Coating method
By performing a pre-drying step at the primer curing starting temperature, the problem of low energy efficiency in existing painting methods is solved, rapid evaporation of water and avoidance of uneven drying are achieved, significantly saving energy and improving the efficiency of the painting process. .
Patent Information
- Application Number
- CN202310467404.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-27
- Publication Date
- 2024-10-29
AI Technical Summary
In existing coating methods, the preheating step consumes a lot of energy and affects low energy efficiency. Although the flash-drying primer method is energy-saving, it takes a long time, resulting in high energy consumption and it is difficult to effectively solve the problem of low energy efficiency.
The pre-drying step is carried out at the primer curing starting temperature, and the water is evaporated in a short time through air blowing to avoid uneven drying and paint film bursting. The pendulum test is used to measure the primer curing starting temperature to determine the appropriate blowing temperature. and time.
It achieves rapid evaporation of water before the primer starts to cross-link, shortens the pre-drying time, saves energy, avoids uneven drying and paint film bursting, and improves energy efficiency.
Smart Images

Figure CN118847482A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a coating method. Background Art
[0002] Since the beginning, efforts have been made to mitigate climate change or reduce its impact, and in order to achieve the above-mentioned goals, research and development related to reducing carbon dioxide emissions is being carried out.
[0003] Most existing coating methods use wet-on-wet coating. Wet-on-wet coating involves first applying a primer, and after setting and preheating, applying a clear coat on the primer, and then baking. The aforementioned preheating step has the function of volatilizing the solvent, inhibiting paint cracking, and film formation. However, the preheating step is usually performed at a high temperature, resulting in low energy efficiency; if it is changed to a low-temperature preheating, the paint will harden and cracking will not be inhibited.
[0004] Therefore, in order to improve the above problems, some studies have been conducted to replace the above preheating step with a flash-off primer at room temperature. However, in order to reduce carbon dioxide emissions, the above flash-off primer method requires a long time, resulting in high energy consumption, so how to solve the low energy efficiency is a problem. Summary of the invention
[0005] The present invention aims to achieve energy saving in order to solve the above-mentioned problems and further contribute to the mitigation of climate change or the reduction of its impact.
[0006] According to an embodiment of the present invention, a coating method includes a first coating step, a pre-drying step, a second coating step and a main drying step. The first coating step is to apply a primer on a workpiece. The pre-drying step is to blow air to the applied primer to pre-dry the primer, wherein the temperature of the air is the curing starting temperature of the primer. The second coating step is to apply a clear coat on the pre-dried primer. The main drying step is to dry the workpiece coated with the clear coat.
[0007] In the coating method according to the embodiment of the present invention, the humidity of the wind is below 50%.
[0008] In the coating method according to the embodiment of the present invention, a measurement step of measuring the curing start temperature of the primer in advance is also included, the measurement step includes contacting a pendulum with the liquid primer and measuring the cycle of the pendulum, and heating the primer while measuring the cycle and measuring the temperature of the primer. The temperature when the cycle of the pendulum decreases is the curing start temperature.
[0009] In the coating method according to the embodiment of the present invention, the curing start temperature of the clear coating is higher than the curing start temperature of the primer.
[0010] In the coating method according to the embodiment of the present invention, the primer is a multi-layer primer, and the multi-layer primer is coated on the workpiece in the first coating step.
[0011] In the coating method according to the embodiment of the present invention, the multi-layer primer has different curing start temperatures, and the lowest temperature among the different curing start temperatures is used as the temperature of the wind in the pre-drying step.
[0012] Based on the above, since in the coating method of the present invention, by blowing air at the curing starting temperature of the primer, water can be evaporated before the primer starts cross-linking, and compared with the method of flash drying the primer at room temperature, the pre-drying step of the present invention is shorter, so energy can be saved.
[0013] In order to make the above features and advantages of the present invention more clearly understood, embodiments are given below with reference to the accompanying drawings for detailed description. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is a step diagram of a coating method according to an embodiment of the present invention.
[0015] Figure 2 It is a curve chart obtained by a pendulum test performed by the coating method of the embodiment.
[0016] Description of Reference Numerals
[0017] 100: First painting step
[0018] 102: Measurement steps
[0019] 110: Pre-drying step
[0020] 120: Second painting step
[0021] 130: Main drying steps DETAILED DESCRIPTION
[0022] Figure 1 It is a step diagram of a coating method according to an embodiment of the present invention.
[0023] Please refer to Figure 1The coating method of this embodiment includes first performing a first coating step 100, wherein the first coating step 100 is to apply a primer on a workpiece, wherein the workpiece is not particularly limited, for example, a car body. In one embodiment, the first coating step 100 only applies a layer of primer; in another embodiment, the first coating step 100 may apply multiple layers of primer, and the curing starting temperatures of the multiple layers of primer may be the same or different.
[0024] The primer is not particularly limited, and for example, a well-known water-based primer can be used.
[0025] The resin component contained in the water-based primer is not particularly limited, and examples thereof include water-based acrylic resins, acrylic resin emulsions, water-based polyester resins, water-based polyurethane resins, water-based melamine resins, and water-based blocked isocyanate resins.
[0026] The pigment contained in the water-based primer is not particularly limited, and examples thereof include aluminum paste and the like.
[0027] The additives contained in the water-based primer are not particularly limited, and examples thereof include ultraviolet absorbers, defoamers, surfactants, rheology control agents, dispersants, and amines.
[0028] The organic solvent contained in the water-based base coating material is not particularly limited, and examples thereof include alcohols and esters.
[0029] In addition, the primer can be a one-component system or a two-component system.
[0030] The method of applying the primer is not particularly limited, and examples thereof include spray coating, rotary atomization coating, and inkjet coating.
[0031] Then, a pre-drying step 110 is performed, wherein the pre-drying step 110 is to blow air on the applied primer to pre-dry the primer, wherein the temperature of the air is the curing starting temperature of the primer. In one embodiment, if only one layer of primer is applied in the first coating step 100, the temperature of the air is the curing starting temperature of the primer; in another embodiment, if multiple layers of primer are applied in the first coating step 100 and the curing starting temperatures of these primers are different, the temperature of the air is the one with the lowest curing starting temperature among these primers. In the pre-drying step 110, the wind speed is, for example, greater than 3 m / s and less than 7 m / s, preferably greater than 4 m / s and less than 6 m / s; the time for blowing air on the applied primer is, for example, greater than 10 minutes and less than 15 minutes, preferably greater than 10 minutes and less than 11 minutes. However, the present invention is not limited thereto, and the wind speed and blowing time may also be changed as required.
[0032] By blowing air at the curing starting temperature, the moisture can be volatilized in a shorter time than flashing off at room temperature without being trapped, thereby achieving energy saving. Moreover, flashing off at room temperature will also cause the problem of uneven drying, but by blowing air at the curing starting temperature of the present invention, the situation of uneven drying can be suppressed. On the other hand, if the temperature of the wind is higher than the curing starting temperature of the primer, the primer will begin to cross-link, making it difficult for the moisture to volatilize and bubbles to be generated, and there will be problems with the paint film bursting later. By flashing off in the above manner of the present invention, the moisture can be volatilized to prevent the generation of bubbles and bursting.
[0033] In the pre-drying step 110, the humidity of the wind may be below 50%, for example, 50% humidity or below 50% humidity. By blowing air at the curing starting temperature and humidity below 50%, the moisture in the primer can be volatilized more effectively and the pre-drying can be completed in a short time, thereby saving energy.
[0034] In addition, before the pre-drying step 110, shaping may be performed as needed. The conditions for shaping the workpiece coated with the primer are not particularly limited, for example, 20° C. or higher and 30° C. or lower, and 5 minutes or higher and 15 minutes or lower. However, the present invention is not limited thereto, and the shaping time may also be changed as needed.
[0035] In the present embodiment, the coating method further comprises a measuring step 102 for pre-measuring the curing starting temperature of the primer. The measuring step 102, for example, brings a pendulum into contact with the liquid primer and measures the period of the pendulum, and while measuring the period, heats the primer and measures the primer temperature. The "curing starting temperature" of the present embodiment is the temperature when the period of the pendulum obtained from the above-mentioned measuring step 102 decreases. If the pre-drying step 110 is performed according to the curing starting temperature of the primer determined by the period measured by the above swing test, water can be volatilized more effectively and pre-dried in a short time, which is conducive to saving energy.
[0036] Figure 2 The graph shows the results of the pendulum test performed by the coating method of this embodiment, which can be measured using an existing pendulum tester. In the pendulum test, the temperature of the primer is increased from 25°C in a step-by-step manner while measuring the period of the pendulum. Figure 2 It can be seen that after the temperature gradually rises, the period of the pendulum changes twice. The first change occurs at 18.5 minutes, when the temperature is close to 60°C, and the second change occurs at around 31 minutes, where the period is significantly reduced. The first change is when the primer begins to cure, so the curing starting temperature of the tested primer can be obtained from the above test to be 60°C.
[0037] Next, a second coating step 120 is performed to coat the clearcoat on the pre-dried primer. In one embodiment, the curing starting temperature of the clearcoat is higher than the curing starting temperature of the primer. Therefore, even if a little water remains in the primer in the pre-drying step 110, it is possible to prevent water from being retained in the film layer formed by the clearcoat in the subsequent drying step, thereby avoiding cracking.
[0038] The varnish is not particularly limited, and for example, a well-known solvent-based varnish can be used.
[0039] The resin component contained in the solvent-based varnish is not particularly limited, and examples thereof include acrylic resins and hexamethylene diisocyanate (HMDI)-based isocyanurate prepolymers.
[0040] The additives contained in the solvent-based varnish are not particularly limited, and examples thereof include ultraviolet ray absorbers (UV agents), light stabilizers, surface conditioners, anti-sagging agents, curing accelerators, and rheology control agents.
[0041] The organic solvent contained in the solvent-based varnish is not particularly limited, and examples thereof include aromatic solvents, alcohols, esters, ketones, petroleum solvents, hydrocarbons, and the like.
[0042] In addition, the varnish may be a one-component system or a two-component system.
[0043] The method of applying the varnish is not particularly limited, and examples thereof include spray coating, rotary atomization coating, and inkjet coating.
[0044] After that, the main drying step 130 is performed to dry the workpiece coated with the varnish. The drying method is not particularly limited, such as heating drying (baking drying), and the drying conditions are not particularly limited, such as 80° C. to 100° C., and 15 minutes to 60 minutes. However, the present invention is not limited thereto, and the drying temperature and time can also be changed according to needs.
[0045] According to this embodiment, the purpose of energy saving can be achieved, and further, it can also help to mitigate climate change or reduce its impact.
[0046] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A coating method, characterized in that: include: A first coating step of applying a primer to the workpiece; A pre-drying step of blowing air to the applied primer to pre-dry the primer; A second coating step of applying a clear coat on the pre-dried primer; as well as a main drying step of the workpiece coated with the varnish, The temperature of the wind is the curing starting temperature of the primer.
2. The coating method according to claim 1, characterized in that: The humidity of the wind is below 50%.
3. The coating method according to claim 1, characterized in that: The method further includes a step of measuring the curing starting temperature of the primer in advance, wherein the measuring step comprises: placing a pendulum in contact with the primer in liquid form and measuring the period of the pendulum; and while measuring the cycle, heating the primer at an increasing temperature and measuring the temperature of the primer, The temperature at which the period of the pendulum decreases is the curing start temperature.
4. The coating method according to claim 1, characterized in that: The curing starting temperature of the clear coating is higher than the curing starting temperature of the primer.
5. The coating method according to claim 1, characterized in that: The primer is a multi-layer primer, and the multi-layer primer is applied to the workpiece in the first coating step.
6. The coating method according to claim 5, characterized in that: The multi-layer primer has different curing start temperatures, and the lowest temperature among the different curing start temperatures is used as the temperature of the wind in the pre-drying step.