 to form a barrier layer 22 a.

[0054] Preferably, the flow rate and time of the silicon source gas are greater than the flow rate and time of the titanium source gas, so as to increase the content of silicon and nitrogen in the interstitial solid solution to increase the content of the amorphous structure (silicon nitride) therein, thereby improving its etching selectivity relative to the work function layer. The atomic percentage of silicon in the composite barrier layer 22 can be 5% to 20%. In addition, the flow rate and time of the nitrogen source gas are greater than the flow rate and time of the silicon source gas, so as to provide a nitrogen source for the amorphous silicon nitride and the crystalline titanium nitride.

[0055] In one example, the process temperature for performing atomic layer deposition can be 400℃~500℃, the pressure in the chamber can be 20~30Torr, the titanium source gas can include titanium tetrachloride, the flow rate of which can be 30sccm~50sccm, and the introduction time of the titanium source gas can be 200ms~500ms; the nitrogen source gas can include ammonia, the flow rate of which can be 3500sccm~4000sccm, and the introduction time of the nitrogen source gas can be 1000ms~1500ms; the silicon source gas can include monosilane, the flow rate of which can be 200sccm~500sccm, and the introduction time of the silicon source gas can be 500ms~2000ms. When performing the purge operation, the purge gas used may preferably be argon, and the flow rate of the purge gas may be 4000sccm to 5000sccm, and the introduction time may match the atoms to be purged. For example, the introduction time in step S021 is 500ms, and the introduction time in step S022 is 700ms. Of course, in step S023, the purge time may be extended to purge all unreacted atoms on the surface of the gate dielectric layer 21, and the introduction time may be 1000ms.

[0056] In addition, after forming the composite barrier layer 22, an annealing process may be performed to solidify it. Preferably, before performing the annealing process, an amorphous silicon layer may be first formed to cover the surface of the composite barrier layer 22, and the annealing process may be performed to prevent oxidation of the composite barrier layer 22 using the amorphous silicon layer, and then the amorphous silicon layer may be removed.

[0057] Next, step S03 is performed to form a plurality of work function layers on the composite barrier layer 22 to form a metal gate structure, wherein the composite barrier layer 22 protects the gate dielectric layer 21 when etching the work function layers.

[0058] In this embodiment, the first gate trench 11a can be used to form a metal gate structure of an N-type field effect transistor, and the second gate trench 11b can be used to form a metal gate structure of a P-type field effect transistor. The specific steps of forming the metal gate structure may include:

[0059] Please refer to Figure 2e , forming an etch stop layer 31 to cover the inner walls of the first gate trench 11a and the second gate trench 11b, the material of the etch stop layer 31 is different from the material of the composite barrier layer 22 and the material of the etch stop layer 31 includes metal nitride. Among them, the material of the etch stop layer 31 can be preferably a P-type work function layer 32, so as to reduce the influence on the work function value of the second gate trench 11b when it is retained in the second gate trench 11b. In this embodiment, the material of the etch stop layer 31 can be tantalum nitride, and can be formed by an atomic layer deposition process to improve the film quality and step coverage.

[0060] Please refer to Figure 2fA P-type work function layer 32 is formed to cover the etching stop layer 31 in the first gate trench 11a and the second gate trench 11b. The material of the P-type work function layer 32 can be titanium nitride.

[0061] Please refer to Figure 2g , a patterned mask 33 is formed to cover the second gate trench 11b and expose the first gate trench 11a, and the P-type work function layer 32 and the etch stop layer 31 in the first gate trench 11a are removed by metal halide using the patterned mask 33, and the etching stops on the surface of the composite barrier layer 22. Wherein, taking the material of the P-type work function layer 32 as titanium nitride and the material of the etch stop layer 31 as tantalum nitride as an example, a wet etching method including tungsten chloride (such as tungsten pentachloride) can be preferably used to remove the P-type work function layer 32 and the etch stop layer 31, and the etching selectivity of the amorphous silicon nitride in the composite barrier layer 22 relative to the work function layer is larger, so that the etching stops at the composite barrier layer 22 to prevent damage to the composite barrier layer 22, thereby protecting the high dielectric constant dielectric layer.

[0062] Please refer to Figure 2h , forming an N-type work function layer 34 to cover the inner wall of the first gate trench 11a, that is, the surface of the composite barrier layer 22. The material of the N-type work function layer 34 can be, for example, TiAlC, and can be formed by an atomic layer deposition process. Then, a layer of titanium nitride can be formed on the N-type work function layer 34 to prevent the escape of aluminum therein. Since the composite barrier layer 22 of this embodiment is adopted, not only can the etching stop be achieved accurately, but also the metal ions in the work function layer can be prevented from entering the gate dielectric layer 21, thereby simplifying the formation process of the entire work function layer. It is not difficult to understand that if the composite barrier layer 22 in this embodiment does not have a better etching resistance during etching, the above-mentioned etching stop layer 31 cannot be completely removed to prevent damage to the gate dielectric layer 21, and thus a part of the thickness of the etching stop layer 31 will remain in the first gate trench 11a, so that the work function value in the first gate trench 11a cannot be further reduced, that is, it is not conducive to reducing the threshold voltage of the N-type transistor.

[0063] Please refer to Figure 2i , remove the patterned mask 33, and fill the first gate trench 11a and the second gate trench 11b with a gate metal 35 to form a metal gate structure. The gate metal 35 may be made of tungsten.

[0064] It should be noted here that in other examples of the present embodiment, the first gate trench 11a can also be used to form a metal gate structure of a P-type field effect transistor, and the second gate trench 11b can be used to form a metal gate structure of an N-type field effect transistor. That is, after forming the etch stop layer, an N-type work function layer is first formed to cover the first gate trench 11a and the second gate trench 11b, and then the N-type work function layer and the etch stop layer in the first gate trench 11a are removed, and a P-type work function layer is formed to cover the inner wall of the first gate trench 11a to form a corresponding metal gate structure.

[0065] Embodiment 2

[0066] Embodiment 2 provides a method for forming a metal gate structure.

[0067] The method for forming the metal gate structure provided in this embodiment is similar to the method provided in the first embodiment, and the difference lies mainly in that the second embodiment is used to form a metal gate structure of a surround gate transistor, while the first embodiment is used to form a metal gate structure of a fin transistor, that is, the shape of the conductive channel in the second embodiment and the position in the gate trench are different from those of the conductive channel in the first embodiment. Specifically, in the second embodiment, a plurality of sheet-shaped or linear conductive channels pass through the gate trench and the four sides (outer walls) of the conductive channel are exposed in the gate trench, and subsequently a gate dielectric layer is formed to cover the inner wall of the gate trench and the outer wall of the conductive channel, a composite barrier layer is formed to cover the gate dielectric layer, and a work function layer and a gate metal are formed in the gate trench to form a metal gate structure similar to that in the first embodiment, which will not be described in detail here.

[0068] Embodiment 3

[0069] Embodiment 3 provides a method for forming a metal gate structure.

[0070] The method for forming the metal gate structure provided in this embodiment is similar to the method provided in the first or second embodiment, and the difference lies mainly in the metal gate structure for forming a fin-type transistor in the third embodiment, that is, the shape of the conductive channel in the third embodiment and its position in the gate trench are different from those in the first and second embodiments. Specifically, in the third embodiment, the conductive channel is in the shape of a fin, which is located in the lower middle of the gate trench and the top wall and the two side walls of the conductive channel are exposed in the gate trench, and subsequently a gate dielectric layer is formed to cover the inner wall of the gate trench (including the exposed outer wall of the conductive channel), a composite barrier layer is formed to cover the gate dielectric layer, and a work function layer and a gate metal are formed in the gate trench to form a metal gate structure similar to that in the first and second embodiments, which will not be described in detail here.

[0071] Embodiment 4

[0072] Embodiment 4 provides a metal gate structure.

[0073] The metal gate structure provided in the fourth embodiment can be formed by the method provided in the first embodiment, the second embodiment or the third embodiment, that is, it can be used to form a metal gate structure of a planar transistor, a fin transistor or a surround gate transistor. Specifically, the metal gate structure may include a substrate, a gate dielectric layer, a composite barrier layer and a work function layer. Among them, the surface of the substrate has a gate groove and a conductive channel, and the conductive channel is at least partially (outer wall) exposed in the gate groove; the gate dielectric layer covers the inner wall of the gate groove and the exposed outer wall of the conductive channel; the composite barrier layer covers the surface of the gate dielectric layer, and the composite barrier layer is formed by introducing the interstitial solid solution element silicon in the process of forming titanium nitride by atomic layer deposition process; the work function layer covers the composite barrier layer and fills the gate groove.

[0074] To sum up, in the metal gate structure provided by the present invention, a composite barrier layer is arranged between the gate dielectric layer and the work function layer. The composite barrier layer is formed by introducing interstitial solid solution element silicon in the process of forming titanium nitride by atomic layer deposition process. The composite barrier layer can be regarded as amorphous silicon nitride and crystalline titanium nitride formed by solid solution at the atomic level, so that the composite barrier layer has the characteristics of both, that is, the larger etching selectivity (etching resistance) of the amorphous silicon nitride relative to the work function layer is utilized, and the blocking property of titanium nitride to metal ions in the work function layer is retained, thereby preventing damage to the gate dielectric layer and metal ions from entering the gate dielectric layer, thereby preventing the risk of leakage caused thereby, and the etching process of the work function layer can also be simplified, thereby forming a thinner work function layer.

[0075] The above description is only a description of the preferred embodiments of the present invention, and is not intended to limit the scope of the present invention. Any changes or modifications made by a person skilled in the art in the field of the present invention based on the above disclosure shall fall within the scope of protection of the claims.

Claims

1. A method for forming a metal gate structure, characterized in that: include: Providing a substrate, wherein a gate trench is formed on the substrate, and an inner wall of the gate trench is covered with a gate dielectric layer; forming a composite barrier layer on the surface of the gate dielectric layer, wherein the composite barrier layer is formed by introducing interstitial solid solution element silicon during the process of forming titanium nitride by atomic layer deposition; A plurality of work function layers are formed on the composite barrier layer to form the metal gate structure, wherein the composite barrier layer protects the gate dielectric layer when etching the work function layer.

2. The method for forming a metal gate structure according to claim 1, wherein: The gate dielectric layer includes an interface layer and a high dielectric constant dielectric layer which are formed in sequence.

3. The method for forming a metal gate structure according to claim 1, wherein: The composite barrier layer is formed by stacking a plurality of barrier layers, and the steps of forming each barrier layer include: Passing titanium source gas to the surface of the gate dielectric layer to adsorb the titanium source, and performing a purge operation on the gate dielectric layer; Introducing nitrogen source gas into the surface of the gate dielectric layer to adsorb the nitrogen source to react with the titanium source, and performing a purge operation on the gate dielectric layer; A silicon source gas is introduced into the surface of the gate dielectric layer to adsorb the silicon source to react with the titanium source and the nitrogen source, and a purge operation is performed on the gate dielectric layer to form the barrier layer.

4. The method for forming a metal gate structure according to claim 3, wherein: The thickness of the composite barrier layer is 10 angstroms to 30 angstroms.

5. The method for forming a metal gate structure according to claim 3, wherein: The flow rate and time of introducing the nitrogen source gas are greater than the flow rate and time of introducing the silicon source gas, and the flow rate and time of introducing the silicon source gas are greater than the flow rate and time of introducing the titanium source gas.

6. The method for forming a metal gate structure according to claim 5, characterized in that: The titanium source gas includes titanium tetrachloride, and the flow rate of the titanium source gas is 30 sccm to 50 sccm. The nitrogen source gas includes ammonia, and the flow rate of the nitrogen source gas is 3500 sccm to 4000 sccm. The silicon source gas includes monosilane, and the flow rate of the silicon source gas is 200 sccm to 500 sccm.

7. The method for forming a metal gate structure according to claim 3, wherein: The purging operation was performed using argon as the purging gas.

8. The method for forming a metal gate structure according to claim 1, wherein: After forming the composite barrier layer, an amorphous silicon layer is formed to cover the composite barrier layer and the surface of the substrate, and after performing an annealing process, the amorphous silicon layer is removed.

9. The method for forming a metal gate structure according to claim 1, wherein: The gate trench includes a first gate trench and a second gate trench. After the composite barrier layer is formed in the first gate trench and the second gate trench, the steps of forming the metal gate structure include: Forming an etch stop layer to cover the inner walls of the first gate trench and the second gate trench, wherein the material of the etch stop layer is different from the material of the composite barrier layer and the material of the etch stop layer includes metal nitride; Forming a first type work function layer to cover the first gate trench and the etching stop layer in the second gate trench; Forming a patterned mask to cover the second gate trench and expose the first gate trench, using the patterned mask and the metal halide to remove the first type work function layer and the etch stop layer in the first gate trench, and staying on the surface of the composite barrier layer; forming a second type work function layer to cover the inner wall of the first gate trench; The patterned mask is removed, and gate metal is filled in the first gate trench and the second gate trench to form the metal gate structure.

10. A metal gate structure, characterized in that: include: A substrate, wherein a surface of the substrate has a gate trench; A gate dielectric layer covering an inner wall of the gate trench; A composite barrier layer covers the surface of the gate dielectric layer, and the composite barrier layer is formed by introducing interstitial solid solution element silicon during the process of forming titanium nitride by atomic layer deposition process; A work function layer covers the composite barrier layer.

Citation Information

Cited By

  • Semiconductor structure preparation method and semiconductor structure

    CN121126843A