Cutting line structure and semiconductor element thereof

By forming cutting line structures and copper pillar bumps on the semiconductor wafer, the problem of the large area occupied by the LPDDR5 memory chip circuit detection pad is solved, and the cost and volume of the memory chip are reduced and the high-speed electronic characteristics are satisfied.

CN118738027APending Publication Date: 2024-10-01NAN YA TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311062541.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-03-31
Filing Date
2023-08-23
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The circuit detection pad of the LPDDR5 memory chip occupies a large area, resulting in high cost and large volume of the memory chip. The traditional wire-bonded BGA package cannot meet the high-speed electronic characteristics requirements.

Method used

Using a cutting line structure, the die area, cutting line area, bump pads and metal lines are formed on the semiconductor wafer, the bump pads are electrically connected to the circuit detection pads, and copper pillar bumps are formed after testing to flip the chip packaging, reducing the area of ​​the die area.

Benefits of technology

The total area of ​​the grain area is significantly reduced, reducing the cost and volume of the memory chip while meeting high-speed electronic characteristic requirements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118738027A_ABST
    Figure CN118738027A_ABST
Patent Text Reader

Abstract

The invention provides a dicing line structure and a semiconductor element thereof. The dicing line structure includes a die region, a dicing line region, one or more bump pads, one or more circuit detection pads, and one or more metal lines. The die region is disposed on a semiconductor wafer. The dicing line region surrounds the die region. The one or more bump pads are disposed on a first upper surface of an edge region of the die region. The one or more circuit detection pads are arranged on a second upper surface of the cutting line area. The one or more metal lines are disposed on the first upper surface of the die region and on the second upper surface of the dicing line region, and are configured to electrically connect the one or more bump pads to the one or more circuit detection pads.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application claims priority to U.S. patent application No. 18 / 129,204 (i.e., the priority date is "March 31, 2023"), the contents of which are incorporated herein by reference in their entirety.

[0002] The present disclosure relates to a semiconductor element, and more particularly to a cutting line structure, a semiconductor element, and a method for preparing a semiconductor wafer. Background Art

[0003] When designing a LPDDR5 (Low Power Double Data Rate 5) memory chip, circuit probing pads and bonding pads may be located near an edge of the memory chip to improve high-speed electrical characteristics.

[0004] Since the data rate of LPDDR5 memory chips can exceed 5000Mbps, the general wire bonding BGA package is not enough, so the copper pillar flip chip package is preferred. Standard flip chip technology uses copper pillars as a medium to bridge with the substrate, and the lower surface of a copper pillar can be as small as 10μm×10μm. However, the area of ​​a probe pad is larger than 50μm×50μm, so the area occupied by the probe pad in the total area of ​​the memory chip is considerable, resulting in higher cost and larger size of the memory chip.

[0005] The above “prior art” description only provides background technology, does not admit that the above “prior art” description reveals the subject matter of the present disclosure, does not constitute the prior art of the present disclosure, and any description of the above “prior art” should not be regarded as any part of this case. Summary of the invention

[0006] One embodiment of the present disclosure provides a cutting line structure. The cutting line structure includes a die area, a cutting line area, one or more bump pads, one or more circuit detection pads and one or more metal wires. The die area is arranged on a semiconductor wafer. The cutting line area surrounds the die area. The one or more bump pads are arranged on a first upper surface of an edge area of ​​the die area. The one or more circuit detection pads are arranged on a second upper surface of the cutting line area. The one or more metal wires are arranged on the first upper surface of the die area and on the second upper surface of the cutting line area, and are configured to electrically connect the one or more bump pads to the one or more circuit detection pads.

[0007] Another embodiment of the present disclosure provides a semiconductor element, comprising a plurality of die regions, a cutting line region, a plurality of bump pads, a plurality of circuit detection pads, and a plurality of metal wires. The plurality of die regions are disposed on a semiconductor wafer. The cutting line region is disposed between the plurality of die regions. The plurality of bump pads are disposed on a first upper surface of an edge region of each die region. The plurality of circuit detection pads are disposed on a second upper surface of the cutting line region. The plurality of metal wires are disposed on the first upper surface of each die region and on the second upper surface of the cutting line region, and are configured to electrically connect the plurality of bump pads to the corresponding circuit detection pads.

[0008] Another embodiment of the present disclosure provides a method for preparing a semiconductor wafer. The method includes the following steps: manufacturing a die region on a semiconductor wafer, wherein the die region is surrounded by a cut line region; forming a bump pad on a first upper surface of the die region, and forming a metal line on the first upper surface of the die region and on a second upper surface of the cut line region; forming a circuit detection pad on the second upper surface of the cut line region, wherein the bump pad is electrically connected to the circuit detection pad via the metal line; and forming a copper pillar bump on the bump pad.

[0009] The above has outlined the technical features and advantages of the present disclosure in a fairly broad manner, so that the detailed description of the present disclosure below can be better understood. Other technical features and advantages that constitute the subject matter of the claims of the present disclosure will be described below. It should be understood by those with ordinary knowledge in the technical field to which the present disclosure belongs that the concepts and specific embodiments disclosed below can be used to modify or design other structures or processes to achieve the same purpose as the present disclosure. It should also be understood by those with ordinary knowledge in the technical field to which the present disclosure belongs that such equivalent constructions cannot depart from the spirit and scope of the present disclosure as defined by the appended claims. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] A more complete understanding of the present disclosure may be obtained by referring to the detailed description and claims.The present disclosure should also be understood to be associated with the element numbers of the drawings, which represent similar elements throughout the description.

[0011] Figure 1 is a top view schematically illustrating a semiconductor wafer according to some embodiments of the present disclosure.

[0012] Figure 2A is an enlarged schematic diagram illustrating the embodiment of the present disclosure. Figure 1 an area.

[0013] Figure 2B is an enlarged schematic diagram, illustrating Figure 2A Cutting line structure.

[0014] Figure 2C to Figure 2D is a schematic cross-sectional view, illustrating Figure 2B Section line AA' of the semiconductor wafer.

[0015] Figure 3A is another enlarged schematic diagram illustrating the embodiment of the present disclosure. Figure 1 an area.

[0016] Figure 3B is an enlarged schematic diagram, illustrating Figure 3A Cutting line structure.

[0017] Figure 3C to Figure 3E is a schematic cross-sectional view, illustrating Figure 3B A semiconductor wafer with a cross section line BB'.

[0018] Figure 4A 2 is a top view schematically illustrating a die region after a sawing process according to an embodiment of the present disclosure. Figure 4B is a schematic cross-sectional view, illustrating Figure 4A Section along section line CC'.

[0019] Figure 4C FIG. 4 is a side view schematic diagram illustrating a semiconductor chip package according to an embodiment of the present disclosure.

[0020] Figure 5 1 is a flow chart illustrating a method for preparing a semiconductor wafer according to an embodiment of the present disclosure. The reference numerals are described as follows:

[0021] 1: Semiconductor wafer

[0022] 110: Grain area

[0023] 1101: Surface

[0024] 1102: Surface

[0025] 120: Area

[0026] 121: Cutting line area

[0027] 121': Remaining cutting line area

[0028] 122: Cutting Path

[0029] 200: Cutting line structure

[0030] 231: Circuit detection pad

[0031] 232: Copper pillar bump

[0032] 300: Cutting line structure

[0033] 331: Circuit Detection Pad

[0034] 331': Remaining circuit probe pads

[0035] 332: Bump pad

[0036] 333: Metal Wire

[0037] 340: Circuit Probe

[0038] 334: Copper pillar bump

[0039] 400A: Top view

[0040] 400B: Cutaway view

[0041] 400C: Cutaway view

[0042] 410: Incision area

[0043] 420: Base

[0044] 421: Metal wire

[0045] 422: Solder ball

[0046] 500: Preparation method

[0047] d: width

[0048] S510: Steps

[0049] S512: Steps

[0050] S514: Steps

[0051] S516: Steps

[0052] S518: Steps

[0053] S520: Steps DETAILED DESCRIPTION

[0054] Specific examples of components and configurations are described below to simplify the embodiments of the present disclosure. Of course, these embodiments are for illustration only and are not intended to limit the scope of the present disclosure. For example, in the description, the first component is formed on the second component, which may include an embodiment in which the first and second components are in direct contact, and may also include an embodiment in which additional components are formed between the first and second components so that the first and second components are not in direct contact. In addition, the embodiments of the present disclosure may repeat reference numbers and / or letters in many examples. The purpose of these repetitions is to simplify and clarify, and unless otherwise specified in the text, they do not themselves represent a specific relationship between the various embodiments and / or the configurations discussed.

[0055] It should be understood that although the terms first, second, third, etc. may be used herein to describe various elements, components, regions, layers, or sections, these elements, components, regions, layers, or sections are not limited by these terms. Instead, these terms are only used to distinguish one element, component, region, layer, or section from another region, layer, or section. Therefore, without departing from the teachings of the progressive conception of the present invention, the first element, component, region, layer, or section discussed below may be referred to as a second element, component, region, layer, or section.

[0056] References throughout this specification to "an example" or "an embodiment" mean that a particular feature, structure, or characteristic described in conjunction with the example is included in at least one example of the present disclosure. Thus, the phrases "in one example" or "in one embodiment" appearing throughout this specification do not necessarily all refer to the same example. Furthermore, the particular features, structures, or characteristics may be combined in any suitable manner in one or more examples.

[0057] The terms used herein are only for the purpose of describing specific embodiments and are not intended to limit the present invention. As used herein, the singular forms "a", "an", and "the" are intended to include the plural forms as well, unless the context clearly indicates otherwise. It will be further understood that when the terms "comprises" and / or "comprising" are used in this specification, these terms specify the presence of stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups of the above.

[0058] For ease of description, spatially relative terms may be used herein to describe the relationship of one element or feature to another element or feature, such as "beneath," "below," "lower," "under," "above," "upper," or the like, as shown in the figures. It should be understood that the spatially relative terms are intended to encompass different orientations of the elements in use or operation in addition to the orientations shown in the figures. For example, if the device in the figure is flipped, an element described as "below" or "beneath" or "under" other elements or features would be oriented as "above" the other elements or features. Thus, the exemplified terms "below" and "under" may encompass both above and below orientations. The elements may be otherwise oriented (e.g., rotated 90 degrees or in other orientations), and the spatially relative descriptors used herein interpreted accordingly. In addition, it will also be understood that when a layer is referred to as being 'between' two layers, it can be the only layer between the two layers, or one or more intervening layers may also be present.

[0059] It should be understood that when an element is referred to as being "connected" or "coupled" to another element, it may be directly connected or coupled to the other element, or there may be intervening elements. Conversely, when an element is referred to as being "directly connected" or "directly coupled" to another element, there are no intervening elements. Other words used to describe the relationship between elements should be interpreted in a similar manner (e.g., "between" versus "directly between," "adjacent" versus "directly adjacent," etc.).

[0060] It should be understood that when an element or layer is referred to as being "formed on" another element or layer, it can be formed directly or indirectly on the other element or layer. That is, for example, there may be intervening elements or layers. In contrast, when an element or layer is referred to as being "formed directly on" another element, there are no intervening elements or layers. Other words used to describe the relationship between elements or layers should be interpreted in a similar manner (e.g., "between" versus "directly between," "adjacent" versus "directly adjacent," etc.).

[0061] Figure 1 is a top view schematically illustrating a semiconductor wafer 1 according to some embodiments of the present disclosure.

[0062] like Figure 1As shown, the semiconductor wafer 1 includes a plurality of die regions 110, each of which is surrounded by a dicing line region 121, so that every two adjacent die regions 110 are separated by the dicing line region 121. The dicing line region 121 is a non-functional region on the semiconductor wafer 1. In addition, one or more dicing paths may be defined on the dicing line region 121. In some embodiments, the dicing path may be from top to bottom and from left to right, or from bottom to top and from right to left, depending on the dicing equipment.

[0063] In some embodiments, a semiconductor chip or die (e.g., an image sensor chip) is typically fabricated with hundreds (in some cases, thousands) of copies of the same die on a single semiconductor wafer. The cutting required to separate the individual dies from a semiconductor wafer (a process called "dicing" or "wafer dicing") can be performed using a die saw (e.g., a diamond saw). The cutting is performed along non-functional areas of semiconductor material, called dicing lines (i.e., dicing line areas 121), which separate the die areas 110 on the semiconductor wafer 1.

[0064] Figure 2A is an enlarged schematic diagram illustrating the embodiment of the present disclosure. Figure 1 An area of ​​120. Please refer to Figure 1 and Figure 2A .

[0065] Figure 1 An enlarged top view of region 120 in FIG. Figure 2A For example, there are two die regions 110 in the region 120. The two die regions 110 are separated by a cutting line region 121, and a cutting path 122 is defined on the cutting line region 121. In addition, a plurality of circuit detection pads 231 are disposed on an upper surface ( Figure 2A For the purpose of description, the circuit detection pad 231 is disposed at the left edge region of the two die regions 110, such as Figure 2A shown.

[0066] In some embodiments, the functional circuits may be located under the plurality of circuit probe pads 231, so that each die region 110 may be probed by one or more circuit probes ( Figure 2A The circuit probes 231 are electrically connected to an external testing device and placed on the circuit detection pads 231. In some embodiments, the width d of the scribe line region 121 may be in the range of 80 to 100 μm, but the present disclosure is not limited thereto.

[0067] Figure 2B yes Figure 2A2 is an enlarged view of the cutting line structure 200 in FIG. In some embodiments, the size of each circuit detection pad 231 may be x μm*y μm, where the values ​​of x and y may be 68 and 60, respectively. Therefore, the size of each circuit detection pad 231 is sufficient to accommodate a circuit probe thereon.

[0068] Figure 2C to Figure 2D is a schematic cross-sectional view, illustrating Figure 2B The semiconductor wafer 1 is shown in cross section line AA'. Please refer to Figure 2B to Figure 2D .

[0069] like Figure 2C As shown, the circuit detection pad 231 is disposed on the upper surface of the left edge region of each die region 110. It should be understood that a margin between the circuit detection pad 231 and the dicing line region 121 ensures that the circuit detection pad 231 will not be cut out from the semiconductor wafer 1 together with the dicing line region 121.

[0070] In some embodiments, after forming a circuit detection pad 231 on the upper surface of the left edge region of each die area 110, the functional circuit of each die area 110 can be tested via one or more circuit probes electrically connected to an external test device and placed on each circuit detection pad 231. After the functional circuit of each die area 110 on the semiconductor wafer 1 has been tested, a copper pillar bump 232 can be formed on each circuit detection pad 231 to connect the die area 110 to a substrate of a printed circuit board using a flip chip package.

[0071] In some other embodiments, a copper pillar bump 232 may be formed on each circuit probing pad 231 before testing the functional circuit of each die region 110 via one or more circuit probes.

[0072] exist Figures 2A to 2D In the embodiment of the present invention, for the purpose of description, the die area 110 may be, for example, a 2Gb LPDDR5 die. For example, the size of a 2Gb LPDDR5 die may have an area of ​​2000μm*4000μm, and the die size of a 2Gb LPDDR5 die is approximately 8mm. 2 In addition, the size of the circuit detection pad 231 can be 60 μm×68 μm, which is approximately equal to 0.00408 mm. 2 When the total number of the circuit detection pads 231 in one die area 110 is equal to 200, the total area of ​​the circuit detection pads 231 is approximately 0.00408 mm 2 *200=0.816mm 2 Therefore, the circuit detection pad 231 may occupy 10.2% (ie, 0.816 / 8=10.2%) of the total area of ​​the die region 110 .

[0073] Taking an 8Gb LPDDR5 die as an example, the size of an 8Gb LPDDR5 die may be 4000μm*8000μm, and the die size of an 8Gb LPDDR5 die is approximately 32mm 2 Therefore, assuming that the total number of the circuit probing pads 231 is equal to 200 for one die region 110 , the bump pads 332 may occupy 2.55% (ie, 0.816 / 32=2.55%) of the total area of ​​the die region 110 .

[0074] Figure 3A is another enlarged schematic diagram illustrating the embodiment of the present disclosure. Figure 1 An area of ​​120. Please refer to Figure 1 and Figure 3A .

[0075] Figure 1 Another enlarged top view of the middle area 120 is shown in FIG. Figure 3A For example, there are two die regions 110 in the region 120. The two die regions 110 are separated by a cutting line region 121, and a cutting path 122 is defined on the cutting line region 121. In addition, a plurality of circuit detection pads 331 are disposed on the upper surface ( Figure 3A (not shown).

[0076] A plurality of bump pads 332 are formed on an edge region of each die region 110, and the plurality of bump pads 332 correspond to the plurality of circuit detection pads 331. In addition, each circuit detection pad 331 is bridged to each bump pad 332 via a corresponding metal line 333, and the metal line 333 can be implemented by copper or other suitable metal materials. For the purpose of description, the plurality of bump pads 332 are arranged on the left edge region of each die region 110. In some embodiments, a semiconductor chip package can have input / output pins on one or more edges thereof, and the bump pads 332 can be arranged on two edge regions of each die region 110, such as two adjacent edge regions, or two opposite edge regions.

[0077] It should be understood that a plurality of copper pillar bumps ( Figure 3A Not shown), so these bump pads 332 can be regarded as copper pillar bump pads. In addition, the size of each bump pad 332 is smaller than the size of each circuit detection pad 331, and its details will be described later.

[0078] In some embodiments, there may be functional circuits under the plurality of bump pads, wherein the bump pads are connected to the circuit probe pads 331 via the metal lines, so that during the manufacturing or testing of the die area 110, each die area 110 may be probed by one or more circuit probes ( Figure 3AFor testing (not shown), one or more circuit probes are electrically connected to an external testing device and placed on the plurality of circuit detection pads 331.

[0079] In some embodiments, the width d of the scribe line region 121 between the two die regions 110 may be in a range of 80 to 100 μm, but the disclosure is not limited thereto.

[0080] Figure 3B yes Figure 3A 3. In some embodiments, the size of each circuit detection pad 331 may be xμm*yμm, where the values ​​of x and y may be 68 and 60, respectively. Therefore, the size of each circuit detection pad 331 is sufficient to place a circuit probe ( Figure 3B In some embodiments, the center of each circuit detection pad 331 may be disposed on the center line of the scribe line region 121. Therefore, there is a safety margin between the right edge of each circuit detection pad 331 and the left edge of the right die region 110, and another safety margin between the left edge of each circuit detection pad 331 and the right edge of the left die region 110. Therefore, when the semiconductor wafer 1 is cut on the scribe line region to separate each die region 110, the die region 110 will not be damaged.

[0081] In some embodiments, each bump pad 332 may be a square metal patch with a size of 10 μm*10 μm, which is much smaller than the size of each circuit detection pad 331. In addition, the length of the metal line 333 may depend on the margin from the left edge to the corresponding bump pad 332. The width of the metal line 333 may be less than or equal to one dimension of the circuit detection pad 331 (e.g., 10 μm).

[0082] In some embodiments, the bump pad 332 and the metal line 333 may be implemented using the same metal material, such as copper, and may be simultaneously formed on the upper surface of the semiconductor wafer 1 during manufacturing. In some other embodiments, the metal material of the metal line 333 may be different from the metal material of the bump pad 332.

[0083] It should be understood that Figure 3B The upper surfaces of the scribe line region 121 and the die region 110 may be substantially flush and may be regarded as a common upper surface of the semiconductor wafer 1 .

[0084] Figure 3C to Figure 3E is a schematic cross-sectional view, illustrating Figure 3B The semiconductor wafer 1 is shown in cross section line BB'. Please refer to FIG. 3B to FIG. 3E .

[0085] like Figure 3CAs shown, the circuit detection pads 331 are disposed on the upper surface of the dicing line region 121. It should be understood that there is a safety margin between the right edge of each circuit detection pad 331 and the left edge of the right die region 110, and another safety margin between the left edge of each circuit detection pad 331 and the right edge of the left die region 110. Therefore, when the semiconductor wafer 1 is cut on the dicing line region to separate each die region 110, the die region 110 will not be damaged.

[0086] In some embodiments, after the bump pad 332, the metal line 333 and the circuit detection pad 331 are formed at corresponding positions on the upper surface of the semiconductor wafer 1, as shown in FIG. Figure 3D As shown, the functional circuit of each die region 110 can be tested via one or more circuit probes 340, and the one or more circuit probes 340 are electrically connected to an external test device and placed on each circuit detection pad 331. After the functional circuit of each die region 110 on the semiconductor wafer 1 has been tested, as shown in FIG. Figure 3E As shown, a copper pillar bump 334 can be formed on each bump pad 332 to connect the die area 110 to a substrate of a printed circuit board using a flip chip package. In some embodiments, the diameter of the copper pillar bump 334 can be approximately equal to or slightly smaller than the width of the bump pad 332 (i.e., assuming a square metal patch).

[0087] In some other embodiments, the copper pillar bump 334 may be formed on each circuit probing pad 231 before testing the functional circuit of each die region 110 via one or more circuit probes 340. The timing of forming the copper pillar bump 334 on the bump pad 332 before or after testing the functional circuit of each die region 110 may be determined according to manufacturing needs.

[0088] refer to FIG. 3A to FIG. 3E In the embodiment of the present invention, the cutting line structure can be gradually constructed. For example, the bump pad 332 and the metal line 333 can be first formed on the upper surface of the semiconductor wafer 1, wherein the bump pad 332 is arranged on the edge area of ​​each die area, and the metal line 333 can be arranged between the edge area and the cutting line area 121. Then, the circuit detection pad 331 is formed on the upper surface of the cutting line area 121. After testing the functional circuit of each die area 110, the circuit detection pad 331 will be cut out from the semiconductor wafer 1 together with a part of the cutting line area 121.

[0089] use Figure 3A-3E In the embodiment of the saw line structure, the size of the die area 110 (or semiconductor wafer package) can be significantly reduced. Figures 3A to 3DIn the embodiment of the present invention, for the purpose of description, a 2Gb LPDDR5 die is used as an example. For example, the size of a 2Gb LPDDR5 die may be 2000μm*4000μm, and the die size of a 2Gb LPDDR5 die is approximately 8mm. 2 In addition, the size of the circuit detection pad 331 can be 60 μm*80 μm, which is approximately equal to 0.00408 mm. 2 It should be understood that the circuit detection pad 331 is arranged on the upper surface of the cutting line area 121, and the total area of ​​the circuit detection pad 331 is not included in the total area of ​​the die area 110. In addition, the bump pad 332 and part of the metal wire 333 are arranged at the edge area of ​​the die area, and the size of a bump pad 332 is 10μm*10μm=0.0001mm 2 Therefore, assuming that for one die region 110, the total number of bump pads 332 is equal to 200, the total area of ​​the bump pads is approximately 0.00001 mm 2 *200=0.02mm 2 Therefore, the bump pad 332 may occupy 0.25% (ie, 0.02 / 8=0.25%) of the total area of ​​the die region 110 .

[0090] Therefore, compared to Figures 2A to 2D The cutting line structure 200 of the embodiment, FIG. 3A to FIG. 3E The illustrated saw line structure 300 can save 9.95% of the total area of ​​the die region 110 .

[0091] Taking the 8Gb LPDDR5 die as an example, the size of the 8Gb LPDDR5 die may be 4000μm*8000μm, and the die size of the 8Gb LPDDR5 die is about 32mm 2 Therefore, assuming that for one die region 110, the total number of bump pads 332 is equal to 200, the total area of ​​the bump pads 332 is approximately 0.00001 mm 2 *200=0.02mm 2 Therefore, the bump pad 332 may occupy 0.0625% (ie, 0.02 / 8=0.25%) of the total area of ​​the die region 110, which is Figures 2A to 2D Compared with the cutting line structure in the embodiment of FIG. 1 , 2.49% of the total area of ​​the die region is saved.

[0092] Figure 4A FIG. 400 is a top view schematic diagram illustrating the die region 110 after a sawing process according to an embodiment of the present disclosure. Figure 4B is a cross-sectional schematic diagram 400B, illustrating an example of Figure 4A Section along section line CC'. Figure 4C FIG. 400 is a side view schematic diagram 400C illustrating a semiconductor chip package according to an embodiment of the present disclosure. Figure 3Aand FIG. 4A to FIG. 4C .

[0093] exist Figure 3A After the cutting line area 121 in FIG. 1 is cut to separate the die area 110, the top view of the cut die area 110 is as shown in FIG. Figure 4A For example, the cutout area 410 of the cutting line area 121 may be uneven, and a Figure 3A Part or all of the circuit detection pad 331 in the semiconductor wafer 1 can also be cut out of the metal wire 333. Figure 4A As shown, the cutout area 410 surrounds the die area 110, and the remaining circuit detection pad 331' is still together with the remaining dicing line area 121'. Since the circuit detection pad 331 will no longer be used after the functional circuit test of the die area 110 of the semiconductor wafer 1 is completed, the circuit detection pad 331 can be cut off from the semiconductor wafer 1 together with the dicing line area 121.

[0094] Since the bump pad 332 and the copper pillar bump 334 are still on the upper surface of the die area 110, the functional circuit of the die area 110 will not be affected. In some embodiments, Figure 4B The device shown is part of an integral device in a semiconductor chip package SCP. The die area 110 can be electrically connected to a substrate 420 of a printed circuit board using a flip chip package, such as Figure 4C shown.

[0095] For example, in Figure 4B In FIG. 1 , surfaces 1101 and 1102 are respectively the upper surface and the lower surface of the die region 110 during the manufacturing process of the die region 110. When a flip chip package is used, the die region 110 is "flipped" so that surfaces 1101 and 1102 face downward and upward, respectively. Figure 4C As shown. Therefore, the functional circuit of the die area 110 can be electrically connected to the substrate 420 (e.g., a copper clad laminate, CCL) via the copper pillar bumps 334 placed on the metal wires 421 of the substrate 420, on which one or more solder balls 422 are disposed. Therefore, the device in the cross-sectional view 400C can be packaged into a semiconductor chip package SCP, wherein the solder balls 422 can be regarded as physical pads or pins of the semiconductor chip package SCP.

[0096] Figure 5 is a flow chart illustrating a method for preparing a semiconductor wafer according to an embodiment of the present disclosure. Figure 5 and FIG. 3A to FIG. 3E .

[0097] In step S510, a die region 110 is fabricated on a semiconductor wafer 1, wherein the die region 110 is surrounded by a scribe line region 121. For example, a single semiconductor wafer 1 may include hundreds or thousands of copies of the same die region 110. The die regions 110 on the semiconductor wafer 1 are separated by a "dicing" process on the scribe line region 121 of the semiconductor wafer 1, wherein each die region 110 may include a functional circuit, and the scribe line region 121 may be a non-functional region.

[0098] In step S512, a bump pad 332 is formed on a first upper surface of the die region 110, and a metal line 333 is formed on the first upper surface of the die region 110 and a second upper surface of the dicing line region 121. For example, the bump pad 332 and the metal line 333 may be implemented using the same metal material such as copper, and they may be formed together on the upper surface of the semiconductor wafer 1 during manufacturing. In some other embodiments, the metal material of the metal line 333 may be different from the metal material of the bump pad 332.

[0099] In step S514, a circuit detection pad 331 is formed on the second upper surface of the dicing line area 121, wherein the bump pad 332 is electrically connected to the circuit detection pad 331 via the metal wire 333, and the circuit detection pad 331 is larger than the bump pad 332. In some embodiments, the size of each circuit detection pad 331 may be 60μm*68μm, and the size of each bump pad 332 may be 10μm*10μm, but the present disclosure is not limited thereto. It should be understood that the first upper surface of the die area 110 and the second upper surface of the dicing line area 121 may be substantially flush, and they may be regarded as the common upper surface of the semiconductor wafer 1.

[0100] In step S516, the functional circuit of the die area 110 is tested via a circuit probe 340 in contact with the circuit detection pad 331. For example, the bump pad 332 and the metal line 333 can be implemented using the same metal material such as copper, and the functional circuit of the die area 110 can be arranged under the bump pad 332. In addition, the circuit detection pad 331 is electrically connected to the bump pad 332 via the metal line 333. Therefore, when the circuit probe 340 electrically connected to the external test equipment is placed on the circuit detection pad 331, the functional circuit of the die area 110 can be tested. Although one bump pad 332, one metal line 333 and one circuit detection pad 331 are described here, it can be understood by those with ordinary knowledge in the art that a plurality of bump pads 332, metal lines 333 and circuit detection pads 331 can be formed on the upper surface of the semiconductor wafer 1.

[0101] In step S518, a copper pillar bump 334 is formed on the bump pad 332. For example, the copper pillar bump 334 can be used to connect the die region 110 to a substrate of a printed circuit board using a flip chip package. In some embodiments, the diameter of the copper pillar bump 334 can be approximately equal to or slightly smaller than the width of the bump pad 332 (i.e., assuming a square metal patch).

[0102] In step S520, the semiconductor wafer 1 is cut along the cutting path 122 defined on the cutting line area 121. For example, since the circuit detection pad 331 is formed on the upper surface of the cutting line area 121, after testing the functional circuit of the die area 110, the circuit detection pad 331 will be cut out from the semiconductor wafer 1 together with a part of the cutting line area 121.

[0103] Preparation method 500 is merely an example and is not intended to limit the present disclosure beyond what is explicitly recited in the claims. Additional steps may be provided before, during, or after each step of preparation method 500, and some of the steps described may be replaced, eliminated, or reordered for additional embodiments of the preparation method. In some embodiments, preparation method 500 may include Figure 5 Other steps not shown.

[0104] One embodiment of the present disclosure provides a cutting line structure. The cutting line structure includes a die area, a cutting line area, one or more bump pads, one or more circuit detection pads and one or more metal wires. The die area is arranged on a semiconductor wafer. The cutting line area surrounds the die area. The one or more bump pads are arranged on a first upper surface of an edge area of ​​the die area. The one or more circuit detection pads are arranged on a second upper surface of the cutting line area. The one or more metal wires are arranged on the first upper surface of the die area and on the second upper surface of the cutting line area, and are configured to electrically connect the one or more bump pads to the one or more circuit detection pads.

[0105] In some embodiments, the die region includes functional circuits, and the scribe line region is a non-functional region.

[0106] In some embodiments, the bump pad is electrically connected to the functional circuit of the die area. The functional circuit of the die area is tested via one or more probes electrically connected to an external test device and placed on the one or more circuit probing pads.

[0107] In some embodiments, each circuit detection pad is larger than each bump pad. A center of each circuit detection pad is disposed on a center line of the cutting line area.

[0108] In some embodiments, the scribe line structure further includes one or more copper pillar bumps disposed on the one or more bump pads.

[0109] In some embodiments, a sawing process is performed on the semiconductor wafer along a sawing path defined on the saw line region, and a portion or all of each circuit probing pad is sawed from the semiconductor wafer.

[0110] In some embodiments, the die region, the one or more bump pads, and the one or more copper pillar bumps are packaged into a semiconductor chip.

[0111] In some embodiments, the die region is electrically connected to a substrate of a printed circuit board via one or more copper pillar bumps using a flip chip package on the semiconductor wafer.

[0112] Another embodiment of the present disclosure provides a semiconductor element, comprising a plurality of die regions, a cutting line region, a plurality of bump pads, a plurality of circuit detection pads, and a plurality of metal wires. The plurality of die regions are disposed on a semiconductor wafer. The cutting line region is disposed between the plurality of die regions. The plurality of bump pads are disposed on a first upper surface of an edge region of each die region. The plurality of circuit detection pads are disposed on a second upper surface of the cutting line region. The plurality of metal wires are disposed on the first upper surface of each die region and on the second upper surface of the cutting line region, and are configured to electrically connect the plurality of bump pads to the corresponding circuit detection pads.

[0113] In some embodiments, each die region includes a functional circuit, and the scribe line region is a non-functional region, and the functional circuit of each die region is tested via a plurality of circuit probes electrically connected to an external test device and placed on the circuit detection pad.

[0114] In some embodiments, each circuit detection pad is larger than each bump pad. A center of each circuit detection pad is disposed on a center line of the cutting line area.

[0115] In some embodiments, the semiconductor device further includes a plurality of copper pillar bumps disposed on the bump pad.

[0116] In some embodiments, a dicing process is performed on the semiconductor wafer along one or more dicing paths defined on the dicing line region, and a portion or all of each circuit probing pad is cut from the semiconductor wafer.

[0117] In some embodiments, the die region, the bump pads, and the copper pillar bumps are packaged in a semiconductor chip.

[0118] In some embodiments, the semiconductor wafer further includes a remaining scribe line structure and a remaining circuit probing pad obtained after the dicing process.

[0119] In some embodiments, the die region is electrically connected to a substrate of a printed circuit board through the copper pillar bumps using a flip chip package on the semiconductor wafer.

[0120] Another embodiment of the present disclosure provides a method for preparing a semiconductor wafer. The method includes the following steps: manufacturing a die region on a semiconductor wafer, wherein the die region is surrounded by a cut line region; forming a bump pad on a first upper surface of the die region, and forming a metal line on the first upper surface of the die region and on a second upper surface of the cut line region; forming a circuit detection pad on the second upper surface of the cut line region, wherein the bump pad is electrically connected to the circuit detection pad via the metal line; and forming a copper pillar bump on the bump pad.

[0121] In some embodiments, the die region includes functional circuits, and the scribe line region is a non-functional area.

[0122] In some embodiments, the bump pads are electrically connected to the functional circuit in the die area.

[0123] In some embodiments, before a copper pillar bump is formed on the bump pad, the manufacturing method further includes testing the functional circuit of the die region via a circuit probe in contact with the circuit detection pad.

[0124] In some embodiments, the circuit probing pad is larger than the bump pad.

[0125] In some embodiments, a center of the circuit detection pad is disposed on a center line of the cutting line area.

[0126] In some embodiments, after a copper pillar bump is formed on the bump pad, the preparation method further includes cutting the semiconductor wafer along a cutting path defined on the cutting line area; and cutting a portion of the circuit detection pad from the semiconductor wafer.

[0127] In some embodiments, the preparation method further includes: packaging the die region, the bump pad, and the copper pillar bump into the semiconductor wafer.

[0128] In some embodiments, the semiconductor wafer further includes a remaining dicing line structure and a remaining circuit detection pad after the dicing process.

[0129] In some embodiments, the die region is electrically connected to a substrate of a printed circuit board via the copper pillar bumps using a flip chip package on the semiconductor wafer.

[0130] Although the present disclosure and its advantages have been described in detail, it should be understood that various changes, substitutions and replacements may be made without departing from the spirit and scope of the present disclosure as defined in the claims. For example, many of the above processes may be implemented in different ways, and other processes or combinations thereof may be used to replace many of the above processes.

[0131] Furthermore, the scope of the present application is not limited to the specific embodiments of the processes, machines, manufactures, compositions of matter, means, methods, and steps described in the specification. A person skilled in the art can understand from the disclosure of the present disclosure that existing or future developed processes, machines, manufactures, compositions of matter, means, methods, or steps that have the same functions or achieve substantially the same results as the corresponding embodiments described herein can be used according to the present disclosure. Accordingly, such processes, machines, manufactures, compositions of matter, means, methods, or steps are included in the claims of the present application.

Claims

1. A cutting line structure, comprising: A die region is disposed on a semiconductor wafer; a cut line region surrounding the die region; One or more bump pads are disposed on a first upper surface of an edge region of the die region; One or more circuit detection pads are disposed on a second upper surface of the cutting line area; and One or more metal lines are disposed on the first upper surface of the die region and the second upper surface of the scribe line region and are configured to electrically connect the one or more bump pads to the one or more circuit detection pads. 2 . The saw line structure as claimed in claim 1 , wherein the die region includes a functional circuit, and the saw line region is a non-functional region. 3 . The saw line structure as claimed in claim 2 , wherein the one or more bump pads are electrically connected to the functional circuit of the die area. 4 . The saw line structure of claim 3 , wherein the functional circuit of the die region is tested via one or more probes electrically connected to an external test device and placed on the one or more circuit probing pads. 5 . The saw line structure as claimed in claim 1 , wherein each circuit detection pad is larger than each bump pad. 6 . The cutting line structure as claimed in claim 1 , wherein a center of each detection pad is disposed on a center line of the cutting line area. 7 . The cutting line structure as claimed in claim 1 , further comprising one or more copper pillar bumps disposed on the one or more bump pads. 8 . The saw line structure of claim 7 , wherein a sawing process is performed on the semiconductor wafer along a sawing path, the sawing path is defined on the sawing line area, and a part or all of each circuit detection pad is cut from the semiconductor wafer. 9 . The saw line structure as claimed in claim 8 , wherein the die region, the one or more bump pads and the one or more copper pillar bumps are packaged into a semiconductor chip package. 10 . The saw line structure as claimed in claim 9 , wherein after the sawing process, the semiconductor chip packaging further comprises obtaining a reserved saw line structure and a reserved circuit detection pad. 11 . The saw line structure of claim 9 , wherein the die area is electrically connected to a substrate of a printed circuit board via the one or more copper pillar bumps using a flip chip package on the die area.

12. A semiconductor element, comprising: A plurality of crystal grain regions are arranged on a semiconductor wafer; A cutting line area is arranged between the plurality of die areas; A plurality of bump pads are disposed on a first upper surface of an edge region of each die region; A plurality of circuit detection pads are disposed on a second upper surface of the cutting line area; as well as A plurality of metal lines are disposed on the first upper surface of each die region and on the second upper surface of the scribe line region and are configured to electrically connect the plurality of bump pads to the corresponding plurality of circuit detection pads.

13. The semiconductor device as claimed in claim 12, wherein each die region comprises a functional circuit, and the scribe line region is a non-functional region. 14 . The semiconductor device as claimed in claim 13 , wherein the plurality of bump pads are electrically connected to the functional circuit in the die region. 15 . The semiconductor device of claim 14 , wherein the functional circuit of each die region is tested via a plurality of probes electrically connected to an external testing device and placed on the plurality of circuit probing pads.

16. The semiconductor device as claimed in claim 12, wherein each circuit probing pad is larger than each bump pad. 17 . The semiconductor device as claimed in claim 12 , wherein a center of each circuit detection pad is disposed on a center line of the scribe line region.

18. The semiconductor device as claimed in claim 12, further comprising a plurality of copper pillar bumps disposed on the plurality of bump pads; wherein a cutting process is performed on the semiconductor wafer along one or more cutting paths, the one or more cutting paths are defined on the cutting area, and a part or all of a circuit detection pad is cut from the semiconductor wafer; wherein the die area, the plurality of bump pads and the plurality of copper pillar bumps are packaged into a semiconductor chip package; wherein the semiconductor chip package further comprises obtaining a retained cutting line structure and a retained circuit detection pad after the cutting process; wherein the die area is electrically connected to a substrate of a printed circuit board via the one or more copper pillar bumps using a flip chip package on the die area.