Wafer packaging body capable of preventing aluminum crystal pad of chip from being damaged in probe detection operation
By forming a metal stack structure of nickel and gold layers on the surface of the aluminum crystal pad of the chip, the problem of crystal pad damage during probe detection is solved, and the quality of the welding operation and product competitiveness are improved.
Patent Information
- Application Number
- CN202310314693.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-28
- Publication Date
- 2024-10-01
AI Technical Summary
During the probe inspection operation, the aluminum crystal pad of the chip is susceptible to pressure, causing the formation of concave holes, which affects the quality and reliability of subsequent welding operations and reduces the market competitiveness of the product.
A metal stack structure of nickel and gold layers is formed on the surface of the aluminum crystal pad of the chip through chemical plating technology to enhance the strength of the crystal pad and avoid the formation of concave holes.
It effectively avoids damage to the aluminum crystal pad during probe detection, improves the quality and reliability of subsequent welding operations, and enhances the market competitiveness of the product.
Smart Images

Figure CN118738024A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a wafer package, and more particularly to a wafer package in which at least one bump is arranged on at least one aluminum die pad of each chip before the die is subjected to a probe test to prevent the surface of the aluminum die pad of the chip from being damaged during the probe test. Background Art
[0002] In the semiconductor industry, after wafer manufacturing is completed, before subsequent operations such as redistribution layer (RDL) operations are carried out, probe testing is generally performed first, in which probes are used to contact the aluminum pads of each chip (die) on the wafer to create electrical connections for testing. Figure 8 The embodiment shown in is an existing wafer 5, wherein a surface 5a of the existing wafer 5 includes a plurality of chips 5b, and each chip 5b is provided with at least one aluminum pad 5c and at least one passivation layer 5d; wherein when the existing wafer 5 is subjected to a probe detection operation, at least one probe 3 is used to contact each aluminum pad 5c of each chip 5b on the existing wafer 5 to generate an electrical connection for testing, and the electrical signal is transmitted back to a related test machine for analysis and determination of the function, characteristic or condition of each chip 5b to filter out defective products; wherein the segmentation operation of the existing wafer 5 is performed after the probe detection operation is completed, so as to segment the existing wafer 5 into a plurality of chip packaging units 5e, and each chip packaging unit 5e can be used for operations such as wire bonding operations or other welding operations, taking wire bonding operations as an example but not limited to Fig.10 As shown, a first solder joint 4a is formed on each aluminum pad 5c and a second solder joint 4b is formed on an external electronic component 2 through a solder wire 4, so that each chip packaging unit 5e is electrically connected to the electronic component 2. However, the probe 3 (such as Figure 8 When the probe 3 (as shown) contacts the aluminum pads 5c of the chips 5b on the existing wafer 5 to make electrical connections for testing, the probe 3 (as shown) Figure 8 The positive pressure (as shown) generated by the aluminum crystal pads 5c during the test Figure 8 As shown in the direction of arrow N in the figure, a concave hole 5f will be left on the surface of each aluminum crystal pad 5c which is relatively soft metal (as shown in the direction of arrow N in the figure). Fig. 9 and Fig.10 This affects the quality and reliability of subsequent operations such as wire bonding or other welding operations on each chip, which is not conducive to the market competitiveness of the product.
[0003] Therefore, a wafer package that prevents the aluminum pad of the chip from being damaged during the probe detection operation is urgently expected by the relevant industry. Summary of the invention
[0004] The main purpose of the present invention is to provide a wafer package that prevents the aluminum crystal pads of the chip from being damaged during the probe detection operation. Before the multiple chips in the wafer package are subjected to the probe detection operation, at least one bump is formed and set on the surface of at least one aluminum crystal pad of each chip in the wafer package using a chemical electroplating technique, and each bump is a metal stacking structure with a certain thickness formed by stacking a nickel layer and a gold layer, or a nickel layer, a palladium layer and a gold layer on top of each aluminum crystal pad, thereby enhancing the structural strength of each aluminum crystal pad of each chip to avoid damage during the probe detection operation, and effectively solving the problem that the probe in the probe detection operation will leave a concave hole on at least one aluminum crystal pad of multiple chips in the existing wafer.
[0005] To achieve the above-mentioned purpose, the present invention provides a wafer package that prevents the aluminum crystal pad of the chip from being damaged during the probe detection operation. The wafer package includes a plurality of chips (die), at least one dielectric layer and a plurality of bumps (bump); wherein the plurality of chips are arranged in an array on a surface of the wafer package, and each of the chips is provided with at least one aluminum crystal pad (die pad) and at least one protective layer (passivation); wherein the at least one dielectric layer is provided on the surface of the wafer package, and the at least one dielectric layer has at least one opening corresponding to the position of the at least one aluminum crystal pad of the plurality of chips, and the at least one aluminum crystal pad is electrically connected to the outside from the at least one opening; wherein the plurality of bumps are formed by chemical electroplating technology and are provided in the at least one opening of the at least one dielectric layer, and are electrically connected to the at least one aluminum crystal pad in the at least one opening, and the plurality of bumps are a nickel (Ni) layer and a gold (Au) layer sequentially from the at least one aluminum crystal pad upward. ) layers and having a certain thickness, or a metal stacked structure having a certain thickness formed by stacking a nickel (Ni) layer, a palladium (Pd) layer and a gold (Au) layer in sequence on the at least one aluminum crystal pad, so as to enhance the structural strength of the at least one aluminum crystal pad of the multiple chips to avoid damage during the probe detection operation; wherein the manufacturing method of the wafer package comprises the following steps: step S1: providing a wafer package, wherein a surface of the wafer package has a plurality of chips (die) arranged in an array, and the plurality of chips are provided with at least one aluminum crystal pad (die) Step S2: before the multiple chips in the wafer package are subjected to probe detection, at least one dielectric layer is disposed on the surface of the wafer package, the at least one dielectric layer has at least one opening corresponding to the position of the at least one aluminum crystal pad of the multiple chips, and the at least one aluminum crystal pad is electrically connected to the outside through the at least one opening; and Step S3: at least one bump is formed and disposed in the at least one opening of the at least one dielectric layer by using chemical electroplating technology, the at least one bump It is electrically connected to the at least one aluminum crystal pad in the at least one opening, and the at least one bump is a metal stacking structure having a certain thickness formed by stacking a nickel (Ni) layer and a gold (Au) layer in sequence on the at least one aluminum crystal pad, or a metal stacking structure having a certain thickness formed by stacking a nickel (Ni) layer, a palladium (Pd) layer and a gold (Au) layer in sequence on the at least one aluminum crystal pad, which helps to improve the quality and reliability of the multiple chips when performing other operations subsequently, so as to increase the market competitiveness of the products.
[0006] In a preferred embodiment of the present invention, after the step S2, a dividing operation step is further included, which is to divide the wafer package into a plurality of chip package units by using a dividing tool.
[0007] In a preferred embodiment of the present invention, the multiple chip packaging units are provided for a wire bonding operation, where a first solder joint is formed on at least one bump of the multiple chip packaging units and a second solder joint is formed on an external electronic component through a bonding wire, so that the multiple chip packaging units and the electronic component are electrically connected together. BRIEF DESCRIPTION OF THE DRAWINGS
[0008] Figure 1 is a schematic plan view of a side cross-section of a wafer package in one embodiment of the present invention.
[0009] Figure 2 It is a schematic plan view of a side cross-section of a chip packaging unit in one embodiment of the present invention.
[0010] Figure 3 FIG. 4 is a schematic plan view of a side cross-section of a wafer package in another embodiment of the present invention.
[0011] Figure 4 It is a schematic plan view of a side cross-section of a chip packaging unit in another embodiment of the present invention.
[0012] Figure 5 It is a partial top plan view of the wafer package of the present invention.
[0013] Figure 6 It is a schematic plan view of a side cross section of a chip packaging unit and an electronic component electrically connected together in one embodiment of the present invention.
[0014] Figure 7 It is a schematic side cross-sectional plan view of a chip packaging unit and an electronic component electrically connected together in another embodiment of the present invention.
[0015] Figure 8 It is a schematic plan view of a side cross-section of an existing wafer.
[0016] Fig. 9 It is a partial top view schematic diagram of an existing wafer.
[0017] Fig.10 The invention is a schematic plan view of a side cross section of a chip packaging unit divided from an existing wafer and electrically connected to an electronic component.
[0018] Explanation of the reference numerals: 1-wafer package; 1a-surface; 1b-chip packaging unit; 10-chip; 11-aluminum crystal pad; 12-protective layer; 20-dielectric layer; 21-opening; 30-bump; 31-nickel layer; 32-palladium layer; 33-gold layer; 2-electronic component; 3-probe; 4-bonding wire; 4a-first solder joint; 4b-second solder joint; 5-existing wafer; 5a-surface; 5b-chip; 5c-aluminum crystal pad; 5d-protective layer; 5e-chip packaging unit; 5f-recess. DETAILED DESCRIPTION
[0019] With the help of illustrations, the structure and technical features of the present invention are described in detail as follows, wherein each illustration is only used to illustrate the structural relationship and related functions of the present invention, so the size of each element in each illustration is not drawn according to the actual scale and is not used to limit the present invention.
[0020] refer to Figure 1 and Figure 3 The present invention provides a wafer package 1 for preventing the aluminum pad of a chip from being damaged during a probe detection operation. The wafer package 1 includes a plurality of chips (Die) 10, at least one dielectric layer 20 and a plurality of bumps (Bump) 30.
[0021] Each chip 10 is arranged in an array on a surface 1a of the wafer package 1. Each chip 10 is provided with at least one aluminum die pad 11 and at least one passivation layer 12. Figure 1 and Figure 3 shown.
[0022] Each dielectric layer 20 is disposed on the surface 1a of the wafer package 1. Each dielectric layer 20 has at least one opening 21 corresponding to the position of each aluminum pad 11 of each chip 10, and each aluminum pad 11 is electrically connected to the outside through each opening 21. Figure 1 and Figure 3 shown.
[0023] Each bump 30 is formed in each opening 21 of each dielectric layer 20 by chemical plating technology, and is electrically connected to each aluminum pad 11 in each opening 21. Each bump 30 is a metal stack structure having a certain thickness, which is formed by stacking a nickel (Ni) layer 31 and a gold (Au) layer 33 in sequence from top to bottom of each aluminum pad 11. Figure 1 , Figure 2 and Figure 6 As shown, or a metal stack structure having a certain thickness formed by stacking a nickel (Ni) layer 31, a palladium (Pd) layer 32 and a gold (Au) layer 33 in sequence from each aluminum crystal pad 11 upwards as shown Figure 3 , Figure 4 and Figure 7As shown, the structural strength of each aluminum pad 11 of each chip 10 is improved to avoid damage during the probe detection operation.
[0024] In the formation of each bump 30, only a portion of the gold (Au) layer 33 is used, and the rest of the metal source of each bump 30 is the nickel (Ni) layer 31. Figure 2 As shown, or the combination of the nickel (Ni) layer 31 and the palladium (Pd) layer 32 is as shown Figure 4 As shown, such distribution can reduce the usage of the relatively high-cost gold (Au) layer 33, while also ensuring that each bump 30 does not lose a certain structural strength, thereby helping to reduce manufacturing costs.
[0025] After the wafer package 1 with the bumps 30 is subjected to a probe test, the aluminum pads 11 of the chips 10 are subjected to a positive pressure from the probe 3, because the bumps 30 of the present invention are used to replace the aluminum pads 11 of the chips 10. Figure 1 and Figure 3 As shown in the direction of the arrow N in the figure, no concave holes will be left on the aluminum pads 11 of each chip 10, and even no concave holes will be left on each bump 30, but it is not limited to the following. Figure 5 shown.
[0026] The manufacturing method of the wafer package 1 of the present invention comprises the following steps:
[0027] Step S1: Provide a wafer package 1, wherein a surface 1a of the wafer package 1 has a plurality of chips 10 arranged in an array, and each chip 10 is provided with at least one aluminum die pad 11 and at least one protective layer 12. Figure 1 and Figure 3 shown.
[0028] Step S2: Before the probe detection operation is performed on each chip 10 in the wafer package 1, at least one dielectric layer 20 is disposed on the surface 1a of the wafer package 1, each dielectric layer 20 has at least one opening 21 corresponding to the position of each aluminum pad 11 of each chip 10, and each aluminum pad 11 is electrically connected to the outside through each opening 21. Figure 1 and Figure 3 shown.
[0029] Step S3: Using chemical plating technology to form at least one bump 30 in each opening 21 of each dielectric layer 20, each bump 30 is electrically connected to each aluminum pad 11 in each opening 21, and each bump 30 is a metal stack structure having a certain thickness, which is formed by stacking a nickel (Ni) layer 31 and a gold (Au) layer 33 in sequence from top to bottom of each aluminum pad 11. Figure 1 and Figure 2As shown, or a metal stack structure having a certain thickness formed by stacking a nickel (Ni) layer 31, a palladium (Pd) layer 32 and a gold (Au) layer 33 in sequence from each aluminum crystal pad 11 upwards as shown Figure 3 and Figure 4 shown.
[0030] In addition, after the step S2, a further step of dividing the operation is included but not limited to, which is to use a dividing tool to divide the wafer package 1 (such as Figure 1 and Figure 3 As shown) is divided into a plurality of chip packaging units 1b (as shown Figure 2 and Figure 4 Each chip package unit 1b is provided for a wire bonding operation but is not limited to the following Figure 6 and Figure 7 As shown, a first solder joint 4a is formed on each bump 30 of each chip packaging unit 1b and a second solder joint 4b is formed on an external electronic component 2 through a solder wire 4, so that each chip packaging unit 1b is electrically connected to the electronic component 2 as shown in FIG. Figure 6 and Figure 7 shown.
[0031] The wafer package 1 of the present invention (such as Figure 1 and Figure 3 ) and the existing wafer 5 (as shown Figure 8 Compared with the above, it has the following advantages:
[0032] Before the probe detection operation is performed on each chip 10 in the wafer package 1 of the present invention, at least one dielectric layer 20 having openings 21 is first provided on the surface 1a of the wafer package 1. Each opening 21 corresponds to the position of each aluminum crystal pad 11 of each chip 10, and each bump 30 is formed and arranged in each opening 21 by chemical electroplating technology. Each bump 30 is a metal stack structure having a certain thickness and formed by stacking a nickel (Ni) layer 31 and a gold (Au) layer 33 in sequence from the top of each aluminum crystal pad 11. Figure 1 and Figure 2 As shown, or a metal stacking structure having a certain thickness formed by stacking each aluminum crystal pad 11 in sequence including a nickel (Ni) layer 31, a palladium (Pd) layer 32 and a gold (Au) layer 33, thereby enhancing the structural strength of each aluminum crystal pad 11 of each chip 10 to avoid damage during the probe detection operation, and no concave holes will be left on the aluminum crystal pads 11 of each chip 10, which helps to improve the quality and reliability of each chip 10 when performing other operations subsequently, so as to increase the market competitiveness of the product.
[0033] The above description is only a preferred embodiment of the present invention, which is only illustrative rather than restrictive of the present invention. A person skilled in the art will understand that many changes, modifications, and even equivalent changes may be made to the present invention within the spirit and scope defined by the claims of the present invention, but all of these will fall within the scope of protection of the present invention.
Claims
1. A wafer package that prevents the aluminum pad of a chip from being damaged during a probe inspection operation. It is characterized in that Include: A plurality of chips are arranged in an array on a surface of the wafer package, and each of the chips is provided with at least one aluminum pad and at least one protective layer; At least one dielectric layer, the at least one dielectric layer is disposed on the surface of the wafer package, the at least one dielectric layer has at least one opening corresponding to the position of the at least one aluminum crystal pad of the plurality of chips, and the at least one aluminum crystal pad is electrically connected to the outside through the at least one opening; and A plurality of bumps, wherein the plurality of bumps are formed by chemical plating technology and are disposed in the at least one opening of the at least one dielectric layer, and are electrically connected to the at least one aluminum crystal pad in the at least one opening, and the plurality of bumps are a metal stacking structure having a certain thickness formed by stacking a nickel layer and a gold layer in sequence on the at least one aluminum crystal pad, or a metal stacking structure having a certain thickness formed by stacking a nickel layer, a palladium layer and a gold layer in sequence on the at least one aluminum crystal pad, so as to enhance the structural strength of the at least one aluminum crystal pad of the plurality of chips to avoid damage during a probe detection operation; The manufacturing method of the wafer package comprises the following steps: Step S1: providing a wafer package, wherein a surface of the wafer package has a plurality of chips arranged in an array, and each chip is provided with at least one aluminum pad and at least one protective layer; Step S2: before the multiple chips in the wafer package are subjected to a probe detection operation, at least one dielectric layer is disposed on the surface of the wafer package, the at least one dielectric layer having at least one opening corresponding to the position of the at least one aluminum pad of the multiple chips, and the at least one aluminum pad is electrically connected to the outside through the at least one opening; and Step S3: Using chemical electroplating technology to form at least one bump in the at least one opening of the at least one dielectric layer, the at least one bump is electrically connected to the at least one aluminum crystal pad in the at least one opening, and the at least one bump is a metal stacked structure having a certain thickness formed by stacking a nickel layer and a gold layer in sequence on the at least one aluminum crystal pad, or a metal stacked structure having a certain thickness formed by stacking a nickel layer, a palladium layer and a gold layer in sequence on the at least one aluminum crystal pad.
2. The wafer package according to claim 1, It is characterized in that After the step S2, a dividing operation step is further included, which is to divide the wafer package into a plurality of chip package units by using a dividing tool.
3. The wafer package as claimed in claim 2, It is characterized in that The plurality of chip packaging units are provided for a wire bonding operation, and a first solder joint is formed on the plurality of bumps of the plurality of chip packaging units and a second solder joint is formed on an external electronic component through a solder wire, so that the plurality of chip packaging units and the electronic component are electrically connected together.