Preparation method of DTC device

By combining the ALD and PVD processes to deposit a metal layer in the preparation of DTC devices, and forming a multi-layer film structure on the substrate and trench surface, the problem of insufficient thickness of the metal layer deposited by the PVD process is solved, the product yield is improved and the production cost is reduced. cost.

CN118763076APending Publication Date: 2024-10-11HUA HONG SEMICON WUXI LTD +1
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410867445.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-28
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

During the preparation process of DTC devices, the thickness of the metal electrode formed by depositing the metal layer through the PVD process is difficult to meet the requirements of the etching stop layer, which affects the product yield.

Method used

The ALD process and the PVD process are combined to sequentially deposit metal layers to form the lower electrode layer or upper electrode layer of the MIM capacitor, and form a multi-layer film structure on the surface of the substrate and trench. The dielectric layer is composed of high dielectric constant material, and is heated by thermal The oxidation process creates a linear oxide layer to improve coverage.

Benefits of technology

It solves the problem of insufficient thickness of the covering film caused by the metal layer deposited by the PVD process. It also avoids the high production cost and high resistivity caused by the ALD process and improves the product yield.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118763076A_ABST
    Figure CN118763076A_ABST
Patent Text Reader

Abstract

The preparation method of the DTC device comprises the steps that a substrate is provided, a groove is formed in the substrate, and the ratio of the depth to the width of the groove is larger than 4; sequentially forming at least one layer of MIM capacitor multilayer film structure on the surfaces of the substrate and the groove, wherein the MIM capacitor multilayer film structure sequentially comprises a lower electrode layer, a dielectric layer and an upper electrode layer from bottom to top; wherein in the process of forming the lower electrode layer and the upper electrode layer, the lower electrode layer or the upper electrode layer is formed by depositing a metal layer through an ALD (Atomic Layer Deposition) process and a PVD (Physical Vapor Deposition) process in sequence. In the preparation process of the DTC device, the metal layer is deposited through the ALD technology and the PVD technology in sequence to form the lower electrode layer or the upper electrode layer of the MIM capacitor, so that the problem that the thickness of a covering film on the side wall and the bottom of a groove is small due to the fact that the metal layer is deposited only through the PVD technology is solved; and meanwhile, the problems of high production cost and high resistivity caused by depositing the metal layer only through the ALD process are solved, and the product yield is improved while the production cost of the product is kept.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor devices and integrated circuit technology, and in particular to a method for preparing a DTC device. Background Art

[0002] Compared with traditional planar capacitors, deep trench capacitors (DTC) have a three-dimensional structure and can achieve ultra-high capacitance density, thus being widely used. Generally, DTC devices are composed of metal electrodes and high dielectric constant (high k) dielectric layers (dielectrics with dielectric constants greater than 3). After alternately depositing metal layers and high k dielectric layers in the trenches for multiple times, parallel capacitors are formed through metal interconnections, thereby further improving capacitance density.

[0003] In the process of manufacturing the metal electrode of the DTC device, a physical vapor deposition (PVD) process is usually used to deposit a metal layer as the metal electrode of the capacitor. When a groove for a metal contact (CT) needs to be etched in the subsequent process, the upper metal electrode needs to be used as an etch stop layer. However, due to the poor step coverage ability of the PVD process, the thickness of the metal layer deposited by the PVD process is difficult to meet the requirements of the etch stop layer, thereby affecting the yield of the product. Summary of the invention

[0004] The present application provides a method for preparing a DTC device, which can solve the problem of poor product yield caused by depositing metal electrodes of MIM capacitors through a PVD process in the DTC preparation method provided in the related art. The method comprises:

[0005] Providing a substrate, wherein a groove is formed in the substrate, and the ratio of the depth to the width of the groove is greater than 4;

[0006] At least one MIM capacitor multilayer film structure is sequentially formed on the surface of the substrate and the groove, wherein the MIM capacitor multilayer film structure includes a lower electrode layer, a dielectric layer and an upper electrode layer from bottom to top, and the MIM capacitor multilayer film structures are isolated by the dielectric layer;

[0007] In the process of forming the lower electrode layer and the upper electrode layer, the metal layer is deposited in sequence through the ALD process and the PVD process to form the lower electrode layer or the upper electrode layer.

[0008] In some embodiments, the metal layer includes at least one of a titanium nitride layer, a titanium layer, a nickel layer, a tantalum layer, and a tantalum nitride layer.

[0009] In some embodiments, the dielectric layer may be made of a material having a dielectric constant greater than 3.

[0010] In some embodiments, the dielectric layer includes at least one of an aluminum oxide layer, a zirconium dioxide layer, a hafnium dioxide layer, a tantalum pentoxide layer, a niobium pentoxide layer, a titanium dioxide layer, and a yttrium oxide layer.

[0011] In some embodiments, at least one MIM capacitor multilayer film structure is sequentially formed on the surface of the substrate and the groove, further comprising:

[0012] forming a linear oxide layer on the substrate and the surface of the groove;

[0013] At least one MIM capacitor multilayer film structure is sequentially formed on the linear oxide layer.

[0014] In some embodiments, forming a linear oxide layer on the substrate and the groove surface includes:

[0015] The linear oxide layer is formed on the substrate and the surface of the trench by a thermal oxidation process.

[0016] The technical solution of this application has at least the following advantages:

[0017] In the preparation process of the DTC device, the metal layer is deposited by the ALD process and the PVD process in sequence to form the lower electrode layer or the upper electrode layer of the MIM capacitor, thereby solving the problem of thin thickness of the side wall and bottom covering film of the groove caused by depositing the metal layer only by the PVD process. At the same time, it also solves the problem of high production cost and high resistivity caused by depositing the metal layer only by the ALD process, thereby improving the product yield while maintaining the production cost of the product. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0019] Figure 1 is a flow chart of a method for preparing a DTC device provided by an exemplary embodiment of the present application;

[0020] Figures 2 to 4 It is a schematic diagram of preparing the first metal layer in the preparation process of a DTC device provided by an exemplary embodiment of the present application. DETAILED DESCRIPTION

[0021] The following will be combined with the accompanying drawings to clearly and completely describe the technical solutions in this application. Obviously, the described embodiments are part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0022] In the description of the present application, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present application. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.

[0023] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, it can also be the internal connection of two components, it can be a wireless connection, or it can be a wired connection. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0024] In addition, the technical features involved in the different embodiments of the present application described below can be combined with each other as long as they do not conflict with each other.

[0025] refer to Figure 1 , which shows a flow chart of a method for preparing a DTC device provided by an exemplary embodiment of the present application, such as Figure 1 As shown, the method includes:

[0026] Step S1, providing a substrate, wherein a groove is formed in the substrate, and the ratio of the depth to the width of the groove is greater than 4.

[0027] Step S2, at least one MIM capacitor multilayer film structure is formed in sequence on the surface of the substrate and the groove, and the MIM capacitor multilayer film structure includes a lower electrode layer, a capacitor dielectric layer and an upper electrode layer from bottom to top. In the process of forming the lower electrode layer and the upper electrode layer, the metal layer is deposited in sequence through the ALD process and the PVD process to form the lower electrode layer or the upper electrode layer.

[0028] Before forming the MIM capacitor multilayer film structure, a linear oxide layer can be formed on the substrate and the groove surface (to repair the surface morphology of the groove and the substrate), and then at least one metal-insulator-metal (MIM) capacitor multilayer film structure is sequentially formed on the linear oxide layer, and a dielectric layer is formed between each layer of the MIM capacitor multilayer film structure. The preparation of the electrode layer of the MIM capacitor multilayer film structure is described below, taking the first lower electrode layer as an example:

[0029] refer to Figure 2 , which shows a cross-sectional schematic diagram after the linear oxide layer is formed; reference Figure 3 , which shows a schematic cross-sectional view of a metal layer after being deposited by an atomic layer deposition (ALD) process; Figure 4 , which shows a cross-sectional schematic diagram after a metal layer is deposited by a PVD process.

[0030] For example, Figures 2 to 4 As shown, a groove 201 is formed in the substrate 210, and the groove 201 is a groove with a high aspect ratio (i.e., the ratio of depth to width is greater than 4). A linear oxide layer 210 can be formed on the surface of the substrate 210 and the groove 201 by a thermal oxidation process, a first metal layer 231 is deposited on the linear oxide layer 210 by an ALD process, and a second metal layer 232 is deposited on the first metal layer 231 by a PVD process. The first metal layer 231 and the second metal layer 232 constitute the lower electrode layer of the first MIM capacitor multilayer film structure. In the subsequent process, a dielectric layer can be deposited on the second metal layer 232, and a metal layer is deposited on the dielectric layer by an ALD process and a PVD process in sequence to form an upper electrode layer of the first MIM capacitor multilayer film structure, and so on, and each time a MIM capacitor multilayer film structure is formed, a dielectric layer is deposited for isolation. Since the ALD process has a strong step coverage capability, the PVD process is used to deposit the metal layer to supplement the ALD process, thereby avoiding the high production cost (caused by the slow deposition rate) and high resistivity caused by using the ALD process to deposit the electrode layer.

[0031] In the embodiment of the present application, when the ALD process and the PVD process are performed to deposit a metal layer, the optional parameter value ranges are as follows: (1) The temperature affects the resistivity, deposition rate and step coverage of the metal layer formed in the ALD deposition process, and its value is usually lower than 420 degrees Celsius (°C); (2) The pressure affects the gas ionization rate and the mean free path of atomic motion in the ALD process and the PVD process, and its value is usually 0.1 Pascal (Pa) to 1 Pascal; (3) The vacuum degree affects the purity of the film in the ALD process and the PVD process, and its value is usually less than 5×10-7 Torr.

[0032] In an embodiment of the present application, the metal layer constituting the electrode layer (upper electrode layer or lower electrode layer) includes at least one of a titanium nitride (TiN) layer, a titanium (Ti) layer, a nickel (Ni) layer, a tantalum (Ta) layer and a tantalum nitride (TaN) layer; the dielectric layer includes a high dielectric constant layer, which includes at least one of an aluminum oxide (Al2O3) layer, a zirconium dioxide (ZrO2) layer, a hafnium dioxide (HfO2) layer, a tantalum pentoxide (Ta2O5) layer, a niobium pentoxide (Nb2O5) layer, a titanium dioxide (TiO2) layer and a yttrium oxide (Y2O3) layer.

[0033] To summarize, in the embodiment of the present application, during the preparation process of the DTC device, the metal layer is deposited sequentially through the ALD process and the PVD process to form the lower electrode layer or the upper electrode layer of the MIM capacitor, thereby solving the problem of thin thickness of the side wall and bottom covering film of the groove caused by depositing the metal layer only through the PVD process. At the same time, it also solves the problem of high production cost and high resistivity caused by depositing the metal layer only through the ALD process, thereby improving the product yield while maintaining the production cost of the product.

[0034] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection created by this application.

Claims

1. A method for preparing a DTC device, It is characterized in that include: Providing a substrate, wherein a groove is formed in the substrate, and the ratio of the depth to the width of the groove is greater than 4; At least one MIM capacitor multilayer film structure is sequentially formed on the surface of the substrate and the groove, wherein the MIM capacitor multilayer film structure includes a lower electrode layer, a dielectric layer and an upper electrode layer from bottom to top, and the MIM capacitor multilayer film structures are isolated by the dielectric layer; In the process of forming the lower electrode layer and the upper electrode layer, the metal layer is deposited in sequence through the ALD process and the PVD process to form the lower electrode layer or the upper electrode layer.

2. The method according to claim 1, It is characterized in that The metal layer includes at least one of a titanium nitride layer, a titanium layer, a nickel layer, a tantalum layer and a tantalum nitride layer.

3. The method according to claim 2, It is characterized in that The dielectric constant of the material constituting the dielectric layer is greater than 3.

4. The method according to claim 3, It is characterized in that The dielectric layer includes at least one of an aluminum oxide layer, a zirconium dioxide layer, a hafnium dioxide layer, a tantalum pentoxide layer, a niobium pentoxide layer, a titanium dioxide layer and a yttrium oxide layer.

5. The method according to any one of claims 1 to 4, It is characterized in that The method further comprises: forming at least one MIM capacitor multilayer film structure in sequence on the surface of the substrate and the groove; forming a linear oxide layer on the substrate and the surface of the groove; At least one MIM capacitor multilayer film structure is sequentially formed on the linear oxide layer.

6. The method according to claim 5, It is characterized in that The forming of a linear oxide layer on the substrate and the groove surface comprises: The linear oxide layer is formed on the substrate and the surface of the trench by a thermal oxidation process.

Citation Information

Cited By

  • 3D capacitor and preparation method thereof

    CN121368183A