Clethodim-containing missible oil as well as preparation method and application thereof
By using specific surfactants and stabilizers in the formula of clethodim emulsifiable concentrate, the problem of easy decomposition of clethodim is solved, and the effect of high stability and low decomposition rate is achieved, making it suitable for the field of weeding.
Patent Information
- Application Number
- CN202410816667.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-24
- Publication Date
- 2024-10-11
AI Technical Summary
Clethodim is easily decomposed by heat, light and moisture, and the use of polar solvents and surfactants in existing formulas can easily accelerate its decomposition, resulting in poor stability and poor use effects.
Emulsifiable concentrate formula containing clethodim is used, using fatty alcohol polyoxyethylene ether, sorbitan trioleic acid polyoxyethylene ether and succinic acid sulfonate as surfactants, methyl oleate as synergist, and through modification Use longleaf acid as a stabilizer to avoid the use of polar solvents and alcohols to improve the decomposition rate and stability.
Significantly reduces the decomposition rate of clethodim, improves the stability and dilution stability of the emulsifiable concentrate, and ensures the long-term use effect of the product.
Smart Images

Figure BDA0004907872820000131
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of pesticides, and in particular to an emulsifiable concentrate containing clethodim and a preparation method and application thereof. Background Art
[0002] Clethodim is an organic compound with a molecular formula of C 17 H 26 C l NO 3 S, molecular weight is 359.91, light yellow liquid. The original drug of clethodim is an amber transparent liquid. Relative density is 1.15 (20℃), vapor pressure is 1.3×10Pa (20℃), soluble in a variety of organic solvents, unstable to light. Chemical name: (±)-2-[(E)-3-chloroallyloxyimino]propyl-5-[2-(ethylthio)propyl]-3-hydroxycyclohex-2-enone. It has excellent selectivity. It is suitable for controlling barnyard grass, wild oats, crabgrass, foxtail grass, goosegrass, foxtail grass, bluegrass, hard grass and other grass weeds in broad-leaved fields such as soybeans, rapeseed, cotton, and peanuts. After clethodim is applied, it can be quickly absorbed by the stems and leaves of grass weeds and transmitted to the stem tip and meristem, inhibiting the activity of meristems, destroying cell division, and ultimately leading to the death of weeds.
[0003] The factors that affect the decomposition of sethoxydim are mainly heat, light and moisture. From a technical point of view, the formulation system should not use highly polar substances (solvents and surfactants), especially substances containing hydroxyl groups, otherwise it will easily accelerate the decomposition of sethoxydim.
[0004] In view of the above situation, the present invention provides an emulsifiable concentrate containing clethodim and a preparation method and application thereof. Summary of the invention
[0005] The object of the present invention is to provide an emulsifiable concentrate containing clethodim, wherein the raw materials for preparing the emulsifiable concentrate include:
[0006] Clethodim
[0007] Surfactants
[0008] Synergist
[0009] Stabilizer
[0010] Solvent naphtha.
[0011] As an embodiment of the present invention, the raw materials for preparing the emulsifiable concentrate include, by mass percentage:
[0012] Clethodim 25%
[0013] Surfactant 9%
[0014] Synergist 30%
[0015] Stabilizer 10%
[0016] Solvent oil residue.
[0017] As an embodiment of the present invention, the surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate.
[0018] As an embodiment of the present invention, the surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate in a mass ratio of: (2-7): (1-6): (2-5).
[0019] As an embodiment of the present invention, the surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate in a mass ratio of 4:2:3.
[0020] As an embodiment of the present invention, the synergist is methyl oleate.
[0021] As an embodiment of the present invention, the stabilizer is a polymer stabilizer.
[0022] As an embodiment of the present invention, the stabilizer is modified palustric acid.
[0023] The second aspect of the present invention provides a method for preparing the emulsifiable concentrate containing clethodim, and the steps of the preparation method are as follows: after the original drug, emulsifier and solvent are evenly mixed, the remaining ingredients are added, and then stirred.
[0024] The third aspect of the present invention provides an emulsifiable concentrate containing clethodim, which is used in the field of weed control.
[0025] By adopting the above technical scheme, the present invention has the following beneficial effects: the emulsifiable concentrate containing clethodim prepared by the present invention has a low decomposition rate and high stability; and the emulsion dilution stability is qualified, and the particle size of the diluted liquid is small. DETAILED DESCRIPTION
[0026] The technical solution of the present invention will be described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0027] The object of the present invention is to provide an emulsifiable concentrate containing clethodim, wherein the raw materials for preparing the emulsifiable concentrate comprise, by mass percentage:
[0028] Clethodim 25%
[0029] Surfactant 9%
[0030] Synergist 30%
[0031] Stabilizer 10%
[0032] Solvent oil residue.
[0033] As an embodiment of the present invention, the surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate.
[0034] As an embodiment of the present invention, the surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate in a mass ratio of: (2-7): (1-6): (2-5).
[0035] As an embodiment of the present invention, the surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate in a mass ratio of 4:2:3.
[0036] As an embodiment of the present invention, the synergist is methyl oleate.
[0037] As an embodiment of the present invention, the stabilizer is a polymer stabilizer.
[0038] As an embodiment of the present invention, the stabilizer is modified palustric acid. In particular, the preparation method of the modified palustric acid is as follows:
[0039] S01: palustric acid, maleic anhydride and xylene are reacted at 190°C for 1.2 hours under an ammonia atmosphere to obtain compound 1;
[0040] Wherein, palustric acid: maleic anhydride: xylene = 4:5:1 (mass ratio);
[0041] S02 (1R, 2S, 3R, 4S, 5R)-8-azabicyclo (3.2.1) octane-1, 2, 3, 4-tetraol and potassium hydroxide were dehydrated, and propylene oxide was added in an ammonia atmosphere at 110°C and a pressure of 0.3 MPa, and the reaction was carried out for 1.5 hours. Ethylene oxide was added while maintaining the conditions, and the reaction was continued for 1.5 hours to obtain compound 2;
[0042] Among them, (1R,2S,3R,4S,5R)-8-azabicyclo(3.2.1)octane-1,2,3,4-tetraol:potassium hydroxide:propylene oxide:ethylene oxide=160:1.5:100:110 (mass ratio);
[0043] S03: dimethylformamide, compound 1, compound 2, and castor oil polyoxyethylene ether are completely dissolved, and concentrated sulfuric acid is added, and the mixture is reacted at 150° C. for 3 hours, and then dehydrated. Potassium hydroxide is added, and the mixture is dehydrated under an ammonia environment, and then vacuum stripped at 110° C. for 2 hours, and then propylene oxide is introduced, and the reaction is aged at 140° C. and a pressure of 0.3 MPa for 1.5 hours. Ethylene oxide is introduced under the same conditions, and the reaction is carried out for 1.5 hours. The polymer stabilizer is obtained by neutralization and filtration;
[0044] Among them, dimethylformamide: compound 1: compound 2: castor oil polyoxyethylene ether: concentrated sulfuric acid: potassium hydroxide: propylene oxide: ethylene oxide = 10:60:5:8:0.6:0.2:12:20 (mass ratio).
[0045] The second aspect of the present invention provides a method for preparing the emulsifiable concentrate containing clethodim, and the steps of the preparation method are as follows: after the original drug, emulsifier and solvent are evenly mixed, the remaining ingredients are added, and then stirred.
[0046] Due to the structural properties of sethoxydim itself, from the perspective of environmental factors, the factors affecting the decomposition of sethoxydim are mainly heat, light and moisture; from a technical perspective, the formulation system should not use highly polar substances (solvents and surfactants), especially hydroxyl-containing substances, otherwise it will easily accelerate the decomposition of sethoxydim.
[0047] On the one hand, polar solvents should not be used as solvents. It is recommended to use solvents with low polarity and no hydroxyl group, such as solvent oil. On the other hand, anionic surfactants in the formula, such as emulsifier 500#, should not contain alcohol substances, but should use solvent oil systems. A better choice is to choose anionic surfactants that do not use alcohol substances as solvents in the synthesis process, so as to avoid the influence of alcohol substances in the surfactants on sethoxydim from the source (because some anionic surfactants use alcohols as solvents in the synthesis process. Although the post-treatment process will recover the alcohol substances, there will still be trace amounts of alcohol remaining in the product).
[0048] Therefore, the present invention has found that the emulsifier obtained by compounding fatty alcohol polyoxyethylene ether and succinic acid sulfonate has qualified emulsion dilution stability; however, the particle size of the diluted liquid is not suitable, resulting in poor emulsification performance. Therefore, the present invention adds sorbitan trioleate polyoxyethylene ether to the emulsifier to improve the situation of inappropriate particle size of the diluted liquid. However, since it is found that the overall system decomposition rate is still relatively high, the modified palustric acid is added to obtain a clethodim emulsifiable concentrate preparation with a small decomposition rate and stable product performance.
[0049] Example 1
[0050] This embodiment provides an emulsifiable concentrate containing clethodim. The raw materials for preparing the emulsifiable concentrate include, by mass percentage:
[0051] Clethodim 25%
[0052] Surfactant 9%
[0053] Synergist 30%
[0054] Stabilizer 10%
[0055] Solvent oil residue.
[0056] The surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate in a mass ratio of 4:2:3.
[0057] The synergist is methyl oleate.
[0058] The stabilizer is modified palustric acid; the preparation method of the modified palustric acid is as follows:
[0059] S01: palustric acid, maleic anhydride and xylene are reacted at 190°C for 1.2 hours under an ammonia atmosphere to obtain compound 1;
[0060] Wherein, palustric acid: maleic anhydride: xylene = 4:5:1 (mass ratio);
[0061] S02 (1R, 2S, 3R, 4S, 5R)-8-azabicyclo (3.2.1) octane-1, 2, 3, 4-tetraol and potassium hydroxide were dehydrated, and propylene oxide was added in an ammonia atmosphere at 110°C and a pressure of 0.3 MPa, and the reaction was carried out for 1.5 hours. Ethylene oxide was added while maintaining the conditions, and the reaction was continued for 1.5 hours to obtain compound 2;
[0062] Among them, (1R,2S,3R,4S,5R)-8-azabicyclo(3.2.1)octane-1,2,3,4-tetraol:potassium hydroxide:propylene oxide:ethylene oxide=160:1.5:100:110 (mass ratio);
[0063] S03: dimethylformamide, compound 1, compound 2, and castor oil polyoxyethylene ether are completely dissolved, and concentrated sulfuric acid is added, and the mixture is reacted at 150° C. for 3 hours, and then dehydrated. Potassium hydroxide is added, and the mixture is dehydrated under an ammonia environment, and then vacuum stripped at 110° C. for 2 hours, and then propylene oxide is introduced, and the reaction is aged at 140° C. and a pressure of 0.3 MPa for 1.5 hours. Ethylene oxide is introduced under the same conditions, and the reaction is carried out for 1.5 hours. The polymer stabilizer is obtained by neutralization and filtration;
[0064] Among them, dimethylformamide: compound 1: compound 2: castor oil polyoxyethylene ether: concentrated sulfuric acid: potassium hydroxide: propylene oxide: ethylene oxide = 10:60:5:8:0.6:0.2:12:20 (mass ratio).
[0065] Example 2
[0066] This embodiment provides an emulsifiable concentrate containing clethodim. The raw materials for preparing the emulsifiable concentrate include, by mass percentage:
[0067] Clethodim 25%
[0068] Surfactant 9%
[0069] Synergist 30%
[0070] Stabilizer 10%
[0071] Solvent oil residue.
[0072] The surfactant comprises fatty alcohol polyoxyethylene ether and sorbitan trioleate polyoxyethylene ether in a mass ratio of 4:2.
[0073] The synergist is methyl oleate.
[0074] The stabilizer is modified palustric acid; the preparation method of the modified palustric acid is as follows:
[0075] S01: palustric acid, maleic anhydride and xylene are reacted at 190°C for 1.2 hours under an ammonia atmosphere to obtain compound 1;
[0076] Wherein, palustric acid: maleic anhydride: xylene = 4:5:1 (mass ratio);
[0077] S02 (1R, 2S, 3R, 4S, 5R)-8-azabicyclo (3.2.1) octane-1, 2, 3, 4-tetraol and potassium hydroxide were dehydrated, and propylene oxide was added in an ammonia atmosphere at 110°C and a pressure of 0.3 MPa, and the reaction was carried out for 1.5 hours. Ethylene oxide was added while maintaining the conditions, and the reaction was continued for 1.5 hours to obtain compound 2;
[0078] Among them, (1R,2S,3R,4S,5R)-8-azabicyclo(3.2.1)octane-1,2,3,4-tetraol:potassium hydroxide:propylene oxide:ethylene oxide=160:1.5:100:110 (mass ratio);
[0079] S03: dimethylformamide, compound 1, compound 2, and castor oil polyoxyethylene ether are completely dissolved, and concentrated sulfuric acid is added, and the mixture is reacted at 150° C. for 3 hours, and then dehydrated. Potassium hydroxide is added, and the mixture is dehydrated under an ammonia environment, and then vacuum stripped at 110° C. for 2 hours, and then propylene oxide is introduced, and the reaction is aged at 140° C. and a pressure of 0.3 MPa for 1.5 hours. Ethylene oxide is introduced under the same conditions, and the reaction is carried out for 1.5 hours. The polymer stabilizer is obtained by neutralization and filtration;
[0080] Among them, dimethylformamide: compound 1: compound 2: castor oil polyoxyethylene ether: concentrated sulfuric acid: potassium hydroxide: propylene oxide: ethylene oxide = 10:60:5:8:0.6:0.2:12:20 (mass ratio).
[0081] Example 3
[0082] This embodiment provides an emulsifiable concentrate containing clethodim. The raw materials for preparing the emulsifiable concentrate include, by mass percentage:
[0083] Clethodim 25%
[0084] Surfactant 9%
[0085] Synergist 30%
[0086] Stabilizer 10%
[0087] Solvent oil residue.
[0088] The surfactant comprises fatty alcohol polyoxyethylene ether and succinic acid sulfonate in a mass ratio of 4:3.
[0089] The synergist is methyl oleate.
[0090] The stabilizer is modified palustric acid; the preparation method of the modified palustric acid is as follows:
[0091] S01: palustric acid, maleic anhydride and xylene are reacted at 190°C for 1.2 hours under an ammonia atmosphere to obtain compound 1;
[0092] Wherein, palustric acid: maleic anhydride: xylene = 4:5:1 (mass ratio);
[0093] S02 (1R, 2S, 3R, 4S, 5R)-8-azabicyclo (3.2.1) octane-1, 2, 3, 4-tetraol and potassium hydroxide were dehydrated, and propylene oxide was added in an ammonia atmosphere at 110°C and a pressure of 0.3 MPa, and the reaction was carried out for 1.5 hours. Ethylene oxide was added while maintaining the conditions, and the reaction was continued for 1.5 hours to obtain compound 2;
[0094] Among them, (1R,2S,3R,4S,5R)-8-azabicyclo(3.2.1)octane-1,2,3,4-tetraol:potassium hydroxide:propylene oxide:ethylene oxide=160:1.5:100:110 (mass ratio);
[0095] S03: dimethylformamide, compound 1, compound 2, and castor oil polyoxyethylene ether are completely dissolved, and concentrated sulfuric acid is added, and the mixture is reacted at 150° C. for 3 hours, and then dehydrated. Potassium hydroxide is added, and the mixture is dehydrated under an ammonia environment, and then vacuum stripped at 110° C. for 2 hours, and then propylene oxide is introduced, and the reaction is aged at 140° C. and a pressure of 0.3 MPa for 1.5 hours. Ethylene oxide is introduced under the same conditions, and the reaction is carried out for 1.5 hours. The polymer stabilizer is obtained by neutralization and filtration;
[0096] Among them, dimethylformamide: compound 1: compound 2: castor oil polyoxyethylene ether: concentrated sulfuric acid: potassium hydroxide: propylene oxide: ethylene oxide = 10:60:5:8:0.6:0.2:12:20 (mass ratio).
[0097] Example 4
[0098] This embodiment provides an emulsifiable concentrate containing clethodim. The raw materials for preparing the emulsifiable concentrate include, by mass percentage:
[0099] Clethodim 25%
[0100] Surfactant 9%
[0101] Synergist 30%
[0102] Stabilizer 10%
[0103] Solvent oil residue.
[0104] The surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate in a mass ratio of 1:1:1.
[0105] The synergist is methyl oleate.
[0106] The stabilizer is modified palustric acid; the preparation method of the modified palustric acid is as follows:
[0107] S01: palustric acid, maleic anhydride and xylene are reacted at 190°C for 1.2 hours under an ammonia atmosphere to obtain compound 1;
[0108] Wherein, palustric acid: maleic anhydride: xylene = 4:5:1 (mass ratio);
[0109] S02 (1R, 2S, 3R, 4S, 5R)-8-azabicyclo (3.2.1) octane-1, 2, 3, 4-tetraol and potassium hydroxide were dehydrated, and propylene oxide was added in an ammonia atmosphere at 110°C and a pressure of 0.3 MPa, and the reaction was carried out for 1.5 hours. Ethylene oxide was added while maintaining the conditions, and the reaction was continued for 1.5 hours to obtain compound 2;
[0110] Among them, (1R,2S,3R,4S,5R)-8-azabicyclo(3.2.1)octane-1,2,3,4-tetraol:potassium hydroxide:propylene oxide:ethylene oxide=160:1.5:100:110 (mass ratio);
[0111] S03: dimethylformamide, compound 1, compound 2, and castor oil polyoxyethylene ether are completely dissolved, and concentrated sulfuric acid is added, and the mixture is reacted at 150° C. for 3 hours, and then dehydrated. Potassium hydroxide is added, and the mixture is dehydrated under an ammonia environment, and then vacuum stripped at 110° C. for 2 hours, and then propylene oxide is introduced, and the reaction is aged at 140° C. and a pressure of 0.3 MPa for 1.5 hours. Ethylene oxide is introduced under the same conditions, and the reaction is carried out for 1.5 hours. The polymer stabilizer is obtained by neutralization and filtration;
[0112] Among them, dimethylformamide: compound 1: compound 2: castor oil polyoxyethylene ether: concentrated sulfuric acid: potassium hydroxide: propylene oxide: ethylene oxide = 10:60:5:8:0.6:0.2:12:20 (mass ratio).
[0113] Example 5
[0114] This embodiment provides an emulsifiable concentrate containing clethodim. The raw materials for preparing the emulsifiable concentrate include, by mass percentage:
[0115] Clethodim 25%
[0116] Surfactant 9%
[0117] Synergist 30%
[0118] Stabilizer 10%
[0119] Solvent oil residue.
[0120] The surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate in a mass ratio of 2:3:4.
[0121] The synergist is methyl oleate.
[0122] The stabilizer is modified palustric acid; the preparation method of the modified palustric acid is as follows:
[0123] S01: palustric acid, maleic anhydride and xylene are reacted at 190°C for 1.2 hours under an ammonia atmosphere to obtain compound 1;
[0124] Wherein, palustric acid: maleic anhydride: xylene = 4:5:1 (mass ratio);
[0125] S02 (1R, 2S, 3R, 4S, 5R)-8-azabicyclo (3.2.1) octane-1, 2, 3, 4-tetraol and potassium hydroxide were dehydrated, and propylene oxide was added in an ammonia atmosphere at 110°C and a pressure of 0.3 MPa, and the reaction was carried out for 1.5 hours. Ethylene oxide was added while maintaining the conditions, and the reaction was continued for 1.5 hours to obtain compound 2;
[0126] Among them, (1R,2S,3R,4S,5R)-8-azabicyclo(3.2.1)octane-1,2,3,4-tetraol:potassium hydroxide:propylene oxide:ethylene oxide=160:1.5:100:110 (mass ratio);
[0127] S03: dimethylformamide, compound 1, compound 2, and castor oil polyoxyethylene ether are completely dissolved, and concentrated sulfuric acid is added, and the mixture is reacted at 150° C. for 3 hours, and then dehydrated. Potassium hydroxide is added, and the mixture is dehydrated under an ammonia environment, and then vacuum stripped at 110° C. for 2 hours, and then propylene oxide is introduced, and the reaction is aged at 140° C. and a pressure of 0.3 MPa for 1.5 hours. Ethylene oxide is introduced under the same conditions, and the reaction is carried out for 1.5 hours. The polymer stabilizer is obtained by neutralization and filtration;
[0128] Among them, dimethylformamide: compound 1: compound 2: castor oil polyoxyethylene ether: concentrated sulfuric acid: potassium hydroxide: propylene oxide: ethylene oxide = 10:60:5:8:0.6:0.2:12:20 (mass ratio).
[0129] Example 6
[0130] This embodiment provides an emulsifiable concentrate containing clethodim. The raw materials for preparing the emulsifiable concentrate include, by mass percentage:
[0131] Clethodim 25%
[0132] Surfactant 9%
[0133] Synergist 30%
[0134] Solvent oil residue.
[0135] The surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate in a mass ratio of 4:2:3.
[0136] The synergist is methyl oleate.
[0137] Example 7
[0138] This embodiment provides an emulsifiable concentrate containing clethodim. The raw materials for preparing the emulsifiable concentrate include, by mass percentage:
[0139] Clethodim 25%
[0140] Surfactant 9%
[0141] Synergist 30%
[0142] Stabilizer 10%
[0143] Solvent oil residue.
[0144] The surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate in a mass ratio of 4:2:3.
[0145] The synergist is methyl oleate.
[0146] The stabilizer is modified rosin acid; the preparation method of the modified rosin acid is as follows:
[0147] S01: Abietic acid, maleic anhydride and xylene are reacted at 190°C for 1.2 hours under an ammonia atmosphere to obtain compound 1;
[0148] Wherein, rosin acid: maleic anhydride: xylene = 4:5:1 (mass ratio);
[0149] S02 (1R, 2S, 3R, 4S, 5R)-8-azabicyclo (3.2.1) octane-1, 2, 3, 4-tetraol and potassium hydroxide were dehydrated, and propylene oxide was added in an ammonia atmosphere at 110°C and a pressure of 0.3 MPa, and the reaction was carried out for 1.5 hours. Ethylene oxide was added while maintaining the conditions, and the reaction was continued for 1.5 hours to obtain compound 2;
[0150] Among them, (1R,2S,3R,4S,5R)-8-azabicyclo(3.2.1)octane-1,2,3,4-tetraol:potassium hydroxide:propylene oxide:ethylene oxide=160:1.5:100:110 (mass ratio);
[0151] S03: dimethylformamide, compound 1, compound 2, and castor oil polyoxyethylene ether are completely dissolved, and concentrated sulfuric acid is added, and the mixture is reacted at 150° C. for 3 hours, and then dehydrated. Potassium hydroxide is added, and the mixture is dehydrated under an ammonia environment, and then vacuum stripped at 110° C. for 2 hours, and then propylene oxide is introduced, and the reaction is aged at 140° C. and a pressure of 0.3 MPa for 1.5 hours. Ethylene oxide is introduced under the same conditions, and the reaction is carried out for 1.5 hours. The polymer stabilizer is obtained by neutralization and filtration;
[0152] Among them, dimethylformamide: compound 1: compound 2: castor oil polyoxyethylene ether: concentrated sulfuric acid: potassium hydroxide: propylene oxide: ethylene oxide = 10:60:5:8:0.6:0.2:12:20 (mass ratio).
[0153] Performance Testing
[0154] The emulsion stability of the preparations obtained in Examples 1-7 was tested according to the following standard: the sample was diluted 200 times with 342 ppm standard hard water, and the emulsion stability test method (GB / T1603-2001) was used. The sample was qualified if there was no floating oil or precipitation above or below. The precipitation of floating oil, floating cream and precipitation at 0.5h, 2h and 24h was recorded.
[0155] Thermal storage stability: Store the product in a (54±2)℃ constant temperature oven for 2 weeks to accelerate aging and predict the performance changes of the product after 2 years of storage at room temperature. The product is qualified if the test decomposition rate is less than or equal to 5%.
[0156] Cold storage stability: Store in a (0±1)℃ refrigerator for 1 week. If there is no visible precipitate, it is qualified.
[0157] Table 1 Determination of various indicators of emulsifiable concentrate
[0158] Group 0.5h 2h 24h Example 1 qualified qualified good Example 2 qualified qualified 0.5mL floating oil Example 3 qualified qualified White granular sediment Example 4 qualified qualified 0.5mL floating ointment Example 5 qualified qualified 0.5mL floating ointment Example 6 qualified qualified 2.5mL floating ointment Example 7 qualified qualified 0.5mL floating ointment
[0159] Table 2 Hot storage test
[0160] Group Decomposition rate Thermal storage stability Cold storage stability Example 1 1.8% qualified qualified Example 2 3.9% qualified qualified Example 3 4.3% Failure qualified Example 4 2.4% qualified qualified Example 5 2.3% qualified qualified Example 6 9.5% Failure Failure Example 7 4.2% qualified qualified
[0161] Field efficacy testing
[0162] Field test on the efficacy of 25% clethodim emulsifiable concentrate in controlling annual grass weeds in rapeseed fields
[0163] Experimental crop: rapeseed, variety: Zhejiang oil 51.
[0164] Targets of prevention and control: Alopecurus aequalis and Beckmannia syzigachne.
[0165] The trial starts on February 14, 2021.
[0166] Test completion time: 2021.5.9.
[0167] The experimental field covers an area of about 2 mu. The experimental field is located in Xinggongshan Village, Dongpu Town, Shaoxing City, Zhejiang Province. GPS positioning: 120°31'33" east longitude, 30°0'34" north latitude. The soil type, rapeseed variety, transplanting density, transplanting time, fertility level, etc. are consistent, and scientific cultivation and management techniques are used for management. The cultivation and management conditions are consistent and meet the test requirements.
[0168] Test crop: rapeseed; variety: Zhejiang Oil 51. Transplanted on November 6, 2020, with a row spacing of 30cm*40cm. When the pesticide was applied, the rapeseed was in the seedling stage. The soil in the test site was yellow purple mud with a pH of 6.50-6.70. Water and fertilizer management was the same as that of conventional rapeseed fields, and manual weeding was carried out once in the manual weeding treatment area 7 days after the pesticide was applied. It was sunny when the pesticide was applied, with a west wind of 1.0-1.3m / s, a temperature of 19.5-20.8℃, and a relative humidity of 79.8%-80.4%.
[0169] Weeds at 3-5 leaf stage, rapeseed seedling stage, stem and leaf spraying. The backpack electric sprayer 3WBD-16 produced by Beijing Zhongbao Green Agriculture Group has a fan-shaped nozzle (110-03) and a working pressure of 0.2-0.4MPa.
[0170] Table 3 Experimental treatment design
[0171] Processing number Drug Name Active ingredient dosage (g / hectare) A Example 1 54 B Example 3 54 C Example 4 54 D Example 6 54 E Example 7 54 F Manual weeding / G Blank control /
[0172] Plant control effect (%) = (number of weeds in the blank control area - number of weeds in the treatment area) / number of weeds in the blank control area * 100
[0173] Fresh weight control effect (%) = (fresh weight of weeds in blank control area - fresh weight of weeds in treatment area) / fresh weight of weeds in blank control area * 100
[0174] Table 4 Test results
[0175]
[0176] Therefore, the test agent, sethoxydim emulsifiable concentrate, can be used to control grass weeds in rapeseed fields.
[0177] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. An emulsifiable concentrate containing clethodim, characterized in that: The raw materials for preparing the emulsifiable concentrate include: Clethodim Surfactants Synergist Stabilizer Solvent naphtha.
2. The emulsifiable concentrate containing clethodim according to claim 1, characterized in that: According to mass percentage, the raw materials for preparing the emulsifiable concentrate include: Clethodim 25% Surfactant 9% Synergist 30% Stabilizer 10% Solvent oil residue.
3. The emulsifiable concentrate containing clethodim according to claim 1, characterized in that: The surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate.
4. The emulsifiable concentrate containing clethodim according to claim 3, characterized in that: The surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate in a mass ratio of: (2-7): (1-6): (2-5).
5. The emulsifiable concentrate containing clethodim according to claim 1, characterized in that: The surfactant comprises fatty alcohol polyoxyethylene ether, sorbitan trioleate polyoxyethylene ether and succinic acid sulfonate in a mass ratio of 4:2:
3.
6. The emulsifiable concentrate containing clethodim according to claim 1, characterized in that: The synergist is methyl oleate.
7. The emulsifiable concentrate containing clethodim according to claim 1, characterized in that: The stabilizer is a polymer stabilizer.
8. The emulsifiable concentrate containing clethodim according to claim 7, characterized in that: The stabilizer is modified palustric acid.
9. The method for preparing an emulsifiable concentrate containing clethodim according to any one of claims 1 to 8, characterized in that: The preparation method comprises the following steps: mixing the original drug, the emulsifier and the solvent evenly, adding the remaining ingredients, and then stirring.
10. An emulsifiable concentrate containing clethodim according to any one of claims 1 to 8, characterized in that: Used in the field of weed control.