Test structure and test method
By designing the test structure in the photoelectric sensor and using the combination of substrate, photosensitive element, dielectric layer and light-shielding layer to obtain the current value of the photosensitive element, the need for improving the performance of the photoelectric sensor is solved, and cost reduction and efficiency improvement are achieved.
Patent Information
- Application Number
- CN202310342225.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-10-01
AI Technical Summary
The performance of existing photoelectric sensors has not yet reached its optimal state, resulting in a need for performance improvement in ranging scenarios.
A test structure is designed, including a substrate, a photosensitive element, a dielectric layer and a light-shielding layer. By loading test signals on the anode and cathode connections of the photosensitive element, the current value of the photosensitive element in the non-exposed area under the photosensitive environment is obtained to characterize The extent to which a photosensitive element is subject to crosstalk from ambient light.
It reduces process costs, improves process efficiency, simplifies the test process, reduces dependence on darkrooms and high-end equipment, and can more accurately evaluate the performance of photoelectric sensors.
Smart Images

Figure CN118737863A_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present invention relate to the field of semiconductor manufacturing, and in particular to a test structure and a test method. Background Art
[0002] Photoelectric sensors are devices that convert light signals into electrical signals. Their working principle is based on the photoelectric effect, which refers to the phenomenon that when light shines on certain substances, the electrons of the substances absorb the energy of photons and produce corresponding electrical effects.
[0003] For example, CCD (Charge Coupled Device) image sensors and CMOS image sensors, which are currently widely used in digital cameras and other electronic optical devices, use the photoelectric conversion function to convert optical images into electrical signals and then output digital images. ToF (Time of Flight) distance sensors, such as DTOF (Direct Time of Flight) sensors, record the time when light pulses are emitted and detected, and convert the time difference into distance information. This technology can be used in various distance measurement scenarios such as autonomous driving, sweeping robots, VR (Virtual Reality) / AR (Augmented Reality) modeling, etc.
[0004] However, the performance of current photoelectric sensors still needs to be improved. Summary of the invention
[0005] The problem solved by the embodiments of the present invention is to provide a test structure and a test method, which are beneficial to further improve the performance of the semiconductor structure.
[0006] To solve the above problems, an embodiment of the present invention provides a test structure, including: a substrate, the substrate including exposure areas arranged in an array and non-exposure areas located between adjacent exposure areas; a photosensitive element located in the substrate between the exposure areas and the non-exposure areas, the photosensitive element having an anode connection terminal and a cathode connection terminal, the anode connection terminal being used to connect to a first test signal loading terminal, and the cathode connection terminal being used to connect to a second test signal loading terminal; a dielectric layer located on the top of the photosensitive element and the top of the substrate; a light shielding layer located on the top of the dielectric layer in the non-exposure area, and the light shielding layer exposes the top of the photosensitive element in the exposure area.
[0007] Optionally, the thickness of the light-shielding layer is 50 nanometers to 500 nanometers.
[0008] Optionally, the material of the light shielding layer includes one or more of aluminum, copper and tungsten.
[0009] Optionally, the substrate further includes isolation regions located between adjacent exposure regions, between adjacent non-exposure regions, and between the exposure region and the non-exposure region; the semiconductor structure further includes: a deep trench isolation structure located in the substrate of the isolation region.
[0010] Optionally, the dielectric layer is located on the top of the deep trench isolation structure; the light shielding layer penetrates the dielectric layer located on the top of the deep trench isolation structure, and is electrically connected to the deep trench isolation structure.
[0011] Optionally, the deep trench isolation structure includes a conductive layer and an insulating layer located between the conductive layer and the substrate.
[0012] Optionally, the material of the conductive layer includes one or more of tungsten, aluminum, titanium, titanium nitride, tantalum nitride, and copper; the material of the insulating layer includes any one or more of silicon nitride, silicon oxide, aluminum oxide, titanium oxide, hafnium oxide, zirconium oxide, magnesium oxide, calcium oxide, yttrium oxide, tantalum oxide, strontium oxide, lanthanum oxide, and barium oxide.
[0013] Optionally, the first test signal loading terminal is used to load a low voltage, and the second test signal loading terminal is used to load a high voltage.
[0014] Optionally, the test structure is disposed on a wafer, the wafer includes a cutting path, and the test structure is located in the cutting path.
[0015] Optionally, the test structure is a test structure of an optical device, and the optical device has the same substrate and photosensitive element as the test structure.
[0016] Correspondingly, an embodiment of the present invention also provides a testing method, including: providing the testing structure provided in the embodiment of the present invention; irradiating the photosensitive element in the exposure area with ambient light; loading corresponding test signals on the first test signal loading end and the second test signal loading end; obtaining the current value of the photosensitive element in the non-exposure area per unit time, and the current value is used to characterize the degree of crosstalk of the photosensitive element in the non-exposure area caused by the ambient light.
[0017] Optionally, the step of loading corresponding test signals on the first test signal loading terminal and the second test signal loading terminal includes: loading a low voltage on the first test signal loading terminal and loading a high voltage on the second test signal loading terminal.
[0018] Optionally, the step of obtaining the current value of the photosensitive element in the non-exposure area per unit time includes: obtaining the number of avalanche breakdowns occurring in the photosensitive element in the non-exposure area per unit time, and the number of avalanche breakdowns is proportional to the current value of the photosensitive element.
[0019] Compared with the prior art, the technical solution of the embodiment of the present invention has the following advantages:
[0020] An embodiment of the present invention provides a test structure, wherein a photosensitive element is located in a substrate in an exposure area and a non-exposure area, the photosensitive element has an anode connection terminal and a cathode connection terminal, the anode connection terminal is used to connect to a first test signal loading terminal, the cathode connection terminal is used to connect to a second test signal loading terminal, a dielectric layer is located on the top of the photosensitive element and the top of the substrate, a light shielding layer is located on the top of the dielectric layer in the non-exposure area, and the light shielding layer exposes the top of the photosensitive element in the exposure area, and by loading test signals on the first test signal loading terminal and the second test signal loading terminal, the current value of the photosensitive element in the non-exposure area in a photosensitive environment is obtained, thereby characterizing the degree of crosstalk of the photosensitive element in the non-exposure area by the ambient light. Compared with the existing test equipment that requires a darkroom, a high-end oscilloscope, a complete set of optoelectronic test platforms, etc., the embodiment of the present invention reduces process costs and improves process efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 to Figure 2 It is a schematic diagram of the structures corresponding to the steps in the first embodiment of the test structure of the present invention.
[0022] Figure 3 It is a flow chart of the steps of an embodiment of the testing method of the present invention. DETAILED DESCRIPTION
[0023] The existing steps for characterizing optical crosstalk include: after the wafer completes the entire process flow, the basic performance test is first performed on the wafer, and it is shipped after confirming that there are no problems with the parameters. The customer cuts and packages the wafer, and then starts the optical crosstalk test. It is necessary to select an array of photosensors in a professional dark environment, add an operating voltage to each photosensor in the array, and illuminate a device in the array with the optical signal to be detected. This method is a conventional method for detecting optical crosstalk, and the test results are relatively accurate.
[0024] However, the test requires some pre-processing of the wafer, including slicing, packaging and other process flows. It also requires a dark environment and specially built test equipment to obtain more accurate test results. If the optical crosstalk results of the photosensitive element are poor, there is no remedial measure at all, which increases the cost of time, equipment and manpower, and prolongs the development cycle of the photosensitive element.
[0025] In order to solve the above technical problems, an embodiment of the present invention provides a test structure, including: a substrate, the substrate including exposure areas arranged in an array and non-exposure areas located between adjacent exposure areas; a photosensitive element located in the substrate of the exposure areas and the non-exposure areas, the photosensitive element having an anode connection terminal and a cathode connection terminal, the anode connection terminal is used to connect to a first test signal loading terminal, and the cathode connection terminal is used to connect to a second test signal loading terminal; a dielectric layer, located on the top of the photosensitive element and the top of the substrate; a light shielding layer, located on the top of the dielectric layer in the non-exposure area, and the light shielding layer exposes the top of the photosensitive element in the exposure area.
[0026] In the test structure provided in this embodiment, by loading the test signal on the first test signal loading terminal and the second test signal loading terminal, the current value of the photosensitive element in the non-exposure area in the photosensitive environment is obtained, thereby characterizing the degree of crosstalk of the photosensitive element in the non-exposure area caused by the ambient light. Compared with the existing test equipment that requires a darkroom, a high-end oscilloscope, a complete set of optoelectronic test platforms, etc., the embodiment of the present invention reduces the process cost and improves the process efficiency.
[0027] In order to make the above-mentioned purposes, features and advantages of the embodiments of the present invention more obvious and understandable, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0028] Figure 1 to Figure 2 1 is a schematic diagram of a test structure of an embodiment of the present invention. Figure 1 It is a top view. Figure 2 yes Figure 1 Cross-sectional view along the AA direction.
[0029] The test structure includes: a substrate 100, wherein the substrate 100 includes exposure areas 100A arranged in an array and non-exposure areas 100B located between adjacent exposure areas 100A; a photosensitive element 101 located in the substrate 100 in the exposure areas 100A and the non-exposure areas 100B, wherein the photosensitive element 101 has an anode connection terminal (not shown) and a cathode connection terminal (not shown), wherein the anode connection terminal is used to connect to a first test signal loading terminal, and the cathode connection terminal is used to connect to a second test signal loading terminal; a dielectric layer 103 located on the top of the photosensitive element 101 and the top of the substrate 100; and a light shielding layer 106 located on the top of the dielectric layer 103 in the non-exposure area 100B, and wherein the light shielding layer 106 exposes the top of the photosensitive element 101 in the exposure area 100A.
[0030] It should be noted that, by loading test signals on the first test signal loading terminal and the second test signal loading terminal, the current value of the photosensitive element 101 in the non-exposure area 100B in the photosensitive environment is obtained, thereby characterizing the degree of crosstalk of the photosensitive element 101 in the non-exposure area 100B caused by the ambient light. Compared with the existing test equipment that requires a darkroom, a high-end oscilloscope, a complete set of optoelectronic test platforms, etc., the embodiments of the present invention reduce process costs and improve process efficiency.
[0031] In this embodiment, the test structure is taken as a photoelectric sensor as an example for explanation. The photoelectric sensor includes TOF (Time of Flight) sensor, DTOF (Direct Time of Flight) sensor, iTOF (indirect Time of Flight) sensor, CCD (Charge Coupled Device) image sensor, CMOS image sensor and other types of photoelectric sensors.
[0032] In this embodiment, the test structure is a test structure of an optical device, and the optical device has a substrate 100 and a photosensitive element 101 that are the same as those of the structure being tested, so that the performance of the optical device can be characterized by testing the test structure, and the design and process of the optical device can be adjusted accordingly based on the test results of the test structure.
[0033] The substrate 100 is used to provide an operating platform for forming a photosensor.
[0034] In this embodiment, the base 100 includes a substrate (not shown). Specifically, the material of the substrate may include one or more of silicon, germanium, silicon germanium, silicon carbide, gallium arsenide, and indium gallium. As an example, the substrate is a silicon substrate. In other embodiments, the substrate may also be a silicon substrate on an insulator or a germanium substrate on an insulator, or other types of substrates.
[0035] In this embodiment, the substrate 100 includes a first surface 108 and a second surface 109 opposite thereto.
[0036] The first surface 108 is the back side of the substrate 100, and the second surface 109 is the front side of the substrate 100. Specifically, the substrate 100 is a backside illumination (BSI) pixel wafer, and the first surface 108 of the substrate 100 is a light-receiving surface.
[0037] The substrate 100 includes exposure regions 100A arranged in an array and non-exposure regions 100B located between adjacent exposure regions 100A.
[0038] In the subsequent process of irradiating the test structure with ambient light, the exposure area 100A is used to receive the optical signal and convert the optical signal into an electrical signal.
[0039] In the subsequent exposure test of the photosensitive element 101 in the exposure area 100A, the photosensitive element 101 in the non-exposure area 100B is not irradiated by ambient light, and by loading test signals on the first test signal loading terminal and the second test signal loading terminal, the current value of the photosensitive element 101 in the non-exposure area 100B in the photosensitive environment is obtained, thereby characterizing the degree of crosstalk of the photosensitive element 101 in the non-exposure area 100B caused by the ambient light.
[0040] In this embodiment, the substrate 100 further includes isolation regions (not shown) located between adjacent exposure regions 100A, between adjacent non-exposure regions 100B, and between the exposure region 100A and the non-exposure region 100B.
[0041] The isolation region is used to reduce the probability of optical crosstalk and electrical crosstalk between adjacent exposure regions 100A, between adjacent non-exposure regions 100B, and between adjacent exposure regions 100A and non-exposure regions 100B.
[0042] In this embodiment, the test structure further includes a deep trench isolation (DTI) structure located in the substrate 100 in the isolation region.
[0043] The deep trench isolation structure 102 penetrates the substrate 100 to reduce the probability of optical crosstalk and electrical crosstalk between adjacent exposure regions 100A, between adjacent non-exposure regions 100B, and between adjacent exposure regions 100A and non-exposure regions 100B.
[0044] In this embodiment, the deep trench isolation structure 102 includes a conductive layer (not shown) and an insulating layer (not shown) located between the conductive layer and the substrate.
[0045] By applying voltage to the conductive layer, the conductive layer is connected to a negative potential, thereby adsorbing positive charges on the side walls of the deep trench isolation structure 102, which is beneficial to improving the interface state of the side walls of the deep trench isolation structure 102 and reducing the probability of generating dark current between adjacent exposure areas 100A, between adjacent non-exposure areas 100B, and between adjacent exposure areas 100A and non-exposure areas 100B.
[0046] In this embodiment, the conductive layer is made of metal material, which has good conductivity and is usually opaque, and can also shield light between adjacent exposure areas 100A, between adjacent non-exposure areas 100B, and between adjacent exposure areas 100A and non-exposure areas 100B.
[0047] In this embodiment, the material of the conductive layer includes one or more of tungsten, aluminum, titanium, titanium nitride, tantalum nitride, and copper. As an embodiment, the material of the conductive layer is tungsten, which is not easy to diffuse and has a relatively outstanding hole filling ability, thereby improving the filling effect of the conductive layer, and tungsten is an opaque metal material and can play a role in light isolation.
[0048] The insulating layer is used to achieve insulation between the conductive layer and the substrate 100 .
[0049] In this embodiment, the material of the insulating layer includes any one or more of silicon nitride, silicon oxide, aluminum oxide, titanium oxide, hafnium oxide, zirconium oxide, magnesium oxide, calcium oxide, yttrium oxide, tantalum oxide, strontium oxide, lanthanum oxide and barium oxide.
[0050] Specifically, the photosensitive element 101 is used to receive an optical signal so as to convert the optical signal into an electrical signal.
[0051] In this embodiment, the photosensitive element 101 has an anode connection terminal (not shown) and a cathode connection terminal (not shown), wherein the anode connection terminal is used to connect to the first test signal loading terminal, and the cathode connection terminal is used to connect to the second test signal loading terminal.
[0052] Specifically, the first test signal loading terminal is used to load a low voltage, and the second test signal loading terminal is used to load a high voltage.
[0053] It should be noted that in the subsequent process of performing ambient light testing on the test structure, by loading a low voltage on the first test signal loading end and a high voltage on the second test signal loading end, the photosensitive element 101 is made to be a PN junction diode operating under reverse voltage bias, and photons irradiated into the light receiving area of the photosensitive element 101 generate electron-hole pairs inside the junction area. The electron-hole pairs undergo avalanche multiplication under the action of the built-in electric field in the junction area and are swept to the two ends of the junction, generating photocurrent, thereby realizing the detection of optical signals.
[0054] In the formation process of the test structure, the dielectric layer 103 is used to provide a spatial position for forming the light shielding layer 106, reducing the risk of leakage between adjacent light shielding layers 106, and at the same time, protecting the photosensitive elements 101 located in the exposure area 100A and the non-exposure area 100B.
[0055] In this embodiment, the material of the dielectric layer 103 is an insulating material, and the material of the dielectric layer 103 includes one or more of silicon oxide, silicon nitride, silicon oxynitride and silicon carbide.
[0056] In this embodiment, the dielectric layer 103 is also located on the top of the deep trench isolation structure 102 .
[0057] It should be noted that the dielectric layer 103 is also located on the top of the deep trench isolation structure 102 . In the process of forming the test structure, the dielectric layer 103 provides a process basis for forming the light shielding layer 106 on the top of the deep trench isolation structure 102 .
[0058] In the subsequent process of performing ambient light testing on the test structure, the shading layer 106 is used to shield the photosensitive element 101 in the non-exposure area 100B, thereby reducing the probability that the photosensitive element 101 in the non-exposure area 100B is exposed to ambient light. Correspondingly, the accuracy of obtaining the current value of the photosensitive element 101 in the non-exposure area 100B per unit time is improved, thereby accurately characterizing the degree to which the photosensitive element 101 in the non-exposure area 100B is affected by light crosstalk.
[0059] It should be noted that the thickness of the light shielding layer 106 should not be too large or too small. If the thickness of the light shielding layer 106 is too large, the overall thickness of the photoelectric sensor is likely to be too large, which affects the integration of the photoelectric sensor; if the thickness of the light shielding layer 106 is too small, the probability of the photosensitive element 101 in the non-exposure area 100B being irradiated by ambient light is likely to increase, and in the subsequent process of performing ambient light testing on the test structure, the accuracy of obtaining the current value of the photosensitive element 101 in the non-exposure area 100B per unit time is reduced, thereby affecting the accuracy of the light crosstalk of the photosensitive element 101 in the non-exposure area 100B. For this reason, in this embodiment, the thickness of the light shielding layer 106 is 50 nanometers to 500 nanometers.
[0060] In this embodiment, the material of the light shielding layer 106 includes one or more of aluminum, copper and tungsten.
[0061] Aluminum, copper and tungsten are all metal materials, which have conductive properties and are not easy to diffuse, thereby improving the filling effect of the light shielding layer 106. In addition, aluminum, copper and tungsten are opaque metal materials and can play a role in light isolation.
[0062] In this embodiment, the light shielding layer 106 penetrates the dielectric layer 103 located on the top of the deep trench isolation structure 102 , and is electrically connected to the deep trench isolation structure 102 .
[0063] It should be noted that the shading layer 106 is electrically connected to the deep trench isolation structure 102. By applying a voltage to the deep trench isolation structure 102, the deep trench isolation structure 102 is connected to a negative potential, thereby adsorbing positive charges on the side walls of the deep trench isolation structure 102, which is beneficial to improving the interface state of the side walls of the deep trench isolation structure 102 and reducing the probability of dark current being generated between adjacent exposure areas 100A, between adjacent non-exposure areas 100B, and between adjacent exposure areas 100A and non-exposure areas 100B.
[0064] In this embodiment, the test structure is arranged on the wafer, and the wafer includes a cutting path, and the test structure is located in the cutting path, so that the process of forming a device product on the wafer can be adopted, and the test structure is formed on the wafer at the same time, which simplifies the process flow, improves the process efficiency, and saves the process cost. At the same time, online testing can be realized, saving testing time, further saving process costs, and it is also beneficial to ensure the consistency of the test structure and the device product. In addition, the test structure is located in the cutting path. After the test, the test structure can be cut and removed through the cutting path, so that the device product on the wafer can be directly obtained.
[0065] Correspondingly, an embodiment of the present invention also provides a testing method. Figure 3 It is a flow chart of the steps of an embodiment of the testing method of the present invention.
[0066] In this embodiment, the testing method includes the following basic steps:
[0067] Step S1: providing a test structure of the aforementioned embodiment of the invention;
[0068] Step S2: irradiating the photosensitive element in the exposure area with ambient light;
[0069] Step S3: loading corresponding test signals to the first test signal loading end and the second test signal loading end;
[0070] Step S4: obtaining the current value of the photosensitive element in the non-exposure area per unit time, wherein the current value is used to characterize the degree of crosstalk of the photosensitive element in the non-exposure area caused by the ambient light.
[0071] In the test method provided in the embodiment of the present invention, by loading the test signal to the first test signal loading terminal and the second test signal loading terminal, the current value of the photosensitive element in the non-exposure area under the photosensitive environment is obtained, thereby characterizing the degree of crosstalk of the photosensitive element in the non-exposure area caused by the ambient light. Compared with the existing test equipment that requires a darkroom, a high-end oscilloscope, a complete set of optoelectronic test platforms, etc., the embodiment of the present invention reduces the process cost and improves the process efficiency.
[0072] In order to make the above-mentioned purposes, features and advantages of the embodiments of the present invention more obvious and easy to understand, the following is a summary of the present invention. Figure 3 The specific embodiments of the present invention are described in detail.
[0073] refer to Figure 3 , execute step S1: provide the test structure of the aforementioned invention embodiment.
[0074] The detailed description of the aforementioned embodiments of the invention refers to the description of the test structure, which will not be repeated here.
[0075] Execute step S2: irradiate the photosensitive element in the exposure area with ambient light.
[0076] Specifically, by irradiating the photosensitive element in the exposure area with ambient light, the photons irradiated in the light receiving area of the photosensitive element generate electron-hole pairs inside the junction area. These electron-hole pairs undergo avalanche multiplication under the action of the built-in electric field in the junction area and are swept to the two ends of the junction, generating photocurrent, thereby realizing the detection of optical signals.
[0077] Execute step S3: load corresponding test signals to the first test signal loading end and the second test signal loading end.
[0078] It should be noted that when the photosensitive element in the exposure area detects a light signal, electron-hole pairs will be generated in its photosensitive area and avalanche multiplication will occur. Most of the carriers generated by avalanche multiplication will serve as photocurrent in the photosensitive element, but a small part of the electron-hole pairs will undergo radiation recombination to generate new photons. The newly generated photons may spill over into the photosensitive element in the non-exposure area, so that the photosensitive element in the non-exposure area senses the photocurrent when there is no light environment, and generates an optical crosstalk signal. Correspondingly, by loading the test signal on the first test signal loading end and the second test signal loading end, the current value of the photosensitive element in the non-exposure area in the photosensitive environment is obtained, thereby characterizing the degree of crosstalk of the photosensitive element in the non-exposure area caused by the ambient light. Compared with the existing test equipment that needs to provide a darkroom, a high-end oscilloscope, a complete set of optoelectronic test platforms, etc., the embodiment of the present invention reduces the process cost and improves the process efficiency.
[0079] In this embodiment, the step of loading corresponding test signals on the first test signal loading terminal and the second test signal loading terminal includes: loading a low voltage on the first test signal loading terminal and loading a high voltage on the second test signal loading terminal.
[0080] It should be noted that, in the process of performing ambient light testing on the test structure, by loading a low voltage on the first test signal loading end and a high voltage on the second test signal loading end, the photosensitive element is made to work as a PN junction diode under reverse voltage bias, and photons irradiated into the light receiving area of the photosensitive element generate electron-hole pairs inside the junction area. The electron-hole pairs undergo avalanche multiplication under the action of the built-in electric field in the junction area and are swept to the two ends of the junction, generating photocurrent, thereby realizing the detection of optical signals.
[0081] Execute step S4: obtain the current value of the photosensitive element in the non-exposure area per unit time, wherein the current value is used to characterize the degree of crosstalk of the photosensitive element in the non-exposure area caused by the ambient light.
[0082] Specifically, the performance of the photoelectric sensor is judged by characterizing the degree of crosstalk of the photosensitive element in the non-exposure area by the ambient light.
[0083] In this embodiment, the step of obtaining the current value of the photosensitive element in the non-exposure area per unit time includes: obtaining the number of avalanche breakdowns of the photosensitive element in the non-exposure area per unit time, and the number of avalanche breakdowns is proportional to the current value of the photosensitive element.
[0084] That is, the more times the photosensitive element in the non-exposure area undergoes avalanche breakdown per unit time, the greater the current value generated by the photosensitive element in the non-exposure area, thereby indicating the degree to which the photosensitive element in the non-exposure area is affected by optical crosstalk.
[0085] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A test structure, characterized in that: include: A substrate, the substrate comprising exposure areas arranged in an array and non-exposure areas located between adjacent exposure areas; A photosensitive element is located in the substrate in the exposure area and the non-exposure area, the photosensitive element has an anode connection terminal and a cathode connection terminal, the anode connection terminal is used to connect to the first test signal loading terminal, and the cathode connection terminal is used to connect to the second test signal loading terminal; a dielectric layer located on top of the photosensitive element and on top of the substrate; The light shielding layer is located on the top of the dielectric layer in the non-exposure area, and the light shielding layer exposes the top of the photosensitive element in the exposure area.
2. The test structure according to claim 1, characterized in that The thickness of the light shielding layer is 50 nanometers to 500 nanometers.
3. The test structure according to claim 1, characterized in that: The material of the light shielding layer includes one or more of aluminum, copper and tungsten.
4. The test structure according to claim 1, characterized in that: The substrate further includes an isolation region between adjacent exposure regions, between adjacent non-exposure regions, and between the exposure region and the non-exposure region; The test structure further includes: a deep trench isolation structure located in the substrate of the isolation region.
5. The test structure according to claim 4, characterized in that: The dielectric layer is located on top of the deep trench isolation structure; The light shielding layer penetrates the dielectric layer located on the top of the deep trench isolation structure and is electrically connected to the deep trench isolation structure.
6. The test structure according to claim 4, characterized in that: The deep trench isolation structure includes a conductive layer and an insulating layer located between the conductive layer and a substrate.
7. The test structure according to claim 6, characterized in that: The material of the conductive layer includes one or more of tungsten, aluminum, titanium, titanium nitride, tantalum nitride, and copper; The material of the insulating layer includes any one or more of silicon nitride, silicon oxide, aluminum oxide, titanium oxide, hafnium oxide, zirconium oxide, magnesium oxide, calcium oxide, yttrium oxide, tantalum oxide, strontium oxide, lanthanum oxide and barium oxide.
8. The test structure according to claim 1, characterized in that: The first test signal loading terminal is used for loading a low voltage, and the second test signal loading terminal is used for loading a high voltage.
9. The test structure according to claim 1, characterized in that: The test structure is arranged on a wafer, the wafer comprises a dicing line, and the test structure is located in the dicing line.
10. The test structure according to claim 1, characterized in that: The test structure is a test structure of an optical device, and the optical device has the same substrate and photosensitive element as the test structure.
11. A testing method, characterized in that: include: Providing a test structure as claimed in any one of claims 1 to 10; irradiating the photosensitive element in the exposure area with ambient light; Loading corresponding test signals to the first test signal loading end and the second test signal loading end; The current value of the photosensitive element in the non-exposure area per unit time is obtained, and the current value is used to characterize the degree of crosstalk of the photosensitive element in the non-exposure area caused by the ambient light.
12. The testing method according to claim 11, characterized in that: The step of loading corresponding test signals to the first test signal loading terminal and the second test signal loading terminal includes: loading a low voltage to the first test signal loading terminal and loading a high voltage to the second test signal loading terminal.
13. The testing method according to claim 11, characterized in that: The step of obtaining the current value of the photosensitive element in the non-exposure area per unit time includes: obtaining the number of avalanche breakdowns of the photosensitive element in the non-exposure area per unit time, and the number of avalanche breakdowns is proportional to the current value of the photosensitive element.