Preparation method of VCSEL chip
Through the method based on epitaxial layer peeling and bonding transfer, the problem of heat accumulation in VCSEL chips is solved, the heat dissipation capacity and comprehensive performance are significantly improved, and efficient heat dissipation and performance improvement are achieved.
Patent Information
- Application Number
- CN202410821428.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-24
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2044-06-24
AI Technical Summary
Heat accumulation in VCSEL chips during the working process causes the deterioration of threshold current, threshold voltage and output power, reducing the efficiency and stability of the device. High-emission power laser chips have higher requirements for heat dissipation design.
A VCSEL chip preparation method based on epitaxial layer peeling and bonding transfer is used, including growing a buffer layer and a DBR structure on the substrate to form a mesa-type device structure, temporarily bonding the support carrier, thinning the substrate, and removing the remaining substrate and buffer layer to form a highly thermally conductive substrate for permanent bonding, significantly improving heat dissipation efficiency.
It significantly improves the heat dissipation capacity of the VCSEL chip and improves the overall performance of the device, including increasing the laser output power and emission spectrum purity, simplifying the structure and process, and achieving excellent heat dissipation efficiency.
Smart Images

Figure CN118783233A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of semiconductors, and in particular to a method for preparing a VCSEL chip. Background Art
[0002] VCSEL (Vertical-cavity surface-emitting laser), or vertical cavity surface emitting laser, is a laser whose laser emission direction is perpendicular to the substrate surface. It has the advantages of low threshold current, high quantum efficiency, large modulation bandwidth and low energy consumption, and has broad application prospects in atomic clocks, optical communications, solid-state laser pumping and other fields. Since VCSEL uses DBR as the reflector of the laser cavity, its active area is very small. The reduction in volume makes the heat dissipation of the active area of the device difficult. A large amount of heat will be generated during operation, and the accumulation of heat in the active area will cause the threshold current, threshold voltage, output power, etc. to deteriorate, thereby reducing the efficiency and stability of the device, and even damaging the chip. In addition, with the demand for higher emission power laser chips in application scenarios such as lidar and security lighting, higher requirements are placed on the heat dissipation design of VCSEL. Summary of the invention
[0003] The present invention aims to solve the problem that heat cannot be effectively dissipated in current VCSEL applications, and proposes a method for preparing a VCSEL chip based on epitaxial layer peeling and bonding transfer, which can effectively improve the heat dissipation capacity of the device and enhance the overall performance of the device.
[0004] The technical solution to achieve the purpose of the present invention is: a method for preparing a VCSEL chip, comprising the following steps:
[0005] 1) A buffer layer, a stop layer, an N-contact layer, an N-DBR, an active layer, a P-DBR and a P-contact layer are sequentially grown on the front side of substrate A;
[0006] 2) Make a P contact metal on the P contact layer, then etch the epitaxial structure to the stop layer to form a mesa-type VCSEL device structure, and oxidize its surface;
[0007] 3) Spin-coating a temporary adhesive on the surface of substrate A to cover the device structure;
[0008] 4) temporarily bonding the substrate A to the front side of the support carrier;
[0009] 5) thinning the substrate A temporarily bonded to the support carrier from the back side;
[0010] 6) removing the remaining substrate and the buffer layer except the epitaxial layer from the substrate A temporarily bonded to the support carrier to expose the back side of the stop layer;
[0011] 7) removing the stop layer to obtain a VCSEL epitaxial layer structure temporarily bonded to the support carrier and exposing the back side of the N contact layer;
[0012] 8) preparing an N electrode on the back side of the N contact layer;
[0013] 9) Preparing a bonding metal layer on the front side of another high thermal conductivity substrate B;
[0014] 10) The back N electrode of the VCSEL epitaxial layer temporarily bonded to the support carrier is placed opposite to the front surface of the B substrate and permanently bonded through the bonding metal layer;
[0015] 11) Debonding the permanent bonding structure formed by the support carrier, substrate B and VCSEL epitaxial layer, and cleaning it;
[0016] 12) A VCSEL chip formed on a high thermal conductive substrate B is obtained.
[0017] Furthermore, the material of substrate A in step 1) includes but is not limited to InP, GaAs or GaN, the thickness of substrate A is 100 μm to 1000 μm, the stop layer is InGaAs, InGaP, AlN or InGaAsP, and the thickness of VCSEL epitaxial layer is 500 nm to 15 μm.
[0018] Furthermore, in step 2), the P electrode material is TiPtAu, WTiAuTi or NiAlAu, the electrode thickness is 50nm to 1000nm, the etching gas is chlorine-based or fluorine-based gas, and the oxidation method is wet or dry oxidation.
[0019] Furthermore, the adhesive in step 3) is a polymer, including but not limited to one of photoresist, high temperature wax or BCB, and the thickness of the adhesive is 1 μm to 40 μm.
[0020] Furthermore, the support carrier in step 4) includes but is not limited to one of sapphire, silicon, silicon carbide or aluminum nitride wafers, the thickness of the support carrier is 300μm-1200μm, the temporary bonding temperature is 90-230°C, the pressure is 10MPa-50MPa, and the time is 10-60 minutes.
[0021] Furthermore, the substrate thinning method in step 5) is any one or more of mechanical grinding, mechanical polishing, and chemical polishing, and the remaining substrate thickness after thinning is not less than 10 μm and not more than 120 μm.
[0022] Furthermore, the method for removing the remaining substrate in step 6) is wet etching or dry etching, and the ratio of the removal rate of the substrate and the stop layer material by the removal method is 5:1 to 500:1.
[0023] Furthermore, the removal method of the stop layer in step 7) is wet etching or dry etching, and the ratio of the removal rate of the stop layer and the N-contact layer material by the removal method is 5:1 to 500:1.
[0024] Furthermore, the N electrode material in step 8) is AuGeNiAu, TiPtAu, WTiAuTi or NiPdAu, and the electrode thickness is 50nm to 1000μm.
[0025] Furthermore, the substrate B in step 9) includes but is not limited to one of silicon carbide, aluminum nitride, and diamond wafer, and the thickness of substrate B is between 100μm and 1000μm; the bonding metal layer includes but is not limited to TiAu, TiPtAu, WTiAu, AuSn or AuIn, and the thickness of the bonding metal layer is between 100nm-3μm.
[0026] Furthermore, the permanent bonding method in step 10) includes but is not limited to one of eutectic bonding, hot pressing bonding, activation bonding and direct bonding, the bonding temperature is room temperature to 300°C, the bonding time is 5 minutes to 2 hours, and the bonding pressure is 200N to 50000N.
[0027] Furthermore, the debonding method in step 11) includes but is not limited to thermal debonding, laser debonding and gas debonding; the cleaning solvent includes but is not limited to acetone, alcohol or isopropanol.
[0028] The method for preparing a VCSEL chip with efficient heat dissipation effect of the present invention has at least the following advantages: 1) the original semiconductor epitaxial substrate is removed, and the N electrode is directly led out through a metal bonding layer with extremely low resistivity, thereby reducing the series resistance introduced by the semiconductor substrate in the original device, which helps to improve the device performance; 2) the original substrate with low thermal conductivity is removed, and is bonded to a high thermal conductivity substrate through a high thermal conductivity metal, which can significantly improve the heat dissipation efficiency, help to increase the laser output power, improve the emission spectrum purity, and improve the comprehensive performance of the VCSEL laser; 3) the VCSEL chip prepared by the method has the advantages of simple structure, convenient process implementation, and excellent heat dissipation efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 A buffer layer, a stop layer and a VCSEL epitaxial layer structure are grown on the front side of substrate A at one time.
[0030] Figure 2 The device structures such as P electrode and VCSEL table are manufactured on the front side of substrate A.
[0031] Figure 3 The adhesive is spin-coated on the front side of substrate A which has completed the mesa structure.
[0032] Figure 4 The substrate A after spin coating of adhesive is temporarily bonded to the support carrier.
[0033] Figure 5 The back side of the temporarily bonded substrate A is thinned.
[0034] Figure 6 The remaining substrate and buffer layer are removed.
[0035] Figure 7 The buffer layer and the stop layer are removed.
[0036] Figure 8 The N electrode is prepared on the back side of the N contact layer.
[0037] Fig. 9 The back N electrode of the VCSEL epitaxial layer is permanently bonded to the front side of another substrate B with a metal bonding layer prepared on the front side.
[0038] Fig.10 The permanent bonding structure formed by the support carrier, substrate B and VCSEL epitaxial layer is debonded, and then cleaned to obtain a VCSEL wafer with only the epitaxial layer film bonded to substrate B.
[0039] Figure numerals: 1-substrate A; 2-buffer layer; 3-stop layer; 4-VCSEL epitaxial layer consisting of N-contact layer, N-DBR, active layer, P-DBR and P-contact layer; 5-P electrode; 6-temporary adhesive; 7-support carrier; 8-N electrode; 9-metal layer on substrate B; 10-substrate B. DETAILED DESCRIPTION
[0040] The technical solution of the present invention is further described below in conjunction with the accompanying drawings.
[0041] A method for preparing a VCSEL chip comprises the following steps:
[0042] 1) A buffer layer 2, a stop layer 3, an N contact layer, an N-DBR, an active layer, a P-DBR and a P contact layer are sequentially grown on the front side of a substrate A1, wherein the N contact layer, the N-DBR, the active layer, the P-DBR and the P contact layer constitute a VCSEL epitaxial layer 4; wherein the material of the substrate A includes but is not limited to InP, GaAs or GaN, the thickness of the substrate A is between 100 μm and 1000 μm, the stop layer is InGaAs, InGaP, AlN or InGaAsP, and the thickness of the VCSEL epitaxial layer is between 500 nm and 15 μm, such as Figure 1 shown.
[0043] 2) Make a P contact metal on the P contact layer, then etch the P contact layer, P-DBR, active layer, N-DBR and N contact layer from the upper surface in sequence, and stop at the stop layer to form a mesa-type VCSEL device structure, and oxidize its surface, wherein the P electrode 5 material is TiPtAu, WTiAuTi or NiAlAu, the electrode thickness is 50nm to 1000nm, the etching gas is chlorine-based or fluorine-based gas, and the oxidation method is wet or dry oxidation, such as Figure 2 shown.
[0044] 3) Spin-coat a temporary adhesive 6 on the surface of the substrate A on which the mesa-type VCSEL device structure has been formed to cover the device structure, wherein the adhesive is a polymer, including but not limited to one of photoresist, high-temperature wax or BCB, and the thickness of the adhesive is 1 μm to 40 μm, such as Figure 3 shown.
[0045] 4) Temporarily bonding the substrate A to the front side of the support carrier 7, wherein the support carrier includes but is not limited to one of sapphire, silicon, silicon carbide or aluminum nitride wafers, the thickness of the support carrier is 300 μm-1200 μm, the temporary bonding temperature is 90-230° C., the pressure is 10 MPa-50 MPa, and the time is 10-60 minutes. Figure 4 shown.
[0046] 5) Thinning the substrate A temporarily bonded to the support carrier from the back side, wherein the substrate thinning method is any one or more of mechanical grinding, mechanical polishing, and chemical polishing, and the remaining substrate thickness after thinning is not less than 10 μm and not more than 120 μm, such as Figure 5 shown.
[0047] 6) removing the remaining substrate and the buffer layer except the epitaxial layer from the substrate A temporarily bonded to the support carrier to expose the back of the stop layer, wherein the method for removing the remaining substrate and the buffer layer is wet etching or dry etching, and the ratio of the removal rate of the substrate and the stop layer material by the removal method is 5:1 to 500:1, such as Figure 6 shown.
[0048] 7) removing the stop layer to obtain a VCSEL epitaxial layer structure temporarily bonded to the support carrier and exposing the back side of the N contact layer, wherein the stop layer is removed by wet etching or dry etching, and the ratio of the removal rate of the stop layer to the N contact layer material by the removal method is 5:1 to 500:1, such as Figure 7 As shown;
[0049] 8) Prepare an N electrode 8 on the back of the N contact layer, wherein the N electrode material is AuGeNiAu, TiPtAu, WTiAuTi or NiPdAu, and the electrode thickness is 50nm to 1000nm, such as Figure 8 shown.
[0050] 9) A bonding metal layer 9 is prepared on the front side of another high thermal conductivity substrate B10, wherein substrate B includes but is not limited to one of silicon carbide, aluminum nitride, and diamond wafer, the thickness of substrate B is between 100 μm and 1000 μm, the bonding metal layer includes but is not limited to TiAu, TiPtAu, WTiAu, AuSn or AuIn, and the thickness of the bonding metal layer is between 100 nm and 3 μm.
[0051] 10) The back N electrode of the VCSEL epitaxial layer temporarily bonded to the support carrier is placed opposite to the front surface of the B substrate, and is permanently bonded through a bonding metal layer, wherein the permanent bonding method includes but is not limited to one of eutectic bonding, hot pressing bonding, activation bonding and direct bonding, the bonding temperature is room temperature to 300° C., the bonding time is 5 minutes to 2 hours, and the bonding pressure is 200N to 50000N, such as Fig. 9 shown.
[0052] 11) Debonding and cleaning the permanent bonding structure formed between the support wafer, substrate B and VCSEL epitaxial layer, wherein the debonding method includes but is not limited to thermal debonding, laser debonding and gas debonding; the cleaning solvent includes but is not limited to acetone, alcohol or isopropanol, such as Fig.10 shown.
[0053] 12) A VCSEL chip with efficient heat dissipation effect is obtained on a high thermal conductivity substrate B, such as Fig.10 As shown, the total thermal resistance of the device is reduced by more than 30% compared with the original substrate.
[0054] The present invention is described in detail below with reference to the embodiments.
[0055] Example
[0056] A method for preparing a VCSEL chip comprises the following steps:
[0057] (1) InGaP, AlGaAs, GaAs N-DBR, active layer, P-DBR, P contact layer and other epitaxial layer structures are grown in sequence on the GaAs substrate wafer. The thickness of the InGaP layer is 100nm, and the total thickness of the VCSEL epitaxial functional layer is about 2μm.
[0058] (2) Deposit 20nm Ti+50nm Pt+50nm Au on the P contact layer as the P contact layer, and then use the P contact layer as a mask to etch the VCSEL epitaxial functional layer with a fluorine-based gas until the InGaP stop layer stops.
[0059] (3) Spin-coat a 20 μm thick layer of HT10.10 on the GaAs substrate wafer as a temporary adhesive at a spin-coating speed of 1500 rpm for 60 s and a pre-baking temperature of 160° C. for 2 minutes.
[0060] (4) Place the GaAs VCSEL wafer spin-coated with a temporary adhesive opposite to the front side of the sapphire carrier and place it in a wafer bonding machine for temporary bonding. The bonding process parameters are a temperature of 180° C., a bonding time of 20 minutes, and a bonding pressure of 20 MPa.
[0061] (5) The back side of the GaAs VCSEL wafer temporarily bonded to the sapphire carrier is thinned by mechanical grinding to 50 μm.
[0062] (6) Use a solution with a ratio of H2SO4:H2O2:H2O (1:2:5) to etch the remaining GaAs substrate and buffer layer until the InGaP stop layer is reached.
[0063] (7) Use a solution with a ratio of HCL:H3P04:H2O2 (1:10:1) to etch the 100nm InGaP stop layer.
[0064] (8) After removing the stop layer and exposing the N-contact layer, 100nm AuGeNi+Au is deposited by evaporation on the back side of the VCSEL structure.
[0065] (9) A 1 μm thick bonding metal layer is formed on the surface of the diamond substrate wafer by electroplating, and is also led out as an N-electrode test block.
[0066] (10) The back side of the GaAs VCSEL wafer after the substrate is removed is placed opposite to the front side of the diamond substrate. The VCSEL device structure is aligned with the metal pattern on the diamond substrate through an alignment bonding device, and then placed in a bonding machine for permanent bonding. The bonding process parameters are a temperature of 300° C., a bonding time of 60 minutes, and a bonding pressure of 4000 MPa.
[0067] (11) The temporary carrier, the bonded GaAs VCSEL wafer and the diamond wafer are placed face up on a heating table for heating at 250° C. The temporary carrier is separated by a hot sliding stripping method and cleaned with a debonding agent, acetone and alcohol.
[0068] After the above steps, the preparation of a VCSEL chip integrated on a high thermal conductivity diamond substrate with excellent heat dissipation effect is achieved.
[0069] The above contents are further detailed descriptions of the present invention in combination with specific preferred embodiments, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. For ordinary technicians in the technical field to which the present invention belongs, several simple deductions or substitutions can be made without departing from the concept of the present invention, which should be regarded as falling within the protection scope of the present invention.
Claims
1. A method for preparing a VCSEL chip, characterized in that: The following steps are involved: 1) A buffer layer, a stop layer, an N-contact layer, an N-DBR, an active layer, a P-DBR and a P-contact layer are sequentially grown on the front side of substrate A; 2) Make a P contact metal on the P contact layer, then etch the epitaxial structure to the stop layer to form a mesa-type VCSEL device structure, and oxidize its surface; 3) Spin coating a temporary adhesive on the surface of substrate A to cover the device structure; 4) Temporarily bonding the substrate A to the front side of the support carrier; 5) thinning the substrate A temporarily bonded to the support carrier from the back side; 6) removing the remaining substrate and the buffer layer except the epitaxial layer from the substrate A temporarily bonded to the support carrier to expose the back side of the stop layer; 7) removing the stop layer to obtain a VCSEL epitaxial layer structure temporarily bonded to the support carrier and exposing the back side of the N contact layer; 8) preparing an N electrode on the back side of the N contact layer; 9) Preparing a bonding metal layer on the front side of another high thermal conductivity substrate B; 10) The back N electrode of the VCSEL epitaxial layer temporarily bonded to the support carrier is placed opposite to the front surface of the B substrate and is permanently bonded through a bonding metal layer; 11) Debonding the permanent bonding structure formed by the support carrier, substrate B and VCSEL epitaxial layer, and cleaning it; 12) A VCSEL chip formed on a high thermal conductive substrate B is obtained.
2. The method for preparing a VCSEL chip according to claim 1, characterized in that: In step 1), the substrate A is made of InP, GaAs or GaN, the thickness of the substrate A is between 100 μm and 1000 μm, the stop layer is made of InGaAs, InGaP, AlN or InGaAsP, and the thickness of the VCSEL epitaxial layer is between 500 nm and 15 μm.
3. The method for preparing a VCSEL chip according to claim 1, characterized in that: In step 2), the P electrode material is TiPtAu, WTiAuTi or NiAlAu, the electrode thickness is 50nm to 1000nm, the etching gas is chlorine-based or fluorine-based gas, and the oxidation method is wet oxidation or dry oxidation.
4. The method for preparing a VCSEL chip according to claim 1, characterized in that: In step 3), the adhesive is a polymer, selected from photoresist, high temperature wax or BCB, and the thickness of the adhesive is 1 μm to 40 μm.
5. The method for preparing a VCSEL chip according to claim 1, characterized in that: In step 4), the support carrier is one of sapphire, silicon, silicon carbide or aluminum nitride wafers, the thickness of the support carrier is 300μm-1200μm, the temporary bonding temperature is 90-230°C, the pressure is 10MPa-50MPa, and the time is 10-60 minutes.
6. The method for preparing a VCSEL chip according to claim 1, characterized in that: In step 5), the substrate is thinned by any one or more of mechanical grinding, mechanical polishing, and chemical polishing, and the remaining substrate thickness after thinning is not less than 10 μm and not more than 120 μm.
7. The method for preparing a VCSEL chip according to claim 1, characterized in that: In step 6), the method for removing the remaining substrate is wet etching or dry etching, and the ratio of the removal rate of the substrate and the stop layer material by the removal method is 5:1 to 500:
1.
8. The method for preparing a VCSEL chip according to claim 1, characterized in that: In step 7), the stop layer is removed by wet etching or dry etching, and the ratio of the removal rate of the stop layer and the N-contact layer material by the removal method is 5:1 to 500:
1.
9. The method for preparing a VCSEL chip according to claim 1, characterized in that: In step 8), the N electrode material is AuGeNiAu, TiPtAu, WTiAuTi or NiPdAu, and the electrode thickness is 50nm to 1000nm; In step 9), substrate B includes but is not limited to one of silicon carbide, aluminum nitride, and diamond wafer, and the thickness of substrate B is 100μm to 1000μm; the bonding metal layer includes but is not limited to TiAu, TiPtAu, WTiAu, AuSn or AuIn, and the thickness of the bonding metal layer is 100nm-3μm.
10. The method for preparing a VCSEL chip according to claim 1, characterized in that: In step 10), the permanent bonding method is one of eutectic bonding, hot pressing bonding, activation bonding and direct bonding, the bonding temperature is room temperature to 300° C., the bonding time is 5 minutes to 2 hours, and the bonding pressure is 200N to 50000N; In step 11), the debonding method includes thermal debonding, laser debonding and gas debonding; the cleaning solvent is acetone, alcohol or isopropanol.
Citation Information
Patent Citations
Substrate-free high-power amplitude limiter and preparation method thereof
CN114023826A
VCSEL chip with aluminum nitride ceramic substrate and manufacturing method of VCSEL chip
CN114204403A
Batch high-precision layer transfer heterogeneous integration method
CN115223876A
Vertical cavity surface emitting laser and manufacturing method thereof
CN115473123A
Dilute nitrogen laser chip and preparation method thereof
CN117856042A
Cited By
Laser N-surface contact preparation method
CN120834498A